Cables used in nuclear power plants, manufacturing processes, and cable connectors used in conjunction with them
By adjusting the radial distance and the in-furnace traction speed, and combining the induction power supply section and the induction power supply section, the problem of inconsistent heat treatment between the 304L stainless steel sheath and the copper core in nuclear power plant cables was solved, achieving continuity of the internal state of the cable and stability of the termination.
Patent Information
- Application Number
- CN202611627664.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-21
- Publication Date
- 2026-11-17
AI Technical Summary
In the manufacturing of nuclear power plant cables, the heat treatment response of the 304L stainless steel sheath and the copper core is inconsistent. Existing technology makes it difficult to meet the heat treatment requirements of both without disassembling the cable structure, and the internal state of the cable is difficult to continue to the termination process.
By adjusting the radial distance from the copper core wire to the inner surface of the sheath and the traction speed in the furnace, combined with the use of the induction power supply section, the heat treatment process of the copper core and the 304L stainless steel sheath is controlled respectively, and the continuity of the internal state of the cable is maintained before termination.
It achieves the ability to meet the heat treatment requirements of 304L stainless steel sheath and copper core without disassembling the cable structure, reduces the adaptation deviation caused by fixed parameters, and ensures the stability of the internal state of the cable during the termination process.
Smart Images

Figure CN123120428A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of mineral-insulated armored cable manufacturing and termination technology, and more specifically, to cables used in nuclear power plants, their manufacturing processes, and cable connectors used in conjunction with them. Background Technology
[0002] In the manufacturing of nuclear power plant cables, cross-linked polyethylene insulated power cables and cable accessories can usually complete conductor processing, insulation forming, and accessory assembly separately. However, mineral-insulated armored cables used in severe accident environments require the copper core, SiO2 insulation medium, and stainless steel sheath to be combined into one piece first, and then the outer diameter is gradually reduced through multiple drawing and intermediate heat treatment. Existing technology has adopted a processing method that uses stainless steel shell, conductor core wire, and inorganic insulation materials such as SiO2 for joint drawing and annealing. For severe accident cables used in nuclear power plants, which employ four copper cores, SiO2 insulation, and 304L stainless steel armor, the heat treatment responses of the copper core and 304L stainless steel after drawing are not the same. However, since they are separated by SiO2 and encapsulated in the same cross section, they cannot be annealed separately like independent metal billets. Instead, they must pass through the heat treatment zone together with the entire cable. At the same time, external heat needs to act on the 304L sheath first, and then be transferred to the internal copper core through SiO2. Since the thermal conductivity of SiO2 is lower than that of MgO and Al2O3, the sheath and copper core undergo different heating processes within the limited furnace pass-through time. As the cable diameter is gradually reduced from a larger blank diameter to the target outer diameter in consecutive passes, the reduction degree, sheath thickness, and radial heat transfer distance of the previous pass are constantly changing. If the furnace temperature and throughput speed shared by the entire cable are still used as the basis for heat treatment, increasing the heat input can enhance the recovery of the 304L sheath, but it will also increase the heating of the copper core. Reducing the heat input to limit the heating of the copper core may result in insufficient recovery of the 304L before entering the next reduction pass. Therefore, it is difficult to meet the processing requirements of the two metals separately by simply adjusting the uniform furnace temperature, holding time, or traction speed. Furthermore, after cabling, the end sheath needs to be cut to complete the welding and resealing of the multi-core connector. However, the existing multi-core termination already has the problem of misalignment between the cable core and the connector point, as well as the requirement for moisture-proof treatment of the SiO2 end. This indicates that the internal state formed by the aforementioned heat treatment must continue until the final termination process. Therefore, the technical problem to be solved by this application is: under the condition that the 304L stainless steel sheath, SiO2 insulation medium and copper core have been integrated and the diameter has been continuously reduced, how to meet the different heat treatment requirements of the sheath and the copper core without disassembling the cable structure, and maintain the internal state of the cable until the matching connector completes the termination and sealing. Summary of the Invention
[0003] To overcome the aforementioned deficiencies of the prior art, embodiments of the present invention provide cables, manufacturing processes, and matching cable connectors for use in nuclear power plants. By adjusting the furnace penetration time and furnace traction speed based on the radial distance from the copper core wire to the inner surface of the sheath, and controlling the induction power supply range based on the wall thickness of the 304L stainless steel sheath, the closed state is extended to core wire positioning, drying treatment, and connector welding termination, thereby solving the problems mentioned in the background art.
[0004] To achieve the above objectives, the present invention provides the following technical solution: a manufacturing process for cables used in nuclear power plants, comprising: S1. Place four copper core wires into a 304L stainless steel sheath, fill and compact SiO2 insulating medium between the copper core wires and between the copper core wires and the sheath, and press and weld the empty tube sections at both ends of the 304L stainless steel sheath to form a cable blank. S2. The cable blank is drawn in turns. In the annealing turns, four radial distances from the outer surface of the copper core wire to the inner surface of the sheath are obtained. The values are retained and not exceed the other three values. The furnace penetration time of the current turn is obtained by multiplying the square of the ratio of the retained value of the current turn to the retained value of the first turn by the furnace penetration time of the first turn. The furnace traction speed is determined by dividing the furnace power supply section length by the furnace penetration time of the current turn. In S2, the annealing pass refers to the drawing pass in which the furnace body is set up for energy supply during the multi-pass drawing process. It is used to restore the plastic processing state of the 304L stainless steel sheath and copper core wire after diameter reduction before entering the subsequent drawing. The radial distance from the outer surface of the copper core wire to the inner surface of the sheath is the length of the line segment measured from the intersection of the outer contour of the copper core wire and the radial direction to the intersection of the inner contour of the 304L stainless steel sheath and the same radial direction within the same axial detection section. The four copper core wires each form a radial distance. The four radial distances are used to characterize the thickness of the medium that the furnace body energy needs to pass through when it is transferred from the 304L stainless steel sheath to the four copper core wires through the SiO2 insulating medium. The retention value for this pass represents a value selected from the four radial distances obtained in this pass, not exceeding the other three radial distances. This ensures that the furnace treatment time is determined based on the copper core wire closest to the inner surface of the sheath, avoiding the copper core wire closer to the inner surface of the sheath being subjected to additional furnace treatment when the treatment time is determined by the radial distances of the other three copper core wires. The first pass retention value represents the radial distance obtained in the first annealing pass according to the same value selection rules, and the first pass duration represents the distance traveled by the cable blank from entering the furnace power supply section to leaving the furnace power supply section in the first annealing pass. The time taken is used as the reference time for subsequent annealing passes. The furnace penetration time of this pass is obtained by "squaring the retention value of this pass by the retention value of the first pass, and then multiplying the square of the ratio, and then multiplying the time of the first pass". When the composition of SiO2 insulation medium, the furnace body setting in Celsius and the power supply method remain unchanged, the characteristic distance of radial energy transfer has a corresponding relationship with the square root of the action time. Therefore, the action time is converted by the square of the distance ratio so that when the radial thickness of SiO2 changes after the cable diameter reduction, the action time in the furnace changes synchronously with the actual transfer distance. The length of the furnace body energy supply section represents the effective axial length of the cable receiving energy input inside the furnace. The furnace traction speed is obtained by dividing the length of the furnace body energy supply section by the furnace passage time of this pass, so that the cable passes through the furnace body energy supply section according to the calculated working time. This directly converts the actual SiO2 radial distance after the diameter reduction of this pass into the furnace traction speed required for the next annealing, and reserves processing space for S3 to implement independent supplementary energy supply to the 304L stainless steel sheath. S3. After passing through the furnace body power supply section, enter the induction power supply section before the drawing die. Determine the length of the induction power supply section by the product of the drawing speed and the annealing time of the sheath. Adjust the induction power so that the Celsius value when the sheath leaves the induction power supply section enters the Celsius range of 304L stainless steel sheath annealing. Then enter the drawing die to complete this reduction. The induction energy supply section refers to the electromagnetic induction area located between the furnace energy supply section and the drawing die, surrounding the 304L stainless steel sheath. It is used to supplement the energy required for sheath annealing separately after the overall annealing is completed in S2. The drawing speed refers to the axial running speed of the cable blank through the induction energy supply section and the drawing die. The sheath annealing time refers to the duration for which the 304L stainless steel sheath receives the induction effect. The product of the two is the length of the induction energy supply section, so that the actual time for the sheath to pass through the induction energy supply section is equal to the sheath annealing time. Induction power represents the electromagnetic energy input to the 304L stainless steel sheath per unit time. By adjusting the induction power, the Celsius value of the sheath surface measured at the outlet of the induction power supply section is brought into the Celsius range specified by the annealing process of 304L stainless steel material. Then, it directly enters the drawing die to complete the diameter reduction in this pass, so that S2 undertakes the overall annealing control of the copper core wire and S3 undertakes the supplementary annealing control of the 304L stainless steel sheath. S4. After this reduction, determine the furnace traction speed for the next annealing pass according to S2. Repeat annealing and reduction until the outer diameter reaches 5mm, and keep the empty tube sections at both ends sealed. In S4, the current diameter reduction refers to the diameter reduction process of the cable blank after the current drawing die is completed. After the diameter reduction, the radial distance of SiO2 between the copper core wire and the 304L stainless steel sheath changes with the cross-sectional size. Therefore, the furnace traction speed is recalculated according to S2 in the next annealing pass, so that the dwell time of the cable in the furnace energy supply section is adjusted synchronously with the current radial transmission distance, avoiding the mismatch between the energy receiving process of the copper core wire and the current cross-sectional size caused by using the first furnace pass time. Repeated annealing and diameter reduction means that after each diameter reduction is completed, the next annealing pass is determined using the current cross-sectional data, and then the next diameter reduction is implemented. This makes each processing pass form a successive energy-reduction process until the outer diameter reaches 5mm. The empty tube sections at both ends are kept sealed during the cyclic processing to isolate the SiO2 insulating medium end face from the external environment. This prevents the end face from being exposed and introducing moisture during multiple furnace passes, traction, and mold changes, so that the state of the insulating medium after diameter reduction can directly accept the S5 termination treatment. S5. After the final diameter reduction, the cable is moved into the drying termination cavity. The closed empty pipe section is cut off in the cavity and the end sheath is stripped. The four copper core wires are inserted into the four-hole ceramic positioning body in the metal transition sleeve. The sheath is welded to the metal transition sleeve, the copper core wires to the contact, and the metal transition sleeve to the connector tail sleeve. A closed termination structure is formed before the SiO2 end face leaves the drying termination cavity.
[0005] In a preferred embodiment, the furnace power supply section parameter limitation and subsequent annealing pass conversion are performed based on the first furnace penetration time in S2, including: S21. For the first annealing pass, the furnace body is set to 1000°C, the furnace body power supply section length is set to 5000mm, the furnace traction speed is set to 1000mm / min, and 5min is used as the first pass through the furnace. S22. In subsequent annealing passes, the furnace body setting value in Celsius and the furnace body power supply section length remain unchanged. Based on the furnace penetration time obtained in S2, the furnace traction speed is determined by dividing 5000mm by the furnace penetration time, and the furnace penetration is performed according to the determined furnace traction speed.
[0006] In a preferred embodiment, the electromagnetic penetration range limitation of the 304L stainless steel sheath is implemented based on the inductive power supply section in S3, including: S31. After the diameter reduction is completed, select the same axial section at the mold exit and collect X-ray projection images along two mutually perpendicular transmission directions. Obtain the outer and inner contours of the 304L stainless steel sheath from the two X-ray projection images. Obtain a wall thickness value every 45° along the circumference and retain no more than the other seven wall thickness values from the eight wall thickness values. S32. Obtain the resistivity and permeability of 304L stainless steel at the outlet of the furnace power supply section in Celsius. Divide the resistivity by the product of pi, the induction frequency and the permeability, and take the square root of the result as the electromagnetic penetration depth. S33. In the next annealing pass, adjust the induction frequency until the electromagnetic penetration depth does not exceed the wall thickness value reserved in S31. Fix the induction frequency and the length of the induction power supply section, and then adjust the induction power so that the surface Celsius value of the 304L stainless steel sheath when it leaves the induction power supply section enters the annealing Celsius range of the 304L stainless steel sheath.
[0007] In a preferred embodiment, the radial distance acquisition and final core position recording in S2 are performed based on the two X-ray projection images acquired in S31, including: S41. Obtain the coordinates of the center, inner contour, and center of the four copper core wires of the 304L stainless steel sheath from the two X-ray projection images respectively. S42. For each copper core wire, draw a radial line passing through the center of the sheath and the center of the copper core wire. Take the length of the line segment between the intersection of the radial line and the outer contour of the copper core wire and the intersection of the radial line and the inner contour of the sheath to form four radial distances, and input the four radial distances into S2. S43. Record the center coordinates of the four copper core wires after each reduction pass, and use the center coordinates of the four copper core wires after the final reduction pass as input for determining the circumferential angle position of the joint during the termination stage.
[0008] In a preferred embodiment, the pulling mode switching is performed based on the reduction path in S4 and the induction power supply section length in S3, including: S51. The diameter of the cable blank is reduced sequentially from Φ25 to Φ18, Φ14, Φ12, Φ10.7, Φ9.3, Φ8.0, Φ7.5, Φ6.4, Φ5.5 and Φ5.0, with the diameter reduction ratios for each stage being 28%, 22%, 14%, 11%, 13%, 14%, 6%, 15%, 14% and 9% respectively. For the three reduction passes from S52 to Φ25 to Φ12, a straight-material chain drawing machine is used and the drawing speed is 6m / min. From Φ12 to Φ10.7, a coil drawing machine is used and the drawing speed is 15m / min. When the drawing speed is changed from 6m / min to 15m / min, the supplementary annealing time of the 304L stainless steel sheath is kept unchanged, and the length of the induction power supply section is re-determined by multiplying 15m / min by the supplementary annealing time.
[0009] In a preferred embodiment, based on the closed empty pipe section formed by S1, the closed boundary migration is performed when changing the formwork and traction head, including: S61. Before cutting off the original traction head, press a 304L stainless steel pipe again on the side of the original closed empty pipe section near the SiO2 insulating medium and weld it circumferentially to form an inner closed section. S62. After the inner sealing section is completed, the original sealing section and the original traction head are cut off. Then, the end of the inner sealing section away from the SiO2 insulating medium is processed into a traction head that is adapted to the next drawing die inlet. S63. Subsequent mold changes shall be performed in the order of first forming the inner closed section and then cutting off the original closed section, so that the end face of the SiO2 insulating medium is always within the weld seal boundary during the replacement of the traction head.
[0010] In a preferred embodiment, insulation testing and drying treatment after the SiO2 insulating dielectric end face is opened is performed based on the drying termination cavity in S5, including: S71. After the final diameter reduction, move the cable with the sealed section into the dry terminal cavity. Cut off the sealed section in the cavity and strip the 304L stainless steel sheath at the end of 12-15mm. Use one copper core wire as the first detection electrode and connect the other three copper core wires and the 304L stainless steel sheath in parallel as the second detection electrode. Apply a DC voltage of 500V and hold for 1 minute. Replace the first detection electrode in sequence until four insulation resistance values are obtained. S72. If any insulation resistance value does not exceed 1GΩ, purge the end face of the SiO2 insulating medium with nitrogen gas dried by molecular sieve for 1 minute, and then repeat the insulation test in S71. Cycle the purging and insulation test until all four insulation resistance values exceed 1GΩ, and then proceed to the copper core wire positioning and contact welding process.
[0011] In a preferred embodiment, the determination of the circumferential angle position of the joint and the closing termination are performed based on the center coordinates of the four copper core wires recorded after the final diameter reduction, including: S81. Obtain the center coordinates of the four axial positioning holes of the ceramic positioning body. Pair the center coordinates of the four copper core wires with the center coordinates of the four axial positioning holes according to the predetermined core wire numbers. Rotate the ceramic positioning body from 0° to 359° at 1° intervals with the cable axis as the center. Calculate the sum of the planar distances between the four pairs of paired centers for each angular position. Keep the angular positions where the sum of the distances does not exceed the sum of the other 359 distances. S82. Fix the ceramic positioning body at the corner position reserved in S81, so that the four copper core wires are respectively inserted into the four axial positioning holes and welded to the four contact welding cups. Then weld the 304L stainless steel sheath to the metal transition sleeve circumferentially, and weld the metal transition sleeve to the connector tail sleeve circumferentially. S83. After welding, apply a 500V DC voltage between the four copper core wires and the 304L stainless steel sheath and hold for 1 minute. After all four insulation resistance values exceed 1GΩ, apply a 1600V AC voltage and hold for 1 minute. The termination is completed when no breakdown or arcing occurs and the leakage current does not exceed 10mA.
[0012] Cables used in nuclear power plants consist of: four spaced-apart copper cores, a SiO2 insulation layer surrounding the four copper cores, a 304L stainless steel sheath covering the SiO2 insulation layer, and metal transition sleeves at the cable ends. The cable body has an outer diameter of 5mm or less, and each copper core has a cross-sectional area of 1mm². 2 Within; the metal transition sleeve is circumferentially welded to the 304L stainless steel sheath, and a ceramic positioning body is fixed inside the metal transition sleeve. The ceramic positioning body has four axial positioning holes, and four copper core wires pass through the four axial positioning holes respectively. The end face of the SiO2 insulation layer terminates at the side of the ceramic positioning body facing the cable body. The outer circumference of the metal transition sleeve is provided with an axial orientation groove. The angular position of the four axial positioning holes around the axis of the metal transition sleeve is limited by the axial orientation groove. The end of the metal transition sleeve away from the cable body is circumferentially sealed by a cut-off metal end cap.
[0013] A cable connector used in conjunction with cables in nuclear power plants includes: a 316L stainless steel connector housing, a metal end sleeve, a ceramic insulator, four contacts, and a styrene-based silicone rubber sealing ring. The metal end sleeve is connected to the 316L stainless steel connector housing. The ceramic insulator is fixed inside the 316L stainless steel connector housing and has four through holes. The four contacts pass through the four through holes, and the ends of the four contacts facing the metal end sleeve form welding cups. The mating ends of the four contacts have a copper-plated nickel structure. The metal end sleeve has an annular receiving section for inserting a metal transition sleeve at the cable end. The inner wall of the annular receiving section has an axial orientation key, which is used to embed into the axial orientation groove on the outer circumference of the metal transition sleeve. The angular positions of the four welding cups around the axis of the connector housing are defined by the axial orientation key. The outer circumference of the annular receiving section has an annular welding part. After the metal transition sleeve is inserted into the annular receiving section, it is circumferentially welded to the metal end sleeve through the annular welding part. The styrene-based silicone rubber sealing ring is located between the ceramic insulator and the 316L stainless steel connector housing.
[0014] The technical effects and advantages of this invention are as follows: 1. The furnace penetration time is calculated by converting the radial distance from the four copper core wires to the inner surface of the sheath, and an induction energy supply section facing the 304L sheath is set after the furnace energy supply section. This allows the overall heating time of the copper core to be adjusted according to the radial transmission distance, and the sheath to receive independent supplementary energy. This constrains the annealing process of the copper core and the 304L sheath separately without disassembling the cable cross-section, and alleviates the mutual restraint between the two metal heat treatments caused by the shared furnace parameters of the whole cable. 2. The furnace penetration time is calculated by the square relationship between the retention value of this pass and the retention value of the first pass, and the furnace traction speed is calculated by back-calculating the energy supply section length of the furnace body. This allows the energy supply time of each annealing pass to be updated as the radial transmission distance after the diameter reduction changes, thereby reducing the adaptation deviation of fixed furnace penetration parameters to cross-sectional changes. 3. Calculate the electromagnetic penetration depth and adjust the induction frequency by using the sheath wall thickness, resistivity and permeability in eight directions. Then adjust the induction power according to the outlet Celsius value so that the supplementary power supply range is constrained by the actual wall thickness of the 304L sheath, and reduce the expansion of the sheath supplementary power supply towards the copper core wire. 4. By first forming the inner closed section and then cutting off the outer closed section, and completing the opening, insulation inspection and welding in the dry termination cavity, the SiO2 end face is kept under controlled exposure during the termination process, reducing the fluctuation of insulation status caused by end moisture absorption. 5. Calculate the circumferential angle of the ceramic positioning body using the coordinates of the four cores after the final diameter reduction, and use axial grooves and axial keys to maintain the circumferential positional relationship between the core wire and the contact, so that the four copper core wires enter the contact according to the predetermined hole positions, reducing the bending of the core wires and the position offset during the termination process. Attached Figure Description
[0015] Figure 1 This is a flowchart of the present invention. Detailed Implementation
[0016] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0017] Refer to the instruction manual appendix Figure 1 The present invention relates to cables, manufacturing processes, and matching cable connectors for use in nuclear power plants, comprising: Example 1: Cable blank formation, multi-stage annealing and progressive diameter reduction; Four copper core wires of the same specification and a 304L stainless steel tube are selected. The four copper core wires are numbered 1, 2, 3, and 4 respectively. During assembly, four-hole positioning fixtures are set at both ends of the 304L stainless steel tube. The four positioning holes are set around the tube axis. The four copper core wires pass through the corresponding positioning holes, so that the four copper core wires extend along the axial direction of the 304L stainless steel tube and maintain a gap inside the tube. The space inside the 304L stainless steel tube, except for the space occupied by the four copper core wires, is used as a SiO2 insulating medium filling space. The cross-sectional area of the filling space is obtained by subtracting the sum of the cross-sectional areas of the four copper core wires from the cross-sectional area of the inner hole of the 304L stainless steel tube. The effective filling length is obtained by the axial length between the empty tube sections at both ends. The same batch of SiO2 insulating medium is used. During filling, the SiO2 insulating medium is added in sections from one end of the 304L stainless steel tube. After each addition, axial vibration is used to allow the powder to enter between the four copper core wires and between the copper core wires and the inner surface of the 304L stainless steel tube. Each vibration cycle uses the same vibration frequency, amplitude, and duration. After the vibration ends, the SiO2 material surface is replenished to the end mark position of the effective filling length before the next vibration cycle is executed. The replenishment is terminated when the material surface remains at the end mark position after two adjacent vibration cycles. This ensures that each axial filling section of the same cable blank uses the same filling process, and SiO2 insulating medium is not re-added or removed during subsequent diameter reduction. Empty pipe sections are reserved at both ends of the 304L stainless steel pipe; the reserved length at the traction end is calculated based on the number of times a closed section needs to be formed during the mold changing process. Specifically, the length occupied by one inner closed section, one cutting allowance, and one traction head processing length are added together, multiplied by the number of planned closed boundary migrations, and the end processing retention length is added. When the tail end needs to be migrated in the same way, it is calculated in the same way. When migration is not performed, the pipe section length that meets the requirements of initial welding and end processing is retained. After SiO2 filling is completed, the empty pipe section is first pressed together to make the relative pipe walls fit together, and then the metal closed boundary is formed by welding along the circumference of the pressed section. During the subsequent diameter reduction process, the SiO2 insulating medium and the four copper core wires are always located between the metal closed boundaries at both ends. After the cable blank is formed, the diameter is reduced in multiple passes. In this embodiment, the initial outer diameter of the cable blank is Φ25, which is reduced to Φ18, Φ14, Φ12, Φ10.7, Φ9.3, Φ8.0, Φ7.5, Φ6.4, Φ5.5 and Φ5.0 in sequence, with corresponding diameter reduction ratios of 28%, 22%, 14%, 11%, 13%, 14%, 6%, 15%, 14% and 9% in sequence. An annealing process is set before the start of each diameter reduction pass, so that the copper core wire and 304L stainless steel sheath before entering the drawing die are first powered by the furnace body, and then powered by the 304L stainless steel sheath through induction, and then the diameter reduction of this pass is completed. The first annealing pass is set to 1000°C, with the furnace power supply section length set to 5000mm and the furnace traction speed set to 1000mm / min. The cable blank takes 5 minutes from entering the furnace power supply section to leaving it, which is designated as the first pass duration. The furnace power supply and drawing processes are performed in two separate stages. The furnace traction speed only controls the time the cable spends passing through the 5000mm furnace power supply section, while the drawing speed only controls the axial speed of the cable passing through the induction power supply section and the drawing die. After the furnace power supply is completed, the processed cable section is wound up and then enters the induction power supply and drawing stages again, thus allowing 1000mm / min, 6m / min, and 15m / min to be applied to different processing stages. At the start of the first annealing pass, four radial distances from the outer surface of the four copper core wires to the inner surface of the 304L stainless steel sheath are obtained at the same axial detection section. The value of no more than the other three values is retained from the four radial distances as the first pass retention value. After each reduction pass is completed, four new radial distances are obtained at the axial detection section at the die exit. The value of no more than the other three values is retained from the four values as the current pass retention value. The current pass retention value is divided by the first pass retention value, the ratio is multiplied by itself, and then multiplied by 5min. The result is used as the furnace penetration time of the next annealing pass. 5000mm is divided by the furnace penetration time of the current pass, and the result is used as the furnace traction speed of the next annealing pass. The square conversion uses the first annealing pass as the benchmark for the same cable blank, without using the first pass duration of other cable blanks; throughout the conversion, the batch, filling quality, furnace setting in Celsius, and furnace power supply method of the SiO2 insulation medium remain unchanged, and the filling space inside the 304L stainless steel sheath is not opened subsequently, nor is the SiO2 composition changed; each conversion only converts the radial transmission distance change caused by diameter reduction into a time change relative to 5 minutes; the radial distance change relationship of the four copper core wires is checked according to the cross-sectional coordinate processing method of Example 2, and if the four copper core wires do not maintain the same radial scaling, the next annealing pass is stopped, and the single retained value of this pass is not used for further conversion; After the furnace body is powered, the cable enters the induction power supply section set before the drawing die inlet; the sheath annealing time is taken according to the action time recorded in the processing documents of the same batch of 304L stainless steel pipes; the length of the induction power supply section is obtained by multiplying the drawing speed of this pass by the sheath annealing time, and the time unit and speed unit are first converted to the same unit system; the induction power supply section is set around the 304L stainless steel sheath, and the induction frequency is determined according to the calculation process of sheath wall thickness and electromagnetic penetration depth in Example 2; after the induction frequency is determined, it remains unchanged, and then the induction power is adjusted so that the Celsius value of the 304L stainless steel sheath surface measured at the outlet of the induction power supply section enters the annealing Celsius range specified in the processing documents of the same batch of 304L materials; after entering the range, no additional dwell section is set, and the cable enters the drawing die in the same drawing direction. For the three diameter reduction passes from Φ25 to Φ18, Φ18 to Φ14, and Φ14 to Φ12, a straight-material chain wire drawing machine is used with a working frequency of 27Hz and a drawing speed of 6m / min. From Φ12 to Φ10.7 onwards, a coil wire drawing machine is used with a working frequency of 30Hz and a drawing speed of 15m / min. When switching from 6m / min to 15m / min, the annealing time of the 304L stainless steel sheath is not changed. Instead, the length of the induction power supply section is re-determined by multiplying the sheath annealing time by 15m / min. This ensures that the speed change only changes the axial dimension of the induction power supply section and does not change the duration of the sheath receiving the induction effect. After each diameter reduction is completed, the following steps are performed in sequence: obtaining the cross section, calculating the radial distance, converting the furnace passage time for the next annealing pass, calculating the furnace traction speed, supplying energy to the furnace body, supplying energy through induction, and proceeding to the next diameter reduction, until the outer diameter reaches Φ5.0. The closed empty tube sections at both ends maintain a metal closed boundary throughout the entire diameter reduction process. When the traction head needs to be remade for mold replacement, the closed boundary migration process in Example 3 is adopted. After the final diameter reduction is completed, the cable with an outer diameter of Φ5.0, along with the end sealing section, is moved into the drying terminal cavity. Inside the drying terminal cavity, the sealing section is removed and the 12-15mm end 304L stainless steel sheath is stripped. The four copper core wires are inserted into the four-hole ceramic positioning body inside the metal transition sleeve according to the numbers 1 to 4. Then, the copper core wires are welded to the contact, the 304L stainless steel sheath to the metal transition sleeve, and the metal transition sleeve to the connector tail sleeve. This ensures that the SiO2 insulating dielectric end face is back inside the metal closed terminal structure before leaving the drying terminal cavity. Implementation method: The multi-pass reduction does not use a fixed furnace pass time; each reduction will change the radial path of SiO2 from the outer surface of the copper core wire to the inner surface of the 304L stainless steel sheath. Therefore, the geometric result of this pass directly participates in the time calculation of the next annealing pass; the first 5 minutes serve as the time reference, and the subsequent times are only calculated relative to the actual radial size of the same cable, so that "reduction result - next annealing pass - next reduction" are connected one after another; The furnace body power supply and induction power supply respectively control the energy receiving time of the copper core wire and supplement the energy receiving of the 304L stainless steel sheath; the two stages of processing use different execution variables. The furnace body stage changes the furnace penetration time, and the induction stage changes the power after the action time is determined. This avoids the two metals being adjusted in the same direction at the same time when only the furnace body setting value or the furnace traction speed is changed. Example 2: X-ray cross-section processing, radial distance conversion, and induction frequency determination; In this embodiment, an axial detection position is set at the die exit after each diameter reduction pass, and the axial position of the detection section is defined by the outer diameter detection ring; a circumferential reference mark is set at the end of the 304L stainless steel sheath during the billet assembly stage. The circumferential reference mark extends along the cable axis to the end after each diameter reduction pass, and is used to determine the X-ray projection direction and the circumferential direction of the subsequent joint. A first X-ray projection image is acquired at the axial detection position. The first projection direction passes through the axis of the 304L stainless steel sheath and coincides with the circumferential reference direction. Keeping the detection section position unchanged, the cable is rotated 90° around its own axis and a second X-ray projection image is acquired. The two images use the same geometric magnification and the same pixel size calibration relationship, and the image coordinates are converted to millimeter coordinates. The first projection drawing obtains the outer contour of the 304L stainless steel sheath along both sides of the first projection direction, the inner contour along both sides of the first projection direction, and the center coordinates of the four copper core wires along the first projection direction. The second projection drawing obtains the outer contour boundary, inner contour boundary, and center coordinates of the four copper core wires along the second direction in the same way. The outer contour center, first half-axis, and second half-axis are obtained based on the outer contour boundaries of the two directions, and the inner contour center, first half-axis, and second half-axis are obtained based on the inner contour boundaries of the two directions. An outer contour ellipse and an inner contour ellipse are established respectively. When a circular drawing die is used for diameter reduction, the two half-axis are the same, thus forming a circular expression. When there is drawing ellipticity, an elliptical expression is formed according to the two actual half-axis, and the single projection width is not directly used as the wall thickness of the entire circumference. The first test section is numbered 1 to 4 according to the circumferential order of the four copper core wires surrounding the center of the 304L stainless steel sheath. For subsequent test sections, when the core wire coordinates in the two projections need to be restored to four two-dimensional coordinates, 24 numbering combinations of the four core wires are first formed. Each numbering combination forms four two-dimensional core wire center coordinates. Then, the sheath center coordinates are subtracted from the four center coordinates to obtain four relative coordinates. The four relative coordinates of this section are then compared with the four relative coordinates of the previous section with the same number, and the sum is calculated. From the 24 results, combinations whose sum of squared displacements does not exceed the remaining 23 are retained, thus inheriting the core wire numbering from 1 to 4. When two sets of squared displacements are the same, the squared displacements are compared one by one in the order of core wires 1, 2, 3, and 4. The group with the first numerical difference retains the numbering combination whose value precedes that of the other group. After establishing the center coordinates of the four copper core wires, a radial line is drawn for each copper core wire, passing through the center of the 304L stainless steel sheath and the center of the copper core wire. The cross-section of the copper core wire forms a circular outline according to the measured outer diameter. The intersection point of the radial line and the outer outline of the copper core wire facing the 304L stainless steel sheath is calculated. Then, the intersection point of the same radial line and the inner elliptical outline is calculated. The length of the axial cross-section line segment between the two intersection points forms the radial distance of one copper core wire. Each of the four copper core wires forms a radial distance. The value of no more than three of the four values is retained as the retained value for this pass. To avoid using a single retention value for the current pass when the four copper core wires have undergone different radial displacements, four ratios are calculated for copper core wires 1 to 4: "radial distance of this pass divided by radial distance of the first pass with the same number". The radial dimensions formed by the four ratios are quantified according to the actual length corresponding to one pixel in the X-ray image. If the difference between the four ratios after conversion to the actual length does not exceed the length corresponding to one pixel, the furnace penetration time of this pass is obtained by multiplying the square of the ratio of the retention value of this pass to the retention value of the first pass by 5 minutes of the first pass. If the difference after conversion of any ratio exceeds the length corresponding to one pixel, the process stops and the core position formed by the diameter reduction of this pass is processed. The copper core wire closest to the inner surface of the sheath is not used to represent the other three copper core wires for further conversion. The sheath wall thickness is obtained using the same outer and inner contour ellipse. Starting from the center of the outer contour of the 304L stainless steel sheath, eight rays are established along 0°, 45°, 90°, 135°, 180°, 225°, 270° and 315° respectively. The parameters of each ray are written as follows: the x-coordinate is equal to the center x-coordinate plus the ray length multiplied by the angle cosine, and the y-coordinate is equal to the center y-coordinate plus the ray length multiplied by the angle sine. The ray parameters are substituted into the equations of the outer and inner contour ellipses respectively, and the intersection points formed along the positive direction of the rays are taken. The distance from the intersection point of the outer contour to the intersection point of the inner contour forms a wall thickness value. Thus, eight wall thickness values are obtained, and the values not exceeding the remaining seven values are retained as the wall thickness boundary of the induction electromagnetic penetration range of this channel. After the furnace body is powered, the Celsius value of the 304L stainless steel sheath surface at the outlet of the furnace body power supply section is read, and the resistivity and permeability under the corresponding Celsius conditions are obtained from the material property file of the same batch of 304L materials. When the material property file uses discrete Celsius points, if the current Celsius value is between two adjacent data points, the resistivity and permeability are converted according to the linear ratio between the two data points to form the resistivity and permeability used for the current calculation. The electromagnetic penetration depth is obtained by dividing resistivity by the product of pi, the induced frequency, and the permeability, and then taking the square root of the quotient. The induced frequency boundary is calculated based on the relationship that the electromagnetic penetration depth does not exceed the retained wall thickness of the current channel. This is achieved by first dividing resistivity by the product of pi, the permeability, and the square of the retained wall thickness of the current channel; the result is used as the initial value of the induced frequency. When the induction power supply uses discrete frequency ranges, the first range that reaches the initial value of the induced frequency is selected from the frequency ranges supported by the equipment. When the equipment supports stepless adjustment, the calculated initial value of the induced frequency is used directly. After determining the frequency, keep the length of the induction power supply section unchanged, and then change the induction power so that the surface Celsius value of the 304L stainless steel sheath when it leaves the induction power supply section enters the annealing Celsius range specified in the 304L processing document; after the Celsius state changes, re-obtain the resistivity and permeability according to the exit Celsius value and recalculate the electromagnetic penetration depth; when the recalculated electromagnetic penetration depth exceeds the reserved wall thickness value of this pass, adjust the induction frequency to the equipment setting corresponding to the recalculated frequency boundary, and then readjust the induction power; repeat the calculation of frequency and power in this order until the electromagnetic penetration depth does not exceed the reserved wall thickness value of this pass, and at the same time, the surface Celsius value of the exit sheath is within the 304L annealing Celsius range; When the calculated induction frequency exceeds the current operating range of the induction power supply, instead of extending the induction time to replace frequency adjustment, the current induction process is stopped, and the induction power supply or induction coil with a frequency range that covers the calculated result is used and the process is restarted. In this way, the electromagnetic penetration range of the sheath is kept within the actual wall thickness of the current process, and the insufficient frequency range of the equipment is not compensated by extending the action time. Only an axial guide is set between the outlet of the induction power supply section and the entrance of the drawing die, and no additional station is set. After the induction power supply is completed, it immediately enters the drawing die, so that the supplementary energy acting on the 304L stainless steel sheath directly receives the diameter reduction of this section, without increasing the dwell time of the sheath after leaving the induction power supply section and being transferred into the SiO2 insulating medium. Implementation method: Two mutually perpendicular projection directions first form the center and semi-axis of the inner and outer contours in two orthogonal directions, and then the intersection points of eight fixed circumferential directions are recovered by the ellipse equation. Therefore, the eight wall thickness values all come from two sets of geometric data of the same detection section. The four copper core wires are calculated one by one using 24 number combinations to calculate the square of displacement, so that the coordinate components formed by the two projection directions can inherit the core wire number in each diameter reduction. The induction frequency is first calculated from the sheath wall thickness, resistivity and permeability of this channel. The induction power is then used to change the Celsius state of the sheath exit. After the change in power causes the material parameters to change, the electromagnetic penetration depth is calculated again to ensure that the wall thickness limit and the annealing Celsius range are established simultaneously in the same process. The induction frequency is responsible for the radial range of action, and the induction power is responsible for the energy input per unit time. The two are not replaced by the same variable. Example 3: Closed boundary migration, drying end face opening and end treatment; During the initial assembly stage of the cable blank, the reserved length of the empty pipe section at the traction end is determined according to the number of times the traction head needs to be replaced; the length occupied by the first pressing and welding is recorded as the length of the closed section, the length that the tool needs to retain when cutting the old closed section is recorded as the cutting allowance, and the length occupied by the traction head processing required for the next pulling die is recorded as the traction head length; the empty pipe section at the traction end should at least cover the length of each closed section, each cutting allowance, each traction head length, and the length that needs to be retained for the final termination; each length is obtained directly according to the structural dimensions of the welding fixture, cutting fixture, and traction fixture, without supplementing the pipe section based on the diameter reduction result; When the traction head needs to be replaced for the first time, do not cut off the original traction head first. Select a new pressing position on the side of the original closed section closest to the SiO2 insulating medium, press the 304L stainless steel hollow pipe section together so that the relative pipe walls are in contact, and then weld along the circumference of the pressed section to form an inner closed section. After the inner closed section is formed, check the metal closure state of the circumferential weld. After confirming that the weld has formed a closed ring boundary around the 304L stainless steel pipe, cut off the original closed section and the original traction head from the side of the inner closed section away from the SiO2 insulating medium. After cutting off, use the hollow pipe material retained on the outside of the inner closed section to process the traction head required for the next pulling mold. Each subsequent mold change is performed in the same order: first, a new inner closed section is formed, then the outer closed section and traction head are cut off, and then a new traction head is processed. The old and new closed sections overlap in the axial direction for a period of protection. Therefore, the SiO2 insulating dielectric end face is always within at least one metal closed boundary during the mold change, and there is no processing stage of opening the end face first and then re-closing it. After the final diameter reduction is completed, the end-sealed section is retained, and the cable is sent into the drying end cavity. The drying end cavity includes a sealed cavity, a nitrogen inlet, an exhaust port, a molecular sieve drying cylinder, a cable entry sealing sleeve, a glove operating port, and an insulation resistance test lead-out terminal. Nitrogen first passes through the molecular sieve drying cylinder, then enters the cavity through the nitrogen inlet and exits through the exhaust port. After the cable passes through the sealing sleeve, the sealing sleeve is closed, and the end-sealed section is left uncut. Before cutting off the sealed section, keep dry nitrogen flowing from the inlet to the outlet; dew point measuring elements are installed at the nitrogen inlet and outlet respectively; after the difference between the dew point at the outlet and the dew point at the inlet is within one display resolution unit of the dew point meter, keep the nitrogen flowing and start end processing; the dew point judgment is only used to determine that the cavity has completed the dry gas replacement when the end face is open, and is not used as the result of cable performance judgment. Inside the drying end cavity, cut off the end sealing section, then strip 12-15mm of the 304L stainless steel sheath at the end, exposing the four copper core wires and the SiO2 insulation medium end face inside the drying end cavity; when stripping the sheath, cut the sheath along the cable axis, without pressing the cutting tool into the SiO2 insulation medium direction; after removing the sheath, clean up the metal chips, keeping the numbering of the four copper core wires unchanged; After the end is opened, four insulation resistance tests are performed. The first test uses copper core wire No. 1 as the first testing electrode, and copper core wires No. 2, 3, and 4 and the 304L stainless steel sheath are connected in parallel as the second testing electrode. A DC voltage of 500V is applied and held for 1 minute. The second test uses copper core wire No. 2 alone as the first testing electrode, and copper core wires No. 1, 3, and 4 and the 304L stainless steel sheath are connected in parallel. The third and fourth tests are performed on copper core wires No. 3 and No. 4 respectively in the same way, thus forming four insulation resistance results. If all four insulation resistance results exceed 1GΩ, the end drying process is terminated, and the core wire positioning and contact welding are performed. If any result does not exceed 1GΩ, the cable is kept in the drying end cavity, and nitrogen gas treated with molecular sieve is blown towards the SiO2 insulating medium end face for 1 minute. Then, the same wiring method is repeated four times to perform the 500V DC insulation resistance test for 1 minute. The 1-minute blow and the four re-tests constitute one processing cycle. If the insulation resistance reading for the same copper core wire does not change within one resolution unit of the tester in two adjacent processing cycles, and the result does not exceed 1GΩ, the termination welding process is stopped; end protection is re-formed and the entire section is transferred to drying treatment, without endless repeated purging in the drying termination cavity; after adopting this exit method, 1GΩ still serves as the only electrical performance boundary for entering welding, and the changes in readings in two adjacent cycles only serve as the processing judgment for ending invalid purging; After entering the termination process, a four-hole ceramic positioning body is installed inside the metal transition sleeve. The four holes are set according to the core wire numbers 1 to 4. The exposed roots of the copper core wires are first insulated and moisture-proofed, and then passed into the corresponding axial positioning holes. After the copper core wires pass through the positioning holes, they maintain an effective length of 5mm between themselves and the contact welding cups. The four copper core wires are welded to the four contact welding cups in sequence. After the core wire welding is completed, the circumferential welding of the 304L stainless steel sheath to the metal transition sleeve and the circumferential welding of the metal transition sleeve to the connector tail sleeve are completed, so that the originally open SiO2 insulating dielectric end face is once again in the closed area enclosed by the metal transition sleeve, ceramic positioning body and connector tail structure. Implementation method: The migration of the closed boundary relies on the processing sequence to maintain end face isolation: the new metal closed boundary is formed first, and the old closed boundary is cut off later; the reserved length of the empty pipe section is pre-calculated according to the number of migrations and the actual length occupied each time, so that the closure process will not be interrupted due to the exhaustion of end material when multiple mold changes are made. The dry termination cavity serves as a transition space between the SiO2 end face and the joint closed state. The end face is only open in a dry nitrogen environment. A 1-minute purging and four-core insulation resistance check are used to determine whether to proceed to welding. After the copper core welding, sheath welding and joint tail sleeve welding are completed, the end face re-enters the closed structure. Ordinary working environment is not used as an intermediate step in the termination process. Example 4: Assembly of final core position conversion, metal transition sleeve and matching cable connector; After the final Φ5.0 diameter reduction is completed, the center coordinates of copper core wires No. 1 to No. 4 are obtained at the die outlet according to the double projection method of Example 2, and the circumferential reference direction of the cable is retained; when establishing the cable cross-section coordinate system, the center of the 304L stainless steel sheath is used as the coordinate origin, the circumferential reference direction is used as the 0° direction, and the center coordinates of all core wires are converted to millimeters. A four-hole ceramic locator is installed inside the metal transition sleeve. The four axial locating holes are numbered as hole 1, hole 2, hole 3, and hole 4, respectively. An axial orientation groove is machined on the outer circumference of the metal transition sleeve. The angular position of the center of hole 1 relative to the axial orientation groove is fixed during the part machining stage. Starting from hole 1, holes 2, 3, and 4 are determined in the same circumferential sequence. After the ceramic locator is fixed inside the metal transition sleeve, it does not rotate relative to the circumference, so that the axial orientation groove becomes the mechanical angular reference for the four axial locating holes. When establishing the coordinate system of the positioning holes, the axis of the ceramic positioning body is taken as the origin of the coordinate system, and the radial direction where the axial orientation groove is located is taken as the 0° direction. The center coordinates of the four axial positioning holes are converted into millimeters. Copper core wire No. 1 and hole No. 1, copper core wire No. 2 and hole No. 2, copper core wire No. 3 and hole No. 3, and copper core wire No. 4 and hole No. 4 form a fixed pairing relationship respectively. Starting from 0°, rotate the four-hole ceramic positioning body around the central axis in increments of 1° up to 359°. For each angular position, calculate the center coordinates of the four axial positioning holes after rotation using planar rotation coordinates. Then, calculate the planar distances between the center of core wire 1 and the center of hole 1, the center of core wire 2 and the center of hole 2, the center of core wire 3 and the center of hole 3, and the center of core wire 4 and the center of hole 4, respectively. Add the four planar distances to obtain the distance sum for the current angular position. After completing the calculation of 360 angular positions, retain the angular positions that do not exceed the sum of the remaining 359 distances from the 360 distance sums. When two angular positions have the same distance sum, retain the angular position that appears first in ascending order from 0° to 359°. After determining the angular position, a geometric check of the core wire through-hole is performed. For each group of core wires and axial positioning holes, the planar distance from the center of the rotated core wire to the center of the hole is calculated and added to the radius of the copper core wire. If the sum does not exceed the radius of the axial positioning hole, the corresponding core wire can enter the positioning hole axially. After all four groups meet this relationship, the ceramic positioning body is fixed according to the calculated angular position. If any group does not meet the requirement, the termination of this part is stopped, and the position of the core wire inside the SiO2 insulating medium is not changed by forced bending. An axial stop surface is provided inside the metal transition sleeve; after the corner position of the ceramic positioning body is determined, four copper core wires are passed through the four axial positioning holes respectively, and the 304L stainless steel sheath is inserted into the metal transition sleeve and abuts against the axial stop surface. Then, circumferential welding is performed along the junction of the 304L stainless steel sheath and the metal transition sleeve; the axial stop surface limits the axial position of the metal transition sleeve relative to the cable body, and the axial orientation groove limits the circumferential position of the metal transition sleeve. When it is necessary to form a cable product without a joint installed, a cut-off metal end cap is installed at the end of the metal transition sleeve away from the cable body, and circumferentially welded along the junction of the metal end cap and the metal transition sleeve; the ends of the four copper core wires, the four-hole ceramic positioning body, and the end face of the SiO2 insulation medium are formed by a 304L stainless steel sheath, the metal transition sleeve, and the cut-off metal end cap to form a metal closed boundary; when installing the matching cable joint, the cable with the cut-off metal end cap is sent back into the dry termination cavity, and after the metal end cap is cut off in the cavity, it is directly put into the joint assembly; The matching cable connector includes a 316L stainless steel connector housing, a metal end sleeve, a ceramic insulator, four contacts, and a styrene-silicone rubber sealing ring. The ceramic insulator has four through holes, and the four contacts pass through the four through holes respectively, forming four welding cups at the end facing the metal end sleeve. An anti-rotation positioning surface is provided on the outer periphery of the ceramic insulator, and a positioning surface that fits with the anti-rotation positioning surface is provided inside the 316L stainless steel connector housing. After the ceramic insulator is installed, axial movement is restricted by the axial step, and circumferential rotation is restricted by the positioning surface, so that the four welding cups form a fixed angle relationship with the connector housing. The metal tail sleeve has an annular receiving section inside, and an axial orientation key is provided on the inner wall of the annular receiving section. The angular position of the axial orientation key relative to the four through holes of the ceramic insulator is fixed during the joint assembly stage. An axial stop surface is provided inside the annular receiving section. When the metal transition sleeve is inserted into the annular receiving section, the axial orientation groove slides in along the axial orientation key until the end face of the metal transition sleeve abuts against the axial stop surface. The axial orientation key restricts the circumferential rotation of the metal transition sleeve, and the axial stop surface restricts the insertion depth, thereby transferring the angular position of the four-hole ceramic positioning body calculated in the embodiment to the position of the four contact welding cups. After the four copper core wires are inserted into their respective welding cups, the exposed roots of the copper core wires are kept insulated and moisture-proof, and a 5mm effective length is retained on one side of the welding cup. Then, the four copper core wires are welded to the four contacts. After the core wires are welded, the annular welding part of the metal transition sleeve and the metal tail sleeve is circumferentially welded together. Then, the connection between the metal tail sleeve and the 316L stainless steel connector housing is completed, so that the end face of the SiO2 insulating medium and the exposed roots of the four copper core wires are within the closed area of the connector tail. The styrene-based silicone rubber sealing ring is set between the ceramic insulator and the 316L stainless steel connector housing to provide isolation and sealing around the ceramic insulator. After termination, perform an insulation resistance test at 500V DC for 1 minute, using copper core wires No. 1 to No. 4 as the first test electrode and the remaining three copper core wires connected in parallel with the 304L stainless steel sheath as the second test electrode. After all four results exceed 1GΩ, apply 1600V AC voltage and maintain it for 1 minute. The termination process ends when no breakdown or arcing occurs and the leakage current does not exceed 10mA. Implementation method: The center coordinates of the last copper core wire are not directly adjusted and converted to the joint welding cup position by manual adjustment. Instead, the distances of four sets of core holes are obtained by rotating 0° to 359° angle by angle. Then, the calculated angular position is stored by the axial orientation groove on the outer circumference of the metal transition sleeve. During assembly, the angular position is transferred to the four welding cups by the axial orientation key in the metal tail sleeve. The axial stop surface fixes the insertion depth at the same time, so that the circumferential position and axial position are respectively limited by the mechanical structure. The cut-off metal end cap corresponds to the product stage where the cable manufacturing is completed but the connector has not yet been installed; the end cap is cut off only in the dry termination cavity, so that the closed boundary formed in the manufacturing stage is directly transformed into the closed boundary formed in the connector stage, without setting a normal environment open step in between. Comparative Example 1: Eliminates the need to calculate the time required for each furnace pass; Except for the furnace penetration time control, the other SiO2 filling, end sealing, diameter reduction, induction power supply, drawing speed and termination method are the same as in Example 1; the radial distance from the four copper core wires to the 304L stainless steel sheath is not obtained again in each annealing pass, and the furnace penetration time of 5 min and the furnace traction speed of 1000 mm / min are used in the first pass. Implementation method: The diameter reduction causes the radial transmission distance of SiO2 to change step by step, while the furnace treatment time remains at 5 minutes corresponding to the Φ25 stage. The geometric result formed by the subsequent diameter reduction does not enter the next annealing pass. After omitting the retained value and square conversion of this pass, the transmission chain between "actual cross-sectional size and furnace passage time" is cut off. Therefore, the parameters of the first pass can only be used as fixed process parameters and cannot bear the energy time correction after the geometric changes of each pass. Comparative Example 2: Induction power supply without 304L stainless steel sheath; The following steps are taken: four radial distances are retained, the retention value of this channel is selected, the square conversion of the furnace penetration time is calculated, and the traction speed in the furnace is adjusted. After the furnace body is powered, the induction power supply section is omitted, and the cable directly enters the pulling mold. The 304L stainless steel sheath and copper core wire only accept the furnace body power supply. Implementation method: After eliminating induction power supply, when it is necessary to change the annealing state of 304L stainless steel sheath, only the furnace body setting value in Celsius or the furnace traction speed can be changed. Both variables act simultaneously on 304L stainless steel sheath, SiO2 insulating medium and copper core wire; thus forming a single power supply process again, it is impossible to separately execute the control of copper core wire furnace passage time and the supplementary power supply of 304L stainless steel sheath. Comparative Example 3: The sensing frequency is the same as the first stage setting; The induction power supply section and induction power adjustment are retained, but the induction frequency is determined only once in the first annealing pass; subsequent diameter reduction no longer obtains eight 304L stainless steel sheath wall thickness values, and the resistivity and permeability are no longer updated according to the exit Celsius condition, nor is the electromagnetic penetration depth recalculated. All passes use the first induction frequency. Implementation method: Reducing the diameter will change the wall thickness of the 304L stainless steel sheath, and induction power supply will change the Celsius state of the 304L material; fixed frequency can only maintain the frequency setting of the first pass, and cannot guarantee that the electromagnetic penetration depth of subsequent passes is still limited by the sheath wall thickness of this pass; the purpose of using progressive wall thickness calculation, material parameter update and frequency recalculation is to ensure that each induction power supply uses the actual sheath state of this pass as input. Comparative Example 4: The length of the induction power supply section remains unchanged after the drawing speed is switched; For diameters from Φ25 to Φ12, the drawing speed is 6 m / min. When the diameter of Φ12 is reduced to Φ10.7, the speed is switched to 15 m / min. The remaining diameter reduction dimensions remain unchanged. After the drawing speed is switched, the length of the induction power supply section determined in the 6 m / min stage is still used. The length of the induction power supply section is not recalculated by multiplying 15 m / min by the sheath annealing time. Implementation method: The actual working time of the induction power supply section is equal to the length of the induction power supply section divided by the drawing speed; when the length of the induction power supply section is fixed and the drawing speed is changed from 6m / min to 15m / min, the actual residence time of the 304L stainless steel sheath in the induction power supply section varies with the speed; the length of the induction power supply section is re-determined by "drawing speed multiplied by sheath annealing time" in order to keep the sheath annealing time itself unchanged when the drawing method is switched. Comparative Example 5: The closed boundary migration and drying end face treatment are omitted; The diameter reduction and annealing process remains the same as in Example 1; when changing the mold, the original traction head and the original closed section are cut off first, and then the new closed section is processed; after the final diameter reduction, the end closed section is cut off in the normal operation area and the 304L stainless steel sheath is stripped off. It does not enter the drying terminal cavity, nor does it perform 1 minute nitrogen purging and insulation resistance re-check. It directly enters the copper core wire positioning and contact welding. Implementation method: First, cutting off the original closed section will create an open stage of SiO2 end face before the formation of the new closed section; after the final diameter reduction, opening the end in the normal operation area will create a second open stage between the manufacturing closed state and the joint closed state; Example 3 adopts the sequence of "first forming the inner closed section, then cutting off the outer closed section" and "opening the end face after entering the drying end cavity", so that there is always a metal closed boundary or dry gas isolation space between the two manufacturing stages; The 1-minute nitrogen purging and 1 GΩ entry into the welding boundary are responsible for the end treatment process control, but not for proving the invention's effects; their function is to determine when the dried SiO2 end face ends the drying process and enters the welding process. Comparative Example 6: The calculation of the final core position rotation and mechanical orientation transfer are omitted; The four-hole ceramic positioning body, metal transition sleeve and matching connector are retained, but the center coordinates of the four copper core wires are not recorded after the final diameter reduction, and the distance and calculation from 0° to 359° in 1° intervals are not performed; the axial orientation groove is omitted on the outer periphery of the metal transition sleeve, and the axial orientation key is omitted inside the metal tail sleeve. During assembly, the operator rotates the ceramic positioning body and bends the four copper core wires so that the copper core wires enter the corresponding welding cup. Implementation method: After eliminating the rotation calculation, the circumferential position of the four-hole ceramic positioning body is no longer determined by the actual core position of the last cable; after eliminating the axial orientation groove and axial orientation key, even if a perforation position is obtained by manual adjustment at the end, there is no structural support for the angular position transmission when the metal transition sleeve is inserted into the connector; in Example 4, the core position data of the last cable is converted into the angular position of the ceramic positioning body, and then the angular position is fixed to the axial orientation groove, axial orientation key and four welding cups in sequence, so that the core position acquisition, hole position selection and connector assembly form the same mechanical position chain.
[0018] Table 1 Results of the first five diameter reduction processes:
[0019] Table 1 shows the dimensional changes of the cable blank from Φ25 to Φ9.3 for the first five stages; the first three stages are drawn at 6m / min, and when Φ12 is reduced to Φ10.7, the speed is switched to 15m / min. Therefore, Φ12 simultaneously constitutes the position for the change of drawing method and drawing speed; the diameter reduction ratio adopts the process values that have been formed in the production process. The drawing speed only applies to the induction power supply section and the drawing stage, and is not used in conjunction with the furnace traction speed. When calculating the length of the induction power supply section, use 6 m / min or 15 m / min in Table 1 as the speed input, so that the drawing mode can be switched to the induction power supply section length calculation. Table 2 Results of the last five diameter reduction processes:
[0020] Table 2 follows the Φ9.3 state in Table 1, and reaches Φ5.0 after five rounds of coil drawing; the 6th to 10th rounds maintain a drawing speed of 15m / min, so that the drawing speed no longer constitutes the change between subsequent rounds, and the length of each induction power supply section is determined by the annealing time of the sheath. Tables 1 and 2 together form a chain of dimensions from Φ25 to Φ5.0. After each reduction pass is completed, the new cross section is used to obtain the four radial distances and sheath wall thickness for the next annealing pass. Therefore, the subsequent furnace penetration time, furnace traction speed and induction frequency are all based on the cross section that has been formed. Table 3. Calculation results of radial distance variation and furnace penetration parameters:
[0021] In Table 3, the first pass retention value is recorded as 1, and the first pass duration of 5 min and the furnace body power supply section length of 5000 mm are used as the calculation basis. Five sets of radial distance ratios are used to calculate the furnace penetration relationship. Table 3 illustrates how the radial distance, once obtained, can lead to a unique furnace penetration result. Taking a radial distance ratio of 0.9 as an example, 0.9 squared equals 0.81, 0.81 multiplied by 5 min equals 4.05 min, and then 5000 mm divided by 4.05 min equals 1234.6 mm / min. The remaining groups are calculated in the same order. Therefore, once the retention value for this pass is obtained, the furnace penetration time and the traction speed inside the furnace are determined accordingly. The values 0.95, 0.9, 0.85, and 0.8 in the table are calculated inputs and do not represent the radial distance obtained from the cable trial production. In actual processing, the ratio of the retention value of this pass to the retention value of the first pass obtained by X-ray is used instead of the calculated input. The first pass's 5000mm, 1000mm / min and 5min maintain a relationship of 5000÷1000=5, and only the time ratio generated by the radial distance is changed in subsequent passes. Table 4. Results of Sheath Wall Thickness Variation and Induction Frequency Calculation:
[0022] In one calculation, the resistivity and permeability of 304L stainless steel are kept constant. The sheath wall thickness, electromagnetic penetration depth and induced frequency in the first calculation state are recorded as 1, and the constraint relationship between the wall thickness change and the induced frequency is calculated. The electromagnetic penetration depth is inversely related to the square root of the induction frequency. Therefore, when the sheath wall thickness ratio changes from 1 to 0.8, in order to keep the electromagnetic penetration depth synchronously limited to 0.8, the induction frequency ratio is 1 divided by 0.8 squared, resulting in 1.5625; when the sheath wall thickness ratio is 0.6, the frequency ratio is 1 divided by 0.6 squared, resulting in 2.7778. Table 4 is used for numerical verification of the induction frequency calculation chain. In actual processing, eight sheath wall thickness values are first formed by two X-ray projections, and then the values of no more than the remaining seven are retained. Then, the resistivity and permeability of the 304L stainless steel in this process are substituted to obtain the induction frequency. After the induction power is adjusted to change the Celsius value at the sheath exit, the resistivity and permeability are obtained again according to the Celsius value at the exit and the electromagnetic penetration depth is recalculated. Therefore, the fixed material parameters in Table 4 only represent one frequency calculation process and do not replace the material parameter update in the processing. Table 5. Calculation results of drawing speed and induction power supply section length:
[0023] In Table 5, 1s, 2s and 3s were taken as time calculation inputs to verify the calculation relationship of the length of the induction power supply section under two pulling speeds of 6m / min and 15m / min. 6 m / min is converted to 100 mm / s, and 15 m / min is converted to 250 mm / s; the length of the induction power supply section is obtained by multiplying the drawing speed by the sheath annealing time. Therefore, when the sheath annealing time remains unchanged, if the drawing speed changes from 6 m / min to 15 m / min, the length of the induction power supply section will simultaneously become 2.5 times the original length. Taking the 2s calculation of the action time as an example, the length of the induction power supply section is 200mm in the 6m / min stage and 500mm in the 15m / min stage; the action time obtained by dividing the length of the induction power supply section by the pulling speed in both states is 2s; this shows that after the pulling speed is changed from Φ12 to Φ10.7, the length of the induction power supply section needs to be recalculated, and the axial length in the 6m / min stage cannot be kept unchanged; Table 6 Existing Measured Foundations and Processing Judgment Boundaries for Cable and Termination Structures:
[0024] In Table 6, the finished product has an outer diameter of 5.0 mm and a single copper core wire cross-sectional area of 1.0 mm². 2 The insulation resistance is not less than 2000MΩ under 500V DC conditions, the leakage current is 1.3mA when 700V / 50Hz is maintained for 1 minute, and the leakage current is 2.1mA when 2000V / 50Hz is maintained for 1 minute. These data serve as references for the structure and electrical performance of the cable consisting of four copper core wires, SiO2 insulation medium and 304L stainless steel sheath. They are used as the basis for evaluating the finished product size, electrical insulation status and withstand voltage status. The termination criteria in Table 6 use a 500V DC voltage held for 1 minute to check the insulation resistance. Once the insulation resistance of all four copper core wires exceeds 1GΩ, the subsequent termination process begins. After termination, a 1600V AC voltage is applied and held for 1 minute. Termination ends when no breakdown or arcing occurs and the leakage current does not exceed 10mA. Thus, Table 6 serves as the endpoint for determining the finished product dimensions, electrical insulation status, and termination completion status, providing clear process termination conditions for open end faces, core wire welding, metal sealing, and electrical performance checks. Tables 1 and 2 show the outer diameter changes and drawing speeds for each reduction pass. The cross-sectional dimensions formed by the reduction are converted into radial distance and furnace penetration parameters in Table 3. The sheath cross-sectional dimensions are calculated into electromagnetic penetration depth and induction frequency in Table 4. The drawing speed is calculated into the induction power supply section length in Table 5. After reducing diameter, annealing, induction power supply, and termination, Table 6 provides the finished product dimensions, electrical performance, and termination endpoint. The six tables progressively transition from processing dimensions to furnace penetration time, furnace traction speed, induction range, induction power supply section length, and termination results, forming a progressively connected data chain of inputs, calculation results, and execution results at each stage.
[0025] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A manufacturing process for cables used in nuclear power plants, characterized in that, include: S1. Place four copper core wires into a 304L stainless steel sheath, fill and compact SiO2 insulating medium between the copper core wires and between the copper core wires and the sheath, and press and weld the empty tube sections at both ends of the 304L stainless steel sheath to form a cable blank. S2. The cable blank is drawn in turns. In the annealing turns, four radial distances from the outer surface of the copper core wire to the inner surface of the sheath are obtained. The values are retained and not exceed the other three values. The furnace penetration time of the current turn is obtained by multiplying the square of the ratio of the retained value of the current turn to the retained value of the first turn by the furnace penetration time of the first turn. The furnace traction speed is determined by dividing the furnace power supply section length by the furnace penetration time of the current turn. S3. After passing through the furnace body power supply section, enter the induction power supply section before the drawing die. Determine the length of the induction power supply section by the product of the drawing speed and the annealing time of the sheath. Adjust the induction power so that the Celsius value when the sheath leaves the induction power supply section enters the Celsius range of 304L stainless steel sheath annealing. Then enter the drawing die to complete this reduction. S4. After this reduction, determine the furnace traction speed for the next annealing pass according to S2. Repeat annealing and reduction until the outer diameter reaches 5mm, and keep the empty tube sections at both ends sealed. S5. After the final diameter reduction, the cable is moved into the drying termination cavity. The closed empty pipe section is cut off in the cavity and the end sheath is stripped. The four copper core wires are inserted into the four-hole ceramic positioning body in the metal transition sleeve. The sheath is welded to the metal transition sleeve, the copper core wires to the contact, and the metal transition sleeve to the connector tail sleeve. A closed termination structure is formed before the SiO2 end face leaves the drying termination cavity.
2. The manufacturing process of the cable used in nuclear power plants according to claim 1, characterized in that, Based on the first furnace penetration time in S2, the parameters of the furnace body power supply section are limited and the conversion of subsequent annealing passes is performed, including: S21. For the first annealing pass, the furnace body is set to 1000°C, the furnace body power supply section length is set to 5000mm, the furnace traction speed is set to 1000mm / min, and 5min is used as the first pass through the furnace. S22. In subsequent annealing passes, the furnace body setting value in Celsius and the furnace body power supply section length remain unchanged. Based on the furnace penetration time obtained in S2, the furnace traction speed is determined by dividing 5000mm by the furnace penetration time, and the furnace penetration is performed according to the determined furnace traction speed.
3. The manufacturing process for cables used in nuclear power plants according to claim 2, characterized in that, Based on the induction power supply section in S3, the electromagnetic penetration range of the 304L stainless steel sheath is limited, including: S31. After the diameter reduction is completed, select the same axial section at the mold exit and collect X-ray projection images along two mutually perpendicular transmission directions. Obtain the outer and inner contours of the 304L stainless steel sheath from the two X-ray projection images. Obtain a wall thickness value every 45° along the circumference and retain no more than the other seven wall thickness values from the eight wall thickness values. S32. Obtain the resistivity and permeability of 304L stainless steel at the outlet of the furnace power supply section in Celsius. Divide the resistivity by the product of pi, the induction frequency and the permeability, and take the square root of the result as the electromagnetic penetration depth. S33. In the next annealing pass, adjust the induction frequency until the electromagnetic penetration depth does not exceed the wall thickness value reserved in S31. Fix the induction frequency and the length of the induction power supply section, and then adjust the induction power so that the surface Celsius value of the 304L stainless steel sheath when it leaves the induction power supply section enters the annealing Celsius range of the 304L stainless steel sheath.
4. The manufacturing process of the cable applied to a nuclear power plant according to claim 3, characterized in that, Based on the two X-ray projection images acquired in S31, the radial distance acquisition and last trace core position recording in S2 are performed, including: S41. Obtain the coordinates of the center, inner contour, and center of the four copper core wires of the 304L stainless steel sheath from the two X-ray projection images respectively. S42. For each copper core wire, draw a radial line passing through the center of the sheath and the center of the copper core wire. Take the length of the line segment between the intersection of the radial line and the outer contour of the copper core wire and the intersection of the radial line and the inner contour of the sheath to form four radial distances, and input the four radial distances into S2. S43. Record the center coordinates of the four copper core wires after each reduction pass, and use the center coordinates of the four copper core wires after the final reduction pass as input for determining the circumferential angle position of the joint during the termination stage.
5. The manufacturing process of the cable applied to a nuclear power plant according to claim 4, characterized in that, The pulling mode is switched based on the reduction path in S4 and the length of the induction power supply section in S3, including: S51. The diameter of the cable blank is reduced sequentially from Φ25 to Φ18, Φ14, Φ12, Φ10.7, Φ9.3, Φ8.0, Φ7.5, Φ6.4, Φ5.5 and Φ5.0, with the diameter reduction ratios for each stage being 28%, 22%, 14%, 11%, 13%, 14%, 6%, 15%, 14% and 9% respectively. For the three reduction passes from S52 to Φ25 to Φ12, a straight-material chain drawing machine is used and the drawing speed is 6m / min. From Φ12 to Φ10.7, a coil drawing machine is used and the drawing speed is 15m / min. When the drawing speed is changed from 6m / min to 15m / min, the supplementary annealing time of the 304L stainless steel sheath is kept unchanged, and the length of the induction power supply section is re-determined by multiplying 15m / min by the supplementary annealing time.
6. The manufacturing process of the cable applied to a nuclear power plant according to claim 5, characterized in that, Based on the closed empty pipe section formed by S1, the closed boundary migration is performed when replacing the formwork and traction head, including: S61. Before cutting off the original traction head, press a 304L stainless steel pipe again on the side of the original closed empty pipe section near the SiO2 insulating medium and weld it circumferentially to form an inner closed section. S62. After the inner sealing section is completed, the original sealing section and the original traction head are cut off. Then, the end of the inner sealing section away from the SiO2 insulating medium is processed into a traction head that is adapted to the next drawing die inlet. S63. Subsequent mold changes shall be performed in the order of first forming the inner closed section and then cutting off the original closed section, so that the end face of the SiO2 insulating medium is always within the weld seal boundary during the replacement of the traction head.
7. The manufacturing process of the cable for use in nuclear power plants according to claim 6, characterized in that, Based on the drying termination cavity in S5, insulation testing and drying treatment are performed after the SiO2 insulating dielectric end face is opened, including: S71. After the final diameter reduction, move the cable with the sealed section into the dry terminal cavity. Cut off the sealed section in the cavity and strip the 304L stainless steel sheath at the end of 12-15mm. Use one copper core wire as the first detection electrode and connect the other three copper core wires and the 304L stainless steel sheath in parallel as the second detection electrode. Apply a DC voltage of 500V and hold for 1 minute. Replace the first detection electrode in sequence until four insulation resistance values are obtained. S72. If any insulation resistance value does not exceed 1GΩ, purge the end face of the SiO2 insulating medium with nitrogen gas dried by molecular sieve for 1 minute, and then repeat the insulation test in S71. Cycle the purging and insulation test until all four insulation resistance values exceed 1GΩ, and then proceed to the copper core wire positioning and contact welding process.
8. The manufacturing process of the cable applied to a nuclear power plant according to claim 7, characterized in that, Based on the center coordinates of the four copper core wires recorded after the final diameter reduction, the circumferential angle position of the joint is determined and the termination is closed, including: S81. Obtain the center coordinates of the four axial positioning holes of the ceramic positioning body. Pair the center coordinates of the four copper core wires with the center coordinates of the four axial positioning holes according to the predetermined core wire numbers. Rotate the ceramic positioning body from 0° to 359° at 1° intervals with the cable axis as the center. Calculate the sum of the planar distances between the four pairs of paired centers for each angular position. Keep the angular positions where the sum of the distances does not exceed the sum of the other 359 distances. S82. Fix the ceramic positioning body at the corner position reserved in S81, so that the four copper core wires are respectively inserted into the four axial positioning holes and welded to the four contact welding cups. Then weld the 304L stainless steel sheath to the metal transition sleeve circumferentially, and weld the metal transition sleeve to the connector tail sleeve circumferentially. S83. After welding, apply a 500V DC voltage between the four copper core wires and the 304L stainless steel sheath and hold for 1 minute. After all four insulation resistance values exceed 1GΩ, apply a 1600V AC voltage and hold for 1 minute. The termination is completed when no breakdown or arcing occurs and the leakage current does not exceed 10mA.
9. A cable used in a nuclear power plant, characterized in that, include: The cable consists of four spaced-apart copper cores, a SiO2 insulation layer surrounding the four copper cores, a 304L stainless steel sheath covering the SiO2 insulation layer, and a metal transition sleeve at the cable end. The cable body has an outer diameter of less than 5mm, and each copper core has a cross-sectional area of 1mm². 2 Within; the metal transition sleeve is circumferentially welded to the 304L stainless steel sheath, and a ceramic positioning body is fixed inside the metal transition sleeve. The ceramic positioning body has four axial positioning holes, and four copper core wires pass through the four axial positioning holes respectively. The end face of the SiO2 insulation layer terminates at the side of the ceramic positioning body facing the cable body. The outer circumference of the metal transition sleeve is provided with an axial orientation groove. The angular position of the four axial positioning holes around the axis of the metal transition sleeve is limited by the axial orientation groove. The end of the metal transition sleeve away from the cable body is circumferentially sealed by a cut-off metal end cap.
10. A cable connector used in conjunction with cables in nuclear power plants, characterized in that, include: 316L stainless steel connector housing, metal tail sleeve, ceramic insulator, four contacts and styrene-silicone rubber sealing ring; The metal tail sleeve is connected to the 316L stainless steel connector housing. The ceramic insulator is fixed inside the 316L stainless steel connector housing and has four through holes. Four contacts pass through the four through holes respectively, and the ends of the four contacts facing the metal tail sleeve form welding cups. The mating ends of the four contacts adopt a copper-plated nickel structure. The metal tail sleeve has an annular receiving section for the insertion of the metal transition sleeve at the end of the cable. The inner wall of the annular receiving section has an axial orientation key, which is used to embed into the axial orientation groove on the outer circumference of the metal transition sleeve. The angular position of the four welding cups around the axis of the connector housing is defined by the axial orientation key. The outer circumference of the annular receiving section has an annular welding part. After the metal transition sleeve is inserted into the annular receiving section, it is circumferentially welded to the metal tail sleeve through the annular welding part. A styrene-based silicone rubber sealing ring is set between the ceramic insulator and the 316L stainless steel connector housing.