A research and development method and system for corrosion-resistant automotive fasteners
By collecting data on the vehicle assembly location and compatible models, and combining multi-factor coupled tests on vibration characteristics, temperature and humidity, and corrosive environment, the fastener design was optimized, solving the corrosion failure problem of fasteners in actual use and reducing the failure risk in the later stages of research and development.
Patent Information
- Application Number
- CN202611382192.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-08
- Publication Date
- 2026-11-17
AI Technical Summary
In the current research and development of automotive fasteners, the risk of failure is high due to the coupling of multiple factors. Traditional single-condition testing cannot effectively reduce the probability of corrosion failure of fasteners in actual use.
Data on the vehicle assembly location and compatible models were collected. A finite element simulation model was established for preliminary optimization, taking into account vibration characteristics, temperature and humidity environment, and corrosion environment. Data was obtained through multi-factor coupling tests, and the structural design was iteratively optimized to meet the corrosion resistance performance indicators.
By identifying potential corrosion failure risks in advance during the R&D phase and optimizing through multiple rounds of iterations, the risk of fastener failure due to corrosion after mass production can be reduced, thereby improving design accuracy and adaptability.
Smart Images

Figure CN123116451A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of fastener research and development technology, and in particular to a research and development method and system based on corrosion-resistant automotive fasteners. Background Technology
[0002] Fastener R&D refers to the entire process of innovation and development, from concept to mass production, for mechanical parts such as bolts, screws, nuts, and washers that serve to connect and fix. Automotive fastener R&D primarily focuses on high-strength bolts, studs, nuts, and matching anti-loosening connectors for key components such as powertrains, chassis load-bearing systems, body safety connections, and new energy batteries and motors.
[0003] Currently, when improving and developing automotive fasteners, the general process involves first defining technical specifications based on operating conditions, then selecting options for materials, structures, and processes. Finite element simulation is then used to virtually verify strength, fatigue, and loosening risks. The structure is optimized based on the simulation results, and small-batch samples are prepared through mold and process development. Multi-dimensional performance tests, including dimensional physicochemical properties, torque, fatigue vibration, and corrosion, are conducted, along with on-machine assembly verification. Root cause analysis is performed on the failures exposed by the tests, and the structure, materials, or processes are iteratively optimized and the simulation trial production process is repeated. Once all indicators meet the standards, the drawings, processes, and inspection specifications are solidified, and the fastener product is finally finalized and the project is completed.
[0004] When developing automotive fasteners, standardized single-condition tests are generally used to test multiple dimensions of performance such as dimensional physicochemical properties, torque, fatigue vibration, and corrosion. However, in actual vehicle use, multiple factors can easily be coupled, resulting in a higher probability of failure after the development is completed. Summary of the Invention
[0005] To reduce the probability of failure after the development of automotive fasteners, this invention provides a development method and system based on corrosion-resistant automotive fasteners.
[0006] In a first aspect, the present invention provides a research and development method for corrosion-resistant automotive fasteners, employing the following technical solution: A research and development method for corrosion-resistant automotive fasteners includes: Collect the vehicle assembly location of the fastener to be developed and the corresponding compatible vehicle models; Vibration characteristics, temperature and humidity environment, and corrosive environment are determined based on the vehicle model to be adapted; Based on the assembly location of the vehicle, the structure of the fastener to be developed is selected to obtain a structural selection scheme; A finite element simulation model of the fastener is established based on the structural selection scheme to conduct simulation analysis of structural strength and connection performance. The structural selection scheme is then optimized and adjusted based on the simulation results to obtain an optimized structural scheme. Based on the structural optimization scheme, prototypes were fabricated to obtain fastening test pieces; Multi-factor coupled tests were conducted on the fastening test specimens based on vibration characteristics, temperature and humidity environment, and corrosion environment, and multi-factor test data were obtained. The structural optimization scheme is iteratively optimized based on multi-factor test data until the preset anti-corrosion performance index is met, and the finalized structural scheme is obtained. Production is carried out based on a structural design scheme to obtain the final fastener product.
[0007] By adopting the above technical solution, data on the vehicle assembly location and compatible models can be collected to accurately match the vibration characteristics, temperature and humidity environment, and corrosion environment of the fasteners at that location. Then, preliminary optimization is completed through finite element simulation, followed by multi-factor coupling tests on physical samples. This allows the corrosion environment of fasteners under the combined effect of multiple factors during actual service to be reproduced during the R&D stage. Compared with traditional single-condition tests, this is more in line with real-world usage scenarios, thereby identifying potential corrosion failure risks in advance. Through multiple rounds of iterative optimization, the solution can meet corrosion performance requirements, ultimately effectively reducing the probability of fastener failure due to corrosion after mass production and use.
[0008] Optionally, multi-factor coupled tests are conducted on the fastened test specimens based on vibration characteristics, temperature and humidity environment, and corrosion environment, and the multi-factor test data are obtained, including: Based on the vehicle assembly location, combined with vibration characteristics, temperature and humidity environment, and corrosion environment, vibration factor threshold, temperature and humidity factor threshold, and corrosion factor threshold are obtained respectively. A multi-factor coupled test scheme was constructed based on the threshold values of vibration, temperature and humidity, and corrosion. According to the multi-factor coupling test scheme, benchmark tests under the individual effects of each factor and coupling tests under the combined effects of at least two factors were conducted. Record the time when the protective layer first corrosion appears, the time when the protective layer corrosion reaches the preset area ratio, and the time when the base metal begins to corrode under each benchmark test and coupling test, and use these as the initial corrosion time, intermediate corrosion time, and late corrosion time, respectively. Images of the fastened test specimens were acquired based on the initial corrosion time, intermediate corrosion time, and late corrosion time, and were used as initial corrosion images, intermediate corrosion images, and late corrosion images, respectively. The data were combined based on the initial corrosion time, intermediate corrosion time, late corrosion time, initial corrosion images, intermediate corrosion images, and late corrosion images, and used as multi-factor experimental data.
[0009] By adopting the above technical solution, basic data of different corrosion stages are first obtained through single-factor benchmark tests, and then multi-factor joint coupling tests are carried out. This allows for a direct comparison of the impact of multiple factors on the corrosion process of fasteners. At the same time, by combining time data and image data, the corrosion resistance performance of fasteners under different test conditions can be fully characterized from both time and morphology dimensions, providing comprehensive and accurate data support for subsequent scheme optimization.
[0010] Optional methods for determining the structural design scheme include: The coupling effect coefficient was determined by combining the initial corrosion time, intermediate corrosion time, and late corrosion time under various benchmark tests and coupled tests. The changes in corrosion resistance were determined by combining images of initial corrosion, intermediate corrosion, and late corrosion. The corrosion protection reference value is determined based on the coupling effect coefficient and the corrosion protection change. When the anti-corrosion reference value does not meet the preset anti-corrosion performance index, the type of structural adjustment and the structural adjustment parameters are determined based on the comparison between the anti-corrosion reference value and the preset anti-corrosion performance index. The structural adjustment scheme is determined by combining the type of structural adjustment, structural adjustment parameters and structural optimization scheme, and the sample is re-produced based on the structural adjustment scheme; When the anti-corrosion reference value meets the preset anti-corrosion performance index, the structural adjustment scheme will be used as the structural finalization scheme.
[0011] By adopting the above technical solutions, the coupling effect coefficient and corrosion resistance changes are determined respectively, thereby quantifying the influence of multi-factor coupling on the corrosion resistance of fasteners. Combined with the analysis results of corrosion morphology changes, it is possible to more accurately determine whether the current design scheme meets the corrosion resistance requirements under actual working conditions. If it does not meet the requirements, the design parameters can be adjusted and the prototype can be re-tested and verified. Through iterative optimization, the preset performance requirements can be gradually approached, and finally a finalized scheme that meets the actual service requirements can be obtained, thus improving the accuracy of corrosion resistance design from the R&D process.
[0012] Optional methods for determining the coupling effect coefficient include: The initial corrosion time, intermediate corrosion time, and late corrosion time under the benchmark test are defined as the initial benchmark time, intermediate benchmark time, and late benchmark time, respectively. The initial corrosion time, intermediate corrosion time, and final corrosion time under the coupling test are defined as the initial coupling time, intermediate coupling time, and final coupling time, respectively. The initial offset coefficient is calculated based on the initial coupling time and the initial reference time; the intermediate offset coefficient is calculated based on the intermediate coupling time and the intermediate reference time; and the later offset coefficient is calculated based on the later coupling time and the later reference time. The comprehensive coupling estimate is determined by combining the initial offset coefficient, the intermediate offset coefficient, and the later offset coefficient, and the comprehensive coupling estimate is used as the coupling effect coefficient.
[0013] By adopting the above technical solution, defining the reference time and coupling time for each stage, and then determining the initial offset coefficient, the intermediate offset coefficient, and the later offset coefficient, the comprehensive coupling estimate is determined and used as the coupling effect coefficient. This can intuitively reflect the degree to which the coupling effect of multiple factors accelerates the corrosion process compared to the effect of a single factor, making it easier to obtain accurate anti-corrosion reference values in the future.
[0014] Optional methods for determining the comprehensive coupled estimate include: Determine the stage weighting coefficients based on the vehicle model and the location of the fastening requirements; The initial weight coefficient, the intermediate weight coefficient, and the later weight coefficient are retrieved based on the stage weight coefficient. Calculate the product of the initial offset coefficient and the initial weight coefficient and use it as the initial weighting value; Calculate the product between the intermediate offset coefficient and the intermediate weight coefficient, and use it as the intermediate weighted value; Calculate the product between the later offset coefficient and the later weight coefficient, and use it as the later weighting value; The sum of the initial weighted value, the intermediate weighted value, and the later weighted value is calculated and used as the comprehensive coupled estimate.
[0015] By adopting the above technical solution, and considering the different tolerance requirements of different vehicle models and different assembly positions for the corrosion stage, differentiated weighting coefficients are introduced to weight the offset coefficients of each stage. This allows the final comprehensive coupling estimate to better fit the needs of actual service scenarios, further improving the accuracy of the quantitative characterization of the coupling effect and providing a more reliable data foundation for subsequent corrosion resistance performance assessment.
[0016] Optional methods for determining stage weight coefficients include: Determine the failure priority of corrosion protection performance based on the location of fastening requirements; The initial coefficients for the initial stage, the initial coefficients for the intermediate stage, and the initial coefficients for the later stage are determined based on the failure priority. Determine the initial model preference coefficient, the mid-term model preference coefficient, and the late-term model preference coefficient based on the vehicle model; Calculate the product between the initial coefficient and the initial coefficient of model preference, and use it as the initial weighting coefficient; Calculate the product between the initial mid-term coefficient and the mid-term model preference coefficient, and use it as the mid-term weighting coefficient; Calculate the product between the initial coefficients and the model preference coefficients in the later stage, and use it as the later weighting coefficient. The initial, intermediate, and later weight coefficients are combined and used as the stage weight coefficients.
[0017] By adopting the above technical solution, the priority of the impact of corrosion failure on the operation of the whole vehicle is first determined by combining the safety level of the fastener assembly position. Then, the coefficient weight of each corrosion stage is adjusted according to the vehicle model. This can adapt to the personalized anti-corrosion needs of different models and different positions, so that the final weight coefficient is more in line with the actual R&D positioning, and further improve the adaptability of the entire R&D process to actual working conditions.
[0018] Optional methods for determining changes in corrosion resistance include: Based on the comparison between the initial corrosion image and the intermediate corrosion image, the location points of intermediate changes and the area values of intermediate changes are determined; Based on the comparison between the intermediate and late erosion images, the location points and area values of the late changes are determined; Calculate the vector distance between the intermediate-term change location point and the later-term change location point and use it as the change location distance value; Calculate the ratio between the mid-term and late-term area changes and use it as the area change ratio. The changes in location distance and the changes in area ratio are combined to represent the changes in corrosion resistance.
[0019] By adopting the above technical solution and comparing and analyzing corrosion images at different stages, the extension and expansion of corrosion sites and the growth of corrosion area during the corrosion process can be quantified into specific data. This clearly and intuitively presents the development law of fastener corrosion under the coupled effect of multiple factors. Compared with judging the degree of corrosion solely based on time points, this approach increases the consideration of corrosion morphology changes, making the characterization of corrosion resistance more comprehensive and further improving the accuracy of the final performance judgment.
[0020] Optional methods for determining corrosion protection reference values include: Determine the coupling distinguishing factors based on the coupling effect coefficient; Determine the reference weights of factors based on the coupling differentiation factors; Based on the changes in corrosion resistance, retrieve the distance values of the changed locations and the ratio values of the changed areas; The distance value of the changed location and the ratio of the changed area are calculated based on the reference weight of the factors, and the calculation results are used as the reference value for corrosion prevention.
[0021] By adopting the above technical solution, the coupling effect coefficient is used to retrieve the coupling differentiation factors to determine the reference weight of the factors. Then, the quantitative data of corrosion location expansion rate and corrosion area growth ratio are combined for weighted calculation. The final anti-corrosion reference value can take into account the influence of multiple factors coupling and the actual corrosion development characteristics. This further improves the scientificity and accuracy of anti-corrosion performance judgment and provides a more reliable decision-making basis for subsequent structural adjustment and optimization.
[0022] Optional methods for constructing multi-factor coupled experimental schemes include: The vibration reference value, temperature and humidity reference value, and corrosion factor reference value are determined according to the vehicle model to be adapted; The vibration coupling value is determined by comparing the vibration reference value with the vibration factor threshold. The temperature and humidity coupling value is determined by comparing the temperature and humidity reference values with the temperature and humidity factor thresholds. The corrosion coupling value is determined by comparing the reference values and threshold values of corrosion factors. Based on the comparison results of vibration coupling value, temperature and humidity coupling value and corrosion coupling value with the preset coupling reference value, the coupling selection scheme is determined and the coupling selection scheme is used as the multi-factor coupling test scheme.
[0023] By adopting the above technical solution, vibration reference values, temperature and humidity reference values, and corrosion factor reference values are determined for the actual service environment of different compatible vehicle models, and then compared and screened with the corresponding thresholds. This allows for flexible adjustment of the combination of factors in the coupled test according to the severity of the actual working conditions, thereby simplifying the test process under low-severity conditions, reducing R&D costs, and ensuring the comprehensiveness of test coverage under high-severity conditions, further improving the adaptability and pertinence of the multi-factor coupled test scheme.
[0024] Secondly, the present invention provides a research and development system based on corrosion-resistant automotive fasteners, employing the following technical solution: A research and development system based on corrosion-resistant automotive fasteners includes: The data acquisition module is used to collect information on the vehicle assembly location and compatible vehicle models. The memory stores a program for implementing a research and development method for corrosion-resistant automotive fasteners as described in any one of the first aspects; The processor loads and executes programs stored in memory.
[0025] In summary, the present invention has at least one of the following beneficial technical effects: 1. By collecting data on the assembly location and compatible vehicle models, the vibration characteristics, temperature and humidity environment, and corrosion environment of the fasteners at that location can be accurately matched. Then, preliminary optimization is completed through finite element simulation, followed by multi-factor coupling tests on physical samples. This allows the corrosion environment of fasteners under the combined effect of multiple factors during actual service to be reproduced during the R&D stage. Compared with traditional single-condition tests, this is more in line with real-world usage scenarios, thereby identifying potential corrosion failure risks in advance. Through multiple rounds of iterative optimization, the solution can meet the corrosion performance requirements, ultimately effectively reducing the probability of fastener failure due to corrosion after mass production and use. 2. First, basic data of different corrosion stages are obtained through single-factor benchmark tests. Then, multi-factor joint coupling tests are carried out to intuitively compare the influence of multiple factors on the corrosion process of fasteners. At the same time, by combining time data and image data, the corrosion resistance performance of fasteners under different test conditions can be fully characterized from the time dimension and morphology dimension, providing comprehensive and accurate data support for subsequent scheme optimization. 3. For the actual service environment of different compatible vehicle models, vibration reference values, temperature and humidity reference values, and corrosion factor reference values are determined and then compared with the corresponding thresholds for screening. This allows for flexible adjustment of the combination of factors in the coupled test according to the severity of the actual working conditions, thereby simplifying the test process under low-severity conditions, reducing R&D costs, and ensuring comprehensive test coverage under high-severity conditions, further improving the adaptability and relevance of the multi-factor coupled test scheme. Attached Figure Description
[0026] Figure 1 This is a flowchart of the research and development methodology for corrosion-resistant automotive fasteners; Figure 2 This is a flowchart of a method for conducting multi-factor coupled tests on fastened test specimens based on vibration characteristics, temperature and humidity environment, and corrosion environment, and obtaining multi-factor test data; Figure 3 This is a flowchart illustrating the construction method of a multi-factor coupled experimental scheme; Figure 4 This is a schematic diagram illustrating the overall R&D steps for corrosion-resistant automotive fasteners. Detailed Implementation
[0027] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments.
[0028] Reference Figure 1 This invention discloses a research and development method for corrosion-resistant automotive fasteners, comprising: S100: Collect the vehicle assembly location of the fastener to be developed and the corresponding compatible vehicle models.
[0029] Among them, the vehicle assembly location refers to the fixed installation point of the fastener to be developed on the vehicle. The vehicle assembly location includes installation areas with different corrosion risk levels, such as chassis suspension, engine block, battery pack housing, and exhaust pipe.
[0030] The compatible vehicle model refers to the vehicle model that the fastener to be developed will be equipped with. Different vehicle models correspond to different vehicle usage environments, road profiles and anti-corrosion design standards.
[0031] The vehicle assembly location and compatible models are collected synchronously from the vehicle parts BOM, vehicle 3D assembly drawings, and vehicle environmental condition files, serving as the basic input data for subsequent condition analysis and structural selection.
[0032] S101: Determine the vibration characteristics, temperature and humidity environment, and corrosive environment based on the vehicle model to be adapted.
[0033] Vibration characteristics refer to the vibration effects experienced by the fasteners during vehicle operation, including road impact vibration amplitude, alternating vibration frequency, and duration of continuous vibration. Temperature and humidity environment refers to the temperature and humidity ranges in which the fasteners operate within the vehicle's service life. Corrosive environment refers to the chemical and electrochemical factors that cause corrosion that the fasteners encounter during vehicle service. Corrosive environment includes the duration of immersion in mud and water, and the duration of contact with acidic or alkaline chemical media.
[0034] By inputting the compatible vehicle models into a preset vehicle model database, the system obtains the road impact vibration amplitude, alternating vibration frequency, continuous vibration duration, temperature range, humidity range, mud and water immersion duration, and acid and alkali chemical medium contact duration corresponding to the sold vehicles of the compatible models. Then, the average values of each road impact vibration amplitude, alternating vibration frequency, and continuous vibration duration are calculated and combined to form the vibration characteristics. The average values of each temperature range and humidity range are calculated and combined to form the temperature and humidity environment. The average values of each mud and water immersion duration and acid and alkali chemical medium contact duration are calculated and combined to form the corrosion environment.
[0035] The vehicle model database pre-stores the road impact vibration amplitude, alternating vibration frequency, continuous vibration duration, temperature range, humidity range, mud and water immersion duration, and acid and alkali chemical medium contact duration for sold vehicles of different compatible models. The vehicle model database is obtained after the operator pre-inputs the data.
[0036] S102: Select the structure of the fastener to be developed based on the assembly location of the vehicle to obtain a structural selection scheme.
[0037] Among them, the structural selection scheme refers to the complete combination of technical parameters formed after the structural selection decision. The structural selection scheme includes a series of technical specifications such as the geometric dimensions of fasteners, material grade, mechanical performance grade, surface treatment type and coating thickness requirements.
[0038] The type of fastener to be developed is determined based on its assembly location on the vehicle. The type of fastener to be developed includes chassis parts, powertrain parts, body parts, or interior and exterior trim parts. The type of fastener to be developed is then entered into a preset type selection database to obtain a structural selection scheme.
[0039] The type selection database pre-stores different types of fasteners to be developed and their corresponding structural selection schemes. The type selection database is pre-set by the operator according to the general selection rules of the automotive fastener industry.
[0040] S103: Establish a finite element simulation model of the fastener based on the structural selection scheme to conduct simulation analysis of structural strength and connection performance, and optimize and adjust the structural selection scheme according to the simulation results to obtain the structural optimization scheme.
[0041] Among them, the finite element simulation model refers to the numerical calculation model formed by discretizing the geometry of the fastener into a finite number of element meshes and assigning material constitutive relations, boundary conditions, and load conditions to each element. The structural optimization scheme refers to the improved technical solution combination formed by adjusting the geometric dimensions, material parameters, or thread parameters in the initial structural selection scheme based on the simulation analysis results.
[0042] The 3D geometric model of the fasteners in the structural selection scheme is imported into finite element preprocessing software. The fastener entity is meshed using tetrahedral or hexahedral elements. Local mesh refinement is performed in stress concentration areas such as the thread root and head transition fillets. The fastener material is assigned the corresponding elastic modulus, Poisson's ratio, and elastoplastic constitutive model. Simultaneously, a contact pair with the connected parts is established, and the friction coefficient is defined. Preload and external working loads are applied, thus forming a complete finite element simulation model. The finite element simulation model is then analyzed, and the optimization direction is determined based on the specific stress distribution in the simulation results. Adjustments are made to the geometric dimensions, material parameters, or thread parameters to obtain the optimized structural scheme.
[0043] S104: Prototype preparation is carried out according to the structural optimization scheme to obtain fastening test pieces.
[0044] Among them, fastening test pieces refer to physical samples of fasteners that have been obtained after the sample preparation is completed, and whose various geometric dimensions and mechanical properties have been tested and confirmed to meet the design indicators of the structural optimization scheme.
[0045] By distributing the two-dimensional engineering drawings of fasteners in the structural optimization scheme to the prototype workshop, materials are selected according to the drawing requirements for production and surface treatment to obtain physical samples. The key dimensions of the physical samples are then tested to ensure that they meet the tolerance requirements of the engineering drawings. The physical samples that pass the inspection are the fastening test pieces.
[0046] S105: Conduct multi-factor coupled tests on fastened test specimens based on vibration characteristics, temperature and humidity environment, and corrosion environment, and obtain multi-factor test data.
[0047] Among them, multi-factor coupling test refers to an accelerated testing method that applies vibration load, temperature and humidity environment and corrosion environment individually or in combination to the fastening test piece to simulate the failure behavior and performance degradation law of fasteners when subjected to multiple environmental and mechanical factors during the actual service of the vehicle.
[0048] Multifactor test data refers to the sum of various original records and test results collected from the fastened test specimens during and after the multifactor coupling test.
[0049] By considering vibration characteristics, temperature and humidity environment, and corrosion environment as factors in a multi-factor coupled test, and conducting tests on fastened test specimens, the data collected during the test process are used as multi-factor test data for convenient subsequent use.
[0050] S106: Based on multi-factor test data, the structural optimization scheme is iteratively optimized until the preset anti-corrosion performance index is met, and the finalized structural scheme is obtained.
[0051] Among them, the corrosion resistance performance index refers to the quantitative judgment standard pre-set during the R&D initiation phase based on the corrosion resistance and durability requirements of the applicable vehicle model. The corrosion resistance performance index is obtained after being pre-input by the operator.
[0052] The structural finalization scheme refers to the technical solution formed by the combination of structural parameters, material parameters and process parameters when the results of multi-factor coupling tests corresponding to a certain round of structural optimization scheme fully meet the requirements.
[0053] The structural optimization scheme is iteratively optimized using multi-factor experimental data, and each optimized scheme is compared with the preset anti-corrosion performance index. When the preset anti-corrosion performance index is met, the scheme corresponding to this optimization is taken as the finalized structural scheme.
[0054] S107: Production is carried out based on the structural design scheme to obtain the final fastener product.
[0055] In this process, mass production is carried out according to the structural design plan to obtain the final fastener product. This allows potential corrosion failure risks to be identified in advance during the research and development phase. Through multiple rounds of iterative optimization, the design can meet the corrosion performance requirements, and ultimately the probability of corrosion failure after the fastener is put into mass production and use can be effectively reduced.
[0056] To further ensure the rationality of conducting multi-factor coupled tests on fastening test specimens based on vibration characteristics, temperature and humidity environment, and corrosive environment, and to obtain multi-factor test data, it is necessary to perform further separate analysis and calculation on the multi-factor coupled tests on fastening test specimens based on vibration characteristics, temperature and humidity environment, and corrosive environment, and to obtain multi-factor test data. The specific steps are explained in detail below.
[0057] Reference Figure 2 The following steps were taken to conduct multi-factor coupled tests on the fastened test specimens based on vibration characteristics, temperature and humidity environment, and corrosion environment, and to obtain multi-factor test data: S200: Based on the vehicle assembly location, vibration factor thresholds, temperature and humidity factor thresholds, and corrosion factor thresholds are obtained by combining vibration characteristics, temperature and humidity environment, and corrosion environment.
[0058] Among them, the vibration factor threshold refers to the upper limit boundary value of the vibration parameter in the multi-factor coupled test. The temperature and humidity factor threshold refers to the upper limit boundary value of the temperature and humidity parameter in the multi-factor coupled test. The corrosion factor threshold refers to the upper limit boundary value of the corrosion parameter in the multi-factor coupled test.
[0059] The system obtains vibration, temperature and humidity, and corrosion adjustment coefficients by inputting the vehicle assembly position into a preset position adjustment database. Then, it retrieves the road impact vibration amplitude, alternating vibration frequency, and duration of continuous vibration from the vibration characteristics to calculate the root mean square (RMS) value of acceleration. The product of the RMS value and the vibration adjustment coefficient is used as the vibration factor threshold. Temperature and humidity ranges are retrieved from the temperature and humidity environment, along with their endpoints and spans. These are input into a preset range conversion formula to obtain range conversion values. The temperature and humidity range conversion values are then adjusted according to the temperature and humidity adjustment coefficients, resulting in adjusted temperature and humidity range conversion values, which are used as the temperature and humidity factor thresholds. Finally, the immersion time in mud and water and the contact time with acidic or alkaline chemical media are multiplied by the corrosion adjustment coefficient, and the results are used as the corrosion factor threshold.
[0060] The position adjustment database pre-stores a table showing the correspondence between different vehicle assembly positions and their corresponding vibration adjustment coefficients, temperature and humidity adjustment coefficients, and corrosion adjustment coefficients. The database is retrieved after pre-input by the operator. The higher the vibration level of a vehicle assembly position, the smaller the vibration adjustment coefficient; the higher the temperature and humidity level of the corresponding assembly position, the smaller the temperature and humidity adjustment coefficient; and the easier the corrosion contact at the corresponding assembly position, the smaller the corrosion adjustment coefficient.
[0061] The interval conversion formula is: Interval conversion value = smaller end value * A + larger end value * B + span value * C, where A, B, and C are their respective conversion coefficients and are preset by the operator.
[0062] S201: Construct a multi-factor coupled test scheme based on the threshold values of vibration factor, temperature and humidity factor, and corrosion factor.
[0063] Among them, the multi-factor coupling test scheme refers to the test scheme required after combining and arranging vibration, temperature, humidity and corrosion factors.
[0064] By analyzing the threshold values of vibration, temperature and humidity, and corrosion, benchmark tests for vibration, temperature and humidity, and corrosion, as well as coupled tests under the combined effect of at least two factors, were constructed, and a multi-factor coupled test scheme was obtained.
[0065] A benchmark test refers to a test conducted under the individual effects of vibration, temperature and humidity, and corrosion. A coupled test refers to a test conducted under the combined effects of at least two of these factors.
[0066] S202: Conduct benchmark tests under the individual effects of each factor and coupled tests under the combined effects of at least two factors, according to the multi-factor coupling test scheme.
[0067] In this process, the benchmark and coupled tests in the multi-factor coupling test scheme are retrieved, and then the tests are carried out according to the benchmark and coupled tests respectively, which facilitates subsequent data collection.
[0068] S203: Record the time when the protective layer first corrodes, the time when the protective layer corrosion reaches the preset area ratio, and the time when the base metal begins to corrode under each benchmark test and coupling test, and use these as the initial corrosion time, intermediate corrosion time, and late corrosion time, respectively.
[0069] The initial corrosion time refers to the time when the protective layer begins to corrode on the fastened test specimen. The intermediate corrosion time refers to the time when the protective layer corrosion reaches a predetermined area proportion. The late corrosion time refers to the time when the base metal begins to corrode.
[0070] The initial corrosion time, intermediate corrosion time, and late corrosion time under various benchmark tests and coupled tests are recorded for future use.
[0071] S204: Images of the fastened test specimens were acquired based on the initial corrosion time, intermediate corrosion time, and late corrosion time, and were used as initial corrosion images, intermediate corrosion images, and late corrosion images, respectively.
[0072] The initial corrosion image refers to the image corresponding to the initial corrosion time of the fastened test specimen. The intermediate corrosion image refers to the image corresponding to the intermediate corrosion time of the fastened test specimen. The late corrosion image refers to the image corresponding to the late corrosion time of the fastened test specimen.
[0073] Images of the fastened test specimens were acquired by pre-set image acquisition devices at the sites corresponding to the benchmark test and the coupling test at the initial corrosion time, intermediate corrosion time and late corrosion time, respectively, so as to obtain the initial corrosion image, intermediate corrosion image and late corrosion image, which are convenient for subsequent use.
[0074] S205: The data is based on a combination of initial corrosion time, intermediate corrosion time, late corrosion time, initial corrosion image, intermediate corrosion image, and late corrosion image, and is used as multi-factor experimental data.
[0075] The dataset is created by combining the initial corrosion time, intermediate corrosion time, late corrosion time, initial corrosion image, intermediate corrosion image, and late corrosion image, and serves as multi-factor experimental data for convenient subsequent use.
[0076] To further ensure the rationality of the structural design scheme, it is necessary to conduct further separate analysis and calculations on the structural design scheme, which will be explained in detail through the steps shown below.
[0077] The method for determining the structural design scheme includes the following steps: S300: Determine the coupling effect coefficient by combining the initial corrosion time, intermediate corrosion time, and late corrosion time under various benchmark tests and coupling tests.
[0078] The coupling effect coefficient is a numerical index that quantifies the degree and direction of the interactive influence of vibration, temperature, humidity and corrosion factors on the corrosion process of fasteners when they act together.
[0079] By combining and analyzing the initial corrosion time, intermediate corrosion time, and late corrosion time under various benchmark tests and coupled tests, the coupling effect coefficient is determined for convenient subsequent use.
[0080] S301: Determine the changes in corrosion resistance by combining initial corrosion images, intermediate corrosion images, and late corrosion images.
[0081] Among them, the corrosion change refers to a comprehensive set of parameters that describe the spatial evolution of the protective layer and the substrate of the fastened test piece during the corrosion process.
[0082] By combining and analyzing images of initial corrosion, intermediate corrosion, and late corrosion, the changes in corrosion resistance can be determined, facilitating subsequent use.
[0083] S302: Determine the corrosion protection reference value based on the coupling effect coefficient and the corrosion protection change.
[0084] Among them, the corrosion protection reference value refers to a comprehensive index parameter that quantifies the combined effect of multiple factors on the corrosion process and its spatial expansion and evolution.
[0085] By combining the analysis of the coupling effect coefficient with the changes in corrosion resistance, a reference value for corrosion resistance can be determined to facilitate subsequent use.
[0086] S303: When the anti-corrosion reference value does not meet the preset anti-corrosion performance index, the type of structural adjustment and the structural adjustment parameters shall be determined based on the comparison between the anti-corrosion reference value and the preset anti-corrosion performance index.
[0087] Among them, structural adjustment types refer to the classification of different types of technical parameters in the structural optimization scheme that are adjusted to improve corrosion resistance when the corrosion resistance reference value does not meet the preset index. Structural adjustment types include geometric structure adjustment, material structure adjustment, and surface treatment structure adjustment. Structural adjustment parameters refer to the target values for adjusting the structural adjustment type.
[0088] When the anti-corrosion reference value is greater than the preset anti-corrosion performance index, it indicates that the test results of the fastening test piece do not meet the requirements and the test needs to be continued. Therefore, the difference between the anti-corrosion reference value and the preset anti-corrosion performance index is calculated and used as a reference deviation value. Then, the corrosion propagation direction is determined by the anti-corrosion change. The reference deviation value and the corrosion propagation direction are then input into the preset structural adjustment database to match and obtain the structural adjustment type and type adjustment benchmark value. Finally, the product value between the reference deviation value and the type adjustment benchmark value is calculated and used as the structural adjustment parameter.
[0089] The structural adjustment database pre-stores a table showing different reference deviation values, corrosion propagation directions, corresponding structural adjustment types, and adjustment benchmark values. The structural adjustment database is obtained after the operator pre-inputs the data.
[0090] For example, the structural adjustment database can store the following: If the corrosion propagation direction shows that corrosion preferentially starts from the outer edge of the flange face and extends radially inward, with a reference deviation value between 0.05 and 0.15, then the corresponding structural adjustment type is to increase the outer diameter of the flange face or increase the thickness of the flange face edge, with the adjustment benchmark value being an increase in outer diameter of 2 mm or an increase in thickness of 1 mm. If the corrosion propagation direction shows that corrosion starts at the root of the thread and extends along the side of the thread to the crest, with a reference deviation value between 0.10 and 0.20, then the corresponding structural adjustment type is to increase the coating thickness, with the adjustment benchmark value being an increase in thickness of 2 μm. If the corrosion protection reference value is greater than 0.2, then the corresponding structural adjustment type is to replace the base material with one with a higher corrosion resistance, with the adjustment benchmark value being an increase in the material's corrosion resistance level by one grade.
[0091] S304: Determine the structural adjustment scheme by combining the type of structural adjustment, structural adjustment parameters and structural optimization scheme, and re-produce the sample according to the structural adjustment scheme.
[0092] Among them, the structural adjustment scheme refers to a complete set of technical parameters used to guide the next round of sample production.
[0093] By using the current structural optimization scheme as a basic template, and then mapping the determined structural adjustment types and corresponding structural adjustment parameters one by one to the corresponding parameter items in the template, the original values in the template are overwritten or modified, while all parameter items not involved in the adjustment are retained unchanged, forming an updated complete parameter list, thereby obtaining the structural adjustment scheme. Then, the sample is re-produced according to the structural adjustment scheme, and the test is carried out again.
[0094] S305: When the anti-corrosion reference value meets the preset anti-corrosion performance index, the structural adjustment scheme shall be used as the structural finalization scheme.
[0095] When the anti-corrosion reference value is not greater than the preset anti-corrosion performance index, it means that the test results of the fastening test piece meet the requirements and no further testing is needed. Therefore, the structural adjustment scheme at this time is directly used as the structural finalization scheme.
[0096] To further ensure the rationality of the coupling effect coefficient, it is necessary to perform a further separate analysis and calculation of the coupling effect coefficient, which will be explained in detail through the steps shown below.
[0097] The method for determining the coupling effect coefficient includes the following steps: S400: Define the initial corrosion time, intermediate corrosion time, and final corrosion time under the benchmark test as the initial benchmark time, intermediate benchmark time, and final benchmark time, respectively.
[0098] The initial reference time refers to the initial corrosion time under the reference test. The intermediate reference time refers to the intermediate corrosion time under the reference test. The late reference time refers to the late corrosion time under the reference test.
[0099] Defining the initial, intermediate, and final reference times facilitates subsequent use.
[0100] S401: Define the initial corrosion time, intermediate corrosion time, and late corrosion time under the coupling test as the initial coupling time, intermediate coupling time, and late coupling time, respectively.
[0101] The initial coupling time refers to the initial corrosion time under the coupling test. The intermediate coupling time refers to the intermediate corrosion time under the coupling test. The late coupling time refers to the late corrosion time under the coupling test.
[0102] Defining the initial coupling time, intermediate coupling time, and late coupling time facilitates subsequent use.
[0103] S402: Calculate the initial offset coefficient based on the initial coupling time and the initial reference time, calculate the intermediate offset coefficient based on the intermediate coupling time and the intermediate reference time, and calculate the late offset coefficient based on the late coupling time and the late reference time.
[0104] The initial offset coefficient is a quantitative proportion reflecting the degree to which the combined effect of multiple factors accelerates or delays the initial stage of corrosion. The intermediate offset coefficient is a quantitative proportion reflecting the degree to which the combined effect of multiple factors accelerates or delays the intermediate stage of corrosion. The late offset coefficient is a quantitative proportion reflecting the degree to which the combined effect of multiple factors accelerates or delays the late stage of corrosion.
[0105] The initial offset coefficient is calculated by taking the difference between the initial coupling time and the initial reference time, and then using the ratio of this difference to the initial reference time. Similarly, the initial offset coefficient is calculated by taking the difference between the intermediate coupling time and the intermediate reference time, and then using the ratio of this difference to the intermediate reference time. Finally, the initial offset coefficient is calculated by taking the difference between the later coupling time and the later reference time.
[0106] S403: Combine the initial offset coefficient, the intermediate offset coefficient and the later offset coefficient to determine the comprehensive coupling estimate, and use the comprehensive coupling estimate as the coupling effect coefficient.
[0107] Among them, the comprehensive coupling prediction value refers to the degree of comprehensive influence of the combined effect of multiple factors in the entire corrosion process.
[0108] By combining the initial offset coefficient, the intermediate offset coefficient, and the later offset coefficient, a comprehensive coupling estimate is determined. This comprehensive coupling estimate is then used as the coupling effect coefficient to improve the accuracy of the obtained coupling effect coefficient.
[0109] To further ensure the rationality of the comprehensive coupling estimate, it is necessary to perform a further separate analysis and calculation on the comprehensive coupling estimate, which will be explained in detail through the steps shown below.
[0110] The method for determining the comprehensive coupled estimate includes the following steps: S500: Determine the stage weighting coefficient based on the vehicle model and the location of the fastening requirement.
[0111] Among them, the stage weight coefficient refers to the weighted allocation coefficient assigned to the initial corrosion stage, the intermediate corrosion stage, and the late corrosion stage respectively when calculating the comprehensive coupling estimate.
[0112] By combining the analysis of vehicle models and the locations of fastening requirements, the stage weight coefficients are determined to facilitate subsequent use.
[0113] S501: Retrieve the initial weight coefficient, intermediate weight coefficient, and late weight coefficient based on the stage weight coefficient.
[0114] The initial weighting coefficient refers to the weighted allocation coefficient assigned to the initial corrosion stage. The intermediate weighting coefficient refers to the weighted allocation coefficient assigned to the intermediate corrosion stage. The late weighting coefficient refers to the weighted allocation coefficient assigned to the late corrosion stage. The stage weighting coefficients include the initial weighting coefficient, the intermediate weighting coefficient, and the late weighting coefficient.
[0115] The initial, intermediate, and later weight coefficients can be retrieved through stage weight coefficients for convenient subsequent use.
[0116] S502: Calculate the product of the initial offset coefficient and the initial weight coefficient and use it as the initial weighting value.
[0117] The initial weighted value refers to the product of the initial offset coefficient and the initial weight coefficient.
[0118] Calculating the initial weighted values facilitates subsequent use.
[0119] S503: Calculate the product between the intermediate offset coefficient and the intermediate weight coefficient and use it as the intermediate weight value.
[0120] The intermediate weighted value refers to the product of the intermediate offset coefficient and the intermediate weight coefficient.
[0121] The intermediate weighted value is calculated to facilitate subsequent use.
[0122] S504: Calculate the product between the later offset coefficient and the later weight coefficient and use it as the later weighting value.
[0123] The later weighted value refers to the product of the later offset coefficient and the later weight coefficient.
[0124] Calculating the weighted values in the later stages makes it easier to use later.
[0125] S505: Calculate the sum of the initial weighted value, the intermediate weighted value, and the later weighted value and use it as a comprehensive coupled estimate.
[0126] Specifically, by calculating the sum of the initial weighted value, the intermediate weighted value, and the later weighted value, and using the calculation result as the comprehensive coupling estimate, the accuracy of the obtained comprehensive coupling estimate is improved.
[0127] To further ensure the rationality of the stage weight coefficients, it is necessary to perform further separate analysis and calculation on the stage weight coefficients, which will be explained in detail through the steps shown below.
[0128] The method for determining the stage weight coefficients includes the following steps: S600: Determine the failure priority of corrosion protection performance based on the location of fastening requirements.
[0129] Among them, failure priority refers to the determination of the importance of different failure modes in the corrosion process based on the specific assembly position of the fastener on the whole vehicle and the severity of its impact on the vehicle's safety and functionality after failure.
[0130] By inputting the fastening requirement location into a preset failure priority database, the failure priority can be matched and obtained for convenient subsequent use.
[0131] The failure priority database pre-stores a table that maps different fastening requirements to their corresponding failure priorities. The failure priority database is retrieved after the operator has pre-entered the information.
[0132] For example, the failure priority database pre-stores: when the fastening requirement is at the location of a safety structural component, the failure priority is mid-to-late stage priority; when the fastening requirement is at the location of a functional accessory, the failure priority is balanced priority; and when the fastening requirement is at the location of a general assembly, the failure priority is early-to-mid stage priority.
[0133] Locations of safety structural components include braking system mounting points, steering knuckle connection points, subframe-body connection points, and suspension control arm ball joint mounting points. Locations of functional accessories include engine mount mounting points, exhaust pipe suspension points, and battery pack housing mounting points. Locations of general assembly parts include interior trim panel mounting points, exterior trim mounting points, and wiring harness bracket mounting points.
[0134] S601: Determine the initial coefficients for the initial stage, the initial coefficients for the intermediate stage, and the initial coefficients for the later stage based on the failure priority.
[0135] The initial coefficient refers to the initial numerical weight assigned to the initial stage of corrosion in the corrosion process. The intermediate initial coefficient refers to the initial numerical weight assigned to the intermediate stage of corrosion in the corrosion process. The late initial coefficient refers to the initial numerical weight assigned to the late stage of corrosion in the corrosion process.
[0136] Different initial coefficients are assigned to the initial, intermediate, and late stages of failure based on the failure priority level, which facilitates subsequent use.
[0137] For example, when the failure priority is mid-to-late stage priority, the corresponding initial coefficient is 0.2 for the initial stage, 0.3 for the mid-stage, and 0.5 for the late stage. When the failure priority is balanced priority, the corresponding initial coefficient is 0.3 for the initial stage, 0.35 for the mid-stage, and 0.35 for the late stage. When the failure priority is early-to-mid stage priority, the corresponding initial coefficient is 0.45 for the initial stage, 0.35 for the mid-stage, and 0.2 for the late stage.
[0138] S602: Determine the initial model preference coefficient, the mid-term model preference coefficient, and the late-term model preference coefficient based on the vehicle model.
[0139] Among them, the initial model preference coefficient refers to the initial model preference weight assigned to the initial corrosion stage of the corrosion process. The intermediate model preference coefficient refers to the initial model preference weight assigned to the intermediate corrosion stage of the corrosion process. The late model preference coefficient refers to the initial model preference weight assigned to the late corrosion stage of the corrosion process.
[0140] By inputting the vehicle model into a preset model preference database, the initial model preference coefficient, the mid-term model preference coefficient, and the late-term model preference coefficient are obtained for convenient subsequent use.
[0141] The model preference database pre-stores a table showing the correspondence between different vehicle models and their corresponding initial, mid-term, and late-term model preference coefficients. The model preference database is obtained after the operator pre-inputs the information.
[0142] For example, when a vehicle model targets a coastal region with high salt spray, the manufacturer pays more attention to all stages of corrosion than ordinary models, and the initial, mid-term, and late-term model preference coefficients are all set to 1. When the vehicle model is a commercial vehicle or a special vehicle with a long expected service life, the OEM is more concerned about the structural integrity after long-term corrosion. In this case, the late-term model preference coefficient is set to 0.95, the initial model preference coefficient is set to 0.75, and the mid-term model preference coefficient is set to 0.75.
[0143] S603: Calculate the product between the initial coefficient and the initial coefficient of model preference and use it as the initial weight coefficient.
[0144] The calculation of initial weighting coefficients facilitates subsequent use.
[0145] S604: Calculate the product between the initial intermediate coefficient and the intermediate coefficient of model preference and use it as the intermediate weight coefficient.
[0146] The calculation of the intermediate weighting coefficient facilitates subsequent use.
[0147] S605: Calculate the product between the initial coefficients and the later coefficients of model preference and use it as the later weighting coefficient.
[0148] The calculation of the later weighting coefficients facilitates subsequent use.
[0149] S606: The initial weight coefficient, the intermediate weight coefficient and the later weight coefficient are combined and used as the stage weight coefficient.
[0150] In this method, the initial weight coefficient, the intermediate weight coefficient, and the later weight coefficient are combined to form a dataset, which is then used as the stage weight coefficient, thereby improving the accuracy of the obtained stage weight coefficients.
[0151] To further ensure the rationality of the changes in corrosion resistance, it is necessary to conduct a more detailed separate analysis and calculation of the changes in corrosion resistance, which will be explained in detail through the steps shown below.
[0152] The method for determining changes in corrosion resistance includes the following steps: S700: Based on the comparison between the initial corrosion image and the intermediate corrosion image, determine the intermediate change location points and the intermediate change area values.
[0153] The intermediate change location point refers to the geometric centroid coordinates of the region that was not eroded in the initial erosion image but newly appears as erosion in the intermediate erosion image. The intermediate change area value refers to the actual physical area of the newly added erosion region in the intermediate stage.
[0154] Spatially register the initial and intermediate erosion images to generate binary images. Perform a difference operation between the intermediate and initial erosion binary images, and define the regions with pixel values equal to 1 in the difference result as newly added erosion regions in the intermediate stage. Then, label the newly added erosion regions in the difference result image as connected components, calculate the total number of pixels in all labeled regions, and multiply this number by the actual area corresponding to a single pixel; the product is the intermediate change area value. Calculate the centroid coordinates of all newly added erosion regions in the difference result image, and use these centroid coordinates as the intermediate change location points.
[0155] S701: Based on the comparison between the intermediate and late erosion images, determine the location points of the late changes and the area values of the late changes.
[0156] In this context, the "later change location point" refers to the geometric centroid coordinates of a region that did not show corrosion in the intermediate erosion image but newly appears as corrosion in the later erosion image. The "later change area value" refers to the actual physical area of the newly added corrosion region in the later stage.
[0157] Spatially register the intermediate and late-stage erosion images to generate binary images. Perform a difference operation between the late-stage and intermediate-stage erosion binary images, and use regions with pixel values equal to 1 in the difference result as newly added erosion regions in the late stage. Then, label the newly added erosion regions in the difference result image as connected components, calculate the total number of pixels in all labeled regions, and multiply this number by the actual area corresponding to a single pixel; the product is the area value of the late-stage change. Calculate the centroid coordinates of all newly added erosion regions in the difference result image, and use these centroid coordinates as the location points for the late-stage change.
[0158] S702: Calculate the vector distance between the intermediate change location point and the later change location point and use it as the change location distance value.
[0159] The change location distance value refers to the vector distance between the mid-term change location point and the late-term change location point.
[0160] By analyzing and calculating the distance and direction between the intermediate and later change points, and combining the distance and direction as the change point distance value, it is convenient for subsequent use.
[0161] S703: Calculate the ratio between the intermediate-term change area value and the later-term change area value and use it as the change area ratio value.
[0162] The change area ratio refers to the ratio between the change area value in the middle period and the change area value in the later period.
[0163] Calculating the percentage of changed area facilitates subsequent use.
[0164] S704: The change in location distance and the change in area ratio are combined to determine the corrosion resistance variation.
[0165] By combining the distance values of the changing locations with the proportion values of the changing areas, a dataset is formed and used as a representation of the corrosion resistance changes, thereby improving the accuracy of the obtained corrosion resistance changes.
[0166] To further ensure the rationality of the corrosion protection reference values, it is necessary to perform further separate analysis and calculation on the corrosion protection reference values, which will be explained in detail through the steps shown below.
[0167] The method for determining corrosion protection reference values includes the following steps: S800: Determine the coupling differentiation factor based on the coupling effect coefficient.
[0168] Among them, the coupling distinguishing factor refers to the specific factor that plays a dominant contribution to coupling in a multi-factor coupling experiment.
[0169] By comparing the coupling effect coefficient with the preset coupling benchmark coefficient, and selecting the benchmark test and coupling test corresponding to the coupling effect coefficient being greater than the preset coupling benchmark coefficient, the factors in the coupling test that are equivalent to the addition of the benchmark test are used as the coupling differentiation factors for convenient subsequent use.
[0170] The coupling reference coefficient refers to the reference coefficient when coupling has no effect. The coupling reference coefficient is obtained after being pre-input by the operator.
[0171] S801: Determine the reference weight of the factor based on the coupling differentiation factors.
[0172] Among them, the factor reference weight refers to the weighting coefficients assigned to the subsequent change location distance value and change area ratio value based on the coupling distinguishing factors.
[0173] By inputting the coupling differentiation factors into a preset factor database, factor reference weights are obtained through matching, which facilitates subsequent use.
[0174] The factor database pre-stores a table of different coupling distinguishing factors and their corresponding factor reference weights, which is obtained after the operator pre-inputs the data.
[0175] For example, the factor database can be configured as follows: when the coupling differentiating factor is vibration, the weight of the change area ratio in the corresponding factor reference weight is set to 0.6, and the change location distance value is set to 0.4. When the coupling differentiating factor is corrosion, the weight of the change area ratio in the corresponding factor reference weight is set to 0.4, and the change location distance value is set to 0.6. When the coupling differentiating factor is temperature and humidity, the weight of the change area ratio in the corresponding factor reference weight is set to 0.5, and the change location distance value is set to 0.5.
[0176] S802: Retrieve the distance value of the changed location and the ratio value of the changed area based on the changes in corrosion resistance.
[0177] Among them, the distance value of the changed location and the ratio value of the changed area are retrieved by the corrosion resistance change situation, which is convenient for subsequent use.
[0178] S803: Calculate the distance value of the changed location and the ratio value of the changed area based on the reference weight of the factors, and use the calculation result as the corrosion protection reference value.
[0179] Specifically, the weights of the distance value at the changed location and the proportion value of the changed area are retrieved by the factor reference weight. Then, the product value between the distance at the changed location, the proportion value of the changed area and their respective weights is calculated. Finally, the two product values are added together to obtain the corrosion prevention reference value, thereby improving the accuracy of the obtained corrosion prevention reference value.
[0180] To further ensure the rationality of the multi-factor coupling test scheme, it is necessary to perform further separate analysis and calculation on the multi-factor coupling test scheme, which will be explained in detail through the following steps.
[0181] Reference Figure 3 The method for constructing a multi-factor coupled experimental scheme includes the following steps: S900: Vibration reference values, temperature and humidity reference values, and corrosion factor reference values are determined according to the vehicle model being adapted.
[0182] Among them, vibration reference value refers to the maximum parameter value describing vibration factors. Temperature and humidity reference value refers to the maximum parameter value describing temperature and humidity factors. Corrosion factor reference value refers to the maximum parameter value describing corrosion factors.
[0183] By inputting the compatible vehicle models into a preset vehicle model database, the system obtains the road impact vibration amplitude, alternating vibration frequency, continuous vibration duration, temperature range, humidity range, mud and water immersion duration, and acid / alkali chemical media contact duration for sold vehicles of the compatible models. Then, the maximum values of each road impact vibration amplitude, alternating vibration frequency, and continuous vibration duration are selected, and the root mean square value of acceleration is calculated and used as the vibration reference value. The maximum and minimum values of each temperature and humidity range are selected and combined to form temperature and humidity reference ranges. The endpoints and span values of the two ranges are then retrieved and input into a preset range conversion formula to obtain the range conversion value, which is used as the temperature and humidity reference value. Finally, the maximum value from the mud and water immersion duration and the acid / alkali chemical media contact duration is selected as the corrosion factor reference value.
[0184] S901: Determine the vibration coupling value based on the comparison between the vibration reference value and the vibration factor threshold.
[0185] Among them, the vibration coupling value refers to the parameter value used to describe whether a vibration coupling test is required.
[0186] By comparing the vibration reference value with the vibration factor threshold, when the vibration reference value is greater than the vibration factor threshold, it indicates that a coupling test is required for the vibration, so 1 is output as the vibration coupling value. When the vibration reference value is not greater than the vibration factor threshold, it indicates that a coupling test is not required for the vibration, so 0 is output as the vibration coupling value.
[0187] S902: Determine the temperature and humidity coupling value based on the comparison between the temperature and humidity reference values and the temperature and humidity factor thresholds.
[0188] Among them, the temperature and humidity coupling value refers to the parameter value used to describe whether a temperature and humidity coupling test is required.
[0189] By comparing the temperature and humidity reference values with the temperature and humidity factor thresholds, if the temperature and humidity reference values are greater than the temperature and humidity factor thresholds, it indicates that a temperature and humidity coupling test is required. Therefore, 1 is output as the temperature and humidity coupling value. If the temperature and humidity reference values are not greater than the temperature and humidity factor thresholds, it indicates that a temperature and humidity coupling test is not required. Therefore, 0 is output as the temperature and humidity coupling value.
[0190] S903: Determine the corrosion coupling value based on the comparison between the reference value and the threshold value of the corrosion factor.
[0191] The corrosion coupling value refers to a parameter value used to describe whether corrosion coupling tests are necessary.
[0192] By comparing the reference value of corrosion factor with the threshold value of corrosion factor, if the reference value of corrosion factor is greater than the threshold value of corrosion factor, it indicates that a corrosion coupling test is required. Therefore, 1 is output as the corrosion coupling value. If the reference value of corrosion factor is not greater than the threshold value of corrosion factor, it indicates that a corrosion coupling test is not required. Therefore, 0 is output as the corrosion coupling value.
[0193] S904: Based on the comparison results of vibration coupling value, temperature and humidity coupling value and corrosion coupling value with the preset coupling reference value, determine the coupling selection scheme and use the coupling selection scheme as the multi-factor coupling test scheme.
[0194] The coupling reference value refers to the reference parameter value for which coupling experiments are required. This value is obtained through pre-input by the operator. In this embodiment, the coupling reference value is set to 1. The coupling selection scheme refers to the final selection of the comprehensive scheme to be tested.
[0195] By comparing the vibration coupling value, temperature and humidity coupling value, and corrosion coupling value with the preset coupling benchmark value, and selecting the coupling test corresponding to the vibration coupling value, temperature and humidity coupling value, and corrosion coupling value that are consistent with the coupling benchmark value, the selected coupling test is combined with the three benchmark tests of vibration, temperature and humidity, and corrosion to form a coupling selection scheme. The coupling selection scheme is then used as a multi-factor coupling test scheme to improve the accuracy of the obtained multi-factor coupling test scheme.
[0196] Reference Figure 4This paper presents a research and development method for corrosion-resistant automotive fasteners. The method involves collecting data on the vehicle assembly location and compatible vehicle models of the fasteners under actual service conditions. It analyzes the vibration characteristics, temperature and humidity, and corrosion environment of the corresponding vehicles. Based on a comprehensive analysis of these multi-dimensional environmental conditions, the method selects the fastener structure. Using finite element simulation, it verifies and optimizes the structural strength and connection performance. After fabricating test fasteners, it constructs a multi-factor coupled test scheme matching the actual vehicle conditions. Layered single-factor benchmark tests and multi-factor coupled tests are conducted. Corrosion duration and corrosion images are collected in stages to form multi-factor test data. Quantitative corrosion reference values are obtained by calculating the coupling effect coefficient and corrosion changes step by step. The structure is iteratively adjusted using preset corrosion performance indicators as the judgment standard. Once the indicators meet the standards, the finalized structural design is locked, and mass production begins. This method proactively identifies potential corrosion failure risks and optimizes the design through multiple rounds of iteration to ensure it meets corrosion performance requirements. Ultimately, it effectively reduces the probability of corrosion failure after the fasteners are mass-produced and put into use.
[0197] Based on the same inventive concept, embodiments of the present invention provide a research and development system for corrosion-resistant automotive fasteners, comprising: The data acquisition module is used to collect information on the vehicle assembly location and compatible vehicle models. The memory stores a program for implementing a research and development method for corrosion-resistant automotive fasteners as described above; The processor loads and executes programs stored in memory.
[0198] Those skilled in the art will clearly understand that, for the sake of convenience and brevity, the above-described division of functional modules is used as an example. In practical applications, the above functions can be assigned to different functional modules as needed, that is, the internal structure of the device can be divided into different functional modules to complete all or part of the functions described above. The specific working process of the system, device, and unit described above can be referred to the corresponding process in the foregoing method embodiments, and will not be repeated here.
[0199] The above description is merely a preferred embodiment of the present invention. The scope of protection of the present invention is not limited to the above embodiments. All technical solutions falling within the scope of the present invention's concept are within the scope of protection of the present invention. It should be noted that for those skilled in the art, any improvements and modifications made without departing from the principles of the present invention should also be considered within the scope of protection of the present invention.
Claims
1. A research and development method for corrosion-resistant automotive fasteners, characterized in that, include: Collect the vehicle assembly location of the fastener to be developed and the corresponding compatible vehicle models; Vibration characteristics, temperature and humidity environment, and corrosive environment are determined based on the vehicle model to be adapted; Based on the assembly location of the vehicle, the structure of the fastener to be developed is selected to obtain a structural selection scheme; A finite element simulation model of the fastener is established based on the structural selection scheme to conduct simulation analysis of structural strength and connection performance. The structural selection scheme is then optimized and adjusted based on the simulation results to obtain an optimized structural scheme. Based on the structural optimization scheme, prototypes were fabricated to obtain fastening test pieces; Multi-factor coupled tests were conducted on the fastening test specimens based on vibration characteristics, temperature and humidity environment, and corrosion environment, and multi-factor test data were obtained. The structural optimization scheme is iteratively optimized based on multi-factor test data until the preset anti-corrosion performance index is met, and the finalized structural scheme is obtained. Production is carried out based on a structural design scheme to obtain the final fastener product.
2. The research and development method for corrosion-resistant automotive fasteners according to claim 1, characterized in that, Multi-factor coupled tests were conducted on the fastening test specimens based on vibration characteristics, temperature and humidity environment, and corrosion environment, and the multi-factor test data were obtained, including: Based on the vehicle assembly location, combined with vibration characteristics, temperature and humidity environment, and corrosion environment, vibration factor threshold, temperature and humidity factor threshold, and corrosion factor threshold are obtained respectively. A multi-factor coupled test scheme was constructed based on the threshold values of vibration, temperature and humidity, and corrosion. According to the multi-factor coupling test scheme, benchmark tests under the individual effects of each factor and coupling tests under the combined effects of at least two factors were conducted. Record the time when the protective layer first corrosion appears, the time when the protective layer corrosion reaches the preset area ratio, and the time when the base metal begins to corrode under each benchmark test and coupling test, and use these as the initial corrosion time, intermediate corrosion time, and late corrosion time, respectively. Images of the fastened test specimens were acquired based on the initial corrosion time, intermediate corrosion time, and late corrosion time, and were used as initial corrosion images, intermediate corrosion images, and late corrosion images, respectively. The data were combined based on the initial corrosion time, intermediate corrosion time, late corrosion time, initial corrosion images, intermediate corrosion images, and late corrosion images, and used as multi-factor experimental data.
3. The research and development method for corrosion-resistant automotive fasteners according to claim 2, characterized in that, The methods for determining the structural design scheme include: The coupling effect coefficient was determined by combining the initial corrosion time, intermediate corrosion time, and late corrosion time under various benchmark tests and coupled tests. The changes in corrosion resistance were determined by combining images of initial corrosion, intermediate corrosion, and late corrosion. The corrosion protection reference value is determined based on the coupling effect coefficient and the corrosion protection change. When the anti-corrosion reference value does not meet the preset anti-corrosion performance index, the type of structural adjustment and the structural adjustment parameters are determined based on the comparison between the anti-corrosion reference value and the preset anti-corrosion performance index. The structural adjustment scheme is determined by combining the type of structural adjustment, structural adjustment parameters and structural optimization scheme, and the sample is re-produced based on the structural adjustment scheme; When the anti-corrosion reference value meets the preset anti-corrosion performance index, the structural adjustment scheme will be used as the structural finalization scheme.
4. The research and development method for corrosion-resistant automotive fasteners according to claim 3, characterized in that, Methods for determining the coupling effect coefficient include: The initial corrosion time, intermediate corrosion time, and late corrosion time under the benchmark test are defined as the initial benchmark time, intermediate benchmark time, and late benchmark time, respectively. The initial corrosion time, intermediate corrosion time, and final corrosion time under the coupling test are defined as the initial coupling time, intermediate coupling time, and final coupling time, respectively. The initial offset coefficient is calculated based on the initial coupling time and the initial reference time; the intermediate offset coefficient is calculated based on the intermediate coupling time and the intermediate reference time; and the later offset coefficient is calculated based on the later coupling time and the later reference time. The comprehensive coupling estimate is determined by combining the initial offset coefficient, the intermediate offset coefficient, and the later offset coefficient, and the comprehensive coupling estimate is used as the coupling effect coefficient.
5. The research and development method for corrosion-resistant automotive fasteners according to claim 4, characterized in that, The methods for determining the comprehensive coupled estimate include: Determine the stage weighting coefficients based on the vehicle model and the location of the fastening requirements; The initial weight coefficient, the intermediate weight coefficient, and the later weight coefficient are retrieved based on the stage weight coefficient. Calculate the product of the initial offset coefficient and the initial weight coefficient and use it as the initial weighting value; Calculate the product between the intermediate offset coefficient and the intermediate weight coefficient, and use it as the intermediate weighted value; Calculate the product between the later offset coefficient and the later weight coefficient, and use it as the later weighting value; The sum of the initial weighted value, the intermediate weighted value, and the later weighted value is calculated and used as the comprehensive coupled estimate.
6. The research and development method for corrosion-resistant automotive fasteners according to claim 5, characterized in that, Methods for determining stage weight coefficients include: Determine the failure priority of corrosion protection performance based on the location of fastening requirements; The initial coefficients for the initial stage, the initial coefficients for the intermediate stage, and the initial coefficients for the later stage are determined based on the failure priority. Determine the initial model preference coefficient, the mid-term model preference coefficient, and the late-term model preference coefficient based on the vehicle model; Calculate the product between the initial coefficient and the initial coefficient of model preference, and use it as the initial weighting coefficient; Calculate the product between the initial mid-term coefficient and the mid-term model preference coefficient, and use it as the mid-term weighting coefficient; Calculate the product between the initial coefficients and the model preference coefficients in the later stage, and use it as the later weighting coefficient. The initial, intermediate, and later weight coefficients are combined and used as the stage weight coefficients.
7. The research and development method for corrosion-resistant automotive fasteners according to claim 3, characterized in that, Methods for determining changes in corrosion resistance include: Based on the comparison between the initial corrosion image and the intermediate corrosion image, the location points of intermediate changes and the area values of intermediate changes are determined; Based on the comparison between the intermediate and late erosion images, the location points and area values of the late changes are determined; Calculate the vector distance between the intermediate-term change location point and the later-term change location point and use it as the change location distance value; Calculate the ratio between the mid-term and late-term area changes and use it as the area change ratio. The changes in location distance and the changes in area ratio are combined to represent the changes in corrosion resistance.
8. The research and development method for corrosion-resistant automotive fasteners according to claim 7, characterized in that, Methods for determining corrosion protection reference values include: Determine the coupling distinguishing factors based on the coupling effect coefficient; Determine the reference weights of factors based on the coupling differentiation factors; Based on the changes in corrosion resistance, retrieve the distance values of the changed locations and the ratio values of the changed areas; The distance value of the changed location and the ratio of the changed area are calculated based on the reference weight of the factors, and the calculation results are used as the reference value for corrosion prevention.
9. The research and development method for corrosion-resistant automotive fasteners according to claim 2, characterized in that, Methods for constructing multi-factor coupled experimental schemes include: The vibration reference value, temperature and humidity reference value, and corrosion factor reference value are determined according to the vehicle model to be adapted; The vibration coupling value is determined by comparing the vibration reference value with the vibration factor threshold. The temperature and humidity coupling value is determined by comparing the temperature and humidity reference values with the temperature and humidity factor thresholds. The corrosion coupling value is determined by comparing the reference values and threshold values of corrosion factors. Based on the comparison results of vibration coupling value, temperature and humidity coupling value and corrosion coupling value with the preset coupling reference value, the coupling selection scheme is determined and the coupling selection scheme is used as the multi-factor coupling test scheme.
10. A research and development system based on corrosion-resistant automotive fasteners, characterized in that, include: The data acquisition module is used to collect information on the vehicle assembly location and compatible vehicle models. The memory stores a program for implementing a research and development method for corrosion-resistant automotive fasteners as described in any one of claims 1 to 9; The processor loads and executes programs stored in memory.