High-pulling-speed small square billet continuous casting crystallizer
By using an inner water jacket and a multi-sink structure in the square-bill continuous casting crystallizer to achieve uniform cooling and support of copper pipes, the problem of uneven cooling of copper pipes at high pull speed is solved, and the service life and uniformity of the blank shell is improved. reduces the risk of steel leakage.
Patent Information
- Application Number
- CN202420555135.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-21
- Publication Date
- 2024-11-05
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Under high-pull speed continuous casting conditions, the copper tube of the billet crystallizer is unevenly cooled due to uneven cooling, which increases the risk of steel leakage accidents and reduces the strength and service life of the crystallizer.
A high-pull speed square billet continuous casting crystallizer is designed, adopting an inner water jacket and multiple sink structures. The cooling water flows out from the upper part of the copper tube through the sink to ensure uniform cooling of the copper tube and a buffer is set at the corners. The groove is used to increase the thickness of the slag layer, prevent the liquid steel from flowing into the buffer groove, and achieve corner cooling uniformity.
Through uniform cooling and support structure, the service life of the crystallizer and the strength of the copper tube are improved, and the uneven growth of the blank shell and the occurrence of steel leakage accidents are reduced.
Smart Images

Figure CN221952272U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of continuous steel casting, in particular to a high-speed billet continuous casting crystallizer. Background Art
[0002] The crystallizer is the heart of the continuous casting machine and also the cavity where the molten steel solidifies. In the continuous casting process of steel, the molten steel completes the initial solidification in the water-cooled crystallizer to form a solidified shell with a certain strength to ensure that the shell can withstand the static pressure of the molten steel and prevent the shell from breaking after it leaves the crystallizer under the support of the roller array and its own shell structure.
[0003] In recent years, with the development of efficient continuous casting technology, the continuous casting speed has been improved to varying degrees. In particular, for small square billets, in order to adapt to the production capacity of subsequent rolling mills, the pulling speed needs to be increased to more than 5m / min. The increase in pulling speed means that the shell of the small square billet in the crystallizer becomes thinner, the temperature of the copper tube of the crystallizer rises, and the strength decreases. However, for traditional small square billet crystallizers, since the copper tube is cooled by an annular water gap, under high pulling speed conditions, even if the cooling water flow rate is increased, the crystallizer cooling water jacket with a single tube inlet and outlet water outside the copper tube cannot achieve uniform cooling of the copper tube circumference. While causing uneven growth of the billet shell, it will also cause uneven deformation of the copper tube of the crystallizer, which will further aggravate the uneven growth of the billet shell and lead to steel leakage accidents. The strength and service life of the copper tube of the crystallizer will also be greatly reduced. Therefore, in order to adapt to high-speed continuous casting, the copper tube of the small square billet crystallizer must solve the problems of cooling uniformity and its own strength during use.
[0004] In order to solve the above problems, a high-speed billet continuous casting crystallizer is proposed. Utility Model Content
[0005] The utility model aims to provide a high-speed billet continuous casting crystallizer in order to solve the above problems.
[0006] The technical solution adopted by the utility model is as follows: a high-speed billet continuous casting crystallizer, comprising:
[0007] The water jacket in the crystallizer has a cavity disposed therein;
[0008] The crystallizer copper tube is fixedly installed inside the cavity. The crystallizer copper tube also includes a tube body. The outer walls of the tube body are each provided with a plurality of water grooves. A solidification cavity is provided in the middle of the tube body. Buffer grooves are provided at the four corners of the solidification cavity.
[0009] Through the above technical scheme, when the molten steel is ready to be poured, cold water is introduced into the water jacket in the crystallizer, and the cooling water enters from the upper part of the copper tube of the crystallizer through multiple water troughs at the same time and flows out from the lower part to cool the crystallizer. The cooling water enters from the top and flows out from the bottom, which can improve the cooling capacity of the meniscus area of the crystallizer, reduce the meniscus temperature, and increase the service life of the crystallizer. The water jacket in the crystallizer supports the copper tube of the crystallizer in the axial direction through the water trough interval, so as to achieve uniform deformation and uniform cooling of the copper tube of the crystallizer. When the molten steel solidifies in the solidification chamber, the molten steel flows into the crystallizer through an immersed water nozzle. Therefore, the molten steel will not flow into the buffer tank of the crystallizer during the initial solidification. The buffer tank position will contact with the continuous casting protective slag, increase the thickness of the slag layer, and achieve slow cooling of the corner to ensure the uniformity of the cooling of the billet shell near the corner of the crystallizer.
[0010] In a preferred embodiment, the tube body is made of AgCu, and the wall thickness of the tube body is 15-25 mm.
[0011] In a preferred embodiment, the buffer groove is a conical structure, and its depth is 0.3-0.5 times the wall thickness of the tube body.
[0012] In a preferred embodiment, the water tank is a rectangular structure.
[0013] In a preferred embodiment, the number of the water troughs located on a single side of the tube body is 5-7, and the multiple water troughs are horizontally equidistantly distributed.
[0014] In a preferred embodiment, the four corners of the tube body are all arc-shaped structures.
[0015] In summary, due to the adoption of the above technical solution, the beneficial effects of the utility model are as follows: the utility model provides a high-speed billet continuous casting crystallizer.
[0016] 1. The cooling water adopts a trough-type channel, which solves the problem that the water-seam copper tube has no circumferential support and is prone to uneven deformation.
[0017] 2. By opening multiple water grooves on the outside of the copper tube of the crystallizer, it can be ensured that cooling water flows in simultaneously along the circumference of the copper tube, ensuring the consistency of the cooling water temperature around the crystallizer, and solving the problem of low temperature at the water inlet position of the water-slit copper tube and slightly higher temperature at other circumferential positions.
[0018] 3. By making grooves at the corners of the crystallizer, on the one hand, the heat transfer at the corners of the crystallizer is slowed down, and on the other hand, a protective slag layer slightly thicker than other areas is formed at the corners to increase the thermal resistance, further slowing down the uneven solidification of the corner area during the initial solidification of the billet shell. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a top view of the utility model;
[0020] Figure 2 It is a top view of the crystallizer copper tube in the utility model.
[0021] Markings in the figure: 1-water jacket in crystallizer; 2-crystallizer copper tube; 21-tube body; 22-water tank; 23-solidification chamber; 24-buffer tank. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solution and advantages of the embodiments of the utility model clearer, the technical solution in the embodiments of the utility model will be clearly and completely described below in combination with the embodiments of the utility model. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0023] The following will be combined Figure 1-2 A high-speed billet continuous casting crystallizer according to an embodiment of the utility model is described in detail.
[0024] Example:
[0025] A high-speed billet continuous casting crystallizer, comprising:
[0026] The inner water jacket 1 of the crystallizer has a cavity therein, and the inner water jacket 1 of the crystallizer supports the crystallizer copper tube 2 in the axial direction to achieve uniform deformation and uniform cooling of the crystallizer copper tube 2;
[0027] The crystallizer copper tube 2 is fixedly installed inside the cavity. The crystallizer copper tube 2 also includes a tube body 21. The four corners of the tube body 21 are all arc-shaped structures. The tube body 21 is made of AgCu material. The wall thickness of the tube body 21 is 15-25mm. A plurality of water tanks 22 are provided on the four outer walls of the tube body 21. The water tanks 22 are rectangular structures. The number of water tanks 22 located on a single side of the tube body 21 is 5-7, and the plurality of water tanks 22 are horizontally equidistantly distributed. When the molten steel is ready to be poured, cold water is introduced into the water jacket 1 in the crystallizer. The cooling water enters from the upper part of the crystallizer copper tube 2 through the plurality of water tanks 22 at the same time and flows out from the lower part to realize cooling of the crystallizer. The cooling water enters from the upper part and flows out from the lower part, which can improve the cooling capacity of the meniscus area of the crystallizer, reduce the meniscus temperature, and improve the service life of the crystallizer.
[0028] A solidification cavity 23 is opened in the middle of the tube body 21, and buffer grooves 24 are arranged at the four corners of the solidification cavity 23. The buffer groove 24 is a conical structure, and its depth is 0.3-0.5 times the wall thickness of the tube body 21. When the molten steel solidifies in the solidification cavity 23, the molten steel flows into the crystallizer through an immersed water nozzle. Therefore, the molten steel will not flow into the buffer groove 24 of the crystallizer during the initial solidification. The buffer groove 24 will contact with the continuous casting protective slag, increase the thickness of the slag layer, and realize slow cooling of the corners, so as to ensure the uniformity of the cooling of the billet shell near the corners of the crystallizer.
[0029] Working principle:
[0030] When the molten steel is ready to be poured, cold water is introduced into the water jacket 1 in the crystallizer. The cooling water enters from the upper part of the crystallizer copper tube 2 through multiple water troughs 22 at the same time and flows out from the lower part to cool the crystallizer. The cooling water enters from the top and flows out from the bottom to improve the cooling capacity of the meniscus area of the crystallizer, reduce the meniscus temperature, and increase the service life of the crystallizer. The water jacket 1 in the crystallizer supports the crystallizer copper tube 2 in the axial direction through the water troughs 22, so as to achieve uniform deformation and uniform cooling of the crystallizer copper tube 2. When the molten steel solidifies in the solidification chamber 23, the molten steel flows into the crystallizer using an immersed water inlet. Therefore, the molten steel will not flow into the crystallizer buffer tank 24 during the initial solidification. The buffer tank 24 will contact with the continuous casting protective slag, increase the thickness of the slag layer, and achieve slow cooling of the corner to ensure the uniformity of the cooling of the billet shell near the corner of the crystallizer.
[0031] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A high-speed billet continuous casting crystallizer, characterized in that: include: A water jacket (1) in the crystallizer, wherein a cavity is provided inside the water jacket; A crystallizer copper tube (2) is fixedly installed inside the cavity. The crystallizer copper tube (2) also includes a tube body (21). The four outer walls of the tube body (21) are each provided with a plurality of water grooves (22). A solidification cavity (23) is provided in the middle of the tube body (21). Buffer grooves (24) are each provided at the four corners of the solidification cavity (23).
2. A high-speed billet continuous casting crystallizer according to claim 1, characterized in that: The tube body (21) is made of AgCu material, and the wall thickness of the tube body (21) is 15-25 mm.
3. A high-speed billet continuous casting crystallizer according to claim 1, characterized in that: The buffer groove (24) is a conical structure, and its depth is 0.3-0.5 times the wall thickness of the tube body (21).
4. A high-speed billet continuous casting crystallizer according to claim 1, characterized in that: The water tank (22) is a rectangular structure.
5. The high-speed billet continuous casting crystallizer according to claim 1, characterized in that: The number of the water grooves (22) located on a single side of the tube body (21) is 5-7, and the plurality of water grooves (22) are horizontally equidistantly distributed.
6. A high-speed billet continuous casting crystallizer according to claim 1, characterized in that: The four corners of the tube body (21) are all arc-shaped structures.