Demoulding mechanism in cake mould

By designing the mold release mechanism in the cake mold, and using the pressing ring to lightly press the bonded edge and thread connection, the problem of cumbersome demolding operation in the existing technology is solved, and rapid and convenient mold release is achieved, and the quality and efficiency of the cake is improved.

CN223142759UActive Publication Date: 2025-07-25卡尔顿(集团)有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202422274281.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-09-18
Publication Date
2025-07-25
Estimated Expiration
2034-09-18

AI Technical Summary

Technical Problem

The existing cake molds are cumbersome to operate during the demolding process, which affects the quality of the finished product and processing efficiency.

Method used

A mold release mechanism including an outer mold, an inner mold, a lower mold and a edge pressing mechanism is designed. The cake is slightly recessed by light pressure contacting the adhesive edge of the pressing ring, combining the threaded connection and a detachable structure to achieve convenient mold release.

Benefits of technology

A fast and convenient mold release process is achieved, which avoids the damage to the finished cake products by violent mold release, and improves the quality and processing efficiency of the cake.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN223142759U_ABST
    Figure CN223142759U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of cake making, in particular to a demoulding mechanism in a cake mould, which comprises an outer mould, an inner mould, a lower mould and an edge pressing mechanism. When the cake needs to be demoulded, the edge pressing ring is firstly descended to be in contact with the adhesion edge of the cake and the inner mould, then the edge pressing ring is slightly pressed downwards, so that the cake is slightly sunken downwards, the adhesion edge of the cake and the adhesion edge of the inner mould are separated, then the inner mould is rotated, the inner mould is pulled out from the outer mould, and the inner wall of the inner mould is separated from the side wall of the cake in the process; then, the lower mold is pulled out from the notch, the lower mold plate of the lower mold is separated from the bottom surface of the cake, and finally, the cake is poured out from the outer mold, so that the cake can be quickly demolded, the use is convenient, the influence of violent demolding on a cake finished product is greatly avoided, and the processing efficiency is further improved while the cake quality is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of cake making, in particular to a demoulding mechanism in a cake mold. Background Art

[0002] In the prior art, relevant molds are often needed for baking cakes to make cakes that meet requirements. The existing baking molds for cakes are often inconvenient for demoulding the processed cakes, and the operation is rather cumbersome, which is likely to affect the production quality and processing efficiency of the finished products. Content of the Utility Model

[0003] Aiming at the deficiencies mentioned in the above background art, the utility model provides a demoulding mechanism in a cake mold.

[0004] The utility model adopts the following technical scheme:

[0005] A demoulding mechanism in a cake mold, characterized by comprising:

[0006] An outer mold, on the upper surface of which there is a downwardly concave installation groove, and a notch is formed at the bottom edge of the installation groove;

[0007] An inner mold, on the bottom surface of which there is an upwardly concave accommodation groove, and an opening penetrates through the center of the bottom of the accommodation groove;

[0008] A lower mold, which includes a lower mold plate and a clamping part. The lower mold plate is adapted to the installation groove, and a clamping part is provided on the outer side wall of the lower mold plate, and the clamping part is adapted to the notch;

[0009] A pressing edge mechanism, which includes a pressing edge ring, and the pressing edge ring is arranged to lift in the accommodation groove;

[0010] Wherein, the lower mold is detachably connected to the outer mold. After the lower mold plate passes through the notch and is placed into the installation groove, the clamping part is embedded into the notch. The inner mold is detachably connected to the outer mold by threads. After the inner mold is placed into the outer mold, the inner mold is placed on the upper surface of the lower mold plate, and an accommodation space is formed between the inner mold and the lower mold plate. Cake raw materials are poured into the accommodation space through the opening.

[0011] As a further improvement, a convex first grip ring is provided on the outer side of the top of the outer mold, and a convex second grip ring is provided on the outer side of the top of the inner mold. After the inner mold is placed into the outer mold, there is a gap between the first grip ring and the second grip ring.

[0012] As a further improvement, the gap between the first grip ring and the second grip ring is greater than 3 cm.

[0013] As a further improvement, a handle is provided on the outer wall of the clamping portion, and the handle is used to operate the lower mold.

[0014] As a further improvement, the cross-section of the edge pressing ring is a semi-circular structure.

[0015] As a further improvement, threaded holes are symmetrically provided at the bottom of the accommodating groove, symmetric connecting rods are provided on the upper surface of the edge pressing ring, a connecting sleeve is sleeved outside the connecting rod, the connecting sleeve rotates outside the connecting rod, the connecting sleeve penetrates through the threaded hole in a liftable manner, and the bottom of the connecting sleeve is threadedly connected to the threaded hole.

[0016] As a further improvement, the connecting rod is composed of a guide rod, a limiting block and a screw. The connecting sleeve is sleeved outside the guide rod in a liftable manner, and a limiting block is fixed to the top of the guide rod by a screw. The diameter of the limiting block is larger than the diameter of the connecting sleeve.

[0017] As can be seen from the above description of the structure of the present invention, compared with the prior art, the present invention has the following advantages: When it is necessary to demold the cake, first lower the edge pressing ring to contact the adhesive edge between the cake and the inner mold, and then gently press down the edge pressing ring to make the cake slightly concave downward, separate the adhesive edge between the cake and the inner mold, then rotate the inner mold, pull out the inner mold from the outer mold. During the process, the inner wall of the inner mold is separated from the side wall of the cake, and then the lower mold is pulled out from the notch to separate the lower template of the lower mold from the bottom surface of the cake. Finally, pour the cake out of the outer mold, and the demolding of the cake can be quickly completed. It is convenient to use, greatly avoids the influence of violent demolding on the finished cake, improves the quality of the cake and further improves the processing efficiency at the same time. Description of the Drawings

[0018] Figure 1 It is a three-dimensional structural schematic diagram of the present invention.

[0019] Figure 2 It is a sectional structural schematic diagram of the present invention.

[0020] Figure 3 It is a three-dimensional structural schematic diagram of the outer mold.

[0021] Figure 4 It is a three-dimensional structural schematic diagram of the inner mold.

[0022] Figure 5 It is a three-dimensional structural schematic diagram of the lower mold.

[0023] Figure 6 It is a three-dimensional structural schematic diagram of the edge pressing mechanism.

[0024] Figure 7 It is an exploded structural schematic diagram of the edge pressing mechanism.

[0025] Figure 8 Schematic cross-sectional structure diagram when demolding a cake. Specific embodiments

[0026] The following will describe the specific embodiments of the present utility model with reference to the accompanying drawings.

[0027] As shown in the attached Figure 1 figure, a demolding mechanism in a cake mold includes an outer mold 1, an inner mold 2, a lower mold 3, and a pressing edge mechanism 4.

[0028] As shown in the attached Figures 2 to 5 , and Figure 8 figure, the upper surface of the outer mold 1 is provided with a downwardly concave installation groove 11. A notch 12 is opened at the bottom edge of the installation groove 11. The lower mold 3 is detachably provided at the notch 12. The lower mold 3 includes a lower template 31 and a clamping portion 32. The lower template 31 is adapted to the installation groove 11. The outer side wall of the lower template 31 is provided with a clamping portion 32 adapted to the notch 12. And the inner mold 2 is detachably provided in the installation groove 11 of the outer mold 1. The inner mold 2 and the outer mold 1 are detachably connected by threads. Specifically, internal threads 13 are provided on the groove wall of the installation groove 11, and external threads 23 are provided on the outer wall of the inner mold 2. In the assembled outer mold 1 and inner mold 2, the internal threads 13 and the external threads 23 are screwed together. And the bottom surface of the inner mold 2 is provided with an upwardly concave accommodating groove 21. An opening 22 penetrates through the center of the bottom of the accommodating groove 21. During use, the lower template 31 is inserted into the installation groove 11 through the notch 12. At this time, the clamping portion 32 is embedded in the notch 12. Then the inner mold 2 is inserted into the outer mold 1, and the inner mold 2 and the outer mold 1 are screwed and fixed until the inner mold 2 is placed on the upper surface of the lower template 31. At this time, the inner mold 2 and the lower template 31 form an accommodating space. The cake raw material is poured into this accommodating space through the opening 22 for baking. When it is necessary to demold the cake, the inner mold 2 can be rotated to separate the internal threads 13 from the external threads 23, separate the inner mold 2 from the outer mold 1. During the process, the inner wall of the inner mold 2 is separated from the side wall of the cake. Then the inner mold 2 is lifted upward and the inner mold 2 is pulled out. Then the lower mold 3 is pulled out from the notch 12 to separate the lower template 31 of the lower mold 3 from the bottom surface of the cake. Finally, the cake is poured out from the outer mold 1, and the demolding of the cake can be quickly completed. It is convenient to use, greatly avoiding the influence of violent demolding on the cake finished product, improving the cake quality while further improving the processing efficiency.

[0029] Furthermore, as shown in the attached Figures 2 to 4As shown, a protruding first grip ring 14 is provided on the outer side of the top of the outer mold 1, and a protruding second grip ring 24 is provided on the outer side of the top of the inner mold 2. After the inner mold 2 is placed into the outer mold 1, there is a gap of more than 3 centimeters between the first grip ring 14 and the second grip ring 24. This gap can provide space for the fingers to grip the first grip ring 14 and the second grip ring 24, and gripping the first grip ring 14 and the second grip ring 24 can quickly fix or rotate the outer mold 1 and the inner mold 2, facilitating the disassembly and assembly of the outer mold 1 and the inner mold 2. And a handle 33 is provided on the outer wall of the clamping portion 32, and this handle 33 is used to operate the lower mold 3 to facilitate the disassembly and assembly of the lower mold 3.

[0030] It is worth mentioning that, as shown in the attached Figure 4 , Figure 6 , Figure 7 and Figure 8 As shown, a hemming mechanism 4 is provided in the accommodation groove 21 of the inner mold 2. The hemming mechanism 4 includes a hemming ring 41. The hemming ring 41 is arranged to lift and lower in the accommodation groove 21. Specifically, threaded holes 25 are symmetrically provided at the bottom of the accommodation groove 21. Symmetric connecting rods 42 are provided on the upper surface of the hemming ring 41. A connecting sleeve 43 is sleeved outside the connecting rod 42. The connecting sleeve 43 rotates outside the connecting rod 42. The connecting sleeve 43 can lift and lower through the threaded hole 25, and the bottom of the connecting sleeve 43 is threadedly connected to the threaded hole 25. When pouring cake raw materials into the inner mold 2 through the opening 22 for baking, the connecting sleeve 43 is screwed with the threaded hole 25 so that the hemming ring 41 is suspended at the top of the accommodation groove 21, away from the cake. When the cake needs to be demolded, first rotate the connecting sleeve 43 to separate the connecting sleeve 43 from the threaded hole 25. At this time, the connecting sleeve 43 can drive the hemming ring 41 to move downward along the threaded hole 25 until the hemming ring 41 contacts the adhesion edge of the cake and the inner mold 2. Then gently press down the hemming ring 41 to make the cake slightly concave downward, separating the adhesion edge of the cake and the inner mold 2. While facilitating the subsequent quick demolding of the cake, it can effectively ensure the smoothness and flatness of the side of the cake, reducing the breakage rate of the cake. During the process, because the cake has a certain elasticity, gently pressing the cake will not cause the cake to break. In addition, since the cross-section of the hemming ring 41 is a semi-circular structure, the risk of the hemming ring 41 pressing the cake and causing breakage can be reduced.

[0031] Among them, as shown in the attached Figure 6 and Figure 7 As shown, the connecting rod 42 is composed of a guide rod 421, a limit block 422 and a screw 423. The connecting sleeve 43 can lift and lower and is sleeved outside the guide rod 421. The top of the guide rod 421 is fixed with a limit block 422 through a screw 423. The diameter of the limit block 422 is larger than the diameter of the connecting sleeve 43. The setting of the limit block 422 enables the connecting sleeve 43 to lift and lower outside the guide rod 421 without detaching from the guide rod 421, facilitating the use of the connecting sleeve 43 and the hemming ring 41.

[0032] In summary, when the present utility model is in use, the lower template 31 is inserted into the installation groove 11 through the notch 12. At this time, the clamping portion 32 is embedded into the notch 12. Then, the inner mold 2 is placed into the outer mold 1 until the inner mold 2 is located on the upper surface of the lower template 31. At this time, the inner mold 2 and the lower template 31 form a receiving space, and the cake raw materials are poured into this receiving space through the opening 22 for baking. During the process, the pressing edge ring 41 is always suspended at the top of the receiving groove 21, away from the cake. When the cake needs to be demolded, first lower the pressing edge ring 41 to contact the adhesive edge between the cake and the inner mold 2, and then gently press the pressing edge ring 41 downward to make the cake slightly concave downward, separating the adhesive edge between the cake and the inner mold 2. Then rotate the inner mold 2 and pull the inner mold 2 out of the outer mold 1. During the process, the inner wall of the inner mold 2 is separated from the side wall of the cake. Then, pull the lower mold 3 out of the notch 12 to separate the lower template 31 of the lower mold 3 from the bottom surface of the cake. Finally, pour the cake out of the outer mold 1 to quickly complete the demolding of the cake. It is convenient to use, greatly avoiding the influence of violent demolding on the finished cake, improving the cake quality and further enhancing the processing efficiency at the same time.

[0033] The above is only the specific embodiment of the present utility model, but the design concept of the present utility model is not limited thereto. Any non-substantive modification made to the present utility model using this concept shall fall within the scope of infringement of the protection scope of the present utility model.

Claims

1. A demolding mechanism in a cake mold, characterized in that, Including: An outer mold, on the upper surface of which there is a downwardly concave mounting groove, and a notch is formed at the bottom edge of the mounting groove; An inner mold, on the bottom surface of which there is an upwardly concave accommodating groove, and an opening penetrates through the center of the bottom of the accommodating groove; A lower mold, which includes a lower template and a clamping portion. The lower template is adapted to the mounting groove, and a clamping portion is provided on the outer side wall of the lower template, and the clamping portion is adapted to the notch; A hemming mechanism, which includes a hemming ring, and the hemming ring is arranged to lift and lower in the accommodating groove; Among them, the lower mold and the outer mold are detachably connected. After the lower template passes through the notch and is placed in the mounting groove, the clamping portion is embedded in the notch. The inner mold and the outer mold are detachably connected by threads. After the inner mold is placed in the outer mold, the inner mold is placed on the upper surface of the lower template, and the inner mold and the lower template form an accommodating space, and the cake raw materials are poured into the accommodating space through the opening.

2. The demolding mechanism in a cake mold according to claim 1, wherein: A convex first grip ring is provided on the outer side of the top of the outer mold, and a convex second grip ring is provided on the outer side of the top of the inner mold. After the inner mold is placed in the outer mold, there is a gap between the first grip ring and the second grip ring.

3. The demolding mechanism in a cake mold according to claim 2, characterized in that: The gap between the first grip ring and the second grip ring is greater than 3 cm.

4. The demoulding mechanism in a cake mould according to claim 1, characterized in that: A handle is provided on the outer wall of the clamping portion, and the handle is used to operate the lower mold.

5. The demolding mechanism in a cake mold as described in claim 1, characterized in that: The cross-section of the hemming ring is a semi-circular structure.

6. The demoulding mechanism in a cake mould according to claim 5, characterized in that: Threaded holes are symmetrically provided at the bottom of the accommodating groove. Symmetric connecting rods are provided on the upper surface of the hemming ring. A connecting sleeve is sleeved on the outer side of the connecting rod. The connecting sleeve rotates on the outer side of the connecting rod, and the connecting sleeve can lift and lower through the threaded holes, and the bottom of the connecting sleeve is threadedly connected to the threaded holes.

7. The demoulding mechanism in a cake mold according to claim 6, characterized in that: The connecting rod is composed of a guide rod, a limiting block and a screw. The connecting sleeve can lift and lower and is sleeved on the outer side of the guide rod. The top of the guide rod is fixed with a limiting block by a screw, and the diameter of the limiting block is larger than the diameter of the connecting sleeve.