A Glauber's salt crystallization device

By etching the lattice structure on the surface of the microfiltration membrane and combining it with electrically driven membrane treatment, the problem of amorphous crystallization of Glauber's salt was solved, achieving crystallization results with high purity and high recovery rate.

CN224949657UActive Publication Date: 2026-11-10JIANDE LANXIN ENVIRONMENTAL SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522101792.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-09-29
Publication Date
2026-11-10
Estimated Expiration
2035-09-29

AI Technical Summary

Technical Problem

Existing microfiltration membranes cannot form a stable crystal structure during the crystallization process of Glauber's salt, resulting in amorphous crystals that affect the yield and quality of crystals.

Method used

A lattice structure is introduced on the surface of a microfiltration membrane. Using a 0.45-micron polypropylene microfiltration membrane as the base membrane, after treatment with a mixed solvent of n-butyl ketone and sulfolane, and combined with ultrafine nickel crystal particles as a template agent, a sunken shape is formed under microwave heating to etch out the lattice structure. Then, an electrically driven membrane is used for concentration treatment to achieve stable crystallization of Glauber's salt.

Benefits of technology

This improved the purity and recovery rate of Glauber's salt crystals, solved the amorphous problem, and achieved a highly efficient crystallization process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224949657U_ABST
    Figure CN224949657U_ABST
Patent Text Reader

Abstract

This utility model discloses a water treatment technology and equipment, specifically relating to a sodium sulfate crystallization device. The utility model includes a cooling component, a crystallization component, and a concentration component, connected sequentially. The cooling component is equipped with a sodium sulfate solution inlet and a refrigerant inlet, as well as a refrigerant outlet and a sodium sulfate coolant outlet, the latter connected to the crystallization component. A microfiltration membrane with a lattice structure is placed inside the crystallization component. The upper end of the crystallization component has a crystal discharge outlet and a crystallization mother liquor outlet, the latter connected to the concentration component. The concentration component has a dilute solution inlet and a concentrated solution inlet; its outlets include a dilute solution discharge outlet and a sodium sulfate concentrated solution circulation outlet connected to the sodium sulfate solution inlet. The advantages of this utility model are that it solves the amorphous problem in the sodium sulfate crystallization process and improves the recovery rate and purity in the treatment of sodium sulfate solution.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model belongs to the field of water treatment technology, specifically relating to a device with a Glauber's salt lattice structure containing a flat microfiltration membrane. Background Technology

[0002] The primary function of crystal lattice structure is to ensure the stability and uniformity of crystal formation and growth, playing a crucial role in the crystallization process. A crystal lattice structure is typically a geometric unit. An object with a specific crystal lattice structure can adsorb substances in solution, forming crystals of that lattice structure on its surface. When the solution is supersaturated, this substance can help molecules arrange themselves into a single structure, thus reducing the difficulty of crystallization. This not only makes the crystallization process easier but also ensures the uniformity and consistency of crystal growth, thereby improving crystal yield and quality. For example, some substances crystallize slowly under natural conditions; adding substances with a lattice structure on their surface can accelerate this process. In other cases, such as the crystallization of certain polymers, the presence of seed crystals is essential for forming perfect crystals.

[0003] Microfiltration membranes are classified into inorganic membranes and organic polymer membranes based on their membrane-forming materials. Inorganic membranes are further divided into ceramic membranes and metal membranes, while organic polymer membranes are divided into natural polymer membranes and synthetic polymer membranes. Based on membrane form, they are classified into flat sheet membranes, tubular membranes, spiral wound membranes, and hollow fiber membranes. According to the membrane-forming principle, polymer membrane preparation methods include dissolution methods (dry-wet methods), stretching pore-forming methods, phase inversion methods, thermally induced phase methods, dip-coating methods, irradiation methods, surface chemical modification methods, nuclear track methods, and kinetic formation methods. Inorganic membrane preparation methods mainly include sol-gel methods, sintering methods, and chemical precipitation methods. Filtration membranes are classified into four types based on micropore size: microfiltration membranes (MF), ultrafiltration membranes (UF), nanofiltration membranes (NF), and reverse osmosis membranes (RO). Microfiltration membranes generally refer to filtration membranes with pore sizes between 0.1 and 1 micrometer.

[0004] Regarding the mechanism of microfiltration, it was initially believed that the microfiltration process was essentially a simple mechanical sieving process. However, years of research have revealed that, in addition to mechanical sieving, two other factors determine the separation characteristics of the membrane: first, the interaction between the solute, solvent, and membrane material. These forces include van der Waals forces, electrostatic forces, and hydrogen bonding. The attraction or repulsion of solute molecules on the membrane surface or pore walls affects the membrane's separation efficiency; second, the average pore size and pore size distribution of the membrane influence its separation characteristics. After extensive experiments and electron microscopy observations, scholars such as Ye Lingbi concluded that the retention effects of microfiltration membranes can be broadly categorized into four types: ① mechanical retention; ② adsorption retention; ③ bridging retention; and ④ retention within the network of network-type membranes.

[0005] In addition, microfiltration generally operates in two modes: dead-end filtration and cross-flow filtration. For raw water with low turbidity and good quality, dead-end filtration is typically used, which significantly reduces energy consumption. For water with high turbidity and severe pollution, cross-flow filtration is used to prevent the accumulation of large amounts of contaminants on the membrane surface, thus avoiding membrane fouling and reduced filtration performance. Cross-flow filtration, also known as dynamic filtration, is superior because during microfiltration, the membrane surface is continuously subjected to the scouring and shearing action of the flowing solution, promptly washing away large molecular solutes accumulated on the membrane surface, preventing the formation of a concentration polarization layer, mitigating membrane fouling, and reducing the frequency of membrane cleaning.

[0006] Existing microfiltration membranes typically retain pollutants by using pores smaller than the pollutant diameter—a principle known as sieving. However, these membranes do not aid in the crystallization of sodium sulfate (Glauber's salt). This invention thoroughly analyzes the characteristics of sodium sulfate crystallization and finds that most sodium sulfate produced during freeze-crystallization fails to form a stable crystal structure; instead, it exhibits an amorphous structure, resulting in unstable crystals that cannot form a stable solid. By initiating the crystallization of supersaturated sodium sulfate in water onto the surface of the microfiltration membrane through a lattice structure and a chain reaction, a stable sodium sulfate structure can be formed. Summary of the Invention

[0007] This utility model addresses the shortcomings of existing technologies by proposing a solution that effectively solves the current problems. This utility model is achieved through the following technical solution: A sodium sulfate crystallization device includes a cooling component, a crystallization component, and a concentration component connected in sequence. The cooling component has a sodium sulfate solution inlet and a refrigerant inlet, as well as a refrigerant outlet and a sodium sulfate coolant outlet, the latter connected to the crystallization component. The crystallization component has a crystallization inlet connected to the sodium sulfate coolant outlet. A microfiltration membrane is placed inside the crystallization component; the microfiltration membrane is a polypropylene microfiltration membrane with a pore size of 0.45 micrometers, and is a flat sheet microfiltration membrane with a lattice structure on its surface. The upper end of the crystallization component has a crystal discharge outlet and a crystallization mother liquor outlet connected to the concentration component. The concentration component has a dilute inlet and a concentrated inlet; its outlet has a dilute discharge outlet and a sodium sulfate concentrated liquid circulation outlet connected to the sodium sulfate solution inlet. As a preferred embodiment, the microfiltration membrane in the aforementioned Glauber's salt crystallization apparatus uses a polypropylene microfiltration membrane with a pore size of 0.45 micrometers as the base membrane. The base membrane is treated with a mixture of n-butyl ketone and sulfolane as the surface treatment solvent for 2-5 hours. Then, ultrafine nickel crystal particles with a particle size of 0.5-5 micrometers are used as a template agent, which is uniformly sprayed onto the surface of the base membrane. The nickel crystals are heated to 120-150°C using microwaves, causing the base membrane in contact with the ultrafine nickel crystal particles to begin to melt. Under the influence of gravity, the particles sink, forming a sunken shape. The membrane is then left to stand for 10-50 minutes under nitrogen protection at an ambient temperature of 50-60°C, and then cooled to room temperature. Finally, it is washed away from the ultrafine nickel crystal particles by reverse rinsing with pure water at a pressure of 0.1-0.3 MPa, thus completing the etching process of the crystal structure and completing the preparation of the specialized microfiltration membrane. The main functional component of the crystallization unit is a microfiltration membrane. Under the action of this functional component, sodium sulfate will crystallize out in large quantities at a temperature of 5-8℃ while filtering, and the concentration of the crystallization mother liquor will drop to 20-50g / L.

[0008] As a preferred embodiment, in the above-mentioned Glauber's salt crystallization device, the sodium sulfate solution inlet feed of the cooling component is a sodium sulfate solution with a concentration of 150-260 g / L, and the sodium sulfate coolant outlet temperature is controlled at 6-8°C; the refrigerant inlet temperature is controlled at 1-5°C, and the refrigerant outlet temperature is controlled at 1-5°C. As a more preferred embodiment, the sodium sulfate solution inlet feed contains 1-50 g / L of sodium chloride, and the feed temperature is controlled at 5-40°C.

[0009] As a preferred embodiment, the concentration component of the aforementioned Glauber's salt crystallization apparatus is based on an electrically driven membrane, equipped with an AEM12 anion membrane and a CEM12 cation membrane from Fuji Film Co., Ltd. of Japan, with an operating current density of 300-600 A / m³. 2During the operation of the device, the crystallization mother liquor with a controlled concentration of 3-30 g / L enters the concentration unit from the dilute inlet and the concentrated inlet of the concentration unit. After concentration treatment, it is discharged from the dilute outlet with a concentration of 0.1-5 g / L. The sodium sulfate solution with a concentration of 150-260 g / L is circulated from the sodium sulfate concentrated solution and discharged to the cooling unit, where it enters the cooling unit together with the next batch of feed liquid.

[0010] Beneficial effects: This utility model is designed and developed based on the characteristics of Glauber's salt in the crystallization process. By utilizing the lattice structure characteristics of the device of this utility model, the amorphous problem in the crystallization process of Glauber's salt can be solved, and the recovery rate and purity can be improved in the treatment of sodium sulfate solution. Attached Figure Description

[0011] Figure 1 Structural diagram of this utility model 1. Cooling component; 2. Crystallization component; 3. Concentration component; 4. Sodium sulfate solution inlet; 5. Refrigerant inlet; 6. Refrigerant outlet; 7. Sodium sulfate coolant outlet; 8. Crystallization component inlet; 9. Crystal discharge outlet; 10. Crystallization mother liquor outlet; 11. Concentration component dilute solution inlet; 12. Concentration component concentrated solution inlet; 13. Dilute solution outlet; 14. Sodium sulfate concentrated solution circulation; 15. Microfiltration membrane. Detailed Implementation

[0012] Example 1 A polypropylene microfiltration membrane with a pore size of 0.45 micrometers was surface-treated for 3 hours using a mixture of n-butyl ketone and sulfolane. Ultrafine nickel crystal particles with a particle size of 0.5 micrometers were used as a template agent and uniformly sprayed onto the substrate membrane surface using a particle spraying machine. The nickel was heated to 120°C using microwaves, causing the substrate membrane in contact with the ultrafine nickel crystal particles to melt. Under gravity, the particles sank, forming a sunken shape. After standing for 20 minutes under nitrogen protection at an ambient temperature of 55°C and cooling to room temperature, the particles were washed off the substrate membrane with pure water at a pressure of 0.2 MPa, thus completing the etching process of the crystal structure and completing the preparation of the special microfiltration membrane 15; this microfiltration membrane 15 is a planar microfiltration membrane.

[0013] High-salt, high-COD wastewater containing 180 g / L sodium sulfate, 20 g / L sodium chloride, 500 mg / L COD, and 50 mg / L silicon was tested. The test solution entered through the sodium sulfate solution inlet 4 of cooling component 1; refrigerant at 3°C ​​entered through the refrigerant inlet 5; after heat exchange, the refrigerant outlet 6 reached a temperature of 25°C; and the sodium sulfate coolant outlet 7 reached a temperature of 6°C.

[0014] Sodium sulfate coolant at 6°C enters crystallization component 2 through outlet 7. Crystallization component 2 is equipped with crystallization component inlet 8 and is connected to sodium sulfate coolant outlet 7. Under the action of the special microfiltration membrane 15 of the main functional component, sodium sulfate will crystallize and precipitate out in large quantities at 6°C and be discharged from crystal outlet 9, while the concentration of crystallization mother liquor drops to 30g / L and is discharged from crystallization mother liquor outlet 10.

[0015] The crystallization mother liquor discharged from the crystallization mother liquor outlet 10 enters the concentration unit 3. This unit is based on an electrically driven membrane and is equipped with an AEM12 anion membrane and a CEM12 cation membrane from Fuji Film Co., Ltd. of Japan. The operating current density is 400A / m2. The crystallization mother liquor with a concentration of 30g / L enters the concentration unit 3 from the dilute liquid inlet 11 and the concentrated liquid inlet 12 of the concentration unit. After concentration treatment, it is discharged from the dilute liquid outlet 13 with a concentration of 5g / L; and discharged from the sodium sulfate concentrated liquid circulation 14 with a concentration of 180g / L. It is circulated to the sodium sulfate solution inlet 4 of the cooling unit 1 and enters the cooling unit 1 together with the next batch of feed liquid.

[0016] After the sodium sulfate in the test solution is recycled into this device, the purity of the crystals reaches 99.2%, and the sodium sulfate recovery rate reaches 96%.

[0017] Example 2 A polypropylene microfiltration membrane with a pore size of 0.45 micrometers was used, and a mixture of n-butyl ketone and sulfolane was used as the surface treatment solvent for 3 hours. Ultrafine nickel crystal particles with a particle size of 1 micrometer were used as a template agent and uniformly sprayed onto the substrate membrane surface using a particle spraying machine. The nickel was heated to 120°C using microwaves, causing the substrate membrane in contact with the ultrafine nickel crystal particles to begin to melt. Under the influence of gravity, the particles sank, forming a sunken shape. After standing for 100 minutes under nitrogen protection at an ambient temperature of 55°C, the membrane was cooled to room temperature and then washed off from the ultrafine nickel crystal particles by reverse rinsing with pure water at a pressure of 0.1 MPa, thus completing the etching process of the crystal structure and completing the preparation of the special microfiltration membrane 15.

[0018] High-salinity, high-COD wastewater containing 200 g / L sodium sulfate, 50 g / L sodium chloride, 800 mg / L COD, and 80 mg / L silicon was tested. The test solution entered through the sodium sulfate solution inlet 4 of cooling component 1; refrigerant at 4°C entered through the refrigerant inlet 5; after heat exchange, the refrigerant outlet 6 reached a temperature of 35°C; and the sodium sulfate coolant outlet 7 reached a temperature of 8°C.

[0019] Sodium sulfate coolant 7 at a temperature of 8°C enters the crystallization component 2. The crystallization component 2 is equipped with a crystallization component inlet 8 and is connected to the sodium sulfate coolant outlet 7. Under the action of the special microfiltration membrane 15 of the main functional component, sodium sulfate will crystallize and precipitate out in large quantities at a temperature of 7°C and be discharged from the crystal outlet 9, while the concentration of the crystallization mother liquor drops to 35g / L and is discharged from the crystallization mother liquor outlet 10.

[0020] The crystallization mother liquor discharged from the crystallization mother liquor outlet 10 enters the concentration unit 3. This unit is based on an electrically driven membrane and is equipped with an AEM12 anion membrane and a CEM12 cation membrane from Fuji Film Co., Ltd. of Japan. The operating current density is 450A / m2. The crystallization mother liquor with a concentration of 35g / L enters the concentration unit 3 from the dilute liquid inlet 11 and the concentrated liquid inlet 12 of the concentration unit. After concentration treatment, it is discharged from the dilute liquid outlet 13 with a concentration of 2g / L; and discharged from the sodium sulfate concentrated liquid circulation 14 with a concentration of 200g / L. It is circulated to the sodium sulfate solution inlet 4 of the cooling unit 1 and enters the cooling unit 1 together with the next batch of feed liquid.

[0021] After the sodium sulfate in the test solution is recycled into this device, the purity of the crystals reaches 99.6%, and the sodium sulfate recovery rate reaches 97%.

[0022] Example 3 The preparation of the special microfiltration membrane 15 is as described in Example 2.

[0023] High-salinity, high-COD wastewater containing 150 g / L sodium sulfate, 20 g / L sodium chloride, 300 mg / L COD, and 20 mg / L silicon was tested. The test solution entered through the sodium sulfate solution inlet 4 of cooling component 1; refrigerant at 5°C entered through the refrigerant inlet 5; after heat exchange, the refrigerant outlet 6 reached a temperature of 30°C; and the sodium sulfate coolant outlet 7 reached a temperature of 8°C.

[0024] Sodium sulfate coolant at 8°C enters crystallization component 2 through outlet 7. Crystallization component 2 is equipped with crystallization component inlet 8 and is connected to sodium sulfate coolant outlet 7. Under the action of the special microfiltration membrane 15 of the main functional component, sodium sulfate will crystallize and precipitate out in large quantities at 8°C and be discharged from crystal outlet 9, while the concentration of crystallization mother liquor drops to 40g / L and is discharged from crystallization mother liquor outlet 10.

[0025] The crystallization mother liquor discharged from the crystallization mother liquor outlet 10 enters the concentration unit 3. This unit is based on an electrically driven membrane and is equipped with an AEM12 anion membrane and a CEM12 cation membrane from Fuji Film Co., Ltd. of Japan. The operating current density is 400A / m2. The crystallization mother liquor with a concentration of 40g / L enters the concentration unit 3 from the dilute liquid inlet 11 and the concentrated liquid inlet 12 of the concentration unit. After concentration treatment, it is discharged from the dilute liquid outlet 13 with a concentration of 2g / L; and discharged from the sodium sulfate concentrated liquid circulation 14 with a concentration of 150g / L. It is circulated to the sodium sulfate solution inlet 4 of the cooling unit 1 and enters the cooling unit 1 together with the next batch of feed liquid.

[0026] After the sodium sulfate in the test solution is recycled into this device, the purity of the crystals reaches 98.5%, and the sodium sulfate recovery rate reaches 93%.

Claims

1. A Glauber's salt crystallization apparatus, comprising a cooling component (1), a crystallization component (2), and a concentration component (3); characterized in that: The cooling component (1) is provided with a sodium sulfate solution inlet (4) and a refrigerant inlet (5), as well as a refrigerant outlet (6) and a sodium sulfate coolant outlet (7). The sodium sulfate coolant outlet (7) controls the temperature of the liquid at 6-8℃, the refrigerant inlet (5) controls the temperature of the refrigerant at 1-5℃, and the refrigerant outlet (6) controls the temperature at 1-5℃. The crystallization component (2) is provided with a crystallization component inlet (8) and connected to the sodium sulfate coolant outlet (7). A microfiltration membrane (15) is placed inside the crystallization component (2). The microfiltration membrane (15) is a polypropylene microfiltration membrane with a pore size of 0.45 micrometers. The microfiltration membrane (15) is a flat microfiltration membrane with a recessed lattice structure etched on the membrane surface. The upper end of the crystallization component (2) has a crystal outlet (9) and a crystallization mother liquor outlet (10). The crystallization mother liquor outlet (10) is connected to the concentration component (3). The concentration component (3) is based on an electrically driven membrane and is equipped with an anion membrane and an cation membrane. The operating current density is 300-600A / m2. The inlet of the concentration component (3) is provided with a concentration component dilute liquid inlet (11) and a concentration component concentrated liquid inlet (12). The outlet is provided with a dilute liquid outlet (13) and a sodium sulfate concentrated liquid circulation (14) connected to the sodium sulfate solution inlet (4).