An encapsulated electron gun and its fabrication method, and vacuum electronic devices.

By employing a conical ceramic ring structure in the electron gun of a vacuum electronic device, the local electric field and electron trajectory are adjusted, thus solving the problem of surface flashover of the electron gun under high potential difference and improving the insulation and sealing performance of the device.

CN123120582APending Publication Date: 2026-11-17SOUTHEAST UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611380279.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-07
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In existing vacuum electronic devices, electron guns are prone to surface flashover under high potential difference and vacuum conditions. This is mainly due to the local electric field enhancement and field-induced electron emission caused by solder burrs, particles or sealing gaps, which in turn leads to secondary electron multiplication and surface charge accumulation.

Method used

A conical ceramic ring structure is adopted, and the design of the outer and inner ceramic rings is changed so that their width gradually decreases along the electron gun axis, and a conical surface is formed between the inner and outer circumferences. This adjusts the local electric field and electron trajectory, reducing the possibility of electrons bombarding the surface of the ceramic ring.

Benefits of technology

It effectively suppresses surface flashover, reduces the risk of electron bombardment and secondary electron multiplication, and improves the insulation reliability and vacuum sealing of the electron gun.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120582A_ABST
    Figure CN123120582A_ABST
Patent Text Reader

Abstract

This disclosure provides a sealed electron gun and its fabrication method, as well as a vacuum electronic device. The sealed electron gun includes: an anode, a control electrode, a cathode, an anode connector, an outer ceramic ring, a control electrode connector, an inner ceramic ring, and a cathode connector. The anode connector, outer ceramic ring, control electrode connector, inner ceramic ring, and cathode connector form a coaxial sealed structure from the outside to the inside in a radial direction. The anode, control electrode, and cathode are arranged along the axial direction of the electron gun. At least one of the outer and inner ceramic rings is a conical ceramic ring. The conical ceramic ring is generally annular, and its width along the axial direction of the electron gun gradually decreases from the inner circumference to the outer circumference, making the inner circumference wider than the outer circumference, and forming a conical surface extending around the electron gun axis between the inner and outer circumferences. This disclosure can reduce the possibility of electron bombardment of the ceramic ring surface and the resulting secondary electron multiplication, thereby suppressing the development of surface flashover and reducing the risk of surface flashover.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of vacuum electronics technology, and in particular to an encapsulated electron gun and its fabrication method, as well as vacuum electronic devices. Background Technology

[0002] Electron guns in vacuum electronic devices such as traveling wave tubes and klystrons are used to generate, modulate, and extract electron beams. They typically include electrodes such as anodes, control electrodes, and cathodes. A high potential difference exists between the electrodes inside the electron gun, and the insulating structure, which provides mechanical support, vacuum sealing, and electrical insulation, needs to remain stable under vacuum, high electric field, and thermal cycling conditions. During electron gun manufacturing, different joining processes are employed depending on the materials and the objects being joined, such as brazing, laser welding, argon arc welding, and diffusion welding. Among these, brazing is typically used to form a ceramic-metal sealing interface with mechanical strength and hermeticity between the insulating ceramic and the metal connector.

[0003] Figure 1 This is a schematic diagram of the axial cross-sectional structure of an encapsulated electron gun in related technologies, such as... Figure 1 As shown, the enclosed electron gun includes an anode 1', a control electrode 2', and a cathode 3', as well as an anode connector 4', an outer ceramic ring 5', a control electrode connector 6', an inner ceramic ring 7', and a cathode connector 8'. Based on a near-cylindrical annular body, the outer ceramic ring 5' and the inner ceramic ring 7' have annular protrusions that extend continuously in the circumferential direction on the surface of the annular body. The annular protrusions can increase the creepage distance on the surface of the insulator and reduce the risk of withstand voltage degradation caused by the formation of a through-deposition layer of cathode evaporates on the surface of the insulator.

[0004] However, the aforementioned annular protrusions are mainly used to extend the surface creepage distance and block the surface penetration path. In the three-in-one region where ceramic, metal and vacuum intersect, solder burrs, particles or sealing gaps may also cause local electric field enhancement and field-induced electron emission. After the emitted electrons bombard the insulating surface, they may trigger secondary electron multiplication, surface charge accumulation and gas desorption, thereby promoting the development of surface flashover. Summary of the Invention

[0005] This disclosure provides an encapsulated electron gun and its fabrication method, as well as a vacuum electronic device. Without changing the basic electrode composition and encapsulation connection layers of the electron gun, at least one of the outer and inner ceramic rings is made of conical ceramic ring according to the potential difference, local field strength, and structural requirements of each insulating section. This adjusts the local electric field and electron trajectory near the corresponding sealing area, reduces the possibility of electron bombardment of the ceramic ring surface and the resulting secondary electron multiplication, thereby suppressing the development of surface flashover and reducing the risk of surface flashover.

[0006] To achieve the above objectives, in a first aspect, a sealed electron gun is provided, comprising: an anode, a control electrode, a cathode, an anode connector, an outer ceramic ring, a control electrode connector, an inner ceramic ring, and a cathode connector; The anode connector, outer ceramic ring, control electrode connector, inner ceramic ring and cathode connector form a coaxial sleeve structure in a radial direction from the outside to the inside, and the anode, control electrode and cathode are arranged along the electron gun axis; At least one of the outer ceramic ring and the inner ceramic ring is a conical ceramic ring. The conical ceramic ring is generally annular, and its width along the electron gun axis gradually decreases from the inner circumference to the outer circumference, making the inner circumference of the conical ceramic ring wider than the outer circumference, and forming a conical surface extending around the electron gun axis between the inner and outer circumferences. The outer circumferential surface of the outer ceramic ring is sealed to the anode connector, and the inner circumferential surface is sealed to the control electrode connector; The outer circumferential surface of the inner ceramic ring is sealed to the control electrode connector, and the inner circumferential surface is sealed to the cathode connector; The anode connector, control electrode connector, and cathode connector are insulated from each other by the outer and inner ceramic rings, and together form a vacuum-sealed structure for the electron gun.

[0007] In conjunction with the first aspect, in one possible implementation, the conical surface of each of the conical ceramic rings is a rotary conical surface.

[0008] In conjunction with the first aspect, in one possible implementation, the angle between the generatrix of the conical surface of each of the conical ceramic rings and the axis of the electron gun is 30° to 60°.

[0009] In conjunction with the first aspect, in one possible implementation, the ceramic between the outer ceramic ring and the anode connector and the control electrode connector... The metal sealing interface, and the ceramic between the inner ceramic ring and the control electrode connector and the cathode connector. The metal sealing interface is sealed by brazing.

[0010] In conjunction with the first aspect, in one possible implementation, each of the said conical ceramic rings is made of alumina ceramic.

[0011] Secondly, a method for manufacturing a sealed electron gun is provided, including: An anode, a control electrode, a cathode, an anode connector, an outer ceramic ring, a control electrode connector, an inner ceramic ring, and a cathode connector are prepared. At least one of the outer ceramic ring and the inner ceramic ring is a conical ceramic ring. The conical ceramic ring is generally annular, and its width along the electron gun axis gradually decreases from the inner circumference to the outer circumference, making the inner circumference of the conical ceramic ring wider than the outer circumference, and forming a conical surface extending around the electron gun axis between the inner and outer circumferences. The outer ceramic ring is placed between the anode connector and the control electrode connector, and the inner ceramic ring is placed between the control electrode connector and the cathode connector, and all components are positioned coaxially. The outer ceramic ring is sealed to the anode connector and the control electrode connector, and the inner ceramic ring is sealed to the control electrode connector and the cathode connector to form an electron gun insulation and vacuum sealing assembly with a sleeve structure. The anode, control electrode, and cathode are assembled and connected to their respective connectors, and the resulting assembly is then subjected to a vacuum sealing test.

[0012] In conjunction with the second aspect, in one possible implementation, the ceramic between the outer ceramic ring and the anode connector and the control electrode connector... The metal sealing interface, and the ceramic between the inner ceramic ring and the control electrode connector and the cathode connector. The metal sealing interface is sealed by brazing. Before brazing, the surfaces of the ceramic ring and metal connector to be welded are cleaned, assembled and positioned, and the brazing gap is checked.

[0013] In conjunction with the second aspect, in one possible implementation, the vacuum seal inspection includes an airtightness inspection, and after the airtightness inspection is passed, the electron gun is subjected to vacuum baking and high-pressure aging.

[0014] Thirdly, a vacuum electronic device is provided, including an encapsulated electron gun as described in the first aspect, or in any possible embodiment in conjunction with the first aspect.

[0015] In conjunction with the third aspect, in one possible implementation, the vacuum electronic device is a traveling wave tube or a klystron.

[0016] The beneficial effects of the embodiments disclosed herein include: (i) The conical surface of the conical ceramic ring can change the direction of the local electric field and the trajectory of electrons near the triple bonding region, causing electrons emitted from the triple bonding region to tend to move away from the surface of the ceramic ring, reducing the possibility of electron bombardment, secondary electron multiplication, surface charge accumulation and gas desorption, thereby suppressing the development of surface flashover and reducing the risk of surface flashover.

[0017] (ii) At least one of the outer ceramic ring and the inner ceramic ring shall be a conical ceramic ring, so that the conical structure can be preferentially configured in the insulation section with high requirements for potential difference, local field strength or surface insulation; when necessary, the interface of the two insulation levels may be made of conical ceramic rings, which is suitable for the coaxial layer structure of the electron gun.

[0018] (iii) This structure is achieved by changing the axial width of the ceramic ring along the radial direction, without changing the basic functions of the anode, control electrode and cathode, which makes it easy to apply in existing sleeve connection layers.

[0019] (iv) The ceramic ring and the adjacent metal connector can still use the mature ceramic-metal brazing process, while other metal-metal connections of the electron gun can be selected according to the material and structure, which is conducive to the connection with the existing electron gun manufacturing process.

[0020] (v) The electron gun with the conical ceramic ring can be used as an electron emission component for different vacuum electronic devices such as traveling wave tubes and klystrons, and has good device applicability. Attached Figure Description

[0021] Figure 1 This is a schematic diagram of the axial cross-sectional structure of an encapsulated electron gun in related technologies; Figure 2 This is an axial cross-sectional view of an electron gun with a sleeve structure provided in an embodiment of this disclosure.

[0022] Explanation of reference numerals in the attached figures: 1'. Anode; 2'. Control electrode; 3'. Cathode; 4'. Anode connector; 5'. Outer ceramic ring; 6'. Control electrode connector; 7'. Inner ceramic ring; 8'. Cathode connector; 1. Anode; 2. Control electrode; 3. Cathode; 4. Anode connector; 5. Outer ceramic ring; 6. Control electrode connector; 7. Inner ceramic ring; 8. Cathode connector. Detailed Implementation

[0023] This disclosure provides an encapsulated electron gun and its fabrication method, as well as a vacuum electronic device. Preferred embodiments of this disclosure are described below with reference to the accompanying drawings. It should be understood that the preferred embodiments described herein are for illustrative and explanatory purposes only and are not intended to limit the scope of this disclosure. Furthermore, the embodiments and features described herein can be combined with each other unless otherwise specified.

[0024] This disclosure provides an enclosed structure electron gun. Figure 2 This is an axial cross-sectional view of an electron gun with a sleeve structure provided in an embodiment of this disclosure, as shown below. Figure 2 As shown, the enclosed electron gun includes: anode 1, control electrode 2, cathode 3, anode connector 4, outer ceramic ring 5, control electrode connector 6, inner ceramic ring 7, and cathode connector 8. Anode connector 4, outer ceramic ring 5, control electrode connector 6, inner ceramic ring 7 and cathode connector 8 form a coaxial sleeve structure in the radial direction from the outside to the inside. Anode 1, control electrode 2 and cathode 3 are arranged along the electron gun axis. At least one of the outer ceramic ring 5 and the inner ceramic ring 7 is a conical ceramic ring. The conical ceramic ring is ring-shaped in general, and its width along the electron gun axis gradually decreases from the inner circumference to the outer circumference, making the inner circumference of the conical ceramic ring wider than the outer circumference, and forming a conical surface extending around the electron gun axis between the inner and outer circumferences. The outer circumferential surface of the outer ceramic ring 5 is sealed to the anode connector 4, and the inner circumferential surface is sealed to the control electrode connector 6; The outer circumferential surface of the inner ceramic ring 7 is sealed to the control electrode connector 6, and the inner circumferential surface is sealed to the cathode connector 8; The anode connector 4, the control electrode connector 6, and the cathode connector 8 are insulated from each other by the outer ceramic ring 5 and the inner ceramic ring 7, and together they form the vacuum-sealed structure of the electron gun.

[0025] It should be noted that the accompanying drawings are only for illustrating the structural relationship of the present invention and are not drawn to scale. Those skilled in the art can adjust the specific dimensions and materials according to the voltage level, operating voltage waveform, operating current, vacuum degree, material properties and assembly space of the electron gun without departing from the technical concept of the present invention.

[0026] In this embodiment, the anode connector 4, outer ceramic ring 5, control electrode connector 6, inner ceramic ring 7, and cathode connector 8 form a coaxial hierarchy from the outside to the inside around the axis. At least one of the outer ceramic ring 5 and the inner ceramic ring 7 is a conical ceramic ring, which is beneficial for adjusting the local electric field and electron trajectory, reducing the risk of surface flashover. This electron gun is suitable for vacuum electronic devices such as traveling wave tubes and klystrons.

[0027] At least one of the outer ceramic ring 5 and the inner ceramic ring 7 is a conical ceramic ring, including: the outer ceramic ring 5 is a conical ceramic ring, the inner ceramic ring 7 is a conical ceramic ring, and both the outer ceramic ring 5 and the inner ceramic ring 7 are conical ceramic rings.

[0028] Figure 2 In the illustrated embodiment, both the outer ceramic ring 5 and the inner ceramic ring 7 are conical ceramic rings, i.e., the entire ring is annular. The width of each ceramic ring along the electron gun axis gradually decreases from the inner circumference to the outer circumference, making the inner circumference wider than the outer circumference, and forming a conical surface extending around the electron gun axis between the inner and outer circumferences. The outer circumferential surface of the outer ceramic ring 5 is positioned opposite to and sealed with the inner circumferential surface of the anode connector 4, and the inner circumferential surface of the outer ceramic ring 5 is positioned opposite to and sealed with the outer circumferential surface of the control electrode connector 6. The outer circumferential surface of the inner ceramic ring 7 is positioned opposite to and sealed with the inner circumferential surface of the control electrode connector 6, and the inner circumferential surface of the inner ceramic ring 7 is positioned opposite to and sealed with the outer circumferential surface of the cathode connector 8. Thus, the control electrode connector 6 is located between the outer ceramic ring 5 and the inner ceramic ring 7. The outer ceramic ring 5 provides insulation between the anode connector 4 and the control electrode connector 6, and the inner ceramic ring 7 provides insulation between the control electrode connector 6 and the cathode connector 8. The conical surfaces of the outer ceramic ring 5 and the inner ceramic ring 7 are arranged according to... Figure 2 The respective sealing positions are shown.

[0029] In other embodiments, one of the outer ceramic ring 5 and the inner ceramic ring 7 is the aforementioned conical ceramic ring, while the other can be a conical ceramic ring, a near-cylindrical annular ceramic component, an annular ceramic component with an annular protrusion, or other suitable annular insulating structures, depending on the potential difference between their corresponding electrodes, the local electric field distribution, surface insulation requirements, mechanical and sealing strength, and available space. For example, when the potential difference and local field strength between the anode and the control electrode are significantly higher than those between the control electrode and the cathode, the outer ceramic ring 5 can be set as a conical ceramic ring, while the inner ceramic ring 7 can adopt other annular ceramic structures that meet the insulation and sealing requirements between the control electrode and the cathode.

[0030] For the outer ceramic ring 5 and the inner ceramic ring 7, which employ a conical structure, the cone angle, axial width, inner and outer diameters, cone surface length, minimum wall thickness, cone surface direction, and sealing overlap width are determined based on the electrical boundary conditions of the insulation section. These electrical boundary conditions include the potential difference between the anode and the control electrode or between the control electrode and the cathode, the operating voltage waveform, the overall electric field distribution, the tangential electric field strength on the vacuum side surface of the ceramic ring, the local peak field strength at the triple junction point, the uniformity of the electric field along the surface of the ceramic ring, the electron trajectory, the effective surface insulation distance, the ceramic dielectric properties, and the secondary electron emission characteristics. By comprehensively analyzing these factors, the trajectory of electrons emitted from the triple junction region can be kept as far away from the ceramic ring surface as possible, reducing the likelihood of electron bombardment, secondary electron multiplication, surface charge accumulation, and gas desorption promoting surface flashover.

[0031] When determining the above-mentioned structural parameters of the conical ceramic ring, the differences in thermal expansion coefficients between the ceramic and the adjacent metal material, brazing temperature cycles and residual thermal stress, the mechanical strength of the ceramic body, the strength of the ceramic-metal joint, vacuum tightness, pressure difference between the inside and outside of the vacuum, thermal shock, vibration and transportation loads, component stiffness and coaxiality, machining and assembly tolerances, and available space on the vacuum side should also be considered. When both the outer ceramic ring 5 and the inner ceramic ring 7 adopt a conical structure, they are designed according to the above-mentioned boundary conditions of their respective insulation sections. The resulting cone angle and other dimensional parameters can be the same or different. Common metal edge rounding or chamfering structures can continue to be used, but are not essential distinguishing features of this invention.

[0032] In another embodiment provided in this disclosure, the conical surface of each conical ceramic ring is a rotary conical surface.

[0033] In this embodiment, the rotary conical surface eliminates the sharp corners and steps of the traditional structure, effectively preventing local electric field concentration, guiding the electron trajectory away from the ceramic ring surface, and homogenizing the sealing thermal stress, thereby significantly reducing the risk of surface flashover and improving the reliability of vacuum sealing.

[0034] In another embodiment provided in this disclosure, the angle between the generatrix of the conical surface of each conical ceramic ring and the axis of the electron gun is 30° to 60°.

[0035] In this embodiment, by limiting the angle between the conical busbar and the electron gun axis to the range of 30° to 60°, an optimal balance can be achieved between the radial dimension and the axial creepage distance, effectively guiding the electron trajectory away from the ceramic ring surface, significantly reducing the risk of secondary electron multiplication and surface flashover caused by electron bombardment; at the same time, this angle range is conducive to the uniform release of thermal stress during brazing and thermal cycling, taking into account the withstand voltage margin of the insulation section, the structural compactness, and the long-term reliability of the ceramic-metal seal.

[0036] Figure 2 In this embodiment, the angle α5 between the generatrix of the conical surface of the outer ceramic ring 5 and the axis of the electron gun, and the angle α7 between the generatrix of the conical surface of the inner ceramic ring 7 and the axis of the electron gun, are both 45°. The cone angle referred to in this specification is the smaller angle between the corresponding generatrix of the conical surface and the axis of the electron gun. In other embodiments, α5 and α7 can each be within the range of 30° to 60°, and they can be the same or different; the outer ceramic ring 5 and the inner ceramic ring 7 can also adopt continuous conical surfaces or segmented conical surfaces for transition, as long as the required conical surface can be formed at the corresponding sealing interface and a reliable seal with the adjacent metal connector can be maintained.

[0037] In another embodiment provided in this disclosure, the ceramic ring 5 is positioned between the outer ceramic ring 5 and the anode connector 4 and the control electrode connector 6. The metal sealing interface, and the ceramic between the inner ceramic ring 7 and the control electrode connector 6 and the cathode connector 8 The metal sealing interface is sealed by brazing.

[0038] In this embodiment, to ensure the mechanical strength and airtightness of the ceramic-metal interface, the ceramic-metal interfaces between the outer ceramic ring 5 and the anode connector 4, the outer ceramic ring 5 and the control electrode connector 6, the inner ceramic ring 7 and the control electrode connector 6, and the inner ceramic ring 7 and the cathode connector 8 are preferably brazed. For processes requiring ceramic metallization, the surface of the ceramic ring to be welded can be subjected to appropriate metallization and cleaning treatment before brazing; the metallization layer, brazing filler metal, and brazing temperature regime are not limited to a specific material or value, but should be matched with the selected ceramic and metal system. The metal-metal connection in the electron gun can be selected from brazing, laser welding, argon arc welding, diffusion welding, or other applicable connection processes according to the materials, structure, and subsequent assembly requirements.

[0039] In another embodiment provided in this disclosure, each conical ceramic ring is made of alumina ceramic.

[0040] In this embodiment, the outer ceramic ring 5 and the inner ceramic ring 7 can be made of the same insulating ceramic material as existing electron guns, such as alumina ceramic.

[0041] Based on the same technical concept, this disclosure provides a method for manufacturing a sleeved electron gun, the method comprising: Anode 1, control electrode 2, cathode 3, anode connector 4, outer ceramic ring 5, control electrode connector 6, inner ceramic ring 7, and cathode connector 8 are prepared. At least one of the outer ceramic ring 5 and inner ceramic ring 7 is a conical ceramic ring. The conical ceramic ring is ring-shaped as a whole, and its width along the electron gun axis gradually decreases from the inner circumference to the outer circumference, so that the inner circumference of the conical ceramic ring is wider than the outer circumference, and a conical surface extending around the electron gun axis is formed between the inner and outer circumferences. The outer ceramic ring 5 is placed between the anode connector 4 and the control electrode connector 6, and the inner ceramic ring 7 is placed between the control electrode connector 6 and the cathode connector 8, and all components are positioned coaxially. The outer ceramic ring 5 is sealed to the anode connector 4 and the control electrode connector 6, and the inner ceramic ring 7 is sealed to the control electrode connector 6 and the cathode connector 8 to form an electron gun insulation and vacuum sealing assembly with a sleeve structure. Anode 1, control electrode 2 and cathode 3 are assembled and connected to their corresponding connectors, and the resulting assembly is then subjected to a vacuum sealing test.

[0042] In another embodiment provided in this disclosure, the ceramic ring 5 is positioned between the outer ceramic ring 5 and the anode connector 4 and the control electrode connector 6. The metal sealing interface, and the ceramic between the inner ceramic ring 7 and the control electrode connector 6 and the cathode connector 8 The metal sealing interface is sealed by brazing. Before brazing, the surfaces of the ceramic ring and metal connector to be welded are cleaned, assembled and positioned, and the brazing gap is checked.

[0043] In this embodiment of the disclosure, the metal-metal connection can be achieved by brazing, laser welding, argon arc welding, diffusion welding or other applicable processes, depending on the material and structural requirements, and is not limited to the ceramic-metal brazing steps.

[0044] In another embodiment provided in this disclosure, the vacuum sealing test includes an airtightness test, and after the airtightness test is qualified, the electron gun is subjected to vacuum baking and high-pressure aging.

[0045] In this embodiment of the disclosure, by sequentially performing airtightness testing, vacuum baking, and high-pressure aging, vacuum sealing defects can be eliminated in a timely manner, effectively removing gases and impurities adsorbed on the ceramic ring and sealing interface, and eliminating potential field emission points. This significantly reduces the risk of surface flashover and secondary electron multiplication of the electron gun under strong electric fields and vacuum environments, ensuring the insulation reliability and lifespan of the electron gun under long-term high-voltage operation.

[0046] For example, the manufacturing method of this embodiment is as follows: First, according to the design dimensions of the electron gun, anode 1, control electrode 2, cathode 3, anode connector 4, control electrode connector 6, cathode connector 8, and outer ceramic ring 5 and inner ceramic ring 7 in the form of conical ceramic rings are prepared respectively; Second, the surfaces to be welded of each ceramic ring and metal connector are cleaned, and the direction of the conical surface, coaxiality, sealing overlap surface and brazing gap are checked; Then, according to the outer to inner layer of anode connector 4-outer ceramic ring 5-control electrode connector 6-inner ceramic ring 7-cathode connector 8, they are assembled and positioned, and the four ceramic-metal interfaces are brazed and sealed; Subsequently, using a connection process suitable for the corresponding materials and structures, anode 1, control electrode 2 and cathode 3 are assembled and connected with the corresponding metal connectors to complete the overall assembly of the electron gun; Finally, the airtightness of the components is tested, and after passing the test, vacuum baking and high-pressure aging are performed.

[0047] To reduce the risks of gas leakage and contamination from repeated furnace feeding of ceramic components, a staged welding process can be adopted: first, complete and inspect the ceramic-metal sealing components, and then connect subsequent components; when using multi-stage brazing, the melting temperature of the brazing filler metal used in subsequent welds is lower than that of the previous stage brazing filler metal, in order to reduce the risk of remelting of the previous weld. The heating and cooling rates of ceramic-metal brazing can be lower than those of conventional metal-metal brazing, so that the thermal stress caused by different coefficients of thermal expansion can be released slowly.

[0048] During ceramic-metal brazing, the relative positions of the ceramic ring and the metal connector should be controlled, and the amount of brazing filler metal and the holding time should be adjusted to ensure that the filler metal fully fills the sealing gap and to prevent it from overflowing to the vacuum side and forming sharp protrusions, burrs, particles, or deep and narrow gaps. After sealing, the sealing quality can be evaluated through visual inspection, microscopic inspection, airtightness testing, and necessary cross-sectional or non-destructive testing. High-pressure aging can be carried out using a step-by-step pressure increase method, and the specific pressure increase regime should be determined according to the electron gun structure and equipment conditions.

[0049] like Figure 1 As shown, the existing structure of the outer ceramic ring 5' and inner ceramic ring 7' is based on a near-cylindrical annular body, and annular protrusions extending continuously in the circumferential direction are provided on the surface of the annular body. Figure 1In contrast, this embodiment uses a conical ceramic ring with an inner circumferential axial width greater than the outer circumferential axial width as the outer ceramic ring 5 and the inner ceramic ring 7, while maintaining the sealing connection layer with the anode connector 4, the control electrode connector 6, and the cathode connector 8, thereby introducing the electric field and electron trajectory regulation effect of the conical surface into the original sealed electron gun. The actual effect can be evaluated by comparing or simulating existing ceramic ring structures with annular protrusions under the same material, voltage boundary, and comparable spatial dimensions. Electrical indicators may include the peak value of the tangential electric field on the ceramic ring surface, the local peak field strength at the three junction points, the uniformity of the electric field, the position and proportion of electron bombardment, flashover voltage, leakage current, discharge position, and performance stability after aging. Structural and process indicators may include the thermal and mechanical stress of the ceramic and sealing areas, component coaxiality, joint strength, and sealing airtightness.

[0050] Based on the same technical concept, this disclosure provides a vacuum electronic device, including the encapsulated electron gun provided in any of the foregoing embodiments.

[0051] In another embodiment provided in this disclosure, the vacuum electronic device is a traveling wave tube or a klystron.

[0052] Those skilled in the art will understand that the accompanying drawings are merely schematic diagrams of a preferred embodiment, and the modules or processes in the drawings are not necessarily essential for implementing this disclosure.

[0053] The sequence numbers of the embodiments disclosed above are for descriptive purposes only and do not represent the superiority or inferiority of the embodiments.

[0054] Obviously, those skilled in the art can make various modifications and variations to this disclosure without departing from its spirit and scope. Therefore, if such modifications and variations fall within the scope of the claims of this disclosure and their equivalents, this disclosure is also intended to include such modifications and variations.

Claims

1. A sleeve-seal structure electron gun, characterized by, include: Anode (1), control electrode (2), cathode (3), anode connector (4), outer ceramic ring (5), control electrode connector (6), inner ceramic ring (7), and cathode connector (8); The anode connector (4), outer ceramic ring (5), control electrode connector (6), inner ceramic ring (7) and cathode connector (8) form a coaxial sleeve structure in the radial direction from the outside to the inside. The anode (1), control electrode (2) and cathode (3) are arranged along the electron gun axis. At least one of the outer ceramic ring (5) and the inner ceramic ring (7) is a conical ceramic ring. The conical ceramic ring is generally ring-shaped, and its width along the electron gun axis gradually decreases from the inner circumference to the outer circumference, so that the inner circumference of the conical ceramic ring is wider than the outer circumference, and a conical surface extending around the electron gun axis is formed between the inner and outer circumferences. The outer circumferential surface of the outer ceramic ring (5) is sealed to the anode connector (4), and the inner circumferential surface is sealed to the control electrode connector (6); The outer circumferential surface of the inner ceramic ring (7) is sealed to the control electrode connector (6), and the inner circumferential surface is sealed to the cathode connector (8); The anode connector (4), control electrode connector (6), and cathode connector (8) are insulated from each other by the outer ceramic ring (5) and the inner ceramic ring (7), and together form a vacuum-sealed structure for the electron gun.

2. The sleeve-envelope electron gun of claim 1, wherein The conical surface of each of the conical ceramic rings is a rotary conical surface.

3. The sleeve-envelope electron gun of claim 1, wherein The angle between the generatrix of the conical surface of each of the conical ceramic rings and the axis of the electron gun is 30° to 60°.

4. The envelope structure electron gun of claim 1, wherein, The ceramic-metal sealing interface between the outer ceramic ring (5) and the anode connector (4) and the control electrode connector (6), and the ceramic-metal sealing interface between the inner ceramic ring (7) and the control electrode connector (6) and the cathode connector (8) are brazed.

5. The envelope structure electron gun of claim 1, wherein Each of the conical ceramic rings is made of alumina ceramic.

6. A method for manufacturing a field emission electron gun, comprising the steps of: forming a field emission electron gun; and forming a sleeve structure around the field emission electron gun. include: Prepare an anode (1), a control electrode (2), a cathode (3), an anode connector (4), an outer ceramic ring (5), a control electrode connector (6), an inner ceramic ring (7), and a cathode connector (8), wherein at least one of the outer ceramic ring (5) and the inner ceramic ring (7) is a conical ceramic ring. The conical ceramic ring is generally annular, and its width along the electron gun axis gradually decreases from the inner circumference to the outer circumference, so that the inner circumference of the conical ceramic ring is wider than the outer circumference, and a conical surface extending around the electron gun axis is formed between the inner and outer circumferences. The outer ceramic ring (5) is placed between the anode connector (4) and the control electrode connector (6), and the inner ceramic ring (7) is placed between the control electrode connector (6) and the cathode connector (8), and all components are positioned coaxially. The outer ceramic ring (5) is sealed to the anode connector (4) and the control electrode connector (6), and the inner ceramic ring (7) is sealed to the control electrode connector (6) and the cathode connector (8) to form an electron gun insulation and vacuum sealing assembly with a sleeve structure. The anode (1), control electrode (2) and cathode (3) are assembled and connected to their respective connectors, and the resulting assembly is then subjected to a vacuum sealing test.

7. The method of manufacturing according to claim 6, wherein, The ceramic-metal sealing interface between the outer ceramic ring (5) and the anode connector (4) and the control electrode connector (6), and the ceramic-metal sealing interface between the inner ceramic ring (7) and the control electrode connector (6) and the cathode connector (8) are brazed. Before brazing, the surfaces of the ceramic ring and the metal connector to be brazed are cleaned, assembled and positioned, and the brazing gap is checked.

8. The method of manufacturing according to claim 6, wherein, The vacuum sealing test includes an airtightness test. After the airtightness test is passed, the electron gun is subjected to vacuum baking and high-pressure aging.

9. A vacuum electronic device, characterized by The electron gun includes the enclosed structure as described in any one of claims 1 to 5.

10. The vacuum electron device of claim 9, wherein, The vacuum electronic device is a traveling wave tube or a klystron.