Screen printing plate

By arranging a surface energy layer on the side wall of the second line slot of the printing screen, the problems of low conductive efficiency and uneven printing of the traditional printing screen are solved, and the printing quality and conductive performance of the electrode film are improved.

CN221851458UActive Publication Date: 2024-10-18SHINE OPTOELECTRONICS (KUNSHAN) CO LTD
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202323670030.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2024-10-18
Estimated Expiration
2033-12-29

AI Technical Summary

Technical Problem

In traditional printing screens, the conductive efficiency of the electrode film is low due to the nodes formed by the intersection of longitude and latitude lines, and the poor ink passing ability of the stencil screen and uneven printing results in a short lifespan.

Method used

Design a printing screen, which includes a stacked first metal layer and a second metal layer, grid lines are formed by arranging penetrating first and second line troughs, and surface energy is provided on the side walls of the second line trough. layer, such as a coating or plating, to improve the ink-passing ability of the conductive paste.

Benefits of technology

By increasing the ink passing ability of the conductive paste, the printing quality and ink dispensing properties are improved, thereby improving the conductive efficiency of the electrode film and the life of the printing screen.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221851458U_ABST
    Figure CN221851458U_ABST
Patent Text Reader

Abstract

The utility model discloses a screen printing plate which comprises a first metal layer, a second metal layer and grid lines. The first metal layer comprises a first wire slot which is arranged in a penetrating manner, and a printing surface and a first matching surface which are oppositely arranged; the second metal layer comprises a second wire slot which is arranged in a penetrating manner, and a bottom surface and a second matching surface which are oppositely arranged; the first metal layer and the second metal layer are laminated through the matching of the first matching surface and the second matching surface; the first wire slots and the second wire slots are correspondingly arranged and are communicated with each other to form the grid lines; a surface energy layer is arranged on the side wall of the second wire groove so as to change the surface energy of the side wall, the ink passing capacity of the conductive paste can be improved when the conductive paste is printed, and therefore the ink discharging performance and the printing quality can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of screen printing, and in particular to a printing screen. Background Art

[0002] Printing screens are important tools in the electronics field. Taking printing the electrodes of solar cells as an example, slurry is poured onto the printing screen and moved on the printing screen with a scraper so that the slurry is squeezed through the mesh holes on the printing screen onto the solar cell, forming a corresponding pattern on the solar cell to form the electrodes of the solar cell.

[0003] The traditional printing screen has nodes formed by the intersection of longitude and latitude lines, so the final electrode will have knots, which will affect the conductivity or conversion efficiency of the electrode film. To solve the above problems, the existing printing screen adopts a knot-free design and uses a steel plate mesh; however, the steel plate mesh has printing problems such as poor ink passing ability and uneven ink delivery, and also has the problem of unstable performance and low life. Therefore, it is urgent to provide a printing screen with a new structure to solve at least one technical problem in the prior art. Utility Model Content

[0004] Based on this, it is necessary to provide a printing screen to solve at least one of the above technical problems.

[0005] A technical solution of this application is:

[0006] A printing screen, comprising:

[0007] A first metal layer, comprising a first wire groove arranged through, a printing surface and a first matching surface arranged opposite to each other;

[0008] The second metal layer comprises a second wire groove provided through the second wire groove, a bottom surface and a second mating surface provided opposite to each other, wherein the first metal layer and the second metal layer are stacked by matching the first mating surface and the second mating surface;

[0009] A gate line, wherein the first line groove and the second line groove are arranged correspondingly and are interconnected to form the gate line;

[0010] Wherein, a surface energy layer is arranged on the side wall of the second wire groove.

[0011] In one embodiment, the surface energy layer is a coating or a plating layer.

[0012] In one embodiment, the coating layer is a fluorine-containing layer, and the plated layer is an electroplated metal layer.

[0013] In one embodiment, a surface energy layer is disposed on the side wall of the first wire trough, and the surface energy layer is a coating or a plating layer.

[0014] In one embodiment, the opening width of the second wire groove close to the first wire groove is smaller than or equal to the opening width away from the first wire groove.

[0015] In one embodiment, the side wall of the second wire groove is inclined, and the inclination angle is greater than 0 degree and less than or equal to 45 degrees.

[0016] In one embodiment, the printing surface and / or the bottom surface is provided with a surface energy layer, and the surface energy layer is a coating or a plating layer.

[0017] In one embodiment, the printing surface is provided with a micro-nano structure with protrusions and / or depressions, and the micro-nano structure is a grid texture, an AG texture or a brushed texture.

[0018] In one embodiment, the thickness of the grid texture ranges from 3μm to 25μm or the depth ranges from 3μm to 25μm, the average pore size of the grid of the grid texture is 10μm to 200μm, and the width of the mesh line ranges from 5μm to 150μm; the thickness of the AG texture does not exceed 25μm or the depth does not exceed 25μm, and the width of the AG texture ranges from 5μm to 150μm; the thickness of the brushed texture ranges from 3μm to 25μm or the depth ranges from 3μm to 25μm, and the width of the brushed texture ranges from 5μm to 150μm.

[0019] In one embodiment, an AG structure is disposed on the micro-nano structure, the height of the AG structure is in the range of 10 nm-5 μm, and the width of the AG structure is in the range of 50 nm-50 μm.

[0020] In one embodiment, the grid lines are defined as extending along the Y direction, and the printing direction is defined as the X direction, wherein the X direction and the Y direction are arranged to intersect each other; at least part of the micro-nano structure extends in a direction that forms an angle with the X direction, and the angle ranges from 5° to 85°.

[0021] Beneficial effects of the present application: A surface energy layer is provided on the side wall of the second line groove of the printing screen of the present application to change the surface energy of the side wall, thereby increasing the ink passing ability of the conductive paste when printing the conductive paste, thereby improving the ink taking property and printing quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 A schematic diagram of the planar structure of a printing screen for this application;

[0023] Figure 2 for Figure 1 A schematic diagram of the cross-sectional structure of a printing screen;

[0024] Figure 3 This is another schematic diagram of the cross-sectional structure of a printing screen of the present application;

[0025] Figure 4 This is another schematic diagram of the cross-sectional structure of a printing screen of the present application;

[0026] Figure 5 This is another schematic diagram of the cross-sectional structure of a printing screen of the present application;

[0027] Figure 6 Another schematic diagram of the planar structure of a printing screen for this application;

[0028] Figure 7 for Figure 6 A schematic diagram of the cross-sectional structure of a printing screen;

[0029] Figure 8 This is another schematic diagram of the cross-sectional structure of a printing screen of the present application;

[0030] Fig. 9 This is another schematic diagram of the cross-sectional structure of a printing screen in the present application. DETAILED DESCRIPTION

[0031] In order to facilitate the understanding of the present application, the present application will be described more comprehensively below with reference to the relevant drawings. The preferred embodiments of the present application are provided in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described below. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thoroughly and comprehensively understood.

[0032] It should be noted that when an element is referred to as being "disposed on" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.

[0033] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those generally understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0034] The utility model discloses a printing screen, which includes a first metal layer and a second metal layer stacked and a grid line running through the first metal layer and the second metal layer. The first metal layer includes a first wire groove running through, a printing surface and a first matching surface that are oppositely arranged. The second metal layer includes a second wire groove running through, a bottom surface and a second matching surface that are oppositely arranged. The first metal layer and the second metal layer are stacked by matching the first matching surface and the second matching surface. The first wire groove and the second wire groove are correspondingly arranged and interconnected to form a grid line. A surface energy layer is provided on the side wall of the second wire groove to change the surface energy of the side wall and increase the ink passing ability of the conductive paste when printing the conductive paste, thereby improving the ink taking property and the printing quality.

[0035] In one embodiment, the surface energy layer is a coating or a plating layer. Preferably, the coating is a fluorine-containing layer, such as a Teflon coating; the plating layer is an electroplated metal layer, such as an electroplated tin layer, an electroplated copper layer, etc.

[0036] In one embodiment, a surface energy layer is provided on the side wall of the first wire groove, and the surface energy layer is a coating or plating layer to change the surface energy of the side wall and increase the ink passing ability of the conductive paste when printing the conductive paste, thereby improving the ink taking property and printing quality.

[0037] In one embodiment, the opening width of the second slot close to the first slot is less than or equal to the opening width away from the first slot, so as to control the ink flow rate and increase the ink passing capacity. For example, the side wall of the second slot is inclined, and the inclination angle is greater than 0 degrees and less than or equal to 45 degrees. Setting the inclination angle of the side wall and providing a surface energy layer on the side wall can effectively control the ink flow rate and improve the ink passing capacity.

[0038] In one embodiment, the printing surface and / or the bottom surface are provided with a surface energy layer, and the surface energy layer is a coating or a plating layer. The surface energy layer is provided on the printing surface, which has the effects of protecting the printing screen, strengthening the strength of the printing screen, controlling the scraper, etc., and the surface layer is provided on the bottom surface, which has the effects of protecting the printing screen, strengthening the strength of the printing screen, and improving the printing quality. The grid texture is a texture distributed in a grid shape, and the grid lines are raised and / or recessed. The AG texture is a plurality of raised structures and / or recessed structures, and at least one of the parameters such as the height, depth, width, length, density, period, curvature, and cross-section of the raised structure or the recessed structure is randomly set. For example, the height, period, and curvature of a plurality of raised structures are randomly set to form an AG texture. The brushed texture is a brushed texture.

[0039] In one embodiment, the printing surface is provided with a micro-nano structure with raised and / or recessed settings, and the micro-nano structure is a grid texture, an AG texture, or a brushed texture. The thickness of the grid texture ranges from 3μm to 25μm or the depth ranges from 3μm to 25μm, the average pore size of the grid of the grid texture is 10μm to 200μm, and the width of the mesh line ranges from 5μm to 150μm; the thickness of the AG texture does not exceed 25μm or the depth does not exceed 25μm, and the width of the AG texture ranges from 5μm to 150μm; the thickness of the brushed texture ranges from 3μm to 25μm or the depth ranges from 3μm to 25μm, and the width of the brushed texture ranges from 5μm to 150μm. The micro-nano structure can effectively control the scraper, thereby controlling the conductive paste, improving the ink-down performance and ensuring the printing quality.

[0040] In one embodiment, an AG structure is provided on the micro-nano structure, and the height range of the AG structure is 10nm-5μm, and the width range of the AG structure is 50nm-50μm. The AG structure is a plurality of raised structures and / or recessed structures, and at least one of the parameters such as the height, depth, width, length, density, period, curvature, and cross-section of the raised structure or the recessed structure is randomly set. For example, the micro-nano texture is a grid texture, and the AG structure is provided on the grid texture to form a composite texture, which can effectively control the resistance of the scraper during printing, so as to control the amount of ink and improve the printing quality. In one embodiment, the grid line is defined as extending along the Y direction, and the printing direction is defined as the X direction, wherein the X direction is cross-set with the Y direction; the direction in which at least part of the micro-nano structure extends is at an angle to the X direction, and the angle range is 5°-85°, so that the micro-nano structure plays a role in the control effect of the scraper.

[0041] The printing screen of the present application is described below with reference to the drawings.

[0042] Please refer to Figure 1 and Figure 2 The utility model discloses a printing screen 100, which includes a first metal layer 1, a second metal layer 2 and a grid line 31. The first metal layer 1 and the second metal layer 2 are stacked, and the grid line 31 runs through the first metal layer 1 and the second metal layer 2. The first metal layer 1 includes a first wire groove 11 that runs through, a printing surface 12 that is arranged oppositely, and a first matching surface 13. The second metal layer 2 includes a second wire groove 21 that runs through, a bottom surface 22 that is arranged oppositely, and a second matching surface 23. The first metal layer 1 and the second metal layer 2 are stacked by matching the first matching surface 13 and the second matching surface 23. The first wire groove 11 and the second wire groove 21 are arranged correspondingly and connected to each other to form the grid line 31, and the groove width of the first wire groove 11 is greater than the groove width of the second wire groove 21. Among them, a surface energy layer 41 is arranged on the side wall of the second wire groove 11 to change the surface energy of the side wall of the second wire groove 11, and increase the ink passing ability of the conductive paste when printing the conductive paste, thereby improving the ink taking property and printing quality.

[0043] The surface energy layer 41 is an electroplated tin layer, which changes the surface energy of the side wall of the second wire groove 21 through the electroplated tin layer to increase the ink passing ability and improve the printing quality. In other embodiments, it can also be a metal or alloy coating formed by other coating methods such as an electroplated alloy tin layer, an electroplated copper layer, and a vapor-deposited tin layer. In other embodiments, the surface energy layer 41 can also be a coating formed on the side wall of the second wire groove 21 by coating. Preferably, the coating is a Teflon coating, which can change the surface energy of the side wall of the second wire groove 21 and improve the ink passing ability.

[0044] Please continue reading Figure 2 The opening width of the second wire groove 21 close to the first wire groove 11 is smaller than the opening width away from the first wire groove 11. The side wall of the second wire groove 21 is inclined, and the inclination angle α is greater than 0 degrees and less than or equal to 45 degrees to control the ink flow rate and increase the ink passing capacity.

[0045] For other embodiments, please refer to Figure 3 The side wall of the first line groove 11 is also provided with a surface energy layer 42, and the surface energy layer 42 is a coating or plating layer. The side wall of the gate line 31 is provided with a surface energy layer, which can further control the ink passing ability. Figure 4 Furthermore, a surface energy layer 43 is provided on the bottom surface 22. The surface energy layer 43 is a coating or plating layer, which can protect the printing screen, strengthen the printing screen strength, and improve the printing quality. Figure 5 Furthermore, a surface energy layer 44 is provided on the printing surface 12. The surface energy layer is a coating or plating layer, which can protect the printing screen, enhance the strength of the printing screen, control the scraper and the like.

[0046] Please refer to Figure 6 and Figure 7The utility model discloses another printing screen 200. Compared with the printing screen 100, the printing surface 14 of the printing screen 200 is concavely provided with a micro-nano structure 51, and the micro-nano structure 51 is distributed in a grid texture. Preferably, the depth range of the grid texture is 3μm-25μm, the average pore size of the grid is 10μm-200μm, and the width range of the mesh line is 5μm-150μm. The grid texture on the printing surface 14 can effectively control the scraper, improve the scraping quality, control the amount of ink, and increase the printing quality. Furthermore, the grid line 32 is defined as extending along the Y direction, and the printing direction is defined as the X direction, wherein the X direction is cross-set with the Y direction; the direction in which part of the micro-nano structure 51 extends is at an angle to the X direction, and the angle range is 5°-85°, so that the micro-nano structure 51 plays a role in the control effect of the scraper. The micro-nano structure 51 is concave from the printing surface, and its depth can be less than or equal to the thickness of the first metal layer 1. In other embodiments, the micro-nano structure 51 can be convexly arranged, and photoresist embossing glue or the like is coated on the printing surface 14 and the micro-nano structure 51 convexly arranged on the printing surface 14 is formed, which can also achieve the purpose of controlling the scraper, and further control the amount of ink, thereby improving the printing quality. Figure 8 The side walls and bottom surface 24 of the grid line 32 are both provided with a surface energy layer 45, which can improve the surface energy of the side walls and bottom surface 24 of the grid line 32 and improve the ink receiving property and the printing screen quality. Fig. 9 An AG structure 511 is arranged on the grid texture, the height range of the AG structure 511 is 10nm-5μm, and the width range of the AG structure 511 is 50nm-50μm, which can effectively control the scraper, improve the scraping quality, control the amount of ink, and increase the printing quality.

[0047] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail above in conjunction with the accompanying drawings. In the above description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described above, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed above. In addition, the various technical features of the above-mentioned embodiments can be combined arbitrarily. In order to make the description concise, all possible combinations of the various technical features in the above-mentioned embodiments are not described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0048] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the present application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the attached claims.

Claims

1. A printing screen, characterized in that: It includes: A first metal layer, comprising a first wire groove arranged through, a printing surface and a first matching surface arranged opposite to each other; The second metal layer comprises a second wire groove provided through the second wire groove, a bottom surface and a second mating surface provided opposite to each other, wherein the first metal layer and the second metal layer are stacked by matching the first mating surface and the second mating surface; A gate line, wherein the first line groove and the second line groove are arranged correspondingly and are interconnected to form the gate line; Wherein, a surface energy layer is arranged on the side wall of the second wire groove.

2. The printing screen according to claim 1, characterized in that: The surface energy layer is a coating or a plating layer.

3. The printing screen according to claim 2, characterized in that: The coating layer is a fluorine-containing layer, and the plating layer is an electroplated metal layer.

4. The printing screen according to claim 1, characterized in that: A surface energy layer is provided on the side wall of the first wire trough, and the surface energy layer is a coating or a plating layer.

5. The printing screen according to claim 1, characterized in that: The opening width of the second wire groove close to the first wire groove is smaller than or equal to the opening width away from the first wire groove.

6. The printing screen according to claim 5, characterized in that: The side wall of the second wire trough is inclined, and the inclination angle is greater than 0 degree and less than or equal to 45 degrees.

7. The printing screen according to claim 1, characterized in that: The printing surface and / or the bottom surface is provided with a surface energy layer, and the surface energy layer is a coating or a plating layer.

8. The printing screen according to claim 1, characterized in that: The printing surface is provided with a micro-nano structure with protrusions and / or depressions, and the micro-nano structure is a grid texture, an AG texture or a brushed texture.

9. The printing screen according to claim 8, characterized in that: The thickness range of the grid texture is 3μm-25μm or the depth range is 3μm-25μm, the average pore size of the grid of the grid texture is 10μm-200μm, and the width range of the mesh line is 5μm-150μm; the thickness of the AG texture does not exceed 25μm or the depth does not exceed 25μm, and the width range of the AG texture is 5μm-150μm; the thickness range of the brushed texture is 3μm-25μm or the depth range is 3μm-25μm, and the width range of the brushed texture is 5μm-150μm.

10. The printing screen according to claim 8, characterized in that: An AG structure is provided on the micro-nano structure, the height of the AG structure is in the range of 10 nm-5 μm, and the width of the AG structure is in the range of 50 nm-50 μm.

Citation Information

Cited By

  • Screen printing plate

    CN120245586A

  • Screen printing plate and manufacturing method thereof

    CN120902419A

  • Printing plate and preparation method thereof

    CN121224281A

  • Printing screen

    WO2025140378A1