Semiconductor power device with wide safe working area
By designing the gate oxide layer thickness in different regions in semiconductor power devices, the threshold voltage difference in different regions is achieved, the device thermal instability problem is solved, the safe working area is expanded and the heat dissipation capability is improved.
Patent Information
- Application Number
- CN202420605643.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-27
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-03-27
AI Technical Summary
As the cell density of semiconductor devices increases, heat concentration leads to thermal instability of the device, and a turning point appears, limiting the expansion of power consumption and safe working area.
By designing different gate oxide layers in different regions in semiconductor power devices, the threshold voltage difference in different regions is achieved, so that some regions do not turn on under low current conditions, thereby reducing the zero temperature coefficient and expanding the safe working area.
It effectively improves the thermal stability and heat dissipation ability of the device, expands the safe working area, and reduces the current and voltage values in the positive temperature coefficient area.
Smart Images

Figure CN222088613U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of semiconductors, and in particular relates to a semiconductor power device with a wide safe operating area. Background Art
[0002] With the development of MOSFET (Metal-Oxide-semiconductor Field-effect Transistor) technology, it has gradually evolved from Planar MOS to Trench MOS, and the process has been continuously reduced. As the size of the Pitch continues to shrink, the cell density has greatly increased.
[0003] In the structure of traditional SGT or typical trench semiconductor devices, as the cell density increases, the current is more concentrated. Under the same package, the heat of products with smaller pitch is more likely to be concentrated in one place, which will then cause the device to burn out. In actual work, the power consumption limit line in the SOA curve will also have an inflection point due to the thermal instability of the device, which is related to the zero temperature coefficient point of the device.
[0004] Therefore, how to enhance the heat dissipation capability of the device and improve the thermal stability of the device is an urgent problem to be solved. Utility Model Content
[0005] In view of this, the purpose of the utility model is to make the threshold voltages of different positions of the cell different, and to combine the cells according to actual scenarios and needs, so that when the gate-source voltage is small during the use of the device, some areas can be selected not to be turned on. At this time, the current of the device itself is not large, and the work can be completed by turning on some areas. The design of not turning on some areas and turning on some areas first can reduce the zero temperature coefficient (ZTC) of the device. The lower ZTC voltage and current values reduce the positive temperature coefficient area of the device's operation, thereby improving the thermal stability of the device and obtaining a wider safe operating area (SOA).
[0006] To achieve the above object, the utility model provides a method for manufacturing a semiconductor power device with a wide safe operating area, comprising: providing an epitaxial layer, and forming a barrier layer on the epitaxial layer;
[0007] Etching the epitaxial layer and the barrier layer to form a groove;
[0008] forming a first isolation layer, a second isolation layer and a third isolation layer in sequence inside the trench;
[0009] Depositing polysilicon inside the trench and etching back to form source polysilicon;
[0010] forming an isolation oxide layer on the source polysilicon;
[0011] removing the third isolation layer;
[0012] Providing a mask layer, wherein the mask layer covers the first area and does not cover the second area;
[0013] removing the second isolation layer in the second region;
[0014] removing the mask layer;
[0015] Depositing polysilicon inside the trench and etching back to form gate polysilicon;
[0016] Ion implantation is performed separately to form source region and body region.
[0017] Preferably, the first isolation layer includes a silicon oxide layer, the third isolation layer includes a silicon oxide layer, and the second isolation layer includes a silicon nitride layer.
[0018] Preferably, the mask layer is photoresist.
[0019] Another aspect of the utility model provides a semiconductor power device with a wide safe operating area, which is manufactured by the above manufacturing method.
[0020] On the other hand, the utility model provides a semiconductor power device with a wide safe operating area, comprising an epitaxial layer, wherein a first trench and a second trench are arranged in the epitaxial layer; a source polysilicon is arranged at the bottom of the first trench, a third isolation layer, a second isolation layer and a first isolation layer are arranged in sequence on the outer side of the source polysilicon, an isolation oxide layer and a first gate polysilicon are arranged in sequence on the upper end of the source polysilicon, a first gate oxide layer is arranged on the outer side of the first gate polysilicon, and the first gate oxide layer includes a first isolation layer and a second isolation layer;
[0021] A source polysilicon is arranged at the bottom of the second trench, a third isolation layer, a second isolation layer and a first isolation layer are arranged in sequence on the outside of the source polysilicon, an isolation oxide layer and a second gate polysilicon are arranged in sequence on the upper end of the source polysilicon, a second gate oxide layer is arranged on the outside of the second gate polysilicon, and the second gate oxide layer includes the first isolation layer.
[0022] The beneficial effects of the utility model are:
[0023] The utility model comprises a first gate oxide layer in a first groove including a first nitride layer and a first oxide layer, and a second gate oxide layer in a second groove including a first oxide layer, so that the thickness of the first gate oxide layer is greater than that of the second gate oxide layer, and after P+ and N+ injection, the threshold voltage of the region of the thicker first gate oxide layer is higher, and the threshold voltage of the region of the thinner second gate oxide layer is lower, thereby achieving different gate oxide layer thicknesses in different regions of the same device, resulting in different cell threshold voltages in different regions, successfully reducing the zero temperature coefficient point of the device, improving the thermal failure of MOS, and enabling the MOS device to have a wider safe operating area (SOA). BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0025] Figures 1 to 11 A schematic diagram of a manufacturing method according to an embodiment of the present utility model;
[0026] Fig.12 The present invention is a schematic structural diagram of a semiconductor power device according to an embodiment of the present invention. DETAILED DESCRIPTION
[0027] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0028] Figures 1 to 11 A schematic diagram of the manufacturing method of this embodiment is shown. This embodiment provides a method for manufacturing a semiconductor power device with a wide safe operating area, including:
[0029] A substrate 1 and an epitaxial layer 2 are provided. The epitaxial layer 2 is disposed on the substrate 1. A barrier layer 3 is formed on the epitaxial layer 2. Figure 1 As shown;
[0030] Dry etching is performed on the epitaxial layer 2 and the barrier layer 3 to form a trench 4, such as Figure 2 As shown;
[0031] A first isolation layer 51, a second isolation layer 52 and a third isolation layer 53 are sequentially formed inside the trench 4. The first isolation layer 51, the second isolation layer 52 and the third isolation layer 53 are sequentially arranged from the inside to the outside. Figure 3 As shown;
[0032] Polysilicon is deposited inside the trench 4 and etched back to form source polysilicon 6. Figure 4 As shown;
[0033] An isolation oxide layer 7 is formed on the source polysilicon 6 by thermal oxidation, such as Figure 5 As shown; because an oxide layer is grown from the third isolation layer 53 by thermal oxidation above the source polysilicon 6 to form the isolation oxide layer 7, the material of the isolation oxide layer 7 is the same as that of the third isolation layer 53, so the thickness of the isolation oxide layer 7 formed in this step needs to be thicker so that too much of the isolation oxide layer 7 will not be removed in the next wet etching;
[0034] The third isolation layer 53 is removed by wet etching. Figure 6 As shown, at this time, because the isolation oxide layer 7 and the third isolation layer 53 are made of the same material, part of the isolation oxide layer 7 is also removed;
[0035] The second isolation layer 52 in the second region is removed, so that the isolation oxide layer 7 in the second region only includes the first isolation layer 51, and the isolation oxide layer 7 in the first region includes the first isolation layer 51 and the second isolation layer 52. Figure 7 As shown; at this time, the thickness of the isolation layer in the second region is thinner than the thickness of the isolation layer in the first region;
[0036] Fig. 8A and Figure 8B Shows Figure 7 The specific process of the steps, such as Fig. 8A As shown, in the figure, a region a (ie, the first region) is firstly provided with a mask layer 11, and the region filled by the mask layer 11 includes the trench 4 located in the region a and the upper surface of the second isolation layer 52;
[0037] Then wet etching is performed, such as Figure 8B As shown, at this time, since the silicon nitride layer in region a is protected by the mask layer 11, this step only removes the second isolation layer 52 located in region b (ie, the second region);
[0038] Then the mask layer 11 in area a is removed, as shown in FIG. Figure 7 As shown, the region a includes the first isolation layer 51 and the second isolation layer 52, while the region b includes only the first isolation layer 51. Preferably, this step can be completed by using a photolithography process, that is, the mask layer 11 uses photoresist.
[0039] Polysilicon is deposited inside the trench 4 and etched back to form a gate polysilicon 8. At this time, the first isolation layer 51 and the second isolation layer 52 in the first region form a first gate oxide layer, and the first isolation layer 51 in the second region forms a second gate oxide layer. Figures 9 and 10 As shown; after the second isolation layer 52 in the second region is removed in the previous step, the thickness of the second gate oxide layer is the thickness of the first isolation layer 51 located in the second region. Similarly, the thickness of the first gate oxide layer is the sum of the thicknesses of the first isolation layer 51 and the second isolation layer 52 located in the first region.
[0040] Ion implantation is performed to form a semiconductor power device, and a body region 9 and a source region 10 are formed on the outer wall of the trench 4. Fig.11 As shown, the final thicker first gate oxide layer (such as Fig.11 The threshold voltage of the region (shown by x) is higher, and the second gate oxide layer with a thinner thickness (such as Fig.11 The threshold voltage of the area (shown as y in the figure) is lower.
[0041] The purpose of the utility model is to make different cell areas of the device have different isolation layers before filling the gate polysilicon 8, so that the thickness of the gate oxide layer after filling the gate polysilicon 8 is different, so that the threshold voltages at different positions of the cell are different (the area with thicker gate oxide layer corresponds to the high threshold voltage area, and the area with thinner gate oxide layer corresponds to the low threshold voltage area), so as to achieve asynchronous opening under small current conditions (when the gate-source voltage is small), some areas are turned on (areas with thin gate oxide layer), and some areas are not turned on (areas with thick gate oxide layer), so that the overall power density of the device is reduced, the heat dissipation capacity is enhanced, and the zero temperature coefficient point of the device is reduced at the same time.
[0042] As a specific example, the first isolation layer 51 includes a silicon oxide layer, the third isolation layer 53 includes a silicon oxide layer, and the second isolation layer 52 includes a silicon nitride layer. The first isolation layer 51 is formed by thermal oxidation, and the second isolation layer 52 and the third isolation layer 53 are formed by deposition, respectively.
[0043] like Fig.12 As shown, on the other hand, the present embodiment provides a semiconductor power device, including an epitaxial layer 2, wherein a first trench 41 and a second trench 42 are provided in the epitaxial layer 2; a source polysilicon 6 is provided at the bottom of the first trench 41, a third isolation layer 53, a second isolation layer 52 and a first isolation layer 51 are sequentially provided on the outer side of the source polysilicon, an isolation oxide layer 7 and a first gate polysilicon 81 are sequentially provided on the upper end of the source polysilicon 6, a first gate oxide layer is provided on the outer side of the first gate polysilicon 81, and the first gate oxide layer includes a first isolation layer 51 and a second isolation layer 52;
[0044] A source polysilicon 6 is arranged at the bottom of the second trench 42, and a third isolation layer 53, a second isolation layer 52 and a first isolation layer 51 are arranged in sequence on the outside of the source polysilicon 6. An isolation oxide layer 7 and a second gate polysilicon 82 are arranged in sequence on the upper end of the source polysilicon 6, and a second gate oxide layer is arranged on the outside of the second gate polysilicon 82, and the second gate oxide layer includes the first isolation layer 51.
[0045] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0046] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A semiconductor power device with a wide safe operating area, It is characterized in that The invention comprises an epitaxial layer, wherein a first trench and a second trench are arranged in the epitaxial layer; a source polysilicon is arranged at the bottom of the first trench, a third isolation layer, a second isolation layer and a first isolation layer are arranged in sequence on the outer side of the source polysilicon, an isolation oxide layer and a first gate polysilicon are arranged in sequence on the upper end of the source polysilicon, a first gate oxide layer is arranged on the outer side of the first gate polysilicon, and the first gate oxide layer comprises a first isolation layer and a second isolation layer; A source polysilicon is arranged at the bottom of the second trench, a third isolation layer, a second isolation layer and a first isolation layer are arranged in sequence on the outside of the source polysilicon, an isolation oxide layer and a second gate polysilicon are arranged in sequence on the upper end of the source polysilicon, a second gate oxide layer is arranged on the outside of the second gate polysilicon, and the second gate oxide layer includes the first isolation layer.