belt abrasive plate processing device

By using a concave arc-shaped pressure roller and appropriate abrasive belt grit, rotation speed, and rinsing device in the belt abrasive plate processing device, the problem of uneven resin grit on the plate surface was solved, and the uniformity of copper thickness and production efficiency were improved.

CN224951658UActive Publication Date: 2026-11-10GUANGZHOU TERMBRAY ELECTRONICS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202521909668.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-09-04
Publication Date
2026-11-10
Estimated Expiration
2035-09-04

Smart Images

  • Figure CN224951658U_ABST
    Figure CN224951658U_ABST
Patent Text Reader

Abstract

This utility model relates to the field of polishing machine technology, and more specifically, to a belt abrasive board processing device, including a conveying mechanism and a polishing mechanism. The polishing mechanism is disposed above the conveying mechanism and includes a rotating wheel, a pressure wheel, an abrasive belt loop, and a driving device. The driving device is connected to the rotating wheel and is used to drive the rotating wheel to rotate. The pressure wheel is arranged parallel to the rotating wheel, and the abrasive belt loop surrounds the rotating wheel and the pressure wheel. The pressure wheel is a long strip-shaped pressure roller with a concave arc-shaped center. By setting the center of the pressure wheel to a concave arc-shaped surface, it matches the surface of the PCB production board, thereby avoiding the situation where the resin adhesive remaining in the middle area of ​​the board is polished clean while the edge area still has residue, or where although the resin adhesive on the board surface is polished clean, more copper foil is polished in the middle area and less in the edge area, resulting in a thinner copper thickness in the middle area than in the edge area.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of grinding machine technology, and more specifically, to a sanding belt grinding plate processing device. Background Technology

[0002] In PCB manufacturing, resin via plugging is a critical process, primarily used to process non-conductive vias, such as mechanical vias and buried / blind vias, or conductive vias requiring special treatment. Its core advantages are: 1. Preventing residual contaminants within the vias. Resin plugging prevents chemical residues, dust, or impurities from remaining in the vias during PCB processing (e.g., electroplating, etching), which could lead to reliability issues in subsequent processes (e.g., lamination, solder masking). 2. Improving interlayer reliability. Unfilled buried / blind vias in multilayer boards can cause interlayer separation and board breakage during lamination due to air residue or insufficient resin. Resin plugging fills these gaps, enhancing interlayer bonding. The resin's coefficient of thermal expansion is close to that of the PCB substrate, reducing the risk of stress cracking between the via walls and the material at high temperatures (e.g., lead-free soldering). 3. Improving surface flatness. For high-density interconnect (HDI) boards or boards requiring laser drilling, resin plugging followed by grinding provides a flat surface for subsequent layers, preventing misalignment or circuit breakage caused by via depressions. 4. Solder Mask Coverage Requirements. If the via is located in the solder mask area, unfilled vias may allow ink to seep in, affecting the appearance or soldering. Resin plugging makes solder mask coverage easier, ensuring pad integrity. 5. Electrical Performance Optimization. In high-frequency designs, voids can cause signal reflection or electromagnetic interference (EMI). Resin filling reduces parasitic capacitance effects, improving signal integrity. It also prevents short circuits caused by humid or contaminated environments. 6. Adapting to Special Design Needs. For example, when a via is located below a pad, it must be filled with resin and electroplated; otherwise, solder paste will flow into the via during soldering, leading to poor soldering. Some designs require filling with thermally conductive resin after plugging to aid heat dissipation.

[0003] After resin filling, resin protrusions often remain at the orifices and on the board surface, resulting in an uneven surface that can affect subsequent processes. These issues include air bubbles or delamination during lamination, misalignment of solder resist or circuit layers, and unevenness of pads or holes, leading to uneven solder paste printing and cold solder joints. Therefore, after resin filling, a belt sander is typically used to grind the board to remove any remaining resin from the surface. However, in actual production, the production board is affected by the flow of the bonding resin from the center to the periphery, so the board is usually thicker in the center and thinner at the periphery. The pressure roller of the existing belt sander has a regular cylindrical structure. When the pressure roller drives the sanding belt to act on the board, the pressure in the middle area of ​​the board is greater and the pressure in the edge area is less. This results in the resin residue in the middle area of ​​the board being sanded away, while there is still residue in the edge area. Or, although the resin residue on the board surface is sanded away, more copper foil is sanded in the middle area and less copper foil is sanded in the edge area, making the copper thickness in the middle area thinner than that in the edge area. Utility Model Content

[0004] This utility model aims to overcome at least one of the defects (deficiencies) of the prior art and provides a belt sander for processing plates. This device solves the problem that when existing belt sanders grind plates, the resin residue in the middle area of ​​the plate is cleaned up, but there is still residue in the edge area. Alternatively, although the resin residue on the plate surface is cleaned up, more copper foil is ground up in the middle area and less in the edge area, resulting in a thinner copper thickness in the middle area compared to the edge area.

[0005] The technical solution adopted by this utility model is a sanding belt grinding plate processing device, including a conveying mechanism and a grinding mechanism. The grinding mechanism is arranged above the conveying mechanism and includes a rotating wheel, a pressure wheel, a sanding belt loop and a driving device. The driving device is connected to the rotating wheel and is used to drive the rotating wheel to rotate. The pressure wheel is arranged parallel to the rotating wheel. The sanding belt loop is wrapped around the rotating wheel and the pressure wheel. The pressure wheel is a long strip-shaped pressure roller, and the middle part of the pressure wheel is concave into an arc shape.

[0006] In operation, the PCB production board is placed on a conveyor mechanism for transporting the board. A polishing mechanism, positioned above the conveyor mechanism, polishes the PCB. This polishing mechanism includes a drive unit, a rotating wheel, a pressure wheel, and a sanding belt. The rotating wheel is connected to the drive unit, which is connected to a control unit. The pressure wheel is positioned below and parallel to the rotating wheel, determining the polishing pressure distribution. The sanding belt wraps around the rotating wheel and the pressure wheel. When the control unit operates the drive unit, the rotating wheel rotates, driving the sanding belt to move. Under the pressure wheel's action, the PCB is polished. The pressure wheel is designed with a concave arc shape in the center to align with the PCB surface, allowing for a cleaner and more thorough removal of residual resin adhesive without causing differences in copper thickness between the center and edge areas of the board.

[0007] Furthermore, the ratio of the minimum diameter to the maximum diameter of the pressure roller is 0.998 to 0.999.

[0008] The concave arc shape of the pressure roller is designed to match the surface of the PCB production board. If the ratio of its minimum diameter to its maximum diameter is less than 0.998, the through-hole filling ink in the edge area of ​​the PCB production board may be completely removed, but residue may remain in the center area. Alternatively, although the through-hole filling ink on the board surface may be removed, the copper thickness in the edge area may be less than that in the center area, resulting in a thicker center and thinner edges. If the ratio of its minimum diameter to its maximum diameter is greater than 0.999, the through-hole filling ink in the center area of ​​the PCB production board may be completely removed, but residue may remain in the edge area. Alternatively, although the through-hole filling ink on the board surface may be removed, the copper thickness in the center area may be less than that in the edge area, resulting in a thinner center and thicker edges.

[0009] Furthermore, the length of the pressure roller is 620~680mm.

[0010] In PCB manufacturing, the common large board size is 610mm × 610mm (24 inches). Setting the length of the pressure roller to 620~680mm can completely cover the width of the board, ensuring even distribution of grinding pressure and avoiding uneven grinding of the board edges or copper thickness due to the pressure roller being too short. On the other hand, being 20~70mm wider than the common PCB width allows for a safety margin to accommodate minor board misalignment and special process requirements, such as covering the seams during panelization.

[0011] Furthermore, the ratio of the maximum diameter of the pressure roller to the length of the pressure roller is 0.22 to 0.26.

[0012] If the ratio of the maximum diameter of the pressure roller to its length is too large, it will increase the roller's diameter, directly raising the rotation radius and centrifugal force. This will cause the sanding belt loop to swing centrifugally, reducing the contact area between the sanding belt loop and the PCB board, resulting in uneven sanding. Simultaneously, it will cause a surge in starting torque, increasing energy consumption and potentially leading to overheating of the drive unit. Conversely, if the ratio of the maximum diameter of the pressure roller to its length is too small, the roller's bending stiffness will decrease, potentially leading to excessive bending deformation or fatigue fracture. Furthermore, if the ratio is too small, the guiding torque will be insufficient, potentially causing the sanding belt loop to deviate and become uncontrollable.

[0013] Furthermore, the abrasive belt ring has an abrasive particle size of 400-500 mesh and a rotation speed of 8-12 m / s.

[0014] If the abrasive belt has a grit size of less than 400 mesh, the coarse particles and fast cutting speed effectively remove residual resin, but they can easily leave noticeable scratches or excessively wear down the copper layer. If the abrasive belt has a grit size greater than 500 mesh, although the surface of the board is smooth after polishing, the cutting efficiency is significantly reduced. Removing the same amount of resin requires more time or multiple polishing passes, leading to decreased production efficiency and increased abrasive belt wear costs. Using 400-500 mesh abrasive belts achieves the best balance between polishing efficiency and quality after resin-filled vias, providing greater safety and control over the resin and copper layer, and is compatible with most subsequent PCB processes.

[0015] Setting the rotation speed to 8-12 m / s is to match the abrasive grit size, balancing cutting efficiency and thermal control. This avoids excessively high rotation speed causing the resin to heat up too quickly due to friction, or insufficient cutting force due to insufficient rotation speed. The combination of 400-500 grit abrasive belt and a rotation speed of 8-12 m / s protects the resin and copper layer while improving polishing efficiency.

[0016] Furthermore, it also includes a rinsing device, which includes a nozzle disposed on the side where the sand belt loop cloth is detached from the pressure roller.

[0017] The temperature of both the abrasive belt loop and the PCB board rises immediately after polishing. Positioning the nozzle on the side of the abrasive belt loop that is detached from the pressure roller and rinsing both after polishing can lower their temperature, reducing material deformation or belt damage caused by overheating from friction. Furthermore, timely cleaning of debris from the abrasive belt surface prevents particles from embedding in the abrasive gaps, reducing the risk of belt clogging, extending belt life, and maintaining stable polishing results. If the nozzle is positioned on the side of the abrasive belt loop in contact with the pressure roller, the debris washed off may fall onto the PCB board and be pressed back into the PCB surface by the pressure roller, causing scratches or pits and affecting surface flatness. Secondly, if positioned on the contact side, the water flow from the nozzle may disturb the abrasive belt loop, affecting the uniformity of the polishing process.

[0018] Furthermore, the nozzle is oriented downwards from the pressure roller.

[0019] Orient the nozzle downwards from the pressure roller, ensuring the water jet lands on the area where the abrasive belt loop just separates from the PCB board. This effectively rinses both the abrasive belt loop and the PCB board, removing resin and copper shavings, maintaining optimal cutting performance, extending belt life, and preventing debris from re-adhering or accumulating in the sanded area, thus improving PCB surface cleanliness. Furthermore, it cools the sanding belt loop and PCB board after sanding, relieving thermal stress. Additionally, rinsing with water reduces dust and improves the working environment.

[0020] Furthermore, the angle between the nozzle of the rinsing device and the sand belt loop is 70-80 degrees.

[0021] A 70-80 degree angled spray can decompose the horizontal and vertical forces, simultaneously achieving the effects of removing excess resin and cooling. This angled spray not only reduces belt vibration and extends belt life, but also avoids excessive vertical force impacting the PCB board and causing resin tearing at the orifices. If the angle between the nozzle and the belt loop is less than 70 degrees, the horizontal force may be insufficient, resulting in poor rinsing, or higher pressure may be needed to compensate for the same cleaning effect. Additionally, the larger vertical force impacting the PCB board may damage the orifice edges, causing micro-cracks in the resin matrix to propagate. If the angle between the nozzle and the belt loop is greater than 80 degrees, approaching a vertical spray onto the belt loop, it may disturb the belt, causing belt vibration.

[0022] Furthermore, the conveying mechanism is equipped with an adjustment device for adjusting the operating speed of the conveying mechanism.

[0023] The conveyor mechanism is used to transport PCB production boards. An adjustment device can be set to adjust the running speed of the conveyor mechanism to avoid insufficient grinding due to excessive running speed or excessive grinding and reduced production efficiency due to excessive running speed. This allows it to work in conjunction with the grinding mechanism to better grind the PCB production boards.

[0024] Furthermore, the operating speed of the conveying mechanism is 2.0~2.5m / min.

[0025] The operating speed of the conveyor mechanism directly affects the contact time between the PCB production board and the abrasive belt ring. The speed setting must be matched with the abrasive grit size and rotation speed of the abrasive belt. An appropriate conveyor speed can improve production efficiency. A speed of 2.0~2.5 m / min ensures sufficient contact time between the abrasive belt and the PCB surface for effective grinding, without being too slow and impacting production efficiency. Secondly, it achieves better surface quality. Too fast a conveyor speed may lead to insufficient grinding, while too slow a speed may lead to over-grinding. A speed range of 2.0~2.5 m / min balances these two factors, ensuring consistent and stable surface quality. Furthermore, an appropriate conveyor speed helps control the temperature during grinding. Too fast a conveyor speed may result in insufficient grinding, while too slow a speed may generate excessive heat. A speed range of 2.0~2.5 m / min ensures a moderate temperature during grinding, reducing the risk of thermal damage and protecting the PCB surface.

[0026] Compared with existing technologies, the beneficial effects of this utility model are as follows: By setting the middle part of the pressure roller to be a concave arc shape to match the surface of the PCB board, it can effectively remove residual resin glue from the PCB board surface, and the copper thickness in the center area and the edge area of ​​the board will not differ after grinding. By limiting the ratio of the minimum diameter to the maximum diameter of the pressure roller, its overlap with the PCB board surface is improved, controlling the grinding quality and improving product yield. By limiting the length of the pressure roller, it can be used for common large board sizes, and limiting the ratio of the maximum diameter to the length of the pressure roller ensures that the pressure roller has sufficient bending stiffness and sufficient guiding torque, preventing the sanding belt loop from running off-center and avoiding excessive rotation radius due to excessively large pressure roller diameter, which would increase centrifugal force, cause the sanding belt to swing centrifugally, reduce the contact area between the sanding belt loop and the PCB board, and lead to uneven grinding. The abrasive belt's grit size and rotation speed are matched to protect the resin and copper layer, preventing excessive scratches or wear from overly coarse abrasive grains, while avoiding the reduced production efficiency caused by excessively fine abrasive grains requiring more time or multiple passes. The operating speed of the conveyor mechanism is matched to the grit size of the abrasive belt, ensuring sufficient contact time between the belt and the PCB surface for effective grinding, without compromising production efficiency due to excessively slow speeds. Furthermore, it achieves better surface quality, preventing insufficient grinding due to excessively fast conveyor speeds or over-grinding due to excessively slow speeds. This abrasive belt grinding device also includes a rinsing device with a nozzle at a 70-80 degree angle to the belt. This rinsing removes resin and copper shavings from the belt, cools the grinding area, reduces dust, and improves the working environment. The grinding plate power of the grinding mechanism increases with the number of times the sanding belt and ring cloth are used. When the sanding belt and ring cloth are used less often, a smaller power is used for grinding. When the sanding belt and ring cloth are used more often, a larger power is used for grinding to maintain the same grinding effect. Attached Figure Description

[0027] Figure 1 This is a structural diagram of the present invention.

[0028] Figure 2 This is a schematic diagram of the pressure roller of this utility model.

[0029] Figure 3 This is a schematic diagram showing how the improved pressure roller is matched to the surface of the PCB production board.

[0030] Figure 4 This is a schematic diagram of the pressure roller and PCB production board before the improvement. Detailed Implementation

[0031] The accompanying drawings are for illustrative purposes only and should not be construed as limiting the scope of this invention. To better illustrate the following embodiments, some components in the drawings may be omitted, enlarged, or reduced, and do not represent the actual dimensions of the product. It is understandable to those skilled in the art that some well-known structures and their descriptions may be omitted in the drawings.

[0032] like Figure 1 , Figure 2 As shown, a belt abrasive board processing device includes a conveying mechanism 1, a grinding mechanism 2, and a control host 3. The grinding mechanism 2 is located above the conveying mechanism 1 and includes a rotating wheel 21, a pressure wheel 22, an abrasive belt loop 23, and a driving device 24. The driving device 24 is connected to the rotating wheel 21 to drive the rotating wheel 21 to rotate. The pressure wheel 22 is arranged parallel to the rotating wheel 21. The abrasive belt loop 23 surrounds the rotating wheel 21 and the pressure wheel 22. The driving device 24 is electrically connected to the control host 3. The pressure wheel 22 is a long strip-shaped pressure roller. The middle part of the pressure wheel 22 is concave into an arc shape, thereby forming a structure with a smaller diameter D1 in the middle part and a larger diameter D at both ends. Preferably, the ratio of the diameter D1 in the middle to the diameter D at both ends is 0.998~0.999, so that it has a high degree of overlap with the surface of the PCB production board 4. In PCB manufacturing, the common large board size is 610mm × 610mm. To ensure the pressure rollers completely cover the width of the board, guarantee uniform grinding pressure distribution, and allow for a safety margin to accommodate slight board misalignment, the length L of the pressure roller 22 is set to 620~680mm. The ratio of the diameter D at both ends of the pressure roller 22 to its length L is 0.22~0.26. This prevents the diameter D from being too large, causing the sanding belt loop 23 to centrifugally swing and reduce the contact area between the sanding belt loop 23 and the PCB production board 4, or from being too small, resulting in reduced bending stiffness of the pressure roller 22, which could lead to excessive bending deformation or fatigue fracture. The sanding belt loop 23 is annular and is wound around the rotating wheel 21 and the pressure roller 22. When the driving device 24 drives the rotating wheel 21 to rotate, it can drive the sanding belt loop 23 to rotate, thereby grinding the PCB production board 4 below. The preferred particle size of the abrasive belt ring 23 is 400-500 mesh, and the rotation speed is 8-12 m / s. For example... Figure 3 As shown, the improved pressure roller 22 has a high degree of overlap with the surface of the PCB production board 4, which can prevent the resin glue in the middle area of ​​the PCB production board 4 from being polished clean while there are still residues in the edge area, or the resin glue on the board surface from being polished clean but the copper thickness in the middle area is less than that in the edge area, showing a thinner copper thickness in the middle and a thicker copper thickness around the edges. Figure 4The diagram shows the pressure roller and PCB production board 4 before the improvement. At this time, the pressure roller has a cylindrical structure, and the surface of the PCB production board has a certain curvature, with a thicker central area and a thinner edge area. When the PCB production board 4 is polished, the resin in the central area may be polished clean, but there may still be residue in the edge area. Or, although the resin on the board surface may be polished clean, the copper thickness in the central area may be polished more, while the copper thickness in the edge area may be polished less, and the copper thickness in the central area may be less than that in the edge area.

[0033] like Figure 1 As shown, the conveying mechanism 1 is used to convey the PCB production board 4. The conveying mechanism 1 is equipped with an adjustment device 11, which can adjust the running speed of the conveying mechanism 1. Its running speed is matched with the particle size and rotation speed of the sanding belt ring cloth 23, so as to better polish the PCB production board 4. Preferably, the running speed of the conveying mechanism 1 is 2.0~2.5m / min.

[0034] like Figure 1 As shown, the belt abrasive grinding plate processing device also includes a rinsing device 5 (not shown). The rinsing device 5 includes a nozzle 51, which is located on the side where the abrasive belt ring 23 is separated from the pressure roller 22, and the nozzle 51 faces downward of the pressure roller 22. The included angle α between the nozzle 51 and the abrasive belt ring 23 is 70~80 degrees. While rinsing the abrasive belt ring 23, it can also cool down the grinding area, achieve a cooling effect, reduce dust, and improve the working environment.

[0035] When using this device, the PCB production board 4 is placed on the conveyor mechanism 1, and the running speed of the conveyor mechanism 1 is adjusted to match the particle size and rotation speed of the sanding belt ring cloth 23. The grinding power of the grinding mechanism 2 is adjusted by controlling the host 3, and the drive device 24 is started to make the rotating wheel 21 rotate, which in turn drives the sanding belt ring cloth 23 to rotate, thereby grinding the PCB production board 4.

[0036] Before the formal grinding process, a first-board test is usually required. The first-board test process is as follows: S1. Select the appropriate grinding method according to the manufacturing instructions and the surface copper thickness data of the board from the previous process; S2. After grinding the board individually on a belt sander 5 times, or grinding the entire board twice, inspect the appearance. If there is resin residue, the copper thickness of the first board must be measured. S21. If the copper thickness is within the manufacturing instructions or exceeds the control requirements, measure the copper thickness once for each individual pass through the belt sander twice or for each entire grinding plate once. When the total number of grinding passes is 10 individual passes through the belt sander or 4 entire grinding plates, check the appearance. If there is still resin residue, it needs to be manually polished or the shift leader should be notified for handling. S22. If the copper thickness is lower than the MI requirement, suspend grinding, check the appearance, and if there is a small amount of resin residue, it can be manually ground; otherwise, notify the shift leader for handling.

[0037] After the first board test, the grinding parameters of the first board are recorded. The main parameters are the number of grinding cycles with the abrasive belt, the current value of the non-woven fabric grinding, and the grinding speed. After the appearance inspection and copper thickness measurement meet the quality requirements, the formal grinding is carried out according to the grinding parameters of the first board.

[0038] During the actual grinding process, the wear of the abrasive belt ring 23 increases with the number of grinding cycles. Therefore, the grinding power of the grinding mechanism 2 needs to be adjusted accordingly by the control host 3 to ensure a consistent grinding effect. Specifically, when the abrasive belt ring 23 is used 1 to 80 times, the abrasive grains are sharp and have high cutting efficiency, requiring a grinding power of 1.60 to 1.80 kW. When the abrasive belt ring 23 is used 81 to 150 times, the abrasive grains become slightly dull, reducing the cutting force, requiring a grinding power of 1.80 to 2.00 kW. When the abrasive belt ring 23 is used 151 to 400 times, the abrasive grains become severely dull, and resin and copper shavings accumulate between the grains, significantly reducing the cutting force. In this case, a grinding power of 2.00 to 2.50 kW is required. When the sanding belt loop 23 has been used more than 400 times, it needs to be replaced.

[0039] Obviously, the above embodiments of this utility model are merely examples for clearly illustrating the technical solution of this utility model, and are not intended to limit the specific implementation of this utility model. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the claims of this utility model should be included within the protection scope of the claims of this utility model.

Claims

1. A belt abrasive plate processing device, comprising a conveying mechanism and a grinding mechanism, wherein the grinding mechanism is disposed above the conveying mechanism and includes a rotating wheel, a pressure wheel, an abrasive belt loop, and a driving device, the driving device being connected to the rotating wheel for driving the rotating wheel to rotate, the pressure wheel being arranged parallel to the rotating wheel, and the abrasive belt loop surrounding the rotating wheel and the pressure wheel, characterized in that, The pressure roller is a long strip-shaped pressure roller with an inwardly concave arc shape in the middle.

2. The belt abrasive grinding plate processing device according to claim 1, characterized in that, The ratio of the minimum diameter to the maximum diameter of the pressure roller is 0.998 to 0.

999.

3. The belt abrasive grinding plate processing device according to claim 2, characterized in that, The length of the pressure roller is 620~680mm.

4. The belt abrasive grinding plate processing device according to claim 3, characterized in that, The ratio of the maximum diameter of the pressure roller to its length is 0.22 to 0.

26.

5. The belt abrasive grinding plate processing device according to claim 1, characterized in that, The abrasive belt ring has an abrasive particle size of 400-500 mesh and a rotation speed of 8-12 m / s.

6. The belt abrasive grinding plate processing apparatus according to any one of claims 1 to 5, characterized in that, It also includes a rinsing device, which includes a nozzle disposed on the side where the sand belt loop is detached from the pressure roller.

7. The belt abrasive grinding plate processing device according to claim 6, characterized in that, The nozzle faces downwards from the pressure roller.

8. The belt abrasive grinding plate processing device according to claim 7, characterized in that, The angle between the nozzle of the rinsing device and the sand belt loop is 70-80 degrees.

9. The belt abrasive grinding plate processing apparatus according to any one of claims 1 to 5, characterized in that, The conveying mechanism is equipped with a regulating device to adjust the operating speed of the conveying mechanism.

10. The belt abrasive grinding plate processing device according to claim 9, characterized in that, The operating speed of the conveying mechanism is 2.0~2.5m / min.