A high diester-type ester-based quaternary ammonium salt and its preparation method

By employing a preparation method involving esterification followed by hydrolysis and then esterification, the problem of low yield of diester-based quaternary ammonium salts was solved, resulting in ester-based quaternary ammonium salts with a high diester ratio, which improved their bulkiness, softness, and water dispersibility.

CN123106451APending Publication Date: 2026-11-17成都科宏达化学有限责任公司 +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611465347.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-20
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the existing technology, the yield of diester quaternary ammonium salts is difficult to exceed 45-55%, which limits the improvement of the performance of ester quaternary ammonium salts, especially in terms of fluffiness and softness.

Method used

An unconventional preparation method involving esterification, hydrolysis, and re-esterification was adopted. By controlling the ratio of mono-, di-, and tri-esters, an intermediate with a high diester ratio was prepared, which was then quaternized to obtain a high diester-type ester-based quaternary ammonium salt.

Benefits of technology

The proportion of diester was increased to 68%, which significantly improved the fluffiness and softness of the ester-based quaternary ammonium salt, reduced the content of triester, and improved water dispersibility and anti-yellowing properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123106451A_ABST
    Figure CN123106451A_ABST
Patent Text Reader

Abstract

This invention provides a method for preparing a high diester-type ester-based quaternary ammonium salt, comprising the following steps: S1. Esterification: Triethanolamine is mixed with fatty acids, a catalyst is added, and the mixture is heated under vacuum to obtain fatty acid triethanolamine ester; S2. Hydrolysis: After cooling and restoring to atmospheric pressure, water is added for hydrolysis; S3. Esterification: After hydrolysis, vacuum is continued, and after dehydration, the mixture is kept at a temperature until the acid value is ≤5mgKOH / g to obtain an intermediate. The intermediate is then cooled and subjected to a quaternization reaction to obtain the high diester-type quaternary ammonium salt. The method of this invention can obtain quaternary ammonium salts with a diester ratio as high as 68%. Due to the higher diester ratio, the bulkiness, flexibility, and other properties of the ester-based quaternary ammonium salt are significantly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of compound synthesis technology, and more specifically, to a high diester-type ester-based quaternary ammonium salt and its preparation method. Background Technology

[0002] Ester-based quaternary ammonium salts are a new type of green cationic surfactant that achieves "biodegradability" by introducing ester groups into the quaternary ammonium salt molecule. Due to their excellent fabric softening, antistatic properties, and good environmental characteristics, they have become the mainstream choice to replace traditional recalcitrant fabric softeners (such as D1821, bis(octadecyl)dimethylammonium chloride).

[0003] The synthesis of ester-based quaternary ammonium salts mainly depends on the following two types of key raw materials: ① Fatty acids: Long-chain saturated and unsaturated fatty acids of C10-C22 are usually used, such as stearic acid, palmitic acid, oleic acid, etc. ② Alkylamines: Commonly used ones include triethanolamine (TEA) and N-methyldiethanolamine (MDEA), while less common ones include N,N,N',N'-tetra(2-hydroxypropyl)ethylenediamine (EDTP), hydroxyethyl diisopropanolamine, and dihydroxyethyl isopropanolamine.

[0004] As is well known, diester-based quaternary ammonium salts exhibit the best performance among traditional ester-based quaternary ammonium salts, followed by monoester-based quaternary ammonium salts, while trimer-based quaternary ammonium salts are the worst. Therefore, current research in the production of ester-based quaternary ammonium salts mainly focuses on improving the yield of diester-based quaternary ammonium salts. This is primarily achieved by optimizing production process conditions, such as the ratio of alkanolamine to fatty acids, reaction temperature, reaction time, and catalyst type, while mitigating the negative impacts of trimer-based quaternary ammonium salts. However, even with these efforts, the yield of diester-based quaternary ammonium salts in current technologies is typically 45-55%, making further breakthroughs difficult. This significantly limits the performance improvement of ester-based quaternary ammonium salts. Summary of the Invention

[0005] The purpose of this invention is to provide a high diester-type ester-based quaternary ammonium salt and its preparation method, which can obtain an ester-based quaternary ammonium salt with a diester ratio as high as 68%. Due to the higher diester ratio, the ester-based quaternary ammonium salt has better properties such as fluffiness and flexibility.

[0006] The embodiments of the present invention are achieved through the following technical solutions: A high diester-type ester-based quaternary ammonium salt and its preparation method, comprising the following steps: S1. Esterification: Triethanolamine is mixed with fatty acids, a catalyst is added, and the mixture is heated under vacuum to produce fatty acid triethanolamine esters. S2. Hydrolysis: After cooling and restoring to normal pressure, add water for hydrolysis; S3. Esterification: After hydrolysis, vacuum is continued, and after dehydration, the temperature is maintained until the acid value is ≤5mgKOH / g to obtain an intermediate. After cooling, the intermediate is subjected to a quaternization reaction to obtain a high-diester triethanolamine type ester quaternary ammonium salt.

[0007] The present invention also provides a high diester-type ester-based quaternary ammonium salt, which is prepared by the above preparation method.

[0008] The technical solutions of the embodiments of the present invention have at least the following advantages and beneficial effects: In order to prepare high diester-based quaternary ammonium salts, this invention abandons the strategy of directly preparing the target product, high diester-based quaternary ammonium salts, in the prior art. Instead, it adopts an unconventional preparation method: first, a quaternary ammonium salt with a high degree of esterification is prepared, and then hydrolyzed to control the ratio of mono-, di-, and tri-esters. This is a reverse thinking of "do more first, then adjust back". Specifically, an intermediate with a high diester ratio is prepared by esterification, hydrolysis, and esterification, and then quaternization is performed to obtain a high diester-based ester-based quaternary ammonium salt. More specifically: First, the triester in the system is formed based on the high levels of diesters and free fatty acids present in the middle stage of the reaction. During hydrolysis with water, the triester is decomposed more than the diesters and monoesters, ultimately forming a system with high levels of monoesters and diesters and almost no triesters. In subsequent esterification, the triester has low reactivity and high steric hindrance, resulting in a higher proportion of free fatty acids decomposed from the system reacting with the monoesters to form diesters, thus obtaining a high-proportion diester intermediate. Finally, quaternization yields a high-diester type ester-based quaternary ammonium salt. Experimental verification shows that compared to the traditional preparation method where the diester ratio can only reach 45-55%, the present invention's technical solution can achieve a diester ratio as high as 68%. Due to the higher diester ratio, the bulkiness and flexibility of the ester-based quaternary ammonium salt are significantly improved. Attached Figure Description

[0009] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation on the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.

[0010] Figure 1 This is an HPLC chromatogram of the sample and detection of the quaternary ammonium salt obtained in Example 1 of the present invention; Figure 2 This is an HPLC chromatogram of the sample and detection of the quaternary ammonium salt obtained in Example 2 of the present invention; Figure 3 The image shows the HPLC chromatogram of the quaternary ammonium salt prepared in Comparative Example 1 of this invention. Figure 4 The image shows the HPLC chromatogram of the quaternary ammonium salt prepared in Comparative Example 2 of this invention. Figure 5 The image shows the HPLC chromatogram of the quaternary ammonium salt prepared in Comparative Example 3 of this invention. Figure 6 This is an HPLC chromatogram of the sample and detection of the quaternary ammonium salt prepared in Comparative Example 4 of this invention. Figure 7 This is a diagram of the residual sample from the water dispersibility experiment of this invention, wherein, Figure 7 A, Figure 7 B Figure 7 C represents the residual samples of Comparative Example 2, Comparative Example 1, and Example 1, respectively. Detailed Implementation

[0011] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below. Where specific conditions are not specified in the embodiments, conventional conditions or conditions recommended by the manufacturer shall apply. Reagents or instruments whose manufacturers are not specified are all conventional products that can be purchased commercially.

[0012] The following is a detailed description of a high diester-type ester-based quaternary ammonium salt and its preparation method provided by embodiments of the present invention.

[0013] A method for preparing a high diester-type ester-based quaternary ammonium salt includes the following steps: S1. Esterification: Triethanolamine is mixed with fatty acids, a catalyst is added, and the mixture is heated under vacuum to produce fatty acid triethanolamine esters. S2. Hydrolysis: After cooling and restoring to normal pressure, add water for hydrolysis; S3. Esterification: After hydrolysis, vacuum is continued, and after dehydration, the temperature is maintained for a second esterification reaction until the acid value is ≤5mgKOH / g, to obtain an intermediate. After cooling the intermediate, a quaternization reaction is carried out to obtain a high-diester triethanolamine type ester quaternary ammonium salt.

[0014] To prepare high diester-based quaternary ammonium salts, this invention abandons the strategy of directly preparing the target product, high diester-based quaternary ammonium salts, in the prior art. Instead, it adopts an unconventional preparation method: first, a quaternary ammonium salt with a high degree of esterification is prepared, and then hydrolyzed to control the ratio of mono-, di-, and tri-esters. This is a reverse thinking of "do more first, then adjust back." Specifically, an intermediate with a high diester ratio is prepared by first esterification, then hydrolysis, and then esterification. Subsequently, a high diester-based ester quaternary ammonium salt is obtained by quaternization. More specifically: First, the triester in the system is formed based on the high levels of diesters and free fatty acids present in the middle stage of the reaction. During hydrolysis with water, the triester is decomposed more than the diesters and monoesters, ultimately forming a system with high levels of monoesters and diesters and almost no triesters. In subsequent esterification, the triester has low reactivity and high steric hindrance, resulting in a higher proportion of free fatty acids decomposed from the system reacting with the monoesters to form diesters, thus obtaining a high-proportion diester intermediate. Finally, quaternization yields a high-diester type ester-based quaternary ammonium salt. Experimental verification shows that compared to the traditional preparation method where the diester ratio can only reach 45-55%, the present invention's technical solution can achieve a diester ratio as high as 68%. Due to the higher diester ratio, the bulkiness and flexibility of the ester-based quaternary ammonium salt are significantly improved.

[0015] In some embodiments of this application, in S1, the molar ratio of triethanolamine to fatty acid is 1:1.7-2.2. This ratio is a key ratio for the generation of high diester products. It can preferentially ensure that the two hydroxyl groups on the triethanolamine molecule undergo esterification reaction, generate diester intermediates to the maximum extent, and suppress the generation of triester byproducts, avoiding the problem of excessive monoester content, thus laying the foundation for subsequent high diester purity products.

[0016] In some embodiments of this application, in S1, the fatty acid is one or a mixture of several saturated and unsaturated fatty acids of C10-C22; specifically, industrial-grade refined fatty acids such as decanoic acid, lauric acid, myristic acid, palmitic acid, stearic acid, oleic acid, and linoleic acid can be selected, and can be used alone or in combination according to the requirements of product softness and hydrophilicity.

[0017] In some embodiments of this application, in S1, the catalyst includes one or more of phosphorous acid, hypophosphorous acid, and p-toluenesulfonic acid; the catalyst can effectively inhibit the high-temperature oxidation and carbonization of materials, reduce the activation energy of the system, and accelerate the esterification and dehydration rate; the total amount of catalyst added is 0.05-0.15%wt of the mass of triethanolamine, and the compounding ratio can be finely adjusted according to the reaction temperature.

[0018] In some embodiments of this application, in S1, the vacuum condition is -0.09 to -0.1 MPa to isolate air and prevent fatty acid oxidation and deterioration, and yellowing and blackening of the material at high temperature; then, a gradient heating method is used to raise the temperature, first to 120°C, and then to 170-180°C, and the esterification reaction is carried out under constant temperature and reduced pressure for 4-6 hours; during the esterification process, the free water generated in the reaction is continuously removed, which promotes the forward shift of the esterification equilibrium, and the reaction continues until no obvious water is released from the system and the system tends to be stable.

[0019] In some embodiments of this application, in step S2, the temperature is lowered to 160-170°C, water is added for hydrolysis for 1-2 hours, and after the temperature stabilizes, deionized water is slowly added dropwise to the system to carry out a controlled hydrolysis reaction. Most importantly, the inventors found during the experiment that the amount of water added needs to be strictly controlled. Specifically, based on the amount of triethanolamine, the molar ratio of triethanolamine to water is 1:0.1-0.35, which is the most suitable amount of water to add. The core purpose of adding a small amount of water is to selectively hydrolyze the small amount of triester byproducts generated during the initial esterification and convert them into the target diester intermediate.

[0020] In some embodiments of this application, in step S3, after the hydrolysis reaction is completed, the evacuation system is shut off, and the vacuum equipment is restarted to restore the system vacuum to -0.09 to -0.1 MPa, continuously removing free water from the system. The system is then kept at 160-170°C for 1-2 hours for a secondary deep esterification reaction. It should be noted that the acid value of the system is continuously monitored during the reaction, using the national standard acid-base titration method. The endpoint of the secondary esterification reaction is determined when the acid value is ≤5 mg KOH / g. At this point, the residual free fatty acids in the system are extremely low, and the purity of the diester intermediate reaches its optimal state.

[0021] In some embodiments of this application, in step S3, after the reaction endpoint is reached, the heating and vacuum systems are turned off, and the system temperature is lowered to 60-65°C. This temperature range is the optimal temperature for the quaternization reaction, which ensures the activity of the subsequent quaternization reagent while avoiding decomposition of the quaternization reagent and side reactions at high temperatures. After cooling, a high-purity diester triethanolamine ester intermediate is obtained.

[0022] In some embodiments of this application, during S3, when carrying out the quaternization reaction: an organic reagent is added, and the quaternization reagent is slowly added dropwise, with the total addition time strictly controlled at 1.5-2 hours. A uniform dropwise addition method is adopted to avoid side reactions caused by excessively high local reagent concentrations. After the addition is completed, the reaction is continued at a constant temperature of 60-65°C for 2-3 hours to ensure that the quaternization addition reaction is completed, and a high diester-type ester-based quaternary ammonium salt is obtained. The diester content of the product can reach 68%, with low impurity content and stable performance.

[0023] In some embodiments of this application, the organic reagent may be one of ethanol, isopropanol, propylene glycol, ethylene glycol, and dipropylene glycol; the amount added is 8%-15% of the mass of the intermediate.

[0024] In some embodiments of this application, the quaternizing agent is dimethyl sulfate, and the molar ratio of triethanolamine to the quaternizing agent is 1:0.95-1. This invention also provides a high diester-type ester-based quaternary ammonium salt, prepared by the above-described method.

[0025] Example 1 This embodiment provides a method for preparing a high diester-type ester-based quaternary ammonium salt, comprising the following steps: 149.2 kg (1 kmol) of triethanolamine and 512.7 kg (1.95 kmol, acid value 213 mg KOH / g) of a mixture of palmitic acid, stearic acid and oleic acid were added, along with 0.10 kg of phosphorous acid and 0.10 kg of hypophosphorous acid catalyst. The mixture was first heated to 120 °C for 30 min, then heated to 175 °C and reacted under vacuum of -0.095 MPa for 5 h, at which point the acid value was 2.3 mg KOH / g. The mixture was then cooled to 165 °C, nitrogen was restored to atmospheric pressure, and 3.6 kg of deionized water was added. The mixture was then sealed in a container for hydrolysis for 1.5 h. The solution was then evacuated to -0.095 MPa for dehydration and kept at 165°C for 1.5 h. At this point, the acid value was 2.9 mg KOH / g, yielding 622 kg of intermediate. The intermediate was cooled to 60°C, then 82 kg of isopropanol was added, followed by the slow dropwise addition of 123.6 kg (0.98 kmol) of dimethyl sulfate over 2 hours. After the addition was complete, the mixture was kept at 65°C for 3 hours. After the reaction was finished, the mixture was cooled to room temperature to obtain 827.6 kg of the quaternary ammonium salt. The distribution ratio was determined by sampling. Figure 1 .

[0026] Example 2 This embodiment provides a method for preparing a high diester-type ester-based quaternary ammonium salt, comprising the following steps: 149.2 kg (1 kmol) of triethanolamine, 566.2 kg (2.15 kmol, acid value 213 mg KOH / g) of a mixture of palmitic acid, stearic acid and oleic acid, 0.12 kg of phosphorous acid catalyst, and 0.10 kg of p-toluenesulfonic acid were added. The mixture was first heated to 120 °C for 30 min, then heated to 175 °C and reacted under vacuum of -0.095 MPa for 5 h, at which point the acid value was 3.8 mg KOH / g. The mixture was then cooled to 165 °C, nitrogen was restored to atmospheric pressure, and 5.85 kg of deionized water was added. The mixture was then sealed in a container for hydrolysis for 1.5 h. The solution was then vacuumed to -0.095 MPa for dehydration and kept at 165℃ for 1 hour. At this point, the acid value was 4.6 mg KOH / g, yielding 678 kg of intermediate. The intermediate was cooled to 60°C, and 89 kg of isopropanol was added. Then, 123.6 kg (0.98 kmol) of dimethyl sulfate was slowly added dropwise over 1.5 hours. After the addition was complete, the mixture was kept at 65°C for 3 hours. After the reaction was complete, the mixture was cooled to room temperature to obtain 890.6 kg of the quaternary ammonium salt. The distribution ratio was determined by sampling and analysis. Figure 2 .

[0027] Comparative Example 1 - Direct Esterification This comparative example provides a method for preparing an ester-based quaternary ammonium salt, comprising the following steps: 149.2 kg (1 kmol) of triethanolamine and 512.7 kg (1.95 kmol, acid value 213 mg KOH / g) of a mixture of palmitic acid, stearic acid and oleic acid, 0.10 kg of phosphorous acid catalyst and 0.10 kg of hypophosphorous acid catalyst were added. The mixture was heated to 175 °C and reacted under a vacuum of -0.095 MPa for 5 h until the acid value was ≤5 mg KOH / g (acid value 3.5 mg KOH / g), yielding 628 kg of intermediate. The intermediate was cooled to 60°C, and 83.5 kg of isopropanol was added. Then, 123.6 kg (0.98 kmol) of dimethyl sulfate was added dropwise over 2 hours. The mixture was then kept at 65°C for 3 hours to obtain 835.1 kg of quaternary ammonium salt. The distribution ratio was determined by sampling and analysis. Figure 3 .

[0028] Comparative Example 2 - Direct Esterification This comparative example provides a method for preparing an ester-based quaternary ammonium salt, comprising the following steps: 149.2 kg (1 kmol) of triethanolamine and 579.4 kg (2.2 kmol, acid value 213 mg KOH / g) of a mixed acid of palmitic acid, stearic acid and oleic acid, 0.12 kg of phosphorous acid catalyst, and 0.1 kg of p-toluenesulfonic acid were added. The mixture was heated to 175 °C and reacted under a vacuum of -0.095 MPa until the acid value reached 3.8 mg KOH / g, yielding 690.0 kg of intermediate. The intermediate was cooled to 60℃, and 90.4 kg of isopropanol was added. Then, 123.6 kg (0.98 kmol) of dimethyl sulfate was added dropwise over 2 hours. The mixture was then kept at 65℃ for 3 hours, yielding approximately 904.0 kg of quaternary ammonium salt. The distribution ratio was determined by sampling. Figure 4 .

[0029] Comparative Example 3 - Esterification followed by hydrolysis This comparative example provides a method for preparing an ester-based quaternary ammonium salt, comprising the following steps: 149.2 kg (1 kmol) of triethanolamine and 512.7 kg (1.95 kmol, acid value 213 mg KOH / g) of a mixture of palmitic acid, stearic acid, and oleic acid were added, along with 0.10 kg of phosphorous acid and 0.10 kg of hypophosphoric acid catalyst. The mixture was heated to 175 °C and reacted under a vacuum of -0.095 MPa until the acid value reached 3.3 mg KOH / g. The mixture was then cooled to 165 °C, and nitrogen was used to restore atmospheric pressure. 3.6 kg of deionized water was added, and the mixture was hydrolyzed in a sealed container for 1.5 h. The mixture was then dehydrated under a vacuum of -0.095 MPa until the water content was <0.5% wt (at which point the acid value was 31.3 mg KOH / g), yielding 628 kg of intermediate. The intermediate was cooled to 60°C, and 84 kg of isopropanol was added. Then, 123.6 kg (0.98 kmol) of dimethyl sulfate was added dropwise over 2 hours. The mixture was then kept at 65°C for 3 hours to obtain 840.6 kg of quaternary ammonium salt. The distribution ratio was determined by sampling and analysis. Figure 5 .

[0030] Comparative Example 4: Direct Esterification This comparative example provides a method for preparing an ester-based quaternary ammonium salt, comprising the following steps: 149.2 kg (1 kmol) of triethanolamine, 263.4 kg (1 kmol, acid value 213 mg KOH / g) of a mixed acid mixture of palmitic acid, stearic acid and oleic acid, and 0.15 kg of phosphorous acid catalyst were added. The mixture was heated to 175 °C and reacted under a vacuum of -0.095 MPa for 3 hours until the acid value was ≤5 mg KOH / g (acid value 1.2 mg KOH / g). The reaction was terminated prematurely to obtain 395.0 kg of intermediate. The intermediate was cooled to 60℃, and 57.6 kg of isopropanol was added. Then, 123.6 kg (0.98 kmol) of dimethyl sulfate was added dropwise over 2 hours. The mixture was then kept at 65℃ for 3 hours to obtain 576.2 kg of quaternary ammonium salt. The distribution ratio was determined by sampling and analysis. Figure 6 .

[0031] Experimental Example 1 Samples of the quaternary ammonium salts obtained in each embodiment and comparative example and samples from their preparation process were taken and tested. The methods for detecting the content of monoesters, diesters and triesters were the same as those in Example 1 of CN118759107A. The test results are shown in Table 1.

[0032] Table 1

[0033] Depend on Figure 1-6 As shown in Table 1: The results of Comparative Examples 1 and 2 show that when the fatty acid:triethanolamine molar ratio increased from 1.95 to 2.2, the diester content increased by only 2.4%, while the triester content increased by 14.1%. The results of Examples 1 and 2 show that when the fatty acid:triethanolamine molar ratio increased from 1.95 to 2.15, the diester content decreased by 4.9%, while the triester content increased by 7.9%. This indicates that simply adjusting the molar ratio of fatty acids to triethanolamine is insufficient to increase the diester content. In Comparative Example 3, esterification was performed first, followed by hydrolysis without further esterification. This can be understood as an intermediate state of Example 1. As can be seen from Comparative Example 3, after hydrolysis, monoesters, diesters, and trimers all decompose. Triesters decompose into diesters, replenishing the diesters. Diesters decompose into monoesters, and the final system forms a state with high monoester and diester content and almost no trimer content. In Examples 1 and 2, subsequent esterification utilizes the different reactivity of diester and trimer formation to allow more of the decomposed free fatty acids to synthesize diesters, ultimately obtaining quaternary ammonium salts with a high diester content. By comparing Comparative Example 4 with Comparative Examples 1-2, it can be seen that the molar ratio of fatty acid to triethanolamine is not in the range of 1.7-2.2:1. That is, the amount of fatty acid used is too low, which makes the esterification reaction of the two hydroxyl groups on the triethanolamine molecule incomplete. As a result, the amount of diester intermediate generated is greatly reduced, the content of monoester is too high, and finally only quaternary ammonium salt with high monoester content can be obtained.

[0034] Experiment Example 2 - Performance Evaluation By testing the application performance of the quaternary ammonium salts in Examples 1-2 and Comparative Examples 1-2 when used as fabric softeners, the main evaluation factors were bulkiness, softness, yellowing, and water dispersibility. The specific test methods are as follows: (a) Fluffiness 1. Prepare a 0.2% sample solution using 250 mg / kg hard water (preparation method see GB / T13174) for later use; prepare 15 white cotton towels of 35×35 cm, wash the towels with Vitality 28 laundry detergent according to the standard washing program of the washing machine, spin dry, spread them out and shake them flat on the clothesline, and let them air dry naturally for later use. 2. Divide the clean towels into 3 groups (5 towels in each group). Fold each towel in half twice (to form a square). Stack the towels in the same group together neatly to get 3 piles of towels. Place the same weight (about 700g) on ​​each pile of towels and press for 5 minutes. Then remove the weight and immediately measure the height H1 of the towel pile. 3. Take any set of towels and place them in a basin. Add 2 L of the sample solution to be tested, so that the towels are completely submerged in the solution. Soak for 3 minutes, then take them out, wring out the water, and let them air dry naturally.

[0035] 4. Repeat step (3) three times with the same set of towels. After drying the towels on the last occasion, measure the height of the stack of towels soaked in the sample solution according to the method in step (3). 5. Following the method in step (4), take photos to record the stack height H2 of the three sets of towels. Calculate the height difference ΔH = H2 - H1.

[0036] (ii) Compliance 1. Take one towel from each of the above-mentioned sample treatments, mark them for blind testing, and randomly group the towels; 2. Explain the scoring rules clearly to the tester and confirm that the tester understands the scoring rules before scoring. The standards are as follows: Scoring standards (0~5 points), where 0 points: very hard; 1 point: relatively hard; 2 points: somewhat hard; 3 points: soft; 4 points: relatively soft; 5 points: very soft.

[0037] (1) The test subject should wash and dry his / her hands, sit and rest for 10-15 minutes before preparing for the test; (2) Take a set of towels and place them in a clean white porcelain plate. Have the tester gently grab, rub, and knead one towel with their left and right hands at the same time to feel the softness and smoothness of the towels (each test should be completed within 30 seconds). Then exchange the towels in the left and right hands and conduct another test. Finally, ask the tester to score the softness of the towels based on their test feel. (3) Take the average of the scores of all testers as the final experimental result.

[0038] (iii) Yellowing 1. Cut JB-00 white cotton cloth into small pieces of white cotton cloth measuring 6×6 cm. Use an intelligent digital whiteness meter (model WSB-3A, manufacturer: Shanghai Xinrui) to measure the initial whiteness value F1 of each small piece of white cotton cloth.

[0039] 2. Prepare a 0.2% solution of the sample to be tested using 250 mg / kg hard water. Soak the sample in a white cotton cloth for 3 minutes, remove it, wring it out, spread it flat on a clean white porcelain plate, and dry it in a 180℃ electric heating constant temperature drying oven for 3 minutes. Remove it and let it cool naturally to room temperature.

[0040] 3. Take a new sample solution according to step (2) and repeat the experiment 5 times. The drying time for the last time is 10~15 minutes to ensure that the white cotton cloth is completely dried.

[0041] 4. Measure the whiteness value F2 of the white cotton cloth after soaking. Calculate the difference between the initial whiteness and the whiteness after soaking, ΔF = F1 - F2 (the larger the difference, the more obvious the yellowing of the white cotton cloth).

[0042] (iv) Comparison of water dispersibility 1. Place the sample to be tested in a -18 ℃ freezer for 16 h, then remove it and allow it to return to room temperature for later use; 2. At room temperature, add 2g of the sample to 200mL of deionized water, stir at 600rpm for 3min, then filter through a 350-mesh filter cloth. Take a picture to record the sample residue on the filter cloth. Figure 7 The ease with which the above samples dispersed in water was compared using a scoring method. The scoring criteria (0-5 points) for dispersion morphology are as follows: After stirring, the following scores are awarded: 0 points for completely not dispersing or dissolving; 1 point for mostly not dissolving and large residues after filtration; 2 points for partially not dissolving and some residues after filtration; 3 points for mostly dissolving and slight residues after filtration; 4 points for basically dissolving and almost no residues after filtration; and 5 points for completely dissolving and no residues after filtration.

[0043] The test results are shown in Table 2.

[0044] Table 2

[0045] The data in Table 2 shows that: In comparison Example 1 and Comparative Example 1, with the same molar ratio of fatty acids to triethanolamine, Example 1 has a higher diester ratio, resulting in significantly improved fluffiness and softness. The comparison between Example 2 and Example 1, and between Comparative Example 2 and Comparative Example 1, shows that the triester content gradually decreases, the water dispersibility of the sample gradually increases, and the yellowing gradually decreases. The reason may be that the sample with a higher triester content is not evenly dispersed in water, and the particles are too large. After multiple treatments, the sample adsorbed onto the fabric gradually forms visible spots, and changes when exposed to light or heat cause the fabric to yellow.

[0046] Figure 7 middle, Figure 7 A, B, and C are residual sample images of Comparative Example 2, Comparative Example 1, and Example 1, respectively. Figure 7 It can be seen that: in Comparative Example 2, due to the high proportion of triesters (33.3%), it was difficult to disperse after stirring, and large clumps of paste remained on the filter cloth during filtration. In Comparative Example 1, the residue on the filter cloth was significantly reduced after the triester content was reduced. In Example 1, the triester content was the lowest, resulting in the least residue on the filter cloth, and the residue was basically liquid and well dispersed.

[0047] The above are merely preferred embodiments of the present invention and are not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.

Claims

1. A method for producing a high-diester ester quaternary ammonium salt, characterized by, Includes the following steps: S1. Primary esterification: Triethanolamine is mixed with fatty acids, a catalyst is added, and the mixture is reacted under vacuum conditions and heated to obtain fatty acid triethanolamine esters. S2. Hydrolysis: After cooling and restoring to normal pressure, add water for hydrolysis; S3. Secondary esterification S31. Vacuum dehydration and secondary esterification: After hydrolysis, vacuum is continued, and after water removal, the secondary deep esterification reaction is carried out under heat until the acid value is ≤5mgKOH / g, to obtain the intermediate; S32. Cooling pretreatment: The intermediate is subjected to cooling treatment; S33. Low-temperature quaternization reaction: The intermediate after cooling pretreatment is subjected to a quaternization reaction to obtain a high-diester triethanolamine type ester quaternary ammonium salt.

2. The method for producing a high-diester esterquat according to claim 1, characterized by, In S1, the molar ratio of the triethanolamine to the fatty acid is 1:1.7-2.

2.

3. The method for preparing the high diester-type ester-based quaternary ammonium salt according to claim 1, characterized in that, In S1, the fatty acid is one or a mixture of several saturated and unsaturated fatty acids of C10-C22.

4. The method for preparing the high diester-type ester-based quaternary ammonium salt according to claim 1, characterized in that, In S1, the catalyst includes one or more of phosphorous acid, hypophosphorous acid, and p-toluenesulfonic acid.

5. The method for preparing the high diester-type ester-based quaternary ammonium salt according to claim 1, characterized in that, In S1, the vacuum condition is -0.09 to -0.1 MPa; the temperature is raised to 170-180℃.

6. The method for preparing the high diester-type ester-based quaternary ammonium salt according to claim 1, characterized in that, In S2, the temperature is lowered to 160-170℃ and water is added for hydrolysis for 1-2 hours; the amount of water added is calculated based on triethanolamine, and the molar ratio of triethanolamine to water is 1:0.1-0.

35.

7. The method for preparing the high diester-type ester-based quaternary ammonium salt according to claim 1, characterized in that, In S3, the vacuum is evacuated to -0.09~-0.1MPa for dehydration, and then kept at 160-170℃ for 1-2 hours; And / or, the intermediate is cooled to 60-65℃.

8. The method for preparing the high diester-type ester-based quaternary ammonium salt according to claim 1, characterized in that, In S3, when carrying out the quaternization reaction: add the quaternization reagent dropwise, and complete the addition within 1.5-2 hours.

9. The method for preparing the high diester-type ester-based quaternary ammonium salt according to claim 8, characterized in that, The quaternizing agent is dimethyl sulfate, and the molar ratio of triethanolamine to the quaternizing agent is 1:0.95-1.

10. A high diester-type ester-based quaternary ammonium salt, characterized in that, It is prepared by the preparation method of any one of claims 1-9.