Wafers, wafer fabrication methods, and display panel fabrication methods
By fabricating a thin photosensitive layer and a non-photosensitive adhesive on the wafer, the problems of residual photosensitive material and the arrangement of light-emitting elements are solved, thereby improving the yield of display panels and reducing costs.
Patent Information
- Application Number
- CN202510638705.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-16
- Publication Date
- 2026-11-17
AI Technical Summary
In existing MicroLED display technology, the thickness of the photosensitive material leads to residual adhesive problems, affecting the yield of the display panel. Furthermore, the high-temperature bonding and laser stripping processes cannot effectively arrange the light-emitting elements, increasing costs.
A thin first photosensitive layer is pre-prepared on the wafer for laser lift-off to decompose the light-emitting element, and a non-photosensitive adhesive is placed on a temporary substrate to separate the light-emitting element and avoid photosensitive material residue.
By reducing the amount of photosensitive material residue, the yield of the display panel is improved, and the transfer and arrangement of light-emitting elements are simplified, thereby reducing costs.
Smart Images

Figure CN123124548A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of display technology, and in particular to a wafer, a method for fabricating a wafer, and a method for fabricating a display panel. Background Technology
[0002] In existing MicroLED (micro-light-emitting diode) display technology, when transferring the light-emitting element from the wafer to a temporary substrate, a photosensitive material needs to be pre-prepared on the temporary substrate. The light-emitting element is then supported by a photosensitive layer on the temporary substrate using high-temperature bonding or laser lift-off. To ensure the support effect, the photosensitive material needs to be relatively thick. However, a thicker photosensitive material will produce residual adhesive when it is subsequently lifted by laser irradiation, which reduces the yield of the display panel. Summary of the Invention
[0003] This application provides a wafer, a method for fabricating the wafer, and a method for fabricating a display panel, which can improve the yield of the display panel.
[0004] A first aspect of this application provides a wafer comprising: a substrate; a light-emitting element located on one side of the substrate, including a light-emitting body and an electrode disposed on the side of the light-emitting body opposite to the substrate; and a first photosensitive layer disposed on at least a portion of the surface of the light-emitting element on the side opposite to the substrate.
[0005] In one embodiment, the wafer includes: a plurality of light-emitting elements disposed at intervals on one side of the substrate; wherein the plurality of light-emitting elements are located between the first photosensitive layer and the substrate, the first photosensitive layer includes a plurality of first photosensitive blocks corresponding one-to-one with the plurality of light-emitting elements, the light-emitting elements are located between the corresponding first photosensitive blocks and the substrate, and the plurality of first photosensitive blocks are disposed at intervals.
[0006] Preferably, the orthographic projection of the first photosensitive block on the substrate coincides with the orthographic projection of the corresponding light-emitting element on the substrate.
[0007] In one embodiment, the wafer includes a second photosensitive layer located between the light-emitting element and the substrate.
[0008] Preferably, the orthographic projection of the second photosensitive layer on the substrate coincides with the orthographic projection of the light-emitting element on the substrate.
[0009] Preferably, the first photosensitive layer and the second photosensitive layer are made of the same material.
[0010] In one embodiment, the material of the first photosensitive layer includes benzocyclobutene.
[0011] Preferably, the thickness of the first photosensitive layer does not exceed 5 micrometers.
[0012] Preferably, the thickness of the first photosensitive layer is 1 micrometer.
[0013] A second aspect of this application provides a method for fabricating a wafer, the method comprising: providing a substrate; fabricating a light-emitting element on one side of the substrate; wherein the light-emitting element includes a light-emitting body and an electrode disposed on the side of the light-emitting body opposite to the substrate; and fabricating a first photosensitive layer on at least a portion of the surface of the light-emitting element opposite to the substrate.
[0014] In one embodiment, the step of fabricating the light-emitting element on one side of the substrate includes: fabricating a plurality of spaced-apart light-emitting elements on one side of the substrate; and the step of fabricating a first photosensitive layer on at least a portion of the surface of the light-emitting element facing away from the substrate includes: forming a full-surface first photosensitive layer on the side of the light-emitting element facing away from the substrate; patterning the first photosensitive layer to remove the first photosensitive layer between two adjacent light-emitting elements, thereby obtaining a plurality of first photosensitive blocks corresponding one-to-one with the light-emitting elements, wherein the light-emitting element is located between the corresponding first photosensitive block and the substrate, and the plurality of first photosensitive blocks are spaced apart.
[0015] Preferably, before the step of preparing the light-emitting element on one side of the substrate, the method further includes: preparing a second photosensitive layer on one side of the substrate.
[0016] A third aspect of this application provides a method for fabricating a display panel, the method comprising: transferring a light-emitting element located on one side of a substrate on a wafer to a first side of a first temporary substrate, wherein the light-emitting element includes a light-emitting body and at least one electrode disposed on one side of the light-emitting body, and after being transferred to the first temporary substrate, the electrode is located between the light-emitting body and the first temporary substrate, and a first photosensitive layer is formed on at least a portion of the surface of the light-emitting element facing the first temporary substrate; placing a second temporary substrate on the side of the light-emitting element away from the first temporary substrate, and irradiating the first photosensitive layer with a laser to transfer the light-emitting element on the first temporary substrate to the second temporary substrate; placing a driving backplate on the side of the second temporary substrate away from the light-emitting element, and transferring the light-emitting element on the second temporary substrate to the driving backplate.
[0017] In one embodiment, prior to the step of transferring the light-emitting element on the wafer to the first temporary substrate, the method further includes: forming a receiving layer on the first side of the first temporary substrate.
[0018] Preferably, the material of the bonding layer includes a non-photosensitive bonding adhesive.
[0019] Preferably, the material of the non-photosensitive adhesive includes polydimethylsiloxane.
[0020] Preferably, the thickness of the bearing layer is not less than 10 micrometers.
[0021] In one embodiment, the wafer includes a second photosensitive layer located between the light-emitting element and the substrate; the step of transferring the light-emitting element on the wafer to a first side of the first temporary substrate includes: transferring the light-emitting element to the receiving layer by irradiating the second photosensitive layer with a laser.
[0022] In one embodiment, prior to the step of transferring the light-emitting element on the wafer to a first side of the first temporary substrate, the method further includes: adjusting the relative position between the substrate and the first temporary substrate so that the light-emitting element on the substrate corresponds to a target position on the first temporary substrate.
[0023] Unlike existing technologies, the advantages of this application are as follows: This application pre-fabricates a first photosensitive layer on the wafer, that is, a first photosensitive layer is provided on the side of the light-emitting element away from the substrate. In this way, during the subsequent fabrication of the display panel, the first temporary substrate does not need to be provided with a photosensitive layer. Since the first photosensitive layer does not need to provide a receiving effect, the thickness of the first photosensitive layer can be made very thin. Thus, during the subsequent transfer, the first photosensitive layer will not remain on the light-emitting element, thereby improving the yield of the display panel. Attached Figure Description
[0024] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort, wherein:
[0025] Figure 1 This is a schematic diagram of the first scheme for manufacturing display panels in the prior art;
[0026] Figure 2 This is a schematic diagram of a second method for manufacturing display panels in the prior art;
[0027] Figure 3 This is a schematic diagram of the structure of the wafer according to the first embodiment of this application;
[0028] Figure 4 This is a schematic diagram of the structure of the wafer according to the second embodiment of this application;
[0029] Figure 5 yes Figure 4Corresponding top view structural diagram;
[0030] Figure 6 This is a schematic diagram of the structure of the wafer according to the third embodiment of this application;
[0031] Figure 7 This is a schematic flowchart of one embodiment of the wafer fabrication method of this application;
[0032] Figure 8 yes Figure 7 A diagram showing the corresponding steps in the process;
[0033] Figure 9 yes Figure 7 A schematic diagram of another embodiment corresponding to step S200;
[0034] Figure 10 yes Figure 7 A flowchart illustrating another embodiment of step S300;
[0035] Figure 11 yes Figure 10 A schematic diagram of one implementation method corresponding to each step in the process;
[0036] Figure 12 yes Figure 7 A schematic diagram of an embodiment prior to step S200;
[0037] Figure 13 This is a schematic flowchart of one embodiment of the display panel manufacturing method of this application;
[0038] Figure 14 yes Figure 13 A schematic diagram of an embodiment corresponding to step S1000;
[0039] Figure 15 yes Figure 13 A schematic diagram of one embodiment corresponding to step S2000;
[0040] Figure 16 yes Figure 13 A schematic diagram of one embodiment corresponding to step S3000. Detailed Implementation
[0041] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of the embodiments. Based on the embodiments of this application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of this application.
[0042] In the existing technology, there are the following two solutions.
[0043] The first option is high-temperature bonding, see [reference] Figure 1 A light-emitting element 200 is disposed on a substrate 100. The electrode 220 of the light-emitting element 200 is located on the side of the light-emitting body 210 of the light-emitting element 200 away from the substrate 100. A photosensitive layer 400 is disposed on a first temporary substrate 300. After the substrate 100 and the first temporary substrate 300 are aligned, the light-emitting element 200 is supported by the photosensitive layer 400. Then, the light-emitting element 200 is bonded to the first temporary substrate 300 at high temperature, and the electrode 220 of the light-emitting element 200 is embedded in the photosensitive layer 400. Finally, the light-emitting element 200 is separated from the substrate 100. The problem with this scheme is that the photosensitive layer 400 needs to support the light-emitting element 200. To ensure the support effect, the thickness is made relatively thick, but... In the subsequent process, the light-emitting element 200 needs to be separated from the first temporary substrate 300. Since the photosensitive layer 400 is relatively thick, some photosensitive material in the photosensitive layer 400 will remain on the light-emitting element 200. Furthermore, this solution also has the problem that, since a bonding solution is used, the light-emitting element 200 cannot be aligned when it is transferred from the substrate 100 to the first temporary substrate 300. In the prior art, considering the differences in quality and brightness of the light-emitting elements 200, the light-emitting elements 200 are aligned during the transfer process. The above process cannot be used for alignment. Therefore, in order to align the light-emitting elements 200, additional process steps are required, which increases the cost.
[0044] The second option is laser ablation, see [link / reference] Figure 2 After the substrate 100 and the first temporary substrate 300 are aligned, the light-emitting element 200 is separated from the substrate 100 by laser irradiation, and the light-emitting element 200 is supported by the photosensitive layer 400 on the first temporary substrate 300. This scheme realizes the arrangement of the light-emitting element 200 during the transfer of the light-emitting element 200 from the substrate 100 to the first temporary substrate 300. However, the support by the light-emitting element has high requirements. The existing photosensitive layer 400 cannot fully meet the support effect. At the same time, there is still a problem of residual photosensitive material in the photosensitive layer 400, which reduces the yield of the final display panel.
[0045] To solve the above problems, see Figure 3 The first aspect of this application provides a wafer 10, which includes a substrate 100, a light-emitting element 200, and a first photosensitive layer 500. The light-emitting element 200 is located on one side of the substrate 100 and includes a light-emitting body 210 and an electrode 220 disposed on the side of the light-emitting body 210 away from the substrate 100; the first photosensitive layer 500 is disposed on at least a portion of the surface of the light-emitting element 200 on the side away from the substrate 100.
[0046] Specifically, the light-emitting element 200 in wafer 10 is used for the subsequent fabrication of the display panel. The first photosensitive layer 500 can decompose under laser irradiation, thereby enabling the light-emitting element 200 to be separated. Unlike the prior art, this application provides the first photosensitive layer 500 on the side of the light-emitting element 200 facing away from the substrate 100. That is, since the first photosensitive layer 500 is provided on wafer 10, the receiving layer on the subsequent first temporary substrate for supporting the light-emitting element 200 no longer needs to use a photosensitive material. In other words, the receiving layer does not need to take on both photosensitive and receiving functions; it only needs to consider the receiving function. This expands the range of material choices. At the same time, the first photosensitive layer 500 on wafer 10 does not need to provide a receiving function; it only needs to provide the function of decomposition under laser irradiation. The required function exactly matches the function of the first photosensitive layer 500. Thus, the thickness of the first photosensitive layer 500 is not limited by the receiving function, and the thickness of the first photosensitive layer 500 can be reduced, as long as the laser lift-off conditions are met. Therefore, the problem of photosensitive material residue can be improved by adjusting the thickness of the first photosensitive layer 500. Specifically, the thickness of the first photosensitive layer 500 can be reduced to decrease the amount of photosensitive material residue. This reduction in thickness is relative to the thickness of the photosensitive layer on the first temporary substrate in the prior art. In this application, the first temporary substrate still requires a supporting layer to support the light-emitting element 200. Therefore, the thickness of the first photosensitive layer 500 in this application is reduced compared to the photosensitive layer in the prior art. However, the sum of the thickness of the first photosensitive layer 500 and the thickness of the supporting layer in this application is not proportional to the thickness of the photosensitive layer in the prior art. Furthermore, after the problem of photosensitive material residue is improved, the yield of the display panel is also increased.
[0047] It should be noted that the first photosensitive layer 500 is disposed on at least a portion of the surface of the light-emitting element 200 on the side away from the substrate 100. The first photosensitive layer 500 may be disposed only on the surface of the electrode 220 or only on the surface of the non-electrode 220 position. It may be disposed on a portion of the surface or on the entire surface, as long as it is disposed on the surface of the light-emitting element 200 on the side away from the substrate 100.
[0048] In one embodiment, see Figure 4 and Figure 5 The wafer 10 includes a plurality of light-emitting elements 200, which are spaced apart on one side of the substrate 100. The plurality of light-emitting elements 200 are located between the first photosensitive layer 500 and the substrate 100. The first photosensitive layer 500 includes a plurality of first photosensitive blocks 510 corresponding to the plurality of light-emitting elements 200. The light-emitting elements 200 are located between the corresponding first photosensitive blocks 510 and the substrate 100. The plurality of first photosensitive blocks 510 are spaced apart.
[0049] Specifically, each of the multiple first photosensitive blocks 510 corresponds one-to-one with a multiple light-emitting element 200. The multiple first photosensitive blocks 510 are also independent of each other and there is no connection between them. That is, the first photosensitive layer 500 is broken apart from the channels between the light-emitting elements 200 to form multiple independent first photosensitive blocks 510. When separating the light-emitting elements 200 subsequently using the first photosensitive blocks 510, they can be separated one by one as needed, without needing to be separated as a whole. This allows for the arrangement of the light-emitting elements 200 during the transfer process.
[0050] Preferably, the orthographic projection of the first photosensitive block 510 on the substrate 100 coincides with the orthographic projection of the corresponding light-emitting element 200 on the substrate 100. This coincidence ensures that when the light-emitting element 200 is subsequently peeled off by laser, one side of the electrode 220 of the light-emitting element 200 is covered by the first photosensitive block 510, thereby preventing the laser from directly irradiating the light-emitting element 200 and thus avoiding direct damage to the light-emitting element 200 by the laser.
[0051] Of course, in some other implementations, the first photosensitive block 510 may further extend to the outside of the light-emitting element 200, that is, the orthogonal projection of the final light-emitting element 200 on the substrate 100 is located within the orthogonal projection of the first photosensitive block 510 on the substrate 100.
[0052] Further reading Figure 6 The wafer 10 includes a second photosensitive layer 600, which is located between the light-emitting element 200 and the substrate 100. The second photosensitive layer 600 can be decomposed under laser irradiation, thereby achieving separation between the substrate 100 and the light-emitting element 200.
[0053] Preferably, the orthographic projection of the second photosensitive layer 600 on the substrate 100 coincides with the orthographic projection of the light-emitting element 200 on the substrate 100. This coincidence of projections facilitates the simultaneous patterning of the first photosensitive layer 500 and the second photosensitive layer 600, which helps to save on manufacturing costs.
[0054] Preferably, the first photosensitive layer 500 and the second photosensitive layer 600 are made of the same material. This helps to reduce the fabrication difficulty of the first photosensitive layer 500 and the second photosensitive layer 600.
[0055] Of course, in some other implementations, the second photosensitive layer may not be provided, that is, instead of using laser peeling, mechanical peeling may be used.
[0056] In one embodiment, the material of the first photosensitive layer 500 includes benzocyclobutene (BCB), which is a photosensitive adhesive. Of course, the material of the first photosensitive layer 500 can also be other materials, as long as they can be decomposed under laser irradiation to achieve the separation of the light-emitting element 200.
[0057] Furthermore, the thickness of the first photosensitive layer 500 does not exceed 5 micrometers; for example, the thickness of the first photosensitive layer 500 is 5 micrometers, 3 micrometers, or 1 micrometer. Preferably, the thickness of the first photosensitive layer 500 is 1 micrometer. The smaller the thickness, the lower the possibility of photosensitive material residue.
[0058] See Figure 7 and Figure 8 The second aspect of this application provides a method for preparing a wafer 10, the method comprising:
[0059] S100: Provides a substrate 100.
[0060] Specifically, the substrate 100 can be a sapphire substrate or a silicon carbide substrate, etc.
[0061] S200: A light-emitting element 200 is fabricated on one side of the substrate 100; wherein, the light-emitting element 200 includes a light-emitting body 210 and an electrode 220 disposed on the side of the light-emitting body 210 away from the substrate 100.
[0062] Specifically, a light-emitting body 210 and an electrode 220 are sequentially fabricated on one side of the substrate 100. The number of electrodes 220 can be multiple. For example, the electrodes 220 include positive and negative electrodes. Optionally, the light-emitting body 210 includes a P-type semiconductor layer, an N-type semiconductor layer, and a quantum well layer.
[0063] S300: A first photosensitive layer 500 is prepared on at least a portion of the surface of the light-emitting element 200 on the side opposite to the substrate 100.
[0064] Specifically, a photosensitive material is coated onto at least a portion of the surface of the light-emitting element 200 on the side opposite to the substrate 100 using a coating process. As described above, the presence of the first photosensitive layer 500 reduces the residual photosensitive material in subsequent display panel manufacturing processes, thereby improving the yield of the display panel.
[0065] In one embodiment, step S200 includes: fabricating a plurality of spaced light-emitting elements 200 on one side of the substrate 100.
[0066] Specifically, see Figure 9 Multiple light-emitting elements 200 are simultaneously fabricated on one side of the substrate 100, and the light-emitting elements 200 are spaced apart.
[0067] In one embodiment, see Figure 10 and Figure 11 The above step S300 includes:
[0068] S310: A first photosensitive layer 500 is formed on the side of the light-emitting element 200 away from the substrate 100.
[0069] Specifically, a first photosensitive layer 500 is prepared on the entire surface through a coating process. The first photosensitive layer 500 covers the side of the light-emitting element 200 away from the substrate 100, as well as the surface of the substrate 100 where the light-emitting element 200 is not disposed.
[0070] S320: Pattern the first photosensitive layer 500 to remove the first photosensitive layer 500 between two adjacent light-emitting elements 200, thereby obtaining a plurality of first photosensitive blocks 510 corresponding one-to-one with the light-emitting elements 200, wherein the light-emitting elements 200 are located between the corresponding first photosensitive blocks 510 and the substrate 100, and the plurality of first photosensitive blocks 510 are spaced apart.
[0071] Specifically, by performing exposure, development and etching processes on the first photosensitive layer 500, a portion of the first photosensitive layer 500 is removed. The removed portion includes the first photosensitive layer 500 between two adjacent light-emitting elements 200 and the first photosensitive layer 500 located at the edge of the surface of the substrate 100, thereby achieving individual separation when separating the light-emitting elements 200.
[0072] In one embodiment, prior to step S200, a second photosensitive layer 600 is prepared on one side of the substrate 100.
[0073] Specifically, see Figure 12 A second photosensitive layer 600 is prepared on one side of the substrate 100 by a coating process, so that the light-emitting element 200 can be separated from the substrate 100 by laser irradiation.
[0074] Combination Figures 13 to 16 A third aspect of this application provides a method for manufacturing a display panel, the method comprising:
[0075] S1000: The light-emitting element 200 located on one side of the substrate 100 on the wafer 10 is transferred to the first side of the first temporary substrate 300. The light-emitting element 200 includes a light-emitting body 210 and at least one electrode 220 disposed on one side of the light-emitting body 210. After being transferred to the first temporary substrate 300, the electrode 220 is located between the light-emitting body 210 and the first temporary substrate 300. At the same time, a first photosensitive layer 500 is formed on at least a portion of the surface of the light-emitting element 200 facing the first temporary substrate 300.
[0076] In this step, the light-emitting element 200 on the wafer 10 is transferred to the first temporary substrate 300. The first photosensitive layer 500 has been coated on the side of the light-emitting element 200 away from the substrate 100 before the transfer. Therefore, after the transfer, the first photosensitive layer 500 is located between the first temporary substrate 300 and the light-emitting element 200. Compared with the prior art, it is no longer necessary to set a photosensitive layer on the first temporary substrate 300. The first photosensitive layer 500 on the wafer 10 no longer needs to have a bearing effect, so the thickness can be made very thin, less than 5 micrometers, preferably 1 micrometer.
[0077] In one embodiment, prior to the aforementioned transfer, a receiving layer 700 is formed on a first side of the first temporary substrate 300. The receiving layer 700 provides superior receiving performance. Since a first photosensitive layer 500 is already formed on the wafer 10, there is no need to form a photosensitive layer on the first temporary substrate 300; only the receiving layer 700 needs to be formed on the first side of the first temporary substrate 300. The material of the receiving layer 700 includes a non-photosensitive adhesive, such as polydimethylsiloxane, which provides a significantly better receiving performance than the photosensitive materials used in the prior art. The thickness of the receiving layer 700 is not less than 10 micrometers. For example, the thickness of the receiving layer 700 can be 10 micrometers, 15 micrometers, or 20 micrometers. It is understood that since the wafer 10 of this application incorporates a first photosensitive layer 500, the receiving layer 700 on the first temporary substrate 300 no longer needs a photosensitive function; only a receiving function is required. In other words, in the prior art, a photosensitive layer is used to support the light-emitting element, which takes into account both photosensitive and support functions. However, in actual use, there is a problem that the two functions cannot be achieved simultaneously. That is, the support function is guaranteed, but the photosensitive material residue remains after laser stripping. In this application, the two functions are separated into two film layers. The photosensitive function is achieved through the first photosensitive layer 500, which is prepared on the wafer 10 and does not need to bear the support function. Therefore, the thickness of the first photosensitive layer 500 can be made thinner than the thickness of the photosensitive layer in the prior art. The support layer 700 is prepared on the first temporary substrate 300 and only needs to bear the support function. Therefore, this can meet the requirements of supporting the light-emitting element 200 and removing the light-emitting element 200 without leaving photosensitive material residue.
[0078] S2000: A second temporary substrate 800 is placed on the side of the light-emitting element 200 away from the first temporary substrate 300, and the first photosensitive layer 500 is irradiated by a laser to transfer the light-emitting element 200 on the first temporary substrate 300 to the second temporary substrate 800.
[0079] In this step, a laser can be used to irradiate the first photosensitive layer 500 through the first temporary substrate 300, causing the first photosensitive layer 500 to decompose, thereby causing the light-emitting element 200 to separate from the first temporary substrate 300 and fall onto the second temporary substrate 800. A receiving layer can be pre-formed on the receiving surface of the second temporary substrate 800 to ensure the receiving effect.
[0080] S3000: Place a driving backplate 900 on the side of the second temporary substrate 800 away from the light-emitting element 200, and transfer the light-emitting element 200 on the second temporary substrate 800 to the driving backplate 900.
[0081] In this step, after aligning the light-emitting element 200 on the second temporary substrate 800 with the pads (not shown) on the driving backplate 900, the electrode 220 of the light-emitting element 200 is bonded to the pads, so that the light-emitting element 200 and the driving backplate 900 are fixedly connected, and then the second temporary substrate 800 is peeled off.
[0082] As can be seen from the above process, since a photosensitive layer is no longer needed on the first temporary substrate 300, and a first photosensitive layer 500 is provided on the side of the light-emitting element 200 on the wafer 10 away from the substrate 100, the bearing effect of the first photosensitive layer 500 does not need to be considered, making the thickness of the first photosensitive layer 500 thinner. Therefore, when the light-emitting element 200 is separated by laser irradiation in the future, the residue of photosensitive material on the light-emitting element 200 is improved, thereby improving the yield of the display panel.
[0083] In one embodiment, see Figure 14 The wafer 10 includes a second photosensitive layer 600, which is located between the light-emitting element 200 and the substrate 100. The above step S1000 further includes: transferring the light-emitting element 200 onto the receiving layer 700 by irradiating the second photosensitive layer 600 with a laser.
[0084] Specifically, the wafer 10 can also use the same material as the first photosensitive layer 500. That is, in this embodiment, photosensitive material is provided on both the side of the light-emitting element 200 on the wafer 10 that is close to the substrate 100 and the side that is far away from the substrate 100. In this way, when the light-emitting element 200 is separated in the future, it can be separated by laser irradiation. By using the same process method, the process can be simplified and the manufacturing cost can be reduced.
[0085] Of course, in some other implementations, no photosensitive layer is provided between the substrate and the light-emitting element, and the light-emitting element and the substrate can be separated by mechanical peeling.
[0086] In one embodiment, before step S1000, the method further includes: adjusting the relative position between the substrate 100 and the first temporary substrate 300 so that the light-emitting element 200 on the substrate 100 corresponds to the target position on the first temporary substrate 300.
[0087] Specifically, when transferring the light-emitting element 200 from one side of the substrate 100 to the first temporary substrate 300, the position of the light-emitting element 200 can be adjusted accordingly as needed. For example, the light-emitting element 200 can be arranged and adjusted to the target position on the first temporary substrate 300 according to the quality of the light-emitting element 200 or the brightness difference of the light-emitting element 200. The above process is a screening of the light-emitting element 200, that is, by screening, the light-emitting element 200 after transfer can meet the requirements of the target position.
[0088] The above description is merely an embodiment of this application and does not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this application.
Claims
1. A wafer, characterized by, The wafer includes: Substrate; A light-emitting element, located on one side of the substrate, includes a light-emitting body and an electrode disposed on the side of the light-emitting body facing away from the substrate; A first photosensitive layer is disposed on at least a portion of the surface of the light-emitting element on the side opposite to the substrate.
2. The wafer of claim 1, wherein, The wafer includes: Multiple light-emitting elements are spaced apart on one side of the substrate; wherein, the multiple light-emitting elements are located between the first photosensitive layer and the substrate, the first photosensitive layer includes multiple first photosensitive blocks corresponding one-to-one with the multiple light-emitting elements, the light-emitting elements are located between the corresponding first photosensitive blocks and the substrate, and the multiple first photosensitive blocks are spaced apart; Preferably, the orthographic projection of the first photosensitive block on the substrate coincides with the orthographic projection of the corresponding light-emitting element on the substrate.
3. The wafer of claim 2, wherein, The wafer includes: The second photosensitive layer is located between the light-emitting element and the substrate; Preferably, the orthographic projection of the second photosensitive layer on the substrate coincides with the orthographic projection of the light-emitting element on the substrate; Preferably, the first photosensitive layer and the second photosensitive layer are made of the same material.
4. The wafer according to claim 1, characterized in that, The material of the first photosensitive layer includes benzocyclobutene; Preferably, the thickness of the first photosensitive layer does not exceed 5 micrometers; Preferably, the thickness of the first photosensitive layer is 1 micrometer.
5. A method for preparing a wafer, characterized in that, The method includes: Provide a substrate; A light-emitting element is fabricated on one side of the substrate; wherein the light-emitting element includes a light-emitting body and an electrode disposed on the side of the light-emitting body opposite to the substrate; A first photosensitive layer is prepared on at least a portion of the surface of the light-emitting element on the side opposite to the substrate.
6. The preparation method according to claim 5, characterized in that, The step of fabricating the light-emitting element on one side of the substrate includes: A plurality of light-emitting elements are spaced apart and fabricated on one side of the substrate; And, the step of forming a first photosensitive layer on at least a portion of the surface of the light-emitting element on the side opposite to the substrate includes: A first photosensitive layer is formed on the side of the light-emitting element that is away from the substrate. The first photosensitive layer is patterned to remove the first photosensitive layer between two adjacent light-emitting elements, thereby obtaining a plurality of first photosensitive blocks corresponding one-to-one with the light-emitting elements, wherein the light-emitting elements are located between the corresponding first photosensitive blocks and the substrate, and the plurality of first photosensitive blocks are spaced apart. Preferably, before the step of fabricating the light-emitting element on one side of the substrate, the method further includes: A second photosensitive layer is prepared on one side of the substrate.
7. A method for manufacturing a display panel, characterized in that, The method includes: A light-emitting element located on one side of a substrate on a wafer is transferred to a first side of a first temporary substrate. The light-emitting element includes a light-emitting body and at least one electrode disposed on one side of the light-emitting body. After being transferred to the first temporary substrate, the electrode is located between the light-emitting body and the first temporary substrate. At the same time, a first photosensitive layer is formed on at least a portion of the surface of the light-emitting element facing the first temporary substrate. A second temporary substrate is placed on the side of the light-emitting element away from the first temporary substrate, and the first photosensitive layer is irradiated by a laser to transfer the light-emitting element on the first temporary substrate to the second temporary substrate. A driving backplate is placed on the side of the second temporary substrate away from the light-emitting element, and the light-emitting element on the second temporary substrate is transferred to the driving backplate.
8. The preparation method according to claim 7, characterized in that, Prior to the step of transferring the light-emitting element on the wafer to the first temporary substrate, the method further includes: A receiving layer is prepared on the first side of the first temporary substrate; Preferably, the material of the bonding layer includes a non-photosensitive bonding adhesive; Preferably, the material of the non-photosensitive adhesive includes polydimethylsiloxane; Preferably, the thickness of the bearing layer is not less than 10 micrometers.
9. The preparation method according to claim 8, characterized in that, The wafer includes a second photosensitive layer located between the light-emitting element and the substrate; the step of transferring the light-emitting element on the wafer to a first side of the first temporary substrate includes: The light-emitting element is transferred to the receiving layer by irradiating the second photosensitive layer with a laser.
10. The preparation method according to claim 7, characterized in that, Prior to the step of transferring the light-emitting element on the wafer to a first side of the first temporary substrate, the method further includes: The relative position between the substrate and the first temporary substrate is adjusted so that the light-emitting element on the substrate corresponds to the target position on the first temporary substrate.