Display panel structure and OLED device
By setting up a raised and groove blocking mechanism made of non-organic materials between the blind hole area and the display area of the OLED display panel, the UV glue overflow problem is solved, and the optical transmittance and camera imaging effect are improved.
Patent Information
- Application Number
- CN202420053741.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-09
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-01-09
AI Technical Summary
In the blind hole screen of the OLED display panel, fluctuations in UV dispensing position accuracy cause colloid overflow, affecting optical transmittance and imaging effect of the front camera.
A barrier mechanism is provided between the blind hole area and the display area, with several protrusions and/or grooves made of non-organic material, and the width of the barrier mechanism is less than 50 μm, to prevent UV glue from overflowing.
It effectively reduces the risk of colloid overflow in the blind hole area, improves the stability of optical transmittance and the imaging effect of the camera.
Smart Images

Figure CN222073787U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of display devices, and in particular to a display panel structure and an OLED device. Background Art
[0002] Since mobile phones entered the era of full-screen displays, screen-to-body ratio has been a key parameter for major manufacturers to compete. The higher the screen-to-body ratio, the more shocking the phone's field of view will be, and the closer it is to a visual effect where the entire screen is visible. The front camera is one of the main factors that affect the phone's ability to achieve an extreme screen-to-body ratio. With the popularity of full-screen mobile phones, blind-hole screens have gradually come into everyone's field of vision.
[0003] OLED (Organic Light-Emitting Diode, also known as organic electroluminescent display) mobile phone screens include a substrate and a cover plate, which are combined through packaging. The blind hole screen using OLED screens means that the camera area of the screen is transparent, but there are no holes in the cover plate and substrate glass. External light passes through the two-layer structure of the cover plate and the substrate, and after multiple reflections in the interlayer, it finally reaches the camera. It not only affects the light transmittance, but also affects the imaging effect of the mobile phone's front camera to a certain extent.
[0004] Glue is dispensed and filled between the substrate and the cover plate in the corresponding area of the blind hole to ensure the transmittance of the blind hole area. At the same time, UV glue dispensing in the blind hole area has beneficial effects such as improving the Newton rings in the blind hole area, reducing the fluctuation of optical transmittance, and preventing abnormal shooting shapes when the camera passes through the blind hole area.
[0005] However, if Figure 1 As shown in , due to the fluctuation of the UV glue dispensing position accuracy, the UV glue 10 easily overflows along the material after contacting the organic material layer in the non-light-transmitting area. Figure 2 and Figure 3 As shown in FIG. 1 , the overflowed UV glue 10 cannot be cured, and the uncured glue affects the organic material layer in the surrounding display area, resulting in display abnormality or reliability failure.
[0006] Therefore, the utility model provides a novel display panel structure and OLED device that reduce the risk of colloid overflowing out of the blind hole area. Utility Model Content
[0007] In view of the problems in the prior art, the purpose of the present invention is to provide a display panel structure and an OLED device, which can effectively reduce the risk of colloid overflowing out of the blind hole area.
[0008] According to one aspect of the utility model, a display panel structure is provided, which is suitable for an organic electroluminescent device. The display panel structure includes a substrate and a cover plate. A blind hole area and a display area are provided on the substrate. A blocking mechanism is also provided between the blind hole area and the display area. The blocking mechanism is made of non-organic material and includes a plurality of protrusions and / or grooves.
[0009] Preferably, the width of the blocking mechanism is less than 50 μm.
[0010] Preferably, the blocking mechanism is a plurality of protrusions.
[0011] Preferably, the number of the protrusions is ≥ 2, the widths of the protrusions are the same or different, and the heights of the protrusions are the same or different.
[0012] Preferably, the blocking mechanism is a plurality of grooves.
[0013] Preferably, the blocking mechanism is made of inorganic material and / or metal.
[0014] Preferably, the blocking mechanism is made of silicon oxide and / or silicon nitride.
[0015] Preferably, the blocking mechanism is made of one or more of molybdenum, Al, and Ti.
[0016] According to another aspect of the present invention, an OLED device is provided, comprising the above-mentioned display panel structure.
[0017] The utility model provides a display panel structure and an OLED device, which can effectively reduce the risk of colloid overflowing outwards in a blind hole area. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Other features, objectives and advantages of the present invention will become more apparent by reading the detailed description of non-limiting embodiments made with reference to the following drawings.
[0019] Figure 1 It is a schematic diagram of the structure of the colloid overflowing outwards in the blind hole area of the prior art;
[0020] Figure 2 It is a schematic diagram of the structure in which the colloid in the blind hole area of the prior art overflows outward and cannot be solidified;
[0021] Figure 3 It is a schematic diagram of the structure in which the colloid in the blind hole area of the prior art overflows outward and cannot be solidified;
[0022] Figure 4 It is a structural schematic diagram of an embodiment of the utility model;
[0023] Figure 5 This is a schematic diagram of the structure of the embodiment of the utility model when dispensing glue;
[0024] Figure 6 It is a schematic diagram of the structure of the embodiment of the utility model during deposition;
[0025] Figure 7 It is a schematic diagram of the structure of the embodiment of the utility model during etching;
[0026] Figure 8 It is a schematic structural diagram of another embodiment of the utility model during etching. DETAILED DESCRIPTION
[0027] Example embodiments will now be described more fully with reference to the accompanying drawings. However, example embodiments can be implemented in a variety of forms and should not be construed as limited to the embodiments set forth herein. Instead, these embodiments are provided so that the present invention will be comprehensive and complete and fully convey the concepts of the example embodiments to those skilled in the art. The same reference numerals in the figures represent the same or similar structures, and thus their repeated description will be omitted.
[0028] like Figure 4 As shown in the embodiment of the utility model, a display panel structure and an OLED device include a substrate 1 and a blind hole area 2 and a functional area 3 arranged on the substrate 1. A blocking mechanism (5, 6) is also provided between the blind hole area 2 and the functional area 3. The blocking mechanism (5, 6) is made of non-organic material. The blocking mechanism (5, 6) includes a plurality of protrusions 5 and / or grooves 6.
[0029] The OLED panel to which the embodiment of the utility model is applicable is provided with a light-transmitting area and a non-light-transmitting area. The light-transmitting area is mainly formed by the optically transparent adhesive part on the substrate 1, mainly formed by the blind hole area 2 on the substrate 1, or the blind hole area 2 and the blocking mechanism (5, 6).
[0030] The OLED panel of the embodiment of the utility model is mainly filled with optically transparent glue in the blind hole area 2, preferably UV glue curing, which has beneficial effects such as improving Newton rings in the blind hole area and reducing optical transmittance fluctuations.
[0031] like Figure 4 As shown in FIG. 1 , the blind hole region 2 and the functional region 3 are connected, and the blocking mechanism ( 5 , 6 ) is located between the blind hole region 2 and the functional region 3 .
[0032] A glue dispensing position 4 is preset in the blind hole area 2 so as to perform glue dispensing at this position.
[0033] Due to the existence of the blocking mechanism (5, 6), and the blocking mechanism (5, 6) is made of non-organic material, the optically transparent adhesive made of organic material will not overflow to the functional area on the substrate, that is, the residual area of the vapor deposition layer in the non-light-transmitting area. The optically transparent adhesive is located in the blocking mechanism, that is, the blocking mechanism surrounds the optically transparent adhesive to prevent it from overflowing.
[0034] A display panel structure and an OLED device according to an embodiment of the utility model can effectively reduce the risk of colloid overflowing outward from the blind hole area by forming a blocking mechanism at the periphery of the blind hole glue dispensing position.
[0035] In the embodiment of the utility model, the blocking mechanism (5, 6) can be a plurality of protrusions 5, or a plurality of grooves 6, or a combination of a plurality of protrusions 5 and grooves 6.
[0036] In the embodiment of the utility model, the cross-sectional shape of the blind hole and the blind hole area 2 is preferably substantially circular. The dispensing position 4 is within the blind hole and the blind hole area 2, preferably substantially at the center of the circle and its periphery.
[0037] like Figure 4 As shown in the embodiment of the present invention, the area of the glue dispensing position 4 is preferably slightly smaller than or approximately equal to the area of the blind hole area 2. That is, the optically transparent glue formed by the glue dispensing will eventually be located in the blind hole area 2, or slightly overflow the blind hole area 2, but be blocked by the blocking mechanism (5, 6), and eventually will not overflow the blocking mechanism (5, 6).
[0038] Another example Figure 4 As shown in FIG, the protrusion 5 is preferably arranged circumferentially on the periphery of the dispensing position 4 to surround the dispensing position 4 to better prevent the colloid in the blind hole area from overflowing. The blind hole area 2 is connected to the functional area 3 through the protrusion 5 and the groove 6.
[0039] Another example Figure 4 As shown in FIG. 1 , in an embodiment of the present utility model, the protrusion 5 and the groove 6 are preferably close to the functional area 3 and away from the glue dispensing position 4 to avoid affecting the space occupied by the glue.
[0040] It is also preferred that the width of the blocking mechanism (5, 6) is less than 50 μm to avoid being too large and affecting the performance of the panel.
[0041] In addition, in the embodiment of the present utility model, in order to effectively prevent the colloid in the blind hole area from overflowing outward, the material for making the protrusion 5 is preferably selected from a material with low wettability to the colloid.
[0042] Since the filling colloid is generally fixed by UV, the colloid is generally a shadowless glue. The main component of the shadowless glue is organic matter. Therefore, the protrusion 5 is preferably an inorganic material or a metal. Figure 5As shown in , when UV glue is dispensed on the embodiment of the utility model, since the protrusion 5 has low wettability to the UV glue and the protrusion 5 has a height and is blocked by the groove 6, the UV glue tends to overflow inward after contacting the protrusion 5, reducing the risk of the colloid overflowing outward.
[0043] like Figure 6-8 As shown in , in preparing the embodiment of the present utility model, the protrusion 5 and the groove 6 of the present embodiment can be prepared at the same time when the inorganic or metal layer and the blind hole on the substrate 1 are prepared.
[0044] like Figure 6 As shown in FIG. 1 , an inorganic or metallic layer is deposited on a substrate 1 .
[0045] like Figure 7 As shown in FIG. 1 , when etching an inorganic or metal layer on a substrate 1 , protrusions 5 and grooves 6 can be etched on the inner circumference.
[0046] like Figure 8 As shown in FIG. 1 , three protrusions 5 are etched on the substrate 1 and three grooves 6 are formed. The widths of the three protrusions 5 may be the same or not completely the same or completely different. Similarly, the widths of the three grooves 6 may be the same or not completely the same or completely different, so as to effectively reduce the risk of colloid overflowing out of the blind hole area.
[0047] The present invention is described below with reference to the accompanying drawings and in conjunction with specific embodiments:
[0048] Example 1
[0049] like Figure 4 As shown in the figure, a display panel structure and an OLED device include a substrate 1 and a blind hole area 2 and a functional area 3 arranged on the substrate 1.
[0050] A glue dispensing position 4 is preset in the blind hole area 2 so as to perform glue dispensing at this position.
[0051] A protrusion 5 is further provided between the blind hole area 2 and the functional area 3 . The protrusion 5 is provided on the substrate 1 .
[0052] A groove 6 is formed between the protrusion 5 and the functional area 3 , and the groove 6 is also arranged on the substrate 1 .
[0053] The cross section of the blind hole area 2 is roughly circular. The protrusion 5 is circumferentially arranged on the periphery of the dispensing position 4, and is roughly annular in shape and has a trapezoidal cross section, surrounding the dispensing position 4 to better prevent the colloid in the blind hole area from overflowing outward.
[0054] When UV glue is dispensed on the embodiment of the utility model, since the protrusion 5 has low wettability to the UV glue and the protrusion 5 has a height and is blocked by the groove 6, the UV glue tends to overflow inward after contacting the protrusion 5, reducing the risk of the colloid overflowing outward.
[0055] In summary, the display panel structure and device of the utility model can effectively reduce the risk of colloid overflowing out of the blind hole area.
[0056] The above contents are further detailed descriptions of the present invention in combination with specific preferred implementations, and the specific implementation of the present invention cannot be considered to be limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.
Claims
1. A display panel structure, suitable for an organic electroluminescent device, the display panel structure comprising a substrate and a cover plate, the substrate being provided with a blind hole area and a display area, the blind hole area being filled with an optically transparent glue, characterized in that: A blocking mechanism is also provided between the blind hole area and the display area. The blocking mechanism is made of a non-organic material and includes a plurality of protrusions and / or grooves.
2. The display panel structure according to claim 1, characterized in that: The width of the blocking mechanism is less than 50 μm.
3. The display panel structure according to claim 1, characterized in that: The blocking mechanism is a plurality of protrusions.
4. The display panel structure according to claim 1, characterized in that: The number of the protrusions is ≥2, and the widths of the protrusions are the same or different, and the heights of the protrusions are the same or different.
5. The display panel structure according to claim 1, characterized in that: The blocking mechanism is a plurality of grooves.
6. The display panel structure according to claim 1, characterized in that: The blocking mechanism is made of inorganic material and / or metal.
7. The display panel structure according to claim 6, characterized in that: The blocking mechanism is made of silicon oxide and / or silicon nitride.
8. The display panel structure according to claim 6, characterized in that: The blocking mechanism is made of one or more of molybdenum, Al, and Ti.
9. An OLED device, characterized in that: Comprising the display panel structure according to any one of claims 1-8.