Board mobile phone rear shell
By setting ink, bonding, liquid crystal film and varnish on the non-metal base layer of the back shell of the mobile phone, combined with the outer texture layer, the problem that the existing materials cannot meet the market demand is solved, and a more colorful and clear appearance is achieved. The back case of the phone with stable signal.
Patent Information
- Application Number
- CN202323660560.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2033-12-29
AI Technical Summary
The existing PMMA/PC composite board materials cannot meet the market's demand for a brighter effect, clearer texture and higher experience of the phone's back case, and it also needs to ensure signal stability.
Using a non-metallic substrate layer, an ink layer is provided on the first surface, and an adhesive layer, a liquid crystal film layer, a varnish layer and an outer texture layer are provided on the second surface in turn. The liquid crystal film layer improves reflectivity and texture clarity, and the varnish layer enhances the outer texture The adhesion of the layer achieves colorful effect and signal stability.
It achieves a brighter and clearer appearance effect, while ensuring signal stability, improving the quality and user experience of the phone's back case.
Smart Images

Figure CN222073198U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of mobile phone rear shells, in particular to a plate mobile phone rear shell. Background Art
[0002] With the advent of the 5G era, the application scenarios of mobile phones are becoming more and more diverse, and the requirements for the appearance and performance of mobile phones are also getting higher and higher. Traditional metal mobile phones, such as those made of aluminum alloy, have gradually been eliminated by the market due to the interference of metal on the signal. Therefore, it is necessary to find a new mobile phone material that can not only ensure the stability of the signal but also have a good appearance and texture.
[0003] At present, PMMA / PC composite board is mainly used as the main material of mobile phones in the market. PMMA / PC composite board is a plastic material, and its advantage is that it will not affect the mobile phone signal. Through the surface treatment process such as coating, high surface hardness and glass-like effect can be achieved. At the same time, the use of UV transfer, PVD, silk screen printing and other processes on the inner layer can achieve a colorful decorative effect. The cost of this board is relatively low compared to glass, metal and other materials, so it is widely used in the manufacture of mobile phone back covers.
[0004] However, with the development of technology and consumers' pursuit of quality, the existing PMMA / PC composite board can no longer meet the market demand. In order to show more colorful effects, clearer textures and higher user experience on the mobile phone back cover, it is necessary to develop a new mobile phone back cover structure. Utility Model Content
[0005] Based on the above situation, the purpose of the utility model is to provide a plate mobile phone back cover, which can not only ensure signal stability, but also achieve a more colorful, clear texture and high-quality appearance.
[0006] In order to achieve the above-mentioned purpose, the utility model provides a plate mobile phone back shell, including a non-metallic substrate layer, the substrate layer includes a first surface and a second surface arranged opposite to each other, the first surface is provided with an ink layer, and the second surface is provided with an adhesive layer, a liquid crystal film layer, a varnish layer and an outer texture layer in sequence.
[0007] Compared with the prior art, the sheet mobile phone back shell of the utility model adopts a non-metallic substrate layer, which will not affect the mobile phone signal and can ensure the signal stability. At the same time, an ink layer is arranged on the first surface, and an adhesive layer, a liquid crystal film layer, a varnish layer and an outer texture layer are arranged in sequence on the second surface. The introduction of the liquid crystal film layer greatly improves the reflectivity. With the help of the combination of the liquid crystal film layer and the outer texture layer, a clearer and more colorful outer texture effect is achieved. A varnish layer is introduced between the liquid crystal film layer and the outer texture layer to enhance the adhesion of the outer texture layer to the liquid crystal layer, so as to ensure the stability of the outer texture layer. Therefore, the sheet mobile phone back shell of the utility model can not only ensure the signal stability, but also achieve a more colorful, clear texture and high-quality appearance effect.
[0008] In some embodiments, the substrate layer is selected from a PMMA board, a PC board, a PET board or a PMMA / PC composite board.
[0009] In some embodiments, the PMMA / PC composite plate includes a stacked PMMA layer and a PC layer, a surface of the PC layer away from the PMMA layer constitutes the first surface, and a surface of the PMMA layer away from the PC layer constitutes the second surface.
[0010] In some embodiments, the first surface is sequentially provided with an inner texture layer, a PVD layer and the ink layer.
[0011] In some embodiments, the inner texture layer has a thickness of 10 to 15 microns.
[0012] In some embodiments, the liquid crystal film layer includes a single-layer liquid crystal film, a double-layer liquid crystal film, or a multi-layer liquid crystal film.
[0013] In some embodiments, the thickness of the single-layer liquid crystal film is 2 to 3 micrometers.
[0014] In some embodiments, the ink layer has a thickness of 25 to 40 micrometers.
[0015] In some embodiments, the outer texture layer has a thickness of 15 to 30 microns.
[0016] In some embodiments, the varnish layer has a thickness of 5 to 8 micrometers. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 The utility model is a schematic diagram of the structure of the plate mobile phone rear shell.
[0018] Figure 2 This is a schematic diagram of the structure of the mobile phone back shell made of a sheet material according to the utility model, including an inner texture layer and a PVD layer.
[0019] Figure 3 for Figure 2The structure diagram of another embodiment of the plate mobile phone back cover is shown. DETAILED DESCRIPTION
[0020] The following will clearly and completely describe the concept and technical effects of the utility model in combination with the embodiments, so as to fully understand the purpose, features and effects of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of them. Based on the embodiments of the utility model, other embodiments obtained by technicians in this field without creative work are all within the scope of protection of the utility model.
[0021] Please refer to Figure 1 The utility model provides a plate mobile phone back shell, including a non-metallic substrate layer 10, the substrate layer 10 includes a first surface and a second surface arranged opposite to each other, an ink layer 13 is arranged on the first surface, and an adhesive layer 14, a liquid crystal film layer 15, a varnish layer 16 and an outer texture layer 17 are arranged on the second surface in sequence.
[0022] In this technical solution, the non-metallic substrate layer 10 is used, which will not affect the mobile phone signal and can ensure signal stability. At the same time, an ink layer 13 is arranged on the first surface, and an adhesive layer 14, a liquid crystal film layer 15, a varnish layer 16 and an outer texture layer 17 are arranged on the second surface in sequence. The introduction of the liquid crystal film layer 15 greatly improves the reflectivity. With the combination of the liquid crystal film layer 15 and the outer texture layer 17, a clearer and more colorful outer texture is achieved. The varnish layer 16 is introduced between the liquid crystal film layer 15 and the outer texture layer 17 to enhance the adhesion of the outer texture layer 17 to the liquid crystal layer, so as to ensure the stability of the outer texture layer 17.
[0023] In a preferred embodiment, the substrate layer 10 is selected from a PMMA board, a PC board, a PET board or a PMMA / PC composite board. Further, the thickness of the substrate layer 10 is 0.5-0.8 mm, and optionally, the thickness of the substrate layer 10 is 0.5-0.64 mm. As an example, the thickness of the substrate layer 10 may be, but is not limited to, 0.5 mm, 0.55 mm, 0.6 mm, 0.60 mm, 0.64 mm, 0.7 mm, and 0.8 mm.
[0024] In a preferred embodiment, the substrate layer 10 is a PMMA / PC composite board, which includes stacked PMMA layers and PC layers, the surface of the PC layer away from the PMMA layer constitutes a first surface, the surface of the PMMA layer away from the PC layer constitutes a second surface, an ink layer 13 is arranged on the surface of the PC layer, and an adhesive layer 14, a liquid crystal film layer 15, a varnish layer 16 and an outer texture layer 17 are arranged in sequence on the surface of the PMMA layer.
[0025] It is understandable that the ink is formed into an ink layer 13 by silk screen printing or spraying. The ink layer 13 preferably uses water-based ink, but it can also be oil-based ink. A variety of colors of ink can be selected for silk screen printing. The color of the ink layer 13 is not particularly limited. As long as the requirements are met, those skilled in the art can flexibly select according to needs, for example, including but not limited to red, orange, yellow, green, cyan, blue, purple, etc. Thus, any different colors can be selected to meet the needs of different users. In some embodiments, flame retardant materials can also be added to the ink to improve the fireproof properties. Further, the thickness of the ink layer 13 is 25 to 40 microns, optionally, about 25 to 35 microns, about 25 to 30 microns, about 30 to 40 microns. As an example, the thickness of the ink layer 13 can be but not limited to 25 microns, 30 microns, 35 microns, and 40 microns.
[0026] It is understood that the liquid crystal film layer 15 is attached to the second surface of the substrate layer 10 through the adhesive layer 14. The glue of the adhesive layer 14 can be but not limited to optically transparent adhesive, hot melt adhesive, pressure sensitive adhesive and UV adhesive. Preferably, the adhesive layer 14 uses an optically transparent adhesive, such as epoxy resin adhesive, acrylate adhesive, etc. Further, the thickness of the adhesive layer 14 is 8 to 12 microns, optionally, about 8 to 10 microns. As an example, the thickness of the adhesive layer 14 can be but not limited to 8 microns, 9 microns, 10 microns, 11 microns, 12 microns.
[0027] In a preferred embodiment, the liquid crystal film layer 15 includes a single-layer liquid crystal film, a double-layer liquid crystal film or a multi-layer liquid crystal film. The material of the liquid crystal film layer 15 can be, but is not limited to, a monochrome liquid crystal film, a gradient liquid crystal film, or a graphic liquid crystal film, preferably a monochrome liquid crystal film. Furthermore, the transmittance of the liquid crystal film layer 15 is higher than 95%. As an example of a single-layer liquid crystal film, please refer to Figure 1 The second surface is provided with an adhesive layer 14, a first liquid crystal film layer 151, a varnish layer 16 and an outer texture layer 17 in sequence; as an example of a double-layer liquid crystal film, please refer to Figure 3 , the second surface is sequentially provided with an adhesive layer 14, a first liquid crystal film layer 151, a second liquid crystal film layer 153, a varnish layer 16 and an outer texture layer 17. After the double-layer liquid crystal film layer 15 is adopted, the reflectivity will be greatly improved, thereby effectively improving the clarity of the texture. Further, the thickness of the single-layer liquid crystal film is 2 to 3 microns, for example, the thickness of the single-layer liquid crystal film can be but not limited to 2 microns, 2.2 microns, 2.4 microns, 2.6 microns, 2.8 microns, 3 microns. Preferably, the thickness of the double-layer liquid crystal film is 4 to 6 microns.
[0028] It is understandable that by screen printing varnish on the surface of the liquid crystal film layer 15 to form the varnish layer 16, because the surface of the liquid crystal film layer 15 is relatively smooth, directly laminating the outer texture layer 17 on the surface of the liquid crystal film layer 15 may have a problem of insufficient adhesion. By first coating a layer of varnish layer 16 on the surface of the liquid crystal film layer 15, the varnish layer 16 can improve the adhesion between the outer texture layer 17 and the liquid crystal film layer 15 to ensure the stability of lamination. Further, the thickness of the varnish layer 16 is 5 to 8 microns, optionally, about 5 to 7 microns. As an example, the thickness of the varnish layer 16 can be, but not limited to, 5 microns, 6 microns, 7 microns, and 8 microns.
[0029] It can be understood that the outer texture layer 17 is formed by curing the curing liquid, and then the rubbing film of the desired texture structure is pressed on the surface of the curing layer, and then pre-cured by LED light, and then the rubbing film is removed to obtain the outer texture layer 17, which belongs to the outer texture structure formed by the transfer process, but is not limited to this method, as long as the method can form the structure of the outer texture layer 17. Further, the thickness of the outer texture layer 17 is 15 to 30 microns, optionally, about 15 to 25 microns, about 15 to 20 microns, about 20 to 30 microns, as an example, the thickness of the outer texture layer 17 can be but not limited to 15 microns, 20 microns, 25 microns, 30 microns.
[0030] In a preferred embodiment, please refer to Figure 2-Figure 3 In order to further improve the colorful effect, an inner texture layer 11 and a PVD layer 12 are arranged between the substrate layer 10 and the ink layer 13, that is, the first surface is sequentially provided with an inner texture layer 11, a PVD layer 12 and an ink layer 13. The inner texture layer 11 can be formed on the first surface of the substrate layer 10 by a UV transfer process, but is not limited thereto, and can also be achieved by laser technology. Further, the thickness of the inner texture layer 11 is 10 to 15 microns. As an example, the thickness of the inner texture layer 11 can be, but is not limited to, 10 microns, 11 microns, 12 microns, 13 microns, 14 microns, and 15 microns.
[0031] It can be understood that the PVD layer 12 is formed on the surface of the inner texture layer 11 by magnetron sputtering. Further, one or more metals, metal oxides or other inorganic substances are plated on the surface of the inner texture layer 11 by magnetron sputtering to form the PVD layer 12. Further, the thickness of the PVD layer 12 is 30-300nm, about 30-200nm, about 50-300nm. As an example, the thickness of the PVD layer 12 can be, but not limited to, 30nm, 60nm, 100nm, 150nm, 200nm, 250nm, and 300nm.
[0032] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the utility model rather than to limit the protection scope of the utility model. Although the utility model is described in detail with reference to the preferred embodiments, it is not limited to those listed in the embodiments. Ordinary technicians in this field should understand that the technical solution of the utility model can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the utility model.
Claims
1. A sheet metal mobile phone back cover, It is characterized in that The invention comprises a non-metallic substrate layer, wherein the substrate layer comprises a first surface and a second surface arranged opposite to each other, wherein the first surface is provided with an ink layer, and the second surface is provided with an adhesive layer, a liquid crystal film layer, a varnish layer and an outer texture layer in sequence.
2. The sheet mobile phone back cover according to claim 1, It is characterized in that The substrate layer is selected from a PMMA board, a PC board, a PET board or a PMMA / PC composite board.
3. The sheet mobile phone rear cover according to claim 2, It is characterized in that The PMMA / PC composite plate includes a stacked PMMA layer and a PC layer, wherein a surface of the PC layer away from the PMMA layer constitutes the first surface, and a surface of the PMMA layer away from the PC layer constitutes the second surface.
4. The sheet mobile phone rear cover according to claim 1, It is characterized in that The first surface is sequentially provided with an inner texture layer, a PVD layer and the ink layer.
5. The sheet mobile phone rear cover according to claim 4, It is characterized in that The thickness of the inner texture layer is 10 to 15 microns.
6. The sheet mobile phone rear cover according to claim 1, It is characterized in that The liquid crystal film layer includes a single-layer liquid crystal film, a double-layer liquid crystal film or a multi-layer liquid crystal film.
7. The sheet mobile phone rear cover according to claim 6, It is characterized in that The thickness of the single-layer liquid crystal film is 2 to 3 micrometers.
8. The sheet mobile phone rear cover according to claim 1, It is characterized in that The thickness of the ink layer is 25 to 40 microns.
9. The sheet mobile phone rear cover according to claim 1, It is characterized in that The thickness of the outer texture layer is 15 to 30 microns.
10. The sheet mobile phone rear cover according to claim 1, It is characterized in that The thickness of the varnish layer is 5 to 8 microns.