Coaxial lithium-boron alloy cathode collector assembly

By using the design of coaxial distribution of lithium-boron alloy sheets and current collecting layers and asbestos rings combined with non-penetrating nail arrays in high aspect ratio thermal batteries, the problems of coaxial positioning and electronic conductivity are solved, and the flatness of the battery is improved. and safety, simplifying the assembly process and enhancing load capacity.

CN221805570UActive Publication Date: 2024-10-01TIANJIN UNIV +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420280053.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-05
Publication Date
2024-10-01
Estimated Expiration
2034-02-05

AI Technical Summary

Technical Problem

In the existing technology, the coaxial positioning and electronic conductivity problems of high aspect ratio thermal batteries have not been effectively solved, resulting in difficult assembly of the battery stack and low safety and reliability.

Method used

The lithium boron alloy sheet is coaxially distributed with the current collecting layer. The asbestos ring is located on the periphery of the lithium boron alloy sheet. A non-penetrating spike array is set on the current collecting layer. The spikes are used for positioning and conduction. The spike material is metal or carbon. Electronically conductive, the array is designed to improve flatness and heat balance.

Benefits of technology

The coaxial fixation and flattening of the negative electrode components are integrated, reducing the difficulty of stack assembly, improving the safety and reliability of the battery, and enhancing the later pulse load capacity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221805570U_ABST
    Figure CN221805570U_ABST
Patent Text Reader

Abstract

The utility model provides a coaxial lithium-boron alloy cathode current collecting assembly. The coaxial lithium-boron alloy cathode current collecting assembly comprises a lithium-boron alloy sheet, an asbestos ring and a current collecting layer, the lithium-boron alloy sheet and the current collecting layer are coaxially distributed up and down; the asbestos ring is arranged on the current collecting layer and is positioned on the periphery of the lithium-boron alloy sheet; a nail thorn array is arranged on the current collecting layer, the nail thorn array comprises a plurality of nail thorns, the nail thorns are connected with the lithium-boron alloy sheet, and the nail thorns are used for positioning the lithium-boron alloy sheet; and the extension height of the nail thorns is 10%-90% of the thickness of the lithium-boron alloy sheet. The assembly coaxial structure provided by the utility model is favorable for improving the smoothness and reducing the assembly difficulty of the galvanic pile; the needling array can balance heat and reduce thermal shock; and the high-electron-conductivity needling array is beneficial to improving the later-stage pulse load capacity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of chemical power source thermal batteries, in particular to a coaxial lithium-boron alloy negative electrode current collecting component. Background Art

[0002] Thermal batteries are a reserve power source that uses pyrotechnic sources to melt and activate solid electrolytes. They have the advantage of compact space and volume, and are particularly suitable for high-voltage system power design. Due to the high voltage design, the unit battery requires enough single cells to be connected in series and parallel, so high aspect ratio thermal batteries have become an important development direction. Therefore, improving the flatness of the electrodes in the single cell and ensuring the coaxial assembly of the components have become key process points.

[0003] In current research, lithium-boron alloy plays an important role in the development of high-energy thermal batteries, with a specific capacity of about 4000As / g. However, there is free lithium in lithium-boron alloy, which is prone to overflow in application. Therefore, a current limiting ring made of asbestos is generally used on the current collector for protection, and a suitable gap is left to ensure volume expansion during the phase change process. Due to the existence of the gap, the center of the lithium-boron alloy and the current collector are not necessarily coaxial, and relative movement may occur during the assembly process. It may even happen that the lithium-boron alloy is not confined in the asbestos ring. Especially in high aspect ratio thermal batteries, the center of the negative electrode assembly is not coaxial, which can easily cause the battery stack to tilt and bend. Therefore, repeated corrections are required to ensure the reliability of battery assembly.

[0004] The patent document with publication number CN206003891U discloses a new type of thermal battery single cell, including a current collector, a negative electrode, a composite sheet containing a positive electrode and a diaphragm, and a current limiting ring made of insulating material, wherein the current limiting ring is bonded to the current collector, the negative electrode is placed at the bottom of the current limiting ring and in contact with the current collector, the composite sheet is placed in the current limiting ring and above the negative electrode, and a gap is left between the inner wall of the current limiting ring and the outer wall of the composite sheet and the negative electrode sheet. The patent document relates to a single cell with multiple asbestos ring components, which is used to prevent the flow of metallic lithium, but the patent document does not solve the problem of coaxial positioning.

[0005] The patent document with publication number CN109817882A discloses a thermal battery lithium-boron alloy negative electrode assembly and a preparation method thereof, which belongs to the field of thermal battery technology. The thermal battery lithium-boron alloy negative electrode assembly includes a current collector, a metal mesh and a lithium-boron alloy negative electrode sheet; the current collector, the metal mesh and the lithium-boron alloy negative electrode sheet are all cylindrical structures, and a circular groove is opened on the upper surface of the current collector, and the metal mesh and the lithium-boron alloy negative electrode sheet are both located in the circular groove; and the metal mesh is sandwiched between the lithium-boron alloy negative electrode sheet and the current collector. The patent document relates to a metal-wrapped lithium-boron negative electrode material, in which a metal mesh is introduced between the current collector layer and the lithium-boron alloy for positioning, but the metal mesh does not wet with lithium, and an air film layer may be generated, increasing the internal resistance; at the same time, the process is relatively complicated, and the metal has a high strength. In the case of uneven electrodes, it is easy to cause powder electrodes to break, reducing the safety and reliability of the battery.

[0006] Therefore, in the current process, the safety of the negative electrode is mainly improved by restricting the free flow of lithium. There is no report on how to ensure the coaxiality and electronic conductivity of high aspect ratio thermal batteries from the perspective of the current collector. Utility Model Content

[0007] In view of the defects in the prior art, the purpose of the utility model is to provide a coaxial lithium-boron alloy negative electrode current collecting assembly.

[0008] According to the utility model, a coaxial lithium-boron alloy negative electrode current collecting component is provided, comprising: a lithium-boron alloy sheet, an asbestos ring and a current collecting layer;

[0009] The lithium-boron alloy sheet and the current collecting layer are coaxially arranged vertically; the asbestos ring is arranged on the current collecting layer and is located at the periphery of the lithium-boron alloy sheet;

[0010] The current collecting layer is provided with a spike array, which includes a plurality of spikes, which are connected to the lithium-boron alloy sheet and used to position the lithium-boron alloy sheet; the extension height of the spikes is 10% to 90% of the thickness of the lithium-boron alloy sheet.

[0011] Preferably, the total lithium content of the lithium-boron alloy sheet is 50-70%, the thickness of the lithium-boron alloy sheet is 0.05-2 mm, and the free lithium content of the lithium-boron alloy sheet is 20%-50%.

[0012] Preferably, the spike array is a non-penetrating spike array;

[0013] The surface of the current collecting layer where the non-penetrating spike array is located is a first surface, and the surface of the current collecting layer opposite to the first surface is a second surface. There are no through holes or through channels between the first surface and the second surface.

[0014] Preferably, the plurality of spikes include hollow spikes and a mixed arrangement of hollow and solid spikes.

[0015] Preferably, the shapes of the plurality of spikes include any one or more of the following: spike-shaped, needle-shaped, thorn-shaped, cone-shaped, umbrella-shaped, triangular prism, cylindrical, polygonal prism, triangular pyramid, and cone-shaped.

[0016] Preferably, the spikes have electronic conductivity.

[0017] Preferably, the material of the spikes includes metal and / or carbon material;

[0018] The metal is any one or more of the following: stainless steel, iron, nickel, copper, silver, and carbon fiber.

[0019] Preferably, taking the surface of the current collecting layer where the spike array is located as a reference surface, the sum of the bottom areas of a plurality of the spikes is 0.01% to 50% of the area of ​​the reference surface.

[0020] Preferably, the number of the spikes is 1 to 1000, and the distance between two adjacent spikes is 0.01 to 10 mm.

[0021] Preferably, the negative electrode current collecting assembly is an integrated structure, the asbestos ring is adhered to the current collecting layer, and the spikes on the current collecting layer are embedded in the bulk phase of the lithium-boron alloy sheet.

[0022] Compared with the prior art, the utility model has the following beneficial effects:

[0023] 1. The negative electrode current collector coaxial structure of the utility model is conducive to improving flatness and reducing the difficulty of stack assembly. The negative electrode current collector coaxial structure of the utility model is coaxially fixed and flattened and integrated to prevent the movement of components, reduce the time of repeated coaxial correction of the battery stack, and make the process operation simpler.

[0024] 2. The needle array of the utility model can balance heat and reduce thermal shock. The needle array on the current collector layer can slow down the heat conduction at the initial stage of activation from two dimensions: heat transfer thickness (temperature gradient) and heat transfer material (thermal conductivity), reduce transient thermal shock, and prevent local high temperature. At the same time, the hollow needle array can form a small amount of pore layer on the back of the negative current collector layer. The gas thermal conductivity is low, which can reduce the heat conduction at the initial stage of activation, and is more conducive to weakening transient thermal shock and maintaining better safety of the battery.

[0025] 3. The needle puncture array of the utility model can prevent the collapse of the lithium-boron alloy structure, maintain the good structural strength of the negative electrode, prevent the deformation of the negative electrode current collector, and improve the quality reliability of the battery. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Other features, objects and advantages of the present invention will become more apparent by reading the detailed description of non-limiting embodiments with reference to the following drawings:

[0027] Figure 1 It is a schematic diagram of the structure of a coaxial lithium-boron alloy negative electrode current collecting assembly;

[0028] Figure 2 It is a schematic diagram of the assembly of the coaxial lithium-boron alloy negative electrode current collector assembly;

[0029] Figure 3 It is a schematic diagram of the structure of the current collecting layer;

[0030] Figure 4 It is a schematic diagram of the cross-sectional structure of a coaxial lithium-boron alloy negative electrode current collecting assembly;

[0031] Figure 5 This is a schematic diagram of battery discharge performance in Example 2;

[0032] Figure 6 This is a schematic diagram of the activation curve of the battery in Example 2;

[0033] Figure 7 Schematic diagram of the pulse load of the battery in Example 2.

[0034] The figure shows:

[0035] Lithium boron alloy sheet 1 Reference surface 301

[0036] Asbestos 2 Spike Array 4

[0037] Collector layer 3 spike 401 DETAILED DESCRIPTION

[0038] The utility model is described in detail below in conjunction with specific embodiments. The following embodiments will help those skilled in the art to further understand the utility model, but do not limit the utility model in any form. It should be pointed out that for those of ordinary skill in the art, several changes and improvements can be made without departing from the concept of the utility model. These all belong to the protection scope of the utility model.

[0039] Embodiment 1:

[0040] like Figures 1 to 3 As shown, this embodiment provides a coaxial lithium-boron alloy sheet negative electrode current collecting assembly, wherein the negative electrode assembly consists of a lithium-boron alloy sheet 1, an asbestos ring 2 and a current collecting layer 3, wherein the lithium-boron alloy sheet 1 and the current collecting layer 3 are coaxially distributed up and down, and the asbestos ring 2 is arranged on the outer periphery of the lithium-boron alloy sheet 1 on the current collecting layer 3; wherein a non-penetrating spike array 4 is arranged on the current collecting layer 3, and the spike extension height is 10% to 90% of the thickness of the lithium-boron alloy sheet 1.

[0041] The lithium-boron alloy sheet 1 and the current collecting layer 3 are coaxially distributed up and down. The lithium-loaded amount of the lithium-boron alloy sheet 1 is 50% to 70%, the free lithium is 20% to 50%, and the thickness is 0.05 to 2 mm. The lithium-loaded amount is an important indicator for measuring the specific capacity of the negative electrode of the thermal battery. The lithium-boron alloy sheet 1 is composed of a lithium-boron alloy sheet 1 skeleton and adsorbed free lithium. The lithium-loaded amount is the total lithium content, and the free lithium content is the non-alloy lithium content, which can generally be quantitatively determined by differential thermal analysis. Increasing the lithium-loaded amount increases the theoretical capacity, the free lithium content increases synchronously, and the difficulty of safe use also increases. In this embodiment, the lithium-loaded amount is 50% to 70%, and the free lithium is 20% to 50%. When the lithium-loaded amount of the lithium-boron alloy sheet 1 is less than 50%, the hardness is large, the brittleness is strong, the machining performance is poor, and the capacity is low, which is not conducive to the application in the thermal battery. When the lithium-loaded amount is greater than 70%, the lithium-boron alloy sheet 1 is easy to flow at high temperature, and the battery short circuit is easy to occur. The thickness will affect the total mass of the negative electrode and will also indirectly increase the negative electrode capacity. If the thickness is less than 0.05mm, it is difficult to process; if the thickness is greater than 2mm, it is difficult to use thermal balance design. The thickness of 0.05 to 2mm is the commonly used negative electrode thickness.

[0042] The spikes on the current collecting layer 3 extend to the interior of the lithium-boron alloy sheet 1. The spikes are mainly used to ensure the coaxiality of the negative electrode, balance heat and increase electronic conductivity. If the extended height of the spikes is less than 10% of the thickness of the lithium-boron alloy sheet 1, the above effect is not obvious or even non-existent. If the extended height of the spikes is higher than 90%, the negative electrode may be pierced by the spikes, or surface bumps may be formed, reducing the flatness.

[0043] The spike array 4 on the current collecting layer 3 is a non-penetrating structure, and there are no through holes or through channels on the side and back side where the non-penetrating spike array 4 is located. The current collecting layer 3 can isolate the negative electrode from the heating layer (generally Fe-KClO4) to prevent the lithium-boron alloy sheet 1 from reacting with potassium perchlorate and its reaction products.

[0044] The spikes include hollow spikes and solid and hollow mixed spikes. The spikes include hollow spikes to better form an air layer locally, prevent free lithium from splashing in the lithium-boron alloy sheet 1 due to thermal shock, and improve safety performance.

[0045] The shapes of the spikes 401 include spikes, needles, thorns, cones, umbrellas, triangular prisms, cylinders, polygonal prisms, triangular pyramids, cones, cone-like shapes and other regular and irregular shapes with sharp corners. The spikes are mainly used to better penetrate into the lithium-boron alloy sheet 1 to increase the contact area and strength.

[0046] The material of the spike 401 has electronic conductivity, including metal and carbon material, and the metal includes at least one of stainless steel, iron, nickel, copper, silver, and carbon fiber. The spike is located on the current collecting layer 3, and its material is required to have high electronic conductivity. This solution has high cost and processing advantages.

[0047] The array is referenced to the reference plane 301 of the current collecting layer 3, the nail bottom area is 0.01% to 50% of the area of ​​the current collecting layer 3, the number of nails is 1 to 1000, and the nail spacing is 0.01 to 10 mm. The parameters of the nail bottom area, number, and spacing are determined according to the design requirements, processing equipment, and usage.

[0048] The negative electrode assembly structure is an integrated structure, the asbestos ring is adhered to the current collecting layer 3, and the spikes on the current collecting layer 3 are embedded in the bulk of the lithium-boron alloy sheet 1, and there is no slippage under a force of 0.1 to 10 N. The asbestos ring can be adhered to the current collecting layer 3, or it can be embedded on the lithium-boron alloy sheet 1 to form an integrated part by controlling the gap between the lithium-boron alloy sheets 1.

[0049] The high electron conductivity needle array is conducive to improving the later pulse load capacity. The needle array is embedded in the lithium-boron alloy sheet 1 to increase the contact area, provide more electron transfer channels, and ensure the efficient capacity output of the battery, especially at the end of discharge. The excellent conductivity can reduce the internal resistance and improve the large current load capacity.

[0050] This embodiment also provides a method for preparing a coaxial lithium-boron alloy negative electrode current collector assembly, the specific steps of which include:

[0051] S1. Preparation of current collecting layer: Processing the current collecting layer 3 substrate into a current collecting disc without burrs, flatness and wrinkles;

[0052] S2, spike array processing: processing the current collecting wafer into a centrally positioned spike array 4 (after washing and drying), to obtain a current collecting wafer with a spike array 4;

[0053] S3, asbestos ring bonding: bonding the asbestos ring to the outer periphery of one side of the spike array 4 current collecting disc, maintaining the coaxial structure, and drying to obtain the current collecting assembly;

[0054] S4, component integrated processing: the lithium-boron alloy sheet 1 with the center positioned is nested inside the asbestos ring of the current collecting component, and the sheet is flattened and integrated to obtain a coaxial lithium-boron alloy negative electrode current collecting component.

[0055] In step S2, the processing of the spike array 4 includes welding, vacuum plating, 3D printing, spraying, printing, stamping, etc. For example, metal is deposited on the current collecting layer 3 by vacuum plating, or the hollow spike array 4 is stamped by a mold.

[0056] In step S4, the processing methods include extrusion, rolling, welding, riveting, etc. Since the lithium-boron alloy sheet 1 is soft and has a certain ductility, the integrated processing can generally be ensured by mechanical physical contact.

[0057] The preparation method of this embodiment has strong operability and high stability, and the product quality is safe and reliable, and it is easy to realize batch preparation.

[0058] The present embodiment provides a coaxial lithium-boron alloy negative electrode current collector assembly, the lithium-boron alloy sheet 1 can have a lithium loading of 60-72%, and a specific capacity greater than 4000A·s / g, which can meet the assembly requirements of high aspect ratio thermal batteries. The preparation method provided in the present embodiment has a simple process, simple operation, high reliability, and can be manufactured and produced on a large scale. The coaxial structure of the negative electrode current collector assembly provided in the present embodiment is conducive to improving flatness and reducing the difficulty of stack assembly; the needle array can balance heat and reduce thermal shock; the high electronic conductivity needle array is conducive to improving the later pulse load capacity.

[0059] This embodiment aims at the technical problems that the asbestos ring and the lithium-boron alloy sheet 1 in the negative electrode assembly of the high aspect ratio thermal battery are not in close contact, there is a gap, and there is relative sliding and eccentricity between the lithium-boron alloy sheet 1 and the current collecting layer 3, which easily leads to uneven battery stacks of the high aspect ratio thermal battery, and uneven force is easily caused under high-strength fastening pressure, resulting in electrode damage, tilting and bending of the battery stack, and reduced reliability. A coaxial lithium-boron alloy negative electrode current collecting assembly is developed. This embodiment uses a spike array 4 on the current collecting layer 3 to position and fix the lithium-boron alloy sheet 1 to form an integrated concentric coaxial negative electrode current collecting assembly with high flatness, and the spike array 4 with electronic conductivity can reduce the internal resistance of the negative electrode material, accelerate the electron transfer ability in the alloy phase, and enhance the pulse load capacity when free lithium is consumed.

[0060] The coaxial lithium-boron alloy negative electrode current collecting assembly of this embodiment has the following advantages:

[0061] a. The coaxial structure of the negative electrode current collecting assembly is conducive to improving flatness and reducing the difficulty of stack assembly.

[0062] After the thermal battery is activated, the temperature rises rapidly. The volume of the lithium-boron alloy sheet 1 expands due to the metal phase change, and some free metal lithium overflows. Therefore, an asbestos current limiting ring is generally used to prevent the lithium-boron alloy sheet 1 from flowing and overflowing. There is a gap between the lithium-boron alloy sheet 1 and the current limiting ring. The non-fixed lithium-boron alloy sheet 1 may slide relative to the current collecting layer 3 in the ring. Therefore, when the electrode sheet is stacked, it will be repeatedly adjusted and leveled. Especially when the battery stack height exceeds 200mm, it is more likely that the electrode will deviate from the axis, increasing the difficulty of assembly. In severe cases, it will cause electrode damage, and even tilt or twist the top and bottom of the battery stack, reducing quality reliability. The components of this embodiment are coaxially fixed and flattened and integrated to prevent the movement of each component, reduce the time for repeated coaxial correction of the battery stack, and make the process operation simpler.

[0063] b. The needle array can balance heat and reduce thermal shock.

[0064] At the moment of thermal battery activation, the heating sheet ignites quickly, and the instantaneous temperature reaches 1000°C. As the heat is transferred, the temperature drops rapidly to 550°C to 650°C. Therefore, the transient high temperature shock will cause the free lithium in the non-uniform lithium-boron alloy sheet 1 to overflow irreversibly. According to Fourier's law of thermal conductivity, per unit area, the needle array on the current collector 3 of this embodiment can slow down the heat conduction at the initial stage of activation from two dimensions: heat transfer thickness (temperature gradient) and heat transfer material (thermal conductivity), reduce transient thermal shock, and prevent local high temperature. At the same time, the hollow needle array can form a small amount of pore layer on the back of the negative electrode current collector 3. The gas thermal conductivity is low, which can reduce the heat conduction at the initial stage of activation, and is more conducive to weakening the transient thermal shock peak and maintaining better battery safety.

[0065] c. High electronic conductivity needle array is beneficial to improve the later pulse load capacity.

[0066] During the discharge process of the lithium-boron alloy sheet 1, as the depth of discharge consumes the metallic lithium, the free lithium enters the electrolyte, and the alloy phase represented by Li7B6 or Li5B4 has low electronic conductivity. The needle array is embedded in the lithium-boron alloy sheet 1 to increase the contact area, provide more electron transfer channels, and ensure the efficient capacity output of the battery, especially at the end of discharge. The excellent conductivity can reduce the internal resistance and improve the large current load capacity. In addition, the needle array can prevent the structural collapse of the lithium-boron alloy sheet 1, maintain the good structural strength of the negative electrode, prevent the deformation of the negative electrode collector, and improve the quality and reliability of the battery.

[0067] Embodiment 2:

[0068] Those skilled in the art may understand this embodiment as a more specific description of Embodiment 1.

[0069] This embodiment provides a coaxial lithium-boron alloy negative electrode current collecting assembly consisting of a lithium-boron alloy sheet 1, an asbestos ring 2 and a current collecting layer 3, such as Figure 1 As shown, the lithium-boron alloy sheet 1 (diameter Φ48) and the current collecting layer 3 (diameter Φ52) are coaxially distributed up and down, the lithium-boron alloy sheet 1 has a lithium loading of 60%, free lithium of about 32%, and a thickness of 0.5 mm. A non-penetrating spike array 4 is provided on the current collecting layer 3, and the spike extension height is 60% of the thickness of the lithium-boron alloy sheet 1, that is, 0.3 mm.

[0070] There are no through holes or through channels on the surface and back of the non-penetrating spike array 4. The spikes are hollow spikes, the spikes are conical in shape, the bottom diameter is 2mm, and the spike material is stainless steel with electronic conductivity; the array is referenced to the reference plane of the current collecting layer 3, the bottom area of ​​the spikes is about 13.89% of the area of ​​the current collecting layer 3, the number of spikes is (8×10)+1, and the spike spacing is 2mm. The structure of the negative electrode current collecting assembly is an integrated structure, the outer diameter of the asbestos ring is Ф52, the inner diameter is Ф49, it is adhered to the current collecting layer 3, and the spikes on the current collecting layer 3 are embedded in the bulk phase of the lithium-boron alloy sheet 1, and there is no sliding under the action of 8N.

[0071] This embodiment also provides a method for preparing a coaxial lithium-boron alloy negative electrode current collector assembly, such as Figure 2 As shown, the specific steps include:

[0072] S1. Preparation of current collecting layer: Process the current collecting layer 3 substrate into a Φ52 current collecting disc without burrs, flatness and wrinkles;

[0073] S2. Processing of spike array: a centrally positioned spike and spike array 4 (8×10) are processed on the current collecting disc by a die stamping method. Due to the stamping method, the spike is formed by deformation of the current collecting material and is hollow. After washing and drying, a current collecting disc with spike array 4 is obtained;

[0074] S3, asbestos ring bonding: bonding the asbestos ring to one side of the spike array 4 current collecting disc, maintaining the coaxial structure, and drying to obtain the current collecting assembly, such as Figure 3 As shown;

[0075] S4, component integration processing: The centrally positioned lithium-boron alloy sheet 1 is nested with the current collecting assembly, and a sheet press is used to extrude the sheet at a pressure of 0.1 MPa. The spike array 4 on the current collecting assembly is inserted into the ductile lithium-boron alloy sheet 1, and then a 50T hydraulic press (manufactured by Hyde) is used to flatten and integrate the sheet at a pressure of 200KN to obtain a coaxial lithium-boron alloy current collecting negative electrode assembly, the cross-sectional schematic diagram of which is shown in FIG. Figure 4 shown.

[0076] The prepared material was used as a thermal battery current collector negative electrode component, and the positive electrode was manufactured by a high-temperature heat treatment process with iron disulfide: lithium oxide: molten salt electrolyte (LiCl-KCl=45-55) in a ratio of 80:2:18. A mixture of magnesium oxide and a ternary all-lithium electrolyte (LiF-LiCl-LiBr=9.6-22-68.4) was used as a diaphragm in a ratio of 50-50. The positive electrode diaphragm material was prepared into a Ф52 positive electrode sheet (5.5g, about 1mm thick) and a diaphragm sheet (2.5g, about 0.5mm thick) by a powder pressing method. The heating sheet used Fe-KClO4 powder (ratio of 84-16) (6.3g, about 0.75mm). The coaxial lithium-boron alloy negative electrode current collector component and the conventional lithium-boron current collector component (i.e., without needle puncture) were used as negative electrodes, respectively. The battery pack was assembled into 32 cells in parallel with 32 cells, and the electrical performance test showed that the two batteries could discharge normally and the discharge voltage was stable. The discharge curve was as shown in the figure. Figure 5 As shown in the figure, the corresponding working times are 1888s and 1779s respectively, indicating that the coaxial lithium-boron alloy negative electrode current collector assembly can improve the output performance of the battery, especially the high current load capacity in the later stage. Figure 6 As shown in Figure 1, the activation times are 0.9s and 0.6s respectively. The activation time delay indicates that the hollow spike array 4 has the function of adjusting transient thermal shock and can balance the heat. Figure 7 As shown, the voltage drops are 4.8V and 4V respectively, indicating that the spike array 4 in the coaxial lithium-boron alloy negative electrode current collecting assembly can improve the electronic conductivity of the lithium-boron alloy sheet 1 and enhance the large current pulse load capacity.

[0077] The component coaxial structure provided by the utility model is conducive to improving flatness and reducing the difficulty of stack assembly; the needle-pierced array can balance heat and reduce thermal shock; the high electronic conductivity needle-pierced array is conducive to improving the later pulse load capacity.

[0078] In the description of the present application, it should be understood that the terms "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0079] The above describes the specific embodiments of the present invention. It should be understood that the present invention is not limited to the above specific embodiments, and those skilled in the art can make various changes or modifications within the scope of the claims, which does not affect the essence of the present invention. In the absence of conflict, the embodiments of the present application and the features in the embodiments can be combined with each other at will.

Claims

1. A coaxial lithium-boron alloy negative electrode current collecting assembly, It is characterized in that include: A lithium-boron alloy sheet (1), an asbestos ring (2) and a current collecting layer (3); The lithium-boron alloy sheet (1) and the current collecting layer (3) are coaxially arranged in an upper and lower distribution; the asbestos ring (2) is arranged on the current collecting layer (3) and is located at the periphery of the lithium-boron alloy sheet (1); A spike array (4) is provided on the current collecting layer (3), the spike array (4) comprising a plurality of spikes (401), the spikes (401) being connected to the lithium-boron alloy sheet (1), the spikes (401) being used to position the lithium-boron alloy sheet (1); and the extension height of the spikes (401) is 10% to 90% of the thickness of the lithium-boron alloy sheet (1).

2. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The total lithium content of the lithium-boron alloy sheet (1) is 50-70%, the thickness of the lithium-boron alloy sheet (1) is 0.05-2 mm, and the free lithium content of the lithium-boron alloy sheet (1) is 20-50%.

3. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The spike array (4) is a non-penetrating spike array; The surface of the current collecting layer (3) where the non-penetrating spike array is located is the first surface, and the surface of the current collecting layer (3) opposite to the first surface is the second surface, and there are no through holes or through channels between the first surface and the second surface.

4. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The plurality of spikes (401) include hollow spikes and spikes in a mixed arrangement of hollow and solid spikes.

5. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The shapes of the spikes (401) include any one or more of the following: spike-shaped, needle-shaped, thorn-shaped, cone-shaped, umbrella-shaped, triangular prism, cylindrical, polygonal prism, triangular pyramid, and cone-shaped.

6. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The spikes (401) have electronic conductivity.

7. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 6, It is characterized in that The material of the spike (401) includes metal and / or carbon material; The metal is any one or more of the following: stainless steel, iron, nickel, copper, silver, and carbon fiber.

8. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The surface of the current collecting layer (3) where the spike array (4) is located is taken as a reference surface (301), and the sum of the bottom areas of a plurality of spikes (401) is 0.01% to 50% of the area of ​​the reference surface (301).

9. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The number of the spikes (401) is 1 to 1000, and the distance between two adjacent spikes (401) is 0.01 to 10 mm.

10. The coaxial lithium-boron alloy negative electrode current collecting assembly according to claim 1, It is characterized in that The negative electrode current collecting assembly is an integrated structure, the asbestos ring (2) is adhered to the current collecting layer (3), and the spikes (401) on the current collecting layer (3) are embedded in the bulk phase of the lithium-boron alloy sheet (1).