Pole piece and roll core

By arranging recessed paste-reduced areas and full-paste areas on the lithium-ion battery pole pieces, the lithium ion transmission problem caused by the thickness of the pole piece and the powder loss problem caused by laser processing are solved, and the service life and performance of the battery are improved.

CN221841871UActive Publication Date: 2024-10-15ZHUHAI COSMX BATTERY CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202420289418.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-07
Publication Date
2024-10-15
Estimated Expiration
2034-02-07

AI Technical Summary

Technical Problem

The increase in the thickness of the pole pieces of lithium-ion batteries leads to a longer transmission distance of lithium ions, causing lithium ions to accumulate on the surface of the pole pieces and unable to quickly embed into the underlying material, causing lithium precipitation and affecting battery life. In addition, laser hole-making or wire-making solutions cause powder loss. and septal puncture issues.

Method used

Design a pole piece, including a current collector and an active layer. There are concave paste reduction areas and full paste areas on both sides of the active layer. The distance between the paste reduction area and the end side of the active layer is greater than zero, forming an initial bending area to avoid falling off. powder, and improve the lithium precipitation problem by adjusting the relationship between the concave areas.

Benefits of technology

It effectively solves the problems of poor K value of the battery core and puncture of the separator caused by powder falling off in the bending area of ​​the pole piece head, avoids the problem of insufficient adhesion of the active material and broken belts in the hole-making and line-making areas, and improves the battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221841871U_ABST
    Figure CN221841871U_ABST
Patent Text Reader

Abstract

The utility model discloses a pole piece and a roll core, the pole piece comprises a current collector, a first active layer and a second active layer, the first active layer and the second active layer are respectively positioned on two sides of the current collector, the surface of at least one of the first active layer and the second active layer comprises a paste reducing area with a concave part, and the paste reducing area is arranged in the length direction of the pole piece. And the distance between at least one end part side edge of the paste reducing area and the end part side edge of the active layer where the paste reducing area is located is greater than zero. The problems of poor battery cell K value, diaphragm puncture and the like caused by powder falling in the head bending area of the negative plate can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of battery technology, and in particular to a pole piece and a winding core. Background Art

[0002] With the advent of the 5G era and the rapid development of lithium-ion battery technology, people have put forward higher requirements for the energy density, fast charging capability and charge and discharge rate of lithium-ion batteries. High-energy-density fast-charging lithium batteries are also the development trend of consumer lithium-ion batteries. However, with the increase in energy density, the thickness of the positive and negative electrodes of lithium batteries is getting thicker and thicker, and the transmission distance of lithium ions is getting longer and longer. In addition, as the charging speed becomes faster, lithium ions are more likely to gather on the surface of the electrode during the charging and discharging process, causing congestion on the surface of the electrode. Lithium ions cannot be quickly embedded in the underlying material far away from the surface of the electrode and close to the current collector, making it impossible to fully utilize the active material. In addition, the change in potential makes it easy for lithium to be deposited on the surface of the negative electrode in the later stage of the cycle, which seriously affects the service life of the lithium-ion battery.

[0003] At present, researchers usually perform laser hole making or line making on the surface of the negative electrode to solve the lithium plating problem caused by the increasing thickness of the electrode and the increasing distance of lithium ion transmission. However, laser hole making or line making on the surface of the negative electrode will bring new problems. For example, the coating head in the innermost paste folding area near the electrode head and the paste folding area on the radial outside thereof will fall off due to the bending angle of about 180° and the large curvature, which will lead to problems such as poor K value of the battery cell and puncture of the diaphragm. Utility Model Content

[0004] In view of this, the present application provides a pole piece and a winding core, which can solve the problems of poor K value of the battery cell and puncture of the diaphragm caused by powder falling in the bending area of ​​the pole piece head.

[0005] In order to achieve the above application purpose, this application provides the following technical solutions:

[0006] A pole piece comprises a current collector and an active layer, wherein the active layer comprises a first active layer coated on a first side of the current collector, and a second active layer coated on a second side of the current collector; at least one of the first active layer and the second active layer comprises a paste-reducing area having a recessed portion on its surface; in the length direction of the pole piece, the distance between at least one end side edge of the paste-reducing area and the end side edge of the active layer where it is located is greater than zero.

[0007] Optionally, the electrode plate is a negative electrode plate.

[0008] Optionally, in the above-mentioned pole piece, the first active layer includes a first reduced-paste area provided with a recess, and a first full-paste area without a recess and located at an end of the active layer, and a length dimension a of the first full-paste area in the length direction of the pole piece is greater than zero;

[0009] The second active layer includes a second reduced-paste area provided with a recess, and a second full-paste area without a recess and located at an end of the active layer, and a length dimension b of the second full-paste area in the length direction of the negative electrode sheet satisfies a value range of 0<b≤10mm, for example, b=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm;

[0010] The first end side edge of the first active layer is closer to the exposed end of the current collector than the second end side edge of the second active layer.

[0011] Optionally, in the above-mentioned electrode sheet, the length dimension a of the first full paste area in the length direction of the negative electrode sheet satisfies a range of 0<a≤10mm, for example, a=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm;

[0012] Alternatively, the length dimension a of the first full-paste area in the length direction of the negative electrode sheet satisfies a>10mm, for example, a=11mm, 12mm, 13mm......30mm, etc., which is greater than 10mm and is any dimension within the sum of the circumference of the innermost winding layer of the electrode sheet plus the length of part of the second bending zone.

[0013] Optionally, in the above-mentioned electrode sheet, the first active layer further includes a third full-paste area without a recess and located at the other end of the active layer, and the length dimension c of the third full-paste area in the length direction of the negative electrode sheet satisfies a value range of 0<c≤10mm, for example, c=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm;

[0014] The second active layer also includes a fourth full-paste area without a recess and located at the other end of the active layer, and the length dimension c of the fourth full-paste area in the length direction of the negative electrode sheet satisfies the range of 0<c≤10mm, for example, c=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm.

[0015] A winding core, comprising a negative electrode sheet and a positive electrode sheet, wherein the negative electrode sheet is the electrode sheet described above;

[0016] The positive electrode sheet starting end of the positive electrode sheet is located at the straight portion of the winding core;

[0017] The first active layer includes a first initial bending zone located at the inner end of the winding thereof, and also includes a second bending zone located radially outside the first initial bending zone; the first initial bending zone is formed by at least a portion of the first full paste zone, is located on one side of the starting end of the positive electrode sheet, and is closer to the second bending zone than the starting end of the positive electrode sheet;

[0018] The second active layer includes a second initial bending zone located at the inner end of its winding; the second initial bending zone is formed by at least a portion of the second full-paste area, is located on the other side of the starting end of the positive electrode sheet, and extends to the second bending zone.

[0019] Optionally, in the winding core, the first groove of the first paste-reduced area is the first groove, the first groove is adjacent to the first full-paste area, is located on one side of the starting end of the positive electrode sheet, and is located in the straight section of the first active layer closest to the starting end of the positive electrode sheet;

[0020] The first groove of the second reduced-paste area is the second groove, which is adjacent to the second full-paste area, located on the other side of the starting end of the positive electrode sheet, and located in the straight section of the second active layer closest to the starting end of the positive electrode sheet.

[0021] Optionally, in the winding core, along the winding direction, the first groove of the first reduced-paste area is the first groove, and the first groove is adjacent to the first full-paste area;

[0022] Along the winding direction, the first groove of the second reduced-paste area is the second groove, and the second groove is adjacent to the second full-paste area;

[0023] The first groove and the second groove are located in the same straight section of the negative electrode sheet.

[0024] Optionally, in the above winding core, the first groove of the first paste-reduced area is the first groove, the first groove is adjacent to the first full-paste area, and is located in the second bending area;

[0025] The first groove of the second reduced-paste area is the second groove, which is adjacent to the second full-paste area and is located in the straight section of the second active layer closest to the starting end of the positive electrode sheet.

[0026] Optionally, in the winding core, the first groove and the second groove overlap each other in the thickness direction of the pole piece where they are located;

[0027] Alternatively, the first groove is closer to the second bending area than the second groove;

[0028] Alternatively, the first groove is further away from the second bending zone than the second groove.

[0029] Optionally, in the above-mentioned winding core, the distance J between the projection centers of the first groove and the second groove on the negative electrode current collector between the two satisfies 0≤J≤(1~3.5)D / 2, or satisfies 0<J≤(1~3.5)(10~20)B / 2; D is the spacing between adjacent line grooves in the first paste-reducing area; B is the spacing between adjacent hole grooves in the first paste-reducing area.

[0030] Optionally, in the winding core, the projection of the starting end of the positive electrode sheet on the first active layer is located in the first paste-reducing area;

[0031] And / or, the projection of the starting end of the positive electrode sheet on the second active layer is located in the second paste-reducing area;

[0032] And / or, the starting end of the positive electrode sheet is closer to the second bending area than the first paste-reducing area, and the length dimension H thereof exceeding the first paste-reducing area satisfies 0<H≤(1~3.5)D or 0<H≤(1~3.5)(10~20)B;

[0033] And / or, the starting end of the positive electrode sheet is closer to the second bending area than the second paste-reducing area, and the length dimension H thereof exceeding the second paste-reducing area satisfies 0<H≤(1~3.5)D or 0<H≤(1~3.5)(10~20)B;

[0034] Wherein, D is the distance between adjacent line slots in the first paste-reducing area, and B is the distance between adjacent hole slots in the first paste-reducing area.

[0035] Optionally, in the above-mentioned winding core, in the single-sided area of ​​the negative electrode sheet, the thickness of the first active layer is M; in the double-sided area of ​​the negative electrode sheet, the thicknesses of the first active layer and the second active layer are N respectively, M=(0.8~1.15)N; at least part of the first full paste area is located in the single-sided area.

[0036] Optionally, in the above winding core, the first active layer includes a third full-paste area, the third full-paste area is located at the tail end of the first active layer, has a flat surface, and a length dimension c in the length direction of the negative electrode sheet satisfies a value range of 0<c≤10mm, for example, c=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm;

[0037] The second active layer includes a fourth full-paste area, the fourth full-paste area is located at the tail end of the second active layer, has a flat surface, and a length dimension c in the length direction of the negative electrode sheet satisfies a value range of 0<c≤10mm, for example, c=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm;

[0038] The first protective adhesive tape and the second protective adhesive tape which are bonded to the positive electrode sheet are respectively arranged on both sides of the tail end of the negative electrode sheet, wherein:

[0039] The projection of the inner end of the first protective adhesive tape on the tail straight section of the negative electrode sheet is located in the third full paste area; the projection of the inner end of the second protective adhesive tape on the tail straight section of the negative electrode sheet is located in the fourth full paste area;

[0040] Alternatively, the projected overlapping length L1 of the first protective tape and the first paste-reducing area in the direction of the core thickness satisfies 0≤L1≤(1~3.5)D, or satisfies 0≤L1≤(1~3.5)(10~20)B; the projected overlapping length L2 of the second protective tape and the second paste-reducing area in the direction of the core thickness satisfies 0≤L2≤(1~3.5)D, or satisfies 0≤L2≤(1~3.5)(10~20)B; D is the spacing between adjacent line grooves in the first paste-reducing area; B is the spacing between adjacent hole grooves in the first paste-reducing area.

[0041] Compared with the prior art, in the negative electrode sheet and winding core provided by the present application, since the distance between at least one end side of the reduced paste area and the end side of the active layer in the length direction of the electrode sheet is greater than zero, the end area in the active layer on both sides of the electrode sheet for forming the first initial bending area and / or the second initial bending area is a full paste area where no hole making and line making are performed, and the full paste area will not produce powder loss during winding and bending, thereby being able to solve the problems of poor K value of the battery cell and puncture of the diaphragm caused by powder loss in the bending area of ​​the head of the negative electrode sheet. In addition, since the above-mentioned full paste area is located at the end of the electrode sheet and maintains a length distance greater than zero, the reduced paste area adjacent to the full paste area is located in the straight part or other bending part with a smaller curvature of the winding core. Therefore, although the active material adhesion at the hole making and line making part is slightly poor, it is not easy to cause powder loss due to folding and bending. In addition, the above-mentioned full paste area can avoid the problem that the hole making and line making area is too close to the empty foil material and the belt is broken due to stress problems and cannot be mass-produced. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0043] Figure 1 The figure is a schematic diagram of the structure of a winding core.

[0044] Figure 2 This is a schematic diagram of the structure of a negative electrode sheet provided in the first specific embodiment of the present application.

[0045] Figure 3 for Figure 2 A magnified view of a local area.

[0046] Figure 4 This is a schematic diagram of the structure of a negative electrode sheet provided in the second specific embodiment of the present application.

[0047] Figures 5 to 7 Schematic diagram of the internal winding structure of three different types of winding cores provided in the second specific embodiment of the present application.

[0048] Figure 8 and Fig. 9 Schematic diagram of two different adhesive tape pasting structures provided for this application.

[0049] in:

[0050] 1- negative electrode, 2- positive electrode,

[0051] 10-current collector, 11-first active layer, 12-second active layer,

[0052] 20- positive electrode head, 21- positive electrode tail straight section,

[0053] 31-first protective tape, 32-second protective tape,

[0054] 100-exposed end of the negative electrode current collector,

[0055] 110 - first end side, 111 - first initial bending zone, 112 - second bending zone,

[0056] 113-The straight section at the tail of the negative electrode sheet,

[0057] 120 - second end side, 121 - second initial bending area,

[0058] 1101-the first full cream area, 1102-the first reduced cream area,

[0059] 1103-third full paste area, 11C1-first groove,

[0060] 1201-the second full cream area, 1202-the second reduced cream area,

[0061] 1203-the fourth full paste area, 12C1-the second groove. DETAILED DESCRIPTION

[0062] First of all, it should be noted that:

[0063] The "full paste area" mentioned in this article refers to the partial area on the surface of the paste layer (i.e., the active material layer, referred to as the active layer) coated on the side of the current collector where no holes or lines are made, that is, no slots or holes are opened in the partial area on the surface of the active layer, or there are no slots or holes, thereby basically retaining all the active materials after the paste is applied. It should also be noted that the "full paste area" and "no slots and holes" mentioned in this article mean that after the paste layer is coated on the side of the current collector, no holes or lines are made on the surface of the paste layer. It does not include the grooves, holes, and concave structures of the line lamp formed by the uneven surface of the paste layer due to reasons such as material particle size, electrode flatness, and changes in paste layer thickness after the coating of the paste layer is completed, nor does it include microscopic concave structures.

[0064] The "paste reduction area" mentioned in this article refers to the formation of a recess (for example, a concave structure formed by making holes or lines, etc.) in a partial surface area of ​​the active layer after the active material is coated on the side of the current collector to form an active layer in order to solve the lithium plating problem caused by the increasing thickness of the electrode and the longer lithium ion transmission distance. This reduces the amount of paste in this area (i.e., the amount of coated active material), so it is called the paste reduction area.

[0065] The "wound layer" mentioned in this article refers to a layer of structure formed by winding a circle of the pole piece. For example, see Figure 1 During the winding process, the negative electrode sheet is wound from point p1 to point p2 along the direction of the arrow to form the innermost winding layer of the negative electrode sheet; continuing to wind one circle forms the second winding layer.

[0066] The "starting end" and "head" mentioned in this article refer to the pole piece end or active layer end that is first wound and located at the innermost side of the core when the pole piece is wound into a core structure; the "tail", "tail end" and "closing end" mentioned in this article refer to the side end located at the outermost side of the core when the pole piece is wound into a core structure.

[0067] The "first groove" mentioned in this article refers to the groove located at the sidemost side of the paste reduction area in the length direction of the pole piece, which is also the groove on the innermost side of the winding core in the paste reduction area, and is adjacent to the full paste area of ​​the active layer where it is located.

[0068] The "single-sided area" mentioned in this article refers to the area in the pole piece where the active layer is arranged only on one side of the current collector; the "double-sided area" refers to the area in the pole piece where the active layer is arranged on both sides of the current collector; and the "empty foil area" refers to the current collector area in the pole piece where no active layer is arranged.

[0069] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0070] See also Figure 1 In a winding core of a wound lithium-ion battery structure, the winding starting position of the negative electrode sheet is the empty foil area at the head of the negative electrode sheet, and the area of ​​the first bend is located in the negative electrode single-sided coating area (referred to as the single-sided area); in order to balance the thickness difference caused by the positive electrode paste withdrawal at the starting end of the winding (lithium battery design principle, the negative electrode effective paste should cover the positive electrode effective paste, in some products, the positive electrode needs to be withdrawn, and then there will be one fold less of the positive electrode paste thickness at the position of the paste withdrawal. At this time, there is a thickness difference at this position, which needs to be balanced by folding the paste at the head of the negative electrode), the negative electrode sheet needs to be compensated for the thickness difference by folding the paste at the starting end of the winding. For details, please refer to Figure 1 If the head area of ​​the negative electrode paste is provided with a concave portion (e.g., a hole / groove / line, or a concave structure provided for other purposes, which is not shown in the figure), the first paste folding area of ​​the first active layer 11 located on the first side of the negative electrode sheet in the inner circle of the negative electrode sheet winding (see Figure 1 The first paste region 111' in the negative electrode sheet is generally the head region of the first active layer 11), and the first paste region of the second active layer 12 located on the second side of the negative electrode sheet (see Figure 1 The second folded paste area 121' (generally the head area of ​​the second active layer 11) is prone to powdering, which may lead to poor K value of the battery cell, puncture of the diaphragm and other problems.

[0071] In order to solve the above problems, the present application provides a pole piece and a winding core, which can solve the above lithium plating problem by setting a recess on the pole piece surface, and can also effectively improve the above problems by adjusting the relationship between the area where the recess is located and the pole piece paste folding area.

[0072] First specific embodiment

[0073] See also Figure 2 and Figure 3The first specific embodiment of the present application provides a negative electrode sheet and a winding core, wherein the paste layer head regions on both sides of the negative electrode sheet (i.e., the first full paste region 1101 and the second full paste region 1201) are both full paste regions, which are respectively located in the winding core and on both sides of the positive electrode sheet head 20, forming Figure 3 The first initial bending area 111 and the second initial bending area 121 in the embodiment. Since the first full paste area 1101 and the second full paste area 1201 are not subjected to hole making and line making, the problems of poor K value of the battery cell and puncture of the diaphragm caused by powder falling in the bending area of ​​the head of the negative electrode sheet can be solved.

[0074] Specifically, see Figure 2 The negative electrode sheet includes a current collector 10 and an active layer, wherein the active layer includes a first active layer 11 coated on a first side of the current collector 10, and a second active layer 12 coated on a second side of the current collector 10. The first active layer 11 includes a first full paste area 1101 starting from its starting end and having no slot structure, and a first reduced paste area 1102 connected to the first full paste area 1101 and having a slot structure; the second active layer 12 includes a second full paste area 1201 starting from its starting end and having no slot structure, and a second reduced paste area 1202 connected to the second full paste area 1201 and having a slot structure.

[0075] Specifically, the first full paste area 1101 is located at one end of the first active layer 11, and its surface is flat. The length dimension a in the length direction of the negative electrode sheet satisfies the range of 0<a≤10mm, for example, a=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm. In specific implementation, a is actually greater than or equal to the side arc length of the bend of the innermost coil layer of the winding core (i.e., the first paste folding area of ​​the negative electrode sheet) to ensure Figure 2 The first full paste area 1101 can be bent to form at least Figure 3 The first initial bending area 111 in the middle; the first reduced paste area 1102 is connected to the other end of the first full paste area 1101, extends along the length direction of the negative electrode sheet, and is provided with a slot structure. The slot structure refers to the hole making / line making mentioned above for solving the problem of lithium deposition caused by the increasing thickness of the electrode sheet and the increasing distance of lithium ion transmission. It can be specifically obtained by laser processing or other methods.

[0076] Specifically, the second full paste area 1201 is located at one end of the second active layer 12, and its surface is flat. The length dimension b in the length direction of the negative electrode sheet satisfies the range of 0<b≤10mm, for example, b=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm. In specific implementation, b is generally greater than the distance between the two sides of adjacent slots (i.e., the distance between adjacent lines or the distance between adjacent holes), and is less than the side arc length of the bending portion of the second circle layer of the negative electrode sheet on the inner side of the winding core (i.e., Figure 3 The arc length of the second bending zone 112 in the middle) is to ensure Figure 2 The second full paste area 1201 in the positive electrode sheet can at least protrude outward relative to the positive electrode sheet end 20 and bend to extend a distance, thereby forming Figure 3 The second initial bending area 121 in the negative electrode is connected to the second paste-reduced area 1202, which is connected to the other end of the second full paste area 1201, extends along the length direction of the negative electrode sheet, and is provided with a slot structure, which refers to the hole-making / line-making mentioned above in order to solve the problem of lithium deposition caused by the increasing thickness of the electrode sheet and the increasing lithium ion transmission distance, and can be specifically manufactured by laser or other processing methods;

[0077] exist Figure 2 In the negative electrode sheet 1 shown in FIG. 1 , the first end side edge 110 of the first active layer 11 is closer to the head (i.e., the empty foil area at the head of the negative electrode sheet) of the exposed current collector of the negative electrode sheet 1 than the second end side edge 120 of the second active layer 12. Figure 2 The current collector exposed end 100). Figure 2 and Figure 4 a+d>zero. Therefore, the second end side edge 120 is the boundary position between the single-sided area and the double-sided area of ​​the negative electrode sheet 1. Figure 2 As shown in , the first initial bending area 111 , most of the second bending area 112 , and the connecting area therebetween constitute a single-sided area of ​​the negative electrode sheet 1 .

[0078] like Figures 2 to 3As shown in , the range of a and b is between 0 and 10 mm, and no holes or wires are made in this area. The first initial bending area 111 is within the range shown by the length a of the first full paste area 1101, and the second initial bending area 121 is within the range shown by the length b of the second full paste area 1201. The two will not produce powder loss when winding and bending. In addition, the first paste-reduced area 1102 in the first active layer 11 and the second paste-reduced area 1202 in the second active layer 12 are both located in the straight part of the winding core or other bending parts with smaller curvature. Therefore, although the active material adhesion at the hole-making and wire-making parts is slightly poor, it is not easy to cause powder loss due to folding and bending. In addition, through the above-mentioned first full paste area 1101 and the second full paste area 1201, it is possible to avoid the problem that the hole-making and wire-making areas are too close to the empty foil material and the belt is broken due to stress problems and cannot be mass-produced, which also affects the performance of the battery.

[0079] See also Figure 2 The cross-sectional view of the negative electrode sheet shown in the figure, in some embodiments, the first active layer 11 of the negative electrode sheet further includes a third full paste area 1103, the third full paste area 1103 is located at the other end of the first active layer 11, has a flat surface without concave parts, and the length dimension c in the length direction of the negative electrode sheet satisfies 0<c≤10mm, for example, c=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm; the second active layer 12 further includes a fourth full paste area 1203, the fourth full paste area 1203 is located at the other end of the second active layer 12, has a flat surface without concave parts, and the length dimension c in the length direction of the negative electrode sheet satisfies 0<c≤10mm. In short, the paste coating on both sides of the tail of the negative electrode sheet (within a maximum length of 10mm) does not make holes and wires, so as to avoid the problem that the holes and wire making areas are too close to the empty foil material, and the broken tape cannot be mass-produced due to stress problems.

[0080] The winding core provided in the first specific embodiment of the present application includes a negative electrode sheet 1 and a positive electrode sheet 2, and the negative electrode sheet is the negative electrode sheet mentioned above. Moreover, the negative electrode sheet 1 includes a single-sided paste area (referred to as the single-sided area) near the starting end of the winding of the negative electrode sheet, and a double-sided paste area (referred to as the double-sided area) connected to the single-sided area. The head area of ​​the first active layer 11 located on the first side of the current collector 10 forms the above-mentioned single-sided area, and the remaining area and the second active layer 12 located on the second side of the current collector 10 form the above-mentioned double-sided area.

[0081] In some embodiments, the positive electrode sheet starting end 20 of the positive electrode sheet 2 is located at the straight part of the winding core, and the first initial bending area 111 and the second initial bending area 121 are respectively located on both sides of the positive electrode sheet starting end 20, and form the internal structure of the winding core where the positive electrode head is de-pasted and the negative electrode head is folded. Figure 3 :

[0082] The first active layer 11 includes a first initial bending area 111 located at the inner end of the winding thereof, and also includes a second bending area 112 located radially outside the first initial bending area 111, the first initial bending area 111 is formed by at least a part of the first full paste area 1101 (that is, the first initial bending area 111 is a part of the first full paste area 1101 or is formed by bending the entire first full paste area), and is located on one side of the positive electrode sheet starting end 20, and is closer to the second bending area 112 relative to the positive electrode sheet starting end 20;

[0083] The second active layer 12 includes a second initial bending zone 121 located at the inner end of its winding; the second initial bending zone 121 is formed by at least a portion of the second full paste zone 1201 (that is, the second initial bending zone 121 is a portion of the second full paste zone 1201 or is formed by bending the entire second full paste zone), is located on the other side of the starting end 20 of the positive electrode sheet, and extends to the second bending zone 112.

[0084] In some embodiments, the first groove of the first paste reducing area 1102 and the first groove of the second paste reducing area 1202 are both located in the plane area of ​​the core. This is also to avoid the problem of powder falling caused by the folding at nearly 360° at this position.

[0085] See also Figure 3 In some embodiments, the first groove of the first reduced-paste area 1102 located on the first side of the negative electrode sheet is the first groove 11C1, the first groove 11C1 is adjacent to the first full-paste area 1101, is located on one side of the starting end 20 of the positive electrode sheet, and is located in the straight section of the first active layer 11 closest to the starting end 20 of the positive electrode sheet, and is also the straight section of the innermost winding layer of the negative electrode sheet 1; the first groove of the second reduced-paste area 1202 located on the second side of the negative electrode sheet is the second groove 12C1, the second groove 12C1 is adjacent to the second full-paste area 1201, is located on the other side of the starting end 20 of the positive electrode sheet, and is located in the straight section of the second active layer 12 closest to the starting end 20 of the positive electrode sheet, and is also the straight section of the second winding layer of the negative electrode sheet 1 counted from the inside to the outside that is closest to the starting end 20 of the positive electrode sheet.

[0086] In some embodiments, the projection of the positive electrode starting end 20 on the first active layer 11 is located in the first paste-reduced area 1102; and / or, the projection of the positive electrode starting end 20 on the second active layer 12 is located in the second paste-reduced area 1202. This can improve the lithium plating problem caused by the thick electrode not forming holes and lines.

[0087] Alternatively, in other specific embodiments, the positive electrode sheet starting end 20 may be closer to the second bending area 112 relative to the first paste-reducing area 1102, and the length dimension H of the positive electrode sheet starting end 20 beyond the first paste-reducing area 1102 may satisfy 0<H≤(1~3.5)D or 0<H≤(1~3.5)(10~20)B; and / or, the positive electrode sheet starting end 20 may be closer to the second bending area 112 relative to the second paste-reducing area 1202, and the length dimension H of the positive electrode sheet beyond the second paste-reducing area 1202 may satisfy 0<H≤(1~3.5)D or 0<H≤(1~3.5)(10~20)B. Wherein, D is the spacing between adjacent line grooves (i.e., line making) in the first paste-reducing area 1102, and B is the spacing between adjacent hole grooves (i.e., hole making) in the first paste-reducing area 1102, and D=(10~20)B. It can also improve the lithium plating problem caused by not making holes and lines in thick electrodes.

[0088] Considering that the paste and the empty foil are prone to breakage at the end of the negative electrode during mass production, mass production is not possible. Therefore, no holes or wires are made in the tail end of the first active layer 11, and no holes or wires are made in the tail end of the second active layer 12. The length range c of the area without holes or wires is less than 10 mm. After the positive and negative electrode sheets are stacked to form a winding core, the end projection of the protective tape at the end of the positive electrode needs to fall on the hole and wire making area of ​​the negative electrode sheet (see Fig. 9 ), or not in this area (see Figure 8 ). This can improve the lithium plating problem caused by not making holes and lines in thick electrodes.

[0089] For details, please see Figure 1 , Figure 2 , Figure 8 and Fig. 9 In the winding core provided in the embodiment of the present application: the first active layer 11 includes a third full-paste area 1103, the third full-paste area 1103 is located at the tail end of the first active layer 11, the surface is flat, and the length dimension c in the length direction of the negative electrode sheet satisfies 0<c≤10mm, for example, c=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm; the second active layer 12 includes a fourth full-paste area 1203, the fourth full-paste area 1203 is located at the tail end of the second active layer 12, the surface is flat, and the length dimension c in the length direction of the negative electrode sheet satisfies 0<c≤10mm, for example, c=1mm or 2mm or 3mm or 4mm or 5mm or 6mm or 7mm or 8mm or 9mm or 10mm, or any non-integer between 0 and 10mm. Moreover, a first protective adhesive tape 31 and a second protective adhesive tape 32 which are bonded to the negative electrode sheet 1 are respectively disposed on both sides of the tail end of the positive electrode sheet 2 .

[0090] Among them, Figure 8 As shown, the projection of the inner end of the first protective tape 31 on the tail straight section 21 of the positive electrode sheet 2 is located in the third full paste area 1103; the projection of the inner end of the second protective tape 32 on the tail straight section 21 of the positive electrode sheet 2 is located in the fourth full paste area 1203.

[0091] Alternatively, you can Fig. 9 As shown in , the projection of the inner end of the first protective tape 31 on the tail straight section 21 of the positive electrode sheet 2 is located in the first paste reduction area 1102, that is, the overlapping length L1 of the projection of the first protective tape 31 and the first paste reduction area 1102 in the thickness direction of the winding core satisfies 0≤L1≤(1~3.5)D, or satisfies 0≤L1≤(1~3.5)(10~20)B; the projection of the inner end of the second protective tape 32 on the tail straight section 21 of the positive electrode sheet 2 is located in the second paste reduction area 1202, that is, the overlapping length L2 of the projection of the second protective tape 32 and the second paste reduction area 1202 in the thickness direction of the winding core satisfies 0≤L2≤(1~3.5)D, or satisfies 0≤L2≤(1~3.5)(10~20)B. Wherein, D is the spacing between adjacent line grooves in the first paste reduction area 1102; B is the spacing between adjacent hole grooves in the first paste reduction area 1102.

[0092] Second specific embodiment

[0093] The second specific embodiment of the present application provides a negative electrode sheet and winding core, which differs from the first specific embodiment mentioned above only in that the length dimension a of the first full paste area 1101 in the negative electrode sheet 1 in the length direction of the negative electrode sheet satisfies a>10mm, for example, a=11mm, 12mm, 13mm......30mm, etc., which is greater than 10mm and satisfies any dimension within the range of the sum of the circumference of the innermost winding layer of the electrode sheet plus the length of part of the second bending area 112. For details, please refer to Figure 4 .

[0094] At this time, in some embodiments, such as Figure 5 and Figure 6 As shown, in the winding core, the first groove of the first paste-reduced area 1102 located on the first side of the negative electrode sheet is the first groove 11C1, and the first groove 11C1 is adjacent to the first full paste area 1101; the first groove of the second paste-reduced area 1202 located on the second side of the negative electrode sheet is the second groove 12C1, and the second groove 12C1 is adjacent to the second full paste area 1201; the first groove 11C1 and the second groove 12C1 are both located in the double-sided area, and are both located in the straight section closest to the starting end 20 of the positive electrode sheet in the second winding layer from the inside to the outside of the negative electrode sheet 1. Among them, the first groove 11C1 can be closer to the second bending area 112 ( Figure 6 ); or, the first groove 11C1 may be further away from the second bending region 112 relative to the second groove 12C1 ( Figure 5 ).

[0095] Specifically, in some embodiments, the distance J between the projection centers of the first groove 11C1 and the second groove 12C1 on the current collector 10 between the two satisfies 0≤J≤1~3.5D / 2, or satisfies 0<J≤1~3.5(10~20)B / 2. Wherein, D is the spacing between adjacent line grooves (i.e., line formation) in the first paste-reducing area 1102, B is the spacing between adjacent hole grooves (i.e., hole formation) in the first paste-reducing area 1102, and D=(10~20)B.

[0096] Alternatively, in other embodiments, the first groove 11C1 may be located in the single-surface area and at any position of the second bending area 112. Figure 7 As shown: the first groove of the first paste-reduced area 1102 located on the first side of the negative electrode sheet is the first groove 11C1, which is adjacent to the first full paste area 1101 and located in the second bending area 112; the first groove of the second paste-reduced area 1202 located on the second side of the negative electrode sheet is the second groove 12C1, which is adjacent to the second full paste area 1201 and located in the straight section closest to the starting end 20 of the positive electrode sheet in the second active layer 12, and is also the straight section closest to the starting end 20 of the positive electrode sheet in the second winding layer of the negative electrode sheet 1 from the inside to the outside. Its main effect is to avoid the problem of lithium deposition caused by overpressure at the intersection of the single and double sides.

[0097] In some embodiments, no holes or lines are made in the single-sided area of ​​the negative electrode sheet, which can be understood as an upgraded version of the first specific embodiment. Because of the changes in the single and double-sided areas of the negative electrode sheet during the production process, the compaction of the single-sided area is often smaller than that of the double-sided area, and its porosity is higher than that of the double-sided area. In order to more intuitively express the difference in compaction between the two, that is, the difference in porosity, it can be expressed by the difference in the thickness of the paste between the two. For example, assuming that the thickness of the first active layer 11 in the single-sided area of ​​the negative electrode sheet 1 is M, and the thickness of the first active layer 11 and the second active layer 12 in the double-sided area of ​​the negative electrode sheet 1 are N respectively, then M=(0.8~1.15)N. At this time, at least part of the first full paste area 1101 is located in the single-sided area. Moreover, when the above relationship is satisfied, it is possible to not make holes or lines in the single-sided area.

[0098] Finally, it should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device that includes a series of elements includes not only those elements, but also other elements not explicitly listed.

[0099] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0100] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A pole piece, characterized in that: It comprises a current collector (10) and an active layer, wherein the active layer comprises a first active layer (11) on a first side of the current collector (10), and a second active layer (12) on a second side of the current collector (10); At least one of the first active layer (11) and the second active layer (12) comprises a paste-reducing area with a concave portion provided on the surface; In the length direction of the pole piece, the distance between at least one end side edge of the paste reduction area and the end side edge of the active layer where the area is located is greater than zero.

2. The pole piece according to claim 1, characterized in that: The electrode sheet is a negative electrode sheet.

3. The pole piece according to claim 2, characterized in that: The first active layer (11) comprises a first reduced-paste area (1102) provided with a recess, and a first full-paste area (1101) without a recess and located at an end of the active layer, wherein a length dimension a of the first full-paste area (1101) in the length direction of the pole piece is greater than zero; The second active layer (12) comprises a second reduced-paste area (1202) provided with a recess, and a second full-paste area (1201) without a recess and located at an end of the active layer, wherein a length dimension b of the second full-paste area (1201) in the length direction of the pole piece satisfies a value range of 0<b≤10 mm; The first end side edge (110) of the first active layer (11) is closer to the exposed end (100) of the current collector (10) than the second end side edge (120) of the second active layer (12).

4. The pole piece according to claim 3, characterized in that: The value range of the length dimension a of the first full paste area (1101) in the length direction of the electrode sheet satisfies 0<a≤10mm; Alternatively, the length dimension a of the first full-paste area (1101) in the length direction of the pole piece satisfies a>10mm.

5. The pole piece according to claim 2, characterized in that: The first active layer (11) further comprises a third full-paste area (1103) without a recess and located at the other end of the active layer, and the length dimension c of the third full-paste area (1103) in the length direction of the pole piece satisfies a value range of 0<c≤10mm; The second active layer (12) further comprises a fourth full-paste area (1203) without a recess and located at the other end of the active layer, and the length dimension c of the fourth full-paste area (1203) in the length direction of the pole piece has a value range of 0<c≤10mm.

6. A winding core, comprising a negative electrode sheet (1) and a positive electrode sheet (2), characterized in that: The negative electrode sheet is the electrode sheet according to claim 3; The positive electrode sheet starting end (20) of the positive electrode sheet (2) is located at the straight portion of the winding core; The first active layer (11) comprises a first initial bending zone (111) located at the inner end of the winding thereof, and further comprises a second bending zone (112) located radially outside the first initial bending zone (111); the first initial bending zone (111) is located in the first full paste zone (1101); The second active layer (12) comprises a second initial bending zone (121) located at the inner end of the winding thereof; the second initial bending zone (121) is located in the second full paste zone (1201).

7. The winding core according to claim 6, characterized in that: The first groove of the first reduced-paste area (1102) is the first groove (11C1), the first groove (11C1) is adjacent to the first full-paste area (1101), is located on one side of the positive electrode sheet starting end (20), and is located in the straight section of the first active layer (11) closest to the positive electrode sheet starting end (20); The first groove of the second reduced-paste area (1202) is the second groove (12C1), which is adjacent to the second full-paste area (1201), located on the other side of the starting end (20) of the positive electrode sheet, and located in the straight section of the second active layer (12) closest to the starting end (20) of the positive electrode sheet.

8. The winding core according to claim 6, characterized in that: Along the winding direction, the first groove of the first reduced-paste area (1102) is the first groove (11C1), and the first groove (11C1) is adjacent to the first full-paste area (1101); Along the winding direction, the first groove of the second reduced-paste area (1202) is the second groove (12C1), and the second groove (12C1) is adjacent to the second full-paste area (1201); The first groove (11C1) and the second groove (12C1) are located in the same straight section of the negative electrode sheet (1).

9. The winding core according to claim 6, characterized in that: The first groove of the first reduced-paste area (1102) is the first groove (11C1), the first groove (11C1) is adjacent to the first full-paste area (1101), and is located in the second bending area (112); The first groove of the second reduced-paste area (1202) is the second groove (12C1), the second groove (12C1) is adjacent to the second full-paste area (1201), and is located in the straight section of the second active layer (12) closest to the starting end (20) of the positive electrode sheet.

10. The winding core according to claim 8, characterized in that: The first groove (11C1) and the second groove (12C1) overlap each other in the thickness direction of the pole piece where they are located; Alternatively, the first groove (11C1) is closer to the second bending area (112) than the second groove (12C1); Alternatively, the first groove (11C1) is further away from the second bending area (112) than the second groove (12C1).

11. The winding core according to claim 10, characterized in that: The value range of the distance J between the projection centers of the first groove (11C1) and the second groove (12C1) on the current collector (10) between the two satisfies 0≤J≤(1-3.5)D / 2, or satisfies 0<J≤(1-3.5)(10-20)B / 2; D is the distance between adjacent wire slots in the first paste reduction area (1102); B is the distance between adjacent holes and grooves in the first paste-reducing area (1102).

12. The winding core according to claim 6, characterized in that: The projection of the starting end (20) of the positive electrode sheet on the first active layer (11) is located in the first paste-reducing area (1102); And / or, the projection of the starting end (20) of the positive electrode sheet on the second active layer (12) is located in the second paste-reducing area (1202); And / or, the starting end (20) of the positive electrode sheet is closer to the second bending area (112) than the first paste-reducing area (1102), and the value range of its length dimension H exceeding the first paste-reducing area (1102) satisfies 0<H≤(1~3.5)D or 0<H≤(1~3.5)(10~20)B; And / or, the starting end (20) of the positive electrode sheet is closer to the second bending area (112) than the second paste-reduced area (1202), and the value range of its length dimension H exceeding the second paste-reduced area (1202) satisfies 0<H≤(1~3.5)D or 0<H≤(1~3.5)(10~20)B; Wherein, D is the distance between adjacent line grooves in the first paste-reducing area (1102), and B is the distance between adjacent hole grooves in the first paste-reducing area (1102).

13. The winding core according to claim 6, characterized in that: In a single-side region of the negative electrode sheet (1), the thickness of the first active layer (11) is M; In the double-sided area of ​​the negative electrode sheet (1), the thickness of the first active layer (11) and the thickness of the second active layer (12) are respectively N; M = (0.8-1.15) N; At least part of the first full-paste area (1101) is located in the single-sided area.

14. The winding core according to claim 6, characterized in that: The first active layer (11) comprises a third full-paste area (1103), the third full-paste area (1103) is located at the tail end of the first active layer (11), has a flat surface, and has a length dimension c in the length direction of the negative electrode sheet in the range of 0<c≤10 mm; The second active layer (12) comprises a fourth full-paste area (1203), the fourth full-paste area (1203) is located at the tail end of the second active layer (12), has a flat surface, and has a length dimension c in the length direction of the negative electrode sheet in the range of 0<c≤10 mm; A first protective adhesive tape (31) and a second protective adhesive tape (32) are respectively provided on both sides of the tail end of the negative electrode sheet (1) and are bonded to the positive electrode sheet (2), wherein: The projection of the inner end of the first protective adhesive tape (31) on the tail straight section (113) of the negative electrode sheet (1) is located in the third full-paste area (1103); the projection of the inner end of the second protective adhesive tape (32) on the tail straight section (113) of the negative electrode sheet (1) is located in the fourth full-paste area (1203); Alternatively, a projected overlapping length L1 between the first protective tape (31) and the first paste-reducing area (1102) in the direction of the core thickness satisfies 0≤L1≤(1~3.5)D, or satisfies 0≤L1≤(1~3.5)(10~20)B; a projected overlapping length L2 between the second protective tape (32) and the second paste-reducing area (1202) in the direction of the core thickness satisfies 0≤L2≤(1~3.5)D, or satisfies 0≤L2≤(1~3.5)(10~20)B; D is the spacing between adjacent line grooves in the first paste-reducing area (1102); and B is the spacing between adjacent hole grooves in the first paste-reducing area (1102).

Citation Information

Cited By

  • Electrode assembly and battery

    CN119230731A

  • Pole piece and diaphragm compounding device, compounding method and compounding unit

    CN121790692A