Anti-aging environment-friendly asphalt pavement
By using the slag ash base layer, gravel and stone layer structure in the asphalt pavement, combined with the asphalt pavement and fiberglass mesh, the problem of erosion of paving materials after rainwater penetration is solved, and the anti-aging performance and service life of the asphalt pavement are significantly improved.
Patent Information
- Application Number
- CN202323474813.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-20
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2033-12-20
AI Technical Summary
The existing asphalt pavement materials are easily eroded after rainwater penetrates, resulting in poor anti-aging effect.
Use slag ash as the base layer, 200mm grade gravel as the first layer, 68mm coarse gravel as the second layer, and fill the gaps with 20mm fine gravel to form the first cushion layer and 15cm thick asphalt pavement. Asphalt slurry is sprayed on the surface and fiberglass mesh is laid to improve water diversion and moisture management capabilities.
It effectively avoids moisture accumulation, reduces side shear, and improves the anti-aging performance and service life of the road surface.
Smart Images

Figure CN221810489U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of roadbed structures, in particular to an anti-aging and environmentally friendly asphalt pavement. Background Art
[0002] Compared with traditional cement pavement, asphalt pavement has a shorter construction period, is more durable and has lower subsequent maintenance costs. It has become the mainstream roadbed.
[0003] In conjunction with the publication (announcement) number: CN116623492A, the publication (announcement) date: 2023-08-22, an asphalt concrete pavement structure and a paving method thereof are disclosed, wherein the asphalt concrete pavement structure is composed of a 1.5-2.5 cm anti-skid wear layer, a bonding layer, a 5-8 cm anti-rutting load-bearing layer, a 1.5-2 cm anti-fatigue stress absorption layer, a permeable layer and a base layer from top to bottom; the anti-rutting load-bearing layer contains an asphalt modifier with PET recycled material, SBS, LDPE, isocyanate and a compatibilizer as the main components. The pavement structure is easy to pave, which greatly reduces the pavement structure. While achieving a high utilization rate of PET recycled materials, it also significantly reduces the rutting problem and improves the durability of the pavement, improves the low-temperature cracking resistance of the pavement, and the pavement structure has a service life of not less than 15 years for the asphalt upper layer and not less than 30 years for other structural layers under heavy-load traffic conditions. The pavement structure is a durable pavement structure, which greatly improves the service life of the pavement.
[0004] In the prior art including the above patent, the influence of the roadbed paving material on the asphalt pavement is very important. The above patent does not consider the erosion of the paving material after rainwater infiltration, so the anti-aging effect after paving is relatively general. Utility Model Content
[0005] The utility model aims to provide an anti-aging and environmentally friendly asphalt pavement to solve the above problems.
[0006] In order to achieve the above-mentioned purpose, the utility model provides the following technical solutions: an anti-aging and environmentally friendly asphalt pavement, comprising a first paving layer, a base layer, a second paving layer, a fourth paving layer, a first cushion layer, a fiberglass mesh and an asphalt pavement arranged in sequence from the roadbed upward.
[0007] Preferably, the first paving layer is 200 mm grade gravel with a thickness of 10 cm.
[0008] Preferably, the base layer is slag ash with a thickness of 20-25 cm.
[0009] Preferably, the second paving layer is 68 mm coarse-grained stone blocks with a thickness of 5-8 cm.
[0010] Preferably, the fourth paving layer is 20 mm fine-grained stone with a thickness of 5-5 cm.
[0011] Preferably, the fourth paving layer is an asphalt surface with a thickness of 3-4 cm, and asphalt slurry is provided on the surface.
[0012] Preferably, the thickness of the asphalt pavement is 15 cm.
[0013] In the above technical scheme, the utility model provides an anti-aging and environmentally friendly asphalt pavement, which has the following beneficial effects: the base layer of slag ash is paved on the first paving layer of 200mm gravel, and a roller is used to roll it to achieve compaction, and then a fourth paving layer of 20mm fine-grained stone is added on the basis of the second paving layer of 68mm coarse-grained stone blocks to fill the gap of the second paving layer, and then a roller is used to roll it to achieve compaction. Then asphalt is laid to form the first cushion layer, followed by spraying asphalt slurry and laying glass fiber mesh, and finally laying an asphalt pavement with a thickness of 15cm. Gravel is used to quickly form a diversion, thereby preventing seepage water from accumulating on both sides of the paving material, and then the base layer can have a certain conservation effect on water and reduce the side cut caused by water accumulation. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present utility model. For ordinary technicians in this field, other drawings can also be obtained based on these drawings.
[0015] Figure 1 A schematic diagram of the cross-section structure provided for an embodiment of the utility model.
[0016] Description of reference numerals:
[0017] 1. First layer; 2. Base layer; 3. Second layer; 4. Fourth layer; 5. First cushion layer; 6. Fiberglass mesh; 7. Asphalt pavement. DETAILED DESCRIPTION
[0018] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention will be further described in detail below in conjunction with the accompanying drawings.
[0019] like Figure 1As shown, an anti-aging environmentally friendly asphalt pavement uses a base layer 2 of slag ash to be laid on a 200mm grade gravel first paving layer 1, and a roller is used to roll it to achieve compaction. Then, on the basis of laying a second paving layer 3 of 68mm coarse-grained stone blocks, a fourth paving layer 4 of 20mm fine-grained stone is added to fill the gap of the second paving layer 3, and then a roller is used to achieve compaction. Then asphalt is laid to form the first cushion layer 5, followed by spraying asphalt slurry and laying glass fiber mesh 6, and finally laying an asphalt pavement 7 with a thickness of 15cm. Gravel is used to quickly form a diversion, thereby preventing seepage water from accumulating on both sides of the paving material, and then the base layer 2 can have a certain conservation effect on water and reduce the side cut caused by water accumulation.
[0020] The above only describes some exemplary embodiments of the present invention by way of illustration. It is undoubted that those skilled in the art can modify the described embodiments in various ways without departing from the spirit and scope of the present invention. Therefore, the above drawings and descriptions are illustrative in nature and should not be construed as limiting the scope of protection of the claims of the present invention.
Claims
1. An anti-aging and environmentally friendly asphalt pavement, characterized in that: It comprises a first paving layer (1), a base layer (2), a second paving layer (3), a fourth paving layer (4), a first cushion layer (5), a glass fiber mesh (6) and an asphalt pavement (7) which are arranged in sequence from the roadbed upwards; The first paving layer (1) is 200 mm grade gravel with a thickness of 10 cm; The base layer (2) is slag ash with a thickness of 20-25 cm; The second paving layer (3) is made of 68 mm coarse-grained stone blocks with a thickness of 5-8 cm; The fourth paving layer (4) is 20 mm fine-grained stone with a thickness of 5-5 cm; The first paving layer (5) is an asphalt surface with a thickness of 3-4 cm, and an asphalt slurry is provided on the surface; The thickness of the asphalt pavement (7) is 15 cm.