Silicon carbide crystal growth device
By introducing thickened sections, lifting support structures and induction heating tubes into the silicon carbide crystal growth device, the problems of heating temperature adjustment and carbon source supply uniformity are solved, the life of the equipment is extended and the growth performance of silicon carbide crystals is improved.
Patent Information
- Application Number
- CN202323340583.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-08
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2033-12-08
AI Technical Summary
Existing silicon carbide crystal growth devices have problems such as inconvenient adjustment of heating temperature, uneven carbon source supply, and easy erosion of the crucible.
A silicon carbide crystal growth device including a thickened section, a lifting support structure and an induction heating tube is designed. The temperature gradient is adjusted through the bottom heater and side induction heating tubes of the heating chamber, and a middle protrusion is set in the crucible. and sliding engagement structure to uniformly corrode and prevent corrosion.
The growth uniformity of silicon carbide crystals and flexible adjustment of temperature gradient are achieved, the service life of the equipment is extended, and the growth performance of silicon carbide crystals is improved.
Smart Images

Figure CN221895177U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of silicon carbide crystal preparation, and more specifically, to a silicon carbide crystal growing device. Background Art
[0002] The liquid phase method is one of the main ways to prepare silicon carbide crystals. In the process of preparing silicon carbide crystals by the liquid phase method, the growth chamber of the crystal growth furnace includes a crucible, a solution, a seed crystal axis, a seed crystal, and a heating structure. The crucible is a high-purity graphite crucible. The high-purity polycrystalline silicon raw material is placed in the graphite crucible. The high-purity polycrystalline silicon in the crucible is melted by induction heating to form molten silicon. The molten silicon will corrode the graphite crucible, and the carbon source is provided to the molten silicon through the graphite crucible, thereby forming a solution of the Si-C system.
[0003] The seed crystal is attached to the seed crystal rod and immersed in the supersaturated zone of the solution to grow silicon carbide crystals. However, the high-temperature growth raw material solution may melt through the crucible during the long-term preparation of silicon carbide, causing damage to the equipment.
[0004] In the process of providing a carbon source to molten silicon through a graphite crucible, it is mainly the molten silicon in the periphery that contacts the carbon source provided by the graphite crucible, and the contact uniformity between the carbon source and the molten silicon is poor, resulting in poor growth uniformity of silicon carbide crystals.
[0005] In addition, the heating structure in the existing silicon carbide crystal growth device is usually an integral structure, and the distance between the heating element and the crucible is fixed, which leads to a thermal field with a fixed temperature gradient in the axial direction of the crucible. The temperature at a specific position in the axial direction of the crucible cannot be flexibly adjusted, making it difficult to meet personalized crystallization needs. Utility Model Content
[0006] 1. Technical issues to be solved
[0007] In view of the problems existing in the prior art, the utility model provides a silicon carbide crystal growth device to solve the technical problems mentioned in the background technology that the heating temperature of the silicon carbide crystal growth device in the prior art is not easy to adjust, the carbon source supply is uneven and the crucible is easily corroded.
[0008] (II) Technical solution
[0009] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0010] A silicon carbide crystal growth device comprises a crucible, wherein a thickened section is arranged inside the crucible, a middle convex portion is arranged in the middle of the crucible, a heating groove is opened upward at the bottom of the middle convex portion, a heat preservation barrel is arranged on the outside of the crucible, a protective shell is arranged on the outside of the heat preservation barrel, a heating chamber is arranged between the heat preservation barrel and the crucible, a bottom heater is arranged at the bottom of the heating chamber in coordination with the heating groove, and a lifting support structure is arranged in coordination with the crucible, an induction heating tube is arranged on the side of the heating chamber, the winding diameter of the induction heating tube gradually decreases from top to bottom, an opening is arranged at the top of the crucible, a seed crystal rod is arranged at the opening in a liftable manner, and a seed crystal is arranged at the bottom of the seed crystal rod.
[0011] The utility model is further configured such that the lifting support structure includes a support frame arranged at the bottom of the crucible, and a second electric push rod is arranged at the bottom end of the support frame connected to the bottom wall of the heating chamber, and the support and lifting adjustment of the crucible are achieved through the cooperation of the second electric push rod and the support frame.
[0012] The utility model is further configured that the heat-insulating barrel comprises a barrel inner shell and a barrel outer shell which cooperate with each other, and a heat-insulating layer is arranged between the barrel inner shell and the barrel outer shell to enhance the heat-insulating effect of the heat-insulating barrel.
[0013] The utility model is further configured such that the thermal insulation layer comprises a first thermal insulation plate arranged in contact with the inner shell of the barrel, a thermal insulation cotton layer is arranged on the outer side of the first thermal insulation plate, and a second thermal insulation plate is arranged between the thermal insulation cotton layer and the outer shell of the barrel to enhance the thermal insulation performance of the thermal insulation layer.
[0014] The utility model is further configured that the bottom heater comprises a heating base plate, and the heating base plate extends to the heating tank and is provided with a heating column to achieve heating of the bottom of the crucible and the interior of the heating tank.
[0015] The utility model is further configured such that a mounting seat is provided at the bottom of the heating base, a connecting frame is provided on the side of the mounting seat connected to the side wall of the heating chamber, and the supporting frame is passed through the connecting frames and does not contact the heating base, thereby realizing the installation and fixation of the bottom heating plate.
[0016] The utility model is further configured that the thickened section is slidably mounted inside the crucible, and a sliding engaging structure is provided between the thickened section and the crucible.
[0017] The utility model is further configured that the sliding engaging structure includes a fixing bar arranged inside the crucible, a limiting sliding groove is provided on the fixing bar, and a limiting sliding block is provided on the thickened section to cooperate with the limiting sliding groove, so as to realize the detachable installation of the thickened section inside the crucible.
[0018] (III) Beneficial effects
[0019] Compared with the prior art, the present invention provides a silicon carbide crystal growth device having the following features:
[0020] Beneficial effects:
[0021] 1. The utility model provides a thickened section on the inner wall of the crucible, wherein the thickened section corresponds to the liquid surface of the growth melt placed in the crucible, so that when the molten silicon solution corrodes the silicon crucible, the thickened section will be corroded first, so that during the production process of silicon carbide, the molten silicon solution can be prevented from corroding the crucible.
[0022] 2. The utility model provides a middle convex portion at the bottom of the crucible, so that in the process of corrosion of the crucible by the molten silicon solution, uniform corrosion from the inside to the outside can be achieved, so that the carbon source is evenly integrated into the molten silicon solution, thereby improving the growth uniformity of the silicon carbide crystal.
[0023] 3. The utility model provides a bottom heater at the bottom of the heating chamber in conjunction with the heating groove, and a lifting support structure is provided in conjunction with the crucible, and an induction heating tube is provided on the side of the heating chamber, and the coiled diameter of the induction heating tube gradually decreases from top to bottom. In this way, the distance between the induction heating tube and the crucible can be adjusted by controlling the lifting and lowering adjustment of the crucible, thereby adjusting the heating gradient and improving the growth performance of silicon carbide crystals. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 This is a schematic diagram of the overall structure of a silicon carbide crystal growth device in the utility model;
[0025] Figure 2 The overall structure of the utility model is shown in cross-section Figure 1 ;
[0026] Figure 3 The overall structure of the utility model is shown in cross-section Figure 2 ;
[0027] Figure 4 It is a schematic diagram of the exploded structure of the connection between the crucible and the thickened section in the utility model;
[0028] Figure 5 It is a schematic cross-sectional view of the overall structure of the heat preservation barrel in the utility model;
[0029] Figure 6 It is a schematic cross-sectional view of the local structure of the thermal insulation layer in the utility model.
[0030] In the figure: 1. crucible; 2. thickened section; 3. middle raised part; 4. heating tank; 5. insulation barrel; 6. protective shell; 7. heating chamber; 8. bottom heater; 9. induction heating tube; 10. opening; 11. seed crystal rod; 12. seed crystal; 13. support frame; 14. second electric push rod; 15. barrel inner shell; 16. barrel outer shell; 17. insulation layer; 18. first insulation board; 19. insulation cotton layer; 20. second insulation board; 21. heating bottom plate; 22. heating column; 23. mounting seat; 24. connecting frame; 25. fixing bar; 26. limit slide groove; 27. limit slider. DETAILED DESCRIPTION
[0031] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present utility model will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0032] It should be noted that, unless otherwise specified, all technical and scientific terms used in this application have the same meanings as commonly understood by ordinary technicians in the technical field to which this application belongs.
[0033] In the present invention, unless otherwise specified, directions such as "up" and "down" are usually used in reference to the directions shown in the drawings, or in reference to the vertical, perpendicular or gravity direction; similarly, for ease of understanding and description, "left" and "right" are usually used in reference to the left and right shown in the drawings; "inside" and "outside" refer to the inside and outside relative to the outline of each component itself, but the above-mentioned directions are not used to limit the present invention.
[0034] See also Figure 1-6 A silicon carbide crystal growth device comprises a crucible 1, a thickened section 2 is arranged inside the crucible 1, a middle convex portion 3 is arranged in the middle of the crucible 1, a heating groove 4 is opened upward at the bottom of the middle convex portion 3, a heat preservation barrel 5 is arranged on the outside of the crucible 1, a protective shell 6 is arranged on the outside of the heat preservation barrel 5, a heating chamber 7 is arranged between the heat preservation barrel 5 and the crucible 1, a bottom heater 8 is arranged at the bottom of the heating chamber 7 in coordination with the heating groove 4, and a lifting support structure is arranged in coordination with the crucible 1, an induction heating tube 9 is arranged on the side of the heating chamber 7, and the winding diameter of the induction heating tube 9 gradually decreases from top to bottom, an opening 10 is arranged on the top of the crucible 1, a seed crystal rod 11 is arranged at the opening 10 so as to be liftable, and a seed crystal 12 is arranged at the bottom of the seed crystal rod 11.
[0035] In this embodiment, the utility model provides a thickened section 2 on the inner wall of the crucible 1, wherein the thickened section 2 corresponds to the liquid surface of the growth melt placed in the crucible 1, so that when the molten silicon solution corrodes the silicon crucible 1, the thickened section 2 will be corroded first, so that during the production process of silicon carbide, the molten silicon solution can be prevented from corroding the crucible 1.
[0036] More specifically, the utility model is provided with a middle protrusion 3 at the bottom of the crucible 1, so that in the process of corrosion of the crucible 1 by the molten silicon solution, uniform corrosion from the inside to the outside can be achieved, so that the carbon source is evenly integrated into the molten silicon solution, thereby improving the growth uniformity of the silicon carbide crystal.
[0037] Furthermore, the utility model provides a bottom heater 8 at the bottom of the heating chamber 7 in conjunction with the heating groove 4, and a lifting support structure is provided in conjunction with the crucible 1, and an induction heating tube 9 is provided on the side of the heating chamber 7, and the winding diameter of the induction heating tube 9 gradually decreases from top to bottom. In this way, the distance between the induction heating tube 9 and the crucible 1 can be adjusted by controlling the lifting and lowering adjustment of the crucible 1, thereby achieving the adjustment of the heating gradient and improving the growth performance of the silicon carbide crystal.
[0038] See also Figure 2 and Figure 3 As an implementation of the lifting support structure: the lifting support structure includes a support frame 13 arranged at the bottom of the crucible 1, and the bottom end of the support frame 13 is connected to the bottom wall of the heating chamber 7 and a second electric push rod 14 is arranged.
[0039] Specifically, the second electric push rod 14 is started, and the lifting of the support frame 13 can be controlled by the second electric push rod 14. The lifting of the support frame 13 can control the lifting of the crucible 1. The lifting of the crucible 1 can adjust the distance between the side wall of the crucible 1 and the induction heating tube 9 and the distance between the bottom of the crucible 1 and the bottom heater 8.
[0040] See also Figure 5 and Figure 6 As an implementation mode of the heat-insulating barrel 5: the heat-insulating barrel 5 includes a barrel inner shell 15 and a barrel outer shell 16 that cooperate with each other, and an insulation layer 17 is arranged between the barrel inner shell 15 and the barrel outer shell 16. The insulation layer 17 includes a first insulation board 18 arranged to fit the barrel inner shell 15, and an insulation cotton layer 19 is arranged on the outer side of the first insulation board 18, and a second insulation board 20 is arranged between the insulation cotton layer 19 and the barrel outer shell 16.
[0041] Specifically, the cooperation of the first insulation board 18 , the insulation cotton layer 19 and the second insulation board 20 can enhance the insulation performance of the insulation barrel 5 , thereby preventing the heat loss during the heating process of the crucible 1 .
[0042] See also Figure 2 and Figure 3 As an implementation of the bottom heater 8: the bottom heater 8 includes a heating base plate 21, and the heating base plate 21 extends to the heating tank 4 and is provided with a heating column 22.
[0043] Specifically, the bottom of the crucible 1 can be heated evenly and stably by the heating base 21, and the heating column 22 can extend into the heating tank 4 to heat the middle protrusion 3, so that the heating effect of the middle protrusion 3 can be enhanced, so that the crucible 1 can evenly provide the carbon source.
[0044] See also Figure 2 and Figure 3 As an implementation of the heating chassis 21: a mounting seat 23 is provided at the bottom of the heating chassis 21, and a connecting frame 24 is provided on the side of the mounting seat 23 connected to the side wall of the heating chamber 7, and the support frame 13 is passed through the connecting frame 24 and does not contact the heating chassis 21.
[0045] Specifically, the heating base 21 is stably installed through the mounting seat 23 , wherein the mounting frame is installed in the heat preservation barrel 5 through the connecting frame 24 , thereby achieving stable installation of the heating base 21 .
[0046] See also Figure 2-Figure 4 As an implementation of the thickening section 2: the thickening section 2 is slidably installed inside the crucible 1, and a sliding engagement structure is arranged between the thickening section 2 and the crucible 1, wherein the sliding engagement structure includes a fixing bar 25 arranged inside the crucible 1, a limiting slide groove 26 is arranged on the fixing bar 25, and a limiting slider 27 is arranged on the thickening section 2 to cooperate with the limiting slide groove 26.
[0047] Specifically, the crucible 1 is slidably engaged inside the crucible 1 to achieve detachable installation of the thickened section 2 inside the crucible 1, so that after the thickened section 2 is corroded, it can be replaced, thereby preventing the crucible 1 from being corroded and requiring a complete replacement, which can reduce costs;
[0048] When the thickening section 2 is installed, the limiting sliding block 27 is inserted into the corresponding limiting sliding groove 26 , so that the thickening section 2 can be slidably engaged inside the crucible 1 .
[0049] In summary, when the overall equipment is in use:
[0050] The silicon raw material is placed in the crucible 1 and heated to form a molten state. The molten silicon liquid corrodes the heating end of the crucible 1, so that the molten silicon liquid provides a carbon source;
[0051] In the process of heating the crucible 1, the lifting of the support frame 13 can be controlled by the second electric push rod 14, and the lifting of the support frame 13 can control the lifting of the crucible 1. The lifting and lowering of the crucible 1 can adjust the distance between the side wall of the crucible 1 and the induction heating tube 9 and the distance between the bottom of the crucible 1 and the bottom heater 8. In this way, the thermal field of the silicon carbide crystal during the growth process can be adjusted, thereby improving the performance of the silicon carbide crystal during the growth process.
[0052] In the process of heating the crucible 1, the induction heating tube 9 is used to heat the side wall of the crucible 1, the heating base plate 21 is used to heat the bottom of the crucible 1, and the heating rod is mainly used to heat the middle protrusion 3, so that the carbon source can be provided from the middle through the middle protrusion 3, thereby improving the uniformity of the supply of the carbon source;
[0053] After the thickened section 2 is corroded, the thickened section 2 can be removed from the inside of the crucible 1 for replacement, thereby preventing the crucible 1 from being corroded as a whole.
[0054] In all the schemes mentioned above, the connection between two parts can be selected according to actual conditions by welding, bolt and nut matching connection, bolt or screw connection or other well-known connection methods, which are not described here one by one. In the above, all fixed connections are preferably welded. Although the embodiments of the utility model have been shown and described, it can be understood by ordinary technicians in this field that various changes, modifications, substitutions and variations can be made to these embodiments without departing from the principle and spirit of the utility model. The scope of the utility model is defined by the attached claims and their equivalents.
Claims
1. A silicon carbide crystal growth device, comprising a crucible (1), Its characteristics are: The crucible (1) is provided with a thickened section (2) inside, the middle of the crucible (1) is provided with a middle protrusion (3), the bottom of the middle protrusion (3) is provided with a heating groove (4) facing upward, the outside of the crucible (1) is provided with a heat preservation barrel (5), the outside of the heat preservation barrel (5) is provided with a protective shell (6), a heating chamber (7) is provided between the heat preservation barrel (5) and the crucible (1), the bottom of the heating chamber (7) is provided with a bottom heater (8) in coordination with the heating groove (4), and a lifting support structure is provided in coordination with the crucible (1), an induction heating tube (9) is provided on the side of the heating chamber (7), the winding diameter of the induction heating tube (9) gradually decreases from top to bottom, an opening (10) is provided at the top of the crucible (1), a seed crystal rod (11) is provided at the opening (10) in a liftable manner, and a seed crystal (12) is provided at the bottom of the seed crystal rod (11).
2. A silicon carbide crystal growth device according to claim 1, Its characteristics are: The lifting support structure comprises a support frame (13) arranged at the bottom of the crucible (1), and the bottom end of the support frame (13) is connected to the bottom wall of the heating chamber (7) and is provided with a second electric push rod (14).
3. A silicon carbide crystal growth device according to claim 1, Its characteristics are: The heat-insulating barrel (5) comprises a barrel inner shell (15) and a barrel outer shell (16) which cooperate with each other, and a heat-insulating layer (17) is provided between the barrel inner shell (15) and the barrel outer shell (16).
4. A silicon carbide crystal growth device according to claim 3, Its characteristics are: The heat-insulating layer (17) comprises a first heat-insulating plate (18) arranged to fit the barrel inner shell (15), a heat-insulating cotton layer (19) being arranged on the outer side of the first heat-insulating plate (18), and a second heat-insulating plate (20) being arranged between the heat-insulating cotton layer (19) and the barrel outer shell (16).
5. A silicon carbide crystal growth device according to claim 2, Its characteristics are: The bottom heater (8) comprises a heating bottom plate (21), and the heating bottom plate (21) extends into the heating tank (4) and is provided with a heating column (22).
6. A silicon carbide crystal growth device according to claim 5, Its characteristics are: A mounting seat (23) is provided at the bottom of the heating base (21); a connecting frame (24) is provided on the side of the mounting seat (23) connected to the side wall of the heating chamber (7); and the support frame (13) is passed through the connecting frames (24) and does not contact the heating base (21).
7. A silicon carbide crystal growth device according to any one of claims 1 to 6, Its characteristics are: The thickened section (2) is slidably mounted inside the crucible (1), and a sliding engagement structure is provided between the thickened section (2) and the crucible (1).
8. A silicon carbide crystal growth device according to claim 7, Its characteristics are: The sliding engagement structure comprises a fixing bar (25) arranged inside the crucible (1), a limiting sliding groove (26) being provided on the fixing bar (25), and a limiting sliding block (27) being provided on the thickened section (2) in coordination with the limiting sliding groove.