Platinum channel and glass substrate production system
By using the lifting section and clarification section stacked with refractory bricks, and setting up staggered baffles and exhaust channels in the clarification section, the problem of material leakage and collapse of the platinum channel at high temperatures has been solved, the clarification effect has been improved, and the service life has been extended. It also reduces production costs and ensures the quality of the glass substrate.
Patent Information
- Application Number
- CN202420284569.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-06
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-02-06
AI Technical Summary
The existing platinum channels have low strength at high temperatures and are prone to material leakage and collapse, and the clarification section cannot meet the glass liquid clarification requirements in large-scale glass substrate production, resulting in glass substrate quality problems.
The lifting section and the clarification section are made of refractory bricks. The upper and lower baffles are staggered to form an S-shaped channel to improve the structural strength and load-bearing capacity. An exhaust channel and a temperature sensor are installed in the clarification section.
It extends the service life of the platinum channel, reduces production costs, improves the clarification effect and the discharge of bubbles in the glass liquid, and ensures the uniformity and light transmittance of the glass substrate.
Smart Images

Figure CN221854455U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of glass substrate production systems, in particular to a platinum channel and a glass substrate production system. Background Art
[0002] During the production process of glass substrates, the batch materials need to be melted at high temperature in a kiln to form molten glass. The molten glass then passes through the lifting section, clarification section, cooling section and stirring section in the platinum channel to provide qualified and high-quality molten glass to the next process.
[0003] At present, the platinum channel is made of platinum material (mostly platinum-rhodium alloy). After the glass liquid is heated in the lifting section, the temperature in the clarification section is relatively high (generally greater than 1630°C). The strength of the platinum channel is low at high temperatures, and the carrying capacity decreases accordingly. It is prone to safety hazards such as leakage and collapse, resulting in a shorter service life of the platinum channel and increased production costs. Moreover, the main function of the clarification section is to discharge visible bubbles in the glass liquid. With the increasing use of large-generation glass substrates, the flow rate of the glass liquid has increased significantly. The existing clarification section can no longer meet the clarification requirements of the glass liquid, making the bubble defects in the glass substrate particularly obvious, seriously affecting the quality of the glass substrate, such as uniformity and light transmittance. Utility Model Content
[0004] One purpose of the utility model is to provide a platinum channel to improve the bearing capacity of the platinum channel, avoid leakage and collapse of the lifting section and the clarification section, extend the service life of the platinum channel, reduce production costs, and improve the clarification effect of the clarification section.
[0005] Another object of the utility model is to provide a glass substrate production system to improve the bearing capacity of the platinum channel, avoid leakage and collapse of the lifting section and the clarification section, extend the service life of the platinum channel, reduce production costs, and improve the clarification effect of the clarification section.
[0006] To achieve this purpose, the technical solution adopted by the utility model is:
[0007] The platinum channel comprises a lifting section and a clarification section which are made of refractory bricks, wherein the lifting section has a lifting channel, and the clarification section has a clarification channel, wherein one end of the lifting channel can be connected to the outlet of the kiln, and the other end of the lifting channel is connected to the clarification channel;
[0008] An upper baffle is disposed on the inner top wall of the clarification channel, a lower baffle is disposed on the inner bottom wall of the clarification channel, and the upper baffle and the lower baffle are staggered so that the clarification channel forms an S-shaped channel.
[0009] As a preferred solution for the platinum channel, the upper baffle plate and the lower baffle plate are both formed by stacking the refractory bricks, and the upper baffle plate, the lower baffle plate and the clarification section are integrally formed.
[0010] As a preferred solution of the platinum channel, at least two upper baffles are arranged at intervals on the inner top wall of the clarification channel along the flow direction of the glass liquid, and at least two lower baffles are arranged at intervals on the inner bottom wall of the clarification channel along the flow direction of the glass liquid.
[0011] As a preferred solution for the platinum channel, the distance L between adjacent upper baffles and lower baffles is 50 cm to 80 cm.
[0012] As a preferred solution for the platinum channel, the distance between the upper baffle and the inner bottom wall of the clarification channel is H1, the distance between the lower baffle and the inner top wall of the clarification channel is H2, H1=H2, and H1 and H2 are both 30cm to 50cm.
[0013] As a preferred solution of the platinum channel, the clarification section is provided with an exhaust channel, and the exhaust channel is communicated with the clarification channel.
[0014] As a preferred embodiment of the platinum channel, the platinum channel further comprises a cooling section, a stirring section, a feeding section and a discharge port which are connected in sequence, the cooling section, the stirring section, the feeding section and the discharge port are all made of platinum material, and the front end of the cooling section along the flow direction of the glass liquid is connected to the clarification section.
[0015] As a preferred embodiment of the platinum channel, the platinum channel further includes a temperature sensor, which is arranged in the lifting section to detect the temperature of the glass liquid flowing through the lifting channel; the temperature sensor is arranged in the clarification section to detect the temperature of the glass liquid flowing through the clarification channel.
[0016] As a preferred solution of the platinum channel, the clarification section is provided with an observation window, so as to observe the glass liquid flowing through the clarification channel through the observation window.
[0017] A glass substrate production system comprises a kiln and the above-mentioned platinum channel, wherein the outlet of the kiln is communicated with the lifting channel of the platinum channel.
[0018] The beneficial effects of the utility model are:
[0019] In the platinum channel proposed by the utility model, the lifting section and the clarifying section are both made of refractory bricks, which improves the structural strength and bearing capacity of the lifting section and the clarifying section, avoids leakage and collapse of the lifting section and the clarifying section when high-temperature glass liquid flows through, prolongs the service life of the platinum channel, and reduces the production cost of the glass substrate. At the same time, the upper baffle plate and the lower baffle plate with staggered distribution are arranged in the clarifying channel, so that the clarifying channel forms an S-shaped channel, which not only prolongs the flow path of the glass liquid in the clarifying section and increases the discharge amount of bubbles in the glass liquid, but also the glass liquid can discharge bubbles faster when flowing through the upper baffle plate and the lower baffle plate, thereby improving the clarification effect of the clarifying section.
[0020] The production system of glass substrates proposed by the utility model includes the above-mentioned platinum channel, and the lifting section and the clarification section are both made of refractory bricks, which improves the structural strength and bearing capacity of the lifting section and the clarification section, avoids leakage and collapse of the lifting section and the clarification section when high-temperature glass liquid flows through, prolongs the service life of the platinum channel, and reduces the production cost of the glass substrate. At the same time, the upper baffle plate and the lower baffle plate with staggered distribution are arranged in the clarification channel, so that the clarification channel forms an S-shaped channel, which not only prolongs the flow path of the glass liquid in the clarification section and increases the discharge amount of bubbles in the glass liquid, but also the glass liquid can discharge bubbles faster when flowing through the upper baffle plate and the lower baffle plate, thereby improving the clarification effect of the clarification section. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic diagram of the structural distribution of a glass substrate production system provided by an embodiment of the utility model;
[0022] Figure 2 It is a schematic diagram of the structure of the platinum channel provided in an embodiment of the utility model.
[0023] The names and numbers of the components in the figure are as follows:
[0024] 10. Kiln;
[0025] 1. Lifting section; 11. Lifting channel; 2. Clarifying section; 21. Clarifying channel; 22. Upper baffle; 23. Lower baffle; 24. Exhaust channel; 3. Cooling section; 4. Stirring section; 5. Feeding section; 6. Discharging port. DETAILED DESCRIPTION
[0026] In order to make the technical problems solved by the present invention, the technical solutions adopted and the technical effects achieved clearer, the technical solutions of the present invention are further described below in conjunction with the accompanying drawings and through specific implementation methods. It is understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for the convenience of description, only the parts related to the present invention are shown in the accompanying drawings, rather than all of them.
[0027] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0028] In the present utility model, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0029] In the description of this embodiment, the terms "upper", "lower", "right", "left" and other directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplified operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation of the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.
[0030] The technical solution of the utility model is further explained below with reference to the accompanying drawings and through specific implementation methods.
[0031] like Figure 1 As shown, this embodiment provides a glass substrate production system, including a furnace 10 and a platinum channel, wherein the platinum channel includes a lifting section 1, a clarifying section 2, a cooling section 3, a stirring section 4, a feeding section 5 and a discharge port 6 which are connected in sequence. The outlet of the furnace 10 is connected to the lifting channel 11, so that the glass liquid in the furnace 10 flows into the lifting section 1, the clarifying section 2, the cooling section 3, the stirring section 4, and the feeding section 5 in sequence along the direction indicated by the arrow in the figure (i.e., the flow direction of the glass liquid), and finally flows out from the discharge port 6 to provide qualified glass liquid to the next process.
[0032] Specifically, the lifting section 1 is tilted upward so that the glass liquid in the kiln 10 located at a lower position enters the clarification section 2 located at a higher position. At the same time, the lifting section 1 can also heat the glass liquid to further increase the temperature of the glass liquid and ensure that the glass liquid has a better clarification effect in the clarification section 2. The glass liquid discharges internal bubbles in the clarification section 2 to complete the clarification process of the glass liquid. Then the glass liquid enters the stirring section 4 after being cooled in the cooling section 3. In the stirring section 4, the homogenization process of the glass liquid is completed after being stirred by the stirring rod. Finally, the glass liquid flows into the feeding section 5 and flows to the next process from the discharge port 6. Since the processes of clarification, cooling, stirring, etc. of the glass liquid in the platinum channel are all existing technologies, they will not be repeated here.
[0033] The existing platinum channels are all made of platinum materials. The temperature of the glass liquid is high after it is heated by the lifting section. The strength of the platinum channel is low at high temperatures, and the carrying capacity decreases accordingly. It is easy to have safety hazards such as leakage and collapse, resulting in a short service life of the platinum channel and increased production costs. In addition, the main function of the clarification section is to discharge the visible bubbles in the glass liquid. With the increasing use of large-generation glass substrates, the flow rate of the glass liquid has increased significantly. The existing clarification section can no longer meet the clarification requirements of the glass liquid, making the bubble defects in the glass substrate particularly obvious, seriously affecting the uniformity and light transmittance of the glass substrate.
[0034] To solve the above problems, Figure 1 and Figure 2 As shown, this embodiment also proposes a platinum channel, which includes a lifting section 1 and a clarification section 2 made of refractory bricks, a lifting channel 11 in the lifting section 1, and a clarification channel 21 in the clarification section 2, one end of the lifting channel 11 can be connected to the outlet of the kiln 10, and the other end of the lifting channel 11 is connected to the clarification channel 21. An upper baffle 22 is provided on the inner top wall of the clarification channel 21, and a lower baffle 23 is provided on the inner bottom wall of the clarification channel 21, and the upper baffle 22 and the lower baffle 23 are staggered so that the clarification channel 21 forms an S-shaped channel. It should be noted that the cooling section 3, the stirring section 4, the feeding section 5 and the discharge port 6 are all made of platinum material, and the front end of the cooling section 3 along the flow direction of the glass liquid is connected to the clarification section 2.
[0035] In this embodiment, the lifting section 1 and the clarifying section 2 are both made of refractory bricks, which improves the structural strength and bearing capacity of the lifting section 1 and the clarifying section 2, avoids leakage and collapse of the lifting section 1 and the clarifying section 2 when high-temperature glass liquid flows through, prolongs the service life of the platinum channel, and reduces the production cost of the glass substrate. At the same time, the upper baffle 22 and the lower baffle 23 are arranged in a staggered distribution in the clarifying channel 21, so that the clarifying channel 21 forms an S-shaped channel, which not only prolongs the flow path of the glass liquid in the clarifying section 2, increases the discharge amount of bubbles in the glass liquid, but also enables the glass liquid to discharge bubbles faster when flowing through the upper baffle 22 and the lower baffle 23, thereby improving the clarification effect of the clarifying section 2.
[0036] Specifically, the upper baffle 22 and the lower baffle 23 are both formed by stacking refractory bricks, and the upper baffle 22, the lower baffle 23 and the clarification section 2 are integrally formed. The clarification section 2, the upper baffle 22 and the lower baffle 23 are integrally stacked by refractory bricks, which improves the structural strength and stability of the upper baffle 22, the lower baffle 23 and the clarification section 2, and also improves the stacking efficiency of the clarification section 2.
[0037] like Figure 2 As shown, at least two upper baffles 22 are arranged at intervals on the inner top wall of the clarification channel 21 along the flow direction of the glass liquid, and at least two lower baffles 23 are arranged at intervals on the inner bottom wall of the clarification channel 21 along the flow direction of the glass liquid. The flow path and residence time of the glass liquid in the clarification channel 21 are extended by multiple staggered upper baffles 22 and lower baffles 23, which is conducive to the discharge of bubbles in the glass liquid and improves the clarification efficiency. The number of upper baffles 22 and lower baffles 23 can be flexibly adjusted according to the size of the clarification channel 21, and is not specifically limited here.
[0038] like Figure 2 As shown, the spacing L between the adjacent upper baffles 22 and lower baffles 23 is 50 cm to 80 cm. The spacing L can be 50 cm, 60 cm, 70 cm or 80 cm, etc., to ensure that the flow rate of the glass liquid is within an appropriate range. When the spacing L is too small (less than 50 cm), the channel between the adjacent upper baffles 22 and lower baffles 23 is small, which makes the flow rate of the glass liquid small, reduces the rate of the glass liquid passing through the platinum channel, and is not conducive to improving the production efficiency of the glass substrate. When the spacing L is too large (greater than 80 cm), the channel between the adjacent upper baffles 22 and lower baffles 23 is large, which makes the flow rate of the glass liquid large, reduces the discharge amount of bubbles in the glass liquid, and is not conducive to improving the clarification efficiency.
[0039] like Figure 2As shown, the distance between the upper baffle plate 22 and the inner bottom wall of the clarifying channel 21 is H1, and the distance between the lower baffle plate 23 and the inner top wall of the clarifying channel 21 is H2, H1=H2, and H1 and H2 are both 30cm to 50cm. The distances H1 and H2 can be 30cm, 40cm or 50cm, etc., to ensure that the flow rate of the glass liquid is within an appropriate range. When the distances H1 and H2 are too small (less than 30cm), the channel between the upper baffle plate 22 and the inner bottom wall of the clarifying channel 21 and the channel between the lower baffle plate 23 and the inner top wall of the clarifying channel 21 are both small, resulting in a small flow rate of the glass liquid, which reduces the rate at which the glass liquid passes through the platinum channel, and is not conducive to improving the production efficiency of the glass substrate. When the spacings H1 and H2 are too large (greater than 50 cm), the channel between the upper baffle plate 22 and the inner bottom wall of the clarification channel 21 and the channel between the lower baffle plate 23 and the inner top wall of the clarification channel 21 are both larger, resulting in a larger flow rate of the molten glass, which reduces the discharge amount of bubbles in the molten glass and is not conducive to improving the clarification efficiency.
[0040] like Figure 2 As shown, the clarification section 2 is provided with an exhaust channel 24, which is connected to the clarification channel 21, so that the gas discharged from the molten glass in the clarification section 2 is discharged through the exhaust channel 24. It can be understood that the exhaust channel 24 is surrounded by refractory bricks stacked on the clarification section 2, and no additional pipeline is required, which reduces the cost of the platinum channel.
[0041] In an optional embodiment, a temperature sensor is provided in the lifting section 1 to detect the temperature of the glass liquid flowing through the lifting channel 11. A temperature sensor is provided in the clarification section 2 to detect the temperature of the glass liquid flowing through the clarification channel 21. The two temperature sensors can respectively monitor the temperature of the glass liquid in the lifting section 1 and the clarification section 2 in real time to ensure that the temperature of the glass liquid is maintained within a set temperature range.
[0042] In an optional embodiment, the clarification section 2 is provided with an observation window, through which the glass liquid flowing through the clarification channel 21 can be observed. The staff can visually check the bubble discharge of the glass liquid in the clarification channel 21 through the observation window, thereby realizing intuitive monitoring of the glass liquid passing through the clarification section 2.
[0043] The above embodiments are only to illustrate the basic principles and characteristics of the present invention. The present invention is not limited by the above embodiments. Without departing from the spirit and scope of the present invention, the present invention may be subject to various changes and modifications, which are within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. Platinum channel, characterized in that, The invention comprises a lifting section (1) and a clarifying section (2) which are stacked with refractory bricks, wherein the lifting section (1) has a lifting channel (11), and the clarifying section (2) has a clarifying channel (21), one end of the lifting channel (11) can be connected to the outlet of the kiln (10), and the other end of the lifting channel (11) is connected to the clarifying channel (21); An upper baffle (22) is provided on the inner top wall of the clarification channel (21), and a lower baffle (23) is provided on the inner bottom wall of the clarification channel (21), and the upper baffle (22) and the lower baffle (23) are arranged in a staggered manner so that the clarification channel (21) forms an S-shaped channel.
2. The platinum channel according to claim 1, characterized in that: The upper baffle plate (22) and the lower baffle plate (23) are both formed by stacking the refractory bricks, and the upper baffle plate (22), the lower baffle plate (23) and the clarification section (2) are integrally formed.
3. The platinum channel according to claim 1, characterized in that: At least two upper baffles (22) are arranged at intervals on the inner top wall of the clarification channel (21) along the flow direction of the glass liquid, and at least two lower baffles (23) are arranged at intervals on the inner bottom wall of the clarification channel (21) along the flow direction of the glass liquid.
4. The platinum channel according to claim 1, characterized in that: The distance L between the adjacent upper baffles (22) and lower baffles (23) is 50 cm to 80 cm.
5. The platinum channel according to claim 1, characterized in that: The distance between the upper baffle plate (22) and the inner bottom wall of the clarification channel (21) is H1, and the distance between the lower baffle plate (23) and the inner top wall of the clarification channel (21) is H2, H1=H2, and H1 and H2 are both 30cm to 50cm.
6. The platinum channel according to claim 1, characterized in that: The clarification section (2) is provided with an exhaust channel (24), and the exhaust channel (24) is communicated with the clarification channel (21).
7. The platinum channel according to claim 1, characterized in that: The platinum channel further comprises a cooling section (3), a stirring section (4), a feeding section (5) and a discharge port (6) which are connected in sequence; the cooling section (3), the stirring section (4), the feeding section (5) and the discharge port (6) are all made of platinum material, and the front end of the cooling section (3) along the flow direction of the glass liquid is connected to the clarification section (2).
8. The platinum channel according to claim 1, characterized in that: The platinum channel also includes a temperature sensor, the temperature sensor being arranged in the lifting section (1) to detect the temperature of the glass liquid flowing through the lifting channel (11); the temperature sensor being arranged in the clarification section (2) to detect the temperature of the glass liquid flowing through the clarification channel (21).
9. The platinum channel according to claim 1, characterized in that: The clarification section (2) is provided with an observation window, so that the glass liquid flowing through the clarification channel (21) can be observed through the observation window.
10. A glass substrate production system, characterized in that: It comprises a kiln (10) and a platinum channel according to any one of claims 1 to 9, wherein the outlet of the kiln (10) is connected to a lifting channel (11) of the platinum channel.
Citation Information
Cited By
Platinum channel structure and method for quickly clarifying molten glass in production of substrate glass for ultra-wide OLED (Organic Light Emitting Diode) display