Planar gate silicon carbide MOSFET with low source contact resistance
By using metal silicide layers of nickel aluminum and silicon in silicon carbide MOSFETs, combined with specific process steps and ratios, the source contact resistivity is reduced, solving the problem of high resistivity in traditional processes, and achieving low power consumption and Highly efficient silicon carbide MOSFET.
Patent Information
- Application Number
- CN202420175990.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-24
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-01-24
AI Technical Summary
In the traditional silicon carbide ohmic contact process, the resistivity of the contact between single crystal silicon carbide and metal is relatively large, resulting in high source ohmic contact resistivity, which increases the power consumption of the power device.
Using a metal silicide layer of nickel aluminum and silicon, the source contact resistivity is reduced by forming an ohmic contact with low resistivity, combined with a specific metal atomic number ratio and a high-temperature annealing process.
A low-resistance source ohmic contact is achieved, which reduces the on-resistance of silicon carbide MOSFET, reduces the loop power consumption of the device, and effectively avoids electromigration problems.
Smart Images

Figure CN221861582U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a planar gate silicon carbide MOSFET with low source contact resistance. Background Art
[0002] As a typical representative of the third generation of semiconductors, SiC MOSFET has been widely used in the market. Under the condition of unchanged withstand voltage, the reduction of on-resistance is the eternal pursuit of power devices. This is because the greater the on-resistance of the power device, the greater the power consumption in the power circuit. Under high current application conditions, such as 100A freewheeling current, for every 1mΩ increase in on-resistance, the power consumption will increase by 10W, which is particularly critical to improving the efficiency of the power supply system.
[0003] Traditional silicon carbide ohmic contact processes all use highly doped single-crystal silicon carbide to contact metals. Since single-crystal silicon carbide and metals have different material properties, their resistivity is relatively large. Therefore, it is urgent to provide a device that can reduce the resistivity of the source ohmic contact. Utility Model Content
[0004] The technical problem to be solved by the utility model is to provide a planar gate silicon carbide MOSFET with low source contact resistance, thereby reducing the on-resistance of the silicon carbide MOSFET and reducing the loop power consumption of the device.
[0005] The utility model is implemented as follows: a planar gate silicon carbide MOSFET with low source contact resistance, comprising:
[0006] A silicon carbide substrate,
[0007] a drift layer, the drift layer being disposed on the upper side of the silicon carbide substrate;
[0008] a well region, the well region being disposed on the drift layer, and a source region being disposed on the well region;
[0009] a metal silicide layer, the metal silicide layer being disposed on the source region;
[0010] an insulating layer connected to the drift layer;
[0011] a source metal layer, the source metal layer connected to the metal silicide layer;
[0012] a gate metal layer connected to the insulating layer;
[0013] and a drain metal layer connected to the lower side of the silicon carbide substrate.
[0014] Furthermore, the metal silicide layer is a metal silicide of nickel, aluminum and silicon; the thickness of the metal silicide layer is 30-80nm.
[0015] Furthermore, the ratio of the number of metal atoms to the number of silicon atoms in the metal silicide layer is 1:1.
[0016] The utility model has the following advantages: by forming a metal silicide layer, the metal silicide has a small on-resistance, and the contact resistance between the metal silicide and the source metal layer is low, which is 0.1×10 -8 ~1×10 -8 Ωcm 2 Since the material structure of metal silicide and doped single crystal silicon is similar and there is no structural difference, an ohmic contact is formed with a resistivity of 0.1×10 -7 ~1×10 -7 Ωcm 2 (The resistivity of the existing ohmic contact is generally 0.1×10 -6 ~1×10 -6 Ωcm2), forming a low-resistance source ohmic contact as a whole. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The present invention will be further described below in conjunction with the embodiments with reference to the accompanying drawings.
[0018] Figure 1 The utility model is a schematic diagram of a planar gate silicon carbide MOSFET with low source contact resistance.
[0019] Figure 2 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET with low source contact resistance according to the utility model. Figure 1 .
[0020] Figure 3 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET with low source contact resistance according to the utility model. Figure 2 .
[0021] Figure 4 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET with low source contact resistance according to the utility model. Figure 3 .
[0022] Figure 5 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET with low source contact resistance according to the utility model. Figure 4 .
[0023] Figure 6 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET with low source contact resistance according to the utility model. Figure 5 .
[0024] Figure 7 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET with low source contact resistance according to the utility model. Figure 6 .
[0025] Figure 8 This is a cross-sectional view of the process of a planar gate silicon carbide MOSFET with low source contact resistance according to the utility model. Figure 7 . DETAILED DESCRIPTION
[0026] like Figure 1 As shown, a planar gate silicon carbide MOSFET with low source contact resistance comprises:
[0027] A silicon carbide substrate 1,
[0028] a drift layer 2, wherein the drift layer 2 is disposed on the upper side of the silicon carbide substrate 1;
[0029] a well region 3, wherein the well region 3 is disposed on the drift layer 2, and a source region 31 is disposed on the well region 3;
[0030] a metal silicide layer 4, wherein the metal silicide layer 4 is disposed on the source region 31;
[0031] an insulating layer 5, wherein the insulating layer 5 is connected to the drift layer 2;
[0032] a source metal layer 6, wherein the source metal layer 6 is connected to the metal silicide layer 4;
[0033] a gate metal layer 7, wherein the gate metal layer 7 is connected to the insulating layer 5;
[0034] and a drain metal layer 8 , wherein the drain metal layer 8 is connected to the lower side of the silicon carbide substrate 1 .
[0035] The metal silicide layer 4 is a metal silicide of nickel, aluminum and silicon; the resistivity of the contact resistance between the metal silicide layer 4 and the source metal layer 6 is low, which is 0.1×10 -8 ~1×10 -8 Ωcm 2 Since the material structure of metal silicide and doped single crystal silicon is similar and there is no structural difference, an ohmic contact is formed, that is, the resistivity of the ohmic contact between the metal silicide layer 4 and the source region 31 is 0.1×10 -7 ~1×10 -7 Ωcm 2 (The resistivity of the existing ohmic contact is generally 0.1×10 -6 ~1×10 -6 Ωcm2), so during the conduction process, the whole constitutes a low-resistance source ohmic contact.
[0036] Existing metal silicides are formed using aluminum and silicon, which are prone to electromigration under high current application conditions, leading to device failure. Therefore, metal silicides are not used in power devices to reduce source contact resistance. The utility model uses metal silicides of nickel aluminum and silicon, which can effectively solve the electromigration problem; and the metal silicides of nickel aluminum and silicon and the corresponding ratio range are designed to ensure silicide formation and low resistivity and inhibit electromigration.
[0037] like Figures 1 to 8 As shown, the manufacturing method of the above-mentioned silicon carbide MOSFET includes:
[0038] Step 1: Take a silicon carbide substrate 1 provided with a drift layer 2, form a barrier layer a on the drift layer 2, etch the barrier layer a to form a through hole, and perform ion implantation into the drift layer 2 through the through hole to form a well region 3;
[0039] Step 2, re-forming the barrier layer a, etching the barrier layer a to form a through hole, and performing ion implantation into the well region 3 through the through hole to form a source region 31;
[0040] Step 3, re-forming the barrier layer a, etching the barrier layer a to form a deposition window a1, depositing highly doped polysilicon to form a polysilicon layer b;
[0041] Step 4, re-forming the barrier layer a, and etching the source metal region a2 of the barrier layer a, first depositing aluminum, then depositing nickel, then depositing aluminum, and finally depositing nickel on the source metal region a2 to complete the source metal deposition, and controlling the composition ratio of aluminum and nickel through the four-step deposition method, and achieving uniform distribution of aluminum and nickel;
[0042] Step 5, performing high temperature annealing at a temperature of 800-1000° C. for 2-3 minutes to form a metal silicide layer 4 and a source metal layer 6 respectively;
[0043] Step 6, re-forming the barrier layer a, and etching the barrier layer a to form a through hole, and depositing the insulating layer 5 through the through hole;
[0044] Step 7, re-forming the barrier layer a, etching the gate metal region a3 of the barrier layer a, depositing gate metal through the gate metal region a3 to form a gate metal layer 7, and removing the barrier layer a;
[0045] Step 8: depositing metal on the other side of the silicon carbide substrate 1 to form a drain metal layer 8.
[0046] The atomic number ratio of nickel and aluminum is: 2:8 to 4:5; this metal ratio can effectively be compatible with the aluminum gate process, while ensuring the metal strength and the subsequent metal silicide strength; the ratio of the number of metal atoms to the number of silicon atoms in the metal silicide layer 4 is 1:1, which can ensure the conductivity of the metal silicide and at the same time ensure the adhesion with the Si material and metal; the mass ratio under the same atomic number conditions can be calculated based on the molar mass of the material; nickel 58.6934g / mol, aluminum 26.9815g / mol, silicon 28g / mol; mol refers to the atomic number. Calculate the atomic number of 1kg of material based on the molar mass, determine the mass of the deposited aluminum and nickel based on the atomic number, and determine the ratio of the metal atomic number to the silicon atomic number.
[0047] Metal silicide Ni x Al 1-x Si, x is between 0 and 1. A metal silicide is formed by annealing the first layer of aluminum and the first layer of nickel with polysilicon under high temperature conditions. The upper two layers have no contact with SiC, and an alloy is formed.
[0048] The thickness of the polysilicon layer b is 50-100 nm; the doping concentration of the highly doped polysilicon is 1×10 20 cm -3 ~6×10 20 cm -3 . The thickness of the polysilicon b is set to achieve the transition from Si material to metal silicide and then to metal, to ensure low resistivity, high adhesion, and strong material connectivity. This thickness is directly related to the metal silicide thickness set to 30-80nm. When the thickness of the polysilicon layer b is 20nm more than the thickness of the metal silicide layer 4, the connectivity and adhesion with the device structure can be guaranteed. The doping concentration of polysilicon is set to achieve the low resistivity of the polysilicon material. During the annealing reaction, the polysilicon layer b is completely metal silicided. The low resistivity of the polysilicon material reduces the resistivity of the generated metal silicide.
[0049] The doping concentration of the source region 31 is 6×10 18 cm -3 ~1.2×10 19 cm -3 The doping concentration of the well region 3 is 1×10 17 cm -3 ~2×10 17 cm -3 The doping concentration of the drift region 2 is 1×10 16 cm -3 ~2×10 16 cm -3The doping concentration of the source region 31 is to reduce the contact resistance between the source region 31 and the metal silicide layer 4. If the doping concentration of the source region 31 is too high, the source region material is easily damaged by ion implantation, causing the single crystal to become polycrystalline, and the device fails. The well region is used to realize the pn junction shutdown of the source region and the channel region. If the concentration is too low, the pinch-off region it produces will be too large; if the concentration is too high, the withstand voltage characteristics will be insufficient. The doping concentration of the drift region is a compromise between withstand voltage and on-resistance.
[0050] Although the specific implementation methods of the present invention are described above, those skilled in the art should understand that the specific embodiments described are only illustrative and are not intended to limit the scope of the present invention. Equivalent modifications and changes made by those skilled in the art in accordance with the spirit of the present invention should be included in the scope of protection of the claims of the present invention.
Claims
1. A planar gate silicon carbide MOSFET with low source contact resistance, characterized in that: include: A silicon carbide substrate, a drift layer, the drift layer being disposed on the upper side of the silicon carbide substrate; a well region, the well region being disposed on the drift layer, and a source region being disposed on the well region; a metal silicide layer, the metal silicide layer being disposed on the source region; an insulating layer connected to the drift layer; a source metal layer, the source metal layer connected to the metal silicide layer; a gate metal layer connected to the insulating layer; and a drain metal layer connected to the lower side of the silicon carbide substrate.
2. A planar gate silicon carbide MOSFET with low source contact resistance according to claim 1, characterized in that: The thickness of the metal silicide layer is 30-80 nm.