Mini LED display screen
By adopting the chip pad and Mini FC chip with groove structure in the LED display screen, the problems of large device height and point spacing limitation caused by the packaging structure in the prior art are solved, and the thermal conductivity and brightness are improved. Enhanced and reduced package size improve overall performance and reliability of the display.
Patent Information
- Application Number
- CN202323612607.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-28
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-12-28
AI Technical Summary
The packaging structure of existing LED displays leads to large height of the device and high thickness of the plastic packaging, which limits the heat dissipation performance and product reliability of the LEDs. At the same time, it is impossible to achieve lightness and thinness, and the dot spacing is not compatible with products below P1.25.
The chip pad and Mini FC chip with groove structure are used to form an etching area in combination with the semi-etching process. The tin plating process is used to reduce the electroplating wires, and the GOB process is used to improve airtightness and electrical reliability. Small-size package is achieved by tin-plated zones with high temperature solder paste and flux spraying.
It has achieved improved thermal conductivity, enhanced brightness, cost savings, reduced point spacing, and reduced package size, solving the problems of white joints of static modules and bright and dark lines of dynamic joints, and improving the overall performance and reliability of the display screen.
Smart Images

Figure CN221947182U_ABST
Abstract
Description
Technical Field
[0001] The utility model provides a Mini LED display screen, belonging to the technical field of LED display screens. Background Art
[0002] As 5G+8K technology matures, the public has higher requirements and expectations for display effects. The LED display industry has entered the era of ultra-high-definition display with "micro pitch, high brightness, high contrast, and high refresh". At present, the chip carriers of most LED display modules use a foot-wrapped bracket formed by substrate or mold stamping. The minimum shape of TOP bracket LED display devices is 0.1*0.1mm, which is not compatible with products with a pitch below P1.25. In addition, the bent corner bracket is used to carry the front-mounted chip. The device height is as high as 1mm, and the thickness of the panelized package plastic package is as high as 1.1mm. Affected by the environment and material matching, the process and reliability are hindered, the static module joints are white, the gaps are uneven, the flatness is poor, and there are a series of problems such as bright and dark lines in the dynamic joints. The device height is limited by the thermal conductivity of the packaging material itself, the mismatch of thermal expansion, and the limitations of the heat dissipation structure design, which limits the heat dissipation of the LED and the improvement of product reliability. At the same time, the package body is thick and cannot be made thin and light. The device size is large and the device is high, resulting in a high thickness of the plastic package, which cannot reduce the cost and has serious brightness loss. Utility Model Content
[0003] In order to solve the technical problems of high thickness of plastic package, reducing the amount of panel anti-collision glue, reducing the dot pitch while improving the thermal conductivity and enhancing the chip thrust, the utility model proposes a Mini LED display screen suitable for a minimum dot pitch of P0.44 and a reduced package size and a manufacturing process thereof, the purpose of which is to improve the electrical performance of the display panel while achieving lightweight packaging by improving the LED bracket structure and the LED display screen manufacturing process and / or the combined connection of the circuit.
[0004] In order to solve the above technical problems, the technical solution adopted by the utility model is: a Mini LED display screen, including a bracket, a pin, and a plastic package filling area, the bracket is provided with a dam, a chip pad and a common pole are provided in the dam, the chip pad is a groove structure, a tinning area and a Mini FC chip are provided on the chip pad, the tinning area is provided in the groove structure, and the tinning area and the Mini FC chip are provided on the front of the chip pad;
[0005] The Mini FC chip is electrically connected to the common pole;
[0006] The dam is arranged on the front side of the support;
[0007] The bracket is provided with pixel light source pads, and the pixel light source pads are electrically connected to the PCB circuit board;
[0008] The pixel light source pads are arranged on the back of the bracket, and an etching area is arranged on the back of the bracket;
[0009] The pixel light source pads and the etching area are arranged in partitions;
[0010] The chip pads are bridged between the pixel light source pads and the etching area;
[0011] The front sides of the pixel light source pads and the chip pads are electrically connected;
[0012] The front side of the etching area is electrically connected to the chip pads.
[0013] Furthermore, the Mini FC chips are arranged in a "T" shape or a "pin" shape.
[0014] Furthermore, the selective tin plating area is plated with tin using high-temperature solder paste, and there is a temperature difference between the solder paste used for the pixel light source pads.
[0015] Furthermore, the selective tin plating area is coated with flux by spraying flux.
[0016] Furthermore, the dam is filled with encapsulating colloid.
[0017] Furthermore, the bracket is provided with pixel light source polarity marks.
[0018] Furthermore, the etching area is formed by a semi-etching process.
[0019] Furthermore, the bracket is made of a 0.15 - 0.5 mm copper strip, and the etching depth of the etching area is 0.05 - 0.1 mm.
[0020] Furthermore, the chip pads can be formed by an etching process.
[0021] The beneficial effects of the present utility model compared with the prior art are as follows:
[0022] First, the back of the bracket of the present utility model forms an etching area by a semi-etching process, which improves the heat conduction performance of the display screen;
[0023] 2. The substrate of the utility model adopts 0.15-0.5mm copper tape, adopts Mini FC chip, and the chip pad adopts groove structure design. At the same time, the etching area is directly electrically connected to the chip pad, and the etching area is electrically connected to the PCB pad through the pixel light source pad, reducing the electroplating line. The utility model enhances the brightness of the display screen, improves the chip thrust, reduces the amount of anti-collision glue used for panelization of the display screen, and reduces the difficulty of the printing process. At the same time, it realizes a small-size TOP-type package, solves the bottleneck problem of the external size of the existing TOP-type LED device, and can be reduced to length * width * height = 0.7 * 0.7 * 0.45mm;
[0024] 3. The utility model adopts the GOB process to improve the air tightness and electrical reliability, and effectively solves the "caterpillar" problem;
[0025] Fourth, the chip pad of the utility model is designed with a groove structure, and is tinned by a selective tinning process, which saves costs and avoids the leakage of solder paste, affecting the consistency of ink color, and the problem of short product life caused by oxidation;
[0026] 5. The utility model adopts Mini FC flip chip to enhance the brightness of the display screen. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The utility model is further described below in conjunction with the accompanying drawings:
[0028] Figure 1 It is a structural schematic diagram of the utility model;
[0029] Figure 2 This is the first arrangement scheme of the Mini FC chip of the utility model;
[0030] Figure 3 This is the second arrangement scheme of the Mini FC chip of the utility model;
[0031] Figure 4 It is a rear view of the utility model;
[0032] In the figure: 1 is the encapsulation colloid, 2 is the dam, 3 is the pin, 4 is the plastic package filling area, 5 is the optional tin plating area, 6 is the MiniFC chip, 7 is the common pole, 8 is the chip pad, 9 is the pixel light source pad, 10 is the etching area, and 11 is the pixel light source polarity mark. DETAILED DESCRIPTION
[0033] In the present invention, unless otherwise specified, the directional words used, such as "up, down, top, bottom", usually refer to the directions shown in the drawings, or to the components themselves in the vertical, perpendicular or gravity directions; similarly, for ease of understanding and description, "inside and outside" refer to the inside and outside relative to the outline of each component itself, but the above-mentioned directional words are not used to limit the present invention.
[0034] As shown Figures 1 to 4 in the figure, the present utility model provides a Mini LED display screen, which includes a bracket, a pin 3, and a plastic encapsulation body filling area 4. The bracket is made of a copper strip with a thickness of 0.15 - 0.5 mm. A dam 2 is arranged on the bracket. A chip pad 8 and a common electrode 7 are arranged in the dam 2. The chip pad 8 is a groove structure. A selective tin plating area 5 and a Mini FC chip 6 are arranged on the chip pad 8. The selective tin plating area 5 is arranged in the groove structure. The selective tin plating area 5 and the Mini FC chip 6 are arranged on the front surface of the chip pad 8. Tin plating is carried out on the selective tin plating area 5 by using a selective tin plating process, such as coating solder paste by spraying a flux. The upper surface of the plated solder paste does not overflow the groove structure, reducing the tin plating amount and lowering the cost. The depth of the groove can be designed according to the chip height and tin amount requirements. The groove can be formed by an etching process. The common electrode 7 is a common anode or a common cathode;
[0035] The dam 2 is arranged on the front surface of the bracket;
[0036] A pixel light source pad 9 is arranged on the bracket, and the pixel light source pad 9 is electrically connected to a PCB circuit board;
[0037] The pixel light source pad 9 is arranged on the back surface of the bracket. An etching area 10 is arranged on the back surface of the bracket. The etching area 10 is formed by a semi-etching process. The etching height is 0.05 - 0.1 mm. The etching area 10 can provide heat dissipation for the LED lamp beads;
[0038] The chip pad 8 is bridged between the back surface of the pixel light source pad 9 and the back surface of the etching area 10;
[0039] The pixel light source pad 9 is electrically connected to the front surface of the chip pad 8, and the etching area 10 is electrically connected to the front surface of the chip pad 8,
[0040] The front surface of the bracket corresponds to the back surface of the bracket one by one.
[0041] The Mini FC chips 6 are arranged in a "T" shape or a "pin" shape. The minimum dot pitch of the LED lamp beads arranged in a "T" shape with the Mini FC chips 6 can reach P0.55, and the minimum dot pitch of the LED lamp beads arranged in a "pin" shape with the Mini FC chips 6 can reach P0.44. When using the Mini FC chips 6 at the same time, the brightness of the LED display screen can be increased by 100 - 150%;
[0042] The solder paste in the selective tin plating area 5 is plated with high-temperature solder paste, which has a temperature difference from the pixel light source pad 9, avoiding the influence of secondary reflow on the electrical performance of the Mini FC chip;
[0043] The dam 2 is filled with the encapsulating colloid 1. Compared with the prior art, the amount of the encapsulating colloid 1 used in GOB encapsulation is reduced by half, greatly reducing the cost.
[0044] The bracket is provided with a pixel light source polarity identifier 11.
[0045] The TOP type encapsulation process has good application market because of its characteristics of high temperature resistance, good dimensional stability, good sealing performance, low dropout rate, low dead lamp rate, good display effect and good heat dissipation. In the prior art, the TOP encapsulation process is limited by the bracket in reducing its size. When the lamp beads are reduced to a certain extent, only the CHIP type encapsulation technology can be adopted. The design of the present utility model breaks through this bottleneck, realizing that products with a minimum pitch of P0.44 can still adopt the TOP type encapsulation process. After encapsulation, the external dimensions of the LED can be reduced to 0.7mm in length, 0.7mm in width and 0.45mm in height respectively.
[0046] The present utility model reduces the external dimensions of the LED, further reduces the thickness of the module plastic encapsulation, reduces the problem of light loss caused by the plastic encapsulation body, greatly improves the utilization rate of the chip, further improves the heat dissipation and reliability of the pixel light source, reduces the problem of display screen color change caused by heat dynamically, and at the same time reduces the thickness of the module plastic encapsulation body, enhances the stress matching between the encapsulating colloid 1 and the module material, reduces the damage to the module caused by stress under temperature change, and avoids the problems of cracking and delamination of the encapsulating colloid 1 in the module under high temperature or low temperature conditions.
[0047] The manufacturing process flow of the present utility model is as follows:
[0048] S1. The bracket uses a copper strip with a thickness of 0.2mm. An etching area 10 is formed on the back of the bracket by a semi-etching process. The etching height is 0.05 - 0.1mm. After etching, it is filled with a plastic encapsulation body to protect the bracket. The dam 2 structure is set on the front of the bracket through a plastic encapsulation process, realizing the functions of pixel light isolation and light reflection, preventing light crosstalk, improving the luminous intensity at the same time, and reducing the problem of bright and dark lines at the seam. A chip pad 8 is arranged in the dam 2 structure. A Mini FC chip 6 is arranged on the chip pad 8. The Mini FC chip 6 adopts a "T" shape or a "pin" shape to improve the utilization rate of the base material. The chip pad 8 adopts a groove structure, and the groove structure can also be formed by an etching process. The groove depth is designed according to the chip height and the requirement of the solder paste amount. A selective tin plating area 5 is arranged in the groove structure. Tin plating is carried out on the selective tin plating area 5 through a selective tin plating process. The etching area 10 on the back of the chip pad 8 is electrically connected to the front of the chip pad 8. The pixel light source pad 9 is electrically connected to the front of the chip pad 8, reducing the electroplating line, further miniaturizing the pitch, and significantly improving the thermal conductivity.
[0049] S2, coating the selected tin-plating area 5 with solder paste by spraying flux, and fixing the Mini FC chip 6 on the chip pad 8 by a die-bonding process;
[0050] S3, using a high-precision dispensing machine or screen printing process to fill the dam 2 with the encapsulating colloid 1 to fix the MiniFC chip 6, protect the Mini FC chip 6, and form a pixel light source. The specific model of the high-precision dispensing machine is BD8100;
[0051] S4, separating the pixel light source from the bracket by extrusion blanking;
[0052] S5, after passing the test, subdividing the pixel light source and performing tape weaving;
[0053] S6. Spray the soldering flux on the PCB board through a spraying process to make the soldering flux evenly coated, or tinning can be performed through a tinning process;
[0054] S7, complete solder paste eutectic through reflow soldering or laser process to achieve electrical connection between pixel light source and PCB board;
[0055] S8. GOB packaging technology is used to form modules, assemble modules, and form display screens, which reduces the number of physical seams, reduces the impact of seams on the display screen display effect and static consistency, and can solve the problems of module splicing gaps and bright and dark lines. When the size of a single module is larger than 27 inches, the number of physical seams on the entire screen is halved, and the point light source is transformed into a surface light surface, which greatly improves airtightness and reliability, and can solve the "caterpillar" problem.
[0056] Regarding the specific structure of the utility model, it should be explained that the connection relationship between the various component modules adopted in the utility model is definite and feasible. Except for special instructions in the embodiments, the specific connection relationship can bring corresponding technical effects and solve the technical problems raised by the utility model without relying on the execution of corresponding software programs. The components, modules, models of specific components and the connection methods between each other appearing in the utility model, as well as the conventional use methods and expected technical effects brought about by the above-mentioned technical features, except for specific instructions, all belong to the disclosed contents in patents, journal articles, technical manuals, technical dictionaries, and textbooks that can be obtained by technical personnel in this field before the application date, or belong to the existing technologies such as conventional technologies and common knowledge in this field, and there is no need to elaborate, so that the technical solution provided in this case is clear, complete and feasible, and the corresponding physical products can be reproduced or obtained according to the technical means.
[0057] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solution deviate from the scope of the technical solution of the embodiments of the utility model.
Claims
1. A Mini LED display screen, comprising a bracket, pins (3), and a plastic package filling area (4), characterized in that: A dam (2) is provided on the bracket. A chip pad (8) and a common electrode (7) are provided inside the dam (2). The chip pad (8) is of a groove structure. A selective tin plating area (5) and a Mini FC chip (6) are provided on the chip pad (8). The selective tin plating area (5) is arranged inside the groove structure. The selective tin plating area (5) and the Mini FC chip (6) are arranged on the front side of the chip pad (8). The Mini FC chip (6) is electrically connected to the common electrode (7). The dam (2) is arranged on the front side of the bracket. A pixel light source pad (9) is provided on the bracket. The pixel light source pad (9) is electrically connected to a PCB circuit board. The pixel light source pad (9) is arranged on the back side of the bracket. An etching area (10) is provided on the back side of the bracket. The pixel light source pad (9) and the etching area (10) are arranged in a partitioned manner. The chip pad (8) is bridged between the pixel light source pad (9) and the etching area (10). The pixel light source pad (9) is electrically connected to the front side of the chip pad (8). The etching area (10) is electrically connected to the front side of the chip pad (8).
2. A Mini LED display according to claim 1, characterized in that: The Mini FC chips (6) are arranged in a "T" shape or a "pin" shape.
3. The Mini LED display according to claim 1, characterized in that: The selective tin plating area (5) is plated with tin using high-temperature solder paste, and there is a temperature difference from the solder paste used for the pixel light source pad (9).
4. The Mini LED display according to claim 1, characterized in that: The selective tin plating area (5) is coated with flux by means of spraying flux.
5. The Mini LED display according to claim 1, characterized in that: The dam (2) is filled with an encapsulation colloid (1).
6. The Mini LED display according to claim 1, characterized in that: A pixel light source polarity mark (11) is provided on the bracket.
7. The Mini LED display according to claim 1, characterized in that: The etching area (10) is formed by a semi-etching process.
8. The Mini LED display screen according to claim 1, characterized in that: The bracket is made of a copper strip with a thickness of 0.15 - 0.5 mm, and the etching depth of the etching area (10) is 0.05 - 0.1 mm.
9. The Mini LED display screen according to claim 1, characterized in that: The chip pad (8) can be formed by an etching process.
Citation Information