Waveform layout segmented bonded fiber optic sensor for resin flow monitoring and its applications

By arranging waveform segmented adhesive fiber optic sensors inside composite material components, the problem of not being able to monitor resin flow in real time in existing technologies has been solved, enabling long-term, real-time, and continuous monitoring of resin flow, and improving monitoring accuracy and sensitivity.

CN123111884APending Publication Date: 2026-11-17GUANGZHOU UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610502152.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-04-16
Publication Date
2026-11-17

Smart Images

  • Figure CN123111884A_ABST
    Figure CN123111884A_ABST
Patent Text Reader

Abstract

This application provides a waveform-layout segmented bonded fiber optic sensor for resin flow monitoring and its application, belonging to the field of fiber optic sensing technology. This fiber optic sensor, by placing its sensing fiber in the monitored area on the surface of the composite material, enables direct and real-time sensing of the resin flow front when resin flows in the monitored area. This allows for more accurate and real-time perception of the resin flow front within the composite component. Furthermore, the sensing fiber in this fiber optic sensor extends along a preset periodic waveform path. This design significantly increases the contact area and effective area between the fiber and the resin, amplifies the signal changes caused by resin flow, and improves the signal-to-noise ratio and monitoring sensitivity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of fiber optic sensing technology, and in particular to a waveform-layout segmented bonding fiber optic sensor for resin flow monitoring and its application. Background Technology

[0002] Pultruded beams for wind turbine blades are fabricated by vacuum infusion of stacked pultruded plates, achieving the goal of structural lightweighting. This technology offers advantages such as faster, lighter, and higher-quality production, and is widely used in the manufacture of large pultruded beams.

[0003] However, in the fabrication of pultruded beams using Va-RTM (vacuum-assisted resin transfer molding), the pultruded plates are stacked and spliced, then integrally cast with the shell. The splice seams form a closed, narrow cavity and serve as one of the main flow channels. However, due to longitudinal (chordal) deviations in the splice seams, the positions of the seams become staggered and uneven in size, increasing the complexity of resin flow. This can lead to initial internal manufacturing defects such as resin voids during the casting process, affecting the overall strength of the main beam. To address the vacuum casting defects in pultruded beams, ultrasonic and radiographic non-destructive testing technologies are external, post-forming inspection methods. The resin flow front is a dynamic, internal, and rapidly changing process. External inspection methods cannot accurately capture the resin flow front inside the closed, narrow splice seams online. Their offline approach and time lag cannot meet the requirement for real-time, in-situ monitoring of the resin flow front, nor can they achieve long-term, continuous monitoring.

[0004] In summary, the technical problems existing in the relevant technologies need to be improved. Summary of the Invention

[0005] The main objective of this application is to propose a waveform-layout segmented bonded fiber optic sensor for resin flow monitoring and its application. The sensor includes a sensing fiber fixed inside the material to be detected area, extending along a preset periodic waveform path. The fiber can directly contact the resin flow front and significantly increase the contact area and action area between the fiber and the resin, enabling long-term, real-time, and continuous resin flow monitoring.

[0006] To achieve the above objectives, this application proposes a waveform-layout segmented adhesive fiber optic sensor for resin flow monitoring; the fiber optic sensor includes: A sensing fiber extending along a preset periodic waveform path; The sensing optical fiber is fixed to the monitored area on the surface of the composite material component under test with several spaced bonding points, so that when the resin flows in the monitored area, the resin flow front comes into contact with the sensing optical fiber.

[0007] In some embodiments, the preset periodic waveform path may take the form of a continuous and periodically uniform curve, a non-uniform periodic curve, or a variable periodic curve; the continuous and periodically uniform curve may take the form of a sine wave or a cosine wave.

[0008] In some embodiments, the amplitude of the preset periodic waveform path is set according to the height of the area to be monitored.

[0009] In some embodiments, the spacing between the adhesive points is less than or equal to half a wavelength of the preset periodic waveform path.

[0010] In some embodiments, the bonding point is located at one or more of the peaks, troughs, and zero points of the preset periodic waveform path.

[0011] In some embodiments, the number of bonding points is set according to the number and distribution of the peaks, troughs and zero points of the waveform path.

[0012] To achieve the above objectives, this application also provides a resin flow monitoring system; the monitoring system includes an optical fiber sensor, an optical fiber detection module, and a controller; wherein, The fiber optic sensor includes a sensing fiber extending along a preset periodic waveform path; the sensing fiber is fixed to the monitored area on the surface of the composite material component under test at several spaced bonding points, so that when resin flows in the monitored area, the resin flow front contacts the sensing fiber. The fiber optic detection module is used to transmit a broadband scanning light signal to the object being detected and to receive the feedback signal returned by the object being detected. The controller is used to control the optical fiber detection module to transmit optical signals to the sensing optical fiber in the optical fiber sensor and receive the feedback signals returned by the sensing optical fiber to generate a signal to be demodulated; the feedback signals returned by the sensing optical fiber are either backscattered signals returned by the sensing optical fiber or reflected wavelength signals of each fiber grating in the sensing optical fiber; the signal to be demodulated characterizes the response of the sensor before and after the resin flow front comes into contact with the sensing optical fiber; based on the analysis of the signal to be demodulated, the resin flow in the area to be monitored is determined according to the analysis results.

[0013] In some embodiments, when the feedback signal returned by the sensing fiber is a backscattered signal returned by the sensing fiber, the controller controls the fiber detection module to transmit an optical signal to the sensing fiber in the fiber sensor and receive the feedback signal returned by the sensing fiber to generate a signal to be demodulated, the process including: The optical fiber detection module is controlled to transmit optical signals to the sensing optical fiber in the optical fiber sensor. Before the resin is injected into the area to be monitored, the optical fiber detection module is controlled to receive the backscattered signal of the sensing optical fiber and record the reference signal. When the resin flows in the area to be monitored, the signal abrupt change point and its time in the backscattered signal of the sensing optical fiber are identified according to the reference signal, and the demodulated signal is obtained based on the identification result.

[0014] In some embodiments, the process by which the controller analyzes the signal to be demodulated and determines the resin flow in the monitored area based on the analysis results includes: Based on the demodulated signal, several signal abrupt change points and their corresponding occurrence times in the backscattered signal of the sensing optical fiber when the resin flows in the monitored area are determined. Based on several signal abrupt change points and their corresponding occurrence times, the several signal abrupt change points are connected and fitted on a two-dimensional plane to obtain a continuous profile of the resin flow front. The resin flow conditions in the monitored area are determined by analyzing the continuous profile of the resin flow front.

[0015] In some embodiments, the system further includes a plurality of adjacent sensing grid areas disposed in the area to be monitored; the sensing grid areas include a first grid area and a second grid area; the first grid area is disposed at the trough of the preset periodic waveform path; the second grid area is disposed at the peak of the preset periodic waveform path; the controller is further configured to perform the following steps: When the resin flows in the area to be monitored, the strain response generated by the sensing optical fiber at several of the sensing grating regions is acquired. The strain response generated by the sensing optical fiber at adjacent first and second grating regions is analyzed, and the resin flow direction between the adjacent first and second grating regions is determined based on the analysis results, so as to determine the resin flow direction in the area to be monitored.

[0016] The embodiments of this application include at least the following beneficial effects: This application provides a waveform-layout segmented bonded fiber optic sensor for resin flow monitoring and its application. The waveform-layout segmented bonded fiber optic sensor provided by this application sets the sensing fiber in the monitoring area on the surface of the composite material to be tested, so that when there is resin flow in the monitoring area, the sensing fiber can contact the resin flow front. Compared with traditional external monitoring methods, the sensing fiber set in the system of this invention can directly and in real time sense the resin flow front inside the composite material component, and can more accurately and in real time sense the resin flow inside the component. Furthermore, the sensing fiber in the fiber optic sensor of this invention extends with a preset periodic waveform path. Through this design, the contact area and action area between the fiber and the resin can be significantly increased, the signal changes brought about by the resin flow can be amplified, and the signal-to-noise ratio and monitoring sensitivity can be improved. Attached Figure Description

[0017] Figure 1 This is an optional schematic diagram of the fiber optic sensing deployment provided in the embodiments of this application; Figure 2 This is another optional schematic diagram of the sensing fiber optic deployment provided in the embodiments of this application; Figure 3A A flowchart illustrating the fabrication process of a single-waveform fiber optic sensor provided in this application embodiment; Figure 3B This is a flowchart illustrating the fabrication process of the dual-waveform fiber optic sensor provided in an embodiment of this application. Figure 4A These are schematic diagrams illustrating the different optical fiber structures provided in the embodiments of this application; Figure 4B The signal response curves of the resin reaching different sensors are provided in the embodiments of this application; Figure 5 This is a structural block diagram of the resin flow monitoring system based on waveform-deployed segmented adhesive fiber optic sensors provided in the embodiments of this application; Figure 6A This is a schematic diagram of the deployment method of a dual-waveform fiber optic sensor provided in an embodiment of this application; Figure 6B The signal response curves of the resin reaching the corresponding sensors of each gate region are provided in the embodiments of this application; Figure 6C This is a schematic diagram of the deployment method of a dual-waveform distributed optical fiber sensor provided in an embodiment of this application; Figure 6D The signal response curve of the resin reaching the dual-waveform distributed optical fiber sensor provided in the embodiments of this application; Figure 7A This is a schematic diagram of a multi-layer FBG seam monitoring system provided in an embodiment of this application; Figure 7B This is a characteristic signal diagram of the abrupt change in the wavelength of the resin reaching the center of each FBG, provided in the embodiments of this application. Figure 7C The figure shows the experimental results of longitudinal flow field monitoring of multi-layer seams provided in the embodiments of this application. Detailed Implementation

[0018] To make the objectives, technical solutions, and advantages of this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of this application and are not intended to limit it. In the following description, when referring to the accompanying drawings, unless otherwise indicated, the same numbers in different drawings represent the same or similar elements. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with those of this application; they are merely examples of apparatuses and methods consistent with some aspects of the embodiments of this application as detailed in the appended claims.

[0019] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing embodiments of this application only and is not intended to limit this application.

[0020] Before providing a detailed description of the embodiments of this application, some of the nouns and terms involved in the embodiments of this application will be explained first. The nouns and terms involved in the embodiments of this application are subject to the following interpretations.

[0021] 1) Va-RTM (Va-Assisted Resin Transfer Molding): An advanced composite material molding process. Its core is to inject resin into a closed mold cavity pre-laid with dry fiber reinforcements in a vacuum environment.

[0022] 2) Joint seam: The joint mark formed when multiple parts are connected during the processing and manufacturing of materials or components to meet size or shape requirements.

[0023] 3) OFDR (Optical Frequency Domain Reflectometry) technology: A high-precision distributed fiber optic sensing technology. It analyzes the optical frequency signal backscattered by laser light in the optical fiber to continuously measure physical parameters such as strain and temperature along the entire fiber. Its core advantages lie in its extremely high spatial resolution (millimeter level) and measurement accuracy, which can transform the entire optical fiber into tens of thousands of continuous sensing points.

[0024] Pultruded beams for wind turbine blades are fabricated by vacuum infusion of stacked pultruded plates, achieving the goal of structural lightweighting. This technology offers advantages such as faster, lighter, and higher-quality production, and is widely used in the manufacture of large pultruded beams.

[0025] However, when fabricating pultruded beams using Va-RTM (vacuum-assisted resin transfer molding), the following technical issues need to be addressed: Pultruded sheets are integrally cast with the shell after being spliced ​​laterally and stacked longitudinally. The tangential splice seams are narrow and closed, extending along the longitudinal direction to form the casting channels. However, the splice seam arrangement deviations caused by the splicing and stacking of pultruded sheets result in staggered seam positions and uneven sizes, which increases the complexity of resin flow within the splice seam channels. This leads to initial internal manufacturing defects such as resin voids during the casting process, affecting the overall strength of the main beam. Existing technologies lack real-time monitoring methods for the resin flow front within the splice seams during the vacuum casting process of pultruded sheet spliced ​​beam structural components. This makes it impossible to provide timely warnings when defects form in their early stages, thus hindering process optimization. This is mainly reflected in the following aspects: (1) Existing non-destructive monitoring technologies (such as ultrasonic and X-ray detection) are external, offline detection methods after molding, which cannot accurately capture the resin flow front information inside the closed and narrow confined space of the splice seam, and have the problem of insufficient lag; while single-point invasive monitoring technology sensors (such as thermocouples and pressure sensors) are too large and difficult to be embedded in the same splice seam at multiple points at the same time for continuous monitoring.

[0026] (2) Existing non-destructive testing technologies can only monitor for manufacturing defects after the molding process has been completed, and cannot monitor and provide early warnings in the early stages of molding. This means that the problems of high quality, high efficiency, visibility and controllability in the preparation of pultruded beams by Va-RTM process have not yet been effectively solved.

[0027] (3) Some existing detection probes need to be removed after the injection is completed, and cannot be retained inside the structure to take into account subsequent mechanical performance testing and structural health monitoring during service life, resulting in waste of monitoring resources and limited functionality.

[0028] (4) Existing resin flow monitoring technologies do not address special geometric features such as pultruded beam splice joints, and lack dedicated, highly sensitive monitoring methods.

[0029] In the relevant technologies for resin flow monitoring, linear optical fiber sensing is analyzed: The resin flow within the seam can be considered as a steady laminar flow of an incompressible Newtonian fluid between two infinitely large parallel plates, satisfying the no-slip boundary condition, i.e., at the wall surface... The fluid velocity is strictly zero, characterized by equation (1):

[0030] For straight optical fibers deployed on the sidewalls of the joint, the drag force per unit length of fluid, according to Stokes' cylinder drag formula, is... Calculated using equation (2):

[0031] Combining equations (1) and (2), we can see that This application provides a waveform-layout segmented adhesive fiber optic sensor for resin detection, the fiber optic sensor comprising:

[0032] As can be seen from equation (3), when a straight optical fiber is laid on the side wall of the splice, the fluid force it experiences is always zero, and it cannot sense the resin flow front.

[0033] In response, this application provides a waveform-layout segmented bonding fiber optic sensor, which includes: A sensing fiber extending along a preset periodic waveform path; The sensing optical fiber is fixed to the monitored area on the surface of the composite material component under test with several spaced bonding points, so that when the resin flows in the monitored area, the resin flow front comes into contact with the sensing optical fiber.

[0034] In this embodiment, the optical fiber is pre-bent into a waveform structure and laid on the side wall of the splice in a segmented bonding manner, so that the highest point of the fiber bending is located at the midpoint of the splice width direction, which is the position of maximum flow velocity. The axial strain response of the optical fiber is amplified by the superposition effect of bending prestress and fluid viscosity, so as to achieve high sensitivity to weak flow fields, while not changing the outer diameter of the optical fiber.

[0035] Quantitative verification of the waveform fiber optic sensitization effect provided in the embodiments of this application: Optical fiber with amplitude Pre-bending occurs when the highest point of the bend is located at the midpoint of the seam width direction (y=0), at which point the flow velocity is maximum. The calculation is performed using equation (4):

[0036] in, The pressure difference (Pa) between the two ends of the seam. Resin viscosity ( H represents the seam height (m).

[0037] The aforementioned sensing fiber can convert optical signals into electrical signals through reflection and demodulation by a fiber optic grating (FBG), and obtain the fiber strain response signal through signal processing and data output. The FBG center wavelength shift is also considered. With axial strain They satisfy a strict linear relationship, as shown in equation (5):

[0038] in, For the strain sensitivity coefficient, approximately When the resin flow front reaches the FBG sensor position, the optical fiber experiences a sudden strain due to the resin's viscous force, resulting in a step change in the center wavelength. The moment of this step change in center wavelength is used as the criterion for the arrival of the resin flow front, serving as the physical basis for the fiber optic sensor provided in this embodiment to identify resin flow.

[0039] In summary, the waveform-arranged segmented bonded fiber optic sensor provided in this application places the sensing fiber in the monitored area on the surface of the composite material to be tested. When resin flows in the monitored area, the sensing fiber comes into contact with the resin flow front. Compared with traditional external monitoring methods, the sensing fiber in this invention can directly and in real-time sense the resin flow front inside the composite material component, enabling more accurate and real-time sensing of the resin flow inside the component. Furthermore, the sensing fiber in this invention extends along a preset periodic waveform path. This design significantly increases the contact area and action area between the fiber and the resin, amplifies the signal changes caused by resin flow, and improves the signal-to-noise ratio and monitoring sensitivity.

[0040] Regarding the settings for the fiber optic sensor: Fiber optic sensors can be directly implanted into the internal sidewalls of confined spaces. The relaxed section is suspended in the air, directly "sensing" the microscopic strain caused by the impregnation and flow of resin. The measurement signal is direct, accurate, and without intermediate attenuation. This solves the signal shielding and monitoring blind zone problems of traditional external monitoring technologies (such as ultrasound and X-rays) due to the obstruction of molds and vacuum bags, and is especially suitable for critical areas of joints with complex structures that are most prone to defects.

[0041] Specifically, regarding the configuration of the sensing fiber in the fiber optic sensor: Optionally, the preset periodic waveform path is a continuous and periodically uniform curve; the curve form includes sine waves and cosine waves.

[0042] By arranging the sensing optical fibers in the fiber optic sensor in the form of a continuous and periodically uniform curve, the resin flow in the monitored area can be continuously and uniformly sensed; the curve form can be a sine wave, a cosine wave, or other periodically uniform curve forms.

[0043] Optionally, the preset periodic waveform path can be a non-uniform periodic or variable periodic curve.

[0044] In critical areas with complex resin flow channels and dramatic morphological changes (such as channel junctions and areas of abrupt thickness changes), a denser waveform layout (i.e., smaller period and larger amplitude) is used; in areas with gentle flow, a sparser layout is used. This optimizes the allocation of monitoring resources without increasing the total length of optical fibers, achieving a balance between global coverage and high-precision local monitoring.

[0045] Optionally, the amplitude of the preset periodic waveform path can be set according to the height of the area to be monitored.

[0046] In this embodiment, the amplitude of the periodic waveform path is set according to the height of the area to be monitored to ensure that the optical fiber can cover the entire height direction of the area to be monitored.

[0047] Optionally, the period and amplitude of the preset periodic waveform path can be adjusted according to the requirements of monitoring accuracy and monitoring range. The monitoring accuracy of the optical fiber depends on the spatial sampling density and coverage range in the height direction within the monitoring area. The smaller the period, the more peaks and troughs there are per unit length, and the higher the spatial sampling capability of the optical fiber for the minute positional differences caused by resin flow. The larger the amplitude, the greater the undulations in the waveform path in the height direction, making the relaxed section of the optical fiber more easily disturbed by the high-pressure zone of resin flow, and the higher the resolution of the flow front morphology.

[0048] In some embodiments, the areas on the sensing optical fiber with adhesive joints are called adhesive regions, and other areas are called non-adhesive regions. The adhesive joints use instant adhesive to locally fix the optical fiber to the component surface, while the optical fiber in the non-adhesive regions is in a relaxed contact or separated state from the component surface. The adhesive region firmly fixes the optical fiber, preventing interference from resin flow, thus ensuring the stability of the sensor reference and the accuracy of the monitoring point's spatial position. It also effectively isolates interference signals from non-monitoring areas, improving the signal-to-noise ratio and anti-interference capability. The non-adhesive region (free region) serves as a sensitive sensing unit, specifically for sensing the arrival of resin. A segmented adhesive bonding method is used, achieving precise positioning and signal triggering at the adhesive joints, while mechanical decoupling between the optical fiber and the component body is achieved in the non-adhesive regions. This effectively isolates the interference of structural background strain (such as thermal expansion and installation stress) on the sensing signal, significantly improving the signal-to-noise ratio and reliability of the monitoring signal.

[0049] Optionally, the spacing between the bonding points is less than or equal to half a wavelength of a preset periodic waveform path.

[0050] The spacing between the bonding points is less than or equal to half the wavelength of the waveform path, so as to achieve a reasonable acquisition area setting for signals related to resin flow.

[0051] Optionally, the bonding point is located at one or more of the peaks, troughs, and zero points of the preset periodic waveform path.

[0052] Specifically, the period of the waveform sensing fiber can be calculated based on the effective monitoring dimensions of the composite material component (such as a pultruded plate) and the preset sampling density. Using this period as a geometric reference, the peaks, troughs, and zero phase of the waveform path are then used as the locations for segmented bonding points. The bonding points for these segments are located at one or more combinations of the peaks, troughs, or zero phases of the waveform path. By fixing these key nodes, the waveform shape can be constrained most effectively, ensuring that the free segment undergoes controllable and consistent deformation under resin impact.

[0053] Optionally, the number of bonding points can be set according to the number and distribution of peaks, troughs, and zero points of the waveform path.

[0054] In this example, the number of bonding points is set according to the number and distribution of peaks, troughs, and zero points in the periodic waveform path. Therefore, the number of fixed points on the waveform fiber is not fixed and can be set as needed based on the number and distribution of peaks, troughs, or zero-phase points; for example, one, two, or three fixed points can be set for each cycle. By selecting a fixed or variable number of fixed points, the requirements for ease of deployment, path stability, and monitoring accuracy can be balanced.

[0055] In this embodiment, the sensing optical fiber itself is made of glass, and its material properties enable it to withstand chemical corrosion in the resin system, thereby improving the performance stability of the sensor. Optionally, the diameter of the sensing fiber is generally ≤0.5mm and not greater than the width of the splice seam.

[0056] Optionally, the sensing fiber can be a bare fiber structure or a thin cable structure.

[0057] In this embodiment, the sensing optical fiber can be a bare optical fiber or a thin cable structure. Its outer layer has a flexible coating that is corrosion-resistant and high-temperature resistant, which can protect the fiber core and maintain sufficient flexibility in the free section to respond to the flow of resin.

[0058] Optionally, in this embodiment, multiple independent waveform monitoring units can be deployed in parallel or in series on the sensing optical fiber. Each unit covers a specific sub-region and is demodulated by the same optical fiber detection device, thereby realizing zoned collaborative monitoring of large-sized components or complex flow channels.

[0059] In some embodiments, see Figure 1 , Figure 1This is an optional schematic diagram of the fiber optic sensor layout provided in this embodiment, specifically showing a three-dimensional schematic diagram of the waveform fiber optic sensor deployed on the side of the pultruded plate seam. It includes a sensing fiber optic cable 1, a seam 2, a transparent acrylic plate 3, a biaxial fiberglass cloth 4, a carbon fiber pultruded plate 5, a flow guide mesh 6, and instant adhesive 7. The illustrated assembly includes a waveform fiber optic sensor 1 with a diameter of 0.25mm, and a carbon fiber pultruded plate 5 with dimensions of 250mm × 120mm × 5mm (length × width × height). Two plates are joined chordally to form a seam 2, which provides a flow channel for the resin, with a cross-sectional dimension of 5mm × 3mm. The biaxial fiberglass cloth is laid on top of the pultruded plate, and two transparent acrylic plates 3 are placed on top of the biaxial fiberglass cloth, with the seam's cross-sectional dimension of 5mm × 3mm. The fiber optic cable is bonded to the side wall of the carbon fiber pultruded plate at the seam.

[0060] In some embodiments, see Figure 2 , Figure 2 This is another optional schematic diagram of the fiber optic sensing layout provided in this application, specifically showing a planar schematic diagram of the waveform fiber optic sensor layout path in the embodiment of this application; The illustrated optical fiber is laid out as a continuous sinusoidal wave path on the sidewall of the long side of the lower carbon fiber pultruded plate. The period of the sine wave is 250 mm, and the amplitude is 5 mm. This design ensures an effective monitoring height perpendicular to the flow direction in the main direction of resin flow at the joint, sufficient to depict the lateral morphology of the resin flow front. The 250 mm period provides a long resin flow front, thus obtaining a complete view of the resin flow front; we chose this size because the fiber is small in size, lightweight, easy to wire, and easy to embed in the vacuum infusion mold without compromising the seal of the vacuum bag, making it suitable for vacuum-assisted resin transfer molding processes.

[0061] In one embodiment, see Figure 3A and Figure 3B ,in Figure 3A This is a flowchart illustrating the fabrication process of a single-waveform fiber optic sensor provided in an embodiment of this application. Figure 3BThis document provides a flowchart for the fabrication of a dual-waveform fiber optic sensor according to an embodiment of this application. The fabrication process includes: wiping the material surface with an alcohol-based lint-free cloth; testing the fiber optic connector with a visible red light source; precisely positioning the fiber optic cable according to the designed waveform path and completing segmented bonding. High-temperature resistant epoxy resin adhesive is used to spot-bond the fiber at the zero-phase points of all sine waves (i.e., the central axis of the path), forming circular bonding points with a diameter of approximately 3 mm. Each bonding point firmly fixes the fiber optic cable to the mold surface. The highest bending segment of the fiber optic cable is in a free state. To ensure that the resin preferentially pushes the free segment of the fiber optic cable, a 1.5 mm thick polytetrafluoroethylene sheet is placed under each free segment of the fiber optic cable as a micro-shield during installation, creating a small gap between the fiber optic cable and the mold surface. After the fiber optic cable is installed and firmly bonded, this sheet is removed. To prevent the sensor from breaking due to mechanical disturbance during embedding, both ends of the fiber optic cable are encapsulated with sleeves to protect the fiber optic cable's inlet and outlet.

[0062] In some embodiments, the prepared sensor is attached to an equal-strength cantilever beam calibration component. Five sets of static loads with different amplitudes were applied within the range to establish a linear correlation between the center wavelength drift and the axial strain. The linear correlation coefficient of the calibration results was approximately 0.999.

[0063] In some embodiments, after vacuum-filling epoxy resin, a continuous strain signal generated by the waveform segment optical fiber can be monitored by a demodulator. By tracking the location of the abrupt strain signal, the process of vertical resin filling can be successfully monitored.

[0064] In one embodiment, three different fiber optic sensor structures were designed to compare strain response characteristics: the sensors were placed on the sidewall of the splice near the infusion port, a Va-RTM visualization infusion experimental platform was built, a camera was added to the side of the sample to synchronously record resin flow images, and a fiber optic demodulator was used to acquire the center wavelength signal at a sampling frequency of 20Hz. The specific process included: See Figure 4A , Figure 4B , Figure 4A These are schematic diagrams illustrating the different structures of optical fibers provided in the embodiments of this application; wherein... Figure 4A Figure (1) shows a straight optical fiber, Figure (2) shows a waveform optical fiber sensor with an amplitude of 2.5 mm provided in the embodiment of this application, and Figure (3) shows a waveform optical fiber sensor with an amplitude of 5 mm provided in the embodiment of this application. Figure 4B The signal response curves of the resin reaching different sensors are provided in the embodiments of this application; wherein, the horizontal axis is time (s) and the vertical axis is the center wavelength offset (mm); wherein Figure 4BFigure (1) shows the signal response curve corresponding to the straight optical fiber, Figure (2) shows the signal response curve corresponding to the 2.5mm amplitude waveform optical fiber sensor provided in the embodiment of this application, and Figure (3) shows the signal response curve corresponding to the 5mm amplitude waveform optical fiber sensor provided in the embodiment of this application. As can be seen from the figures, when the resin reaches the position of the 5mm amplitude waveform optical fiber sensor, the center wavelength suddenly increases by about 14pm. The absolute error of the resin arrival time is 0.04s and the relative error is 0.04% when the center wavelength steps change abruptly. Compared with the straight optical fiber (without obvious sudden change response), the 5mm amplitude waveform sensor has obvious signal characteristics and significantly improved sensitivity.

[0065] According to equation (5), with amplitude h = 5mm and fixed point spacing H = 130mm, P = 530.7 Pa, μ = 0.2 Pa s, a = 3mm, substituting into the calculation, we get: ε=16.12με Far exceeding the minimum sensing threshold of optical fiber That is, the 5mm amplitude waveform fiber optic sensor provided in this application embodiment can achieve high sensitivity.

[0066] See Figure 5 , Figure 5 This is a structural block diagram of a resin flow monitoring system based on a waveform-layout segmented adhesive fiber optic sensor, as provided in an embodiment of this application. The system includes a fiber optic sensor, a fiber optic detector, and a controller. The fiber optic sensor includes a sensing fiber extending along a preset periodic waveform path; the sensing fiber is fixed to the monitored area on the surface of the composite material component to be tested at several spaced bonding points, so that when the resin flows in the monitored area, the resin flow front comes into contact with the sensing fiber. The fiber optic detection module is used to transmit broadband scanning light signals to the object being detected and to receive feedback signals returned by the object. The controller is used to control the fiber optic detection module to transmit optical signals to the sensing fiber in the fiber optic sensor and receive the feedback signals returned by the sensing fiber to generate a signal to be demodulated. The feedback signals returned by the sensing fiber are either backscattered signals returned by the sensing fiber or reflected wavelength signals of each fiber grating in the sensing fiber. The signal to be demodulated characterizes the response generated by the sensor before and after the resin flow front comes into contact with the sensing fiber. Based on the analysis of the signal to be demodulated, the resin flow in the area to be monitored is determined according to the analysis results.

[0067] On the one hand, the beneficial effects of the fiber optic sensor in this embodiment are the same as those in the above embodiments; on the other hand, the system of the present invention analyzes the response generated by the fiber optic cable before and after the resin flow front contacts the sensing fiber optic cable, and uses the change in the fiber optic response to characterize the resin flow inside the component. After the task is completed, the subsequent manufactured composite material structure can be manufactured according to the recorded data without the need to place the fiber optic cable again; at the same time, this monitoring is non-destructive monitoring and will not affect the molding of the composite material component. It can be permanently retained inside the composite material component, thereby reducing monitoring costs and improving the economic efficiency of the sensor.

[0068] Specifically, the settings for the fiber optic detection module are as follows: Optionally, the fiber optic detection device in the fiber optic detection module of this embodiment adopts a phase-sensitive optical time-domain reflectometer, which senses the vibration or strain of the free segment of the fiber by monitoring the phase change of the back Rayleigh scattered light. It has extremely high sensitivity to weak and dynamic resin contact signals.

[0069] Optionally, when the sensing fiber is a fully distributed sensing fiber or a fiber grating array is set at the peaks and valleys, the fiber detection module can use OFDR technology or a fiber grating demodulator, whose spatial resolution is better than one cycle length of the waveform path, to ensure that the trigger signals of adjacent free segments can be clearly distinguished.

[0070] Regarding the controller's settings and functions: Optionally, the controller in this embodiment has built-in signal filtering and pattern recognition algorithms, which can automatically distinguish between effective signals generated by resin flow and noise interference caused by mechanical vibration or temperature changes, further improving the reliability and accuracy of monitoring results. Furthermore, the controller can collect and store wavelength signals or distributed backscattered signals output by the fiber optic detection module. Based on the collected full-time, full-space sensing signals, through subsequent data processing and reconstruction algorithms, the real-time position, propagation path and complete filling process of the resin flow front can be inverted and restored, and key process parameters such as filling uniformity and filling time can be extracted, providing quantitative basis for the optimization of composite material molding process.

[0071] In some embodiments, when the feedback signal returned by the sensing fiber is a backscattered signal returned by the sensing fiber, the controller controls the fiber detection module to transmit an optical signal to the sensing fiber in the fiber optic sensor and receive the feedback signal returned by the sensing fiber to generate the signal to be demodulated, including but not limited to steps S110 to S130: Step S110: Control the optical fiber detection module to transmit an optical signal to the sensing optical fiber in the optical fiber sensor.

[0072] The fiber optic detection module consists of fiber optic detection equipment, which is a device capable of demodulating optical fibers, such as an optical time-domain reflectometer or an optical frequency-domain reflectometer, used to transmit optical signals to the sensing fiber and receive its backscattered signals.

[0073] In step S120, before the resin is injected into the area to be monitored, the fiber optic detection module is controlled to receive the backscattered signal from the sensing fiber and record the reference signal.

[0074] Before resin injection, the entire sensing fiber is in an initial stress state because it is bonded in waveform segments. The fiber optic testing equipment acquires and stores the initial signal of the fiber at this time as a reference.

[0075] Step S130: When the resin flows in the area to be monitored, the signal abrupt change point and its time in the backscattered signal of the sensing fiber are identified according to the reference signal, and the demodulated signal is obtained based on the identification result.

[0076] When resin flows in the monitored area on the surface of a composite component, specifically when it flows within the mold cavity and contacts a free fiber segment, the fluid pressure and wetting effect of the resin cause significant bending, displacement, or vibration in that free fiber segment, resulting in substantial strain at that location. The fiber optic testing equipment can detect and record these signal abrupt changes caused by resin contact in real time, and finally summarize them to obtain the demodulated signal.

[0077] Optionally, when using distributed fiber optic sensors, the location of the abrupt change can be precisely pinpointed.

[0078] Specifically, in this example, the waveform sensing fiber can monitor resin flow using demodulation techniques based on the strain principle. The pressure of the flowing resin exerts mechanical compression and stretching on the fiber, causing compressive and tensile strains that affect the center wavelength. Demodulation techniques convert the wavelength shift of the fiber grating or the frequency shift of the sensing fiber relative to its initial state into strain values. The strain distribution in the resin flow region can visually reflect the resin flow front, thus revealing the resin space-filling state.

[0079] In some embodiments, the process of the controller analyzing the signal to be demodulated and determining the resin flow in the area to be monitored based on the analysis results includes, but is not limited to, steps S210 to S230: Step S210: Based on the demodulated signal, determine several signal abrupt change points and their corresponding occurrence times in the backscattered signal of the sensing fiber when the resin flows in the monitored area.

[0080] The controller includes a data processing unit; through the data processing unit, based on the demodulated signal, it is possible to determine all signal abrupt change points (i.e., the points where the resin has reached) detected by the fiber optic detection device at various times.

[0081] Step S220: Based on several signal abrupt change points and their corresponding occurrence times, connect and fit several signal abrupt change points on a two-dimensional plane to obtain a continuous profile of the resin flow front.

[0082] By connecting and fitting the detected signal abrupt change points at various moments on a two-dimensional plane, and because the optical fiber is laid out in a "waveform" path, these discrete monitoring points are naturally distributed in space, which can effectively reconstruct the continuous profile of the resin flow front.

[0083] Optionally, the controller in this example can map the length coordinates of the optical fiber to the two-dimensional plane coordinates of the mold through algorithms or finite element simulation, and generate dynamic cloud maps or contour maps of the resin filling process to visualize the flow process.

[0084] Step S230: Analyze the continuous profile of the resin flow front to determine the resin flow status in the area to be monitored.

[0085] By analyzing the continuous profile of the reconstructed resin front, the resin flow on the surface of the composite material component under test can be determined.

[0086] In some embodiments, the system further includes a plurality of adjacent sensing grid areas disposed in the area to be monitored; the sensing grid areas include a first grid area and a second grid area; the first grid area is disposed at the trough of a preset periodic waveform path; the second grid area is disposed at the peak of a preset periodic waveform path; the controller is further configured to perform the following steps: When resin flows in the area to be monitored, the strain response generated by the sensing fiber at several sensing gratings is acquired; the strain response generated by the sensing fiber at adjacent first and second gratings is analyzed, and the resin flow direction between adjacent first and second gratings is determined based on the analysis results, so as to determine the resin flow direction in the area to be monitored.

[0087] Sensing grating regions are arranged at the crests and troughs of the waveform optical fiber. Utilizing two opposite local curvature directions, resin flowing in the same direction produces strain responses in opposite directions in the two grating regions, thus achieving flow direction identification. The "same-direction flow-opposite-response" mechanism: Assume the fiber bends locally downwards at the trough and locally upwards at the crest. When the resin flows upwards from the bottom, the viscous force is upwards: In the first grating region at the trough: the viscous force couples with the curvature direction, causing axial compression of the fiber and a negative shift in the center wavelength. The second grating region at the peak: the coupling between viscous force and curvature direction causes axial stretching of the fiber, resulting in a positive shift of the center wavelength. The combination of the drift directions of the two gate regions uniquely corresponds to the resin flow direction, enabling qualitative determination of the flow direction.

[0088] In some embodiments, taking the dual-waveform fiber optic sensor provided in this application as an example, such as... Figure 6A As shown, sensing grid areas are set in the area to be monitored: the first grid area is located at the trough of the waveform structure, with an initial center wavelength of approximately 1556 nm; the second grid area is located at the peak of the waveform structure, with an initial center wavelength of approximately 1550 nm. The center wavelengths of the two grid areas are spaced approximately 6 nm apart to avoid spectral overlap. The strain response at the location of the grid area is obtained through an FBG sensor. A third FBG sensor is used as a temperature compensation unit, and its complete grid area is fixed to the side wall surface of the pultruded plate with epoxy resin to prevent it from being affected by resin flow stress and to only respond to changes in ambient temperature.

[0089] like Figure 6B As shown, Figure 6B The signal response curves of the resin reaching the corresponding sensors in each gate region are provided in the embodiments of this application; wherein, the first gate region (trough) is 60mm from the injection port end, the second gate region (peak) is 50mm from the first gate region, and the temperature compensation unit is located between the two. Figure 6B It can be concluded that when the resin is first injected, the center wavelength of the first grid region (trough) drops sharply at 70.21s, and the second grid region (peak) rises sharply at 76.55s. The two responses are in opposite directions, verifying the above-mentioned "co-current flow-reverse response" mechanism. When the resin is injected for the second time, the center wavelengths of the two grid regions change sharply in opposite directions again, verifying the sensor's ability to identify the multi-stage flow front. The center wavelength of the FBG3 temperature-compensated sensor does not change throughout the entire process, proving that the monitoring signal is not affected by temperature. The absolute errors of the first grid region and the second grid region in identifying the resin are 0.07s and 0.05s, respectively.

[0090] like Figure 6C As shown, Figure 6C This is a schematic diagram of the deployment method of a dual-waveform distributed optical fiber sensor provided in an embodiment of this application. (The calibration points are set to facilitate subsequent analysis.) The entire fiber optic segment is the sensing area; the strain response of the entire fiber optic segment is obtained through distributed fiber optic sensors.

[0091] like Figure 6D As shown, Figure 6DThe signal response curve of the resin to the dual-waveform distributed optical fiber sensor provided in this embodiment shows that the resin reaches the trough region at 603.8 s, exhibiting a negative strain response. At 1113.68 s, the resin reaches the peak region, exhibiting a positive strain response. This "co-current flow-reverse response" mechanism is consistent with the mechanism revealed by the dual-waveform fiber Bragg grating sensor.

[0092] In some embodiments, such as Figure 7A As shown, Figure 7A This is a schematic diagram of a multi-layer seam monitoring system for tandem FBGs provided in an embodiment of this application. As shown in the figure, this embodiment uses low-loss fiber optic fusion splicing technology to connect multiple FBG units with different center wavelengths in series on a single optical fiber, and arranges them layer by layer in the multi-layer seam area to achieve synchronous layered monitoring of the longitudinal flow field. Five FBG sensing units were selected, each with a grating length of 10 mm and initial center wavelengths of approximately 1555.072 nm, 1555.051 nm, 1550.133 nm, 1544.962 nm, and 1535.274 nm, respectively. The strain sensitivity coefficients were all approximately 1.1 pm / με, and the linear correlation coefficients were all not less than 0.999. The five FBG sensing units were connected in series using a fusion splicing method: the coating layer at the end of each FBG sensor was stripped using fiber optic strippers, and the end face was cut vertically using a fiber optic cleaver; the five FBG sensing units were then connected in series with low loss using a fiber optic fusion splicer, with the splice loss controlled at 0.00 dB; the splice point was encapsulated with a protective sleeve and heat-shrink reinforced; one end of the series fiber was fused to an FC / PC interface single-mode fiber optic patch cord for connection to the fiber optic demodulator 8.

[0093] Reference Figure 7A The structure consists of five layers of pultruded sheets with joints (total thickness 25mm), each layer measuring 250mm × 120mm × 5mm. FBG-1 to FBG-5 are sequentially layered from top to bottom, with each layer segmented and bonded to the joint sidewalls using a waveform pattern of 5mm amplitude and 130mm fixed point spacing. The sensing grid area is located at the midpoint of the length of each layer. A spiral injection method is used, transforming resin injection from point injection to near-line injection, improving the uniformity of multi-layer filling.

[0094] like Figure 7B As shown, Figure 7B This is a characteristic signal diagram of the abrupt change in the wavelength of the resin reaching the center of each FBG, provided in the embodiments of this application. Figure 7C The figure shows the experimental results of longitudinal flow field monitoring at multi-layer seams provided in the embodiments of this application, wherein... Figure 7CFigures (a) to (e) show the experimental results of the flow front at times 330.56 s, 342.67 s, 353.36 s, 362.77 s, and 370.36 s, respectively. The upper part of each figure (a) to (e) is a simulated side view, and the lower part is a physical side view. The final statistical results are shown in Table 1, which compares the time of sudden increase in the center wavelength of the resin reaching each FBG sensor layer with the actual arrival time of the resin front observed by high-speed video recording. Table 1

[0095] The maximum absolute error of each layer is 0.10 s, which meets the accuracy requirements for real-time monitoring of Va-RTM process; the response time sequence progresses from bottom to top, which is consistent with the flow path predicted by PAM-RTM simulation; the instantaneous strain amplitude of each layer increases from top to bottom, which is consistent with the distribution law of vacuum pressure gradient in the joint, verifying the physical rationality of the monitoring results.

[0096] In summary, the embodiments of this system include, but are not limited to, the following beneficial effects: (1) The flow of resin can be monitored in real time through a waveform fiber optic sensor. The sensor reflects the arrival position and time of the resin through changes in wavelength and frequency shift, and can issue early warnings when defects occur in the early stage of molding, so as to avoid problems such as reduced mechanical properties and service life caused by structural failure. Compared with the existing resin flow monitoring technology, which can only issue early warnings when defects are detected after injection molding, this sensor can detect defects in the early stage of molding, realize early warning and intervention, and effectively improve the quality and efficiency of production.

[0097] (2) The fiber optic sensor itself has the characteristics of resisting electromagnetic interference, and is suitable for monitoring the flow of vacuum-infused resin in complex electromagnetic environments, such as wind turbine blades. Experiments have shown that interference from strong electromagnetic environments such as motors and high-voltage lines will not have a significant impact on the sensor's response signal, ensuring the stability and reliability of the sensor in practical applications.

[0098] (3) Fiber optic sensing technology can perform both point and area monitoring. Fiber gratings can be used to form discrete sensor arrays to achieve high-precision sensing of multiple parameters at key points. Distributed optical fibers can achieve continuous full-field monitoring and accurately capture local flow. The two technologies can be flexibly selected or integrated to ensure comprehensive, accurate and reliable monitoring of the resin flow process, significantly improving the applicability and advancement of the method.

[0099] (4) After completing the monitoring task of the injection molding process, the fiber optic sensor records the key process data such as strain during the injection stage. Therefore, the composite material structure manufactured later can be manufactured based on the recorded data without the need to place the fiber optic cable again. At the same time, this monitoring is non-destructive and will not affect the molding of the composite material component. It can be permanently retained inside the composite material component. This sensor reduces the monitoring cost and improves the economic efficiency of the sensor.

[0100] (5) The waveform fiber optic sensor has the ability to identify the flow direction. Through the arrangement of dual grid areas, it realizes the signal identification mechanism of "same flow - reverse response", which can determine the direction and arrival order of resin flowing into the joint.

[0101] (6) Only a single optical fiber is needed to achieve multi-layer synchronous monitoring, making the system simple and low-cost. The series fiber optic grating scheme only requires one optical fiber and one demodulator to achieve real-time monitoring of five-layer seams, with the maximum absolute error of each layer not exceeding 0.10s.

[0102] (7) The same waveform layout can be used for OFDR distributed sensing, with spatial resolution up to the millimeter level, to achieve continuous characterization of the entire resin impregnation process in the seam without blind spots.

[0103] (8) By monitoring resin flow data during manufacturing using fiber optic sensors and comparing it with damage data during blade service, the key issue of how manufacturing defects affect the long-term reliability of the product can be analyzed. For example, it can be found that early cracking in a certain area is always related to slightly slower resin filling in that area during manufacturing. This provides extremely valuable empirical evidence for reverse optimization of the manufacturing process, thereby achieving a closed-loop feedback between process and performance and continuously improving product quality.

[0104] (9) Fiber optic sensors are particularly suitable for monitoring internal resin flow in the vacuum infusion molding process of composite materials. They can achieve real-time, accurate, and in-situ sensing of the resin flow front, avoiding internal defects such as dry spots and pores caused by incomplete resin wetting. They have broad application prospects in the manufacturing of high-end equipment such as wind turbine blades and aerospace composite components. They can be applied to the full life cycle management of manufacturing process monitoring and service life health monitoring of large composite material structures, realizing intelligent closed-loop quality control from "manufacturing" to "use".

[0105] (10) By designing the optical fiber as a waveform path, the spatial coverage is greatly increased within a limited length, and the morphology of the resin flow front in both length and height directions can be scanned simultaneously, realizing a leap from one-dimensional linear monitoring to two-dimensional regional monitoring, effectively avoiding the missed detection of narrow-area defects; and, only a single optical fiber is needed to monitor the entire area, with flexible wiring, high system integration, and a cost far lower than the solution of deploying a large number of point sensors.

[0106] The embodiments described in this application are for the purpose of more clearly illustrating the technical solutions of this application, and do not constitute a limitation on the technical solutions provided in this application. As those skilled in the art will know, with the evolution of technology and the emergence of new application scenarios, the technical solutions provided in this application are also applicable to similar technical problems.

[0107] Those skilled in the art will understand that the technical solutions shown in the figures do not constitute a limitation on the embodiments of this application, and may include more or fewer steps than shown, or combine certain steps, or different steps.

[0108] The device embodiments described above are merely illustrative. The units described as separate components may or may not be physically separate; that is, they may be located in one place or distributed across multiple network units. Some or all of the modules can be selected to achieve the purpose of this embodiment according to actual needs.

[0109] Those skilled in the art will understand that all or some of the steps in the methods disclosed above, as well as the functional modules / units in the systems and devices, can be implemented as software, firmware, hardware, or suitable combinations thereof.

[0110] The terms “first,” “second,” “third,” “fourth,” etc. (if present) in the specification and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms “comprising” and “having,” and any variations thereof, are intended to cover non-exclusive inclusion; for example, a process, method, system, product, or apparatus that comprises a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, methods, products, or apparatus.

[0111] In the several embodiments provided in this application, it should be understood that the disclosed apparatus and methods can be implemented in other ways. For example, the apparatus embodiments described above are merely illustrative; for instance, the division of the units described above is only a logical functional division, and in actual implementation, there may be other division methods. For example, multiple units or components may be combined or integrated into another system, or some features may be ignored or not executed. Furthermore, the coupling or direct coupling or communication connection shown or discussed may be through some interfaces; the indirect coupling or communication connection between apparatuses or units may be electrical, mechanical, or other forms.

[0112] The units described above as separate components may or may not be physically separate. The components shown as units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the units can be selected to achieve the purpose of this embodiment according to actual needs.

[0113] Furthermore, the functional units in the various embodiments of this application can be integrated into one processing unit, or each unit can exist physically separately, or two or more units can be integrated into one unit. The integrated unit can be implemented in hardware or as a software functional unit.

[0114] If the integrated unit is implemented as a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. Based on this understanding, the technical solution of this application, in essence, or the part that contributes to the prior art, or all or part of the technical solution, can be embodied in the form of a software product. This computer software product is stored in a storage medium and includes multiple instructions to cause a computer device (which may be a personal computer, server, or network device, etc.) to execute all or part of the steps of the methods of the various embodiments of this application. The aforementioned storage medium includes various media capable of storing programs, such as USB flash drives, portable hard drives, read-only memory (ROM), random access memory (RAM), magnetic disks, or optical disks.

[0115] The preferred embodiments of the present application have been described above with reference to the accompanying drawings, but this does not limit the scope of the claims of the present application. Any modifications, equivalent substitutions, and improvements made by those skilled in the art without departing from the scope and substance of the embodiments of the present application shall be within the scope of the claims of the present application.

Claims

1. A waveform-layout segmented adhesive fiber optic sensor for resin flow monitoring, characterized in that, The fiber optic sensor includes: A sensing fiber extending along a preset periodic waveform path; The sensing optical fiber is fixed to the monitored area on the surface of the composite material component under test with several spaced bonding points, so that when the resin flows in the monitored area, the resin flow front comes into contact with the sensing optical fiber.

2. The fiber optic sensor according to claim 1, characterized in that, The preset periodic waveform path can take the form of a continuous and periodically uniform curve, a non-uniform periodic curve, or a variable periodic curve; the continuous and periodically uniform curve can take the form of a sine wave or a cosine wave.

3. The fiber optic sensor according to claim 1, characterized in that, The amplitude of the preset periodic waveform path is set according to the height of the area to be monitored.

4. The fiber optic sensor according to claim 1, characterized in that, The spacing between the bonding points is less than or equal to half the wavelength of the preset periodic waveform path.

5. The fiber optic sensor according to claim 1, characterized in that, The bonding point is located at one or more of the peaks, troughs, and zero points of the preset periodic waveform path.

6. The fiber optic sensor according to claim 1, characterized in that, The number of bonding points is set according to the number and distribution of the peaks, troughs, and zero points of the waveform path.

7. A resin flow monitoring system; characterized in that, The monitoring system includes fiber optic sensors, fiber optic detection modules, and a controller; wherein... The fiber optic sensor includes a sensing fiber extending along a preset periodic waveform path; the sensing fiber is fixed to the monitored area on the surface of the composite material component under test at several spaced bonding points, so that when resin flows in the monitored area, the resin flow front contacts the sensing fiber. The fiber optic detection module is used to transmit a broadband scanning light signal to the object being detected and to receive the feedback signal returned by the object being detected. The controller is used to control the optical fiber detection module to transmit optical signals to the sensing optical fiber in the optical fiber sensor and receive the feedback signals returned by the sensing optical fiber to generate a signal to be demodulated; the feedback signals returned by the sensing optical fiber are either backscattered signals returned by the sensing optical fiber or reflected wavelength signals of each fiber grating in the sensing optical fiber; the signal to be demodulated characterizes the response of the sensor before and after the resin flow front comes into contact with the sensing optical fiber; based on the analysis of the signal to be demodulated, the resin flow in the area to be monitored is determined according to the analysis results.

8. The monitoring system according to claim 7, characterized in that, When the feedback signal returned by the sensing fiber is a backscattered signal returned by the sensing fiber, the controller controls the fiber detection module to transmit an optical signal to the sensing fiber in the fiber sensor and receive the feedback signal returned by the sensing fiber to generate the signal to be demodulated, the process including: The optical fiber detection module is controlled to transmit optical signals to the sensing optical fiber in the optical fiber sensor. Before the resin is injected into the area to be monitored, the optical fiber detection module is controlled to receive the backscattered signal of the sensing optical fiber and record the reference signal. When the resin flows in the area to be monitored, the signal abrupt change point and its time in the backscattered signal of the sensing optical fiber are identified according to the reference signal, and the demodulated signal is obtained based on the identification result.

9. The monitoring system according to claim 8, characterized in that, The process by which the controller analyzes the signal to be demodulated and determines the resin flow in the monitored area based on the analysis results includes: Based on the demodulated signal, several signal abrupt change points and their corresponding occurrence times in the backscattered signal of the sensing optical fiber when the resin flows in the monitored area are determined. Based on several signal abrupt change points and their corresponding occurrence times, the several signal abrupt change points are connected and fitted on a two-dimensional plane to obtain a continuous profile of the resin flow front. The resin flow conditions in the monitored area are determined by analyzing the continuous profile of the resin flow front.

10. The monitoring system according to claim 7, characterized in that, The system further includes several adjacent sensing grid areas disposed in the area to be monitored; the sensing grid areas include a first grid area and a second grid area; the first grid area is disposed at the trough of the preset periodic waveform path; the second grid area is disposed at the peak of the preset periodic waveform path; the controller is further configured to perform the following steps: When the resin flows in the area to be monitored, the strain response generated by the sensing optical fiber at several of the sensing grating regions is acquired. The strain response generated by the sensing optical fiber at adjacent first and second grating regions is analyzed, and the resin flow direction between the adjacent first and second grating regions is determined based on the analysis results, so as to determine the resin flow direction in the area to be monitored.