Silicon heterojunction solar cell
By electroplating copper instead of screen printing silver, forming copper grid lines and setting an anti-oxidation metal layer on the silicon plate, the problem of high cost and carrier interface recombination of silicon heterojunction solar cells is solved, and efficiency improvement and cost reduction are achieved.
Patent Information
- Application Number
- CN202322840760.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-23
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2033-10-23
AI Technical Summary
Existing silicon heterojunction solar cells use low-temperature silver paste, which results in high costs and difficulty in large-scale mass production. Moreover, the recombination problem of carriers at the amorphous silicon/crystalline silicon interface affects the cell efficiency.
Electroplated copper is used instead of screen-printed silver to form copper grid lines to reduce metallization costs. An anti-oxidation metal layer is set on the silicon plate to improve adhesion and service life, while the amorphous silicon film is optimized to improve cell efficiency.
It effectively reduces the cost of gate line metallization, improves battery efficiency and service life, avoids the problem of uneven plating and film sandwiching, and improves light absorption efficiency.
Smart Images

Figure CN221885124U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of silicon heterojunction solar cells, in particular to a silicon heterojunction solar cell. Background Art
[0002] An important reason for the high efficiency of silicon heterojunction cells is that the excellent passivation effect of the intrinsic amorphous silicon film on the surface of the crystalline silicon substrate ensures the high open circuit voltage of the cell; the passivation effect of the intrinsic amorphous silicon film on the crystalline silicon surface is closely related to the thin film deposition process. The thin film deposition process is optimized to reduce the recombination of carriers at the amorphous silicon / crystalline silicon interface and improve the interface passivation ability, thereby increasing the cell open circuit voltage; however, the cost of heterojunction solar cells has remained high due to the use of low-temperature silver paste on the front and back sides, making it difficult to further mass-produce them.
[0003] Therefore, how to design a single-crystal silicon heterojunction solar cell that can solve the above-mentioned technical problems has become a technical problem that needs to be solved urgently. Utility Model Content
[0004] The utility model aims to solve at least one of the technical problems existing in the prior art. To this end, the utility model proposes a silicon heterojunction solar cell.
[0005] A silicon heterojunction solar cell according to an embodiment of the first aspect of the utility model, a silicon plate with a first surface and a second surface, wherein the first surface of the silicon plate is sequentially stacked with a first amorphous silicon layer, a first ITO layer, a first metal seed layer, and a first gate line layer;
[0006] The second surface of the silicon plate is sequentially stacked with a second amorphous silicon layer, a second ITO layer, a second metal seed layer, and a second gate line layer;
[0007] The first gate line layer and the second gate line layer each include at least one main gate and at least one auxiliary gate, any one of the main gates is perpendicular to any one of the auxiliary gates, and an anti-oxidation metal layer is disposed on the surfaces of the main gates and the auxiliary gates.
[0008] According to a silicon heterojunction solar cell of the utility model, the first amorphous silicon layer and the second amorphous silicon layer are used for passivation of the silicon plate, the first ITO layer and the second ITO layer are used for anti-reflection and lateral electron transmission, the first metal seed layer and the second metal seed layer are used for preparing for electroplating grid lines, and the first grid line layer and the second grid line layer are used for conduction;
[0009] Electroplated copper replaces screen-printed silver to reduce the cost of grid line metallization. At the same time, the resistivity of electroplated copper is only 30% of that of silver grid, and the grid line width can be 40% of that of silver grid, which increases the light-receiving area and greatly improves the battery efficiency. Compared with conventional copper grid electrodes, the copper grid of the present application has better height uniformity, does not have the problem of uneven electroplating and film sandwiching, and the grid line adhesion can meet the tension and reliability tests. At the same time, it is easier to achieve ink protection on the side of the battery to avoid battery short circuit caused by metal electroplating on the side of the battery. The anti-oxidation metal layer on the surface of the grid line can increase the service life of the battery. In addition, the back of the battery cell is polished, which is more conducive to light absorption and is conducive to the optimization of the amorphous silicon film on the back, thereby improving the conversion efficiency of the battery cell.
[0010] According to some embodiments of the present invention, the first amorphous silicon layer includes a first intrinsic amorphous silicon layer and a first amorphous silicon sublayer, the first amorphous silicon sublayer is arranged at an end of the first intrinsic amorphous silicon layer away from the silicon plate, the first and second amorphous silicon layers include a second intrinsic amorphous silicon layer and a second amorphous silicon sublayer, and the second amorphous silicon sublayer is arranged at an end of the second intrinsic amorphous silicon layer away from the silicon plate.
[0011] According to some embodiments of the present invention, the thickness of the ITO layer is 40nm-200nm.
[0012] According to some embodiments of the present invention, the first amorphous silicon sublayer is an n-type amorphous silicon layer, and the second amorphous silicon sublayer is a p-type amorphous silicon layer.
[0013] According to some embodiments of the present invention, the thickness of the first ITO layer and the second ITO layer is 40nm-200nm, and the first metal seed layer and the second metal seed layer both include conductive metals such as copper, nickel, silver, gold, titanium, and aluminum.
[0014] According to some embodiments of the present utility model, the first surface of the silicon plate is a texturing structure, and the second surface of the silicon plate is a polishing structure.
[0015] According to some embodiments of the present invention, the main gate and the secondary gate are both arranged on the main gate groove and the secondary gate groove, the main gate groove width is 50um-100um, and the secondary gate groove width is 5um-50um.
[0016] According to some embodiments of the present invention, the width of the main grid is 40um-100um, and the width of the secondary grid is 5um-50um.
[0017] According to some embodiments of the present invention, the anti-oxidation metal layer has a thickness of 500nm-10000nm.
[0018] According to some embodiments of the present invention, the intrinsic amorphous silicon layer has a thickness of 2nm-20nm, the doped n-type amorphous silicon layer has a thickness of 2nm-20nm, and the doped p-type amorphous silicon layer has a thickness of 2nm-20nm.
[0019] Additional aspects and advantages of the present invention will be given in part in the following description, and in part will become apparent from the following description, or will be learned through the practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0021] Figure 1 This is a schematic diagram of the layer structure of a novel embodiment of the present invention;
[0022] Figure 2 This is a schematic diagram of the panel structure of a new embodiment of the present invention.
[0023] Figure numerals: 11, first amorphous silicon layer; 12, first ITO layer; 13, first metal seed layer; 14, first gate line layer; 21, second amorphous silicon layer; 22, second ITO layer; 23, second metal seed layer; 24, second gate line layer; 3, silicon plate. DETAILED DESCRIPTION
[0024] The embodiments of the present invention are described in detail below. The embodiments described with reference to the accompanying drawings are exemplary. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0025] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be an intermediate element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time.
[0026] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the technical field of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific implementations and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0027] Example 1
[0028] See also Figure 1 As shown, a silicon heterojunction solar cell comprises a silicon plate 3 with a first surface and a second surface, wherein the first surface of the silicon plate 3 is sequentially stacked with a first amorphous silicon layer 11, a first ITO layer 12, a first metal seed layer 13, and a first gate line layer 14;
[0029] The second surface of the silicon plate 3 is sequentially stacked with a second amorphous silicon layer 21, a second ITO layer 22, a second metal seed layer 23, and a second gate line layer 24;
[0030] The first surface of the silicon plate 3 is a velvet structure, and the second surface of the silicon plate 3 is a polished structure; the first gate line layer 14 and the second gate line layer 24 each include at least one main gate and at least one auxiliary gate, any one of the main gates is perpendicular to any one of the auxiliary gates, and an anti-oxidation metal layer is provided on the surface of the main gate and the auxiliary gate; the first amorphous silicon layer 11 includes a first intrinsic amorphous silicon layer and a first amorphous silicon sublayer, and the first amorphous silicon sublayer is arranged at the end of the first intrinsic amorphous silicon layer away from the silicon plate 3, and the second amorphous silicon layer 21 includes a second intrinsic amorphous silicon layer and a second amorphous silicon sublayer, and the second amorphous silicon sublayer is arranged at the end of the second intrinsic amorphous silicon layer away from the silicon plate 3; the first amorphous silicon sublayer is an n-type amorphous silicon layer, and the second amorphous silicon sublayer is a p-type amorphous silicon layer; the first ITO layer 12 and the second IT The thickness of the O layer 22 is 40nm-200nm, and the metal seed layer includes copper, nickel, silver, gold, titanium, and aluminum conductive metals; the thickness of the first metal seed layer 13 and the second metal seed layer 23 is 30nm-1000nm, and the film layer square resistance is 0.1mΩ-10mΩ; the main gate and the secondary gate are both arranged on the main gate groove and the secondary gate groove, the main gate groove width is 50um-100um, and the secondary gate groove width is 5um-50um; the width of the main gate is 40um-100um, and the width of the secondary gate is 5um-50um; the thickness of the anti-oxidation metal layer is 900nm-10000nm; the thickness of the intrinsic amorphous silicon layer is 2nm-20nm, the thickness of the doped n-type amorphous silicon layer is 2nm-20nm, and the thickness of the doped p-type amorphous silicon layer is 2nm-20nm.
[0031] Electroplating copper instead of screen-printed silver reduces the cost of grid line metallization. The width of the copper grid line can be 40% of the silver grid, which increases the light-receiving area. At the same time, the resistivity of the copper grid is only 30% of the silver grid, which greatly improves the battery efficiency. Compared with conventional copper grid electrodes, the copper grid height uniformity of the present application is better, and there will be no problem of uneven electroplating and film sandwiching. The adhesion of the grid line can meet the tension and reliability tests. At the same time, it is easier to achieve ink protection on the side of the battery to avoid battery short circuit caused by metal electroplating on the side of the battery. The anti-oxidation metal layer on the surface of the grid line can increase the service life of the battery. In addition, the back of the battery cell is polished, which is more conducive to light absorption and is conducive to the optimization of the amorphous silicon film on the back, thereby improving the conversion efficiency of the battery cell.
[0032] Example 2
[0033] A method for preparing a silicon heterojunction solar cell, comprising:
[0034] S10: Place the silicon plate in a 0.5%-10% KOH solution, react at 50℃-85℃ for 1min-20min, and form a double-sided velvet structure on the surface of the silicon plate, with a double-sided velvet reflectivity of 10%-20%; in addition, make a protective film on the first side, the protective film is SIO2, and then place it in a 0.5%-10% KOH solution for 1-5min, and polish the side without the protective film, that is, etch the pyramid, leaving only the base, to reduce the fluidity of the ink on its surface. The reflectivity of the polished surface is 45%-50%.
[0035] S20: depositing a first layer of amorphous silicon S01 on the first surface, and depositing a second layer of amorphous silicon S02 on the second surface.
[0036] S30: depositing a first layer of ITO S03 on the first surface, with an ITO thickness of 40nm-200nm, and depositing a second layer of ITO S04 on the second surface, with an ITO thickness of 40nm-200nm.
[0037] S40: Vacuum sputtering method, including PVD / RPD and electron beam evaporation, is used on the front and back sides to prepare a metal layer S05 and S06 respectively, which serves as the seed layer for subsequent electroplating. Its main function is to enhance the conductivity and improve the subsequent gate line pull-off force. The metal layer includes copper, nickel, silver, gold, titanium, and aluminum conductive metals with a thickness of 30nm-1000nm and a film layer square resistance of 0.1mΩ-10mΩ.
[0038] S50: Form electroplating masks on the polished surface and the textured surface of the cell by screen printing process. The screen pattern of the polished surface of the printed cell includes hollow areas and grid line areas. The screen pattern of the textured surface of the printed cell is all hollow areas without grid line areas. Two different electroplating mask materials are used. The electroplating mask material of the polished surface uses thermosetting material, and the electroplating mask material of the textured surface uses photosensitive material. The thickness of the electroplating mask is 5um-50um. Then, the electroplating mask material is solidified by drying at 80-200℃ for 1min-30min. After the thermosetting material is baked, it does not react with the developer or plating solution. The main grid groove width is 50um-100um, and the sub-grid width is 5um-50um. The photosensitive material of the textured surface is exposed in the non-grid line area of the textured surface by exposure and development. The photosensitive material after exposure will undergo a cross-linking reaction and is not easily removed by the subsequent developer. Then the unexposed area is removed by the developer, and finally the main grid and sub-grid are perpendicular to each other to form the S07 layer of the groove pattern to be electroplated on the textured surface, wherein the main grid width is 40um-100um, and the sub-grid width is 5um-50um. The front grid line width is as narrow as possible to reduce the light shielding area.
[0039] S60: Then, a circle of insulating ink is applied on the edge of the silicon plate by using a fixture or spin coating, and the ink fluidity is used to cover the edge side wall of the silicon plate to prevent the edge metal wire phenomenon caused by thickness electroplating.
[0040] S70: A copper gate layer is formed in the front and back grooves by chemical electroplating, and then an anti-oxidation metal layer with a thickness of 500nm-10000nm is formed on the formed copper gate layer by electroplating, including tin, silver and other metal layers.
[0041] S80: Use KOH solution to remove the front photosensitive mask, the back thermosetting mask and the edge insulating mask; then use H2SO4 plus an oxidizing additive to remove the metal seed layer, and finally form a complete high-efficiency heterojunction solar cell product.
[0042] Based on the above preparation method, compared with the conventional copper electroplating process using dry film as mask for photolithography patterning, the photocurable ink used on the first side of the battery in this preparation method has a cost of 1 / 10-1 / 6 of the dry film, and the thermosetting ink used on the second side has a cost of 1 / 10-1 / 6 of the dry film, and the printing equipment is 1 / 2 of the photolithography exposure equipment.
[0043] Compared with the preparation of conventional copper grid electrodes, the pattern grooving of the battery in the present invention is combined with horizontal electroplating equipment, and the copper grid prepared has better height uniformity, does not have the problem of uneven electroplating and film sandwiching, and the grid line adhesion can meet the requirements of tension and reliability tests.
[0044] In addition, compared with the preparation of conventional copper gate electrodes, the process scheme of the present invention also includes that during electroplating, it is easier to protect the battery side with ink, thereby avoiding battery short circuit caused by metal electroplating on the battery side.
[0045] In addition, polishing the back of the cell is more conducive to light absorption and optimization of the amorphous silicon film on the back, improving FF and thus improving the conversion efficiency of the cell.
[0046] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the utility model.
[0047] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the utility model. In this specification, the schematic expressions of the above terms do not necessarily refer to the same embodiment or example.
[0048] Obviously, the described embodiments are only a part of the embodiments of the present application, rather than all the embodiments. Mentioning "embodiment" in this article means that the specific features, structures or characteristics described in conjunction with the embodiment may be included in at least one embodiment of the present embodiment application. The appearance of this phrase in various positions in the specification is not necessarily the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It can be explicitly and implicitly understood by those skilled in the art that the embodiments described herein can be combined with other embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.
[0049] Although the embodiments of the present invention have been shown and described, those skilled in the art will appreciate that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A silicon heterojunction solar cell, characterized in that: A silicon plate (3) comprising a first surface and a second surface, wherein the first surface of the silicon plate (3) is sequentially stacked with a first amorphous silicon layer (11), a first ITO layer (12), a first metal seed layer (13), and a first gate line layer (14); The second surface of the silicon plate (3) is sequentially stacked with a second amorphous silicon layer (21), a second ITO layer (22), a second metal seed layer (23), and a second gate line layer (24); The first gate line layer (14) and the second gate line layer (24) each comprise at least one main gate and at least one auxiliary gate, any one of the main gates and any one of the auxiliary gates are perpendicular to each other, and a layer of anti-oxidation metal layer is provided on the surfaces of the main gates and the auxiliary gates; The first amorphous silicon layer (11) comprises a first intrinsic amorphous silicon layer and a first amorphous silicon sublayer, the first amorphous silicon sublayer being arranged at an end of the first intrinsic amorphous silicon layer away from the silicon plate (3), the second amorphous silicon layer (21) comprises a second intrinsic amorphous silicon layer and a second amorphous silicon sublayer, the second amorphous silicon sublayer being arranged at an end of the second intrinsic amorphous silicon layer away from the silicon plate (3); The first amorphous silicon sublayer is an n-type amorphous silicon layer, and the second amorphous silicon sublayer is a p-type amorphous silicon layer; The first surface of the silicon plate (3) is a textured structure, and the second surface of the silicon plate (3) is a polished structure; The main gate and the auxiliary gate are both arranged on the main gate groove and the auxiliary gate groove, the main gate groove width is 50um-100um, and the auxiliary gate groove width is 5um-50um; The width of the main grid is 40um-100um, and the width of the secondary grid is 5um-50um.
2. A silicon heterojunction solar cell according to claim 1, characterized in that: The thickness of the first ITO layer (12) and the second ITO layer (22) are both 40nm-200nm, and the first metal seed layer (13) and the second metal seed layer (23) both comprise conductive metals such as copper, nickel, silver, gold, titanium, and aluminum.
3. A silicon heterojunction solar cell according to claim 2, characterized in that: The thickness of the first metal seed layer (13) and the second metal seed layer (23) are both 30 nm-1000 nm, and the sheet resistance of the film layer is 0.1 mΩ-10 mΩ.
4. The silicon heterojunction solar cell according to claim 1, characterized in that: The thickness of the anti-oxidation metal layer is 900nm-10000nm.
5. The silicon heterojunction solar cell according to claim 1, characterized in that: The thickness of the first intrinsic amorphous silicon layer and the second intrinsic amorphous silicon layer is 2nm-20nm, the thickness of the doped n-type amorphous silicon layer is 2nm-20nm, and the thickness of the doped p-type amorphous silicon layer is 2nm-20nm.