Electronic power assembly

The leakage current and breakdown voltage instability problems in electronic power components are solved by forming peripheral grooves on the semiconductor substrate, deposition of oxygen-doped polysilicon and glass layers, and etching and deposition of electrical insulating layers in appropriate steps, simplifying the problem of leakage current and breakdown voltage instability in electronic power components The manufacturing process is reduced and manufacturing costs are reduced.

CN222029043UActive Publication Date: 2024-11-19STMICROELECTRONICS INT NV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420291885.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Priority Date
2024-01-23
Filing Date
2024-02-08
Publication Date
2024-11-19
Estimated Expiration
2034-02-08

AI Technical Summary

Technical Problem

Existing electronic power components have problems of leakage current and breakdown voltage instability during manufacturing, especially when using MESA technology, where large groove depths lead to increased etching complexity and manufacturing costs.

Method used

The peripheral groove is formed on the first surface of the semiconductor substrate, an oxygen-doped polysilicon layer is deposited and a glass layer is locally deposited thereon, an oxygen-doped polysilicon layer is etched to extend it beyond the glass layer, and an electrically insulating layer is deposited at appropriate steps to reduce Leakage current and increase breakdown voltage.

Benefits of technology

Through this method, leakage current is reduced and breakdown voltage is increased, the manufacturing process is simplified, and the manufacturing cost is reduced. Components with groove depths greater than 75 μm can effectively passivate the sides and bottom, enhancing the stability of the components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222029043U_ABST
    Figure CN222029043U_ABST
Patent Text Reader

Abstract

The utility model relates to an electronic power assembly. The present disclosure relates to a method of forming an electronic power component inside and on top of a semiconductor substrate, comprising the following consecutive steps: a) forming a peripheral recess in the semiconductor substrate on one side of a first surface of the semiconductor substrate; b) depositing an oxygen-doped polysilicon layer on and in contact with the bottom of the peripheral recess and the top of the sidewalls and on and in contact with the top of the first surface of the semiconductor substrate; c) locally depositing a glass layer on the oxygen-doped polysilicon layer, the glass layer extending in the peripheral recess and further extending over a portion of the first surface of the semiconductor substrate; and d) etching the oxygen-doped polysilicon layer such that it extends beyond the glass layer on the first surface of the semiconductor substrate.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATION(S)

[0002] This application claims the benefit of priority to French patent application No. 2301163, filed on February 8, 2023, entitled “Formation d'un composantélectronique de puissance”, which is hereby incorporated by reference to the fullest extent permitted by law. Technical Field

[0003] The present disclosure relates generally to semiconductor electronic components, and more particularly to electronic power components, such as thyristors and triacs. Background Art

[0004] Different technologies for power components and for manufacturing these components are known. The MESA technology is particularly known, which consists in surrounding a PN junction formed in the entire surface of the component with a groove filled with glass on at least one surface of the component as a termination of the junction.

[0005] There is a purpose to improve electronic power components, in particular MESA technology electronic components and their manufacturing technology. More specifically, there is a purpose to stabilize the leakage current in these components and / or increase the breakdown voltage in these components. Summary of the invention

[0006] To achieve this, an embodiment provides a method of forming an electronic power component in and on top of a semiconductor substrate, comprising the following consecutive steps:

[0007] a) forming a peripheral groove in the semiconductor substrate on one side of the first surface of the semiconductor substrate;

[0008] b) depositing an oxygen-doped polysilicon layer on and in contact with the bottom and top of the sidewalls of the peripheral recess and on and in contact with the top of the first surface of the semiconductor substrate;

[0009] c) locally depositing a glass layer on the oxygen-doped polysilicon layer, the glass layer extending in the peripheral recess and further extending over a portion of the first surface of the semiconductor substrate; and

[0010] d) etching the oxygen-doped polysilicon layer so that it extends beyond the glass layer on the first surface of the semiconductor substrate.

[0011] According to an embodiment, the method comprises, between steps b) and c), a step e) of depositing an electrically insulating layer on top of and in contact with the oxygen-doped polysilicon layer.

[0012] According to an embodiment, the method comprises a step e) between steps c) and d): depositing an electrically insulating layer on top of and in contact with the glass layer and a portion of the oxygen-doped polysilicon layer not covered by the glass layer.

[0013] According to an embodiment, during step d), the electrically insulating layer is etched simultaneously with the oxygen-doped polysilicon layer.

[0014] According to an embodiment, the deposition of the glass layer during step c) is performed by screen printing.

[0015] According to an embodiment, the grooves have a depth greater than 75 μm.

[0016] According to an embodiment, the thickness of the oxygen-doped polysilicon layer is in the range of 0.1 μm to 2 μm.

[0017] Another embodiment provides an electronic power assembly, comprising:

[0018] a peripheral groove formed in the semiconductor substrate on one side of the first surface of the semiconductor substrate;

[0019] an oxygen-doped polysilicon layer formed on and in contact with the bottom and top of the sidewalls of the peripheral recess and on and in contact with the first surface of the semiconductor substrate; and

[0020] A glass layer is formed on the oxygen-doped polysilicon layer, the glass layer extending in the peripheral groove and further extending on a portion of the first surface of the semiconductor substrate, and the oxygen-doped polysilicon layer extends beyond the glass layer on the first surface of the semiconductor substrate.

[0021] According to an embodiment, the component includes an electrically insulating layer between the oxygen-doped polysilicon layer and the glass layer, the electrically insulating layer contacting the oxygen-doped polysilicon layer via a first surface and contacting the glass layer via a second surface opposite to the first surface.

[0022] According to an embodiment, the component includes an electrically insulating layer, the glass layer contacts the electrically insulating layer via a first surface and contacts the oxygen-doped polysilicon layer via a second surface opposite to the first surface, and the electrically insulating layer contacts a portion of the oxygen-doped polysilicon layer not covered by the glass layer.

[0023] According to an embodiment, the grooves have a depth greater than 75 μm.

[0024] According to an embodiment, the thickness of the oxygen-doped polysilicon layer is in a range of 0.1 μm to 2 μm.

[0025] Another embodiment provides a power control circuit including the described electronic power assembly.

[0026] According to one aspect of the present disclosure, a method for forming an electronic power component is provided, comprising: forming a peripheral groove in a first surface of a semiconductor substrate; depositing an oxygen-doped polysilicon layer, the oxygen-doped polysilicon layer being on and in contact with a bottom and a top of a plurality of sidewalls of the peripheral groove, and on and in contact with a top of the first surface of the semiconductor substrate; locally depositing a glass layer on the oxygen-doped polysilicon layer, the glass layer extending in the peripheral groove and further extending over a portion of the first surface of the semiconductor substrate; and etching the oxygen-doped polysilicon layer so that the oxygen-doped polysilicon layer extends beyond the glass layer on the first surface of the semiconductor substrate.

[0027] According to an embodiment, an electronic power component forming method includes, between depositing an oxygen-doped polysilicon layer and partially depositing a glass layer, depositing an electrically insulating layer on top of and in contact with the oxygen-doped polysilicon layer.

[0028] According to an embodiment, an electronic power component forming method includes, between locally depositing a glass layer and etching an oxygen-doped polysilicon layer, depositing an electrically insulating layer on top of and in contact with the glass layer and a portion of the oxygen-doped polysilicon layer not covered by the glass layer.

[0029] According to an embodiment, during the etching of the oxygen-doped polysilicon layer, the electrically insulating layer is etched simultaneously with the oxygen-doped polysilicon layer.

[0030] According to an embodiment, wherein the deposition of the glass layer is performed by screen printing.

[0031] According to an embodiment, the grooves have a depth greater than 75 μm.

[0032] According to an embodiment, the thickness of the oxygen-doped polysilicon layer is in a range of 0.1 μm to 2 μm.

[0033] According to one aspect of the present disclosure, an electronic power component is provided, comprising: a peripheral groove in a semiconductor substrate, on one side of a first surface of the semiconductor substrate; an oxygen-doped polysilicon layer, on and in contact with the bottom and top of the sidewalls of the peripheral groove, and on and in contact with the top of the first surface of the semiconductor substrate; and a glass layer, on the oxygen-doped polysilicon layer, the glass layer extending in the peripheral groove and on a portion of the first surface of the semiconductor substrate, and the oxygen-doped polysilicon layer extending beyond the glass layer on the first surface of the semiconductor substrate.

[0034] According to an embodiment, an electronic power component includes an electrical insulation layer between an oxygen-doped polysilicon layer and a glass layer, the electrical insulation layer contacting the oxygen-doped polysilicon layer through a first surface and contacting the glass layer through a second surface opposite to the first surface.

[0035] According to an embodiment, the electronic power component includes an electrically insulating layer, the glass layer contacts the electrically insulating layer through a first surface and contacts the oxygen-doped polysilicon layer through a second surface opposite to the first surface, and the electrically insulating layer contacts a portion of the oxygen-doped polysilicon layer not covered by the glass layer.

[0036] According to an embodiment, the grooves have a depth greater than 75 μm.

[0037] According to an embodiment, the thickness of the oxygen-doped polysilicon layer is in a range of 0.1 μm to 2 μm.

[0038] According to one aspect of the present disclosure, a method is provided, comprising: forming a groove in a first surface of a substrate; forming an oxygen-doped polysilicon layer in the groove and on the first surface of the substrate; forming an insulating layer on the oxygen-doped polysilicon layer and in contact with the oxygen-doped polysilicon layer; forming a glass layer on the oxygen-doped polysilicon layer; and forming a conductive layer on the first surface of the substrate, the conductive layer being in contact with the oxygen-doped polysilicon layer.

[0039] According to an embodiment, wherein the groove extends through a central portion of the substrate having a first doping concentration and an outer portion of the substrate having a second doping concentration different from the first doping concentration.

[0040] According to an embodiment, wherein the outer portion of the substrate increases with a gradient from the central portion of the substrate to the first side of the substrate.

[0041] According to an embodiment, wherein the interface between the outer portion of the substrate and the central portion of the substrate is a PN junction.

[0042] According to an embodiment, the method includes forming a doped region in a substrate coplanar with a first surface of the substrate.

[0043] According to an embodiment, the conductive layer is in contact with the doped region.

[0044] According to an embodiment, the glass layer is located between the oxygen-doped polysilicon layer and the insulating layer.

[0045] According to an embodiment, the insulating layer is located between the oxygen-doped polysilicon layer and the glass layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] The above features and advantages as well as other features and advantages will be described in detail in the remainder of the present disclosure of specific embodiments given by way of example and not limitation with reference to the accompanying drawings, in which:

[0047] Figure 1A , Figure 1B , Figure 1C , Figure 1D and Figure 1EThe following are partially simplified cross-sectional views showing the sequential steps of an example of a method for manufacturing a power component according to a first embodiment; and

[0048] Figure 2A , Figure 2B , Figure 2C and Figure 2D Successive steps of an example of a method for producing a power component according to a second embodiment are shown in partially simplified sectional views. DETAILED DESCRIPTION

[0049] Similar features are denoted by similar reference numerals in the various figures. In particular, common structural and / or functional features between various embodiments may have the same reference numerals and may be provided with the same structure, dimensions, and material properties.

[0050] For the sake of clarity, only the steps and elements useful for understanding the embodiments described herein are illustrated and described in detail. In particular, only the formation of the peripheral insulating grooves of the component and the formation of the passivation layer formed in these grooves are described in detail, which participate in the reduction of the leakage current and the increase of the breakdown voltage of the component.

[0051] Unless otherwise specified, when referring to two elements being connected together, this means a direct connection without any intermediate elements except conductors, and when referring to two elements being coupled together, this means the two elements may be connected or they may be coupled via one or more other elements.

[0052] In the following disclosure, unless otherwise stated, when referring to absolute position qualifiers, such as terms "front", "back", "top", "bottom", "left", "right", etc., or relative position qualifiers, such as terms "upper", "lower", "upper", "lower", etc., or orientation qualifiers, such as "horizontal", "vertical", etc., reference is made to the orientation shown in the various figures.

[0053] Unless otherwise indicated, the expressions "about," "approximately," "substantially," and "around" mean within 10%, and preferably within 5%.

[0054] The electronic power component generally includes a semiconductor substrate including at least one horizontal plane PN junction, which is laterally surrounded by a peripheral groove extending vertically in the substrate. In order to limit leakage current and / or increase breakdown voltage, the vertical electronic power component may include a passivation structure covering the side and bottom of the groove and a portion of the surface of the semiconductor substrate at the groove surface. The passivation structure may, for example, include an oxygen-doped polysilicon or SIPOS ("semi-insulating polysilicon") layer. The passivation structure may also include a glass layer formed on the SIPOS layer, and more precisely formed in the groove and on the surface of the semiconductor substrate at the groove surface, so that it completely covers the SIPOS layer.

[0055] In electronic power components, groove depth causes complexity when etching SIPOS layer, and this etching is performed before forming glass layer.More specifically, groove depth causes complexity when forming masking resin by which SIPOS layer is etched, particularly masking resin by lithography structured.In fact, the deposition of masking resin is uneven and a large amount of resin must be deposited so that the top of groove is covered with resin.In some cases, the resin thickness of the upper surface of substrate makes it impossible for a single photolithography step to locally irradiate it across its entire thickness.For example, for electronic power components with very high breakdown voltage (for example, greater than or equal to 1200V), the depth of groove may be greater than hundreds of microns, and the thickness of masking resin may reach tens of microns.Therefore, the deposition of multiple resins and then the cycle of irradiation may be required to obtain the desired thickness.This causes complexity to increase and causes component manufacturing cost to increase.

[0056] Figure 1A , Figure 1B , Figure 1C , Figure 1D and Figure 1E Successive steps of an example of a method for manufacturing a power component according to a first embodiment are shown in partially simplified cross-sectional views. Figures 1A to 1E An example of a method for manufacturing a peripheral passivation structure of a power component according to a first embodiment is illustrated in more detail. It should be noted that in the accompanying drawings, the formation of a single component is shown. In practice, multiple components can be formed simultaneously inside and on top of the same semiconductor substrate, and then the substrate is cut into individual chips, each chip including a single electronic power component.

[0057] The described power electronic components may be used, for example, in various power control, power conversion or power matching circuits, such as industrial equipment, display or lighting equipment, telecommunication equipment, household appliance equipment, automotive equipment, and the like.

[0058] Figure 1AThe initial structure is shown comprising a semiconductor substrate 13, on the upper surface side of which a peripheral groove 15 is formed which laterally surrounds the horizontal plane PN junction of the component. Figure 1A In the figure, only a part of the initial structure is shown. In reality, the structure extends beyond Figure 1A At the right edge shown in dashed lines in FIG. 1 , a peripheral groove 15 surrounds the structure.

[0059] The component has, for example, a square or rectangular general shape in top view, for example with rounded corners or a circle.The substrate 13 is made of silicon, for example.

[0060] As an example, the substrate 13 includes, for example, a central portion 17 doped with a first conductivity type (e.g., N-type doping). As an example, the substrate 13 also includes, for example, an upper portion 19 doped with a second conductivity type different from the first conductivity type (e.g., P-type doping). As an example, the upper portion 19 contacts the upper surface of the central portion 17 of the substrate 13 through its lower surface.

[0061] The upper portion 19 of the substrate 13 comprises, for example, a doping gradient which increases from its lower surface. Furthermore, the upper portion 19 of the substrate 13 comprises, for example, a plurality of different dopant elements.

[0062] As an example, the upper portion 19 of the substrate 13 comprises a first portion 191 which is in contact with the upper surface of the portion 17 of the substrate 13 via its lower surface. The first portion 191 is doped with aluminum atoms, for example.

[0063] Furthermore, the upper portion 19 of the substrate 13 comprises, for example, a second portion 193 in contact with the upper surface of the portion 191 via its lower surface, the second portion 193 being doped with, for example, gallium atoms.

[0064] As an example, the upper portion 19 of the substrate 13 further comprises a third portion 195 which is in contact with the upper surface of the portion 193 via its lower surface. The third portion 195 is doped with gallium atoms, for example.

[0065] As an example, the groove 15 formed on the upper surface of the initial structure extends from the upper surface of the upper portion 19 of the substrate 13 into the substrate 13 and into the first portion 17 of the substrate 13. Thus, the groove extends, for example, through the portions 195, 193 and 191. Thus, the groove 15 passes through the PN junction formed by the horizontal plane of the interface between the upper portion 19 and the central portion 17.

[0066] The depth of the groove 15 from the upper surface of the substrate 13 is, for example, greater than 30 μm, for example, greater than 75 μm, for example, greater than 105 μm, for example, in the range of 105 μm to 150 μm.

[0067] Figure 1AThe structure also includes an oxygen-doped polysilicon or SIPOS ("semi-insulating polysilicon") layer 21, which extends on the top of the upper surface of the substrate 13 and in contact with the upper surface of the substrate 13 on the walls and bottom of the groove 15 and at the surface of the groove 15. As an example, the SIPOS layer 21 has an oxygen content in the range of 10% to 50%, for example 20% to 40%.

[0068] The SIPOS layer 21 is deposited, for example, by a chemical vapor deposition method (e.g., a low pressure chemical vapor deposition or LPCVD method) at the surface of the substrate 13 and in the groove 15. As an example, the thickness of the SIPOS layer 21 is in the range of 0.1 μm to 2 μm, for example, in the range of 0.1 μm to 1 μm, for example, about 0.5 μm.

[0069] Figure 1A The initial structure shown in is, for example, horizontally symmetrical. The substrate 13, for example, includes a lower portion 23, which includes, for example, portions 231, 233, and 235 similar to portions 191, 193, and 195 of the upper portion 19, respectively. The structure, for example, includes a groove 15' formed from the lower surface of the substrate 13. As an example, the groove 15' extends in the lower portion 23 and enters the central portion 17 of the substrate 13. The initial structure, for example, includes an extension on the top of the lower surface of the substrate 13 and in contact with the lower surface of the substrate 13 and another SIPOS layer 21' extending on the wall and bottom of the groove 15' formed from the lower surface of the substrate 13. Therefore, the groove 15' passes through the PN junction formed by the horizontal plane of the interface between the lower portion 23 and the central portion 17 of the substrate.

[0070] The initial structure also comprises a local doped region 25 on the upper surface side of the substrate 13, flush with this same surface. The structure may also comprise a local doped region 27 on the lower surface side of the substrate 13, flush with this same surface.

[0071] As an example, the layers 17, 19 and 23 each extend over the entire surface of the substrate. The regions 25 and 27 are each located on only a portion of the substrate surface.

[0072] Regions 25 and 27 are doped, for example, with a first conductivity type, for example N-type. By way of example, regions 25 and 27 are doped more heavily than central portion 17 of substrate 13 and than portions 195 and 235 of substrate 13. By way of example, regions 25 and 27 are doped with phosphorus atoms.

[0073] Thus, the initial structure is formed by a first vertical stack of four regions 19, 17, 23 and 27 of alternating P and N doping and a second vertical stack of four regions 25, 19, 17 and 23 of alternating N and P doping, which defines a triac. The described embodiments are not limited to this component example. As an example, region 27 can be omitted in the case of a thyristor type structure. More generally, the described embodiments can be applied to any electronic power component referred to as vertical that includes a horizontal PN junction and a passivation structure formed in a peripheral insulating groove that vertically passes through the PN junction.

[0074] Figure 1B The diagram shows Figure 1A The structure obtained at the end of the step of forming an electrically insulating layer 29 on the upper surface of the structure shown in FIG. In this example, an electrically insulating layer 29' is also formed on the lower surface of the structure.

[0075] More specifically, during this step, the layer 29 is continuously formed, i.e. Figure 1A Layer 29 is formed over the entire upper surface of the structure shown in FIG. During this step, layer 29 is formed in contact with SIPOS layer 21. Layer 29 covers the upper surface of layer 21 located on the side and in the bottom of groove 15 and extending at the surface of groove 15, for example.

[0076] Similarly, layer 29' is formed continuously, that is, it Figure 1A Layer 29' is formed over the entire lower surface of the structure shown in FIG. During this step, layer 29' is formed to be in contact with SIPOS layer 21'. Layer 29', for example, covers the lower surface of layer 21' located on the side and in the bottom of groove 15' and extending at the surface of groove 15'.

[0077] As an example, the layers 29 and 29' are made of undoped glass, for example, undoped silica glass (USG) or undoped phosphosilicate glass (PSG). The layers 29 and 29' are deposited, for example, by a chemical vapor deposition method, for example, by a LPCVD deposition method. As an example, the thickness of the layers 29 and 29' is in the range of 0.1 μm to 1.5 μm, for example, in the range of 0.5 μm to 1 μm.

[0078] Figure 1C The diagram shows Figure 1B The structure obtained at the end of the step of forming a glass layer 31 on the upper surface of the structure shown in FIG. In this example, a glass layer 31' is further formed on the lower surface of the structure.

[0079] More specifically, during this step, layer 31 is locally formed at the surface of layer 29 and, for example, in contact therewith. Thus, layer 31 covers layer 29 located in the bottom and on the sides of groove 15 and at the surface of groove 15, but does not extend over the entire surface of layer 29 at the surface of groove 15.

[0080] Similarly, during this step, layer 31' is locally formed at the surface of layer 29' and, for example, in contact therewith. Thus, layer 31' covers layer 29' located in the bottom and on the sides of recess 15' and at the surface of recess 15', but does not extend over the entire surface of layer 29' at the surface of recess 15'.

[0081] Layers 31 and 31' are deposited by a local deposition method, for example by screen printing. This step comprises, for example, depositing a glass paste through a mask located at the surface of layer 29 or layer 29'. As an example, after this deposition, layers 31 and 31' undergo one or more annealing steps. The annealing step may, for example, comprise a step of pyrolysis at a temperature in the range of 300°C to 700°C (for example, around 500°C). The annealing step may also comprise a step of sintering at a temperature in the range of 500°C to 1,000°C (for example, around 800°C).

[0082] As an example, the layers 31 and 31 ' have a non-constant thickness over their entire surface. For example, they are thicker at the bottom of the grooves 15 and 15' (ie in the grooves of the wafer between the components) than at the top and surface of the grooves 15 and 15'.

[0083] The thickness of the layers 31 and 31 ′ at the surface of the substrate 13 at the periphery of the grooves 15 and 15 ′ is, for example, in the range of 10 μm to 40 μm, for example, in the range of 20 μm to 30 μm.

[0084] The thickness of the layers 31 and 31 ′ in the bottom of the grooves 15 and 15 ′ is, for example, in the range of 20 μm to 70 μm, for example in the range of 40 μm to 50 μm.

[0085] Figure 1D The diagram shows Figure 1C The structure obtained at the end of the step of partial removal of layers 21 and 29 and layers 21 ′ and 29 ′ of the structure shown in .

[0086] During this step, for example, firstly by photolithography Figure 1C A mask layer (not shown) made of resist is formed on the upper surface of the structure shown in FIG.

[0087] As an example, the resist of the masking layer is deposited by spin coating, exposed to UV, and then developed in a solvent. As an example, the masking layer covers the entire surface of the glass layer 31. The masking layer extends laterally beyond the glass layer 31, thereby covering a portion of the layers 21 and 29 near the glass layer 31. However, the masking layer does not cover the layers 21 and 29 in front of the central part of the assembly.

[0088] During this step and at a second step, the layers 21 and 29 are etched through the masking layer. As an example, the etching of the layers 21 and 29 is a wet etch.

[0089] Similarly, for example, during this step, photolithography is also performed on Figure 1C A mask layer (not shown) made of a resist is formed on the lower surface of the structure shown in FIG. 1 , and etching layers 21 ′ and 29 ′ are formed through the mask layer.

[0090] At the end of this step, layers 21 and 29 extend, for example, in the bottom and on the sides of groove 15 and over a portion of the upper surface of substrate 13 at the surface of groove 15. By way of example, layers 21 and 29 extend beyond glass layer 31 on the upper surface of substrate 13, i.e., layers 21 and 29 extend on substrate 13 in the entire position in front of glass layer 31 and further extend over a portion of substrate 13 outside of the position in front of glass layer 31. By way of example, at the end of this step, layers 21 and 29 do not cover area 25.

[0091] Similarly, layers 21' and 29' extend over a portion of the lower surface of substrate 13, for example, in the bottom and on the sides of groove 15' and at the surface of groove 15'. As an example, layers 21' and 29' extend beyond glass layer 31' on the lower surface of substrate 13, i.e., layers 21' and 29' extend over a position in front of glass layer 31' on substrate 13, and further extend over a portion of substrate 13 outside of glass layer 31'. As an example, at the end of this step, layers 21' and 29' do not cover area 27.

[0092] Figure 1E The diagram shows Figure 1D The structure obtained at the end of the step of forming conductive layers 33 and 33' on the upper surface and the lower surface of the structure shown in FIG.

[0093] More specifically, during this step, for example, a conductive layer 33 is formed at the surface of the substrate 13 as an extension of the layers 21 and 29. As an example, the layer 33 is formed to contact a portion of the upper surface of the substrate 13 that is not covered by the layers 21 and 29. As an example, the layer 33 extends from the layers 21 and 29, and, for example, its side faces are in contact with the side faces of the layers 21 and 29.

[0094] Similarly, during this step, a conductive layer 33' is also formed, for example, at the surface of the substrate 13 as an extension of the layers 21' and 29'. As an example, the layer 33' is formed to contact a portion of the lower surface of the substrate 13 that is not covered by the layers 21' and 29'. As an example, the layer 33' extends from the layers 21' and 29', and, for example, its side faces are in contact with the side faces of the layers 21' and 29'.

[0095] As an example, the layers 33 and 33' are made of a metallic material, such as gold and / or nickel. As an example, the layers 33 and 33' are formed by wet deposition, such as by electroless chemical deposition.

[0096] In this step, deposition is only formed on the conductive parts of the structure and not on the insulating parts of the structure. Layers 33 and 33' are then selectively formed with Figure 1D 1 . Then layers 33 and 33' are formed in contact with the upper and lower surfaces of substrate 13, respectively. As an example, layers 29 and 29' enable the upper surface of layer 21 and the lower surface of layer 21' to be protected from the deposition of layers 33 and 33', respectively, during this step. Layers 29 and 29' in particular enable the layers 21 and 21' to be protected from the deposition of layers 33 and 33', respectively. In fact, in the absence of layers 29 and 29', layers 33 and 33' would tend to be further formed over a portion of semi-insulating layers 21 and 21'.

[0097] Figure 2A , Figure 2B , Figure 2C and Figure 2D Successive steps of an example of a method for manufacturing a power component according to a second embodiment are shown in partially simplified cross-sectional views.

[0098] More specifically, FIG. 2A to FIG. 2D A power assembly manufacturing method according to a second embodiment is illustrated. FIG. 2A to FIG. 2D Methods and Figures 1A to 1E The main difference between the methods is that FIG. 2A to FIG. 2D In the method, the electrically insulating layer 29 is formed after the glass layer 31 .

[0099] Figure 2A The diagram shows Figure 1A The structure obtained at the end of the step of forming glass layers 31 and 31 ′ on the upper and lower surfaces of the structure shown in FIG.

[0100] Figure 2A The steps of forming the glass layers 31 and 31' shown in FIG. 1 are similar to those shown in FIG. Figure 1C The steps of forming glass layers 31 and 31' shown in FIG. 1 are different in that Figure 2AIn the embodiment, glass layers 31 and 31 ′ are formed on top of and in contact with SIPOS layers 21 and 21 ′, respectively.

[0101] During this step, layer 31 is thus formed locally at the surface of layer 21 and, for example, in contact therewith. Layer 31 thus covers layer 21 located in the bottom and on the sides of recess 15 and at the surface of recess 15, but does not extend over the entire surface of layer 21 at the surface of recess 15.

[0102] Similarly, during this step, layer 31' is locally formed at the surface of layer 21' and, for example, in contact therewith. Thus, layer 31' covers layer 21' located in the bottom and on the sides of recess 15' and at the surface of recess 15', but does not extend over the entire surface of layer 21' at the surface of recess 15'.

[0103] Figure 2B The diagram shows Figure 2A The structure obtained at the end of the step of forming electrical insulating layers 29 and 29' on the upper and lower surfaces of the structure shown in FIG.

[0104] Figure 2B The steps of forming the electrically insulating layers 29 and 29' shown in FIG. 1 are similar to, for example, Figure 1B The steps of forming the electrical insulating layers 29 and 29' shown in FIG. 1 are different in that Figure 2B In the embodiment, the insulating layer 29 is formed on top of and in contact with the glass layer 31, and is formed on top of and in contact with a portion of the SIPOS layer 21 that is not covered by the glass layer 31. In addition, Figure 2B The steps of forming the electrical insulating layers 29 and 29' shown in FIG. Figure 1B The steps of forming the electrical insulating layers 29 and 29' shown in FIG. 1 are different in that Figure 2B In the embodiment, the electrically insulating layer 29' is formed on top of and in contact with the glass layer 31' and is formed on top of and in contact with a portion of the SIPOS layer 21' not covered by the glass layer 31'.

[0105] Thus, layer 29 covers the upper surface of glass layer 31 located on the sides and in the bottom of groove 15 and extending at the surface of groove 15, and further covers a portion of the upper surface of layer 21 at the surface of groove 15 that is not covered by layer 31. As an example, layer 29 covers the sides of glass layer 31 at the surface of groove 15. As an example, at the end of this step, glass layer 31 is in contact with the upper surface of SIPOS layer 21 through its lower surface, and is in contact with the lower surface of layer 29 through its upper surface.

[0106] Similarly, layer 29' thus covers the lower surface of glass layer 31' located on the sides and in the bottom of groove 15' and extending at the surface of groove 15', and further covers a portion of the lower surface of layer 21' at the surface of groove 15' that is not covered by glass layer 31'. As an example, layer 29' covers the sides of glass layer 31' at the surface of groove 31'. As an example, at the end of this step, glass layer 31' is in contact with the lower surface of SIPOS layer 21' through its upper surface, and is in contact with the upper surface of layer 29' through its lower surface.

[0107] Figure 2C The diagram shows Figure 2B The structure obtained at the end of the steps of structuring or local removal of the layers 21 and 29 and the layers 21 ′ and 29 ′ of the structure shown in .

[0108] Figure 2C The structuring steps of the layers 21 and 29 and the layers 21 ′ and 29 ′ shown in FIG. 1 are, for example, similar to Figure 1D The structuring steps of the layers 21 and 29 and the layers 21' and 29' shown in FIG. 1 are different in that Figure 2C In the embodiment, masking layers enabling etching of layers 21 and 29 and layers 21 ′ and 29 ′ are formed on top of and in contact with the upper surface of layer 29 and on top of and in contact with the lower surface of layer 29 ′, respectively.

[0109] Figure 2D The diagram shows Figure 2C The structure obtained at the end of the step of forming conductive layers 33 and 33' on the upper surface and the lower surface of the structure shown in FIG.

[0110] Figure 2D The steps of forming layers 33 and 33' shown in FIG. Figure 1E The steps for forming layers 33 and 33' shown in FIG. 1 are the same.

[0111] An advantage of the described embodiments is that they enable to dispense with one or more photolithography steps and thus reduce the manufacturing costs of the electronic component under consideration.In particular, the local deposition of the glass layers 31 , 31 ′ enables to dispense with a step of local etching of said glass layers.

[0112] Furthermore, the step of local removal of the passivation layers 21, 29 and, if present, 21', 29' is carried out after the deposition of the glass 31, 31' in the grooves 15, 15'. Thus, during this step, the grooves 15, 15' are at least partially filled with the glass 31, 31'. Thus, it is possible to use a masking resist of reduced thickness for the local etching step of the layers 21, 29 and 21', 29'. This makes it possible to simplify this local etching step and reduce its cost.

[0113] Various embodiments and variations have been described. Those skilled in the art will appreciate that certain features of these different embodiments and variations can be combined, and those skilled in the art will appreciate other variations. In particular, the described embodiments are not limited to the examples of dimensions and materials mentioned above, for example.

[0114] Furthermore, although the embodiments have been described with respect to a triac, the present disclosure may be applied to any device including a peripheral mesa groove passivated with a glass layer and a SIPOS layer.

[0115] Finally, based on the functional indications given above, the actual implementation of the described embodiments and variants is within the capabilities of a person skilled in the art.

[0116] A method for forming an electronic power component (100; 200) inside and on top of a semiconductor substrate (13), which can be summarized as comprising the following consecutive steps: a) forming a peripheral groove (15, 15') in a semiconductor substrate (13) on a first surface side of the semiconductor substrate (13); b) depositing an oxygen-doped polysilicon layer (21, 21') on and in contact with the bottom and top of the sidewalls of the peripheral groove (15, 15') and on the semiconductor substrate (13); c) depositing an oxygen-doped polysilicon layer (21, 21') on and in contact with the bottom and top of the sidewalls of the peripheral groove (15, 15') and on the semiconductor substrate (13); c) locally depositing a glass layer (31, 31') on the oxygen-doped polysilicon layer (21, 21'), the glass layer (31, 31') extending in the peripheral groove (15, 15') and further extending over a portion of the first surface of the semiconductor substrate (13); and d) etching the oxygen-doped polysilicon layer (21, 21') so that it extends beyond the glass layer (31, 31') on the first surface of the semiconductor substrate (13).

[0117] The electronic power component forming method may include a step e) between steps b) and c): an electrical insulating layer (29, 29') deposited on top of and in contact with the oxygen-doped polysilicon layer (21, 21').

[0118] The electronic power component forming method may include a step e) between steps c) and d): an electrically insulating layer (29, 29') deposited on top of and in contact with the glass layer (31, 31') and a portion of the oxygen-doped polysilicon layer (21, 21') not covered by the glass layer (31, 31').

[0119] During step d), the electrically insulating layer (29, 29') may be etched simultaneously with the oxygen-doped polysilicon layer (21, 21').

[0120] The deposition of the glass layer ( 31 , 31 ′) during step c) may be performed by screen printing.

[0121] The grooves (15, 15') may have a depth greater than 75 μm.

[0122] The thickness of the oxygen-doped polysilicon layer ( 21 , 21 ′) may be in the range of 0.1 μm to 2 μm.

[0123] An electronic power component (100; 200) can be summarized as comprising: a peripheral groove (15, 15') formed in a semiconductor substrate (13) on a first surface side of the semiconductor substrate (13); an oxygen-doped polysilicon layer (21, 21') formed on and in contact with the bottom and top of the sidewalls of the peripheral groove (15, 15') and on and in contact with the first surface of the semiconductor substrate (13); and a glass layer (31, 31') formed on the oxygen-doped polysilicon layer (21, 21'), the glass layer (31, 31') extending in the peripheral groove (15, 15') and further extending on a portion of the first surface of the semiconductor substrate (13), and the oxygen-doped polysilicon layer (31, 31') extending beyond the glass layer on the first surface of the semiconductor substrate (13).

[0124] The electronic power component (100; 200) may include an electrical insulation layer (29, 29') located between an oxygen-doped polysilicon layer (21, 21') and a glass layer (31, 31'), wherein the electrical insulation layer (29, 29') contacts the oxygen-doped polysilicon layer (21, 21') via a first surface and contacts the glass layer (31, 31') via a second surface opposite to the first surface.

[0125] The electronic power component (100; 200) may include an electrically insulating layer (29, 29'), a glass layer in contact with the electrically insulating layer (29, 29') via a first surface and in contact with an oxygen-doped polysilicon layer (21, 21') via a second surface opposite to the first surface, and the electrically insulating layer (29, 29') in contact with a portion of the oxygen-doped polysilicon layer (21, 21') not covered by the glass layer (31, 31').

[0126] The grooves (15, 15') have a depth greater than 75 μm.

[0127] The thickness of the oxygen-doped polysilicon layer (21, 21') is in the range of 0.1 μm to 2 μm.

[0128] 13. A power control circuit may be generally described as comprising electronic power components.

[0129] The various embodiments described above can be combined to provide further embodiments. Aspects of the embodiments can be modified, if necessary to employ concepts of the various patents, applications and publications to provide further embodiments.

[0130] These and other changes can be made to the embodiments in light of the above detailed description. In general, in the appended claims, the terms used should not be interpreted as limiting the claims to the specific embodiments disclosed in the specification and claims, but should be interpreted to include all possible embodiments and the full scope of equivalents to which these claims are entitled. Therefore, the claims are not limited by the present disclosure.

Claims

1. An electronic power component, characterized in that: include: a peripheral recess in the semiconductor substrate on one side of the first surface of the semiconductor substrate; an oxygen-doped polysilicon layer on and in contact with the bottom and top of the sidewalls of the peripheral recess and on and in contact with the top of the first surface of the semiconductor substrate; as well as A glass layer is on the oxygen-doped polysilicon layer, the glass layer extending in the peripheral groove and extending over a portion of the first surface of the semiconductor substrate, and the oxygen-doped polysilicon layer extends beyond the glass layer on the first surface of the semiconductor substrate.

2. The electronic power assembly according to claim 1, characterized in that: An electrical insulating layer is included between the oxygen-doped polysilicon layer and the glass layer, the electrical insulating layer being in contact with the oxygen-doped polysilicon layer through a first surface and in contact with the glass layer through a second surface opposite to the first surface.

3. The electronic power assembly according to claim 1, characterized in that: An electrical insulating layer is included, wherein the glass layer contacts the electrical insulating layer through a first surface and contacts the oxygen-doped polysilicon layer through a second surface opposite to the first surface, and the electrical insulating layer contacts a portion of the oxygen-doped polysilicon layer not covered by the glass layer.

4. The electronic power assembly according to claim 1, characterized in that: The grooves have a depth of more than 75 μm.