Methods for recycling and treating chemical polishing waste liquid

By combining electrodialysis and nanofiltration, the problem of acid ratios not being suitable for high-precision processes in the recycling and treatment of chemical polishing waste liquid has been solved, enabling the preparation of high phosphorus-to-sulfur ratio reusable acid, thereby increasing product added value and application scenarios.

CN123105904APending Publication Date: 2026-11-17HUIZHOU ZHENDING ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611413724.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-11
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing methods for recycling and treating chemical polishing waste liquid cannot meet the requirements of high-precision processes for specific acid ratios, resulting in limited application scenarios for recycled acids and insufficient product added value and market competitiveness.

Method used

A separation process combining electrodialysis and nanofiltration is adopted. The electrodialysis system removes aluminum ions and metal impurities, the nanofiltration system removes multivalent ions, and finally the high phosphorus-to-sulfur ratio reclaimed acid is obtained by evaporation and concentration.

Benefits of technology

The preparation of reusable acid with a high phosphorus-to-sulfur ratio has been achieved, which is suitable for closed-loop in-situ reuse of chemical polishing fluid, reducing the cost of purchasing new acid and the cost of transporting and disposing of waste acid, and expanding market application scenarios such as fertilizer production and industrial cleaning.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123105904A_ABST
    Figure CN123105904A_ABST
Patent Text Reader

Abstract

This invention discloses a method for recycling and treating chemical polishing waste liquid, comprising: providing chemical polishing waste acid containing phosphoric acid, sulfuric acid, nitric acid, aluminum ions, and metal impurity ions; passing the waste acid into an electrodialysis system for first-stage separation, where aluminum ions, phosphate ions, and metal impurities in the waste acid are enriched in the desalination chamber of the electrodialysis system, while sulfate ions and nitrate ions preferentially permeate through the ion exchange membrane into the concentrate chamber, yielding a first concentrate and a first desalination; passing the first desalination into a nanofiltration system for second-stage separation, where aluminum ions and metal impurities in the first desalination are enriched in the nanofiltration concentrate chamber, while phosphoric acid and sulfuric acid molecules preferentially permeate through the nanofiltration membrane into the nanofiltration desalination chamber, yielding a second concentrate and a second desalination; concentrating the second desalination until the phosphoric acid mass concentration reaches a preset mass concentration to obtain the target reusable acid. The obtained target reusable acid has a high phosphorus-to-sulfur ratio and can be used as a basic raw material for chemical polishing liquid, realizing closed-loop in-situ reuse of waste acid and reducing the cost of purchasing new acid and transporting waste acid.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of waste acid treatment technology, and more specifically, to a method for recycling and treating chemical polishing waste liquid. Background Technology

[0002] Chemical polishing is a key process in the surface treatment of aluminum and aluminum alloy products. The polishing solution typically consists mainly of phosphoric acid and sulfuric acid, supplemented with small amounts of oxidizing agents such as nitric acid. As the polishing process continues, aluminum ions accumulate in the polishing solution. When the aluminum ion concentration reaches a certain level, the treatment effect of the polishing solution significantly decreases, resulting in a large amount of waste acid from chemical polishing. This waste acid mainly contains phosphoric acid, sulfuric acid, aluminum ions, and a small amount of nitric acid. Direct discharge not only wastes resources such as phosphoric acid and sulfuric acid but also imposes a serious environmental burden; therefore, resource recycling and treatment are urgently needed.

[0003] Currently, the main technologies for treating waste acid from chemical polishing include diffusion dialysis membrane separation technology and ion exchange resin adsorption technology. Chinese patent application CN120794227A discloses a comprehensive utilization device and process for waste acid from chemical polishing. This device separates the original waste acid into membrane-generated acid and membrane-generated waste through a diffusion dialysis membrane unit. The membrane-generated acid is evaporated at low temperature to obtain reusable phosphoric acid, while the membrane-generated waste is adsorbed with resin to remove aluminum ions. The saturated resin is then eluted and regenerated using sulfuric acid. The eluent is then regenerated with sulfuric acid through a selective ion exchange membrane unit. The aluminum sulfate waste liquid is evaporated and crystallized to recover aluminum sulfate. Simultaneously, the condensate generated in each step is returned to the system for recycling, achieving the resource recovery of phosphoric acid, sulfuric acid, and aluminum sulfate from the waste acid.

[0004] However, the existing technologies mentioned above are limited to separating and recovering various components from waste acid. The ratio of phosphate to sulfate in the recycled acid after treatment basically depends on the initial composition of the original waste acid, which limits the application scenarios of recycled acid: when the proportion of phosphate in recycled acid is low and the proportion of sulfate is high, its recycling scenarios are limited to rough processes with low requirements for acid composition, and it is difficult to adapt to the strict requirements of high-precision processes such as precision chemical polishing for specific acid ratios, resulting in insufficient product added value and market competitiveness.

[0005] To address the aforementioned issues, existing methods for recycling and treating chemical polishing waste liquid urgently need improvement. Summary of the Invention

[0006] To address the shortcomings of existing technologies, this invention provides a method for recycling and treating chemical polishing waste liquid, comprising the following steps: S10. Provides chemical polishing waste acid containing phosphoric acid, sulfuric acid, nitric acid, aluminum ions and metal impurity ions; S20. The chemical polishing waste acid is passed into the electrodialysis system for first-stage separation. Under the action of the electric field, aluminum ions, phosphate ions and metal impurity ions in the chemical polishing waste acid are enriched in the desalination chamber of the electrodialysis system, while sulfate ions and nitrate ions preferentially pass through the ion exchange membrane into the concentrate chamber to obtain the first concentrate and the first desalination. S30. The first fresh water is passed into a nanofiltration system for second-stage separation. The nanofiltration membrane retains multivalent ions, so that aluminum ions and metal impurity ions in the first fresh water are enriched in the nanofiltration concentrate chamber. Free phosphoric acid and sulfuric acid molecules preferentially pass through the nanofiltration membrane into the nanofiltration fresh water chamber to obtain the second concentrate and the second fresh water. S40. The second freshwater is evaporated and concentrated until the phosphoric acid mass concentration reaches the preset mass concentration to obtain the target recycled acid.

[0007] Preferably, after step S10, the method further includes: Pretreatment of chemical polishing waste liquid removes suspended solids, oil, and organic matter, and controls the content of suspended solids, chemical oxygen demand, and free residual chlorine in the chemical polishing waste liquid within the tolerance range of the ion exchange membrane of the electrodialysis system.

[0008] Preferably, the mass concentrations of each component in the chemical polishing waste acid are as follows: phosphoric acid concentration is 5-16%, sulfuric acid concentration is 2.5-7%, nitric acid concentration is ≤1%, aluminum ion concentration is 2-8%, and metal impurity ion concentration is 0.2-0.5%.

[0009] Preferably, the acidity of the chemical polishing waste liquid is 1.1-3.1 mol / L.

[0010] Preferably, step S20 specifically includes: The chemical polishing waste acid is passed into the desalination chamber of the electrodialysis system; A DC electric field is applied to the membrane to control the current density and adjust the flow ratio between the concentrate chamber and the desalination chamber to maintain the fluids in the concentrate and desalination chambers in a turbulent state. The chemical polishing waste liquid is then subjected to first-stage electrodialysis separation under a first preset temperature condition. This results in aluminum ions, phosphate ions, and metal impurity ions in the chemical polishing waste acid being enriched in the desalination chamber of the electrodialysis system. Sulfate ions and nitrate ions preferentially permeate through the ion exchange membrane into the concentrate chamber, yielding the first concentrate and the first desalination.

[0011] Preferably, step S30 specifically includes: The first fresh water obtained from the first stage separation is passed into a nanofiltration system and subjected to nanofiltration treatment at a first preset pressure and a second preset temperature. By utilizing the retention effect of the nanofiltration membrane on multivalent ions, aluminum ions and metal impurity ions in the first fresh water are enriched in the nanofiltration concentrate chamber, while phosphoric acid and sulfuric acid molecules preferentially pass through the nanofiltration membrane into the nanofiltration fresh water chamber, thus obtaining the second concentrate and the second fresh water.

[0012] Preferably, step S40 specifically includes: The second fresh water is passed into a preheater for preheating; The preheated second fresh water is fed into an evaporator and evaporated and concentrated under the conditions of a third preset temperature and a second preset pressure. The evaporated water vapor is then condensed and recovered. When the mass concentration of phosphoric acid in the second fresh water reaches the preset mass concentration, the second fresh water is cooled to obtain the target reusable acid.

[0013] Preferably, the preset mass concentration is 50-55%.

[0014] Preferably, the target recycled acid has a phosphoric acid to sulfuric acid mass concentration ratio greater than or equal to 7:1 and an aluminum ion mass concentration less than 1 g / L.

[0015] The beneficial effects of this invention are as follows: This invention employs a cascade separation process of electrodialysis, nanofiltration, and evaporation concentration to precisely remove impurity ions in chemical polishing wastewater by addressing the differences in the characteristics of each component: the electrodialysis stage preferentially removes nitrate and most sulfate ions, while the nanofiltration stage selectively retains aluminum ions and metallic impurities, allowing phosphate ions and residual sulfate ions to pass through preferentially. The target recovered acid obtained after this combined separation and evaporation concentration has a high phosphorus-to-sulfur ratio (P / S). This high P / S ratio target recycled acid can be directly used as a base material for chemical polishing solutions, achieving closed-loop in-situ reuse of chemical polishing waste acid, thereby reducing the cost of purchasing new acid and the expense of transporting and disposing of waste acid. Furthermore, the high P / S ratio of the target recycled acid obtained by this invention indicates high phosphoric acid purity, which can also be applied in fertilizer production, industrial cleaning, food additives, and other fields, offering a wide range of market applications. Attached Figure Description

[0016] The accompanying drawings, which are provided to further illustrate the invention and constitute a part of this invention, are illustrative embodiments of the invention and their descriptions are used to explain the invention and do not constitute an undue limitation of the invention.

[0017] Figure 1 This is a schematic flowchart of the method for recycling and treating waste acid from chemical polishing according to the present invention. Detailed Implementation

[0018] The following drawings disclose several embodiments of the present invention. For clarity, many practical details will be described in the following description. However, it should be understood that these practical details are not intended to limit the invention. That is, in some embodiments of the invention, these practical details are not essential. Furthermore, for the sake of simplicity, some conventional structures and components will be shown in the drawings in a simple schematic manner.

[0019] It should be noted that all directional indications in the embodiments of the present invention, such as up, down, left, right, front, back, etc., are only used to explain the relative positional relationship and movement of the components in a specific posture as shown in the attached figure. If the specific posture changes, the directional indication will also change accordingly.

[0020] Furthermore, in this invention, the use of terms such as "first," "second," etc., is for descriptive purposes only and does not specifically refer to any order or sequence, nor is it intended to limit the invention. They are merely used to distinguish items or operations described using the same technical terms and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features. Additionally, the technical solutions of the various embodiments can be combined with each other, but only if they are feasible for those skilled in the art. If a combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.

[0021] To further understand the invention's content, features, and effects, the following embodiments are provided, along with detailed descriptions in conjunction with the accompanying drawings: Reference Figure 1 , Figure 1 This is a schematic flowchart of the chemical polishing waste liquid recycling and treatment method of the present invention. The present invention provides a method for recycling and treating chemical polishing waste liquid, comprising the following steps: S10. Provides chemical polishing waste acid containing phosphoric acid, sulfuric acid, nitric acid, aluminum ions and metal impurity ions.

[0022] In the chemical polishing process of aluminum profiles, a mixed acid consisting of phosphoric acid, sulfuric acid, and nitric acid is typically used to treat the aluminum surface. The ratio of phosphoric acid to sulfuric acid varies from 1:1 to 1:0 depending on the process requirements. The nitric acid content is generally about 10% of the total volume of phosphoric acid and sulfuric acid, and the polishing temperature is generally 80-120℃. As the polishing process proceeds, some aluminum on the surface dissolves, forming aluminum ions that enter the acid solution. When the aluminum ion concentration in the polishing tank rises to a certain value (e.g., 30-45 g / L) and the acid concentration drops to a certain value, the polishing effect significantly decreases, requiring the tank solution to be replaced, generating waste acid from the chemical polishing process. Simultaneously, after polishing, the aluminum profiles need to be rinsed in a water washing tank to remove residual acid from their surface. This process generates a high-concentration first mixed acid waste solution in the acid tank and a low-concentration second mixed acid waste solution during the water washing process.

[0023] The chemical polishing waste liquid recycled and treated by this invention can be the first mixed acid waste liquid, the second mixed acid waste liquid, or a mixed waste liquid obtained by mixing the first mixed acid waste liquid and the second mixed acid waste liquid. The mass concentrations of each component in the chemical polishing waste acid recycled and treated by this invention are as follows: phosphoric acid concentration 5-16%, sulfuric acid 2.5-7%, nitric acid ≤1%, aluminum ions 2-8%, and metal impurity ions 0.2-0.5%. The metal impurity ions include, but are not limited to, iron ions, copper ions, and zinc ions.

[0024] Before recycling chemical polishing wastewater, this invention requires pretreatment of the wastewater. Specifically, after step S10, the pretreatment includes removing suspended solids, solid impurities, oil, and organic matter, and controlling the suspended solids, chemical oxygen demand (COD), and free residual chlorine content within the tolerance range of the ion exchange membrane in the electrodialysis system. Specifically, filtration is first used to remove suspended solids and solid impurities, followed by extraction to remove oil and organic matter. The pretreated wastewater is ensured to have suspended solids <1.0 mg / L, COD <200 mg / L, be oil-free, and free residual chlorine <0.1 mg / L.

[0025] The specific steps for removing suspended solids and solid impurities through filtration are as follows: The chemical polishing waste liquid is introduced into a filtration device and subjected to two stages of filtration—coarse filtration and fine filtration—to remove suspended solids and solid impurities. Coarse filtration can be performed using a grid, screen, or bag filter to intercept larger solid impurities in the waste liquid. Fine filtration can be performed using a precision filter, cartridge filter, or microporous membrane to remove fine suspended solids, resulting in a clear filtrate. The filtered clear filtrate is collected in a filtrate storage tank for subsequent extraction processes. The retained suspended solids and solid impurities are periodically removed and transported off-site.

[0026] The specific steps for removing oil and organic matter through extraction are as follows: The clarified filtrate after filtration is added to the extraction equipment at a certain volume ratio with an organic extractant, and the mixture is thoroughly mixed and contacted to transfer the oil and organic matter from the aqueous phase to the organic phase in the chemical polishing waste liquid. After mixing and contact, the mixture is allowed to stand and separate into layers, yielding a loaded organic phase and a raffinate aqueous phase. The oil and organic matter are enriched in the loaded organic phase. The organic extractant can be one or more of tributyl phosphate, trialkylphosphine oxide, cyclohexane, or kerosene. To ensure extraction efficiency, single-stage or multi-stage countercurrent extraction can be used. The volume ratio V1 of the organic phase to the aqueous phase is controlled within the range of 1:10 to 1:3, and the extraction temperature T1 is controlled within the range of 25-35℃ depending on the properties of the chemical polishing waste liquid. The raffinate aqueous phase after separation is the chemical polishing waste liquid from which oil and organic matter have been removed. The loaded organic phase then enters the back-extraction regeneration process to recover the organic extractant for recycling.

[0027] Among them, the filtration and extraction process parameters, such as filtration accuracy, extraction ratio, number of stages, and temperature, are all within the conventional adjustable range, and can be determined by those skilled in the art based on the actual composition and impurity content of the chemical polishing waste liquid.

[0028] Through the above filtration and extraction processes, a pretreated chemical polishing waste liquid is obtained, with a pH value less than 1 and an acidity of approximately 1.1 to 3.1 mol / L.

[0029] S20. The chemical polishing waste acid is introduced into the electrodialysis system for first-stage separation. Under the action of the electric field, aluminum ions, phosphate ions and metal impurity ions in the chemical polishing waste acid are enriched in the desalination chamber of the electrodialysis system, while sulfate ions and nitrate ions preferentially pass through the ion exchange membrane into the concentrate chamber to obtain the first concentrate and the first desalination.

[0030] In this invention, the pretreated chemical polishing wastewater enters an electrodialysis (ED) system for first-stage separation. The ED system mainly consists of three parts: a membrane stack, an electrode system, and auxiliary equipment. The membrane stack comprises cation exchange membranes, anion exchange membranes, separators, and electrodes. The cation exchange membranes and anion exchange membranes are arranged alternately, with adjacent membranes separated by separators, forming a two-compartment structure of a desalination chamber and a concentrate chamber. The membrane stack contains at least five sets of repeating unit electrodialysis cells, i.e., at least five pairs of cation exchange membranes and anion exchange membranes arranged alternately. The separator thickness is 0.5–2.0 mm, preferably 0.5 mm, and the separator has flow channel distribution grooves to ensure uniform liquid distribution on the membrane surface and reduce dead zones. The anion exchange membrane is a tribasic acid selective ion exchange membrane. This membrane has selective permeability to sulfate and nitrate ions in the chemical polishing wastewater, while retaining polyvalent metal cations such as phosphate, aluminum, iron, copper, and zinc ions. The tribasic acid selective ion exchange membrane can be a quaternary ammonium anion exchange membrane or a pyridine anion exchange membrane, with a membrane thickness of 0.1–0.25 mm, preferably 0.2 mm. The cation exchange membrane can be a sulfonic acid cation exchange membrane.

[0031] The electrode system includes an anode and a cathode respectively disposed at both ends of the membrane stack. The electrode material is titanium-coated ruthenium or titanium-coated iridium. A partition separates the electrode from the adjacent ion exchange membrane to form an electrode chamber, into which an electrode solution is introduced. The electrode solution is a sodium sulfate solution or a sulfuric acid solution with a concentration of 1%–5%, preferably 3%. The electrode solution is used to maintain electrode conductivity and remove gases generated by the electrode reaction.

[0032] The pretreated chemical polishing waste liquid is fed into each desalination chamber, deionized water into each concentration chamber, and electrode solution into the electrode plate chamber. Each liquid flow channel is independent and separated by partitions and ion exchange membranes. Under the action of a DC electric field, phosphate, sulfate, and nitrate ions in the chemical polishing waste liquid in the desalination chamber migrate towards the anode. Phosphate ions, being large trivalent ions, are retained in the desalination chamber; nitrate ions and most sulfate ions pass through the tribasic acid selective anion exchange membrane into the concentration chamber; while aluminum ions and metallic impurity cations (including but not limited to iron, copper, and zinc ions) are retained in the desalination chamber by the tribasic acid selective anion exchange membrane, thereby removing most of the sulfuric acid from the pretreated chemical polishing waste liquid.

[0033] Step S20 specifically includes the following processes: passing the chemical polishing waste acid into the desalination chamber of the electrodialysis system; applying a DC electric field to the membrane voltage, controlling the current density, adjusting the flow ratio of the concentrate chamber to the desalination chamber, maintaining the fluids in the concentrate chamber and the desalination chamber in a turbulent state, and performing first-stage electrodialysis separation on the chemical polishing waste liquid under a first preset temperature condition; so that aluminum ions, phosphate ions, and metal impurity ions in the chemical polishing waste acid are enriched in the desalination chamber of the electrodialysis system; sulfate ions and nitrate ions preferentially permeate through the ion exchange membrane into the concentrate chamber to obtain the first concentrate and the first desalination.

[0034] Among them, the membrane voltage U1 is 1.5-3 V, the current density J1 is 100-300 mA / cm², the first preset temperature T2 is 30-40℃, the fluid velocity SV1 between the concentrate chamber and the desalination chamber is 0.5-1.0 BV / h, and the flow ratio Q1 between the concentrate chamber and the desalination chamber is 0.95-1.05.

[0035] S30. The first fresh water is passed into a nanofiltration system for second-stage separation. The nanofiltration membrane retains multivalent ions, causing aluminum ions and metal impurity ions in the first fresh water to be enriched in the nanofiltration concentrate chamber. Free phosphoric acid and sulfuric acid molecules preferentially pass through the nanofiltration membrane into the nanofiltration desalination chamber, resulting in the second concentrate and the second fresh water.

[0036] Step S30 specifically includes the following processing: the first fresh water obtained from the first stage separation is introduced into a nanofiltration system and subjected to nanofiltration treatment at a first preset pressure and a second preset temperature. By utilizing the retention effect of the nanofiltration membrane on multivalent ions, aluminum ions and metal impurity ions in the first fresh water are enriched in the nanofiltration concentrate chamber, while phosphoric acid and sulfuric acid molecules preferentially pass through the nanofiltration membrane into the nanofiltration fresh water chamber to obtain the second concentrate and the second fresh water.

[0037] The nanofiltration system used in this invention includes a feed tank, a high-pressure pump, a nanofiltration membrane module, a desalination chamber, and a concentrate chamber connected in sequence. The nanofiltration membrane module has an inlet, a desalination outlet, and a concentrate outlet. The membrane module uses a spiral wound nanofiltration membrane made of polyamide composite material. The second preset temperature T3 is 25~35℃, and the first preset pressure P1 is 1.5~4.1 MPa. This is a dynamic process where the operating pressure of the nanofiltration system gradually increases, i.e., as the operating pressure of the nanofiltration system gradually increases from 1.5 MPa to 4.1 MPa, it is maintained within the range of 1.5 MPa to 4.1 MPa. Preferably, the first preset pressure is 2-4.1 MPa, i.e., as the operating pressure of the nanofiltration system gradually increases from 2 MPa to 4.1 MPa, it is maintained within the range of 2 MPa to 4.1 MPa.

[0038] Step S30 specifically includes the following processing: The first freshwater obtained in step S20 is temporarily stored in a feed tank. A high-pressure pump is used to pressurize the first freshwater in the feed tank to a first preset pressure P1, and the temperature is adjusted to a second preset temperature T3 before pumping it into a nanofiltration membrane module for cross-flow filtration. When the first freshwater flows across the surface of the nanofiltration membrane, under pressure, phosphoric acid and sulfuric acid preferentially permeate through the nanofiltration membrane, forming a permeate rich in phosphoric acid and sulfuric acid. This permeate enters the freshwater chamber for collection via the product water outlet, and the collected product water is the second freshwater. Aluminum ions and other metal impurities in the first freshwater are retained by the nanofiltration membrane, forming a concentrated solution rich in aluminum salts. This concentrated solution enters the concentrated solution chamber for collection via the concentrated solution outlet, and the collected concentrated solution is the second concentrated solution.

[0039] S40. The second freshwater is evaporated and concentrated until the phosphoric acid mass concentration reaches the preset mass concentration to obtain the target recycled acid.

[0040] Step S40 specifically includes the following processing: The second fresh water is preheated by passing it through a preheater. The preheated second fresh water is then passed through an evaporator and concentrated under a third preset temperature T4 and a second preset pressure P2. The evaporated water vapor is condensed and recovered. When the mass concentration of phosphoric acid in the second fresh water reaches a preset mass concentration, the second fresh water is cooled to obtain the target reusable acid. The third preset temperature T4 is 75-85℃, and the second preset pressure P2 is 0.085-0.095MPa.

[0041] The evaporation system for concentrating second freshwater according to this invention includes a feed pump, a preheater, an evaporator, a separator, a condenser, a vacuum pump, and a concentrated acid collection tank connected in sequence. The evaporator is a forced circulation evaporator, and its heating medium is steam. Specifically, step S40 includes: feeding the second freshwater into the feed pump, which then delivers it to the preheater for preheating. The preheated second freshwater enters the evaporator and is heated and evaporated under a second preset pressure P2 and a third preset temperature T4. The water in the second freshwater vaporizes upon heating, forming steam, while phosphoric acid and sulfuric acid, due to their higher boiling points, remain in the liquid phase, thus concentrating the phosphoric acid and sulfuric acid in the second freshwater. The steam generated by evaporation undergoes gas-liquid separation in the separator. The separated liquid is returned to the evaporator for further concentration, and the separated steam enters the condenser for cooling, becoming condensate which is then discharged from the system. Non-condensable gases are extracted by the vacuum pump to maintain the system vacuum. When the phosphoric acid concentration in the evaporator reaches a preset mass concentration, the concentrated liquid is discharged into the concentrated acid collection tank through the discharge port, yielding the target recycled acid.

[0042] The preset mass concentration is 50-55%. The mass concentration ratio of phosphoric acid to sulfuric acid in the target recycled acid is greater than or equal to 7:1, and the mass concentration of aluminum ions is less than 1 g / L.

[0043] The technical solution of the present invention will be further described in detail below with reference to specific embodiments. It should be understood that the methods and equipment used for the recycling and treatment of chemical polishing waste liquid in Examples 1-5 are the same as those described above; the only difference lies in the specific process parameters of each embodiment. These embodiments are only used to illustrate the present invention and do not constitute a limitation on the scope of protection of the present invention. Equivalent adjustments or optimizations made by those skilled in the art based on the core concept of the present invention should still fall within the scope of protection of the present invention.

[0044] Example 1 The equipment used in this embodiment 1 for the recovery and treatment of chemical polishing waste liquid includes: filtration equipment, extraction equipment, electrodialysis system, nanofiltration system, and evaporation system. The specific operating steps are as follows: S10. Provide 1000L of chemical polishing waste acid containing phosphoric acid, sulfuric acid, nitric acid, aluminum ions, and metal impurity ions. The concentration of phosphate ions is 58 g / L, sulfate ions are 27.87 g / L, and aluminum ions are 2.4 g / L. The chemical polishing waste liquid is pretreated as follows: The chemical polishing waste liquid is introduced into a filtration device and undergoes two stages of filtration: coarse filtration and fine filtration, to remove suspended solids and solid impurities. Coarse filtration uses a grid filter to intercept larger solid impurities. Fine filtration uses a microporous membrane to remove fine suspended solids, yielding a clear filtrate. The clarified filtrate is then added to the extraction device with the organic extractant trialkylphosphine oxide at a volume ratio V1 of 1:10, and thoroughly mixed to transfer oil and organic matter from the aqueous phase to the organic phase. After mixing, the mixture is allowed to separate into two phases: a loaded organic phase and a raffinate aqueous phase. Oil and organic matter are concentrated in the loaded organic phase. The extraction temperature T1 is controlled at approximately 25°C. The separated raffinate aqueous phase is the chemical polishing waste liquid after the removal of oil and organic matter.

[0045] Through the above filtration and extraction processes, a pretreated chemical polishing waste liquid was obtained, with a pH value less than 1 and an acidity of 1.1 mol / L.

[0046] S20. The chemical polishing waste acid is introduced into the desalination chamber of the electrodialysis system. A DC electric field with a membrane voltage U1 of 1.5 V is applied, the current density J1 is controlled at 100 mA / cm², the fluid velocity SV1 in the concentrate chamber and the desalination chamber is adjusted to 0.75 BV / h and the flow ratio Q1 is 1.0, keeping the fluid in the concentrate chamber and the desalination chamber in a turbulent state, and performing first-stage electrodialysis separation on the chemical polishing waste liquid at T2 of 35°C; so that aluminum ions, phosphate ions and metal impurity ions in the chemical polishing waste acid are enriched on the desalination side of the electrodialysis system; sulfate ions and nitrate ions preferentially permeate through the ion exchange membrane into the concentrate side, obtaining the first desalination water and the first concentrate water.

[0047] S30. The first fresh water is temporarily stored in the feed tank, and its temperature T3 is adjusted to around 25°C. The first fresh water in the feed tank is pressurized to 1.5 MPa using a high-pressure pump and then pumped into the nanofiltration membrane module for cross-flow filtration. During cross-flow filtration, the pressure gradually increases, reaching 4.1 MPa and then maintaining a constant pressure. This means that nanofiltration treatment of the first fresh water is achieved within the first preset pressure P1 range of 1.5 MPa to 4.1 MPa. When the first fresh water flows across the nanofiltration membrane surface, under pressure, phosphoric acid and sulfuric acid preferentially permeate through the membrane, forming a permeate rich in phosphoric acid and sulfuric acid. This permeate is collected in the fresh water tank via the product water outlet, and the collected product water is the second fresh water. Aluminum ions and other metal impurities in the first fresh water are retained by the nanofiltration membrane, forming a concentrate rich in aluminum salts. This concentrate is collected in the concentrate tank via the concentrate outlet, and the collected concentrate is the second concentrate.

[0048] S40. The second fresh water is fed into the feed pump and transported to the preheater for preheating. The preheated second fresh water, at T4 of 85°C, enters the evaporator and is heated and evaporated under a pressure of P2 of 0.085 MPa. The water in the second fresh water vaporizes into steam, while phosphoric acid and sulfuric acid, due to their higher boiling points, remain in the liquid phase, thus concentrating the phosphoric acid and sulfuric acid in the second fresh water. The steam generated by evaporation undergoes gas-liquid separation in a separator. The separated liquid is returned to the evaporator for further concentration, while the separated steam enters the condenser for cooling and is discharged as condensate from the system. Non-condensable gases are extracted by a vacuum pump to maintain the system vacuum. When the phosphoric acid concentration in the evaporator reaches the preset mass concentration of 50%, the concentrated liquid is discharged into the concentrated acid collection tank through the discharge port, thus obtaining the target recycled acid.

[0049] In Example 1, the recovered acid yielded 65.94 L of target reusable acid with a phosphate ion concentration of 500 g / L, a sulfate ion concentration of 38.65 g / L, and an aluminum ion concentration of 0.36 g / L.

[0050] The concentrations of phosphate, sulfate, and aluminum ions in the chemical polishing waste liquid, the first fresh water, the second fresh water, and the target recycled acid in each stage of the chemical polishing waste liquid recycling and treatment method provided in Example 1 were detected, and the corresponding removal rates were calculated. The detection methods are shown in Table 2, and the detection results are shown in Table 3.

[0051] Examples 2-5 The process flow and operation steps of the chemical polishing waste liquid recycling and treatment method provided in Examples 2-5 are the same as those in Example 1. The only difference is that the process parameter values ​​corresponding to each step are adjusted according to the values ​​shown in Table 1 below.

[0052] The concentrations of phosphate, sulfate, and aluminum ions in the chemical polishing waste liquid, the first fresh water, the second fresh water, and the target recycled acid in each stage of the chemical polishing waste liquid recycling and treatment method provided in Examples 2-5 were detected, and the corresponding removal rates were calculated. The detection methods are shown in Table 2, and the detection results are shown in Table 3.

[0053] Table 1:

[0054] Table 2:

[0055] Table 3:

[0056] As can be seen from the above, this invention utilizes a cascade separation process of electrodialysis, nanofiltration, and evaporation concentration to precisely remove impurity ions in stages, taking into account the differences in the characteristics of each component in chemical polishing waste liquid. The electrodialysis stage preferentially removes nitrate and most sulfate ions, while the nanofiltration stage selectively retains aluminum ions and metallic impurities, allowing phosphate ions and residual sulfate ions to pass through preferentially. The target recovered acid obtained after the above combined separation and evaporation concentration has a high phosphorus-to-sulfur ratio (P / S). This high P / S ratio target recycled acid can be directly used as a base raw material for chemical polishing liquid, realizing closed-loop in-situ reuse of chemical polishing waste acid, thereby reducing the cost of purchasing new acid and the cost of transporting and disposing of waste acid. Furthermore, the high P / S ratio of the target recycled acid obtained by this invention indicates high phosphoric acid purity, which can also be applied in fertilizer production, industrial cleaning, food additives, and other fields, with a wide range of market applications.

[0057] The above description is merely an embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principle of the present invention should be included within the scope of the claims of the present invention.

Claims

1. A method for recycling and treating chemical polishing waste liquid, characterized in that, Includes the following steps: S10. Provides chemical polishing waste acid containing phosphoric acid, sulfuric acid, nitric acid, aluminum ions and metal impurity ions; S20. The chemical polishing waste acid is passed into the electrodialysis system for first-stage separation. Under the action of the electric field, aluminum ions, phosphate ions and metal impurity ions in the chemical polishing waste acid are enriched in the desalination chamber of the electrodialysis system, while sulfate ions and nitrate ions preferentially pass through the ion exchange membrane into the concentrate chamber to obtain the first concentrate and the first desalination. S30. The first fresh water is passed into a nanofiltration system for second-stage separation. The nanofiltration membrane retains multivalent ions, so that aluminum ions and metal impurity ions in the first fresh water are enriched in the nanofiltration concentrate chamber. Free phosphoric acid and sulfuric acid molecules preferentially pass through the nanofiltration membrane into the nanofiltration fresh water chamber to obtain the second concentrate and the second fresh water. S40. The second freshwater is evaporated and concentrated until the phosphoric acid mass concentration reaches the preset mass concentration to obtain the target recycled acid.

2. The method for recycling and treating chemical polishing waste liquid according to claim 1, characterized in that, The process following step S10 also includes: Pretreatment of chemical polishing waste liquid removes suspended solids, oil, and organic matter, and controls the content of suspended solids, chemical oxygen demand, and free residual chlorine in the chemical polishing waste liquid within the tolerance range of the ion exchange membrane of the electrodialysis system.

3. The method for recycling and treating chemical polishing waste liquid according to claim 1, characterized in that, The mass concentrations of each component in the chemical polishing waste acid are as follows: phosphoric acid concentration is 5-16%, sulfuric acid concentration is 2.5-7%, nitric acid concentration is ≤1%, aluminum ion concentration is 2-8%, and metal impurity ion concentration is 0.2-0.5%.

4. The method for recycling and treating chemical polishing waste liquid according to claim 3, characterized in that, The acidity of the chemical polishing waste liquid is 1.1-3.1 mol / L.

5. The method for recycling and treating chemical polishing waste liquid according to claim 1, characterized in that, Step S20 specifically includes: The chemical polishing waste acid is passed into the desalination chamber of the electrodialysis system; A DC electric field is applied to the membrane to control the current density and adjust the flow ratio between the concentrate chamber and the desalination chamber to maintain the fluids in the concentrate and desalination chambers in a turbulent state. The chemical polishing waste liquid is then subjected to first-stage electrodialysis separation under a first preset temperature condition. This results in aluminum ions, phosphate ions, and metal impurity ions in the chemical polishing waste acid being enriched in the desalination chamber of the electrodialysis system. Sulfate ions and nitrate ions preferentially permeate through the ion exchange membrane into the concentrate chamber, yielding the first concentrate and the first desalination.

6. The method for recycling and treating chemical polishing waste liquid according to claim 1, characterized in that, Step S30 specifically includes: The first fresh water obtained from the first stage separation is passed into a nanofiltration system and subjected to nanofiltration treatment at a first preset pressure and a second preset temperature. By utilizing the retention effect of the nanofiltration membrane on multivalent ions, aluminum ions and metal impurity ions in the first fresh water are enriched in the nanofiltration concentrate chamber, while phosphoric acid and sulfuric acid molecules preferentially pass through the nanofiltration membrane into the nanofiltration fresh water chamber, thus obtaining the second concentrate and the second fresh water.

7. The method for recycling and treating chemical polishing waste liquid according to claim 1, characterized in that, Step S40 specifically includes: The second fresh water is passed into a preheater for preheating; The preheated second fresh water is fed into an evaporator and evaporated and concentrated under the conditions of a third preset temperature and a second preset pressure. The evaporated water vapor is then condensed and recovered. When the mass concentration of phosphoric acid in the second fresh water reaches the preset mass concentration, the second fresh water is cooled to obtain the target reusable acid.

8. The method for recycling and treating chemical polishing waste liquid according to claim 1 or 7, characterized in that, The preset mass concentration is 50-55%.

9. The method for recycling and treating chemical polishing waste liquid according to claim 8, characterized in that, The target recycled acid has a phosphoric acid to sulfuric acid mass concentration ratio greater than or equal to 7:1 and an aluminum ion mass concentration less than 1 g / L.

Citation Information

Patent Citations

  • Comprehensive resource utilization device and process for chemical waste acid

    CN120794227A