Metal coating enamel steel pipe capable of being used for welding
By covering the metal coating and enamel layer on the enamel steel pipe, the problem of the inability to weld and rust prevention of enamel steel pipes is solved, and the corrosion resistance and weldability effect is achieved, extending the service life and improving the installation efficiency.
Patent Information
- Application Number
- CN202420770590.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-15
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-04-15
AI Technical Summary
The existing enamel steel pipes have short service life due to inability to weld, and the enamel layer is prone to cracking during welding, which cannot meet the anti-rust needs for long-term use.
Use metal coating to cover the welding section of the steel pipe, combine the enamel layer in other areas of the steel pipe, and use nickel powder, tungsten powder and other materials to form a metal coating through spraying technology to ensure that the anti-corrosion layer is not damaged during welding, and provide welding and anti-corrosion. Double protection.
The corrosion resistance and weldability of enamel steel pipes are achieved, extending service life and improving installation efficiency.
Smart Images

Figure CN222046933U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of pipelines, and in particular to a weldable metal-coated enameled steel pipe. Background Art
[0002] Steel pipes are commonly used in pipeline usage scenarios such as building hot water pipes and air-conditioning pipes, but the service life of ordinary steel pipes is generally 10 to 15 years before they need to be replaced due to severe corrosion, insufficient pressure bearing and other factors.
[0003] Although the current baked enameled pipes can solve the problem of high and low temperature resistance and corrosion resistance of pipes, enameled pipes are generally connected by metal flanges. The principle of flange connection is to use sealing rings to seal water. However, due to the thermal expansion and contraction of the pipes during the hot and cold cycles of air conditioning water, the sealing rings at the interfaces are prone to aging and leakage after long-term use. If the baked enameled pipes are connected and fixed by welding, the welding temperature is higher than the melting point of the enamel, and the enamel will crack at the weld during the welding process. It cannot be repaired later. Long-term use in water will cause corrosion and rust at the interface, which cannot meet the service life of the pipeline throughout its life cycle. Therefore, the existing enameled steel pipes have a low service life and cannot be welded while ensuring rust prevention. Summary of the invention
[0004] In view of the defects in the prior art, the embodiments of the present application provide a weldable metal-coated enameled steel pipe, which solves the technical problems in the prior art that the enameled steel pipe cannot be welded while ensuring rust prevention and has a low service life.
[0005] The present application provides a weldable metal-coated enameled steel pipe, comprising:
[0006] Steel pipe body;
[0007] An enamel layer, the enamel layer covering the first area of the steel pipe body;
[0008] A metal coating, wherein the metal coating covers the second area of the steel pipe body;
[0009] The first region and the second region include the entire inner surface and end surface of the steel pipe body, and the second region includes the welding section.
[0010] In a feasible design, the enamel layer is coated on the first region by dipping or powder spraying and then fired.
[0011] In a feasible design, the inner surface and the end surface of the second region are coated with the metal coating to form the welding section.
[0012] In a feasible design, a portion of the first region and a portion of the second region overlap to form a third region.
[0013] In a possible design, on the third region, the metal coating covers the enamel layer.
[0014] In a feasible design, the second area includes two areas, which are arranged at both ends and on the end surface of the steel pipe body.
[0015] In a feasible design, the first area is arranged on the inner surface and the outer surface of the steel pipe body, and the second area is arranged on the inner surface, the outer surface and the end face of the steel pipe body.
[0016] In a feasible design, the metal coating is formed by spraying at least one of nickel powder, tungsten powder, chromium powder, nickel-based high-temperature alloy, nickel-based composite material, tungsten-molybdenum alloy, chromium-molybdenum alloy, cobalt-based alloy and titanium alloy on the second area using a spraying technique.
[0017] The present application provides a weldable metal-coated enameled steel pipe, comprising a steel pipe body, an enamel layer and a metal coating, wherein the enamel layer covers a first region of the steel pipe body, and the metal coating covers a second region of the steel pipe body, wherein the first region and the second region include the entire inner surface and end face of the steel pipe body, and the second region includes a welding section for welding. The present application provides a weldable metal-coated enameled steel pipe that solves the disadvantage of poor corrosion resistance of the steel pipe through the enamel layer, solves the problem that the enamel tank cannot be welded through the metal coating, performs corrosion protection through the enamel layer, and prevents the corrosion protection layer from being damaged during welding through the metal coating, solves the disadvantage that the enameled steel pipe cannot be welded, has the advantages of corrosion resistance and weldability, and achieves the technical effect of improving the installation efficiency and service life of the steel pipe.
[0018] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are listed below. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present application. Also, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0020] Figure 1 A schematic diagram of the overall structure of a weldable metal-coated enameled steel pipe provided in an embodiment of the present application.
[0021] Description of reference numerals: steel pipe body 10 , enamel layer 20 , metal coating 30 . DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0023] In the description of the embodiments of the present application, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present application, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly defined and specifically defined. In the present application, unless otherwise clearly defined and defined, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, it can also be a detachable connection, or it can be integrated; it can be directly connected, it can also be indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For those of ordinary skill in the art, the specific meanings of the above terms in the present application can be understood according to the specific circumstances.
[0024] In the present application, unless otherwise clearly specified and limited, a first feature being “above” or “below” a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being “above”, “above”, and “above” a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being “below”, “below”, and “below” a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0025] In the description of this application, it should be understood that the terms "inside", "outside", "upper", "bottom", "front", "back" and the like indicate directions or positional relationships (if any) based on the attached Figure 1 The orientation or positional relationship shown is only for the convenience of describing the present application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0026] Embodiment 1
[0027] like Figure 1 As shown, the present application provides a weldable metal-coated enameled steel pipe, comprising:
[0028] Steel pipe body 10;
[0029] An enamel layer 20, the enamel layer 20 covers the first area of the steel pipe body 10;
[0030] A metal coating 30, the metal coating 30 covers the second area of the steel pipe body 10, and the metal coating 30 also has an anti-corrosion protection function;
[0031] The first region and the second region include the entire inner surface and end surface of the steel pipe body 10, and the second region includes the welding section.
[0032] The steel pipe body 10 can be a steel pipe of any specification and any size in the prior art, such as a steel pipe used in a hot water pipe.
[0033] In one embodiment, the thickness of the enamel layer 20 should meet the long-term corrosion resistance requirement.
[0034] The thickness of the enamel layer 20 may be set differently according to the circulating medium in the steel pipe after application. For example, the thickness of the enamel layer 20 may be set according to the temperature of the circulating medium.
[0035] In one embodiment, the enamel layer 20 is coated on the first region by dipping or powder spraying and then fired.
[0036] Among them, different bulk densities and adhesion amounts of the enamel layer 20 can be set according to the circulating medium in the steel pipe after application, and dipping or powder spraying can be performed, and sintering can be performed after completion.
[0037] Preferably, the sintering temperature is controlled at 850-950°C, such as 900°C.
[0038] Preferably, the first area is larger than the second area, and the first area is most of the middle section of the steel pipe body 10 . By covering the steel pipe body 10 with the enamel layer 20 , the rust prevention effect of the steel pipe is achieved.
[0039] In one embodiment, the length of the second region on the axis of the steel pipe body 10 can be set based on the size of the welding section by technicians in this field. If the welding section is large, the length of the second region is larger, and vice versa. The metal coating is applied to the inner surface and end face of the second region to form the welding section.
[0040] In one embodiment, part of the first area overlaps part of the second area and forms a third area. By overlapping the first area and the second area, the enamel layer 20 and the metal coating 30 have overlapping parts. In addition to being resistant to high temperatures, the metal coating 30 also isolates the steel pipe body 10 from the outside world and has anti-corrosion and anti-rust effects, so that all surfaces of the steel pipe body 10 that need to be anti-corrosion have anti-corrosion effects.
[0041] In one embodiment, on the third region, the metal coating 30 covers the enamel layer 20 to protect the enamel layer 20 .
[0042] Generally speaking, the two ends of the steel pipe are fixed or connected by welding. Therefore, in one embodiment, the second area includes two areas, which are arranged on the two ends and the end surface of the steel pipe body 10, so that the metal coating 30 has a high temperature protection effect during the welding process of the two ends.
[0043] The two second regions may be of the same size or of different sizes.
[0044] In one embodiment, the first area is arranged on the inner surface of the steel pipe body 10, there is a flowing medium in the steel pipe body 10, and an enamel layer 20 is arranged on the inner surface for rust prevention. The second area is arranged on the inner surface and end face of the steel pipe body 10 for rust prevention and high temperature resistant welding protection.
[0045] In one embodiment, if the outer surface of the steel pipe body 10 may also rust in the environment where it is used, the first area is set on the inner surface and outer surface of the steel pipe body 10, and the second area is set on the inner surface, outer surface and end face of the steel pipe body 10, so that the inner and outer surfaces of the steel pipe body 10 have anti-corrosion and high-temperature corrosion-resistant functions.
[0046] In one embodiment, the metal coating 30 is formed by spraying at least one of nickel powder, tungsten powder, chromium powder, nickel-based high-temperature alloy, nickel-based composite material, tungsten-molybdenum alloy, chromium-molybdenum alloy, cobalt-based alloy and titanium alloy on the second region using a spraying technique.
[0047] The metal coating 30 is preferably formed by spraying using a metal cold spraying technique.
[0048] In summary, the embodiment of the present application provides a weldable metal-coated enameled steel pipe, comprising a steel pipe body, an enamel layer and a metal coating, wherein the enamel layer covers the first area of the steel pipe body, and the metal coating covers the second area of the steel pipe body, wherein the first area and the second area include the entire inner surface and end surface of the steel pipe body, and the second area includes a welding section for welding. The weldable metal-coated enameled steel pipe provided by the present application solves the disadvantage of poor corrosion resistance of the steel pipe through the enamel layer, solves the problem that the enamel tank cannot be welded through the metal coating, performs corrosion protection through the enamel layer, and prevents the corrosion protection layer from being damaged during welding through the metal coating, solves the disadvantage that the enameled steel pipe cannot be welded, has the advantages of corrosion resistance and weldability, and achieves the technical effect of improving the installation efficiency and service life of the steel pipe.
[0049] Although the present application has been described in conjunction with specific features and embodiments thereof, it is obvious that various modifications and combinations may be made thereto without departing from the spirit and scope of the present application. Accordingly, this specification and the accompanying drawings are merely exemplary illustrations of the present application as defined therein, and are deemed to have covered any and all modifications, variations, combinations or equivalents within the scope of the present application. Obviously, a person skilled in the art may make various modifications and variations to the present application without departing from the scope of the present application. Thus, if these modifications and variations of the present application fall within the scope of the present application and its equivalents, the present application is intended to include these modifications and variations.
Claims
1. A weldable metal-coated enameled steel pipe, characterized in that: include: Steel pipe body; An enamel layer, the enamel layer covering the first area of the steel pipe body; A metal coating, wherein the metal coating covers the second area of the steel pipe body; The first region and the second region include the entire inner surface and end surface of the steel pipe body, and the second region includes the welding section.
2. The weldable metal-coated enameled steel pipe according to claim 1, characterized in that: The enamel layer is coated on the first region by dipping or powder spraying and then fired.
3. The weldable metal-coated enameled steel pipe according to claim 1, characterized in that: The metal coating is applied to the inner surface and the end surface of the second region to form the welding section.
4. The weldable metal-coated enameled steel pipe according to claim 1, characterized in that: Part of the first region and part of the second region overlap to form a third region.
5. The weldable metal-coated enameled steel pipe according to claim 4, characterized in that: On the third region, the metal coating covers the enamel layer.
6. The weldable metal-coated enameled steel pipe according to claim 1, characterized in that: The second area includes two areas, which are arranged at both ends and an end surface of the steel pipe body.
7. The weldable metal-coated enameled steel pipe according to claim 1, characterized in that: The first area is arranged on the inner surface and the outer surface of the steel pipe body, and the second area is arranged on the inner surface, the outer surface and the end surface of the steel pipe body.
8. The weldable metal-coated enameled steel pipe according to claim 1, characterized in that: The metal coating is formed by spraying at least one of nickel powder, tungsten powder, chromium powder, nickel-based high-temperature alloy, nickel-based composite material, tungsten-molybdenum alloy, chromium-molybdenum alloy, cobalt-based alloy and titanium alloy on the second area using a spraying technique.