Power switching device structure
By setting the polysilicon layer segmentation blocking voltage in the trench structure of the power switching device, reducing the thickness of the isolation oxide layer, the problem of high on-resistance in the prior art is solved, and the effect of high blocking voltage and low on-resistance is achieved , expanding the scope of application.
Patent Information
- Application Number
- CN202420646497.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-29
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-03-29
AI Technical Summary
In high blocking voltage applications, existing power switching devices have high on-resistance and increased thickness of the isolation oxide layer, limiting their application range, especially when the blocking voltage exceeds 200 volts.
By spaced at least two polysilicon layers along the direction of the semiconductor substrate in the trench structure, the blocking voltage is divided, and isolation oxidation is provided between adjacent polysilicon layers and between the polysilicon layer and between the bottom surface of the trench structure. layer, reduces the thickness of the isolation oxide layer and reduces the on-resistance.
The power switching device structure with high blocking voltage and low specific on-resistance is realized, which avoids stress problems caused by the increase in the thickness of the isolation oxide layer and expands the application range of the device.
Smart Images

Figure CN222088608U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of semiconductors, in particular to a power switch device structure. Background Art
[0002] The structure of all power switching devices includes a drift region (Drift Region), which can withstand a blocking voltage (Blocking Voltage). Figure 1a The structure of a power switch device with a conventional drift region is shown, which includes a drain metal layer 0132, an n-type substrate 011 located on the drain metal layer 0132, a drift region 012 located on the n-type substrate 011, and a source metal layer 0131 located on the drift region 012. Figure 1b , the voltage results in a triangular electric field distribution in the uniformly doped drift region 012, where the slope of the field distribution is determined by the doping concentration of the drift region 012. The maximum voltage (breakdown voltage, BV) that the drift region 012 can withstand is determined by the maximum electric field (Em) that reaches the critical electric field (Ec) for the semiconductor material to break down. The critical electric field and the doping concentration of the drift region 012 determine the maximum depletion width (WD), i.e.
[0003] WD=2×BV / Ec (1)
[0004] The specific on-resistance (Ron.sp, resistance per unit area) of the ideal drift region 012 can be given by the following formula:
[0005] Ron.sp=WD / (q×μn×ND) (2)
[0006] Where q is the charge, μn is the electron mobility, and ND is the doping concentration of the drift region.
[0007] The doping concentration in the drift region 012 required to obtain the breakdown voltage can be given by the following formula:
[0008] ND=εs×Ec×Ec / (2×q×BV) (3)
[0009] Where εs is the dielectric constant of the semiconductor material.
[0010] Combining equations (1), (2) and (3), we get the ideal drift region specific on-resistance:
[0011] Ron.sp=4×BV×BV / (εs×μn×Ec×Ec×Ec) (4)
[0012] It can be seen from the above formula that the specific on-resistance has a strong dependence on the critical electric field, and the specific on-resistance is proportional to the cube of the critical electric field.
[0013] Figure 2a A charge coupling structure with a two-dimensional electric field (i.e., the power switching device structure is a charge coupling structure with a two-dimensional electric field) is shown, and its drift region has a trench electrode, specifically including a drain metal layer 0232, an n-type substrate 021 located on the drain metal layer 0232, a drift region 022 located on the n-type substrate 021, a Schottky contact structure 024 located on the drift region 022, a trench structure (not marked in the figure) located in the drift region 022, a polysilicon layer (i.e., a trench electrode) 025 located in the trench structure, an isolation oxide layer 026 located between the polysilicon layer 025 and the trench structure (bottom surface and sidewalls), and a source metal layer 0231 located on the polysilicon layer 025. The charge coupling structure has a two-dimensional charge coupling effect, that is, a junction in the x direction (for example, a junction formed by a Schottky contact) and another junction in the y direction (for example, a junction formed by the polysilicon layer 025, the isolation oxide layer 026, and the drift region 022 under the source metal layer 0231) generate depletion layers in two directions in the drift region 022 and interact with each other, and the voltage blocking capability is enhanced by extending the depletion layer in the two-dimensional direction. A horizontal PN junction can also be used in the charge coupling structure instead of a Schottky junction. The horizontal PN junction promotes the extension of the depletion region along the y direction, while the vertical trench structure with a trench electrode inside promotes the extension of the depletion region in the x direction. Figure 2b Shows Figure 2a The electric field distribution corresponding to the charge coupling structure in the figure. It has been found that the highest breakdown voltage generated by the charge can be given by the following formula:
[0014] Qoptimum=q×ND×WN / 2=εs×Ec (5)
[0015] Wherein, Qoptimum is the optimal charge coupling amount per unit area, and WN is the width of the drift region 022 between the two trenches.
[0016] The depth of the trench structure can be given by the following formula:
[0017] t=BV / Ec (6)
[0018] Wherein, t is the depth of the trench structure.
[0019] The specific on-resistance (RD.sp, resistance per unit area) of the ideal drift region 022 can be given by the following formula:
[0020] RD.sp=t×p / (q×μn×ND×WN) (7)
[0021] Where p is the unit pitch.
[0022] Combining equations (5), (6) and (7), the specific on-resistance of the ideal drift region with a two-dimensional electric field structure is obtained:
[0023] RD.sp=BV×p / (2×es×μn×Ec×Ec)(8)
[0024] By comparing formula (8) with formula (4) in the one-dimensional case, it can be observed that the specific on-resistance in the one-dimensional electric field structure is proportional to the square of the breakdown voltage, while the specific on-resistance of the charge-coupled device increases linearly with the breakdown voltage. Although the charge-coupled device increases the blocking voltage capability and reduces the on-resistance, a thick isolation oxide layer is required on the sidewall of the trench structure and the bottom surface of the trench structure, and the equidistant potential lines in the isolation oxide layer on the bottom surface of the trench structure are very dense (see Figure 2a ).
[0025] For high blocking voltage applications, the above-mentioned charge coupling structure needs to increase the thickness of the isolation oxide layer (since the maximum electric field strength of the isolation oxide layer is limited to 2×10 6 V / cm, for every 100 volt increase, the thickness of the isolation oxide layer on the sidewall and bottom of the trench structure needs to increase by 0.5 microns). This will cause the isolation oxide layer in the trench structure to be very thick, which will generate strong stress between the drift region (silicon) and the isolation oxide layer (silicon oxide) interface and increase the cell spacing, which will increase the specific on-resistance. Therefore, the above-mentioned charge coupling structure is currently limited to applications with blocking voltages below 200 volts.
[0026] See also Figure 3 The above structure can also be used in an edge terminal structure to avoid a drop in blocking voltage at the edge. The edge terminal structure may include a drain metal layer 0332, an n-type substrate 031 located on the drain metal layer 0332, a drift region 032 located on the n-type substrate 031, a trench structure (not shown in the figure) located in the drift region 032, a polysilicon layer (i.e., a trench electrode) 035 located in the trench structure, an isolation oxide layer 036 located between the polysilicon layer 035 and the trench structure (sidewalls and bottom surface), and a source metal layer 0331 located on the polysilicon layer 035, wherein the isolation oxide layer 036 also extends from the sidewalls of the trench structure to the drift region 032, and the source metal layer 0331 extends to cover a portion of the isolation oxide layer 036. In this structure, the surface at the edge is covered by the isolation oxide layer 036 and connected to the isolation oxide layer 036 on the sidewall of the trench structure, and the source metal layer 0331 is expanded to cover a portion of the isolation oxide layer 036 at the edge. However, due to the same reasons mentioned above, this edge terminal structure is also limited to a blocking voltage of less than 200V.
[0027] In patent application US6110804A, a floating field conductor has been arranged on the top surface of the FET drift region to provide field shaping for the lateral MOSFET at the surface of the drift region. Charges are injected into the floating field conductor so that a depletion region is formed in the drift region. However, the two-dimensional charge coupling is not effective, especially in areas far from the surface, so the improvement of the blocking voltage is not obvious. In addition, the gate electrode transfer capacitance and output capacitance are not improved, and the current density is also low.
[0028] In patent application US8592906A, a lateral MOSFET is described, which has a source and a drain extending along the top surface of a semiconductor substrate, and an active region is arranged between the source region and the drain region in the semiconductor substrate, and the active region is arranged adjacent to a segmented field plate extending from the source region to the drain region, thereby also achieving a two-dimensional charge coupling effect. This structure is easy to implement. However, this structure has a small current density, a high specific on-resistance, and a high transfer capacitance, and is therefore not suitable for high power and high voltage applications. Utility Model Content
[0029] The utility model aims to provide a power switch device structure to obtain a power switch device structure with high blocking voltage and low specific on-resistance.
[0030] In order to achieve the above-mentioned purpose and other related purposes, the utility model provides a power switch device structure, including:
[0031] Drain metal layer;
[0032] A semiconductor substrate, located on the drain metal layer;
[0033] A first conductive type drift region, located on the semiconductor substrate;
[0034] A trench structure located in the first conductive type drift region;
[0035] At least two polysilicon layers are spaced apart and arranged in the trench structure along a direction perpendicular to the semiconductor substrate;
[0036] An isolation oxide layer, located between adjacent polysilicon layers, between the bottom polysilicon layer and the bottom surface of the trench structure, and on the sidewalls of the trench structure;
[0037] The source metal layer is located on the polysilicon layer.
[0038] Optionally, in the power switch device structure, the blocking voltage of the power switch device structure is equal to the sum of the potential difference between all two adjacent polysilicon layers and the potential difference between the bottom polysilicon layer and the bottom surface of the trench structure.
[0039] Optionally, in the power switching device structure, the potential difference between the two adjacent polysilicon layers is obtained according to the thickness of the isolation oxide layer between the two adjacent polysilicon layers, and the potential difference between the bottom polysilicon layer and the bottom surface of the trench structure is obtained according to the thickness of the isolation oxide layer between the bottom polysilicon layer and the bottom surface of the trench structure, and when the thickness of the isolation oxide layer between the two adjacent polysilicon layers is equal to the thickness of the isolation oxide layer between the bottom polysilicon layer and the bottom surface of the trench structure, the corresponding potential differences are the same.
[0040] Optionally, in the power switch device structure, the power switch device structure further includes a Schottky contact structure or a second conductivity type doped region located on the first conductivity type drift region.
[0041] Optionally, in the power switching device structure, when the power switching device structure includes a second conductive type doped region, the power switching device structure also includes a first conductive type source region located on the second conductive type doped region and a gate oxide layer, a gate electrode and a dielectric layer located in sequence between the polysilicon layer at the top of the trench structure and the source metal layer.
[0042] Optionally, in the power switch device structure, the first conductivity type is n-type, and the second conductivity type is p-type; or, the first conductivity type is p-type, and the second conductivity type is n-type.
[0043] Optionally, in the power switching device structure, the power switching device structure further includes a top oxide layer located on the first conductive type drift region, the top oxide layer is connected to the isolation oxide layer, and the source metal layer extends onto a portion of the top oxide layer.
[0044] Optionally, in the power switch device structure, the smaller the thickness of the isolation oxide layer between the two adjacent polysilicon layers, the smaller the thickness of the polysilicon layer on the isolation oxide layer.
[0045] Compared with the prior art, the technical solution of the utility model has the following beneficial effects:
[0046] In the power switch device structure provided by the utility model, at least two polysilicon layers are arranged in a direction perpendicular to the semiconductor substrate in the trench structure, and the blocking voltage is divided, so that the utility model does not increase the thickness of the isolation oxide layer on the side wall and the bottom surface of the trench structure as the blocking voltage of the power switch device structure increases. Moreover, the potential difference between the two adjacent polysilicon layers and the potential difference between the bottom polysilicon layer and the bottom surface of the trench structure of the utility model are both less than the blocking voltage of the power switch device structure, so that the thickness of the isolation oxide layer on the bottom surface of the trench structure and the isolation oxide layer on the side wall of the trench structure is reduced, which can reduce the stress at the interface between the first conductive type drift region and the isolation oxide layer, and thus reduce the specific on-resistance. Therefore, the utility model can obtain a power switch device structure with high blocking voltage and low specific on-resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] Figure 1a A schematic diagram of the structure of a power switch device with a traditional drift region;
[0048] Figure 1b for Figure 1a The electric field distribution diagram under the blocking voltage corresponding to the power switching device in;
[0049] Figure 2a It is a schematic diagram of the structure of a charge coupling structure with a two-dimensional electric field and a distribution diagram of equidistant potential lines under blocking voltage;
[0050] Figure 2b for Figure 2a The electric field distribution diagram under blocking voltage corresponding to the charge coupling structure in the figure;
[0051] Figure 3 It is a structural schematic diagram of an edge terminal structure and a distribution diagram of equidistant potential lines under blocking voltage;
[0052] Figure 4 A schematic diagram of the structure of a power switch device according to an embodiment of the utility model and a distribution diagram of equidistant potential lines under blocking voltage;
[0053] Figure 5 A schematic diagram of the structure of a power switch device according to another embodiment of the utility model and a distribution diagram of equidistant potential lines under blocking voltage;
[0054] Figure 6 It is a schematic diagram of the structure of the power switch device in the utility model applied to a vertical MOSFET and a distribution diagram of equidistant potential lines under blocking voltage;
[0055] Figure 7 It is a schematic diagram of the structure of the power switch device structure in the utility model applied to the edge terminal structure MOSFET. DETAILED DESCRIPTION
[0056] The power switch device structure proposed by the utility model is further described in detail below in combination with the accompanying drawings and specific embodiments. According to the following description, the advantages and features of the utility model will become clearer. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, which are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the utility model.
[0057] See also Figure 4 The utility model provides a power switch device structure, including:
[0058] Drain metal layer 132;
[0059] A semiconductor substrate 11, located on the drain metal layer 132;
[0060] A first conductive type drift region 12, located on the semiconductor substrate 11;
[0061] The trench structure (not marked in the figure) is located in the first conductive type drift region 12 .
[0062] At least two polysilicon layers 15 are spaced apart and arranged in the trench structure along a direction perpendicular to the semiconductor substrate 11;
[0063] An isolation oxide layer 16, located between adjacent polysilicon layers 15, between the bottom polysilicon layer 15 and the bottom surface of the trench structure, and on the sidewalls of the trench structure;
[0064] The source metal layer 131 is located on the polysilicon layer 15 .
[0065] In this embodiment, the drain metal layer 132 and the source metal layer 131 may be made of conventional electrode materials, such as Ti (titanium), Ni (nickel) and Pt (platinum), but are not limited thereto. The source metal layer 131 is electrically connected to the polysilicon layer 15 .
[0066] The semiconductor substrate 11 is located on the drain metal layer 132, and the semiconductor substrate 11 is preferably a semiconductor substrate of the first conductivity type. The first conductivity type is n-type, and the second conductivity type is p-type; or, the first conductivity type is p-type, and the second conductivity type is n-type. The following content is explained by taking the first conductivity type as n-type and the second conductivity type as p-type as an example. That is, in this embodiment, the semiconductor substrate of the first conductivity type is an n-type semiconductor substrate, and is preferably a heavily doped n-type semiconductor substrate, and its doping concentration can be set according to the semiconductor substrate of the power switching device in the prior art, which will not be elaborated here.
[0067] The first conductive type drift region 12 is located on the semiconductor substrate 11. The material of the first conductive type drift region 12 is preferably single crystal silicon, but is not limited thereto. The thickness of the first conductive type drift region 12 depends on the blocking voltage. The higher the required blocking voltage, the greater the thickness of the first conductive type drift region 12. For example, the thickness of the first conductive type drift region 12 required to achieve a blocking voltage of 400V is at least 20 microns. Therefore, the thickness of the first conductive type drift region 12 can be set according to the blocking voltage requirement. In the present embodiment, the first conductive type drift region 12 is an n-type drift region, which is doped with n-type ions, such as phosphorus. The doping concentration of the n-type ions can adopt the doping concentration in the drift region of the power switching device in the prior art, which will not be elaborated here.
[0068] The trench structure is located in the first conductive type drift region 12. In this embodiment, the depth of the trench structure is less than the depth of the first conductive type drift region 12, that is, there is a small space between the bottom surface of the trench structure and the bottom surface of the first conductive type drift region 12. The depth of the trench structure can be set according to formula (6), where the critical electric field (Ec) is a set value, which can be set according to process requirements, for example, 2×10 5 The depth of the trench structure of this embodiment must be adjusted to achieve the desired breakdown voltage.
[0069] In this embodiment, at least two polysilicon layers 15 are arranged in the trench structure along a direction perpendicular to the semiconductor substrate 11 (y direction), and the isolation oxide layer 16 is arranged between adjacent polysilicon layers 15, between the bottom polysilicon layer 15 and the bottom surface of the trench structure, and on the sidewalls of the trench structure, and the isolation oxide layer 16 located on the sidewalls and bottom surface of the trench structure isolates the polysilicon layer 15 from the first conductive type drift region 12. The polysilicon layer 15 in this embodiment can be used as a trench electrode. The polysilicon layer 15 is preferably doped with the first conductive type ions, that is, the material of the polysilicon layer 15 in this embodiment is preferably highly doped n-type polysilicon, and its doping concentration can adopt the doping concentration of the polysilicon layer in the power switch device in the prior art, which will not be described in detail here. The material of the isolation oxide layer 16 is preferably silicon dioxide, but is not limited thereto. Compared with the entire polysilicon layer in the trench structure of the prior art, the entire polysilicon layer in the trench structure is divided into at least two sections in this embodiment.
[0070] The blocking voltage of the power switch device structure is equal to the sum of the potential difference between all two adjacent polysilicon layers 15 and the potential difference between the bottom polysilicon layer 15 and the bottom surface of the trench structure. The potential difference between the two adjacent polysilicon layers 15 is determined by the thickness of the isolation oxide layer 16 between the two adjacent polysilicon layers 15 (i.e., the potential difference between the two adjacent polysilicon layers 15 is obtained according to the thickness of the isolation oxide layer 16 between the two adjacent polysilicon layers 15), and the potential difference between the bottom polysilicon layer 15 and the bottom surface of the trench structure is determined by the thickness of the isolation oxide layer 16 on the bottom surface of the trench structure (i.e., the potential difference between the bottom polysilicon layer 15 and the bottom surface of the trench structure is obtained according to the thickness of the isolation oxide layer 16 between the bottom polysilicon layer 15 and the bottom surface of the trench structure). In this embodiment, the thickness of the isolation oxide layer 16 between adjacent polysilicon layers 15 may be the same or different. The thickness of the isolation oxide layer 16 between two adjacent polysilicon layers 15 and the thickness of the isolation oxide layer 16 on the bottom surface of the trench structure (i.e., the isolation oxide layer 16 between the bottom polysilicon layer 15 and the bottom surface of the trench structure) can be the same or the same. When the thickness of the isolation oxide layer 16 between the two adjacent polysilicon layers 15 is equal to the thickness of the isolation oxide layer 16 between the bottom polysilicon layer 15 and the bottom surface of the trench structure, the corresponding potential differences are the same, i.e., the potential difference between the two adjacent polysilicon layers 15 is equal to the potential difference between the bottom polysilicon layer 15 and the bottom surface of the trench structure. For example, the power switch device structure in FIG. 4 has two polysilicon layers 15, and the two polysilicon layers 15 are a first polysilicon layer 151 and a second polysilicon layer 152. In the case where the thickness of the spacer oxide layer 16 between the first polysilicon layer 151 and the second polysilicon layer 152 is equal to the thickness of the spacer oxide layer 16 between the first polysilicon layer 151 and the bottom surface of the trench structure, the potential difference between the first polysilicon layer 151 and the second polysilicon layer 152 is equal to the potential difference between the first polysilicon layer 151 and the bottom surface of the trench structure, and both are equal to half of the blocking voltage. In this embodiment, under the condition of a certain blocking voltage, equidistant potential lines are uniformly distributed in the spacer oxide layer 16 between the first polysilicon layer 151 and the second polysilicon layer 152 and the spacer oxide layer 16 between the first polysilicon layer 151 and the bottom surface of the trench structure. For another example, for a blocking voltage of 400V and a desired potential difference between two adjacent polysilicon layers 15 equal to 200V, two polysilicon layers are required. This means that the potential difference between the two polysilicon layers and between the bottom polysilicon layer and the bottom surface of the trench structure is the same and equal to 200 V, so the thickness of the isolation oxide layer therebetween should be 1 micron. In addition, the thickness of the isolation oxide layer on the sidewall of the trench structure can also be 1 micron.In the case of a trench structure without trench electrode separation in the prior art, the thickness of the isolation oxide layer on the bottom surface and the sidewall of the trench structure should be 2 microns. Therefore, compared with the prior art, the thickness of the isolation oxide layer on the bottom surface of the trench structure and the sidewall of the trench structure in this embodiment is reduced, which will reduce the stress between the isolation oxide layer and the first conductive type drift region, thereby reducing the specific on-resistance.
[0071] In this embodiment, the potential difference between the first polysilicon layer 151 and the bottom surface of the trench structure should actually be the potential difference between the first polysilicon layer 151 and the first conductive type drift region 12, but the potential drop in the first conductive type drift region 12 below the bottom surface of the trench structure is very small and can be ignored. Therefore, the electric field strength in the isolation oxide layer 16 does not exceed 2×10 6 V / cm, the thickness of the isolation oxide layer therebetween (the isolation oxide layer 16 between the second polysilicon layer 152 and the first polysilicon layer 151 and the isolation oxide layer 16 between the first polysilicon layer 151 and the bottom surface of the trench structure) can also be reduced to half of the thickness required for the same blocking voltage in the prior art. The more polysilicon layers 15 there are in this embodiment, the more the thickness of the isolation oxide layer 16 therebetween is reduced. At the same time, for the same blocking voltage, the thickness of the isolation oxide layer 16 on the sidewall of the trench structure can also be reduced to about half of the required thickness in the prior art.
[0072] In this embodiment, the isolation oxide layer 16 between the polysilicon layers 15 and the isolation oxide layer 16 between the bottom polysilicon layer 15 and the bottom surface of the trench structure (i.e., the middle oxide layer) can withstand the potential difference that the isolation oxide layer 16 on the side wall of the trench structure also needs to be able to withstand. Therefore, the thickness of the isolation oxide layer 16 on the side wall of the trench can be greater than or equal to the thickness of the middle isolation oxide layer 16, and of course, it can also be slightly smaller than the thickness of the middle isolation oxide layer 16, mainly because the first conductive type drift region 12 can withstand a very small part of the voltage.
[0073] In order to further reduce the thickness of the isolation oxide layer on the side wall of the trench structure and the specific on-resistance, more polysilicon layers 15 can be provided. For example, for an application with a blocking voltage of 400V, if four polysilicon layers are provided in the trench structure, and the potential difference between two adjacent polysilicon layers is equal to 100V, the thickness of the isolation oxide layer between the polysilicon layers and the thickness of the isolation oxide layer between the bottom polysilicon layer and the bottom surface of the trench structure are both 0.5 microns. In addition, the thickness of the isolation oxide layer on the wall of each trench side structure is also equal to 0.5 microns, and the thickness of each polysilicon layer is equal to (20–4×0.5) / 4=18 / 4=4.5 microns, where 20 is the depth of the trench structure. Compared with the case where the potential difference between two adjacent polysilicon layers is 200V (two polysilicon layers are provided), the thickness of the isolation oxide layer corresponding to the case where the potential difference between adjacent polysilicon layers is 100V is further reduced. However, the manufacturing process steps of this structure are also increased. In applications, it is necessary to balance the contradiction between improving performance by reducing the thickness of the isolation oxide layer and increasing the manufacturing process steps and increasing the manufacturing cost to achieve the best effect.
[0074] In this embodiment, the smaller the thickness of the isolation oxide layer 16 is, the smaller the thickness of the polysilicon layer 15 adjacent to the isolation oxide layer 16 is, so that the distribution of the electric field will be more uniform. This embodiment uses the design of the polysilicon layer to easily produce a two-dimensional charge coupling effect, and will not increase the thickness of the isolation oxide layer on the side wall and bottom surface of the trench structure. This embodiment will not increase the thickness of the isolation oxide layer on the side wall and bottom of the trench structure as the blocking voltage increases, and will not increase the specific on-resistance. Moreover, as the number of polysilicon layers in the trench structure increases, the thickness of the isolation oxide layer on the side wall and bottom surface of the trench structure will decrease, which can reduce the stress at the interface between the first conductive type drift region and the isolation oxide layer, reduce the cell spacing, and reduce the specific on-resistance. Therefore, the utility model can obtain a power switch device structure with high blocking voltage and low specific on-resistance.
[0075] Continuing to refer to 4, the power switch device structure is a charge coupling structure of a two-dimensional electric field, and the power switch device structure further includes: a Schottky contact structure 14 or a second conductive type doped region located on the first conductive type drift region 12. The junction on the surface of the first conductive type drift region 12 can be a Schottky junction formed by the Schottky contact structure 14 through the Schottky contact (see Figure 4), or a PN junction formed by the second conductive type doping region through the second conductive type doping. For example, if the first conductive type drift region 12 is an n-type drift region, the junction on the surface of the n-type drift region can be a Schottky junction or a PN junction formed by a p-type doping region. For another example, if the first conductive type drift region 12 is a p-type drift region, the junction on the surface of the p-type drift region can be a Schottky junction or a PN junction formed by an n-type doping region. The material of the Schottky contact structure 14 is preferably metal. In this embodiment, the Schottky contact structure 14 or the second conductive type doping region can be arranged and prepared by the Schottky contact structure and the second conductive type doping region in the power switching device structure of the prior art, which will not be described in detail here. For example, when the power switching device structure is applied to a vertical MOSFET, the junction on the surface of the first conductive type drift region 12 is a PN junction. When the power switching device structure is a charge coupling structure of a two-dimensional electric field, and when the power switching device structure includes a second conductive type doped region, the power switching device structure may also include a first conductive type source region located on the second conductive type doped region and a gate oxide layer, a gate electrode, and a dielectric layer located in sequence between the polysilicon layer 15 at the top of the trench structure and the source metal layer 131.
[0076] See also Figure 5 In another embodiment, the power switch device structure is an edge terminal structure to improve the blocking voltage capability of the edge of the trench structure. Figure 4 The difference between the charge coupling structure in the embodiment of the present invention is that the edge terminal structure grows a top oxide layer 17 on the surface of the first conductive type drift layer 12 on one side of the trench structure, instead of growing a Schottky contact structure 14 or a second conductive type doped region, and there is no need to set a gate oxide layer, a gate electrode and a dielectric layer. In addition, the source metal layer 131 is extended to cover part of the top oxide layer 17 to improve the shielding of the electric field, thereby further avoiding a reduction in the breakdown voltage on the surface.
[0077] In this embodiment, the top oxide layer 17 is connected to the isolation oxide layer 16, and the materials of the top oxide layer 17 and the isolation oxide layer 16 are preferably the same. The thickness of the top oxide layer 17 can be set by the thickness of the top oxide layer of the power switch device in the prior art, which will not be described in detail here.
[0078] This embodiment utilizes the above-mentioned design of the polysilicon layer, which can easily produce a two-dimensional charge coupling effect without increasing the thickness of the isolation oxide layer on the sidewall and bottom surface of the trench structure.
[0079] In addition, the utility model also provides a method for preparing the power switch device structure described above, which specifically includes:
[0080] Step S1: providing a semiconductor substrate 11;
[0081] Step S2: forming a first conductive type drift region 12 on the semiconductor substrate 11;
[0082] Step S3: forming a trench structure in the first conductive type drift region 12;
[0083] Step S4: forming at least two polysilicon layers 15 and an isolation oxide layer 16 spaced apart in a direction perpendicular to the semiconductor substrate 11 in the trench structure, wherein the isolation oxide layer 16 is located between adjacent polysilicon layers 15, between the bottom polysilicon layer 15 and the bottom surface of the trench structure, and on the sidewalls of the trench structure;
[0084] Step S5 : forming a source metal layer 131 on the polysilicon layer, and forming a drain metal layer 132 on the lower surface of the semiconductor substrate 11 .
[0085] In step S1 , the semiconductor substrate 11 is preferably a heavily doped semiconductor substrate of the first conductivity type, such as a heavily doped n-type semiconductor substrate.
[0086] In step S2, epitaxial growth is performed on the semiconductor substrate 11 to form a first conductivity type drift region 12. The first conductivity type drift region 12 is, for example, an n-type drift region.
[0087] In step S3 , reactive ion etching is performed using a mask to form a trench structure in the first conductive type drift region 12 .
[0088] In step S4, an isolation oxide layer is grown on the bottom surface of the trench structure by thermal oxidation or CVD process, and then a highly doped n-type polysilicon layer is used as a trench electrode to fill the trench structure; another isolation oxide layer is grown on the polysilicon layer; and then the trench structure is filled with a highly doped n-type polysilicon layer again until all polysilicon layers are formed, and the last polysilicon layer is connected to the source metal layer 131. In this embodiment, when each isolation oxide layer is grown, the isolation oxide layer will also cover the side wall of the trench structure, and after each time the highly doped n-type polysilicon layer is used as a trench electrode to fill the trench structure, a portion of the polysilicon layer needs to be removed so that the thickness of the polysilicon layer formed each time can meet the corresponding potential requirements. Each time a portion of the polysilicon layer is removed, a portion of the isolation oxide layer on the side wall of the trench structure will also be removed, so that the isolation oxide layer on the side wall of the trench structure is flush with the top of the polysilicon layer.
[0089] In step S5 , a source metal layer 131 is formed on the polysilicon layer 15 , and a drain metal layer 132 is formed on a surface of the semiconductor substrate 11 away from the first conductive type drift region 12 .
[0090] When the power switch device structure is a charge coupling structure with a two-dimensional electric field, after step S2 , the preparation method may further include: forming a Schottky contact structure 14 or a second conductivity type doped region on the first conductivity type drift region 12 .
[0091] When the power switching device structure is an edge terminal structure, in step S4, while growing the isolation oxide layer 16 in the trench structure using a thermal oxidation or CVD process, a top oxide layer 17 is also formed on the first conductive type drift region 12; and in step S5, while forming a source metal layer 131 on the polysilicon layer 15, the source metal layer 131 also extends to a portion of the top oxide layer 17.
[0092] Figure 6A specific embodiment of the power device described above being applied to a vertical MOSFET is shown, a trench MOSFET structure combining electrode segmentation with a vertical MOSFET, that is, an example of the application of a vertical power MOSFET with a blocking voltage of 400V having two polysilicon layers in the trench. The device structure of this embodiment includes: a drain metal layer 232; a semiconductor substrate 21, located on the drain metal layer 232; an n-type drift region 22, located on the semiconductor substrate 21; a trench structure, located in the n-type drift region 22; two polysilicon layers, namely a first polysilicon layer 251 and a second polysilicon layer 252, spaced apart in the trench structure along a direction perpendicular to the semiconductor substrate 21; an isolation oxide layer 26, located between the first polysilicon layer 251 and the second polysilicon layer 252, between the first polysilicon layer 251 and the bottom surface of the trench structure and on the sidewall of the trench structure, and the potential difference between the first polysilicon layer 251 and the second polysilicon layer 252 is equal to the potential difference between the first polysilicon layer 251 and the bottom surface of the trench structure, both of which are 200V; a source metal layer 231, electrically connected to the second polysilicon layer 252. The device structure of this embodiment may also include: a gate electrode 210, a gate oxide layer 29 and a dielectric layer 27, wherein the gate electrode 210 is isolated from the second polysilicon layer 252 by the gate oxide layer 29, and the dielectric layer 27 is located between the gate electrode 210 and the source metal layer 231, and the material of the gate electrode 210 is preferably the same as that of the polysilicon layer. The material of the dielectric layer 27 and the gate oxide layer 29 is preferably silicon oxide, but is not limited thereto. The thickness of the gate electrode 210, the dielectric layer 27 and the gate oxide layer 29 may adopt the thickness of the gate electrode 210, the dielectric layer 27 and the gate oxide layer 29 of the power switch device structure in the prior art, which will not be described in detail here.
[0093] The device structure of this embodiment may further include a p-type body region 24 (i.e., a second conductive type doped region) and an n-type source region 28 (i.e., a first conductive type source region), and the p-type body region 24 is located on the n-type drift region 22 on both sides of the gate electrode 210, the n-type source region 28 is located on the p-type body region 24 on both sides of the gate electrode 210 and is adjacent to the gate electrode 210, and the source metal layer 231 sequentially covers the p-type body region 24, the n-type source region 28, the dielectric layer 27, the n-type source region 28 and the p-type body region 24 along a direction parallel to the semiconductor substrate 21 (upper surface).
[0094] After the step of growing the n-type drift region 22 on the semiconductor substrate 21, Figure 6The method for preparing the device structure in the embodiment of the present invention further requires the following steps: forming a p-type body region 24 on the active region (n-type drift region 22) of the device by implanting boron ions, and then generating an n-type source region 28 by implanting phosphorus ions and then performing an annealing process. A mask needs to be set during the ion implantation of the n-type source region 28. Figure 6 In the method for preparing the device structure in the embodiment, in the step of forming two polysilicon layers spaced apart in a direction perpendicular to the semiconductor substrate 21 and an isolation oxide layer 26, a gate oxide layer 29 located on the second polysilicon layer 252, a gate electrode 210 located on the gate oxide layer 29, and a dielectric layer 27 are also formed, and the dielectric layer 27 is used for isolation between the gate electrode and the source metal layer in the trench. That is, an additional polysilicon layer is deposited and flattened to be used as a gate electrode, and then an intermetallic dielectric is deposited to form the dielectric layer 27, and contact windows of the n-type source region and the p-type body region are etched, and finally the device manufacturing is completed by depositing and patterning the source metal layer.
[0095] Figure 7 It is a specific embodiment of the application of the power switch device structure in an edge terminal structure MOSFET, that is, an example of the application of an edge terminal structure MOSFET with a blocking voltage of 400V having two polysilicon layers in a trench. The structure of this embodiment includes: a drain metal layer 332; a semiconductor substrate 31, located on the drain metal layer 332; an n-type drift region 32, located on the semiconductor substrate 31; a trench structure, located in the n-type drift region 32; two polysilicon layers, namely a first polysilicon layer 351 and a second polysilicon layer 352, spaced apart in the trench structure along a direction perpendicular to the semiconductor substrate 31; an isolation oxide layer 36, located between the first polysilicon layer 351 and the second polysilicon layer 352, between the first polysilicon layer 351 and the bottom surface of the trench structure and on the sidewall of the trench structure, and the potential difference between the first polysilicon layer 351 and the second polysilicon layer 352 is equal to the potential difference between the first polysilicon layer 351 and the bottom surface of the trench structure, both of which are 200V; a source metal layer 331, electrically connected to the second polysilicon layer 352. Figure 7 The device structure may further include: a top oxide layer 37 on the n-type drift region 32 on one side of the polysilicon layer, and the top oxide layer 37 is connected to the isolation oxide layer 36 . Figure 7The device structure also includes a p-type body region 34 and an n-type source region 38, and the p-type body region 34 is located on the n-type drift region 32 on the side of the polysilicon layer away from the top oxide layer 37, the n-type source region 38 is located on the p-type body region 34 and away from the polysilicon layer, and the source metal layer 331 sequentially covers the n-type source region 38, the p-type body region 34, the second polysilicon layer 352 and part of the top oxide layer 37 along a direction parallel to the semiconductor substrate 31. The material of the top oxide layer 37 is preferably silicon dioxide, but is not limited thereto. The thickness of the top oxide layer 37 can adopt the thickness of the top oxide layer of the power switch device structure in the prior art, which will not be repeated here.
[0096] Figure 7 In the method for preparing the device structure, in the step of forming the isolation oxide layer 36 in the trench structure, a top oxide layer 37 is also formed on the n-type drift region 32 on one side of the polysilicon layer, and the top oxide layer 37 is connected to the isolation oxide layer 36. After the step of forming the n-type drift region 32 on the semiconductor substrate 31, the preparation method may further include: injecting p-type doping ions (such as boron) into the n-type drift region 32 on the side of the polysilicon layer away from the top oxide layer 37 to form a p-type body region 34; and injecting n-type doping ions (such as phosphorus) into the p-type body region 34 to form an n-type source region 38 away from the polysilicon layer. Figure 6 Compared with the preparation method of the device structure in Figure 7 The method for preparing the device structure in the embodiment of the present invention additionally grows a top oxide layer 37 on the surface of the n-type drift region 32, and does not require a gate electrode to be provided in the trench structure. In addition, the p-type body region 34 does not need to be provided on the right side of the trench structure (i.e., where the top oxide layer is provided), and the source metal layer 331 is extended to cover a portion of the top oxide layer 37 on the right side of the trench structure to improve the shielding of the electric field, thereby further avoiding a reduction in the breakdown voltage on the surface.
[0097] Due to the excessive stress between the isolation oxide layer and the first conductive type drift region and the increase in specific on-resistance, the prior art of increasing the blocking voltage by two-dimensional field generation of a vertical MOSFET with a trench electrode cannot be applied to a high blocking voltage. However, at least two polysilicon layers are provided on the bottom surface of the trench structure, so that it is possible to reduce the thickness of the isolation oxide layer on the sidewall and the bottom surface of the trench structure, while the effect of generating a two-dimensional field in the first conductive type drift region for increasing the blocking voltage is the same as that of the prior art.
[0098] By using the method for preparing the power switch device structure of the utility model, the application of different high blocking voltages can be realized by setting multiple polysilicon layers with fewer manufacturing processes. The segmentation in the vertical direction is combined with the current in the vertical direction from the source metal layer to the drain metal layer to obtain the best current density and better on-resistance. Similarly, the edge terminal structure of the utility model also provides the best breakdown voltage with better compactness and fewer process steps.
[0099] In addition, it is understood that although the present invention has been disclosed as a preferred embodiment, the above embodiment is not intended to limit the present invention. For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiment based on the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the scope of protection of the technical solution of the present invention.
[0100] It should also be understood that the utility model is not limited to the specific methods, compounds, materials, manufacturing techniques, usages and applications described herein, which can vary. It should also be understood that the terms described herein are only used to describe specific embodiments, rather than to limit the scope of the utility model. It must be noted that the singular forms "one", "a kind" and "the" used herein and in the appended claims include plural references unless the context clearly indicates the opposite meaning. Therefore, for example, a reference to "a step" means a reference to one or more steps, and may include secondary steps. All conjunctions used should be understood in the broadest sense. Therefore, the word "or" should be understood to have a logical "or" definition, rather than a logical "exclusive or" definition, unless the context clearly indicates the opposite meaning. The structure described here will be understood to also quote the functional equivalent of the structure. Language that can be interpreted as approximate should be understood that way unless the context clearly indicates the opposite meaning.
Claims
1. A power switch device structure, characterized in that: include: Drain metal layer; A semiconductor substrate, located on the drain metal layer; A first conductive type drift region, located on the semiconductor substrate; A trench structure located in the first conductive type drift region; At least two polysilicon layers are spaced apart and arranged in the trench structure along a direction perpendicular to the semiconductor substrate; An isolation oxide layer, located between adjacent polysilicon layers, between the bottom polysilicon layer and the bottom surface of the trench structure, and on the sidewalls of the trench structure; The source metal layer is located on the polysilicon layer.
2. The power switch device structure according to claim 1, characterized in that: The blocking voltage of the power switch device structure is equal to the sum of the potential difference between all two adjacent polysilicon layers and the potential difference between the bottom polysilicon layer and the bottom surface of the trench structure.
3. The power switch device structure according to claim 2, characterized in that: The potential difference between the two adjacent polysilicon layers is obtained according to the thickness of the isolation oxide layer between the two adjacent polysilicon layers, and the potential difference between the bottom polysilicon layer and the bottom surface of the trench structure is obtained according to the thickness of the isolation oxide layer between the bottom polysilicon layer and the bottom surface of the trench structure, and when the thickness of the isolation oxide layer between the two adjacent polysilicon layers is equal to the thickness of the isolation oxide layer between the bottom polysilicon layer and the bottom surface of the trench structure, the corresponding potential differences are the same.
4. The power switch device structure according to claim 1, characterized in that: The power switch device structure further includes a Schottky contact structure or a second conductivity type doping region located on the first conductivity type drift region.
5. The power switch device structure according to claim 4, characterized in that: When the power switching device structure includes a second conductive type doped region, the power switching device structure also includes a first conductive type source region located on the second conductive type doped region and a gate oxide layer, a gate electrode and a dielectric layer located sequentially between the polysilicon layer at the top of the trench structure and the source metal layer.
6. The power switch device structure according to claim 4, characterized in that: The first conductivity type is n-type, and the second conductivity type is p-type; or, the first conductivity type is p-type, and the second conductivity type is n-type.
7. The power switch device structure according to claim 1, characterized in that: The power switch device structure further includes a top oxide layer located on the first conductive type drift region, the top oxide layer is connected to the isolation oxide layer, and the source metal layer extends onto a portion of the top oxide layer.