Lead nail head and shaft type diode

By designing step-like storage areas and pre-welding processes on the lead nail head, the solder splashing problem is solved, the flux residue on the chip surface is reduced, and the welding quality and reliability of the shaft diode are improved.

CN222126510UActive Publication Date: 2024-12-06YANGZHOU YANGJIE ELECTRONIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323389061.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-13
Publication Date
2024-12-06
Estimated Expiration
2033-12-13

AI Technical Summary

Technical Problem

During the welding process of shaft diodes, the internal heat energy after the solder liquefies cannot be released, causing solder to splash, affecting the reliability and service life of the device. Especially on the diode chips in planar structures, solder debris may cross the protection ring and cause current to occur. Increased density or leaves acid flux residues, reducing reliability.

Method used

Design a lead nail head with a step-shaped storage area. The chip is then soldered by pre-welding welding sheets. The welding is completed on the surface of the lead nail head by using the wetting effect of the solder layer to reduce the flux usage and residues, and use oxygen-free copper Nail head and lead-based tin alloy or lead-tin-silver alloy solder layer.

Benefits of technology

The pre-soldering process pre-injected the wetting process after the solder is liquefied in a chip-free step to ensure that the solder is completely infiltrated, reducing the residual solder on the chip surface, and improving solder quality and device reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222126510U_ABST
    Figure CN222126510U_ABST
Patent Text Reader

Abstract

The utility model discloses a lead nail head and a shaft type diode. Relates to the technical field of semiconductors. Comprising a connecting part which is of a circular truncated cone structure, and a step-shaped storage area is arranged at the front end of the connecting part; and the lead part is fixedly arranged at the tail end of the connecting part. And the lead part is fixedly arranged in the middle of the connecting part. And the cross section of the lead part is of a circular structure. The pair of nail heads are symmetrically arranged up and down; an upper solder layer, a chip and a lower solder layer are sequentially arranged between the pair of nail heads from bottom to top. The nail head is an oxygen-free copper nail head. According to the utility model, the welding flux and the lead nail head are completely infiltrated, and the metal silver on the surface of the chip has good weldability, so that the residual soldering flux on the surface of the chip can be reduced by reducing the consumption of the soldering flux.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of semiconductors, in particular to a lead nail head and an axial diode. Background Art

[0002] The welding process of axial diodes uses a graphite fixture to load the bottom mold lead-solder piece-chip-solder piece-upper mold lead in sequence, and then enter the tunnel furnace. After high temperature, the solder melts and liquefies, and infiltrates the surface of the lead nail head and the chip surface. After cooling and condensing, the purpose of welding is achieved.

[0003] After the solder is liquefied, the thermal motion of the internal atoms intensifies and expands. The liquefied solder infiltrates the surface of the lead pin head and the metal on the chip surface through capillary action. When the wetting process cannot release the internal heat energy of the solder after liquefaction, that is, when the solder infiltration is blocked, splashing will occur and splash on the chip surface. The splashing process is divided into natural splashing and back splashing after encountering the inner wall of the graphite boat.

[0004] The solder debris splashed onto the chip surface will not only cause direct device failure, but also affect the reliability of qualified devices after testing, especially planar diode chips.

[0005] When the splashed solder debris spreads on the edge of the surface silver layer and crosses the guard ring, it will cause failure due to the increase of current density after the local electric field is distorted.

[0006] When splashing on the edge of the surface silver layer, even if it does not cross the guard ring, it will cause a local increase in the concentration of acid flux residues at the boundary of the solder debris and migrate when the circuit is loaded, thereby reducing the reliability of the device and shortening its service life. Utility Model Content

[0007] In view of the above problems, the utility model provides a lead nail head and an axial diode which can reduce the amount of soldering flux used and the residue on the chip surface.

[0008] The technical solution of the utility model is:

[0009] A lead nail head, comprising:

[0010] The connecting part is a truncated cone structure, and a stepped storage area is provided at the front end;

[0011] The lead portion is fixedly arranged at the tail end of the connecting portion.

[0012] Specifically, the lead portion is fixedly arranged in the middle of the connecting portion.

[0013] Specifically, the cross section of the lead portion is a circular structure.

[0014] Specifically, the nail heads are provided with a pair, symmetrically arranged up and down;

[0015] An upper solder layer, a chip and a lower solder layer are arranged in sequence from bottom to top between a pair of nail heads.

[0016] Specifically, the nail head is an oxygen-free copper nail head.

[0017] Specifically, the upper solder layer is a first lead-based tin alloy solder layer or a first lead-tin-silver alloy solder layer.

[0018] Specifically, the lower solder layer is a second lead-based tin alloy solder layer or a second lead-tin-silver alloy solder layer.

[0019] Beneficial effects of the utility model:

[0020] The lead nail head adopts a two-step table design (step-shaped material storage area). Through the process of pre-soldering the solder piece on the lead and then soldering the chip, the "tin explosion" process caused by the obstruction of solder and the lead nail head surface infiltration is pre-placed in the pre-soldering process without the participation of the chip. When the lead and chip are welded after pre-soldering, the solder is liquefied and, under the wetting attraction of the metal on the chip surface, the solder pre-soldered to the surface of the lead nail head infiltrates into the chip surface to achieve the welding purpose. Under this process condition, the solder and the lead nail head have been completely infiltrated, and the metal silver on the chip surface has good solderability, so the amount of flux used and the residue of flux on the chip surface can be reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a schematic diagram of the structure of the lead nail head.

[0022] Figure 2 This is a schematic diagram of the structure when the solder piece is pre-welded on the surface of the lead nail head.

[0023] Figure 3 This is a schematic diagram of the chip and solder connection structure after pre-soldering.

[0024] Figure 4 This is a schematic diagram of the chip and solder connection structure after the secondary reflow process.

[0025] Figure 5 This is a schematic diagram of the product after welding using traditional welding methods;

[0026] In the figure, 100 is a lead nail head.

[0027] 110 is a connection part, 111 is a material storage area,

[0028] 120 is a lead portion,

[0029] 200 is the upper solder layer, 300 is the chip, and 400 is the lower solder layer. DETAILED DESCRIPTION

[0030] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0031] In the description of the present invention, it should be understood that the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0032] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0033] When using traditional welding methods, the solder pieces liquefy and then gather and shrink. The shrinkage direction is from the edge of the chip to the center (such as Figure 5 As shown in the four arrow directions in the figure), during the whole process, the metallic silver on the chip surface will come into contact with the liquefied solder and produce an alloy, so there will be solder infiltration at the edge of the metallic silver layer on the surface.

[0034] The following describes an embodiment of the utility model with reference to FIGS. 1-4 ;

[0035] A lead nail head 100, comprising:

[0036] The connecting portion 110 is a truncated cone structure, and a stepped material storage area 111 is provided at its front end to control the solder infiltration area of ​​the lead nail head 100 and keep the solder infiltration of the boss surface after pre-welding full.

[0037] The lead portion 120 is fixedly disposed at the tail end of the connecting portion 110 .

[0038] The lead portion 120 further defines:

[0039] The lead portion 120 is fixedly disposed in the middle of the connecting portion 110 .

[0040] The cross section of the lead portion 120 is a circular structure.

[0041] Axial diodes, including the nail head, are provided with a pair, symmetrically arranged up and down;

[0042] An upper solder layer 200 , a chip 300 and a lower solder layer 400 are sequentially arranged between the pair of nail heads from bottom to top.

[0043] It is further defined that the nail head is an oxygen-free copper nail head.

[0044] It is further defined that the upper solder layer 200 is a first lead-based tin alloy solder layer or a first lead-tin-silver alloy solder layer.

[0045] It is further defined that the lower solder layer 400 is a second lead-based tin alloy solder layer or a second lead-tin-silver alloy solder layer.

[0046] The processing method in this case is:

[0047] First, the solder sheet is pre-soldered on the surface of the lead pin head 100, and then assembled with the chip 300. After a secondary reflow process, the lead and the chip 300 are welded together; the furnace temperature selected during pre-welding is higher than that when welding the chip 300, so as to achieve the purpose of annealing the oxygen-free copper lead.

[0048] Using this new technology, the solder sheet is pre-soldered on the surface of the lead nail head. When the chip is soldered, the liquefied solder sheet infiltrates from the center of the chip to the surrounding areas (in the direction of the four arrows in the figure). Therefore, no alloy of solder and silver layer is produced in the area where the solder has not infiltrated. The wetting boundary where the flux residue is concentrated is far away from the chip passivation layer, reducing the impact of the flux residue on the material.

[0049] Regarding the contents disclosed in this case, there are a few points that need to be explained:

[0050] (1) The drawings of the embodiments disclosed in this case only involve the structures involved in the embodiments disclosed in this case. Other structures can refer to the general design;

[0051] (2) In the absence of conflict, the embodiments and features of the embodiments disclosed in this case may be combined with each other to obtain new embodiments;

[0052] The above are only specific implementation methods disclosed in this case, but the protection scope of the present disclosure is not limited thereto. The protection scope disclosed in this case should be based on the protection scope of the claims.

Claims

1. A lead nail head, characterized in that: include: The connecting part is a truncated cone structure, and a stepped storage area is provided at the front end; The lead portion is fixedly arranged at the tail end of the connecting portion.

2. A lead nail head according to claim 1, characterized in that: The lead portion is fixedly arranged in the middle of the connecting portion.

3. A lead nail head according to claim 1 or 2, characterized in that: The cross section of the lead portion is a circular structure.

4. An axial diode, comprising a lead nail head according to any one of claims 1 to 3, characterized in that: The nail heads are provided with a pair, symmetrically arranged up and down; An upper solder layer, a chip and a lower solder layer are arranged in sequence from bottom to top between a pair of nail heads.

5. The axial diode according to claim 4, characterized in that: The nail head is an oxygen-free copper nail head.

6. The axial diode according to claim 4, characterized in that: The upper solder layer is a first lead-based tin alloy solder layer or a first lead-tin-silver alloy solder layer.

7. The axial diode according to claim 4, characterized in that: The lower solder layer is a second lead-based tin alloy solder layer or a second lead-tin-silver alloy solder layer.