A high-temperature sensor with a bend-resistant fiber Bragg grating array for use in confined spaces and its fabrication method.
By encasing and fixing a fiber Bragg grating array with a metal corrugated tube, combined with a bend-resistant fiber design, the problems of fiber Bragg grating array breakage and signal tunneling leakage in confined spaces are solved, achieving high mechanical reliability and signal integrity in high-temperature measurements.
Patent Information
- Application Number
- CN202611382642.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-08
- Publication Date
- 2026-11-17
AI Technical Summary
When arranging fiber Bragg grating arrays in confined spaces, optical fibers are prone to breakage, packaging and fixing are difficult, fiber Bragg gratings are difficult to fit tightly, signal tunneling leakage probability is high, resulting in unstable demodulation.
The fiber grating array is encased in a metal corrugated tube and fixed to the object under test by metal fasteners. Combined with the design of bending-resistant optical fiber and special coating, it forms a full metal mechanical protection and efficient heat conduction path, buffering external stress, reducing the risk of breakage, and improving signal integrity.
It achieves high mechanical reliability and high signal quality for high-temperature measurement in confined spaces, reduces the risk of fiber breakage, maintains signal integrity, and is suitable for high-temperature sensors in confined spaces.
Smart Images

Figure CN123111499A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to fiber optic grating high-temperature sensing technology, and more particularly to a high-temperature sensor for a bend-resistant fiber optic grating array for use in confined spaces, and a method for fabricating the high-temperature sensor based on bend-resistant optical fibers with different coatings. Background Technology
[0002] Fiber Bragg grating array high-temperature sensors are fiber optic sensing technologies that use multiple high-temperature resistant fiber Bragg gratings connected in series on a single optical fiber to achieve multi-point, quasi-distributed, and electromagnetic interference-resistant high-temperature measurements.
[0003] However, when arranging fiber Bragg grating arrays inside structures or in confined spaces (such as thin columns, narrow slots, or inside chamfered components), at least one of the following problems is often encountered: (1) Exposed optical fibers are prone to breakage, and encapsulation and fixation are difficult. Fiber gratings are difficult to fit tightly with the object under test to achieve heat conduction. (2) The essence of femtosecond laser writing is to create periodic micro-defects in the fiber. The higher the density of the fiber grating, the more serious the damage to the structural integrity of the fiber per unit length, the more its mechanical strength will decrease significantly, and the risk of bending and breaking will increase significantly. Insufficient density of the fiber grating will lead to the loss of temperature field information. (3) Limited installation space and small bending radius will increase the probability of signal tunneling leakage, thereby causing grating spectrum degradation or signal-to-noise ratio decrease, resulting in demodulation instability. Summary of the Invention
[0004] To address the shortcomings of the prior art, the present invention provides a high-temperature sensor for a bend-resistant fiber grating array used in confined spaces and a method for its fabrication, thereby solving at least one of the aforementioned problems.
[0005] The technical problem to be solved by the present invention is achieved through the following technical solution: A high-temperature sensor with a bend-resistant fiber Bragg grating array for use in confined spaces, comprising: A bend-resistant optical fiber with a fiber grating array is fabricated, wherein the fiber grating array is composed of multiple fiber gratings cascaded in sequence; A metal corrugated tube, which is sleeved outside the fiber grating array of the bending-resistant optical fiber; Multiple metal fasteners are arranged sequentially along the axial direction at different positions on the metal bellows to connect and fix the metal bellows containing the fiber grating array to the object under test along a predetermined wiring path.
[0006] Furthermore, each metal fastener includes a metal base and a metal connecting piece. The metal base is used to connect and fix to the object being measured, and the metal connecting piece is used to connect and fix the metal bellows to the metal base. When the metal bellows is connected and fixed to the metal base by the metal connecting piece through a clamping and fixing method, the metal connecting piece has a groove structure in the middle of the side facing the metal base for accommodating the metal bellows. Both ends of the metal connecting piece are connected and fixed to the metal base to press the metal bellows located in the groove structure onto the metal base.
[0007] Furthermore, the distribution density of each metal fastener at the curved surface position of the object under test is greater than its distribution density at the planar position of the object under test. Alternatively, the distribution density of each metal fastener at the location where the temperature gradient of the object under test changes significantly is greater than its distribution density at the location where the temperature gradient of the object under test changes less.
[0008] Furthermore, the inner diameter of the metal corrugated tube is larger than the outer diameter of the bending-resistant optical fiber, so that when the metal corrugated tube and the bending-resistant optical fiber are bent together, the radius of curvature of the bending-resistant optical fiber at the bend is larger than the radius of curvature of the metal corrugated tube.
[0009] Furthermore, the high-temperature sensor also includes an optical fiber patch cord and a connecting sleeve. One end of the fiber grating array extends out of the metal corrugated tube and is connected to one end of the optical fiber patch cord. The other end of the optical fiber patch cord is provided with a patch cord connector for connecting to a signal demodulation device or a spectrometer. The connecting sleeve is located at the connection between the fiber grating array and the optical fiber patch cord, and is sleeved on the metal corrugated tube and the optical fiber patch cord to connect and fix the metal corrugated tube and the optical fiber patch cord.
[0010] Furthermore, one end of the bend-resistant optical fiber extends out of the metal corrugated tube and is provided with an optical fiber connector for direct connection to a signal demodulation device or a spectrometer; one end of the metal corrugated tube is directly fixed to the optical fiber connector.
[0011] Furthermore, each fiber grating has a different center wavelength to form a wavelength division multiplexing grating array, or each fiber grating has the same center wavelength to form an identical weak reflection grating array.
[0012] A method for fabricating a high-temperature sensor with a bending-resistant fiber Bragg grating array as described above includes the following steps: Step 1: Select a bending-resistant optical fiber with a suitable coating layer according to the operating temperature of the target temperature measurement scenario. The coating layer may be an acrylate coating layer, a polyimide coating layer, or a gold plating layer, etc. Step 2: Using a femtosecond laser, multiple fiber gratings are sequentially etched along the axial direction inside the bending-resistant fiber to form the fiber grating array. Step 3: Insert the bend-resistant optical fiber with the fiber grating array into the metal corrugated tube, and connect and fix the metal corrugated tube to the object under test through multiple metal fasteners. When the coating layer is an acrylate coating layer or a polyimide coating layer, in step 2, the coating layer is retained, and the corresponding fiber grating is formed by using the femtosecond laser to etch inside the optical fiber at each grating measurement point through the coating layer. When the coating layer is a gold plating layer, in step 2, the gold plating layer at each grating measurement point is selectively chemically etched using a mixed solution of iodine and potassium iodide to expose the interior of the fiber of the anti-bending fiber. Then, the femtosecond laser is used to etch the corresponding fiber grating inside the fiber at each grating measurement point where the gold plating layer has been removed.
[0013] Furthermore, the iodine and potassium iodide mixed solution is prepared by adding 8-12g of potassium iodide and 2-3g of elemental iodine to every 100mL of water. During preparation, potassium iodide is first dissolved in water, and then elemental iodine is added and stirred to dissolve. After preparation, the solution is stored in a sealed container away from light.
[0014] Furthermore, the steps for selectively chemically etching the gold plating at each grating measurement point using a mixed solution of iodine and potassium iodide are as follows: Step S1: Mark the location of the fiber optic connector and the location of each grating measurement point on the gold plating layer to be removed; Step S2: The iodine and potassium iodide mixed solution is injected into multiple tubular containers, wherein the inner diameter of the tubular containers is larger than the outer diameter of the bending-resistant optical fiber. Step S3: Wrap each tubular container with a light-shielding material that is not corroded by the mixed solution of iodine and potassium iodide to protect it from light; Step S4: Insert the bending-resistant optical fiber into each tubular container in sequence, and place each tubular container onto the corresponding marked position. Step S5: Replace the iodine and potassium iodide mixed solution in each tubular container at preset time intervals, and observe the etching of the gold plating layer at each marked position when replacing the iodine and potassium iodide mixed solution, until the etching of the gold plating layer at each marked position is completed.
[0015] The present invention has the following beneficial effects: This invention, through the synergistic design of a metal encapsulation structure, bend-resistant fiber, and high-density grating array, addresses the challenges of high-temperature measurement in confined spaces. It provides the fiber Bragg grating array with full metal mechanical protection and an efficient heat conduction path, effectively buffering external stress and preventing fiber breakage. This fundamentally solves the inherent brittleness problem of high-density grating arrays caused by femtosecond laser writing, significantly reducing the risk of breakage during installation and use. Furthermore, utilizing the small core diameter design and ultra-low refractive index layer of the bend-resistant fiber, it maintains extremely low macro-bending loss even with a very small bending radius, ensuring signal integrity in confined spaces from an optical perspective. Depending on the multiplexing scheme, different center wavelengths can be used for each fiber Bragg grating to form a wavelength division multiplexing grating array, or the same center wavelength can be used to form an identical weak reflection grating array. Combined with reflectivity and grating length design, the array's multiplexing capability is improved and optical crosstalk is effectively suppressed under high-density grating deployment. Ultimately, this achieves high spatial resolution, high mechanical reliability, and high signal quality in high-temperature measurements within confined spaces. Attached Figure Description
[0016] Figure 1 This is a schematic diagram of the axial surface and internal structure of the high-temperature sensor provided by the present invention.
[0017] Figure 2 This is a schematic diagram of the radial internal structure of the high-temperature sensor provided by the present invention.
[0018] Figure 3 This is a schematic diagram of the internal structure of the high-temperature sensor provided by the present invention at the bend.
[0019] Figure 4 This is a schematic diagram of the fixing structure of the high-temperature sensor provided by the present invention at a bend.
[0020] Figure 5 This is a schematic diagram of the structure for fixing the high-temperature sensor on a cylinder according to the present invention.
[0021] Figure 6 This is a schematic diagram of the radial internal structure of the bending-resistant optical fiber in the high-temperature sensor provided by the present invention.
[0022] Figure 7 A flowchart illustrating the steps of the method for fabricating a high-temperature sensor provided by this invention.
[0023] Figure 8 A flowchart illustrating the steps of stripping the gold plating layer in the fabrication method of the high-temperature sensor provided by this invention. Detailed Implementation
[0024] The present invention will now be described in detail with reference to the accompanying drawings and embodiments, examples of which are shown in the drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain the present invention, and should not be construed as limiting the present invention.
[0025] In the description of this invention, it should be understood that the terms "length", "width", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.
[0026] Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first," "second," or "third" may explicitly or implicitly include one or more of that feature. In the description of this invention, "multiple" means two or more, unless otherwise explicitly specified.
[0027] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," "fixing," and "setting," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0028] Example 1
[0029] like Figure 1 , 3 As shown in Figure 4, a high-temperature sensor with a bend-resistant fiber Bragg grating array for use in confined spaces includes: A bend-resistant optical fiber 1 with a fiber grating array 10 is fabricated, wherein the fiber grating array 10 is composed of a plurality of fiber gratings 11 cascaded in sequence; Metal corrugated tube 2, which is sleeved on the fiber grating array 10 of the bending-resistant optical fiber 1; Multiple metal fasteners 3 are arranged sequentially along the axial direction at different positions on the metal bellows 2 to connect and fix the metal bellows 2 containing the fiber grating array 10 to the object under test a along a predetermined wiring path.
[0030] The high-temperature sensor of this invention uses the metal corrugated tube 2 and the metal fastener 3 to form a protective and fixing structure for the fiber Bragg grating array 10. The metal corrugated tube 2 serves as a mechanical protective layer for the fiber Bragg grating array 10, preventing it from being exposed. The metal fastener 3 connects and fixes it to the object being measured (a), enabling heat transfer between the object and the array. The metal corrugated tube 2 effectively absorbs and buffers external mechanical stress (such as vibration and impact) and isolates the fiber Bragg grating array 10 from the walls of confined spaces (such as narrow grooves or chamfered interiors), preventing damage from direct contact with sharp edges or repeated friction. Furthermore, the corrugated structure of the metal corrugated tube 2 has flexible deformation characteristics, which can disperse localized stress concentration at bending points of the fiber Bragg grating array 10 to a wider area. This fundamentally solves the inherent brittleness problem of high-density grating arrays caused by femtosecond laser writing, significantly reducing the risk of breakage during installation and use.
[0031] In this embodiment, the fiber grating array 10 is formed by femtosecond laser writing. The femtosecond laser causes a permanent change in the refractive index inside the fiber, thereby forming periodically distributed micro-defects, which are each fiber grating 11; the center-to-center distance between two adjacent fiber gratings 11 is greater than 10 μm.
[0032] Each fiber Bragg grating 11 can be uniformly distributed along the axial direction within the bending-resistant fiber 1, meaning that the center-to-center spacing between any two adjacent fiber Bragg gratings 11 is the same; alternatively, each fiber Bragg grating 11 can be non-uniformly distributed along the axial direction within the bending-resistant fiber 1, meaning that the center-to-center spacing between at least two adjacent fiber Bragg gratings 11 and the other two adjacent fiber Bragg gratings 11 is different. The specific distribution position and center-to-center spacing of each fiber Bragg grating 11 can be determined according to the actual temperature field gradient change of the object under test a. Generally, areas with larger temperature field gradient changes on the object under test a require a higher density of fiber Bragg gratings 11 to capture more details of temperature changes, while areas with smaller temperature field gradient changes can have a lower density of fiber Bragg gratings 11, as long as the reconstruction accuracy is met. It is preferable that the center-to-center spacing between each adjacent fiber Bragg grating 11 is greater than 10 μm.
[0033] The metal corrugated pipe 2 is a thin-walled metal pipe body, whose wall is composed of multiple large-diameter annular structures 21 and multiple small-diameter annular structures 22 arranged alternately and continuously along the axial direction to form a corrugated structure that alternates and undulates along the axial direction. When the metal corrugated pipe 2 is bent, the distance between two adjacent large-diameter annular structures 21 located on the inner side of the bend can be reduced, while the distance between two adjacent small-diameter annular structures 22 located on the inner side of the bend can be increased, while the distance between two adjacent small-diameter annular structures 22 located on the outer side of the bend can be reduced, so as to form a bend channel with a uniform transition.
[0034] like Figure 3 As shown, the inner diameter of the metal corrugated tube 2 is larger than the outer diameter of the bending-resistant optical fiber 1, so that when the metal corrugated tube 2 and the bending-resistant optical fiber 1 bend together, the radius of curvature R of the bending-resistant optical fiber 1 at the bend is larger than the radius of curvature r of the metal corrugated tube 2.
[0035] At the bend, the radius of curvature R of the anti-bending optical fiber 1 is relatively large, that is, the bending angle is small and gentle, which can avoid excessive tensile strain and prevent bending and breakage. The radius of curvature of the metal corrugated tube 2 is relatively small, that is, the bending angle is large and steep, which can closely adhere to the bent surface of the object being tested a, ensuring heat transfer between them. At the middle of the bend, the anti-bending optical fiber 1 contacts the inner wall of the metal corrugated tube 2 on the inner side of the bend, and at both ends of the bend, the anti-bending optical fiber 1 contacts the inner wall of the metal corrugated tube 2 on the outer side of the bend, ensuring heat transfer between them.
[0036] The gap between the metal corrugated tube 2 and the bending-resistant optical fiber 1 needs to be carefully considered. On the one hand, the gap should not be too small to prevent excessive mechanical constraint due to the difference in thermal expansion coefficients between the metal corrugated tube 2 and the bending-resistant optical fiber 1, thereby reducing the risk of the bending-resistant optical fiber 1 failing under tensile stress at high temperatures. On the other hand, the gap should not be too large to ensure that even with a small heat transfer distance, the heat on the metal corrugated tube 2 can still be transferred to the bending-resistant optical fiber 1 through air conduction, local contact heat transfer, and radiation heat transfer at higher temperatures, so that the fiber grating array 10 can respond quickly to changes in external temperature.
[0037] In actual assembly, due to the weight and flexibility of the bending-resistant optical fiber 1 and the internal structural morphology of the metal corrugated tube 2, the bending-resistant optical fiber 1 can form partial or near-contact with the inner wall of the metal corrugated tube 2, further shortening the effective heat transfer path. Therefore, the size of the gap between the metal corrugated tube 2 and the bending-resistant optical fiber 1 needs to be designed comprehensively, taking into account heat transfer efficiency, thermal response speed, and high-temperature reliability. Under the premise of meeting temperature response requirements, appropriately reserving a gap is beneficial to improving the long-term stability and service life of the sensor in high-temperature environments.
[0038] Preferably, the single-sided gap between the metal corrugated tube 2 and the fiber grating array 10 is 50-150 μm.
[0039] like Figure 2 As shown, each metal fastener 3 includes a metal base 31 and a metal connecting piece 32. The metal base 31 is used to connect and fix to the object being measured a, and the metal connecting piece 32 is used to connect and fix the metal bellows 2 to the metal base 31.
[0040] The metal bellows 2 can be connected and fixed to the metal substrate 31 by the metal connecting piece 32 through clamping, laser brazing, ultrasonic welding, laser welding or direct welding, thereby achieving heat conduction through contact with the metal substrate 31.
[0041] Preferably, when the metal bellows 2 is connected and fixed to the metal base 31 by the metal connecting piece 32 through clamping and fixing, the metal connecting piece 32 has a groove structure 33 in the middle of the side facing the metal base 31 for accommodating the metal bellows 2, and the two ends of the metal connecting piece 32 are connected and fixed to the metal base 31, so as to press the metal bellows 2 located in the groove structure 33 onto the metal base 31.
[0042] When the metal connecting piece 32 is used for clamping and fixing, the metal substrate 31 and the metal connecting piece 32 are connected and fixed relative to each other, and the metal bellows 2 is connected and fixed by clamping. At high temperature, when the metal bellows 2 expands due to heat, it can undergo slight axial sliding or radial self-adjustment within the groove structure 33, thereby releasing thermal stress. Furthermore, since there is a gap between the metal bellows 2 and the fiber grating array 10, the stress generated when the metal bellows 2 deforms will not be transmitted to the fiber grating array 10.
[0043] The metal substrate 31 and the metal connecting piece 32 are preferably made of thin sheet metal with a thickness between 0.03 and 0.07 mm, so as to have a certain degree of flexibility and bendable when fixed, so as to better fit the surface of the object being tested a and the metal bellows 2.
[0044] When the metal connecting piece 32 is used for clamping and fixing, the metal substrate 31 and the metal connecting piece 32 can be connected and fixed by means of laser brazing, ultrasonic welding, laser welding, direct welding, or thermally conductive adhesive bonding. Similarly, the metal substrate 31 and the object being tested a can be connected and fixed by means of laser brazing, ultrasonic welding, laser welding, direct welding, or thermally conductive adhesive bonding. However, considering that the thermally conductive adhesive is prone to oxidation and failure under long-term high-temperature environment, it is preferable that the metal substrate 31 and the metal connecting piece 32, as well as the metal substrate 31 and the object being tested a, are connected and fixed by welding methods such as laser brazing, ultrasonic welding, laser welding, or direct welding to achieve oxidation resistance and thus improve connection stability.
[0045] The metal bellows 2, metal substrate 31, and metal connecting piece 32 are preferably made of alloy materials such as stainless steel, titanium alloy, or aluminum alloy, which have good thermal conductivity and are easy to weld.
[0046] In one example, the various metal fasteners 3 are evenly distributed on the metal bellows 2.
[0047] For example, the length of the corrugated pipe or the number of gratings between any two metal fasteners 3 are the same.
[0048] In another example, the individual metal fasteners 3 are not uniformly distributed on the metal bellows 2.
[0049] For example, the metal fasteners 3 are divided into pairs, with each pair of metal fasteners 3 corresponding to one or more fiber gratings 11; the two metal fasteners 3 in each pair are respectively connected and fixed at both ends of the corresponding one or more fiber gratings 11 to the metal corrugated tube 2 encapsulated with the fiber grating array 10 on the object being tested a; the length of the corrugated tube or the number of gratings between the two metal fasteners 3 in different pairs may be the same or different.
[0050] In order to better fit the metal bellows 2 against the surface of the object being tested at the curved position of the object being tested a, thereby achieving higher heat transfer efficiency, preferably, the distribution density of each metal fastener 3 at the curved position of the object being tested a is greater than its distribution density at the planar position of the object being tested a.
[0051] Furthermore, since heat transfer between the metal bellows 2 and the object under test a relies on various metal fasteners 3, in order for the fiber optic grating array 10 to better reflect the temperature gradient change of the object under test a, preferably, the distribution density of each metal fastener 3 at the location where the temperature gradient change of the object under test a is large is greater than its distribution density at the location where the temperature gradient change of the object under test a is small.
[0052] Of course, the number and distribution of the metal fasteners 3 are not limited to the above example, and can also be determined according to the specific wiring path and the surface space of the object being tested a.
[0053] like Figure 1 As shown, the high-temperature sensor also includes an optical fiber patch cord 4 and a connecting sleeve 5. One end of the fiber grating array 10 extends out of the metal corrugated tube 2 and is connected (fused) to one end of the optical fiber patch cord 4. The other end of the optical fiber patch cord 4 is provided with a patch cord connector 41 for connecting to a signal demodulation device or a spectrometer. The connecting sleeve 5 is located at the connection between the fiber grating array 10 and the optical fiber patch cord 4, and is sleeved on the metal corrugated tube 2 and the optical fiber patch cord 4 to connect and fix the metal corrugated tube 2 and the optical fiber patch cord 4.
[0054] With the above structure, the fiber optic grating array 10 is connected and fixed to the fiber optic patch cord 4, and the fiber optic patch cord 4 is connected and fixed to the metal corrugated tube 2 through the connecting sleeve 5, thereby realizing the indirect fixation between the fiber optic grating array 10 and the metal corrugated tube 2, so as to avoid the overall axial displacement between the fiber optic grating array 10 and the metal corrugated tube 2.
[0055] Preferably, the connecting sleeve 5 is any one of heat shrink sleeve, metal sleeve and ceramic sleeve, or other high temperature resistant sleeve that can connect and fix the metal corrugated tube 2 to the optical fiber patch cord 4.
[0056] The heat shrink tubing is a cross-linked modified polymer functional tubing with "shape memory". When heated to a specific temperature, it can shrink radially and uniformly to tightly wrap and fix the fiber optic patch cord 4 and the metal corrugated tube 2.
[0057] The metal sleeve, ceramic sleeve, or other high-temperature resistant sleeve can be bonded and fixed to the metal corrugated tube 2 and the optical fiber patch cord 4 at both ends by interference fit, crimping, welding, high-temperature adhesive, or other high-temperature applicable connection methods.
[0058] In another example, one end of the bend-resistant optical fiber 1 extends out of the metal corrugated tube 2 and is provided with an optical fiber connector for direct connection to a signal demodulation device or a spectrometer; one end of the metal corrugated tube 2 is directly fixed to the optical fiber connector by means of crimping or adhesive.
[0059] By adopting the above structure, the intermediate connection links between the bending-resistant optical fiber 1 and the signal demodulation device or spectrometer can be reduced, connection loss and structural complexity can be reduced, and the overall integration and assembly convenience of the sensor can be improved.
[0060] The "bending resistance" of this invention has two meanings. The first meaning is physical bending resistance, that is, preventing the fiber grating array 10 from breaking when bent, which is mainly achieved by the metal corrugated tube 2. The second meaning is optical bending resistance, that is, preventing the fiber grating array 10 from signal tunneling leakage when bent, which is mainly achieved by the bending-resistant fiber 1.
[0061] The aforementioned bend-resistant optical fiber 1 is a special type of optical fiber that maintains low additional loss even with a small bending radius through a special waveguide structure design. For example... Figure 6 As shown, the bend-resistant fiber 1 includes a core 101, a cladding 103, and a coating 104. The cladding 103 surrounds the outer peripheral sidewall of the core 101, and the coating 104 surrounds the outer peripheral sidewall of the cladding 103. The fiber grating array 10 is formed by femtosecond laser writing to modulate the refractive index of the core 101 of the bend-resistant fiber 1. The core diameter of the bend-resistant fiber 1 is smaller than that of a standard single-mode fiber, which is approximately 9 μm. Therefore, the core diameter of the bend-resistant fiber 1 is less than 9 μm, approximately between 2 and 6 μm.
[0062] In this embodiment, a small-core fiber is selected as the bending-resistant fiber 1. The small-core fiber has a strong mode field confinement effect, which can significantly reduce the mode extension range in the cladding 103 to improve the effective refractive index, thereby reducing the probability of tunneling leakage from the guided mode to the radiating mode when the optical signal is bent.
[0063] The coating layer 104 is an acrylate coating layer 104, a polyimide coating layer 104, or a gold plating layer, depending on the operating temperature of the target temperature measurement scenario. The acrylate coating layer 104 is suitable for temperature measurement scenarios at 150°C and below, while the polyimide coating layer 104 is suitable for temperature measurement scenarios at 300°C and below. Both the acrylate and polyimide coating layers 104 are transparent, allowing the coating layer 104 to be retained during the fabrication of the fiber grating array. Each fiber grating is then formed by femtosecond laser etching through the coating layer 104. The coating layer 104 can also be retained when applied in the corresponding temperature range. The gold plating layer is suitable for temperature measurement scenarios above 300°C. When it is used as coating layer 104, it is opaque and will block the femtosecond laser from entering the fiber. At the same time, the gold plating layer is difficult to remove mechanically, and mechanical removal may scratch the inside of the fiber and reduce its mechanical strength. Therefore, chemical etching is required to selectively remove the gold plating layer at the grating measurement points corresponding to each fiber grating.
[0064] Preferably, an ultra-low refractive index layer 102 is further provided between the core 101 and the cladding 103 of the bending-resistant optical fiber 1. The refractive index of the ultra-low refractive index layer 102 is lower than that of the cladding 103, and the refractive index of the core 101 is higher than that of the cladding 103, so that the refractive index of the ultra-low refractive index layer 102 is much lower than that of the core 101. This ultra-low refractive index distribution can guide the mode field back into the core 101 when it diffuses outward.
[0065] In this embodiment, the relative refractive index difference between the ultra-low refractive index layer 102 and the cladding layer 103 is between -0.4% and -0.65%, and the relative refractive index difference between the fiber core 101 and the cladding layer 103 is between 0.32% and 0.5%.
[0066] To meet different multiplexing and demodulation requirements, each fiber grating 11 has a different center wavelength to form a wavelength division multiplexing grating array, or each fiber grating 11 has the same center wavelength to form an identical weak reflection grating array.
[0067] In the fiber Bragg grating array 10, optical crosstalk mainly originates from spectral overlap. If the center wavelengths of two fiber Bragg gratings 11 are too close, their reflection peaks will overlap. When the reflection spectra of the two fiber Bragg gratings 11 overlap on the wavelength axis, the signal demodulation device cannot distinguish which reflection peak comes from which fiber Bragg grating 11. When each fiber grating 11 has a different center wavelength, the reflection peaks of any two fiber gratings 11 do not overlap at all on the wavelength (horizontal axis). Even if they are physically close, their reflected signals can be clearly separated by wavelength division multiplexing technology. When each fiber grating 11 has the same center wavelength, a fully identical weak reflection grating array can be used. By reducing the reflectivity of a single fiber grating 11 and combining it with the corresponding demodulation method, high-density multiplexing measurement can be achieved.
[0068] Each fiber grating 11 has the same reflectivity and grating length.
[0069] The fiber grating 11 has a grating length that defines the axial temperature sensing range for each temperature measurement point. The shorter the grating length, the smaller the temperature sampling range corresponding to a single temperature measurement point, and the closer the measurement result is to the local one-dimensional point temperature measurement characterization. For example, when the grating length is 0.5 mm, the temperature measurement point can be considered to reflect the average temperature within a range of approximately 0.5 mm along the fiber optic axis. When the temperature change within this range is small, it can be approximated as the point measurement result at that location. Therefore, by shortening the grating length of the fiber grating 11, the effective temperature sensing range of the corresponding temperature measurement point along the fiber optic axis can be reduced, the spatial averaging effect of temperature measurement can be reduced, and the spatial resolution of the sensor and its ability to characterize local temperature distribution can be improved. This is especially suitable for temperature field measurement scenarios in confined spaces or with large temperature gradients.
[0070] However, the grating length also affects the reflection spectrum characteristics of the fiber grating 11. Generally speaking, when the grating length increases, the reflection spectrum bandwidth decreases and the reflectivity increases, which is beneficial to improving the peak resolution. On the other hand, when the grating length is too short, the reflection spectrum bandwidth increases and the reflectivity decreases, which may lead to a low signal-to-noise ratio and overlap of reflection peaks at adjacent different center wavelengths, thereby increasing the demodulation difficulty.
[0071] Therefore, the selection of grating length needs to take into account the spatial resolution requirements of the temperature field, the wavelength multiplexing interval of adjacent fiber gratings 11, and the resolution capability of the actual demodulation system, so as to achieve a balance between local temperature characterization capability and spectral resolvability.
[0072] Example 2
[0073] like Figure 7 As shown, a method for fabricating a high-temperature sensor with a bend-resistant fiber Bragg grating array as described in Example 1 includes the following steps: Step 1: Select a bending-resistant optical fiber with a suitable coating layer according to the operating temperature of the target temperature measurement scenario. The coating layer can be an acrylate coating layer, a polyimide coating layer, or a gold plating layer, etc.
[0074] In step 1, the acrylate coating is suitable for temperature measurement scenarios at 150°C and below, the polyimide coating is suitable for temperature measurement scenarios at 300°C and below, and the gold plating layer is suitable for temperature measurement scenarios above 300°C.
[0075] Step 2: Using a femtosecond laser, multiple fiber gratings are sequentially etched along the axial direction inside the bending-resistant fiber to form the fiber grating array.
[0076] When the coating layer is an acrylate coating layer or a polyimide coating layer, since the acrylate coating layer and the polyimide coating layer are transparent, when preparing the fiber grating array in step 2, the coating layer can be retained, and the corresponding fiber grating can be formed by using the femtosecond laser to etch inside the fiber at each grating measurement point position through the coating layer.
[0077] When the coating layer is an acrylate coating layer or a polyimide coating layer, since the gold plating layer is opaque, the gold plating layer at each grating measurement point needs to be locally stripped before fabricating the fiber grating array in step 2. Furthermore, the gold plating layer is difficult to remove mechanically, as mechanical stripping may scratch the interior of the optical fiber and reduce its mechanical strength. Therefore, chemical etching is preferred to selectively remove the gold plating layer at the grating measurement points corresponding to each fiber grating.
[0078] In this embodiment, when the coating layer is a gold plating layer, in step 2, the gold plating layer at each grating measurement point is selectively chemically etched using a mixed solution of iodine and potassium iodide to expose the interior of the fiber of the anti-bending fiber. Then, the femtosecond laser is used to etch the corresponding fiber grating inside the fiber at each grating measurement point where the gold plating layer has been removed.
[0079] The iodine and potassium iodide mixed solution is prepared by adding 8-12g of potassium iodide and 2-3g of elemental iodine to every 100mL of water. During preparation, potassium iodide is first dissolved in water, and then elemental iodine is added and stirred to dissolve. After preparation, the solution is stored in a sealed container away from light.
[0080] Specifically, such as Figure 8 As shown, the steps for selective chemical etching of the gold plating at each grating measurement point using a mixed solution of iodine and potassium iodide are as follows: Step S1: Mark the location of the fiber optic connector and the location of each grating measurement point on the gold plating layer to be removed.
[0081] In step S1, an oil-based marker may be used to mark the location of the optical fiber connection end and the location of each grating measurement point on the gold plating layer, marking the gold plating layer to be removed.
[0082] Step S2: The iodine and potassium iodide mixed solution is injected into multiple tubular containers, the inner diameter of which is larger than the outer diameter of the bending-resistant optical fiber.
[0083] In step S2, the tubular container is a tube open at both ends, and its inner diameter should not be too large, so as to ensure that the iodine and potassium iodide mixed solution injected into the tubular container can be retained in the tubular container under the action of its own surface tension, without leakage.
[0084] In this embodiment, the inner diameter of the tubular container is approximately 5 mm, and it is preferably made of transparent plastic or transparent glass.
[0085] Step S3: Wrap each tubular container with a light-shielding material that is not corroded by the iodine and potassium iodide mixed solution to protect it from light.
[0086] In step S3, the light-shielding material used to wrap the tubular container to block light can be, but is not limited to, tin foil, light-shielding paper, etc.
[0087] Step S4: Insert the bending-resistant optical fiber into each tubular container in sequence, and place each tubular container on the corresponding marked position.
[0088] In step S4, the iodine and potassium iodide mixed solution in each tubular container is only responsible for etching the gold plating at one marked location.
[0089] Step S5: Replace the iodine and potassium iodide mixed solution in each tubular container at preset time intervals, and observe the etching of the gold plating layer at each marked position when replacing the iodine and potassium iodide mixed solution, until the etching of the gold plating layer at each marked position is completed.
[0090] In step S5, the time interval for replacing the iodine and potassium iodide mixed solution is approximately 1.5 hours, and the number of replacements is between 4 and 5. The tubular containers are preferably transparent tubes, such as glass or plastic tubes, to allow observation of the localized etching of the gold plating layer through each tubular container during solution replacement.
[0091] Step 3: Insert the bending-resistant optical fiber containing the fiber grating array into the metal corrugated tube, and connect and fix the metal corrugated tube to the object under test through multiple metal fasteners.
[0092] Using the above method, the complete coating structure can be preserved within the temperature range corresponding to the acrylate coating or polyimide coating, reducing the stripping process and the resulting fiber damage. When the gold plating layer is used, the gold plating layer is removed only at the local locations that need to be marked by femtosecond laser, while the gold plating layer in other non-marking areas is retained, thus balancing the feasibility of femtosecond laser marking with the protective performance of different coating layers on the optical fiber.
[0093] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the embodiments of the present invention and not to limit them. Although the embodiments of the present invention have been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can still be made to the technical solutions of the embodiments of the present invention, and these modifications or equivalent substitutions cannot cause the modified technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A high-temperature sensor with a bend-resistant fiber Bragg grating array for use in confined spaces, characterized in that, include: A bend-resistant optical fiber with a fiber grating array is fabricated, wherein the fiber grating array is composed of multiple fiber gratings cascaded in sequence; A metal corrugated tube, which is sleeved outside the fiber grating array of the bending-resistant optical fiber; Multiple metal fasteners are arranged sequentially along the axial direction at different positions on the metal bellows to connect and fix the metal bellows containing the fiber grating array to the object under test along a predetermined wiring path.
2. The high-temperature sensor with an anti-bending fiber optic grating array according to claim 1, characterized in that, Each metal fastener includes a metal base and a metal connecting piece. The metal base is used to connect and fix to the object being measured, and the metal connecting piece is used to connect and fix the metal bellows to the metal base. When the metal bellows is connected and fixed to the metal base by the metal connecting piece through a clamping and fixing method, the metal connecting piece has a groove structure in the middle of the side facing the metal base for accommodating the metal bellows. Both ends of the metal connecting piece are connected and fixed to the metal base to press the metal bellows located in the groove structure onto the metal base.
3. The high-temperature sensor with an anti-bending fiber optic grating array according to claim 1 or 2, characterized in that, The distribution density of each metal fastener at the curved surface position of the object under test is greater than its distribution density at the planar position of the object under test. Alternatively, the distribution density of each metal fastener at the location where the temperature gradient of the object under test changes significantly is greater than its distribution density at the location where the temperature gradient of the object under test changes less.
4. The high-temperature sensor with an anti-bending fiber optic grating array according to claim 1, characterized in that, The inner diameter of the metal corrugated tube is larger than the outer diameter of the bending-resistant optical fiber, such that when the metal corrugated tube and the bending-resistant optical fiber are bent together, the radius of curvature of the bending-resistant optical fiber at the bend is larger than the radius of curvature of the metal corrugated tube.
5. The high-temperature sensor with an anti-bending fiber optic grating array according to claim 1, characterized in that, The high-temperature sensor also includes an optical fiber patch cord and a connecting sleeve. One end of the fiber grating array extends out of the metal corrugated tube and is connected to one end of the optical fiber patch cord. The other end of the optical fiber patch cord is provided with a patch cord connector for connecting to a signal demodulation device or a spectrometer. The connecting sleeve is located at the connection between the fiber grating array and the optical fiber patch cord, and is sleeved on the metal corrugated tube and the optical fiber patch cord to connect and fix the metal corrugated tube and the optical fiber patch cord.
6. The high-temperature sensor with an anti-bending fiber optic grating array according to claim 1, characterized in that, One end of the bend-resistant optical fiber extends out of the metal corrugated tube and is provided with an optical fiber connector for direct connection to a signal demodulation device or a spectrometer; one end of the metal corrugated tube is directly fixed to the optical fiber connector.
7. The high-temperature sensor with an anti-bending fiber optic grating array according to claim 1, characterized in that, Each fiber grating has a different center wavelength to form a wavelength division multiplexing grating array, or each fiber grating has the same center wavelength to form an identical weak reflection grating array.
8. A method for fabricating a high-temperature sensor with a bend-resistant fiber grating array as described in claim 1, characterized in that, Includes the following steps: Step 1: Select a bending-resistant optical fiber with a suitable coating layer according to the operating temperature of the target temperature measurement scenario. The coating layer may be an acrylate coating layer, a polyimide coating layer, or a gold plating layer, etc. Step 2: Using a femtosecond laser, multiple fiber gratings are sequentially etched along the axial direction inside the bending-resistant fiber to form the fiber grating array. Step 3: Insert the bend-resistant optical fiber with the fiber grating array into the metal corrugated tube, and connect and fix the metal corrugated tube to the object under test through multiple metal fasteners. When the coating layer is an acrylate coating layer or a polyimide coating layer, in step 2, the coating layer is retained, and the corresponding fiber grating is formed by using the femtosecond laser to etch inside the optical fiber at each grating measurement point through the coating layer. When the coating layer is a gold plating layer, in step 2, the gold plating layer at each grating measurement point is selectively chemically etched using a mixed solution of iodine and potassium iodide to expose the interior of the fiber of the anti-bending fiber. Then, the femtosecond laser is used to etch the corresponding fiber grating inside the fiber at each grating measurement point where the gold plating layer has been removed.
9. The preparation method according to claim 11, characterized in that, The iodine and potassium iodide mixed solution is prepared by adding 8-12g of potassium iodide and 2-3g of elemental iodine to every 100mL of water. During preparation, potassium iodide is first dissolved in water, and then elemental iodine is added and stirred to dissolve. After preparation, the solution is stored in a sealed container away from light.
10. The preparation method according to claim 11 or 13, characterized in that, The steps for selectively chemically etching the gold plating at each grating measurement point using a mixed solution of iodine and potassium iodide are as follows: Step S1: Mark the location of the fiber optic connector and the location of each grating measurement point on the gold plating layer to be removed; Step S2: The iodine and potassium iodide mixed solution is injected into multiple tubular containers, wherein the inner diameter of the tubular containers is larger than the outer diameter of the bending-resistant optical fiber. Step S3: Wrap each tubular container with a light-shielding material that is not corroded by the mixed solution of iodine and potassium iodide to protect it from light; Step S4: Insert the bending-resistant optical fiber into each tubular container in sequence, and place each tubular container onto the corresponding marked position. Step S5: Replace the iodine and potassium iodide mixed solution in each tubular container at preset time intervals, and observe the etching of the gold plating layer at each marked position when replacing the iodine and potassium iodide mixed solution, until the etching of the gold plating layer at each marked position is completed.