Self-winding spiral welding strip
Through the thermal deformation of the self-winding spiral structure welding tape and the dispersed welding tape, the deformation and thermal fatigue problems of the photovoltaic welding tape on the cell are solved, and the stability and durability of the cell are improved after welding.
Patent Information
- Application Number
- CN202420095164.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-16
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2034-01-16
AI Technical Summary
The deformation caused by the difference in thermal expansion coefficient after welding of the photovoltaic welding tape and the solar cell cell is caused by bending and rupture of the cell, and periodic thermal fatigue damage occurs during the alternation of hot and cold.
The welding tape with a self-winding spiral structure is adopted. The copper foil is spirally wound in the long axis direction of the belt body and then flattened, and wraps the solder layer. The heat dissipation deformation becomes a small section deformation, reducing the accumulation of deformation in the long axis direction.
It effectively reduces the impact of welding and cooling on the shrinkage of the battery cell, reduces thermal fatigue damage, and prevents large-size deformation and rupture of the battery cell.
Smart Images

Figure CN221947172U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of photovoltaics, in particular to a self-winding spiral welding tape. Background Art
[0002] Due to the large difference in thermal expansion coefficients between metal and solar cells, the photovoltaic ribbon and solar cell are welded at a high temperature of about 300 degrees Celsius. During welding, both the photovoltaic ribbon and the cell are in a high-temperature extension state, and the lengths of the two are the same during welding. After returning to normal temperature after welding, the shrinkage ratio of the photovoltaic ribbon as a metal is greater than that of the silicon-based cell, resulting in the shrinkage of the photovoltaic ribbon pulling the solar cell to shrink, causing large-scale deformation. Therefore, the cell is pulled and bent, and the large-bent cell is prone to breakage or hidden cracks when entering the lamination. In addition, during the day and night hot and cold alternation of solar modules, the stress of periodic thermal expansion and contraction brought by the photovoltaic ribbon to the solar cell is a destructive thermal fatigue damage. Therefore, it is necessary to reduce the thermal deformation of the photovoltaic ribbon and reduce thermal fatigue damage. Utility Model Content
[0003] In view of the shortcomings of the prior art, the utility model attempts to overcome the above defects, and therefore the utility model provides a self-winding spiral welding strip. In view of the shortcomings of the prior art, the utility model attempts to overcome the above defects, and therefore the utility model provides a self-winding spiral welding strip. Through the self-winding spiral structure, the welding strip has the ability of radial deformation, thereby reducing the shrinkage effect of the photovoltaic welding strip on the solar cell after welding and cooling, and reducing the thermal fatigue damage caused by the photovoltaic welding strip during the power generation operation of the solar module.
[0004] To achieve the above purpose, the utility model is implemented through the following technical scheme: a self-winding spiral welding strip, the welding strip includes a strip body; the strip body is made of copper foil that is spirally self-wound along the long axis direction of the strip body and then flattened, and the outer surface of the strip body is wrapped with a solder layer.
[0005] Furthermore, the copper foil has a thickness of 0.01-0.2 mm.
[0006] Furthermore, the thickness of the solder layer is 0.005-0.03 mm.
[0007] Furthermore, the width of the copper foil is 0.5-20 mm.
[0008] Compared with the prior art, the utility model has the following beneficial effects:
[0009] The copper foil is spirally self-wound along the long axis of the strip and then flattened to form a welding strip. The thermal deformation is dispersed into small segments by the spiral structure. The spiral self-wrap structure will not form deformation accumulation along the long axis, and will not cause large-scale deformation of the solar cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 It is a schematic diagram of the spiral self-winding structure of the belt body of the utility model;
[0011] Figure 2 The utility model is a belt body Figure 1 Schematic diagram of the cross-sectional structure at the dotted line position;
[0012] Figure 3 It is a schematic diagram of the cross-sectional structure of the utility model.
[0013] In the figure: 1. Strip body; 2. Copper foil; 3. Solder layer. DETAILED DESCRIPTION
[0014] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0015] The utility model provides a self-winding spiral welding strip, such as Figure 1-3 As shown, it includes a strip body 1; the strip body 1 is made of a copper foil 2 which is spirally self-wound along the long axis direction of the strip body 1 and then flattened, the outer surface of the strip body 1 is wrapped with a solder layer 3, the thickness of the copper foil 2 is 0.01-0.2 mm, the thickness of the solder layer 3 is 0.005-0.03 mm, and the width of the copper foil 2 is 0.5-20 mm.
[0016] Working principle: The copper foil 2 is spirally self-wound along the long axis direction of the strip 1 and then flattened to form a welding strip. The thermal deformation is dispersed into small segments by the spiral structure. The spiral self-wrap structure will not form deformation accumulation along the long axis direction, and will not cause large-scale deformation of the solar cell.
[0017] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A self-winding spiral welding strip, the welding strip comprising a strip body, characterized in that: The strip body (1) is made of a copper foil (2) which is spirally wound along the long axis direction of the strip body (1) and then flattened. The outer surface of the strip body (1) is wrapped with a solder layer (3).
2. The self-winding spiral welding strip according to claim 1, characterized in that: The thickness of the copper foil (2) is 0.01-0.2 mm.
3. The self-winding spiral welding strip according to claim 1, characterized in that: The thickness of the solder layer (3) is 0.005-0.03 mm.
4. The self-winding spiral welding strip according to claim 1, characterized in that: The width of the copper foil (2) is 0.5-20 mm.