Band saw blade

By arranging the first chamfering part and the second chamfering part on the tooth top of the band saw blade to form a two-level inclined shape, the problem of easy peeling of the hard film on the tooth top is solved, and the strength of the hard film and the tooth top is improved. Film peeling and chipping are suppressed, and processing efficiency and tool wear resistance are improved.

CN221848853UActive Publication Date: 2024-10-18AMADA CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202290000813.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Priority Date
2022-11-14
Filing Date
2022-11-30
Publication Date
2024-10-18
Estimated Expiration
2032-11-30

AI Technical Summary

Technical Problem

The hard coating of existing cutting tools is easy to peel off at the tooth top, especially the band saw blade due to its low rigidity, which easily causes cutting bending and heavy load, resulting in a tendency for the film to peel off and affecting processing efficiency.

Method used

A first chamfer and a second chamfer are provided on the tooth top of the band saw blade to form a two-level inclined shape, which increases the close contact area between the hard coating and the tooth top. By improving the tooth top shape, the hard coating and the tooth top are improved. strength, inhibiting film peeling.

Benefits of technology

By improving the strength of the hard coating and the tooth tip, the peeling and chipping of the hard coating is effectively suppressed, and the processing efficiency and tool wear resistance are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221848853U_ABST
    Figure CN221848853U_ABST
Patent Text Reader

Abstract

The band saw blade (100) is repeatedly provided with a saw tooth group (10) formed by combining more than one saw tooth (20, 40) on a band-shaped main body part (1). The saw teeth (20, 40) are provided with tooth tops (30, 50) provided with hard coatings. A tooth top portion (50) of a saw tooth (40) forming a cut surface includes: a first chamfered portion (55) provided at a first corner portion where a rake face (51) located at a front side in a travel direction (F1) and a flank face (52) located at a rear side in the travel direction (F1) intersect; and a second chamfered portion (56) provided at a second corner portion where a pair of side surfaces (53) spaced apart from each other in the belt thickness direction (F2) intersects with the flank surface (52). The size of the second chamfered portion (56) in the width direction (F3) is larger than the size of the first chamfered portion (55) in the width direction (F3).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a band saw blade. Background Art

[0002] In recent years, high-speed and high-efficiency machining is required, and there is a tendency to target heat-resistant steel and dry cutting. In order to improve the wear resistance of cutting tools, cutting tools with tooth tops covered with hard films have been proposed. For example, Patent Document 1 discloses a hard film for cutting tools with excellent wear resistance.

[0003] On the other hand, various proposals have been made for improving the performance of the tooth tip shape of the cutting tool. For example, Patent Document 2 discloses a shape in which a chamfered portion is provided on the tooth tip.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Publication No. 2003-34859

[0007] Patent Document 2: Japanese Patent No. 6399661 Utility Model Content

[0008] However, since the tooth tops of the cutting tool are formed sharply, the close contact area of ​​the film becomes smaller at the tooth tops, and there is a problem that the hard film is easily peeled off. In addition, when using a high-performance film, it can be expected that the processing speed will increase, but the load applied to the tooth tops will also increase, so the peeling of the film will also become significant. In particular, the band saw blade has lower rigidity than other cutting tools and is also prone to cutting bending, etc., so there is a tendency to apply a large load to the tooth tops, which easily causes the film to peel off at the tooth tops. Therefore, it is required to improve the peeling of the film on the tooth tops.

[0009] A band saw blade according to one embodiment of the present invention has a saw tooth group composed of more than one saw tooth repeatedly provided at an edge of one side of a band-shaped main body extending in the direction of travel. In the band saw blade, the saw teeth each have a tooth top provided with a hard coating. Among the more than one saw teeth included in the saw tooth group, the tooth top of the saw tooth forming the cutting surface includes: a first chamfered portion provided at a first corner portion where a front cutting surface located at the front side in the direction of travel and a back cutting surface located at the back side in the direction of travel intersect; and a second chamfered portion provided at a second corner portion where a pair of side surfaces spaced apart from each other in the direction of strip thickness intersect with the back cutting surface. The dimension of the second chamfered portion in the direction of strip width is larger than the dimension of the first chamfered portion in the direction of strip width.

[0010] According to a band saw blade of one embodiment of the present invention, the tooth top has a first chamfered portion and a second chamfered portion, so that the shape of the tooth top can be blunted. As a result, the area where the hard film is in close contact with the tooth top increases, so that the strength of the hard film can be improved. In addition, by improving the tooth top shape to increase the strength of the hard film, the strength of the tooth top itself can also be improved.

[0011] Furthermore, the tooth top corner portion viewed from the front side in the traveling direction has a two-stage inclined shape. Thus, the tooth angle can be made closer to an obtuse angle compared to the tooth top provided with only the second chamfered portion. As a result, the shape of the tooth top corner portion is further blunted, thereby respectively improving the strength of the hard film and the strength of the tooth top.

[0012] According to one aspect of the present invention, by improving the strength of the hard film, peeling of the hard film can be suppressed. In addition, the strength of the tooth tip itself can be improved, thereby achieving a further effect of suppressing the occurrence of chipping and the like. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a perspective view showing the band saw blade according to the present embodiment.

[0014] Figure 2 This is a diagram showing each saw tooth constituting the saw tooth group from the tooth tip side.

[0015] Figure 3 This is a three-dimensional diagram showing the top of the saw teeth in an enlarged manner.

[0016] Figure 4 This is a diagram showing the tooth top when the saw teeth are viewed in the strip thickness direction.

[0017] Figure 5 It is a magnified representation Figure 4 A view of the tooth tip side of the tooth top shown.

[0018] Figure 6 This is a diagram showing the tooth top when the saw teeth are viewed facing the traveling direction.

[0019] Figure 7 It is a magnified representation Figure 6 A view of the tooth tip side of the tooth top shown.

[0020] Figure 8 It is a perspective view schematically showing a modified example of the band saw blade according to the present embodiment.

[0021] Fig. 9 It is a perspective view schematically showing a modified example of the band saw blade according to the present embodiment.

[0022] Fig.10 It is a perspective view schematically showing a modified example of the band saw blade according to the present embodiment.

[0023] Fig.11 It is a perspective view schematically showing a modified example of the band saw blade according to the present embodiment. DETAILED DESCRIPTION

[0024] Hereinafter, the band saw blade according to the present embodiment will be described with reference to the drawings.

[0025] Figure 1 It is a perspective view showing the band saw blade according to the present embodiment. Figure 2 This is a diagram showing each saw tooth constituting the saw tooth group from the tooth tip side. Figure 3 The three-dimensional diagram shows the top of the saw teeth in an enlarged manner. The symbols F1, F2 and F3 shown in the figure respectively represent the traveling direction of the band saw blade, the band thickness direction (left-right direction) and the band width direction. The band thickness direction is the direction of the plate thickness of the band saw blade, and the band width direction is the direction of the width of the band saw blade.

[0026] First, the outline of the band saw blade 100 of the present embodiment will be described. The band saw blade 100 of the present embodiment has a saw tooth group 10 repeatedly provided with one or more saw teeth 20, 40 combined at an edge portion of one side of a band-shaped main body portion 1 extending along the travel direction F1. In the band saw blade 100, each saw tooth 20, 40 has a tooth top portion 30, 50 provided with a hard coating. Among the one or more saw teeth 20, 40 included in the saw tooth group 10, the tooth top portion 50 of the saw tooth 40 forming the cut surface includes: a first chamfered portion 55, which is provided at a first corner portion where a front cutting surface 51 located on the front side of the travel direction F1 and a back cutting surface 52 located on the rear side of the travel direction F1 intersect; and a second chamfered portion 56, which is provided at a second corner portion where a pair of side surfaces 53 spaced apart from each other in the strip thickness direction F2 intersect the back cutting surface 52. The dimension of the second chamfered portion 56 in the belt width direction F3 is greater than the dimension of the first chamfered portion 55 in the belt width direction F3.

[0027] Next, the details of the band saw blade 100 according to the present embodiment will be described. The band saw blade 100 includes a body portion 1 and a saw tooth portion 2 .

[0028] The main body 1 is a belt-shaped member having a constant width in the belt width direction F3 and extending in the running direction F1. The main body 1 is formed of a high-strength material such as spring steel.

[0029] The toothed portion 2 is provided at one edge of the main body 1. The toothed portion 2 is configured such that a tooth group 10 composed of a plurality of teeth is repeated along the length direction (travel direction F1) of the main body 1. In the band saw blade 100 of the present embodiment, the tooth group 10 is composed of two tooth patterns including a first tooth 20 as a leading tooth and a second tooth 40 as a following tooth continuous with the first tooth 20.

[0030] The first saw teeth 20 and the second saw teeth 40 are formed into a desired tooth shape by grinding, for example. The first saw teeth 20 are honeycomb teeth formed into a bilaterally symmetrical shape in a manner that expands toward the tooth top ridgeline into a honeycomb shape (trapezoidal shape, or dove tail shape), and are configured as bevel gears in which the ridgelines on the left and right sides are chamfered. The second saw teeth 40 are honeycomb teeth, and are configured as deflected teeth having deflected portions that swing to the left and right when viewed from the travel direction F1 of the band saw blade 100.

[0031] The tooth height H2 of the first saw tooth 20 is higher than the tooth height H4 of the second saw tooth 40. The second saw tooth 40 having the swing bias on the left and right of the first saw tooth 20 and the second saw tooth 40 included in the saw tooth group 10 corresponds to the saw tooth having the maximum width in the strip thickness direction F2.

[0032] When cutting a workpiece using the band saw blade 100, the first teeth 20 form a deep groove at the center of the cut, and the second teeth 40 cut the left and right sides of the groove. The second teeth 40 as the subsequent teeth in the tooth set 10 correspond to the teeth that form the cut surface of the workpiece.

[0033] A tooth top portion 30, 50 having a cutting function is provided on the tooth top side of each saw tooth 20, 40. The tooth top portion 30, 50 is formed of a hard blade made of a so-called superhard alloy containing a hard material such as tungsten carbide or cobalt. The parts other than the tooth top portion 30, 50 of each saw tooth 20, 40 are formed of the same material as the main body 1.

[0034] A hard film is provided on each tooth top 30, 50 to protect the tooth top of each sawtooth 20, 40. The hard film may be a single-layer film or a multilayer film formed by stacking a plurality of layers. From the viewpoint of close contact, the thickness of the hard film is preferably 1 to 5 μm. The composition of the outermost surface of the hard film may be AlCrVN. The hard film may also include an AlCrVN layer containing a compound such as AlCrVN. In the case where the hard film is a multilayer film, the AlCrVN layer constitutes a layer of the multilayer film that protects the tooth top of each sawtooth 20, 40, and is basically arranged in the outermost layer. However, the AlCrVN layer may also be arranged in a layer closer to the inner side than the outermost layer.

[0035] By including Al (aluminum) as an element constituting the hard film, the oxidation resistance temperature is increased and the thermal conductivity is increased, thereby producing an effect of protecting the tooth top surface at high temperatures, which is beneficial for high-speed cutting, processing of high-hardness materials, and dry cutting.

[0036] In addition, Cr (chromium) and V (vanadium) maintain the crystal structure of the Al-containing film as a cubic crystal and maintain the hardness of the film. In particular, by adding Cr, the content of aluminum can be increased while maintaining the cubic crystal structure, so the hardness of the first chamfered portion 55 can be maintained. In addition, Cr has an effect of excellent wear resistance in iron-based workpieces.

[0037] In addition, V has a low oxidation start temperature, and during cutting, V is oxidized to generate a low melting point oxide V2O5 of about 650 to 670°C, which has the effect of improving the lubricity of the film and the workpiece. The hard film covers the entire tooth top 30, 50, but the chips are particularly curled on the rake face 51, so AlCrVN containing V and improving lubricity is present on the outermost surface of the rake face 51, which makes it easy for the chips to slide relative to the rake face 51. In addition, in the band saw blade 100, the tool speed is lower than that of lathe processing, and the use of cutting oil is recommended. Therefore, in the processing using the band saw blade 100, the ambient temperature of the tooth top 30, 50 is low compared to the processing temperature (about 800°C) of lathe processing, etc. The oxidation temperature of V is lower than that of Al, so the lubricity can be ensured in the band saw blade 100 used at relatively low or medium temperatures. The effect of V is unique, and such effect is not only found in Y (yttrium), Si (silicon), and B (boron), but also has not been confirmed in elements of the same group as V, such as Nb (niobium) and Ta (tantalum).

[0038] However, if Al becomes a high concentration, it is difficult to maintain the hardness of the hard film. Therefore, the proportion of Al in the whole compound is preferably 70at% or less, more preferably 50-70at%, and further preferably 65-70at%. In addition, based on the above reasons, the ratio of Cr and V is preferably 30at% or more, more preferably 30-50at%, and further preferably 30-35at%. In addition, if the concentration of V is high, its effect becomes dominant, and if it is more than 1.5at%, it is possible to generate fragments at the corner of the blade. Therefore, the proportion of V is preferably 0.5-1.5at%.

[0039] In view of this point, when the composition of the hard film on the outermost surface is AlCrVN, the composition of AlCrVN preferably satisfies the relationship of 0.5≤a≤0.7, a+b+c=1, 0.3≤b+c≤0.5, 0<c<0.015 (a represents the atomic ratio of Al, b represents the atomic ratio of Cr, and c represents the atomic ratio of V).

[0040] In addition, in AlCrVN, which is a compound constituting the hard film, a portion of N (nitrogen) may be replaced by carbon or oxygen to form a carbide or oxide. For example, the hard film may include AlCrVCN or AlCrVON. In addition, in addition to N, other fourth elements other than Al, Cr, and V may be added within a range that does not affect the performance. The content of the fourth element in AlCrVN may be less than 1 at%, less than 0.1 at%, or less than 0.01 at%.

[0041] The hard film may include, for example, a TiAlN layer containing a compound such as TiAlN. In the case where the hard film is a multilayer film, the TiAlN layer may constitute one layer of the multilayer film that protects the tooth tops of the saw teeth 20 and 40, and may be provided in direct contact with the surface of the tooth tops 30 and 50 as the substrate. However, another layer may be provided between the surface of the tooth tops 30 and 50 and the TiAlN layer.

[0042] The TiAlN layer contains Al, which increases the oxidation resistance temperature and the thermal conductivity, thereby protecting the tooth top surface at high temperatures, thereby facilitating high-speed cutting, processing of high-hardness materials, and dry cutting.

[0043] In addition, Ti (titanium) maintains the crystal structure of the Al-containing film as a cubic crystal and maintains the hardness of the film. Ti has the effect of excellent adhesion.

[0044] The ratio of Ti to the total of Ti and Al is preferably 40 at% or more and 60 at% or less. When the ratio of Ti is within the above range, the adhesion and hardness of the TiAlN layer can be improved. In addition, the ratio of Al to the total of Ti and Al is preferably 40 at% or more and 60 at% or less. In view of this, when the composition of the surface of the hard film in contact with the surface of the tooth top 30, 50 is TiAlN, the composition of TiAlN preferably satisfies the relationship of Ti:Al=d:1-d, 0.4≤d≤0.6. Similar to AlCrVN, in TiAlN, part of N can be replaced by carbon or oxygen, and other elements besides Ti and Al can be added within the range that does not affect the performance. The content of other elements in TiAlN can be less than 1 at%, can be less than 0.1 at%, and can also be less than 0.01 at%.

[0045] The hard film can also be a multilayer film formed by stacking an AlCrVN layer and a TiAlN layer. The AlCrVN layer has excellent wear resistance, and the TiAlN layer has excellent adhesion. Therefore, the multilayer film as described above has excellent wear resistance and adhesion. The multilayer film can be a two-layer type multilayer film in which an AlCrVN layer and a TiAlN layer are stacked one layer each, or it can be a repeatedly stacked type multilayer film in which an AlCrVN layer and a TiAlN layer are repeatedly stacked. Compared with a two-layer multilayer film, a repeatedly stacked multilayer film can suppress cracks. Since the AlCrVN layer has excellent wear resistance, it can be arranged on the outermost layer of the hard film and exposed. In addition, since the TiAlN layer has high adhesion, it can be arranged in a manner that directly contacts the surface of the tooth top 30, 50 as a substrate.

[0046] The composition of the AlCrVN layer and the TiAlN layer may be the same as described above. That is, when the hard film is a multilayer film formed by stacking the AlCrVN layer and the TiAlN layer, the composition of the AlCrVN layer preferably satisfies the relationship of 0.5≤a≤0.7, a+b+c=1, 0.3≤b+c≤0.5, 0<c<0.015 (a represents the atomic ratio of Al, b represents the atomic ratio of Cr, and c represents the atomic ratio of V). In addition, the composition of the TiAlN layer preferably satisfies the relationship of Ti:Al=d:1-d, 0.4≤d≤0.6 (d represents the atomic ratio of Ti).

[0047] The hard film may include a gradient layer in which the composition of TiAlN changes continuously to the composition of AlCrVN in the thickness direction of the hard film. In the gradient layer, the two components change continuously. Therefore, the hard film includes a gradient layer, thereby being able to make a hard film with excellent wear resistance, heat resistance and adhesion. In addition, compared with a multilayer film formed by repeatedly stacking AlCrVN layers and TiAlN layers, the processing time can be shortened. The hard film may include only one gradient layer or multiple gradient layers. The number of gradient layers in the hard film may be more than 2 layers, more than 10 layers, more than 30 layers or more than 50 layers. In addition, the number of gradient layers in the hard film may be less than 200 layers, less than 150 layers, less than 100 layers or less than 70 layers. The thickness of a gradient layer is preferably 10nm to 100nm, more preferably 20nm to 50nm.

[0048] In the case where the hard film includes a gradient layer as described above, the composition of AlCrVN and the composition of TiAlN may be the same as described above. Specifically, in the case where the hard film includes a gradient layer as described above, the composition of AlCrVN in the gradient layer preferably satisfies the relationship of 0.5≤a≤0.7, a+b+c=1, 0.3≤b+c≤0.5, 0<c<0.015 (a represents the atomic ratio of Al, b represents the atomic ratio of Cr, and c represents the atomic ratio of V). In addition, the composition of TiAlN preferably satisfies the relationship of Ti:Al=d:1-d, 0.4≤d≤0.6 (d represents the atomic ratio of Ti). By making the composition of the gradient layer within the above range, a hard film with better wear resistance, heat resistance and adhesion can be formed.

[0049] The gradient layer preferably changes continuously from the composition of TiAlN to the composition of AlCrVN from the tooth top 30, 50 toward the exposed surface of the hard film. From the viewpoint of wear resistance and heat resistance, such a gradient layer can be provided on the outermost layer of the hard film and exposed. In addition, from the viewpoint of adhesion, such a gradient layer can be provided in a manner of directly contacting the surface of the tooth top 30, 50 as the substrate.

[0050] In addition, the gradient layer may also continuously change from the composition of TiAlN to the composition of AlCrVN from the two outer surfaces toward the center in the thickness direction of the gradient layer. The position of setting such a gradient layer is not particularly limited, and from the viewpoint of adhesion, it can be set in a manner of directly contacting the surface of the tooth top 30, 50 as the substrate.

[0051] In addition, the gradient layer may also continuously change from the composition of AlCrVN to the composition of TiAlN from the two outer surfaces toward the center in the thickness direction of the gradient layer. The position of setting such a gradient layer is not particularly limited, and from the perspective of wear resistance and heat resistance, it can be set as the outermost layer of the hard film and exposed.

[0052] The hard film may include at least one layer selected from the above-mentioned AlCrVN layer, TiAlN layer and gradient layer. For example, in the hard film, a TiAlN layer, a plurality of gradient layers and an AlCrVN layer may be sequentially arranged from the tooth top 30, 50 toward the exposed surface of the hard film, and the AlCrVN layer may be arranged in the outermost layer. In addition, for example, in the hard film, a TiAlN layer and a plurality of gradient layers may be sequentially arranged from the tooth top 30, 50 toward the exposed surface of the hard film, and the gradient layer may be arranged in the outermost layer. In addition, for example, in the hard film, a plurality of gradient layers and an AlCrVN layer may be sequentially arranged from the tooth top 30, 50 toward the exposed surface of the hard film, and the AlCrVN layer may be arranged in the outermost layer. In these examples, the plurality of gradient layers may be replaced by a single gradient layer.

[0053] In the method for manufacturing the band saw blade 100, the hard film can be applied to the tooth tops 30 and 50 by a general coating method such as physical vapor deposition (PVD) and chemical vapor deposition (CVD). In addition, the temperature during film processing of thermal CVD is about 1000°C, while the temperature during film processing of PVD is as low as about 500°C, which is lower than the annealing temperature of the metal strip used in the band saw blade 100. Therefore, it is difficult to cause deformation of the metal strip due to heat, so it is preferable to form the hard film by PVD such as ion plating. As an example of ion plating, arc evaporation can be cited.

[0054] In the method for manufacturing the band saw blade 100 including the gradient layer, the gradient layer can be formed by an ion plating method using an AlCrV target and a TiAl target. In the ion plating method, a rotating table provided with the tooth tops 30 and 50 before the gradient layer is formed is rotated. Then, the tooth tops 30 and 50 before the gradient layer is formed are gradually moved from the position of one of the AlCrV target and the TiAl target to the position of the other target. The gradient layer can also be formed by ion plating using such a method.

[0055] In the present method, AlCrVN generated by the reaction of AlCrV and nitrogen is formed on the tooth tops 30 and 50 at a position where the position of the tooth tops 30 and 50 is close to the position of the AlCrV target. In addition, TiAlN generated by the reaction of TiAl and nitrogen is formed on the tooth tops 30 and 50 at a position where the position of the tooth tops 30 and 50 is close to the position of the TiAl target. For example, when the turntable is rotated in such a manner that the position of the tooth tops 30 and 50 approaches the AlCrV target from the TiAl target, a gradient layer is formed in such a manner that the composition of TiAlN continuously changes to the composition of AlCrVN in the thickness direction of the hard film. In addition, by rotating the turntable, the tooth tops 30 and 50 alternately approach the AlCrV target and the TiAl target. Therefore, according to such a method, a plurality of gradient layers can also be easily formed.

[0056] The composition of the AlCrV target is the same as that of the above-mentioned AlCrVN, and preferably satisfies the relationship of 0.5≤a≤0.7, a+b+c=1, 0.3≤b+c≤0.5, and 0<c<0.015 (a represents the atomic ratio of Al, b represents the atomic ratio of Cr, and c represents the atomic ratio of V). In addition, the composition of the TiAl target is the same as that of the above-mentioned TiAlN, and preferably satisfies the relationship of Ti:Al=d:1-d, and 0.4≤d≤0.6 (d represents the atomic ratio of Ti).

[0057] The voltage applied to the tooth top 30, 50 as the substrate and the rotation speed of the rotating table can be appropriately adjusted according to the desired thickness of the gradient layer. In addition, in the present method, at least one AlCrV target and at least one TiAl target are sufficient. That is, the gradient layer can be formed using a total of two targets, or can be formed using three or more targets. In addition, the purge gas during ion plating can be nitrogen, but a part of the nitrogen can also be replaced by hydrocarbon gas such as methane or oxygen.

[0058] Below, refer to Figures 3 to 7 Next, the structure of the tooth top portion 50 of the second saw tooth 40 which is one of the features of the band saw blade 100 according to the present embodiment will be described. Figure 4 This is a diagram showing the tooth top when the saw teeth are viewed in the strip thickness direction. Figure 5 It is a magnified representation Figure 4 A view of the tooth tip side of the tooth top shown. Figure 6 This is a diagram showing the tooth top when the saw teeth are viewed facing the traveling direction. Figure 7 It is a magnified representation Figure 6 A view of the tooth tip side of the tooth top shown.

[0059] In the saw tooth group 10, the second saw tooth 40 is a saw tooth having the largest width in the strip thickness direction F2, and is a saw tooth that forms the cut surface of the workpiece. First, the structure of the tooth top 50 of the second saw tooth 40 will be briefly described. The tooth top 50 has a rake face 51 located on the front side of the travel direction F1, a flank face 52 located on the rear side of the travel direction F1, and a pair of side faces 53 spaced apart from each other in the strip thickness direction F2.

[0060] In addition to these structures, the tooth top 50 of the present embodiment further includes a first chamfered portion 55 and a second chamfered portion 56. The first chamfered portion 55 is provided at the first corner portion where the front cutting surface 51 and the back cutting surface 52 intersect, that is, the tooth top ridgeline, and is formed by a tapered surface in the present embodiment. On the other hand, the second chamfered portion 56 is provided at the second corner portion where the side surface 53 and the back cutting surface 52 intersect, and is formed by a tapered surface on both sides extending from the tooth top ridgeline to the rear side of the travel direction F1, and is formed by a tapered surface in the same manner as the first chamfered portion 55. The second chamfered portion 56 is chamfered parallel to the back cutting surface 52.

[0061] Generally, the notch of a band saw blade is in the range of about 0.005 mm to 0.050 mm. In addition, a band saw blade has lower rigidity than other cutting tools. In view of these aspects, the shapes of the first and second chamfered portions 55 and 56 preferably satisfy the following conditions.

[0062] like Figure 4 as well as Figure 5As shown, the first chamfered portion 55 has a tapered shape inclined toward the tooth root side when viewed from the rear side to the front side (from the left side to the right side of the paper) in the travel direction F1. The chamfer angle C of the first chamfered portion 55 is preferably 35° to 55° relative to the vertical line perpendicular to the bandwidth direction F3, and more preferably 45°. In addition, the dimension (distance) D of the first chamfered portion 55 in the bandwidth direction F3 is preferably in the range of 0.010 to 0.150 mm. In particular, when the workpiece is a difficult-to-cut material, the dimension D is preferably 0.02 to 0.06 mm.

[0063] like Figure 6 as well as Figure 7 As shown, the second chamfered portion 56 has a tapered shape that is inclined toward the tooth root side when viewed from the center of the tooth top 50 toward the left and right sides along the belt thickness direction F2. The chamfer angle E of the second chamfered portion 56 is preferably 35° to 55° relative to the vertical line perpendicular to the belt width direction F3, and more preferably 45°. In addition, the dimension (distance) F of the second chamfered portion 56 in the belt width direction F3 is set to be larger than the dimension D of the first chamfered portion 55, preferably in the range of 0.050 to 0.150 mm. In the case where the workpiece is a difficult-to-cut material, the dimension F is preferably 0.08 to 0.12 mm.

[0064] As described above, the second chamfered portion 56 is chamfered parallel to the back cutting surface 52. In addition, the dimension F of the second chamfered portion 56 is set to be larger than the dimension D of the first chamfered portion 55. By such a chamfering method, Figure 7 As shown in FIG. 1 , when the tooth top 50 is viewed from the front side in the travel direction F1, the tooth top corner portion on the right side of the tooth top is composed of two-stage inclined shapes. That is, the tooth top corner portion includes a first inclined side 56a with a chamfer angle E' formed by the first chamfered portion 55 and the second chamfered portion 56, and a second inclined side 56b with a chamfer angle E formed only by the second chamfered portion 56. Figure 7 Only the shape of the right side tooth tip corner portion of the tooth tip is shown, but the left side tooth tip corner portion of the tooth tip is also composed of two-stage inclined shapes.

[0065] Next, the functions and effects of the first and second chamfered portions 55 and 56 provided at the tooth top 50 of the second sawtooth 40 are described. When the angle of the tooth top, i.e., the tooth angle, is an obtuse angle, the area in which the hard film is in close contact with the tooth top increases. Therefore, the strength of the hard film is improved, and the peeling of the hard film can be suppressed. In addition, the strength of the tooth top itself is also increased, so the occurrence of chipping and the like can be suppressed.

[0066] First, if Figure 5 As shown, the tooth top 50 has a first chamfered portion 55, whereby the shape of the tooth top viewed from the belt thickness direction F2 is blunted. This can improve the strength of the hard film and the strength of the tooth top itself. Figure 5, the angle α0 is the angle between the flank surface 52 and the first chamfered portion 55 . The angle α1 is the angle between the first chamfered portion 55 and the rake surface 51 .

[0067] The smaller the chamfer angle C of the first chamfered portion 55, the more obtuse the angle α0 is, so the strength of the hard film and the strength of the tooth top are improved. However, since the first chamfered portion 55 becomes a negative front angle, chips are easily accumulated and the cutting resistance becomes larger. In addition, according to the value of the chamfer angle C, the angle α1 becomes an acute angle, and the strength of the hard film and the strength of the tooth top may be reduced. In contrast, the larger the chamfer angle C of the first chamfered portion 55, the more acute the angle α0 is. In this case, the cutting resistance becomes smaller, but the strength of the tooth top is reduced. Therefore, in this embodiment, considering these factors, the chamfer angle C of the first chamfered portion 55 is set within the range of 35° to 55°. As a result, the strength of the hard film can be improved, so the peeling of the hard film can be suppressed. In addition, by improving the tooth top shape to improve the strength of the hard film, the strength of the tooth top itself can also be improved, which can achieve a new effect of suppressing the occurrence of chipping and the like.

[0068] The smaller the dimension D of the first chamfered portion 55, the sharper the shape of the tooth top. Since the area where the hard film is in close contact with the tooth top is reduced, the peeling of the hard film is likely to occur. On the other hand, the larger the dimension D of the first chamfered portion 55, the blunter the shape of the tooth top. Therefore, the area where the hard film is in close contact with the tooth top is increased, which can suppress the peeling of the hard film. However, if the dimension D of the first chamfered portion 55 is large, chips are easily accumulated in the first chamfered portion 55, and the cutting resistance becomes larger. Therefore, in this embodiment, considering these factors, the dimension D of the first chamfered portion 55 is set within the range of 0.010 to 0.150 mm. As a result, the strength of the hard film can be improved, so the peeling of the hard film can be suppressed. In addition, by improving the shape of the tooth top to increase the strength of the hard film, the strength of the tooth top itself can also be improved, which can achieve a new effect of suppressing the occurrence of chipping and the like.

[0069] Then, if Figure 7 As shown, the tooth top 50 has a second chamfered portion 56, whereby the shape of the tooth top corner portion viewed from the front side in the travel direction F1 is blunted. This can improve the strength of the hard film and improve the strength of the tooth top itself. Figure 7 , the angle α2 is the angle formed by the ridgeline of the flank 52 and the first chamfered portion 55 and the first inclined side 56 a . The angle α3 is the angle formed by the second inclined side 56 b and the ridgeline of the rake face 51 and the side face 53 .

[0070] The larger the chamfer angle E of the second chamfered portion 56 is, the closer the angle α2 is to an acute angle, so the strength of the hard film and the strength of the tooth top are reduced. In addition, since the first and second inclined edges 56a, 56b are close to the extension lines of the ridges of the front cutting surface 51 and the side surface 53, the resistance acting from the left and right directions in the second chamfered portion 56 becomes larger, and the cutting resistance becomes larger. In contrast, the smaller the chamfer angle E of the second chamfered portion 56 is, the more the angle α2 is an obtuse angle, and the strength of the hard film and the strength of the tooth top are improved. However, according to the chamfer angle E, the angle α3 becomes too acute, resulting in a reduction in the strength of the hard film and the strength of the tooth top. Therefore, in this embodiment, considering these factors, the chamfer angle E of the second chamfered portion 56 is set within the range of 35° to 55°. As a result, the strength of the hard film can be improved, so the peeling of the hard film can be suppressed. Furthermore, by improving the tooth tip shape to increase the strength of the hard film, the strength of the tooth tip itself can also be increased, which can produce a new effect of suppressing the occurrence of chipping and the like.

[0071] When the dimension F of the second chamfered portion 56 is small, the shape of the tooth top becomes sharp. Since the area where the hard film is in close contact with the tooth top is reduced, the peeling of the hard film is likely to occur. On the other hand, the larger the dimension F of the second chamfered portion 56 is, the blunter the shape of the tooth top is. Therefore, the area where the hard film is in close contact with the tooth top increases, which can suppress the peeling of the hard film. However, the resistance acting from the left and right directions in the second chamfered portion 56 increases, and the cutting resistance increases. Therefore, in this embodiment, considering these factors, the dimension F of the second chamfered portion 56 is set within the range of 0.050 to 0.150 mm. As a result, the strength of the hard film can be improved, so the peeling of the hard film can be suppressed. In addition, by improving the shape of the tooth top to increase the strength of the hard film, the strength of the tooth top itself can also be improved, which can achieve a new effect of suppressing the occurrence of chipping and the like.

[0072] In addition, in the present embodiment, the dimension F of the second chamfered portion 56 is set to be larger than the dimension D of the first chamfered portion 55. In addition, the second chamfered portion 56 is chamfered parallel to the back face 52. Figure 7As shown, the tooth top 50 has a second chamfered portion 56 in addition to the first chamfered portion 55, so that the tooth top corner portion becomes a two-stage inclined shape composed of the first and second inclined edges 56a and 56b. Therefore, compared with the chamfered angle E (the angle formed by the second inclined edge 56b) of the portion formed by only the second chamfered portion 56, the chamfered angle E' (the angle formed by the first inclined edge 56a) of the portion formed by the first and second chamfered portions 55 and 56 becomes smaller. As a result, compared with the case where only the second chamfered portion 56 is processed, the angle α2 can be made closer to an obtuse angle. As a result, the shape of the tooth top corner portion is further blunted, so that the strength of the hard film and the strength of the tooth top can be respectively improved. As a result, the peeling of the hard film can be suppressed, and the occurrence of chipping and the like can be suppressed.

[0073] When the dimension F of the second chamfered portion 56 is smaller than the dimension D of the first chamfered portion 55, the chips retained at the front end portion tend to flow out in the strip thickness direction F2, thereby increasing the cutting resistance and possibly roughening the cut surface. In this regard, according to the present embodiment, the dimension F of the second chamfered portion 56 is set to be larger than the dimension D of the first chamfered portion 55. The second inclined edge 56b formed only by the second chamfered portion 56 remains at the left and right tooth top corners. As a result, the chips generated in the portion close to the side surface 53 can flow smoothly to the rake face 51, thereby improving the cut surface and maintaining the cut surface well.

[0074] Thus, in this embodiment, the structure of the tooth top of the sawtooth that forms the cut surface of the workpiece is described. According to this structure, the strength of the hard film can be improved, so the peeling of the hard film can be suppressed. In addition, by improving the tooth top shape to increase the strength of the hard film, the strength of the tooth top itself can also be increased, which can achieve a new effect of suppressing the occurrence of chipping and the like.

[0075] In the band saw blade of the present embodiment, the tooth profile of the teeth other than the teeth forming the cut surface of the workpiece (the remaining teeth) among the plurality of teeth constituting the tooth group may be any shape. Figure 1 , Figures 8 to 11 , a modification of the band saw blade 100 of this embodiment will be described. Here, Figures 8 to 11 It is a perspective view schematically showing a modified example of the band saw blade according to the present embodiment.

[0076] For example, Figure 1As shown in the first sawtooth 20, the remaining sawtooth may also be a bevel gear formed by chamfering the ridges on the left and right sides of the bee tooth. In this case, the first and second chamfers which are the same as the tooth top 50 of the second sawtooth 40 may be set for the tooth top 30 of the first sawtooth 20. In this case, it is preferred that a second chamfer which is larger than the second sawtooth 40 with a smaller tooth height H4 is set for the first sawtooth 20 with a larger tooth height H2.

[0077] In addition, the sawtooth set 10 may include a plurality of sawtooths located ahead of the second sawtooth 40. Figure 8 In the figure, the third saw tooth 21 having a larger tooth height than the first saw tooth is shown at a position forward of the first saw tooth 20. In this case, the first and second chamfers similar to the tooth top 50 of the second saw tooth 40 may be set to the tooth tops 30 and 31 of each saw tooth 20 and 21. In this case, it is preferred that the saw teeth 20 and 21 having a larger tooth height have a larger second chamfer.

[0078] Moreover, if Fig. 9 As shown, the tooth tops 61, 62 of the saw teeth 41, 42 forming the cut surface of the workpiece can also have the function of forming the cut surface of the workpiece only on one side of the tooth top. In this case, the second chamfered portion is only provided at the tooth top corner portion on one side of the left and right sides of the cut surface of the workpiece.

[0079] And, if Fig.10 As shown, the saw teeth 43, 44 forming the cut surface of the workpiece may also be eccentric teeth that swing only to one side. In this case, the second chamfered portion set at the tooth top 63, 64 of each saw tooth 43, 44 may be set at one tooth top corner portion on the left or right side forming the cut surface of the workpiece, or may be set at both tooth top corner portions on the left or right side.

[0080] In addition, in this embodiment, as the sawtooth group 10 constituting the sawtooth portion 2, an example of combining a plurality of saw teeth is shown. However, the sawtooth group 10 only needs to include at least one sawtooth, and all of the sawtooth portion 2 may be saw teeth with the same function. For example, the sawtooth portion 2 may also be composed of only saw teeth that form the cut surface. In this case, Fig.11 As shown, the tooth top 65 of the sawtooth 45 forming the cutting surface may also have a notch 65a for cutting off the chips. For example, the notch 65a is formed by cutting a semicircular groove extending in the traveling direction at the tooth top 65. Fig.11 In the example shown, the positions of the cutouts 65a are set to be separated into left and right positions for each tooth, but the cutouts 65a may be set at any positions. In addition, the shapes of the cutouts 65a may be any shapes.

[0081] As described above, the embodiments of the present invention are described, but it should not be understood that the description and drawings constituting a part of this disclosure limit the present invention. Based on this disclosure, various alternative embodiments, examples, and application techniques will be apparent to those skilled in the art.

[0082] The disclosure of this application is related to the subject matter described in Japanese Patent Application No. 2021-209287 filed on December 23, 2021 and Japanese Patent Application No. 2022-181970 filed on November 14, 2022, and all of these disclosures are incorporated herein by reference.

Claims

1. A band saw blade, wherein a saw tooth group composed of one or more saw teeth is repeatedly provided at one edge of a band-shaped main body extending in a traveling direction, wherein: The saw teeth each have a tooth top portion provided with a hard coating. Among the one or more saw teeth included in the saw tooth group, the tooth top of the saw tooth forming the cut surface includes: A first chamfered portion provided at a first corner portion where a rake face located at a front side in the traveling direction intersects a flank face located at a rear side in the traveling direction; and A second chamfered portion is provided at a second corner portion where a pair of side surfaces spaced apart from each other in the strip thickness direction intersect the flank surface, A dimension of the second chamfered portion in a bandwidth direction is greater than a dimension of the first chamfered portion in the bandwidth direction.

2. The band saw blade according to claim 1, characterized in that The second chamfered portion is chamfered parallel to the relief surface.

3. The band saw blade according to claim 1, characterized in that The dimension of the first chamfered portion in the belt width direction is 0.010 to 0.150 mm.

4. The band saw blade according to claim 2, characterized in that The dimension of the first chamfered portion in the belt width direction is 0.010 to 0.150 mm.

5. The band saw blade according to any one of claims 1 to 4, characterized in that The size of the second chamfered portion in the bandwidth direction is 0.050-0.150 mm, which is larger than the size of the first chamfered portion in the bandwidth direction.

6. The band saw blade according to any one of claims 1 to 4, characterized in that The chamfer angle of the first chamfered portion is 35° to 55° relative to a perpendicular line perpendicular to the width direction of the belt.

7. The band saw blade according to claim 5, characterized in that The chamfer angle of the first chamfered portion is 35° to 55° relative to a perpendicular line perpendicular to the width direction of the belt.

8. The band saw blade according to any one of claims 1 to 4, characterized in that The chamfer angle of the second chamfered portion is 35° to 55° relative to a perpendicular line perpendicular to the width direction of the belt.

9. The band saw blade according to claim 5, characterized in that The chamfer angle of the second chamfered portion is 35° to 55° relative to a perpendicular line perpendicular to the width direction of the belt.

10. The band saw blade according to claim 6, characterized in that The chamfer angle of the second chamfered portion is 35° to 55° relative to a perpendicular line perpendicular to the width direction of the belt.