A method for preparing famisit

By using a two-step reaction method with thionyl chloride, pyridine, and cobalt chloride catalysts, the preparation process of defamictes is simplified, solving the problems of multiple steps and low yield in the existing technology, and realizing efficient and low-cost industrial production.

CN123106567APending Publication Date: 2026-11-17SHANDONG INOMIC INST OF PHARM RES CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611373395.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-04
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing processes for preparing famicaster involve numerous steps, low yields, cumbersome operations, and high production costs, making large-scale application difficult.

Method used

Using thionyl chloride as a chlorinating agent, pyridine and/or triethylamine as an acid-binding agent, and cobalt chloride and/or nickel chloride as a catalyst, defamiclast is directly prepared through a two-step reaction, simplifying the synthetic route and improving the yield and purity.

Benefits of technology

It significantly reduces production costs, increases overall reaction yield, reduces multi-step intermediate separation and purification operations, is suitable for industrial production, has stable product quality, and meets the requirements of green chemical production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123106567A_ABST
    Figure CN123106567A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of active pharmaceutical ingredient (API) synthesis technology, specifically relating to a method for preparing defamiclast. The invention involves reacting a mixture of compound 3, an organic solvent, an acid-binding agent, and thionyl chloride to obtain intermediate I, wherein the acid-binding agent includes pyridine and / or triethylamine; then reacting intermediate I, 2-ethoxybenzonitrile, an organic solvent, and a catalyst to obtain defamiclast, wherein the catalyst includes cobalt chloride and / or nickel chloride. The defamiclast preparation method provided by this invention utilizes widely available raw materials, has a simple synthetic route, mild reaction conditions, few byproducts, high product quality, and low cost, making it suitable for industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of active pharmaceutical ingredient synthesis technology, specifically relating to a method for preparing defamiclast. Background Technology

[0002] Difamilast, chemically named N-[2-[4-(difluoromethoxy)-3-isopropoxyphenyl]oxazol-4-ylmethyl]-2-ethoxybenzamide, is a highly selective nonsteroidal phosphodiesterase 4 (PDE4) inhibitor. It exerts a potent local anti-inflammatory effect by inhibiting PDE4 activity and blocking the release of inflammatory factors. It is indicated for atopic dermatitis in adults and children, providing a new topical anti-inflammatory option for the clinical treatment of atopic dermatitis.

[0003] Currently, the relevant technologies disclose the traditional synthesis process of defamicaster, such as Figure 1 As shown. This route uses monobenzylated protocatechuic acid ethyl ester ( Figure 1 Starting from compound 1), the key intermediate 2-[4-(difluoromethoxy)-3-isopropoxyphenyl]oxazole-4-methanol was constructed through a multi-step reaction. Figure 1 Compound 3), then compound 3 reacts with methylsulfonyl chloride to form a sulfonate ester, and lithium bromide is substituted to obtain Figure 1 Compound 5 in the mixture reacts with potassium phthalimide and undergoes hydrolysis of methylamine to yield... Figure 1 Compound 7 in the mixture is then condensed with 2-ethoxybenzoic acid to give the final product, difamicter.

[0004] However, the above preparation method requires more than seven main reactions from the starting raw materials to the final product, involving multiple intermediate separation and purification steps, resulting in a low overall yield and high production costs. Furthermore, it involves multiple halogenation, condensation, and hydrolysis reactions, requiring strict control of reaction conditions and material ratios, leading to complex post-processing and a large amount of waste generation.

[0005] In summary, the existing process for preparing termethimazole has problems such as multiple steps, low yield, cumbersome operation, and difficulty in scaling up, which seriously restricts its industrial application. Summary of the Invention

[0006] The purpose of this invention is to provide a method for preparing defamiclast. The method provided by this invention has simple steps, high yield, easy operation, and is suitable for industrial production of defamiclast, which has important clinical value and industrial significance.

[0007] To achieve the above objectives, the present invention provides the following technical solution: This invention provides a method for preparing famisulant, comprising the following steps: (1) Compound 3, an organic solvent, an acid-binding agent and thionyl chloride are mixed and reacted to obtain intermediate I, wherein the acid-binding agent includes pyridine and / or triethylamine; (2) Intermediate I, 2-ethoxybenzonitrile, organic solvent and catalyst are mixed and reacted to obtain the defamisite, wherein the catalyst includes cobalt chloride and / or nickel chloride; the organic solvent includes one or more of tetrahydrofuran, toluene, dioxane and N,N-dimethylformamide; , .

[0008] Preferably, in step (1), the organic solvent is dichloromethane; the molar ratio of compound 3 to the acid-binding agent is 1:1; and the molar ratio of compound 3 to sulfoxide is 1:1.2~1.5.

[0009] Preferably, in step (1), the mixing includes: dissolving compound 3 in an organic solvent; then adding the acid-binding agent; and then cooling to 0~5°C and adding thionyl chloride dropwise.

[0010] Preferably, in step (1), the reaction temperature is 20~30℃ and the time is 6~8h.

[0011] Preferably, in step (1), after the reaction is completed, a reaction solution is obtained, and the reaction solution is further added to a sodium bicarbonate solution and stirred and separated to obtain an organic phase; the organic phase is washed and concentrated in sequence to obtain intermediate I.

[0012] Preferably, in step (2), the molar ratio of intermediate I to 2-ethoxybenzonitrile is 1:1; the molar amount of the catalyst accounts for 1 to 5% of the molar amount of intermediate I.

[0013] Preferably, in step (2), the mixing includes: dissolving intermediate I and 2-ethoxybenzonitrile in an organic solvent; and then adding the catalyst in a protective gas atmosphere.

[0014] Preferably, in step (2), the reaction temperature is 80~90℃ and the time is 12~14h; the reaction is carried out in a protective gas atmosphere.

[0015] Preferably, in step (2), after the reaction is completed, a reaction solution is obtained; the process further includes: removing the solvent from the reaction solution, purifying the obtained solid product with an ethanol-water mixed solvent to obtain the defamictes; or mixing the reaction solution with water for recrystallization to obtain the defamictes.

[0016] Preferably, the volume ratio of ethanol to water in the ethanol-water mixed solvent is 2~3:1; the recrystallization includes cooling to room temperature for crystallization, and the crystallization time is 1~2 hours.

[0017] This invention provides a method for preparing defamiclast, comprising the following steps: (1) mixing compound 3, an organic solvent, an acid-binding agent, and sulfoxide to react and obtain intermediate I, wherein the acid-binding agent includes pyridine and / or triethylamine; (2) mixing intermediate I, 2-ethoxybenzonitrile, an organic solvent, and a catalyst to react and obtain the defamiclast, wherein the catalyst includes cobalt chloride and / or nickel chloride; and the organic solvent includes one or more of tetrahydrofuran, toluene, dioxane, and N,N-dimethylformamide. The commercially available compound 3 (i.e., 2-[4-(difluoromethoxy)-3-isopropoxyphenyl]oxazole-4-methanol) is used as the starting material, and intermediate I is obtained by chlorination. Intermediate I reacts with 2-ethoxybenzonitrile under the action of a catalyst to generate the final product, defamiclast. This invention uses thionyl chloride as a chlorinating agent and pyridine and / or triethylamine as an acid-binding agent to ensure the successful preparation and high yield of intermediate I; then, cobalt chloride and / or nickel chloride are used as catalysts to prepare defamictes in high yield. Compared with the prior art, this invention has the following advantages: This invention directly uses the commercially available mature intermediate 2-[4-(difluoromethoxy)-3-isopropoxyphenyl]oxazole-4-methanol (compound 3) as the starting material, eliminating the need for independent synthesis of this key intermediate. This avoids the multi-step reaction, complex purification process, and high loss problems required for the synthesis of this intermediate in traditional processes. The raw materials can be directly purchased industrially, ensuring stable and controllable quality. This effectively shortens the overall production supply chain and significantly reduces the cost of raw material preparation and quality control.

[0018] Traditional processes require multiple complex reactions, including sulfonate formation, bromination substitution, phthalimide condensation, methylamine hydrolysis, and acylation condensation. This results in numerous reaction steps, a long production cycle, and significant intermediate losses. In contrast, this invention achieves the preparation of defamictes through only two core reactions: chlorination to prepare intermediate I and catalytic condensation to synthesize the final product. This greatly simplifies the synthetic route, reduces cumbersome operations such as intermediate separation, purification, and transfer, significantly lowers material losses during production, and effectively improves the overall reaction yield.

[0019] The present invention uses thionyl chloride as the chlorinating agent and pyridine and / or triethylamine as the acid-binding agent in the chlorination reaction. The reaction system has good compatibility and high reaction conversion rate. In the final product synthesis stage, cobalt chloride and / or nickel chloride are used as the catalytic system. The reaction conditions are mild and the parameter range is wide. There are no harsh reaction requirements such as high temperature and high pressure. The production equipment requirements are low and the process error tolerance is high. Stable scale-up production can be achieved, which completely solves the drawbacks of traditional processes such as harsh reaction conditions, poor process stability and difficulty in large-scale production.

[0020] This invention features a two-step core reaction with high selectivity and a highly specific catalytic system, effectively inhibiting the formation of byproducts such as isomers and oxidative impurities. The reaction system contains few types and low amounts of impurities. At the same time, it avoids the problems of instability, easy decomposition and deterioration, and easy introduction of unknown impurities in halogenated intermediates in traditional processes. High-purity defamiclast products can be obtained without multiple fine purifications. The product quality is stable and fully meets the pharmaceutical standards for raw materials, significantly reducing the product refining cost and quality control difficulty.

[0021] This invention features fewer reaction steps, higher material utilization, and significantly reduced emissions of waste, making it more in line with the requirements of green chemical production. At the same time, the chlorinating agent, acid-binding agent, catalyst, and reaction solvent used are all commonly used industrial reagents that are inexpensive, easy to purchase, and recyclable. Combined with simplified production processes and higher product yield, the overall production cost is significantly lower than that of existing processes.

[0022] In summary, the method for preparing defamicaster provided by this invention effectively solves the industry pain points of existing technologies, such as lengthy routes, complex operations, low yields, high costs, and difficulties in large-scale production. It has comprehensive advantages such as readily available raw materials, simplified processes, mild conditions, high product purity, low waste, and low cost. It can stably achieve large-scale industrial production and has extremely high industrialization promotion value and market application prospects. Attached Figure Description

[0023] Figure 1 A flowchart of the preparation process of defamiclast provided for existing technologies; Figure 2 The flowchart for the preparation of defamiclast provided by the present invention. Detailed Implementation

[0024] This invention provides a method for preparing famisulant, comprising the following steps: (1) Compound 3, an organic solvent, an acid-binding agent and thionyl chloride are mixed and reacted to obtain intermediate I, wherein the acid-binding agent includes pyridine and / or triethylamine; (2) Intermediate I, 2-ethoxybenzonitrile, organic solvent and catalyst are mixed and reacted to obtain the defamisite, wherein the catalyst includes cobalt chloride and / or nickel chloride; the organic solvent includes one or more of tetrahydrofuran, toluene, dioxane and N,N-dimethylformamide; , .

[0025] The preparation method provided by this invention, compared with existing traditional synthesis processes, overcomes the technical bottlenecks of lengthy process routes, cumbersome operations, high production costs, and difficulty in large-scale production. It possesses numerous advantages such as readily available raw materials, simple process, controllable reaction, high product purity, and green economy. In this invention, unless otherwise specified, all raw materials / components are commercially available products well-known to those skilled in the art.

[0026] In this invention, compound 3, an organic solvent, an acid-binding agent, and thionyl chloride are mixed and reacted to obtain intermediate I, wherein the acid-binding agent includes pyridine and / or triethylamine.

[0027] In this invention, the organic solvent can be dichloromethane. The molar ratio of compound 3 to the acid-binding agent is preferably 1:1. The molar ratio of compound 3 to sulfoxide is preferably 1:1.2~1.5. The mass ratio of compound 3 to the volume ratio of the organic solvent can be (1~2) g:10 mL, and in the examples it can be 1 g:10 mL. In this invention, the mixing preferably includes: dissolving compound 3 in the organic solvent; then adding the acid-binding agent; and then cooling to 0~5°C and adding sulfoxide dropwise. The dissolution is carried out under stirring conditions, and the stirring time is preferably 30~40 min. In this invention, the reaction is carried out by heating after the sulfoxide is added dropwise.

[0028] In this invention, the reaction temperature is preferably 20~30°C. The reaction time is preferably 6~8 hours.

[0029] In this invention, after the reaction is completed, a reaction solution is obtained. Preferably, the invention further includes adding the reaction solution to a sodium bicarbonate solution, stirring, and separating the liquid to obtain an organic phase; the organic phase is then washed and concentrated sequentially to obtain intermediate I. In this invention, the mass fraction of the sodium bicarbonate solution is preferably 3-5%. The stirring and separating time is preferably 30-40 minutes. The washing reagent can be saturated saline solution. The washing frequency is preferably 1-3 times. The concentration is preferably vacuum concentration, and the vacuum concentration temperature is preferably 25-30°C. Vacuum concentration is carried out until no fraction remains.

[0030] After obtaining intermediate I, the present invention mixes intermediate I, 2-ethoxybenzonitrile, organic solvent and catalyst to react and obtain the defamicter, wherein the catalyst includes cobalt chloride and / or nickel chloride.

[0031] In this invention, the organic solvent includes one or more of tetrahydrofuran, toluene, dioxane, and N,N-dimethylformamide (DMF), more preferably tetrahydrofuran, toluene, dioxane, or DMF. The catalyst is an anhydrous catalyst. The cobalt chloride is anhydrous cobalt chloride. The nickel chloride is anhydrous nickel chloride. The molar ratio of intermediate I to 2-ethoxybenzonitrile is preferably 1:1. The molar amount of the catalyst relative to the molar amount of intermediate I is preferably 1-5%, and in the examples, it can be 1% or 5%. This invention does not have special requirements for the amount of organic solvent used, as long as the reaction proceeds smoothly. In this invention, the mixing preferably includes: dissolving intermediate I and 2-ethoxybenzonitrile in an organic solvent; then adding the catalyst under a protective gas atmosphere. The dissolution is carried out under stirring conditions, and the stirring time is preferably 30-40 minutes. The protective gas can be nitrogen. After the dissolution is completed, this invention preferably uses a protective gas for gas replacement, and the number of gas replacements can be 1-3 times.

[0032] In this invention, the reaction temperature is preferably 80-90°C, and in the embodiments, it can be 80, 85, or 90°C. The reaction time is preferably 12-14 hours. The reaction is carried out in a protective gas atmosphere, which can be nitrogen.

[0033] In this invention, a reaction solution is obtained after the reaction is completed. When the organic solvent used in the reaction includes tetrahydrofuran, toluene, or dioxane, this invention preferably further includes: removing the solvent from the reaction solution, and purifying the obtained solid product with an ethanol-water mixed solvent to obtain the defamictes. In this invention, the volume ratio of ethanol to water in the ethanol-water mixed solvent is preferably 2-3:1. The purification preferably includes: mixing the solid product and the ethanol-water mixed solvent, heating to 70-80°C, stirring for 10-30 min, then cooling to room temperature for crystallization for 1-2 h, separating the solid and liquid to obtain a purified solid product; and drying the purified solid product to obtain the defamictes. The solid-liquid separation can be filtration, and the drying can be vacuum drying, preferably at a room temperature of 50-60°C.

[0034] Alternatively, when the organic solvent used in the reaction is DMF, the present invention preferably involves recrystallizing the reaction solution with water to obtain the defamictes. In the present invention, the recrystallization preferably includes mixing the reaction solution (80-90°C) and water (room temperature) and then cooling to room temperature for crystallization, wherein the crystallization is carried out under stirring. The crystallization time is preferably 1-2 hours.

[0035] To further illustrate the present invention, the technical solutions provided by the present invention are described in detail below with reference to embodiments, but these should not be construed as limiting the scope of protection of the present invention. The following embodiments are based on... Figure 2 The preparation process shown is used to synthesize the compound.

[0036] Example 1: Preparation of Intermediate I starting materials Figure 2 Compound 3 (150 g, 0.50 mol) was added to a 2 L three-necked flask, followed by 1.5 L of dichloromethane and stirring for 30 min. Then, pyridine (39.55 g, 0.50 mol) was added, and the mixture was cooled to 0–5 °C. Thionyl chloride (71.38 g, 0.60 mol) was added dropwise. After the addition was complete, the mixture was heated to 30 °C and reacted for 6 h. After the reaction was complete, 200 mL of 5 wt% sodium bicarbonate solution was added, and the mixture was stirred for 30 min. The mixture was then separated, and the organic phase was washed once more with saturated brine. The organic phase was concentrated under reduced pressure at 30 °C until no fraction remained, yielding 156.63 g of solid. Figure 2 Intermediate I was obtained with a yield of 98.6% and a purity of 99.2%.

[0037] 1 HNMR(CDCl3): δ7.71 (s, 1H), 7.63 (d,1H), 7.59 (s, 1H), 7.23 (d, 1H), 6.62 (t, 1H), 4.69 (m, 1H), 4.44 (s, 2H), 1.07 (d, 6H). Example 2: Preparation of Intermediate I starting materials Figure 2 Compound 3 (150 g, 0.50 mol) was added to a 2 L three-necked flask, followed by 1.5 L of dichloromethane and stirring for 30 min. Triethylamine (50.60 g, 0.50 mol) was then added, and the mixture was cooled to 0–5 °C. Thionyl chloride (89.23 g, 0.75 mol) was added dropwise. After the addition was complete, the mixture was heated to 20 °C and reacted for 8 h. After the reaction was complete, 200 mL of 5 wt% sodium bicarbonate solution was added, and the mixture was stirred for 30 min. The mixture was then separated, and the organic phase was washed once more with saturated brine. The organic phase was concentrated under reduced pressure at 30 °C until no fraction remained, yielding 158.06 g of solid. Figure 2 Intermediate I was obtained with a yield of 99.5% and a purity of 98.7%.

[0038] Example 3: Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 1 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask, and tetrahydrofuran (1.5 L) was added and stirred for 30 min, followed by nitrogen purging three times. Anhydrous cobalt chloride (0.52 g, 4 mmol) was added under nitrogen protection, and the mixture was heated to 80 °C and reacted for 12 h. After the reaction was complete, the solvent was evaporated to obtain a brown residual solid. The solid was then purified using an ethanol-water mixture (ethanol and water volume ratio of 2:1). Specifically, 762 mL of the ethanol-water mixture was added to the brown residual solid, and the mixture was heated to 78–80 °C, stirred for 30 min, and then cooled to room temperature for crystallization for 2 h. The crystals were filtered and dried under vacuum at 50 °C to constant weight, yielding 145.00 g of a white solid, namely defamiclast, with a yield of 81.2% and a purity of 99.5%.

[0039] 1 HNMR(CDCl3): δ 8.74 (s, 1H), 8.24 (d, 1H), 7.69 (s, 1H), 7.63 (d,1H), 7.23-7.59 (m, 2H), 6.95-7.08 (m, 2H), 6.62 (t, 1H), 4.69 (m, 1H), 4.36 (s, 2H), 4.19 (q, 4H), 1.32 (d, 6H). Example 4: Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 2 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask, and toluene (1.5 L) was added. The mixture was stirred for 30 min, and the mixture was purged with nitrogen three times. Anhydrous cobalt chloride (0.519 g, 4 mmol) was added under nitrogen protection, and the mixture was heated to 90 °C and reacted for 12 h. After the reaction was complete, the solvent was evaporated to obtain a brown residual solid. The solid was then purified using an ethanol-water mixture (ethanol and water volume ratio of 2:1). Specifically, 762 mL of the ethanol-water mixture was added to the brown residual solid, and the mixture was heated to 78-80 °C, stirred for 30 min, and then cooled to room temperature for crystallization for 2 h. The solid was filtered and dried under vacuum at 50 °C to constant weight, yielding 153.03 g of a white solid, namely defamiclast, with a yield of 85.7% and a purity of 99.6%.

[0040] Example 5: Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 1 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask, and toluene (1.5 L) was added. The mixture was stirred for 30 min, and the mixture was purged with nitrogen three times. Anhydrous nickel chloride (0.518 g, 4 mmol) was added under nitrogen protection, and the mixture was heated to 90 °C and reacted for 14 h. After the reaction was complete, the solvent was evaporated to dryness, yielding a brown residual solid. The solid was then purified using an ethanol-water mixture (ethanol and water volume ratio of 2:1). Specifically, 762 mL of the ethanol-water mixture was added to the brown residual solid, and the mixture was heated to 78–80 °C, stirred for 30 min, and then cooled to room temperature for crystallization for 2 h. The crystals were filtered and dried under vacuum at 50 °C to constant weight, yielding 147.14 g of a white solid, namely defamiclast, with a yield of 82.4% and a purity of 99.6%.

[0041] Example 6: Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 2 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask, and dioxane (1.5 L) was added and stirred for 30 min, followed by nitrogen purging three times. Anhydrous cobalt chloride (0.519 g, 4 mmol) was added under nitrogen protection, and the mixture was heated to 80 °C and reacted for 12 h. After the reaction was complete, the solvent was evaporated to obtain a brown residual solid. The solid was then purified using an ethanol-water mixture (ethanol and water volume ratio of 2:1). Specifically, 762 mL of the ethanol-water mixture was added to the brown residual solid, and the mixture was heated to 78-80 °C, stirred for 30 min, and then cooled to room temperature for crystallization for 2 h. The solid was filtered and dried under vacuum at 50 °C to constant weight, yielding 143.93 g of a white solid, namely defamiclast, with a yield of 80.6% and a purity of 99.7%.

[0042] Example 7: Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 1 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask, and toluene (1.5 L) was added. The mixture was stirred for 30 min, and the mixture was purged with nitrogen three times. Anhydrous cobalt chloride (2.60 g, 20 mmol) was added under nitrogen protection, and the mixture was heated to 90 °C and reacted for 14 h. After the reaction was complete, the solvent was evaporated to obtain a brown residual solid. The solid was then purified using an ethanol-water mixture (ethanol and water volume ratio of 2:1). Specifically, 762 mL of the ethanol-water mixture was added to the brown residual solid, and the mixture was heated to 78-80 °C, stirred for 30 min, and then cooled to room temperature for crystallization for 2 h. The solid was filtered and dried under vacuum at 50 °C to constant weight, yielding 155.89 g of a white solid, namely defamiclast, with a yield of 87.3% and a purity of 99.4%.

[0043] Example 8: Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 2 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask. DMF (1.5 L) was added and the mixture was stirred for 30 min, followed by nitrogen purging three times. Anhydrous nickel chloride (2.59 g, 20 mmol) was added under nitrogen protection, and the mixture was heated to 85 °C and reacted for 12 h. After the reaction was complete, water (3 L) was added, and the mixture was cooled to room temperature and stirred to induce crystallization for 1 h. The precipitated solid was filtered and dried to constant weight to obtain 148.93 g of a white solid, namely defamiclast, with a yield of 83.4% and a purity of 99.3%.

[0044] Comparative Example 1 Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 2 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask, and DMF (1.5 L) was added. The mixture was stirred for 30 min, and the mixture was purged with nitrogen three times. Anhydrous ferric chloride (3.24 g, 20 mmol) was added under nitrogen protection, and the mixture was heated to 85 °C and reacted for 12 h. After the reaction was complete, 3 L of water was added, and the mixture was cooled to room temperature to allow crystallization for 1 h. The precipitated solid was filtered and dried to constant weight to obtain 96.07 g of solid with a defamicetate purity of 62.8% and a yield of 53.8%.

[0045] Comparative Example 2 Preparation of defamiclast Intermediate I (127 g, 0.40 mol) prepared in Example 2 and 2-ethoxybenzonitrile (58.87 g, 0.40 mol) were added to a 2 L three-necked flask, and 1.5 L of ethanol was added. The mixture was stirred for 30 min, and the mixture was purged with nitrogen three times. Anhydrous nickel chloride (2.59 g, 20 mmol) was added under nitrogen protection, and the mixture was heated to 85 °C and reacted for 12 h. After the reaction was complete, the solvent was evaporated to dryness, yielding a brown residual solid. The solid was then heated to 78–80 °C with 762 mL of an ethanol-water mixture (ethanol and water volume ratio 2:1), stirred for 30 min, and cooled to room temperature for 2 h to crystallize. The crystals were filtered and dried under vacuum at 50 °C to constant weight. 92.5 g of solid was obtained, with a defamicteric purity of 18.6%.

[0046] As can be seen from the above embodiments, the present invention provides a method for preparing defamicaster, which has a wide range of raw material sources, a simple synthesis process, mild reaction conditions, few by-products, high product quality, low cost, and is suitable for industrial production.

[0047] Although the above embodiments have provided a detailed description of the present invention, they are only some embodiments of the present invention, and not all embodiments. Other embodiments can be obtained based on these embodiments without creative effort, and these embodiments all fall within the protection scope of the present invention.

Claims

1. A process for the preparation of defamiside, characterized in that, Includes the following steps: (1) Compound 3, an organic solvent, an acid-binding agent and thionyl chloride are mixed and reacted to obtain intermediate I, wherein the acid-binding agent includes pyridine and / or triethylamine; (2) Intermediate I, 2-ethoxybenzonitrile, organic solvent and catalyst are mixed and reacted to obtain the defamisite, wherein the catalyst includes cobalt chloride and / or nickel chloride; the organic solvent includes one or more of tetrahydrofuran, toluene, dioxane and N,N-dimethylformamide; , 。 2. The production method according to claim 1, characterized by, In step (1), the organic solvent is dichloromethane; the molar ratio of compound 3 to the acid binder is 1:1; and the molar ratio of compound 3 to sulfoxide is 1:1.2~1.

5.

3. The production method according to claim 1 or 2, characterized by, In step (1), the mixing includes: dissolving compound 3 in an organic solvent; then adding the acid-binding agent; and then cooling to 0~5°C and adding the dichlorosulfoxide dropwise.

4. The method of claim 1, wherein, In step (1), the reaction temperature is 20~30℃ and the time is 6~8h.

5. The production method according to claim 1 or 4, characterized by, In step (1), after the reaction is completed, a reaction solution is obtained. The reaction solution is then added to a sodium bicarbonate solution and stirred and separated to obtain an organic phase. The organic phase is then washed and concentrated to obtain intermediate I.

6. The method of claim 1, wherein, In step (2), the molar ratio of intermediate I to 2-ethoxybenzonitrile is 1:1; the molar amount of the catalyst accounts for 1 to 5% of the molar amount of intermediate I.

7. The preparation method according to claim 1 or 6, characterized in that, In step (2), the mixing includes: dissolving intermediate I and 2-ethoxybenzonitrile in an organic solvent; and then adding the catalyst in a protective gas atmosphere.

8. The method of claim 1, wherein, In step (2), the reaction temperature is 80~90℃ and the time is 12~14h; the reaction is carried out in a protective gas atmosphere.

9. The production method according to claim 1 or 8, characterized by, In step (2), after the reaction is completed, a reaction solution is obtained; the process also includes: removing the solvent from the reaction solution, purifying the obtained solid product with an ethanol-water mixed solvent to obtain the defamictes; or mixing the reaction solution with water for recrystallization to obtain the defamictes.

10. The method of claim 9, wherein, The volume ratio of ethanol to water in the ethanol-water mixed solvent is 2~3:1; the recrystallization includes cooling to room temperature for crystallization, and the crystallization time is 1~2 hours.