Anti-aging light-cured organic silicon release film
By introducing a nylon mesh layer and an aluminum-plated barrier layer into the release film, the problems of penetration and unstable molding after the release agent is applied are solved, and the anti-aging performance and light blocking ability of the release film are improved.
Patent Information
- Application Number
- CN202420598626.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-27
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-03-27
AI Technical Summary
Existing release films are prone to penetration and unstable molding after the release agent is applied, and have poor anti-aging effect. The smooth surface of the coating layer makes the release agent prone to aging.
The structure consists of a base paper layer, a release agent layer, a first curing layer, a mesh layer, a second curing layer, and a protective layer. The mesh layer is made of nylon mesh with densely packed holes. The first and second curing layers use UV-curable adhesive. The bottom of the protective layer has an aluminum-plated barrier layer to enhance the barrier and stability of the release agent. It is rapidly molded through UV curing.
It achieves stable application and uniform molding of the release agent, enhances the anti-aging effect of the release film, prevents release agent penetration, and improves light blocking performance.
Smart Images

Figure CN222061464U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of release films, in particular to an anti-aging light-curing organic silicon release film. Background Art
[0002] The release film usually includes a base paper and a release agent. The release agent is applied to the base paper. When used, the release agent is used to isolate sticky objects.
[0003] Since the release agent has a certain degree of permeability, if there is no barrier, the release agent will penetrate into the base paper, resulting in waste of release agent, uneven distribution and defective products. Therefore, it is necessary to block the release agent. In the prior art, many pairs of base papers are treated with lamination to block the release agent, but the surface of the lamination layer is smooth, which is not conducive to the stable molding after the release agent is applied. In addition, the base paper is usually relatively thin, and the effect of blocking light is poor, which makes the lamination layer and the release agent easy to age, and needs to be improved. Utility Model Content
[0004] The utility model aims to provide an anti-aging light-curing silicone release film, which avoids the problems of penetration and unstable molding of release agent after application and improves the anti-aging effect.
[0005] To achieve this purpose, the utility model adopts the following technical solutions:
[0006] An anti-aging light-curing silicone release film comprises: a base paper layer, a release agent layer, a first cured layer, a second cured layer and a protective layer, wherein the first cured layer is arranged on the top surface of the base paper layer, a mesh layer is arranged on the first cured layer, the release agent layer is arranged above the mesh layer, the second cured layer is arranged on the bottom surface of the base paper layer, the protective layer is arranged on the bottom surface of the second cured layer, and the release agent layer uses a layer of silicone release agent.
[0007] Wherein, the first curing layer and the second curing layer are respectively made of UV curing glue.
[0008] Wherein, the mesh cloth layer is densely covered with mesh holes.
[0009] Wherein, the mesh layer is made of nylon mesh.
[0010] Wherein, the protective layer is made of PET film, and a barrier layer is arranged at the bottom of the protective layer.
[0011] Wherein, the barrier layer is an aluminum-plated layer.
[0012] The beneficial effects of the utility model are as follows: an anti-aging light-curing silicone release film, with a specially designed first curing layer, which can not only fix the mesh layer, but also avoid the penetration of the release agent after application, and increase the stability of the release agent after application through the mesh layer, avoid the free flow of the release agent, perform stable molding, ensure uniform thickness, and protect the outside through the protective layer to enhance the anti-aging effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a structural schematic diagram of the utility model. DETAILED DESCRIPTION
[0014] Combine the following Figure 1 The technical solution of the utility model is further illustrated by specific embodiments.
[0015] An anti-aging photocurable silicone release film comprises: a base paper layer 1, a release agent layer 2, a first cured layer 4, a second cured layer 5 and a protective layer 7. The first cured layer 4 is arranged on the top surface of the base paper layer 1, and a mesh layer 3 is arranged on the first cured layer 4. The mesh layer 3 can be fixed by the first cured layer 4.
[0016] The release agent layer 2 is arranged above the mesh layer 3. In the present embodiment, the release agent layer 2 adopts a layer of silicone release agent, which can effectively isolate sticky objects and is blocked by the first solidified layer 4 to prevent the release agent layer 2 from leaking into the base paper layer 1.
[0017] In this embodiment, the mesh layer 3 is made of nylon mesh with high structural strength. The mesh layer 3 is densely covered with mesh holes, which increase the stability of the release agent after application, prevent the release agent from flowing freely, and perform stable molding of the release agent layer 2.
[0018] The second cured layer 5 is arranged on the bottom surface of the base paper layer 1, and the protective layer 7 is arranged on the bottom surface of the second cured layer 5. The base paper layer 1 and the protective layer 7 are compounded by the second cured layer 5, and the structure is stable. In this embodiment, the first cured layer 4 and the second cured layer 5 are respectively made of UV curing glue, which can be irradiated by ultraviolet light, quickly cured and formed, and convenient for production.
[0019] In order to protect the outside of the release film, in this embodiment, the protective layer 7 is made of PET film, which has a good waterproof effect. A barrier layer 6 is arranged at the bottom of the protective layer 7 to block light during use and improve the anti-aging effect.
[0020] like Figure 1As shown, the barrier layer 6 can be an aluminum-plated layer. Through the vacuum aluminum-plating process, an aluminum-plated layer that can block light is formed on the bottom surface of the protective layer 7. The aluminum-plated layer can also reflect light, reducing the temperature rise problem of the release film under light and further improving the anti-aging effect.
[0021] The above contents are only preferred embodiments of the present invention. For ordinary technicians in this field, according to the concept of the present invention, there will be changes in the specific implementation methods and application scopes. The contents of this specification should not be understood as limiting the present invention.
Claims
1. An anti-aging light-curing silicone release film, characterized in that: include: A base paper layer, a release agent layer, a first solidified layer, a second solidified layer and a protective layer, wherein the first solidified layer is arranged on the top surface of the base paper layer, a mesh layer is arranged on the first solidified layer, the release agent layer is arranged above the mesh layer, the second solidified layer is arranged on the bottom surface of the base paper layer, the protective layer is arranged on the bottom surface of the second solidified layer, and the release agent layer adopts a layer of silicone release agent.
2. The anti-aging light-curing silicone release film according to claim 1, characterized in that: The first curing layer and the second curing layer are respectively made of UV curing glue.
3. The anti-aging light-curing silicone release film according to claim 1, characterized in that: The mesh cloth layer is densely covered with mesh holes.
4. The anti-aging light-curing silicone release film according to claim 1, characterized in that: The mesh layer is made of nylon mesh.
5. The anti-aging light-curing silicone release film according to claim 1, characterized in that: The protective layer is made of PET film, and a barrier layer is arranged at the bottom of the protective layer.