A highly dispersed, stable-state squid ink melanin colorant and its preparation method
By employing enzymatic hydrolysis of squid ink melanin through water suspension, microfluidic homogenization, and disc centrifugation, combined with polysaccharide and polyphenol stabilizers, a highly dispersed, stable squid ink melanin colorant was prepared. This solved the problems of easy particle sedimentation, large particle size, and short shelf life, and achieved dual liquid and powder form coverage and diverse applications.
Patent Information
- Application Number
- CN202611303996.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-17
AI Technical Summary
Existing squid ink melanin products suffer from problems such as easy particle settling, large particle size, poor color uniformity, short shelf life, and limited product form, making it difficult to meet diverse application needs.
A pretreatment process involving enzymatic hydrolysis followed by water suspension was employed, combined with nano-scale processes such as protease-confined hydrolysis, microfluidic homogenization, and disc centrifugation to construct a dual stabilization mechanism of polysaccharide steric hindrance and polyphenol electrostatic repulsion. Liquid and powder products were then prepared by encapsulation with composite wall materials.
It achieves in-situ nano-dispersion and long-term stability of melanin particles. Liquid products can be stored at room temperature for 12 months without layering or precipitation, and powder products maintain nano-level dispersion after reconstitution. It is suitable for different food processing scenarios, reduces storage and transportation costs, and extends shelf life.
Abstract
Description
Technical Field
[0001] This invention relates to the field of food processing technology, and in particular to a highly dispersed, stable squid ink melanin colorant and its preparation method. Background Technology
[0002] Cuttlefish ink is a black, sticky liquid secreted by the ink sac of cuttlefish (Cuttlefish spp.). Its core coloring substance is melanin, a natural high-molecular-weight indole pigment formed by the polymerization of tyrosine catalyzed by polyphenol oxidase. Cuttlefish ink melanin is pure in color, highly safe, and naturally derived, making it a viable alternative to artificial melanin such as activated carbon black, iron oxide black, and synthetic brilliant black. It has broad application prospects in the food industry, including baking, pastry, sauces, beverages, and ice cream.
[0003] The contents of fresh squid ink sacs are a thick paste with high solids content, typically ranging from 18% to 24%. Traditional processing requires dilution with water before use. Currently, most commercially available squid ink products are seasoning sauces, designed primarily around flavor blending. However, they suffer from three major technical shortcomings: First, poor physical stability. The melanin exists as micron-sized particles of 1-10μm, making it prone to sedimentation and aggregation during storage, resulting in the separation of the upper clear liquid and the formation of precipitates and clumps in the lower layer within a few days. Second, the large particle size leads to poor color uniformity and a rough texture. Third, the product form is limited, mostly liquid pastes, resulting in high storage and transportation costs, limited shelf life, and an inability to meet the application requirements of dry powder formulations.
[0004] Among existing publicly available technologies, Chinese Patent CN117598470A discloses a method for processing deodorized squid ink sauce, which removes the fishy smell through enzymatic hydrolysis. However, its process focuses on deodorization and flavoring, without addressing the issue of melanin particle dispersion and stability. Chinese Patent CN111938130B discloses a squid ink compound seasoning sauce and its preparation method, which improves flavor by adding edible oil and spices, but similarly does not address the nano-dispersion and long-term stability of melanin. Chinese Patent CN110604268A discloses a method for preparing and applying squid ink nanoparticles, but its process is complex and costly, and the product is positioned as a functional ingredient, unsuitable for direct use as a coloring sauce.
[0005] Therefore, developing a natural melanin coloring sauce with high dispersion stability using squid ink as raw material is of great industrial significance, as it solves the problems of easy sedimentation and aggregation of melanin particles, large particle size, and limited application scenarios in existing technologies. Summary of the Invention
[0006] The purpose of this invention is to provide a highly dispersed, stable squid ink melanin colorant and its preparation method. Addressing the shortcomings of existing technologies, this invention is adapted to the highly viscous original state of the squid ink sac contents, solving the defects of existing squid ink products such as easy sedimentation of melanin particles, large particle size, poor coloring uniformity, short shelf life, and limited product form. It achieves in-situ nano-dispersion and long-term stability of melanin, while also covering both liquid and powder product forms to meet diverse application needs.
[0007] This invention provides a method for preparing a highly dispersed, stable squid ink melanin colorant, comprising the following steps: S1. Raw material pretreatment and suspension preparation: Fresh squid ink sacs were collected, and the contents of the ink sacs were removed under light-protected conditions at 2-8℃. Purified water was added and stirred to obtain an ink suspension. The entire process was carried out in the dark to inhibit the photodegradation of melanin.
[0008] S2. Protease-restricted hydrolysis: Neutral protease is added to the ink suspension for enzymatic hydrolysis. After the enzymatic hydrolysis is completed, the enzyme is inactivated to obtain the enzymatic hydrolysate. This enzymatic hydrolysis is a restricted hydrolysis, which only cuts the connecting peptide bonds on the surface of the melanin-protein complex and removes the loose proteins on the surface without destroying the tightly bound protein layer on the surface of the melanin core particles, thus preserving the intrinsic hydrophilicity and charge properties of the particles.
[0009] S3. Coarse filtration and residue removal: The enzymatic hydrolysate is filtered through a 20-60 mesh sieve to remove large pieces of tissue and impurities from the capsule wall, resulting in coarse filtrate. This process removes insoluble impurities such as large pieces of tissue and fascia from the capsule wall, thus protecting subsequent homogenization equipment.
[0010] S4. Microfluidic homogenization and nano-sizing: The coarse filtrate is passed into a microfluidic homogenizer for homogenization, which breaks down the melanin particles to obtain nano-melanin slurry. S5. Disc centrifugation and fine classification: The nano melanin slurry is separated under a centrifugal force of 5000-10000g to remove unbroken coarse particles with a particle size greater than 1μm, and the supernatant is collected to obtain a narrow distribution nano melanin dispersion. S6. Stabilization and Formulation: A stabilizer composition is added to the nano-melanin dispersion, and a pH buffer is added to adjust the pH to obtain a formulation; the stabilizer composition includes a polysaccharide space stabilizer and a polyphenol electrostatic stabilizer; S7. Vacuum degassing: Vacuum degassing is performed on the prepared liquid to obtain a degassed liquid; this removes air bubbles trapped in the liquid, preventing oxidation and color changes during storage, and simultaneously removing some volatile fishy-smelling substances.
[0011] S8. Sterilization and filling: After the degassed liquid is sterilized at ultra-high temperature, it is aseptically filled to obtain liquid squid ink melanin coloring agent.
[0012] Preferably, in S1, the mass ratio of ink sac contents to purified water is 1:0.2 to 1:1, and the solid content of the ink suspension is 12% to 20%. This ratio can dilute the original high-viscosity ink paste to the optimal feed viscosity of the homogenizing equipment, taking into account both enzymatic hydrolysis efficiency and nano-scale effect.
[0013] Preferably, in S2, the amount of protease added is 0.05% to 0.5% of the mass of the ink suspension; The enzymatic hydrolysis conditions are pH 6.5–7.5 and temperature 40–55℃ for 15–45 min; The conditions for enzyme inactivation are to raise the temperature to 85-95℃ and hold it for 5-10 minutes after the enzymatic hydrolysis is completed; The protease is one or more combinations of neutral protease, papain, and bromelain from Bacillus subtilis, and the preferred amount of enzyme added is 0.1% to 0.3%.
[0014] Preferably, in S4, the microfluidic homogenization is performed 2 to 5 times under a pressure of 80–150 MPa, breaking down the melanin particles to D... 90 ≤500nm; preferably, pressure 100~120MPa, homogenization 3~4 times.
[0015] Preferably, S5 further includes low-temperature vacuum concentration or ultrafiltration membrane concentration of the nano-melanin dispersion. Depending on product specifications, the nano-melanin dispersion can be concentrated to the target solids content via low-temperature vacuum concentration or ultrafiltration membrane concentration, followed by stabilization and formulation.
[0016] Preferably, in S6, the amount of polysaccharide space stabilizer added is 0.1% to 0.8% of the dispersion mass; the amount of polyphenol electrostatic stabilizer added is 0.01% to 0.15% of the dispersion mass; this compound combination can form a continuous colloidal network at a low addition amount, with optimal steric hindrance effect and good salt resistance; The polysaccharide space stabilizer is one or more of sodium alginate, xanthan gum, carrageenan, and sodium carboxymethyl cellulose; the polyphenolic electrostatic stabilizer is one or more of tea polyphenols and rosmarinic acid.
[0017] Preferably, the polysaccharide space stabilizer is a complex of sodium alginate and xanthan gum, with a mass ratio of 1:1 to 3:1; the polyphenolic electrostatic stabilizer is tea polyphenol, added at 0.03% to 0.08% of the dispersion mass. Tea polyphenol can be adsorbed onto the surface of melanin particles through hydrogen bonding and hydrophobic interactions, significantly increasing the negative charge density on the particle surface and enhancing electrostatic repulsion.
[0018] Preferably, the pH buffer pair in S6 is a citric acid-sodium citrate buffer pair, with the pH adjusted to 5.5-6.5, preferably 5.8-6.2; within this pH range, melanin stability is optimal and conforms to the pH range of most food matrices.
[0019] The vacuum degassing conditions in S7 are degassing at a vacuum degree of -0.06 to -0.09 MPa for 10 to 20 minutes, preferably at a vacuum degree of ~0.08 MPa for 15 minutes; The ultra-high temperature instantaneous sterilization conditions in S8 are 130-145℃ for 3-8 seconds, preferably 137℃ for 5 seconds.
[0020] Preferably, the process further includes a powder preparation step: adding a composite wall material to the stabilized nano-melanin dispersion after S6 preparation, stirring until completely dissolved and mixed to obtain a mixed solution, and then subjecting the mixed solution to vacuum degassing and spray drying to obtain a powdered squid ink melanin colorant; the vacuum degassing conditions are -0.06 to -0.09 MPa for 10-20 min, and the spray drying process parameters are: inlet air temperature 150-165℃, outlet air temperature 70-78℃, and atomization pressure 0.3-0.5 MPa; after the obtained powdered squid ink melanin colorant is stirred and reconstituted at room temperature, the melanin particles D 90 ≤800nm; The composite wall material includes maltodextrin and gum arabic, with a total addition amount of 30% to 60% of the total solids of the nano-melanin dispersion. The preferred DE value of the maltodextrin is 10 to 15, and the preferred mass ratio of the maltodextrin to gum arabic is 2:1 to 3:1. This composite wall material has good film-forming properties and a moderate glass transition temperature, which can effectively isolate nanoparticles, avoid hard agglomeration caused by protein denaturation and cross-linking during spray drying, and ensure resolubility and dispersibility.
[0021] After the composite wall material is completely dissolved, the total solids in the mixed solution are 15% to 25%, and the liquid has good fluidity, so it can be directly introduced into the subsequent process. If the concentration is too high, purified water can be added for fine adjustment to ensure stable atomization effect.
[0022] A highly dispersed, stable squid ink melanin colorant is provided, prepared by the above-described method; the resulting liquid squid ink melanin colorant contains melanin particles D... 90 ≤500nm, absolute value of zeta potential ≥35mV, no stratification or precipitation after 12 months of storage at room temperature, color difference value ΔE<3; the melanin particles of the powdered squid ink colorant after reconstitution at room temperature by stirring are D 90 ≤800nm.
[0023] Preferably, based on different product forms and application scenarios, the products are divided into four specifications: High concentration type: Solid content 25% to 30%, in paste form, is a liquid squid ink melanin coloring agent, used for coloring baked and biscuit foods; General type: Solid content 15% to 20%, in the form of a sauce, is a liquid squid ink melanin coloring agent, used for coloring noodles and pasta products; Low viscosity type: with a solid content of 8% to 12%, it is in liquid form and is a liquid squid ink melanin coloring agent used for coloring beverages, ice cream, and confectionery.
[0024] Powder type: It is a liquid squid ink melanin colorant with a moisture content of ≤5%; The coloring properties of powdered squid ink melanin colorant are consistent with those of the liquid product after reconstitution, and it is used for long-distance storage and transportation as well as for coloring dry powder formulations of food.
[0025] Therefore, the present invention employs the above-mentioned highly dispersed stable squid ink melanin colorant and its preparation method, which has the following beneficial effects: (1) Adaptable to the characteristics of raw materials, the process is highly feasible: For the high viscosity and non-liquid state of the contents of squid ink sacs, a pretreatment process of adding water to suspend and then enzymatically hydrolyzing is adopted to ensure sufficient contact between the protease and the substrate, and the enzymatic hydrolysis efficiency and batch stability are significantly improved; at the same time, the solid content is adjusted to the optimal range of the homogenizing equipment, which solves the industrial pain point that raw materials cannot be directly put into the nano-scale equipment, and the process can be directly scaled up to industrial production.
[0026] (2) Step-by-step nano-sizing process to achieve in-situ efficient refinement: A combination of "protease-confined hydrolysis, microfluidic homogenization and disc centrifugation" is adopted. First, the loose proteins on the surface of melanin particles are gently peeled off by enzymatic hydrolysis to reduce the protein adhesion between particles. Then, the particles are refined to D size by microfluidic high-pressure physical crushing. 90 ≤500nm, and finally centrifugation is used to remove large particles, achieving a narrow particle size distribution. This process avoids the damage to melanin surface-binding proteins caused by deep enzymatic hydrolysis, and has higher refining efficiency and more uniform particle size distribution than physical homogenization alone, with significantly better coloring uniformity than traditional processes.
[0027] (3) Synergistic dual stabilization system for ultra-long-term storage stability: A dual stabilization mechanism of "polysaccharide steric hindrance and polyphenol electrostatic repulsion" is constructed. The polysaccharide colloid forms a continuous network in the system, preventing melanin particles from approaching each other through steric hindrance; polyphenols are adsorbed on the surface of melanin particles, significantly increasing the absolute value of the zeta potential (≥35mV), and inhibiting particle aggregation through strong electrostatic repulsion. The synergistic effect of the two mechanisms enables the liquid product to remain undivided and unprecipitated for 12 months at room temperature, with a color difference value ΔE<3, solving the industry pain point of traditional squid ink products being prone to sedimentation and deterioration.
[0028] (4) Liquid and powder dual forms cover the application scenarios. It can produce liquid products of various specifications and powder products at the same time to cover different application needs: liquid products can be used directly and are suitable for most food processing scenarios; powder products are encapsulated by composite wall materials, which effectively avoids the hard agglomeration problem caused by protein denaturation and cross-linking in spray drying. After reconstitution, it can retain the nano-level dispersion state and has the advantages of low storage and transportation costs, long shelf life and suitability for dry powder formulations.
[0029] (5) The process is green and safe, and has strong industrial adaptability; the whole process adopts physical processing and mild biological enzymatic hydrolysis, without the use of organic solvents and chemically synthesized additives, which meets the requirements of natural food processing; all equipment used are general industrial equipment for the food industry, without the need for special customization, and easy to implement on a large scale.
[0030] The technical solution of the present invention will be further described in detail below through embodiments. Detailed Implementation
[0031] To better understand the above technical solutions, a detailed description of the specific implementation methods will be provided below. Obviously, the described embodiments are merely some, not all, of the embodiments of the present invention. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.
[0032] The terminology used in the embodiments of this invention is for the purpose of describing particular embodiments only and is not intended to limit the invention. The singular forms “a,” “the,” and “the” as used in the embodiments of this invention and the appended claims are also intended to include the plural forms, and “multiple” generally includes at least two unless the context clearly indicates otherwise.
[0033] It should also be noted that the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that an article or device that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such an article or device. Without further limitation, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the article or device that includes said element.
[0034] Example 1 Preparation of a general-purpose squid ink melanin colorant (liquid): This embodiment prepares a general-purpose colorant with a solid content of approximately 18%, in the form of a sauce, suitable for coloring noodles, pasta, and other pasta products. The steps are as follows: (1) Preparation of raw material suspension: Fresh cuttlefish ink sacs were collected and the contents of the ink sacs were removed under low temperature and light protection at 4℃ (the actual solid content was 21.2%). Purified water was added at a mass ratio of ink sac contents: water = 1:0.3 and stirred at low speed until uniformly dispersed to obtain an ink suspension with a solid content of about 16.3%.
[0035] (2) Protease-restricted hydrolysis: Add neutral protease (enzyme activity ≥ 100,000 U / g) from Bacillus subtilis to the suspension. The amount added is 0.15% of the mass of the suspension. Adjust the pH to 7.0, control the temperature at 50℃, and hydrolyze for 25 min. After the hydrolysis is completed, raise the temperature to 90℃ and keep it at 8 min to inactivate the enzyme, and obtain the hydrolysate.
[0036] (3) Coarse filtration and slag removal: The enzymatic hydrolysate is filtered through a 40-mesh stainless steel screen to remove large pieces of tissue and fascia from the capsule wall, resulting in coarse filtrate.
[0037] (4) Microfluidic homogenization and nano-sizing: The coarse filtrate was passed into a microfluidic homogenizer and homogenized 4 times under a pressure of 120 MPa to obtain nano-melanin slurry; the melanin particles were measured by a laser particle size analyzer. 90 =320±15nm.
[0038] (5) Disc centrifugation for fine separation: The nano slurry is passed into a disc centrifuge and separated under a centrifugal force of 8000g to remove coarse particles larger than 1μm. The supernatant is collected to obtain a nano melanin dispersion.
[0039] (6) Stabilization preparation: Add 0.25% (w / w) sodium alginate and 0.10% (w / w) xanthan gum to the supernatant as a space stabilizer, and add 0.05% (w / w) tea polyphenols as an electrostatic stabilizer; add citric acid-sodium citrate buffer to adjust the pH of the system to 6.0, and stir until completely dissolved and homogeneous.
[0040] (7) Vacuum degassing: Degas the prepared solution under a vacuum of -0.08MPa for 15 minutes.
[0041] (8) Sterilization and filling: The liquid is sterilized at 137℃ for 5 seconds and then aseptically filled to obtain the finished product.
[0042] Example 2 Preparation of high-concentration squid ink melanin coloring agent (liquid): This embodiment prepares a high-concentration colorant with a solid content of approximately 28%, in paste form, suitable for baking, cookies, and other applications requiring high coloring power. The steps are as follows: (1) Preparation of raw material suspension: Same as step (1) in Example 1, using fresh cuttlefish ink sac contents (21.2% solids) and adding water to obtain an ink suspension with approximately 16.3% solids.
[0043] (2) Protease-restricted hydrolysis: Papain (enzyme activity ≥ 100,000 U / g) was added to the suspension at a rate of 0.3% of the suspension mass. The pH was adjusted to 6.5, the temperature was controlled at 45℃, and the enzyme was hydrolyzed for 30 min. The temperature was then raised to 90℃ and kept warm for 8 min to inactivate the enzyme.
[0044] (3) Coarse filtration to remove slag: Same as step (3) in Example 1.
[0045] (4) Microfluidic homogenization and nano-slurry formation: The coarse filtrate was homogenized by circulating it 5 times under a pressure of 100 MPa to obtain a nano-slurry; D was detected. 90 =410±20nm.
[0046] (5) Disc centrifugation classification and concentration: After centrifugation to collect the supernatant, the dispersion is concentrated at low temperature and vacuum at 55℃ and -0.085MPa to a solid content of about 28%.
[0047] (6) Stabilization preparation: Add 0.20% (w / w) sodium alginate and 0.30% (w / w) sodium carboxymethyl cellulose as space stabilizers to the concentrate, and add 0.08% (w / w) tea polyphenols as electrostatic stabilizers; adjust the pH to 6.0 and stir evenly.
[0048] (7) Vacuum degassing: Same as step (7) in Example 1.
[0049] (8) Sterilization and filling: Same as step (8) in Example 1.
[0050] Example 3 Preparation of low-viscosity squid ink melanin colorant (liquid): This embodiment prepares a low-viscosity colorant with a solid content of approximately 10%, which is in a liquid state and suitable for coloring beverages, ice cream, etc. The steps are as follows: (1) Preparation of raw material suspension: Fresh cuttlefish ink sacs (21.2% solids) were collected, purified water was added at a mass ratio of ink sac contents to water of 1:1, and the mixture was stirred evenly to obtain an ink suspension with approximately 10.6% solids.
[0051] (2) Protease-restricted hydrolysis: Add bromelain (enzyme activity ≥ 500,000 U / g) to the suspension at a rate of 0.1% of the suspension mass, adjust the pH to 7.0, control the temperature at 50℃, and hydrolyze for 20 min; then raise the temperature to 90℃ and incubate for 6 min to inactivate the enzyme.
[0052] (3) Coarse filtration to remove slag: Same as step (3) in Example 1.
[0053] (4) Microfluidic homogenization and nano-slurry formation: The coarse filtrate was homogenized by circulating it three times at a pressure of 140 MPa to obtain a nano-slurry; D was detected. 90 =280±12nm.
[0054] (5) Disc centrifugation for fine classification: Same as step (5) in Example 1.
[0055] (6) Stabilization preparation: Add 0.08% (w / w) xanthan gum and 0.05% (w / w) carrageenan to the supernatant as saturation stabilizers, and add 0.03% (w / w) tea polyphenols as electrostatic stabilizers; adjust the pH to 6.0 and stir evenly.
[0056] (7) Vacuum degassing: Same as step (7) in Example 1.
[0057] (8) Sterilization and filling: Same as step (8) in Example 1.
[0058] Example 4 Preparation of powdered squid ink melanin colorant: This embodiment uses the vacuum-degassed preparation solution from Example 1 as a basis to prepare a powdered colorant. The steps are as follows: (1) Wall material compounding: Take the preparation liquid from step (6) of Example 1 and add the composite wall material at 40% of the total solid mass of the system, wherein the mass ratio of maltodextrin (DE12) to gum arabic is 2:1; continue stirring for 30 minutes until the wall material is completely dissolved and the liquid is uniform.
[0059] (2) Vacuum degassing: The compounded wall material is transferred into a vacuum degassing tank and degassed for 20 minutes at a vacuum of -0.06 to remove air bubbles trapped in the liquid.
[0060] (3) Spray drying: The degassed liquid is fed into a centrifugal spray dryer, with the inlet air temperature set at 160℃, the outlet air temperature at 75℃, and the atomization pressure at 0.4MPa. After drying, the powder separated from the cyclone at the bottom of the tower is collected, mixed evenly, and the powder product is obtained.
[0061] Comparative Example 1 Unnano-processed squid ink colorant: The preparation method is basically the same as that in Example 1, except that step (4) microfluidic homogenization and nano-sizing and step (5) disc centrifugation and classification are omitted, and the mixture is directly stabilized after coarse filtration.
[0062] Comparative Example 2 Squid ink coloring without stabilizers: The preparation method is basically the same as that in Example 1, except that in step (6), no polysaccharide and polyphenol stabilizers are added, and only a buffer pair is used to adjust the pH.
[0063] Comparative Example 3 Cuttlefish ink coloring agent with added polysaccharide stabilizer only: The preparation method is basically the same as that in Example 1, except that only sodium alginate and xanthan gum are added in step (6), and tea polyphenols are not added.
[0064] Comparative Example 4 Squid ink powder spray-dried directly without wall material: The preparation method is basically the same as in Example 4, except that no maltodextrin and gum arabic composite wall material is added, and the preparation solution is directly spray-dried.
[0065] The products obtained in Examples 1-4 and Comparative Examples 1-4 were tested using the following methods: Particle size D90: Detected using a laser particle size analyzer, after the sample was diluted to approximately 0.1% solids. Zeta potential: Detected using a dynamic light scattering potentiometer, with the sample diluted to approximately 0.05% solids and measured at 25°C; Color values and color difference ΔE: A spectrophotometer was used with a D65 light source, a 10° standard field of view, and a 1cm path length cuvette. The color was measured using the transmission method under constant temperature conditions of 25℃. All samples were diluted with pure water to a solid content of 1%, degassed, and then measured. The L*, a*, and b* values were recorded. The color difference ΔE is the total color difference of the same sample before and after accelerated storage, calculated using the CIE 1976 Lab color space formula. ; Where ΔL*, Δa*, and Δb* are the differences in brightness, red-green hue, and yellow-blue hue of the sample before and after storage, respectively; Viscosity: Measured using a rotational viscometer at 25°C and 20 rpm.
[0066] The test results are as follows: Example 1 product is a uniform black paste-like fluid with color values L*=21.3±0.2, a*=0.9±0.1, b*=1.1±0.1, and a viscosity of approximately 3500±180 mPa·s at 25℃; melanin particles D... 90 =325±16nm, ζ potential=-38.5±2.1mV. After being stored at a constant temperature of 37℃ for 90 days (equivalent to 12 months of storage at room temperature of 25℃), the product showed no stratification or sedimentation, and the color difference value ΔE=1.8±0.2.
[0067] Example 2: The product is a uniform black paste with color values L*=19.1±0.2, a*=1.1±0.1, b*=0.8±0.1, and a viscosity of approximately 18000±900 mPa·s at 25°C; melanin particles D... 90 =415±21nm, ζ potential=-36.8±2.3mV. After accelerated storage at 37℃ for 90 days, the product showed no stratification or precipitation, and the color difference value ΔE=2.1±0.2.
[0068] Example 3: The product is a uniform black, free-flowing liquid with color values L*=23.8±0.2, a*=0.7±0.1, b*=1.3±0.1, and a viscosity of approximately 800±40 mPa·s at 25°C; melanin particles D 90 =285±13nm, ζ potential=-40.2±1.9mV. After 90 days of accelerated storage at 37℃, the product showed no stratification or sedimentation, and the color difference value ΔE=1.5±0.2.
[0069] Example 4: The product is a uniform black, loose powder, free of lumps, with a moisture content of 3.2% ± 0.3%. 1g of powder was added to 100mL of room temperature pure water and magnetically stirred for 5 minutes until completely reconstituted. After reconstitution, the melanin particles D... 90 =685±25nm, ζ potential=-33.2±2.0mV; no stratification or obvious precipitation after standing for 24h. After accelerated storage at 37℃ for 6 months, the powder showed no clumping or deliquescence, and the color difference value ΔE after reconstitution was 2.2±0.2.
[0070] The melanin granules D obtained in Comparative Example 1 90 =6.8±0.3μm, ζ potential=-12.3±1.5mV. Obvious stratification appeared after 3 days of storage at 37℃, with the upper clear liquid accounting for approximately 15% of the volume; after 7 days of storage, the precipitate layer accounted for 30% of the volume, failing to meet the requirements for commercial storage.
[0071] The melanin granules D obtained in Comparative Example 2 90 =330±17nm, ζ potential=-18.1±1.8mV. Trace precipitation begins to appear after 15 days of storage at 37℃, and the volume of the precipitation layer accounts for about 12% after 30 days. The color difference value ΔE=5.6±0.3. Nano-sizing alone cannot achieve long-term stability.
[0072] Product D obtained in Comparative Example 3 90 =328±16nm, ζ potential=-21.3±2.0mV. A trace amount of precipitation appeared after 60 days of storage at 37℃, and the volume of the precipitation layer accounted for about 5% after 90 days. The color difference value ΔE=3.8±0.3. A single spatial stable system cannot meet the requirements for long-term storage of 12 months.
[0073] The powder obtained in Comparative Example 4 showed severe agglomeration, and a large amount of floating powder and agglomerated particles appeared upon reconstitution; after reconstitution, the melanin particles D 90 =3.2±0.2μm, the particle size rebounded to the micron level, the nano-dispersion characteristics were basically lost, and the coloring uniformity decreased significantly.
[0074] The detection data from Examples 1-4 and Comparative Examples 1-4 above show that: The contents of squid ink sacs are a highly viscous paste with a high solids content and tightly interwoven protein-melanin complexes. Direct homogenization easily causes equipment blockage and has extremely low refining efficiency. This invention employs a pretreatment method of enzymatic hydrolysis followed by water suspension, allowing the protease to fully contact the substrate and gently peel away the loose protein layer on the surface of the melanin particles. This reduces the protein adhesion between particles while avoiding deep enzymatic hydrolysis that damages surface-bound proteins. Data shows that after enzymatic hydrolysis, homogenization, and centrifugation in Examples 1-3, the melanin particle D in the liquid product... 90 All were controlled within the range of 285–415 nm. Example 1 had 325 ± 16 nm, Example 2 had 415 ± 21 nm, and Example 3 had 285 ± 13 nm. However, Comparative Example 1 did not undergo effective pretreatment or refinement. 90 The difference is more than an order of magnitude, reaching 6.8±0.3μm (i.e. 6800nm). This shows that the pretreatment adapts the physical state of the material to the homogenization equipment, creating the necessary conditions for subsequent nano-sizing.
[0075] This invention achieves a narrow-distribution ultrafine particle size through a combined nano-process of confined hydrolysis, microfluidic homogenization, and disc centrifugal classification; Comparative Example 2, although it can reduce D 90 The particle size decreased to 330±17 nm, but the zeta potential was only -18.1±1.8 mV, indicating insufficient electrostatic repulsion. This resulted in precipitation starting after 15 days of storage at 37°C, with a precipitate layer reaching 12% after 30 days. This invention introduces confined enzymatic hydrolysis before homogenization to moderately degrade proteins on the particle surface, reducing protein-protein cross-linking during homogenization. Following this, microfluidic high-pressure crushing is performed, and finally, disc centrifugation removes large, undisturbed particles, achieving a narrow particle size distribution. Examples 1-3 show the D... 90 All particles are ≤500nm, and the particle size distribution is uniform (with a small standard deviation); Example 4: Powder product after reconstitution D 90 The particle size of the first sample was 685±25 nm, slightly larger, but still in the submicron range. In contrast, the particle size of the second sample, which did not use a composite wall material for protection, rebounded to 3.2±0.2 μm (3200 nm) after resolution, resulting in the loss of nanoscale properties. It is evident that the combined process is significantly superior to the single homogenization process in terms of refining efficiency and particle size uniformity.
[0076] The synergistic effect of polysaccharide steric hindrance and polyphenol electrostatic repulsion in this invention achieves long-term anti-settling: the zeta potentials of Examples 1-3 are -38.5±2.1mV, -36.8±2.3mV, and -40.2±1.9mV, respectively, with absolute values all ≥35mV; the zeta potential of Example 4 after reconstitution is -33.2±2.0mV, also close to 35mV. In contrast, Comparative Example 1 has only -12.3±1.5mV, Comparative Example 2 only -18.1±1.8mV, and Comparative Example 3 is -21.3±2.0mV. This invention significantly increases the surface charge density by adding polyphenolic substances adsorbed onto the particle surface, forming a strong electrostatic repulsion force, thereby inhibiting particle aggregation.
[0077] Polysaccharide colloids form a continuous network structure in the system, preventing particles from approaching each other through steric hindrance. With the synergistic effect of both, Examples 1-3, after 90 days of accelerated processing at 37°C (equivalent to 12 months at room temperature 25°C), showed no stratification or precipitation, with color differences ΔE of 1.8, 2.1, and 1.5 respectively, all <3; Example 4 powder, after 6 months of accelerated processing at 37°C, showed no agglomeration or deliquescence, and after reconstitution, ΔE = 2.2 <3. Comparative Example 3, although the particle size (D...)... 90 The nanometer diameter (328±16nm) is similar to that of the example, but the zeta potential is only -21.3mV (not reaching the strong electrostatic repulsion threshold). Relying solely on steric hindrance, 5% precipitation occurs after 90 days, with ΔE=3.8>3, which cannot meet the 12-month storage requirement. Comparative Example 2 lacks electrostatic properties, and Comparative Example 1 lacks both, resulting in even worse stability. The data show that nano-sizing alone (Comparative Example 2) or steric hindrance alone (Comparative Example 3) is insufficient to achieve long-term stability.
[0078] This invention utilizes a composite wall material encapsulation spray drying process to ensure nano-dispersion of the powder after reconstitution. For powder products, proteins are prone to thermal denaturation and cross-linking during spray drying, leading to hard agglomeration. This invention employs composite wall material encapsulation to effectively isolate particles and avoid direct contact. The powder obtained in Example 4 is loose and free of lumps, with a moisture content of only 3.2% ± 0.3%, and after reconstitution, D... 90 =685±25nm (still in the submicron range), ζ-potential=-33.2±2.0mV, no stratification or precipitation after standing for 24h, color difference ΔE=2.2. In contrast, Comparative Example 4, which did not use this wall material for encapsulation, showed severe powder agglomeration; after resolution, the particle size rebounded to 3.2±0.2μm, and the color uniformity significantly decreased. This indicates that the composite wall material not only protects the structural integrity of the nanoparticles during the drying process but also retains their surface charge characteristics, which is crucial for achieving rapid resolution and maintaining stability in powder products.
[0079] The results of Examples 1-4 and Comparative Examples 1-4 above show that the present invention can significantly improve the dispersion stability and shelf life of squid ink melanin colorant through the synergistic effect of the pretreatment process adapted to the raw materials, the nano-process, and the dual stabilization system; and through the spray drying process of composite wall material embedding, a powder product with excellent resolubility can be prepared, achieving full coverage of liquid and powder forms, with outstanding technical effects.
[0080] Therefore, this invention employs the aforementioned highly dispersed, stable-state squid ink melanin colorant and its preparation method. Targeting the highly viscous, non-liquid original state of the squid ink sac contents, a pretreatment process of adding water for suspension followed by enzymatic hydrolysis is used to ensure sufficient contact between the protease and the substrate, significantly improving enzymatic hydrolysis efficiency and batch stability. Simultaneously, the solid content is adjusted to the optimal range of the homogenizing equipment, solving the industrial pain point that the original materials cannot be directly introduced into the nano-scale equipment, and the process can be directly scaled up to industrial production.
[0081] The process employs a combination of "protease-confined hydrolysis, microfluidic homogenization, and disc centrifugation fractionation." First, the loose proteins on the surface of melanin granules are gently exfoliated through enzymatic hydrolysis, reducing protein adhesion between granules. Then, microfluidic high-pressure physical fragmentation refines the granules to a D-size. 90 ≤500nm, and finally centrifugation is used to remove large particles, achieving a narrow particle size distribution. This process avoids the damage to melanin surface-binding proteins caused by deep enzymatic hydrolysis, and has higher refining efficiency and more uniform particle size distribution than physical homogenization alone, with significantly better coloring uniformity than traditional processes.
[0082] A dual stabilization mechanism of "polysaccharide steric hindrance and polyphenol electrostatic repulsion" is constructed. Polysaccharide colloids form a continuous network within the system, preventing melanin particles from approaching each other through steric hindrance. Polyphenols adsorb onto the surface of melanin particles, significantly increasing the absolute value of the zeta potential (≥35mV), and inhibiting particle aggregation through strong electrostatic repulsion. The synergistic effect of these two mechanisms ensures that the liquid product remains undivided and sediment-free after 12 months of storage at room temperature, with a color difference ΔE < 3, thus solving the industry pain point of traditional squid ink products being prone to sedimentation and spoilage.
[0083] It can simultaneously produce liquid products in multiple specifications and powder products, covering different application needs: the liquid products can be used directly and are suitable for most food processing scenarios; the powder products, through composite wall material encapsulation, effectively avoid the hard agglomeration problem caused by protein denaturation and cross-linking during spray drying, and retain a nanoscale dispersion state after reconstitution, while also offering advantages such as low storage and transportation costs, long shelf life, and compatibility with dry powder formulations. The entire process adopts physical processing and gentle biological enzymatic hydrolysis, without the use of organic solvents and chemically synthesized additives, meeting the requirements for natural food processing; all equipment used are general industrial equipment for the food industry, requiring no special customization and facilitating large-scale production.
[0084] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and not to limit them. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can still be made to the technical solutions of the present invention, and these modifications or equivalent substitutions cannot cause the modified technical solutions to deviate from the spirit and scope of the technical solutions of the present invention.
Claims
1. A method for preparing a highly dispersed, stable squid ink melanin colorant, characterized in that, Includes the following steps: S1. Raw material pretreatment and suspension preparation: Fresh squid ink sacs were collected, and the contents of the ink sacs were removed under light-protected conditions at 2-8℃. Purified water was added and stirred to obtain an ink suspension. S2. Protease-restricted hydrolysis: Neutral protease is added to the ink suspension for enzymatic hydrolysis. After the enzymatic hydrolysis is completed, the enzyme is inactivated to obtain the hydrolysate. S3. Coarse filtration and residue removal: The enzymatic hydrolysate is filtered through a 20-60 mesh sieve to remove large pieces of tissue and impurities from the capsule wall, resulting in coarse filtrate. S4. Microfluidic homogenization and nano-sizing: The coarse filtrate is passed into a microfluidic homogenizer for homogenization, which breaks down the melanin particles to obtain nano-melanin slurry. S5. Disc centrifugation and fine classification: The nano melanin slurry is separated under a centrifugal force of 5000-10000g to remove unbroken coarse particles with a particle size greater than 1μm, and the supernatant is collected to obtain a narrow distribution nano melanin dispersion. S6. Stabilization and Formulation: A stabilizer composition is added to the nano-melanin dispersion, and a pH buffer is added to adjust the pH to obtain a formulation; the stabilizer composition includes a polysaccharide space stabilizer and a polyphenol electrostatic stabilizer; S7. Vacuum degassing: The preparation solution is degassed under vacuum to obtain a degassed solution; S8. Sterilization and filling: After the degassed liquid is sterilized at ultra-high temperature, it is aseptically filled to obtain liquid squid ink melanin coloring agent.
2. The method for preparing a highly dispersed, stable squid ink melanin colorant according to claim 1, characterized in that, In S1, the mass ratio of ink sac contents to purified water is 1:0.2 to 1:1, and the solid content of the ink suspension is 12% to 20%.
3. The method for preparing a highly dispersed, stable squid ink melanin colorant according to claim 1, characterized in that, In S2, the amount of protease added is 0.05% to 0.5% of the mass of the ink suspension; The enzymatic hydrolysis conditions are pH 6.5–7.5 and temperature 40–55℃ for 15–45 min; The conditions for enzyme inactivation are to raise the temperature to 85-95℃ and hold it for 5-10 minutes after the enzymatic hydrolysis is completed; The protease is one or a combination of neutral protease, papain, and bromelain from Bacillus subtilis.
4. The method for preparing a highly dispersed, stable squid ink melanin colorant according to claim 1, characterized in that, The microfluidizer homogenization in S4 was performed 2-5 times at a pressure of 80-150 MPa, and the melanin particles were broken to D 90 ≤ 500 nm.
5. The method for preparing a highly dispersed, stable squid ink melanin colorant according to claim 1, characterized in that, S5 also includes low-temperature vacuum concentration or ultrafiltration membrane concentration of the nano-melanin dispersion.
6. The method for preparing a highly dispersed, stable squid ink melanin colorant according to claim 1, characterized in that, In S6, the amount of polysaccharide space stabilizer added is 0.1% to 0.8% of the dispersion mass; the amount of polyphenol electrostatic stabilizer added is 0.01% to 0.15% of the dispersion mass. The polysaccharide space stabilizer is one or more of sodium alginate, xanthan gum, carrageenan, and sodium carboxymethyl cellulose; the polyphenolic electrostatic stabilizer is one or more of tea polyphenols and rosmarinic acid.
7. The method for preparing a highly dispersed, stable squid ink melanin colorant according to claim 1, characterized in that, The pH buffer pair in S6 is citric acid to sodium citrate, and the pH is adjusted to 5.5 to 6.5; The vacuum degassing conditions in S7 are -0.06 to -0.09 MPa for 10 to 20 minutes; The ultra-high temperature instantaneous sterilization conditions in S8 are 130-145℃ for 3-8 seconds.
8. The method for preparing a highly dispersed, stable squid ink melanin colorant according to claim 1, characterized in that, The process also includes a powder preparation step: adding composite wall material to the stabilized nano-melanin dispersion after S6 stabilization, stirring until completely dissolved and mixed to obtain a mixed solution, and then subjecting the mixed solution to vacuum degassing and spray drying to obtain a powdered squid ink melanin colorant; the vacuum degassing conditions are -0.06 to -0.09 MPa for 10-20 min, and the spray drying process parameters are: inlet air temperature 150-165℃, outlet air temperature 70-78℃, and atomization pressure 0.3-0.5 MPa; after the obtained powdered squid ink melanin colorant is stirred and reconstituted at room temperature, the melanin particles D 90 ≤800nm; The composite wall material includes maltodextrin and gum arabic, with the total addition amount being 30% to 60% of the total solids of the nano-melanin dispersion; the mass ratio of maltodextrin to gum arabic is 2:1 to 3:
1. After the composite wall material is completely dissolved, the total solids content of the mixed solution is 15% to 25%.
9. A highly dispersed, stable squid ink melanin colorant, characterized in that, Prepared by the preparation method according to any one of claims 1 to 8; the resulting liquid squid ink melanin colorant contains melanin particles D 90 ≤500nm, absolute value of ζ potential ≥35mV; after reconstitution of powdered squid ink melanin colorant at room temperature with stirring, the melanin particles D 90 ≤800nm.
10. The highly dispersed, stable-state squid ink melanin colorant according to claim 9, characterized in that, Powdered squid ink melanin coloring agents have a moisture content of ≤5% and are used for long-distance storage and transportation, as well as for coloring dry powder formulations in food. Liquid squid ink melanin coloring agents include the following types: High-concentration type: Solid content 25% to 30%, in paste form, used for coloring baked goods and biscuits; General type: Solid content 15% to 20%, in the form of a sauce, used for coloring noodles and pasta. Low viscosity type: Solid content 8% to 12%, in liquid form, used for coloring beverages, ice cream, and confectionery.
Citation Information
Patent Citations
Preparation method and application of cuttlefish ink nanometer particles
CN110604268A
A squid ink compound seasoning sauce and its preparation method
CN111938130B
Processing method of fishy smell-removed cuttlefish juice sauce
CN117598470A