Novel high-brightness reflective film
By using the special structure of modified glass beads and a fluorescent layer in the reflective film, combined with diffuse reflection and protective layers, the problem of existing reflective films being ineffective in dim or no-light environments is solved, and the problem is achieved in any environment. Good reflective and indicator effects, and improved durability and anti-fouling properties.
Patent Information
- Application Number
- CN202420660335.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-02
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-04-02
AI Technical Summary
The existing reflective film has no obvious reflective effect in dim or no-light environments, and cannot effectively serve as a warning and instruction guide.
A new type of high-brightness reflective film is designed, which uses the hemispherical and diamond-shaped structures of modified glass beads, combined with the fluorescent layer and diffuse reflection layer on the metal layer to ensure good reflection in dark environments and automatically light up at night; at the same time Features protective and anti-static layers for durability and anti-fouling properties.
It achieves effective reflection and guidance in any light environment, extends the service life, and avoids light pollution and static electricity problems.
Smart Images

Figure CN221926704U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of reflective films, and more specifically, to a novel high-brightness reflective film. Background Art
[0002] Reflective film is a kind of retro-reflective material that has been made into a film and can be directly used. It is made by using glass bead technology, micro-prism technology, synthetic resin technology, thin film technology, coating technology and micro-replication technology. It produces a strong reflective effect under the illumination of light. It is usually used to attach to the surface of buildings, transportation facilities, vehicles and other objects. It has the purpose of marking and warning, and also provides safety protection for walking at night.
[0003] Existing reflective film generally includes a reflective layer, glass beads and a light-transmitting layer. Although it can reflect light, due to its unreasonable structural design, it can only play a striking warning role under strong light. In dim light, the reflective effect is not obvious, which greatly reduces the warning effect of the reflective film. Moreover, it cannot play a guiding role in the absence of light at night. In response to the above problems, this device was invented. Utility Model Content
[0004] In order to overcome the above defects of the prior art, the utility model provides a new type of high-brightness reflective film to solve the problems raised in the above background technology.
[0005] In order to achieve the above-mentioned purpose, the utility model provides the following technical solutions: a new type of high-brightness reflective film, including a base layer, a resin layer is arranged on the outside of the base layer, a plurality of installation grooves are opened at equal intervals on the outer wall of the resin layer, modified glass beads are arranged in the installation grooves, the lower part of the modified glass beads is a hemispherical structure, and the upper part of the modified glass beads is a diamond structure, the outer wall of the resin layer is coated with a metal layer, a plurality of fluorescent layers are arranged on the metal layer at equal intervals, a diffuse reflection layer is arranged on the outside of the metal layer, the outer wall of the diffuse reflection layer is a wavy structure, a protective layer is arranged on the outside of the diffuse reflection layer, and an antistatic layer is arranged on the outside of the protective layer.
[0006] Optionally, the base layer is made of PVC film.
[0007] Optionally, the resin layer is made of elastic polyurethane resin.
[0008] Optionally, the volume of the modified glass microspheres protruding from the resin layer accounts for 50%-70% of the total volume of the modified glass microspheres.
[0009] Optionally, the modified glass microbeads are spherical structures.
[0010] Optionally, the metal layer is made of metal aluminum.
[0011] Optionally, the protective layer includes an anti-aging layer arranged on the inner side and a corrosion-resistant layer arranged on the outer side, wherein the anti-aging layer is made of LLDPE resin and the corrosion-resistant layer is made of polytetrafluoroethylene.
[0012] Optionally, the antistatic layer is made of ABS material.
[0013] Compared with the prior art, the beneficial effects of the utility model are:
[0014] 1. The new high-brightness reflective film designs the modified glass beads into a structure with a hemispherical lower part and a diamond upper part. The combination of the hemispherical structure and the diamond structure forms a strong light reflector, so that the high-brightness reflective film can still have a good reflective effect even in a dim light environment;
[0015] 2. The new high-brightness reflective film is formed by equidistantly arranging multiple fluorescent layers on the metal layer. The fluorescent layers absorb light energy during the day and automatically emit light at night, so that the high-brightness reflective film can still play a guiding and indicating role even in a lightless environment;
[0016] 3. The new high-brightness reflective film is provided with a diffuse reflection layer, which can refract the light emitted from the inner side of the high-brightness reflective film and diffusely reflect the light incident from the outside to avoid light pollution. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present utility model. For ordinary technicians in this field, other drawings can also be obtained based on these drawings.
[0018] Figure 1 A schematic diagram of the structure provided by the utility model;
[0019] Figure 2 A schematic diagram of the structure of the resin layer provided by the utility model;
[0020] Figure 3 A schematic structural diagram of another embodiment provided by the utility model.
[0021] Description of reference numerals:
[0022] 1. Base layer; 2. Resin layer; 3. Installation groove; 4. Modified glass beads; 5. Metal layer; 6. Diffuse reflection layer; 7. Protective layer; 8. Antistatic layer; 9. Fluorescent layer. DETAILED DESCRIPTION
[0023] The following is a specific embodiment of the present invention. People familiar with the technology can easily understand the other advantages and functions of the present invention from the contents disclosed in this specification. Obviously, the described embodiment is a part of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] In order to enable those skilled in the art to better understand the present application, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0025] See attached Figure 1 The embodiment is a novel high-brightness reflective film, comprising a base layer 1, the base layer 1 is made of PVC film, a resin layer 2 is arranged on the outer side of the base layer 1, the resin layer 2 is made of elastic polyurethane resin, and the elastic polyurethane resin enhances the overall elasticity of the high-brightness reflective film, so that the high-brightness reflective film is not easily torn, that is, the service life of the high-brightness reflective film is effectively extended.
[0026] See attached Figure 1 and Figure 3 The outer wall surface of the resin layer 2 is provided with a plurality of installation grooves 3 at equal intervals, the installation grooves 3 are coated with hot melt adhesive, and modified glass beads 4 are arranged in the installation grooves 3. The outer wall surface of the resin layer 2 is coated with a metal layer 5, the metal layer 5 is made of metal aluminum, and a diffuse reflection layer 6 is arranged on the outer side of the metal layer 5. The inner wall surface of the diffuse reflection layer 6 is provided with a plurality of external grooves adapted to the installation grooves 3 at equal intervals, and the inner wall of the external grooves is also coated with hot melt adhesive. The modified glass beads 4 are placed between the installation grooves 3 and the external grooves, and are fixedly installed in the resin layer 2 and the diffuse reflection layer 6 by the hot melt adhesive on both sides.
[0027] See attached Figure 1 The volume of the modified glass beads 4 protruding from the resin layer 2 accounts for 50%-70% of the total volume of the modified glass beads 4. The lower part of the modified glass beads 4 is a hemispherical structure, and the upper part of the modified glass beads 4 is a diamond structure. The combination of the hemispherical structure and the diamond structure forms a strong light reflector, so that the high-brightness reflective film can still have a good reflective effect even in a dim light environment.
[0028] See attached Figure 2 In this other embodiment, the modified glass microbead 4 is a spherical structure, and the spherical structure makes the light reflect regularly on the surface of the modified glass microbead 4 to generate reflected light.
[0029] See attached Figure 3A plurality of fluorescent layers 9 are arranged at equal intervals on the metal layer 5. The fluorescent layers 9 are made of solidified fluorescent powder. The fluorescent powder absorbs light energy during the day and automatically emits light at night, so that the high-brightness reflective film can still play a guiding and indicating effect even in an environment without light.
[0030] Refer to the attached Figure 1 The outer wall surface of the diffuse reflection layer 6 is a wavy structure. The diffuse reflection layer 6 can refract the light emitted from the inner side of the high-brightness reflective film and diffusely reflect the light incident from the outside to avoid light pollution.
[0031] Refer to the attached Figure 1 A protective layer 7 is arranged outside the diffuse reflection layer 6, and an antistatic layer 8 is arranged outside the protective layer 7. The protective layer 7 includes an anti-aging layer arranged inside and a corrosion-resistant layer arranged outside, wherein the anti-aging layer is made of LLDPE resin, which has excellent environmental stress cracking resistance. By providing the anti-aging layer, the anti-aging performance of the high-brightness reflective film is improved. The corrosion-resistant layer is made of polytetrafluoroethylene, which has excellent chemical stability and corrosion resistance. By providing the corrosion-resistant layer, the corrosion resistance of the high-brightness reflective film is improved, which is beneficial to the use of the high-brightness reflective film. The antistatic layer 8 is made of ABS material, which has excellent electrical insulation. By providing the antistatic layer 8, the high-brightness reflective film is effectively prevented from generating static electricity, thereby preventing the high-brightness reflective film from absorbing dust, and achieving the purpose of enhancing the reflective intensity of the high-brightness reflective film.
[0032] Finally: The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present utility model should be included in the protection scope of the present utility model.
Claims
1. A new type of high-brightness reflective film, characterized in that: The invention comprises a base layer (1), a resin layer (2) is arranged on the outside of the base layer (1), a plurality of installation grooves (3) are formed on the outer wall of the resin layer (2) at equal intervals, modified glass microbeads (4) are arranged in the installation grooves (3), the lower part of the modified glass microbeads (4) is a hemispherical structure, and the upper part of the modified glass microbeads (4) is a diamond structure, the outer wall of the resin layer (2) is coated with a metal layer (5), a plurality of fluorescent layers (9) are arranged on the metal layer (5) at equal intervals, a diffuse reflection layer (6) is arranged on the outer side of the metal layer (5), the outer wall of the diffuse reflection layer (6) is a wavy structure, a protective layer (7) is arranged on the outer side of the diffuse reflection layer (6), and an antistatic layer (8) is arranged on the outer side of the protective layer (7).
2. The novel high-brightness reflective film according to claim 1, characterized in that: The base layer (1) is made of PVC film.
3. The novel high-brightness reflective film according to claim 1, characterized in that: The resin layer (2) is made of elastic polyurethane resin.
4. The novel high-brightness reflective film according to claim 1, characterized in that: The volume of the modified glass microspheres (4) protruding from the resin layer (2) accounts for 50%-70% of the total volume of the modified glass microspheres (4).
5. The novel high-brightness reflective film according to claim 1, characterized in that: The modified glass microspheres (4) are spherical in structure.
6. The novel high-brightness reflective film according to claim 1, characterized in that: The metal layer (5) is made of metal aluminum.
7. The novel high-brightness reflective film according to claim 1, characterized in that: The protective layer (7) comprises an anti-aging layer arranged on the inner side and a corrosion-resistant layer arranged on the outer side, wherein the anti-aging layer is made of LLDPE resin and the corrosion-resistant layer is made of polytetrafluoroethylene.
8. The novel high-brightness reflective film according to claim 1, characterized in that: The antistatic layer (8) is made of ABS material.