Film getter structure for improving activation temperature uniformity

By gradually narrowing the stainless steel or Kerva substrate of the film getter, the problem of temperature unevenness during activation is solved, the intake capacity is improved, and more uniform heat transfer and greater intake efficiency is achieved. .

CN221971275UActive Publication Date: 2024-11-08NANJING HUADONG ELECTRONICS VACUUM MATERIAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323632485.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2024-11-08
Estimated Expiration
2033-12-29

AI Technical Summary

Technical Problem

The existing film getters have temperature unevenness problems when activated, resulting in loss of suction capacity, especially the lowest temperature near the welding boss, resulting in a decrease in suction capacity.

Method used

By gradually narrowing the getter structure at both ends of stainless steel or flake-mounted substrate, the current density at both ends is increased to compensate for the uneven heat transfer, and the design width gradually narrows to 3/4 of the maximum width at both ends of the length direction. To 1/2, and set a constant width zone of 1/4 to 1/2 in the center to improve temperature uniformity.

Benefits of technology

It effectively improves the room temperature intake capacity of the film getter, reduces the temperature difference between the center and the edge of the welding boss, and improves the temperature uniformity during activation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221971275U_ABST
    Figure CN221971275U_ABST
Patent Text Reader

Abstract

The utility model relates to a film getter structure for improving activation temperature uniformity, which is characterized in that getter films are deposited on two sides of sheet-mounted metal such as stainless steel and kovar, the width of the getter is provided with areas which are gradually narrowed at two ends in the length direction, and the broadband is narrowed to 3 / 4 to 1 / 2 of the maximum width. And heat transfer of a welding position is compensated, so that the temperature uniformity of the thin film getter during activation is improved, and the room-temperature getter capacity of the thin film getter is further improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of electronic component materials, and more specifically to a thin film getter structure capable of improving the uniformity of activation temperature. Background Art

[0002] In recent years, as various MEMS devices have become smaller, flatter, and more integrated, the getters they require have gradually evolved from sintered non-evaporable getters to PVD deposited thin film getters. Figure 1 The thin film getter used in MEMS devices is generally a getter alloy such as zirconium vanadium iron, titanium zirconium vanadium, etc. in the form of a thin film ( Figure 1 4) Deposited on a long strip substrate with stainless steel, Kovar and other metal materials as the substrate ( Figure 1 To avoid the film from contacting the soldering bosses in the MEMS device ( Figure 1 1) Collision causes reliability problems, and the length of the deposited film is less than the spacing between the bosses. The thin film getter is fixed to the boss by resistance welding or laser welding the end of the blank position. Figure 1 The 2 in the figure is a weld scar formed by welding. During the MEMS device baking exhaust or after exhaust sealing, the heat generated by energizing the long strip substrate is transferred to the surface to activate the thin film getter alloy on the surface.

[0003] The air absorption capacity of the thin film getter after activation and cooling to room temperature gradually increases with the increase of temperature, and then begins to decrease. When the temperature is low, the passivation layer on the surface of the getter alloy cannot quickly diffuse into the interior of the alloy to expose the active surface. The higher the temperature, the faster the diffusion, the more active surfaces are exposed, and the greater the air absorption capacity after cooling. However, when the temperature is too high, as the getter alloy sinters, its room temperature air absorption capacity after cooling will be greatly reduced. The activation temperature range for obtaining 80% of the maximum room temperature air absorption capacity is generally less than 100°C.

[0004] When the thin film getter of the prior art is activated by electricity, the temperature in the center of the thin film getter is the highest. Due to the strong heat conduction of the welding boss, the temperature near the welding point is the lowest. The temperature difference between the two increases with the increase of current. Generally, the difference between the two is 200-300℃. This uneven temperature during activation also causes the loss of the air absorption capacity of the thin film getter in practical applications. In view of this, we propose a thin film getter structure that improves the uniformity of activation temperature. Utility Model Content

[0005] The utility model aims to provide a thin film getter structure for improving the uniformity of activation temperature, so as to solve the problems raised in the above background technology.

[0006] In order to achieve the above purpose, the utility model provides the following technical solutions:

[0007] A thin film getter structure for improving the uniformity of activation temperature. The getter film is deposited on both sides of a sheet-mounted base metal such as stainless steel or Kovar, and the width of the getter has gradually narrowing areas at both ends in the length direction.

[0008] Preferably, the width of the getter gradually narrows to 3 / 4 to 1 / 2 of the maximum width at both ends in the length direction.

[0009] Preferably, the width of the getter has a constant width region of 1 / 4 to 1 / 2 of the total length in the center in the length direction.

[0010] Compared with the prior art, the beneficial effects of the utility model are:

[0011] The width of the getter gradually narrows to 3 / 4 to 1 / 2 of the maximum width at both ends in the length direction. Due to the increase in current density at both ends, the heat transfer through the welding position is compensated, thereby improving the temperature uniformity of the thin film getter when activated, thereby improving the room temperature getter capacity of the thin film getter. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 Attached Figure 1 It is a schematic diagram of the application of thin film getter in the prior art to MEMS devices.

[0013] 1 in the figure is the boss of the welded thin film getter of the MEMS device, which leads to the outside of the MEMS device; 2 in the figure is the weld scar formed by welding the substrate of the thin film getter to the boss by resistance welding or laser welding; 3 in the figure is a long strip sheet substrate such as stainless steel and Kovar; 4 in the figure is the getter alloy film deposited on both sides of the substrate (generally, the two ends are left empty and not deposited to avoid contact between the welding boss and the deposited getter alloy).

[0014] Attached Figure 2 It is a schematic diagram of the structure of a thin film getter for improving the air absorption efficiency.

[0015] 1 in the figure is a connecting rib for easy overall processing (usually it is removed when welding the getter, but it can be retained if space permits); 2 in the figure is a welding area without deposited getter film; 3 in the figure is a deposited getter film. The constant width area in the figure is optional. DETAILED DESCRIPTION

[0016] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0017] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0018] In the description of this patent, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", and "set" should be understood in a broad sense, for example, it can be fixedly connected or set, or it can be detachably connected or set, or connected or set in one piece. For ordinary technicians in this field, the specific meanings of the above terms in this patent can be understood according to specific circumstances.

[0019] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present utility model, the meaning of "several" is two or more, unless otherwise clearly and specifically defined.

[0020] The technical solution of the utility model is: the getter film is deposited on both sides of the sheet-mounted base metal such as stainless steel and Kovar by the PVD method. The width of the metal base has gradually narrowed areas at both ends in the length direction. According to the actual heat dissipation situation, in order to maximize the area of ​​the getter film, a constant width area can be selected between the two narrowing areas, and the length of the constant width area is 1 / 4 to 1 / 2 of the total length of the getter.

[0021] The width of the getter tapers to 3 / 4 to 1 / 2 of the maximum width at both ends of the length. The exact amount of shrinkage depends on the temperature difference between the center temperature when the getter is activated and the temperature at the soldering location. The greater the temperature difference, the greater the shrinkage required. The shrinkage can be linear or can be finely curvatured according to the original temperature distribution without shrinkage.

[0022] In addition to the shrinkage areas at both ends, welding areas without deposited getter and rib areas for easy processing can be left as needed. There is no limit on the size and shape of these areas.

[0023] The width of the getter gradually narrows at both ends in the length direction. Due to the increase in current density at both ends, the heat transfer through the welding position is compensated, thereby improving the temperature uniformity of the thin film getter when activated, and then improving the room temperature getter capacity of the thin film getter.

[0024] The technical solutions and advantages of the present utility model are further described below based on embodiments. Example

[0025] A stainless steel with a thickness of 0.05mm is processed into a whole array composed of many units by etching. Each unit of the array has a 6mm constant width area in the center, and the length of the narrowing area at both ends is 6mm, and the width gradually narrows linearly from 1.8mm to 1.2mm. Outside the narrowing areas at both ends, there is a welding area with a width of 1.2mm and a length of 1mm. Outside the two welding areas, there is a rib area with a width of 0.5mm and a length of 1mm. All units are connected into a whole by ribs for subsequent processing. Through a mask, a 2μm titanium zirconium cobalt cerium getter film is deposited on both sides of the constant width area and the narrowing area.

[0026] Solder one element of the array to Figure 1 The shell shown in the figure was evacuated and powered on, and the surface temperature of the center of the getter and the edge of the welding boss was measured respectively, and the temperature difference was 30°C. The temperature difference of the sample without the narrowing area was about 180°C when tested under the same conditions. Although the area of ​​the getter film of the utility model is smaller than that of the comparative sample, the carbon monoxide absorption capacity at room temperature under the same conditions was tested, and the use of the utility model increased by about 11%.

[0027] The above shows and describes the basic principle, main features and advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments. The above embodiments and descriptions are only preferred examples of the utility model and are not used to limit the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, which fall within the scope of the utility model to be protected. The scope of protection of the utility model is defined by the attached claims and their equivalents.

Claims

1. A thin film getter structure for improving activation temperature uniformity, characterized in that: The getter film is deposited on both sides of a mounting base metal including stainless steel and Kovar sheet, the width of which has gradually narrowed areas at both ends in the length direction.

2. A thin film getter structure for improving activation temperature uniformity according to claim 1, characterized in that: A constant width zone is arranged between the two narrowed zones, and the length of the constant width zone is 1 / 4 to 1 / 2 of the total length of the getter.

3. A thin film getter structure for improving activation temperature uniformity according to claim 1, characterized in that: The width of the getter gradually narrows to 3 / 4 to 1 / 2 of the maximum width at both ends in the length direction.