A transparent luminescent glass panel and its preparation method

By forming a conductive silver paste layer and an ITO area at the edge of the transparent luminescent glass panel, the problem of visible conductive structure is solved, achieving a transparent, flawless, and uniformly bright luminous effect, suitable for high-end displays and advertising.

CN123124540APending Publication Date: 2026-11-17DONGGUAN SHINE GLASS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611211673.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-11
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

The internal conductive structure of existing transparent luminescent glass panels is visible, which compromises visual transparency and affects aesthetics.

Method used

A conductive silver paste layer is formed around the periphery of the glass substrate, and an indium tin oxide transparent conductive film layer is deposited on the surface. Positive ITO region and negative ITO region are formed by etching. The LED beads in the acrylic light-emitting unit are electrically connected to the ITO region, and the power supply interface is concentrated at the edge.

Benefits of technology

It achieves a transparent and flawless appearance when not in operation, and displays only luminous patterns when powered on, without revealing the panel and wiring. It also has good brightness uniformity, making it suitable for high-end display and advertising applications, and reducing manufacturing costs.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention discloses a transparent luminescent glass panel and its fabrication method. The fabrication method includes: providing a glass substrate; forming a conductive silver paste layer at the periphery of the glass substrate; depositing an indium tin oxide (ITO) transparent conductive film layer on the surface of the glass substrate; etching each display area of ​​the ITO transparent conductive film layer used for displaying graphics and text to divide the ITO transparent conductive film layer within the display area into mutually insulated positive ITO regions and negative ITO regions; fabricating at least one acrylic light-emitting unit; and placing the acrylic light-emitting unit above the corresponding display area on the glass substrate. This invention achieves the effect of graphics and text illuminating when powered on, and the electrodes being completely invisible and the background highly transparent when powered off, by concentrating the conductive silver paste layer at the edges and utilizing the overall conductivity of ITO and the design of positive and negative ITO regions within each display area. Furthermore, the manufacturing process is simple and suitable for applications such as building curtain walls, advertising displays, and decorative signage.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of luminescent glass technology, and in particular to a transparent luminescent glass panel and its preparation method. Background Technology

[0002] In the fields of architectural decoration, commercial display, and advertising, transparent luminescent glass panels for displaying illuminated graphics and text are widely used in brand logos, signs, decorative patterns, and other scenarios. Users expect the glass to appear as ordinary transparent glass when not powered, and only specific graphics and text to illuminate when powered, while the background remains transparent. In existing technologies, one way to achieve a transparent effect is to directly fix LED light strings or illuminated letters onto a high-transparency acrylic or glass substrate. To power these light-emitting elements, copper wires, FPC flexible circuit boards, or busbars need to be laid. These opaque conductive components can create noticeable grids, lines, or color differences on the transparent substrate, especially during the day or in bright environments, severely compromising the transparent aesthetics of the glass, degrading the appearance of the device, and making it difficult to achieve a purely transparent effect.

[0003] Therefore, there is an urgent need for a transparent luminescent glass panel and its preparation method to overcome the shortcomings of existing technologies. Summary of the Invention

[0004] In view of the above problems, the purpose of this invention is to provide a transparent luminescent glass panel and its preparation method, which can effectively solve the technical problem that the internal conductive structure of the transparent luminescent glass panel is visible and destroys the visual transparency in the prior art.

[0005] To achieve the above objectives, the present invention provides a method for preparing a transparent light-emitting glass panel, comprising: Provide a glass substrate; A conductive silver paste layer is formed in the periphery of the glass substrate. The conductive silver paste layer is composed of a first silver paste strip and a second silver paste strip that are insulated from each other. The first silver paste strip is used to connect to the positive terminal of the external power supply, and the second silver paste strip is used to connect to the negative terminal of the external power supply. An indium tin oxide transparent conductive film layer is deposited on the surface of a glass substrate, so that the indium tin oxide transparent conductive film layer covers the surface of the glass substrate, the first silver paste strip and the second silver paste strip; Etching is performed on each display area of ​​the indium tin oxide transparent conductive film layer used to display graphics and text, so that the indium tin oxide transparent conductive film layer in the display area is divided into mutually insulated positive ITO region and negative ITO region. The positive ITO region is electrically connected to the first silver paste strip through the unetched background indium tin oxide transparent conductive film layer, and the negative ITO region is electrically connected to the second silver paste strip through the unetched background indium tin oxide transparent conductive film layer. Make at least one acrylic light-emitting unit, each acrylic light-emitting unit having a shape corresponding to the corresponding display graphics and text, and accommodating at least one LED light bead inside the acrylic light-emitting unit; An acrylic light-emitting unit is placed on the glass substrate above the corresponding display area, so that the positive and negative leads of the LED beads are electrically connected to the positive and negative ITO areas in the display area, respectively.

[0006] As a preferred technical solution, the first and second silver paste strips of the present invention are formed by screen printing.

[0007] As a preferred technical solution, the width of the first and second silver paste strips of the present invention is 3mm to 8mm, and the thickness is 10μm to 25μm.

[0008] As a preferred technical solution, the indium tin oxide transparent conductive film layer of the present invention is obtained by magnetron sputtering.

[0009] As a preferred technical solution, the thickness of the indium tin oxide transparent conductive film layer of the present invention is 100nm~200nm, the sheet resistance is 10Ω / sq~20Ω / sq, and the visible light transmittance is greater than 85%.

[0010] As a preferred technical solution, the etching method of the present invention is laser etching.

[0011] As a preferred technical solution, the width of the insulating isolation strip of the present invention is 20μm~100μm.

[0012] As a preferred technical solution, the first silver paste strip and the second silver paste strip of the present invention extend along different edges of the glass substrate, and a gap is provided in the corner region of the glass substrate to achieve electrical isolation.

[0013] As a preferred technical solution, the electrical connection of the present invention is conductive adhesive bonding.

[0014] As a preferred technical solution, the acrylic light-emitting unit of the present invention is attached to the surface of a glass substrate by means of a transparent adhesive.

[0015] As a preferred technical solution, the glass substrate of the present invention is ultra-white glass.

[0016] As a preferred technical solution, the thickness of the glass substrate of the present invention is 3mm to 15mm.

[0017] In another aspect, the present invention provides a transparent luminescent glass panel, which is prepared using the aforementioned method. This transparent luminescent glass panel is flawless when not in operation, displays a uniform luminescent pattern when in operation, and has power supply interfaces uniformly concentrated at the edge of the panel, facilitating installation and maintenance.

[0018] Compared with the prior art, the present invention has at least the following beneficial effects: (1) This invention uses a conductive silver paste layer set on the edge area of ​​a glass substrate and connected to an external power source as a power supply. It uses an indium tin oxide transparent conductive film layer (i.e., ITO film layer) for conduction and etches in each display area of ​​the indium tin oxide transparent conductive film layer to form a positive ITO region and a negative ITO region. This achieves the effect that the electrodes are completely invisible. After power is applied, only the luminous text or pattern is visible, and the panel and lines are not visible, which meets the transparency requirements of high-end display and advertising applications.

[0019] (2) By setting the conductive silver paste layer on the periphery of the glass substrate, the transmission distance of the current in the ITO film layer is greatly shortened, and the power supply voltage of each display area tends to be consistent, thereby making the LED light bead brightness uniform and overcoming the problem of uneven brightness in a large area caused by single-point power supply.

[0020] (3) The manufacturing process of the present invention is simple. Only three core processes, namely silver paste screen printing and curing, ITO magnetron sputtering coating and laser etching, are required to complete the entire electrode fabrication. It is suitable for mass production and significantly reduces manufacturing costs.

[0021] (4) The acrylic light-emitting unit of the present invention adopts a shape corresponding to the displayed graphics and text, integrates LED beads and is directly electrically connected to the positive and negative areas of ITO. It has a compact structure, is easy to replace and maintain, and can flexibly design graphic and text content as needed. It is suitable for various scenarios such as brand logos, advertising slogans, and signs. Detailed Implementation

[0022] To address the technical problem of visible internal conductive structures in existing transparent luminescent glass panels, which compromises visual transparency, this invention provides a method for preparing a transparent luminescent glass panel, comprising the following steps: A glass substrate is provided; a conductive silver paste layer is formed on the periphery of the glass substrate, the conductive silver paste layer being composed of a first silver paste strip and a second silver paste strip that are insulated from each other, the first silver paste strip being used to connect to the positive terminal of an external power supply, and the second silver paste strip being used to connect to the negative terminal of the external power supply; an indium tin oxide (ITO) transparent conductive film layer is deposited on the surface of the glass substrate, such that the ITO transparent conductive film layer covers the surface of the glass substrate, the first silver paste strip, and the second silver paste strip; each display area of ​​the ITO transparent conductive film layer used for displaying graphics is etched to divide the ITO transparent conductive film layer within the display area into mutually insulated positive ITO regions and negative ITO regions. In the display area, the positive ITO region is electrically connected to the first silver paste strip through an unetched background indium tin oxide transparent conductive film layer, and the negative ITO region is electrically connected to the second silver paste strip through an unetched background indium tin oxide transparent conductive film layer; at least one acrylic light-emitting unit is fabricated, each acrylic light-emitting unit having a shape corresponding to the corresponding display graphic, and at least one LED bead is housed inside the acrylic light-emitting unit; the acrylic light-emitting unit is placed above the corresponding display area on the glass substrate, so that the positive and negative leads of the LED bead are electrically connected to the positive and negative ITO regions in the display area, respectively.

[0023] This invention concentrates a low-resistance silver paste layer for power supply around the perimeter of a glass substrate, utilizing the in-plane transparent ITO layer itself as an invisible conductor to supply power to the display area, thus visually eliminating the conductive structure inside the panel. The technical principle is as follows: the low-resistance silver paste layer acts as a power supply bus around the transparent conductive ITO film, allowing current to flow simultaneously from the edge area to the central area of ​​the ITO film. This significantly shortens the average current transmission path within the ITO film, effectively compensating for the voltage drop caused by the relatively high resistivity of ITO itself. This ensures that the light-emitting elements receive a nearly uniform driving voltage, guaranteeing the overall uniformity of display brightness on the glass substrate. In the display area, the LED beads within the acrylic light-emitting unit are connected across the positive and negative ITO areas via their positive and negative leads, respectively. When the positive terminal of the external power supply supplies power to the background ITO area through the first silver paste strip, current flows through the positive ITO area into the positive terminal of the LED bead, illuminating the LED bead, and then flows out from the negative terminal of the LED bead, before flowing through the negative ITO area into the second silver paste strip, forming a complete circuit. Since the ITO layer and etched channels are invisible, and the edge conductive silver paste layer can be completely hidden by the frame, the entire glass is transparent and flawless when not in use, and only displays luminescent patterns when in use.

[0024] The glass substrate can be ultra-clear glass. In practical applications, this ultra-clear glass can also be further tempered or semi-tempered to improve its structural strength and safety. The thickness of the glass substrate can be 3mm to 15mm. For example, the thickness of the glass substrate can be, but is not limited to, 3mm, 4mm, 5mm, 6mm, 7mm, 8mm, 9mm, 10mm, 11mm, 12mm, 13mm, 14mm, and 15mm. The size of the glass substrate can be customized as needed, for example, a length of 0.3m to 3m and a width of 0.3m to 2m, but is not limited to these. Before subsequent processing, the glass substrate undergoes a cleaning process. The cleaning method includes, but is not limited to, ultrasonic cleaning, to effectively remove stains from the surface of the glass substrate, achieving a coating-grade finish, and effectively eliminating the influence of impurities on the conductive path.

[0025] The first and second silver paste strips are formed by screen printing. Specifically, the screen printing stencil can be 200 mesh, the curing temperature can be 60℃~180℃, and the curing time can be 15min~60min. As an example, the curing temperature can be, but is not limited to, 60℃, 65℃, 70℃, 75℃, 80℃, 90℃, 100℃, 110℃, 120℃, 130℃, 140℃, 150℃, 160℃, 170℃, and 180℃; and the curing time can be, but is not limited to, 15min, 20min, 25min, 30min, 35min, 40min, 45min, 50min, and 60min. Under these conditions, a firmly adhered low-resistance silver paste layer can be formed.

[0026] The width of the first and second silver paste strips is 3mm to 8mm, and the thickness is 10μm to 25μm. For example, the width of the first and second silver paste strips can be, but is not limited to, 3mm, 4mm, 5mm, 6mm, 7mm, or 8mm; the thickness of the first and second silver paste strips can be, but is not limited to, 10μm, 15μm, 20μm, or 25μm. The first and second silver paste strips extend along different edges of the glass substrate, and a gap is provided in the corner area of ​​the glass substrate to achieve electrical isolation. Specifically, the gap width between the two silver paste strips can be 0.5mm to 3mm. For example, the gap width can be, but is not limited to, 0.5mm, 1mm, 1.5mm, 2mm, 2.5mm, or 3mm. In some preferred embodiments, the first and second silver paste strips can be spaced 2mm apart at the upper left and lower right corners of the glass. The output voltage of the external power supply can be arbitrarily selected from 3V, 5V, 12V, 24V, and 48V.

[0027] The indium tin oxide transparent conductive film was deposited using magnetron sputtering. Specifically, magnetron sputtering is a conventional deposition process known in the art, and the specific deposition process will not be described in detail in this invention. The thickness of the indium tin oxide transparent conductive film is 100 nm to 200 nm, the sheet resistance is 10 Ω / sq to 20 Ω / sq, and the visible light transmittance is greater than 85%. As an example, the thickness of the indium tin oxide transparent conductive film layer can be, but is not limited to, 100nm, 110nm, 120nm, 130nm, 140nm, 150nm, 160nm, 170nm, 180nm, 190nm, or 200nm; the sheet resistance can be, but is not limited to, 10Ω / sq, 11Ω / sq, 12Ω / sq, 13Ω / sq, 14Ω / sq, 15Ω / sq, 16Ω / sq, 17Ω / sq, 18Ω / sq, 19Ω / sq, or 20Ω / sq. The indium tin oxide transparent conductive film layer can completely cover the surfaces of the first and second silver paste strips, or it can partially cover the surfaces of the first and second silver paste strips. When partially covered, the overlap width between the conductive silver paste layer and the indium tin oxide transparent conductive film layer is not less than 2mm.

[0028] The etching process employs laser etching. Specifically, picosecond or femtosecond lasers can be used, with a laser pulse width of 5 ns to 50 ns, a laser spot diameter of 15 μm to 50 μm, and an etching speed of 500 mm / s to 1200 mm / s, but these are not limited to these parameters. Laser etching is a conventional etching process known in the art, and the specific etching process will not be described in detail in this invention.

[0029] The acrylic light-emitting unit includes an acrylic sheet and LED beads disposed on the acrylic sheet. Specifically, the acrylic sheet can be a transparent acrylic sheet or a semi-transparent acrylic sheet, and the thickness of the acrylic sheet can be 3mm to 10mm. As an example, the thickness of the acrylic sheet can be, but is not limited to, 3mm, 4mm, 5mm, 6mm, 7mm, 8mm, 9mm, or 10mm. A laser cutting machine can be used to cut the acrylic sheet into shapes with specific patterns or text. The LED beads can be disposed in the acrylic sheet using methods conventional in the art. As an example, multiple grooves for accommodating LED beads can be engraved on the bottom of the acrylic sheet to dispose of the LED beads in the grooves. The acrylic light-emitting unit is bonded to the surface of a glass substrate using a transparent adhesive. Specifically, the transparent adhesive can be selected from at least one of optically transparent adhesive (OCA), optically transparent resin (OCR), and ultraviolet-curable adhesive. The electrical connection is achieved by conductive adhesive bonding. Specifically, the conductive adhesive can be selected from at least one of anisotropic conductive adhesive, conductive silver paste, and conductive double-sided tape.

[0030] The transparent light-emitting panel may further include an outer frame that shields the edge area of ​​the glass substrate to conceal the conductive silver paste layer. The outer frame may be made of one or more of aluminum alloy, stainless steel, plastic, or wood; the width of the outer frame may be arbitrarily selected between 3mm, 5mm, 8mm, 10mm, and 15mm to completely cover the conductive silver paste layer.

[0031] To better illustrate the purpose, technical solution, and beneficial effects of this invention, the invention will be further described below with reference to specific embodiments. It should be noted that the methods described below are further explanations of this invention and should not be construed as limiting it.

[0032] Example 1 This embodiment provides a method for preparing a transparent light-emitting glass panel, including the following steps: A 1000mm × 800mm × 8mm ultra-clear tempered glass substrate with a surface cleanliness reaching coating grade was provided. A 200-mesh screen printing stencil was used to screen print a 5mm wide conductive silver paste layer (Henkel LOCTITE ECI 1010 series) along the four edges of the glass substrate. The silver paste pattern was designed as follows: a first silver paste strip (positive bus) was printed along the top and left edges of the glass, and a second silver paste strip (negative bus) was printed along the bottom and right edges of the glass. The first and second silver paste strips were interrupted at the lower left and upper right corners of the glass, with a 2mm gap between the interruptions. A 5mm × 5mm pad area was reserved at the upper left corner of the first silver paste strip and the lower right corner of the second silver paste strip. The wet film thickness of the printed silver paste was approximately 25μm. The glass substrate was placed in an oven and heated to 130℃ at a rate of 5℃ / min, held at that temperature for 40 minutes, and then allowed to cool naturally to room temperature to complete curing. After drying, the silver paste thickness was approximately 15μm. After curing, the insulation resistance between the two sections of silver paste was measured to be greater than 100MΩ using a 500V megohmmeter, and the resistance of the silver paste strip was measured to be no more than 10Ω using a multimeter.

[0033] An indium tin oxide (ITO) transparent conductive film was deposited on the surface of a glass substrate with a screen-printed conductive silver paste layer using magnetron sputtering. The sputtering power was 3 kW, the deposition rate was approximately 2 nm / s, and the total deposition time was 80 seconds. The thickness of the ITO transparent conductive film was approximately 160 nm. After deposition, the ITO film covered the entire glass surface, with an overlap of approximately 4 mm with the conductive silver paste layer. The sheet resistance of the ITO film was measured to be 15 Ω / sq ± 3 Ω / sq using a four-probe sheet resistance meter.

[0034] Laser etching was used to etch the indium tin oxide (ITO) transparent conductive film layer into each display area, forming mutually insulated positive and negative ITO regions. Specifically, the displayed text consisted of the five letters "GLASS," with each letter representing an independent display area, totaling five areas. Etching was performed within each area to divide the ITO film into positive and negative ITO regions, ensuring that each region remained connected to the background ITO. The laser etching parameters for each area were: laser power 0.8W, scanning speed 800mm / s, and pulse frequency 30kHz. After etching, the insulation resistance between the positive and negative ITO regions was measured to be greater than 10MΩ. After etching, the glass surface was rinsed with deionized water to remove etching residue and then dried with compressed air.

[0035] Take a 5mm thick transparent acrylic sheet and use a laser cutter to cut out five letters: "G", "L", "A", "S", and "S". Each letter is approximately 200mm high and the stroke width is approximately 25mm. On the bottom surface of the acrylic sheet, use a CNC engraving machine to machine grooves to accommodate LED beads. The grooves are 3mm deep, 4mm wide, and their length is determined based on the number of LED beads to be accommodated in each letter stroke. Taking the letter "G" as an example, the total stroke length of this letter is approximately 600mm. Ten LED beads are evenly arranged along the center line of the stroke, with a spacing of approximately 60mm. Ten grooves, each 3mm deep × 4mm wide × 5mm long, are engraved at corresponding positions on the bottom surface of the acrylic sheet. Two 1mm diameter through holes are drilled at the bottom of each groove to allow the positive and negative leads of the LED beads to pass through. The through holes are spaced 2.5mm apart. The LED beads (SMD 2835 white LEDs) are embedded in the grooves, with the positive and negative leads of the LED beads protruding approximately 1mm from the bottom surface of the acrylic sheet through the through holes. After all the LEDs are installed, use transparent epoxy resin to seal the grooves and pin roots to fix the LEDs and protect the pins. Repeat the above steps to complete the fabrication of all five letter-shaped light-emitting units.

[0036] Five acrylic letter-shaped LED units were placed above the corresponding ITO etched areas on the glass panel. Anisotropic conductive adhesive was used to electrically connect the positive and negative leads of each letter's LED to the positive and negative ITO areas within the display area, respectively. Two copper wires were soldered to the pre-reserved pads in the silver paste layer as external power leads. The positive lead was soldered to the first silver paste pad, and the negative lead was soldered to the second silver paste pad. UV adhesive was applied to the solder joints and cured under ultraviolet light. A DC 24V / 3A switching power supply was connected and tested.

[0037] A Konica Minolta CA-2000 imaging luminance meter was used to measure the luminance values ​​(unit: cd / m²) of each display area and each internal LED position at a distance of 1m from the glass panel. 2The average brightness deviation percentage between each display area was calculated to be 8%, and the brightness deviation percentage between different LEDs within the same display area was calculated to be 5%. The visible light transmittance of the glass panel was measured to be 88% using a spectrophotometer (model: Shimadzu UV-3600) in the wavelength range of 380nm to 780nm.

[0038] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to preferred embodiments, it is not limited to those listed in the embodiments. Those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the essence and scope of the technical solutions of the present invention.

Claims

1. A method for preparing a transparent luminescent glass panel, characterized in that, include: Provide a glass substrate; A conductive silver paste layer is formed in the periphery of the glass substrate. The conductive silver paste layer is composed of a first silver paste strip and a second silver paste strip that are insulated from each other. The first silver paste strip is used to connect to the positive terminal of the external power supply, and the second silver paste strip is used to connect to the negative terminal of the external power supply. An indium tin oxide transparent conductive film layer is deposited on the surface of the glass substrate, so that the indium tin oxide transparent conductive film layer covers the surface of the glass substrate, the first silver paste strip and the second silver paste strip; Etching is performed on each display area of ​​the indium tin oxide transparent conductive film layer used to display graphics and text, so as to divide the indium tin oxide transparent conductive film layer in the display area into mutually insulated positive ITO regions and negative ITO regions. The positive ITO regions are electrically connected to the first silver paste strip through the unetched background indium tin oxide transparent conductive film layer, and the negative ITO regions are electrically connected to the second silver paste strip through the unetched background indium tin oxide transparent conductive film layer. At least one acrylic light-emitting unit is manufactured, each acrylic light-emitting unit having a shape corresponding to the corresponding display graphics and text, and at least one LED light bead is housed inside the acrylic light-emitting unit; The acrylic light-emitting unit is disposed above the corresponding display area on the glass substrate, so that the positive and negative pins of the LED lamp bead are electrically connected to the positive ITO area and the negative ITO area in the display area, respectively.

2. The method for preparing a transparent light-emitting glass panel according to claim 1, characterized in that, The first and second silver paste strips are formed by screen printing.

3. The method for preparing a transparent light-emitting glass panel according to claim 1, characterized in that, The width of the first silver paste strip and the second silver paste strip is 3mm~8mm, and the thickness is 10μm~25μm.

4. The method for preparing a transparent light-emitting glass panel according to claim 1, characterized in that, The indium tin oxide transparent conductive film was deposited by magnetron sputtering.

5. The method for preparing a transparent luminescent glass panel according to claim 1, characterized in that, The thickness of the indium tin oxide transparent conductive film is 100nm~200nm, the sheet resistance is 10Ω / sq~20Ω / sq, and the visible light transmittance is greater than 85%.

6. The method for preparing a transparent light-emitting glass panel according to claim 1, characterized in that, The etching is performed using laser etching.

7. The method for preparing a transparent light-emitting glass panel according to claim 1, characterized in that, The first silver paste strip and the second silver paste strip extend along different edges of the glass substrate, and are spaced apart in the corner region of the glass substrate to achieve electrical isolation.

8. The method for preparing a transparent light-emitting glass panel according to claim 1, characterized in that, The electrical connection is achieved by conductive adhesive bonding, and the acrylic light-emitting unit is attached to the surface of the glass substrate by a transparent adhesive.

9. The method for preparing a transparent light-emitting glass panel according to claim 1, characterized in that, The glass substrate is ultra-white glass, and the thickness of the glass substrate is 3mm to 15mm.

10. A transparent luminescent glass panel, characterized in that, It is prepared by the preparation method according to any one of claims 1 to 9.