Sample for simulating debonding defect of coated grain

By using mechanical drilling technology and a sealed screw structure to simulate debonding defects on the grain column test block, the problem of difficulty in simulating small-size defects in the existing technology is solved, and more efficient and accurate detection of debonding defects is achieved.

CN221826584UActive Publication Date: 2024-10-11HUBEI INST OF AEROSPACE CHEMOTECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420240218.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-31
Publication Date
2024-10-11
Estimated Expiration
2034-01-31

AI Technical Summary

Technical Problem

When the existing technology simulates the debonding defect of a small-sized coated grain column, the production process is cumbersome and difficult to succeed, resulting in inconsistent artificial design values ​​and actual values, especially the phenomenon of double-layer film deviation and glue filling when simulated by the buried film method. Frequent occurrences affect the success rate of sample production.

Method used

The mechanical drilling method is used to provide covered arc surface and debonding defect size holes on the grain column test block, and combined with the sealing screw and threaded hole structure, accurate debonding defects are simulated to ensure that the sample design is consistent with the actual value.

Benefits of technology

It improves the success rate and accuracy of test results for simulating the debonding defect of the coated grain column, simplifies the sample production process, and enhances the detection efficiency and the authenticity of the results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221826584U_ABST
    Figure CN221826584U_ABST
Patent Text Reader

Abstract

The sample comprises a grain test block, a coating layer and a sealing screw rod, the grain test block is provided with a coating cambered surface, the coating layer is bonded on the coating cambered surface, the coating cambered surface is provided with a debonding defect size hole, the bottom of the debonding defect size hole is provided with a threaded hole, and the sealing screw rod is arranged in the threaded hole. The sealing screw rod is connected with the threaded hole, and a gap for simulating a debonding defect is reserved between the tail end of a rod body of the sealing screw rod and the coating layer. When the shearing speckle interference system based on the Michelson light path is subjected to external load, tiny non-uniform deformation is generated on the surface of a debonding defect position, the shearing speckle interference system based on the Michelson light path is used for carrying out flaw detection experiment on a sample, a detection result is consistent with an interface debonding defect of an actual coated grain, and the testing efficiency and the authenticity and the accuracy of the testing result are greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of debonding defect detection, in particular to a sample for simulating the debonding defect of a coated drug column. Background Art

[0002] During the coating and transportation process of solid propellants, bonding defects such as debonding, bubbles, and inclusions may occur. In practical flaw detection work, engineers generally use the buried film method to place a double layer of polytetrafluoroethylene film between the propellant and the coating layer to simulate the interface debonding defect. Studies have found that the production process of artificial debonding defects in this way is cumbersome, and phenomena such as double-layer film deviation and glue filling between the two layers of film often occur, resulting in inconsistency between the design value of the artificial debonding defect and the actual value, leading to failure in sample production. Especially when simulating small-sized defects, it is particularly difficult to simulate debonding defects by the buried film method, and it is difficult to succeed. Therefore, there is an urgent need for a simple and reliable specimen with accurate simulated debonding defect values. Utility Model Content

[0003] In order to improve the success rate of making specimens simulating debonding defects of coated grains, the utility model provides a specimen simulating debonding defects of coated grains, which uses mechanical punching to simulate the size of the debonding defects, can more accurately simulate the actual debonding defects, and greatly improve the test efficiency and the accuracy of the test results.

[0004] The purpose of the utility model is achieved through the following technical scheme: a test specimen simulating the debonding defect of a coated grain, comprising a grain test block, a coating layer and a sealing screw, the grain test block being provided with a coating arc surface, the coating layer being bonded to the coating arc surface, the coating arc surface being provided with a debonding defect size hole, the bottom of the debonding defect size hole being provided with a threaded hole, the sealing screw being connected to the threaded hole, and a simulated debonding defect gap being left between the end of the rod body of the sealing screw and the coating layer.

[0005] In a preferred embodiment, the distance between the end of the shaft of the sealing screw and the surface of the coating layer is equal to the thickness of the adhesive coating.

[0006] In a preferred embodiment, the diameter of the shaft of the sealing screw matches the diameter of the debonding defect size hole.

[0007] In a preferred embodiment, a sealing ring is provided between the screw head of the sealing screw and the surface of the drug column test block.

[0008] In a preferred embodiment, the drug column test block is made of low carbon steel.

[0009] In a preferred embodiment, a screw segment is provided between the shaft and the screw head of the sealing screw, and the screw segment is connected to the threaded hole.

[0010] In a preferred embodiment, the diameter of the screw segment is greater than the diameter of the shaft.

[0011] In a preferred embodiment, the diameter of the threaded hole is larger than the diameter of the debonding defect size hole.

[0012] Compared with the prior art, the utility model has the following advantages:

[0013] The utility model can simulate debonding defects of different sizes by changing the size of the debonding defect size hole on the drug column test block. The debonding defect size hole can be punched mechanically, and the size accuracy is easier to accurately control. The utility model has a simple and reliable structure. The sample is used in the flaw detection experiment. The test result is consistent with the interface debonding defect of the actual coated drug column, which greatly improves the test efficiency and the authenticity and accuracy of the test result. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of the structure of the utility model;

[0015] Figure 2 It is a schematic diagram of the Chinese medicine column test block of the utility model;

[0016] Figure 3 It is a schematic diagram of the sealing screw in the utility model. DETAILED DESCRIPTION

[0017] The following detailed description of the embodiments of the present invention is further described in detail in conjunction with the accompanying drawings and examples. The detailed description of the following embodiments and the accompanying drawings are used to exemplarily illustrate the principles of the present invention, but cannot be used to limit the scope of the present invention, that is, the present invention is not limited to the preferred embodiments described, and the scope of the present invention is defined by the claims.

[0018] In the description of the present invention, it should be noted that, unless otherwise specified, “plurality” means two or more; the terms “first”, “second”, etc. are used for descriptive purposes only and cannot be understood as indicating or implying relative importance; for ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances.

[0019] Embodiment 1

[0020] See also Figure 1 , Figure 2A sample simulating the debonding defect of a coated grain column provided in this embodiment includes a grain column test block 1, a coating layer 2 and a sealing screw 3. The grain column test block 1 is provided with a coating arc surface 11, the coating layer 2 is bonded to the coating arc surface 11, a debonding defect size hole 12 is provided on the coating arc surface 11, a threaded hole 13 is provided at the bottom of the debonding defect size hole 12, the sealing screw 3 is connected to the threaded hole 13, and a simulated debonding defect gap 4 is left between the end of the rod body 31 of the sealing screw and the coating layer 2.

[0021] See also Figure 3 The sealing screw 3 is composed of a rod body 31, a screw segment 33 and a screw head 32. The screw segment 33 is arranged between the rod body 31 and the screw head 32, and the screw segment 33 is connected to the threaded hole 13. The rod body 31 is a slender polished rod. The diameter of the rod body 31 of the sealing screw 3 matches the aperture of the debonding defect size hole 12, and the diameter of the screw segment 33 matches the aperture of the threaded hole.

[0022] See also Figure 1 , Figure 3 In this embodiment, a sealing ring 6 is provided between the screw head 32 of the sealing screw 3 and the surface of the drug column test block 1. The surface where the screw head 32 contacts the drug column test block 1 is processed with a sealing ring installation groove 7, and the sealing ring 6 is placed in the sealing ring installation groove 7 to seal the debonding defect size hole 12 of the drug column test block 1.

[0023] In this embodiment, the drug column test block 1 is made of low-carbon steel.

[0024] In this embodiment, by changing the inner diameter of the debonding defect size hole 12 and the matching sealing screw 3, debonding defects of different sizes can be simulated.

[0025] See also Figure 1 In this embodiment, the distance between the end of the shaft 31 of the sealing screw 3 and the surface of the coating layer 2 is equal to the thickness of the adhesive coating 5. The simulated debonding defect size and the adhesive coating thickness are determined according to product design requirements.

[0026] See also Figure 3 In this embodiment, the diameter of the screw segment 33 is greater than the diameter of the rod body 31 .

[0027] See also Figure 1 In this embodiment, the diameter of the threaded hole 13 is larger than the diameter of the debonding defect size hole 12 .

[0028] The assembly process of the sample is as follows: first, install the sealing ring 6 into the sealing ring installation groove 7, then assemble the sealing screw 3 with the grain test block 1, and finally use an adhesive to bond the coating layer 2 and the grain test block 1. For composite material components with internal defects, when subjected to external loads, the surface at the location of the internal defects will produce a small non-uniform deformation.

[0029] By building a shear speckle interferometry optical system and supplemented by negative air pressure loading, the sample is placed in a vacuum chamber, and a high-contrast phase fringe pattern can be obtained with a slight change in air pressure. The shear speckle interferometry technology is used as a non-destructive detection method for debonding defects at the interface of coated grains, with outstanding detection capabilities, meeting the requirements of flaw detection in actual engineering.

[0030] The use of shear speckle interferometry methods and systems to identify and detect debonding defects in coated grains belongs to the scope of the prior art and will not be described in detail here. For example, Chinese invention patent application 202210626459.7 discloses a method for identifying the interface defect type of the coating layer of a solid propellant grain.

[0031] The above is only a specific implementation of the utility model, but the protection scope of the utility model is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the utility model, which should be included in the protection scope of the utility model. Therefore, the protection scope of the utility model should be based on the protection scope of the claims.

Claims

1. A sample simulating the debonding defect of a coated drug column, characterized in that: It includes a drug column test block, a coating layer and a sealing screw, the drug column test block is provided with a coating arc surface, the coating layer is bonded to the coating arc surface, the coating arc surface is provided with a debonding defect size hole, the bottom of the debonding defect size hole is provided with a threaded hole, the sealing screw is connected to the threaded hole, and a simulated debonding defect gap is left between the end of the rod body of the sealing screw and the coating layer.

2. A sample simulating debonding defects of a coated grain according to claim 1, characterized in that: The distance between the end of the shaft of the sealing screw and the surface of the coating layer is equal to the thickness of the adhesive coating.

3. A sample simulating debonding defects of a coated grain according to claim 1, characterized in that: The diameter of the rod body of the sealing screw matches the aperture of the debonding defect size hole.

4. A sample simulating debonding defects of a coated grain according to claim 3, characterized in that: A sealing ring is arranged between the screw head of the sealing screw and the surface of the drug column test block.

5. A sample for simulating debonding defects of coated grains according to claim 1, characterized in that: The drug column test block is made of low carbon steel.

6. A sample simulating debonding defects of a coated grain according to claim 1, characterized in that: A screw segment is provided between the rod body and the screw head of the sealing screw, and the screw segment is connected to the threaded hole.

7. A sample for simulating debonding defects of coated grains according to claim 6, characterized in that: The diameter of the screw segment is greater than the diameter of the shaft.

8. A sample for simulating debonding defects of coated grains according to claim 7, characterized in that: The diameter of the threaded hole is larger than the diameter of the debonding defect size hole.