A cover plate structure

By designing perforations and uniform pressing force in the cover plate structure, the welding problem caused by uneven pressing in traditional cover plate designs is solved, which improves the packaging yield and reliability, simplifies the production process, and reduces costs.

CN224960042UActive Publication Date: 2026-11-10SILICONWARE TECH SUZHOU
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522417239.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-14
Publication Date
2026-11-10
Estimated Expiration
2035-11-14

AI Technical Summary

Technical Problem

Traditional cover plate designs result in uneven pressing in the outer area of ​​the substrate, leading to problems such as soldering failure, bridging, and chip breakage during the soldering process, which cannot meet the requirements of modern electronic devices for packaging reliability and stability.

Method used

A cover plate structure is designed, including a perforated section consisting of multiple first windows arranged in an array and multiple second windows surrounding the central perforated section. The shortest distance between the outer perforated section and the outer edge of the cover plate body is between 6mm and 12mm. It is processed by stamping and cutting processes, combined with magnetic adsorption components and anti-loosening grooves to ensure uniform pressing force.

Benefits of technology

Effective control of substrate deformation improves packaging yield, reduces warpage and stress concentration, enhances welding quality and chip packaging reliability, simplifies production processes, and reduces costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224960042U_ABST
    Figure CN224960042U_ABST
Patent Text Reader

Abstract

The cover plate structure of the utility model discloses a cover plate main body and a hollow part, the hollow part includes a middle hollow part and a peripheral hollow part, the middle hollow part is formed by a plurality of first windows arranged in an array, and the peripheral hollow part is formed by a plurality of second windows arranged around the middle hollow part. Wherein, the shortest distance D between the peripheral hollow part and the outer edge of the cover plate main body is between 6mm-12mm. Through forming the hollow part on the cover plate main body, the pressing force of the substrate corner and the peripheral area is equivalent to the inside, the deformation of the substrate in the reflow soldering furnace heating welding process can be effectively controlled, and the problem of the decrease of the rigidity of the substrate due to the thinning of the substrate thickness and the reduction of the packaging volume in the prior art is solved. This design significantly reduces the warping and stress concentration phenomenon in the welding process, improves the welding quality and the reliability of the chip packaging.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The utility model relates to the technical field of semiconductor packaging, specifically, a cover plate structure. BACKGROUND

[0002] With the rapid development of semiconductor technology, flip chip level packaging process has become one of the mainstream packaging technologies due to its high density, high performance and small size advantages. The process usually integrates multiple single substrates onto a whole substrate, then connects the circuits by reflow soldering, and finally gets multiple flip chip level packaging units by cutting. This packaging method not only improves the packaging efficiency, but also significantly reduces the packaging cost, meeting the demand of modern electronic devices for high performance and miniaturization.

[0003] However, in actual production, the deformation of the substrate caused by thermal stress during reflow soldering will cause problems such as soldering rejection, bridging and chip cracking, which seriously affect the packaging yield. The main reason for these problems is that the substrate will generate stress due to thermal expansion during heating, and this stress is particularly pronounced in the edge and corner areas of the substrate. When the stress exceeds the yield strength of the substrate material, it will cause permanent deformation of the substrate, thereby affecting the soldering quality. The traditional cover plate design usually uses SUS430, SUS301 or SK5 steel sheet to hollow out the window corresponding to the substrate chip soldering area, and presses the cover plate on the substrate by magnetic attraction. This design can control the deformation of the substrate to some extent, but as the volume of modern packaging continues to shrink and the thickness of the substrate gradually thins, the rigidity of the substrate gradually decreases. This design is particularly evident in the peripheral area of the substrate, resulting in a high incidence of soldering problems in the peripheral or corner positions during chip packaging. This is because the traditional cover plate design has uneven pressing force in the peripheral area of the substrate, which cannot effectively control the deformation of the substrate, thereby causing various problems during soldering. In addition, modern electronic devices have increasingly high requirements for the reliability and stability of packaging, and the traditional cover plate design cannot meet these requirements. SUMMARY

[0004] In view of the problems existing in the prior art described above, the present application provides a cover plate structure that can effectively control the deformation of the substrate and improve the packaging yield.

[0005] To achieve the above-mentioned and other related purposes, the utility model provides a cover plate structure, comprising:

[0006] a cover plate body;

[0007] a hollow part, including a middle hollow part and a peripheral hollow part, the middle hollow part is composed of a plurality of first windows arranged in an array, and the peripheral hollow part is composed of a plurality of second windows arranged around the middle hollow part;

[0008] The shortest distance D between the peripheral hollow part and the outer edge of the cover plate body is between 6mm and 12mm.

[0009] Optionally, the first window and the second window are both rectangular windows.

[0010] Optionally, the cover plate structure further comprises a lettering area arranged at the edge of the cover plate body.

[0011] Optionally, the width of the first window is less than or equal to 5mm, and the width of the second window is less than or equal to 5mm.

[0012] Optionally, the cover plate structure further comprises a two-dimensional code lettering area arranged at the edge of the cover plate body.

[0013] Optionally, the cover plate structure further comprises an anti-rust coating arranged on the upper surface of the cover plate body.

[0014] Optionally, the thickness of the cover plate body is between 0.5mm and 2mm.

[0015] Optionally, the shortest distance D between the peripheral hollow part and the outer edge of the cover plate body is between 6mm and 8mm.

[0016] Optionally, the distance between adjacent first windows is between 0.6mm and 1.0mm, the distance between adjacent second windows is between 0.6mm and 1.0mm, and the shortest distance between the first window and the second window is between 0.6mm and 1.0mm.

[0017] Optionally, the cover plate structure further comprises a positioning hole arranged at the edge of the cover plate body.

[0018] As described above, the cover plate structure provided by the utility model has at least the following beneficial technical effects:

[0019] The cover plate structure comprises a cover plate body and a hollow part, the hollow part comprises a middle hollow part and a peripheral hollow part, the middle hollow part is composed of a plurality of first windows arranged in an array, and the peripheral hollow part is composed of a plurality of second windows arranged around the middle hollow part. The shortest distance D between the peripheral hollow part and the outer edge of the cover plate body is between 6mm and 12mm.

[0020] The application forms a hollow part on the cover plate body, so that the pressing force of the substrate corner and the peripheral area is equivalent to the internal equivalent, effectively improves the welding workability, and significantly improves the packaging yield of the chip packaging. This design overcomes the problems of welding rejection, bridging and chip fracture caused by uneven pressing in the traditional cover plate structure design.

[0021] The cover plate structure of the present application can effectively control the deformation of the substrate during the reflow soldering process, solving the problem of reduced substrate rigidity caused by the thinning of the substrate thickness and the reduction of the package size. This design significantly reduces the warping and stress concentration phenomenon during the soldering process, improving the soldering quality and the reliability of the chip package.

[0022] The cover plate structure of the present application adopts a simple stamping and cutting process, simplifying the design and assembly process of the chip cap, greatly improving the integration and assembly efficiency of the package structure. This design overcomes the complexity in the manufacturing process of traditional cover plate structures, reduces production costs, and improves production efficiency.

[0023] The cover plate structure of the present application realizes effective suppression of the chip soldering area while ensuring the rigidity of the substrate, solving the problem of substrate deformation caused by uneven suppression of the cover plate in the prior art, thereby significantly improving the overall quality and reliability of the chip package. BRIEF DESCRIPTION OF DRAWINGS

[0024] Figure 1 The structure of the cover plate structure provided by an embodiment of the present application is shown.

[0025] REFERENCE NUMERALS

[0026] 1, cover plate main body; 11, hollow part; 111, middle hollow part; 1111, first window; 112, peripheral hollow part; 1121, second window; 12, lettering area; 13, two-dimensional code printing area; 14, positioning hole. DETAILED DESCRIPTION

[0027] The embodiments of the present application will be described in detail below through specific and concrete examples, and those skilled in the art can easily understand other advantages and effects of the present application from the content disclosed in the present specification. The present application can also be implemented or applied in different specific embodiments, and various modifications or changes can be made to the details in the present specification based on different viewpoints and applications without departing from the spirit of the present application.

[0028] It should be noted that the illustrations provided in the present embodiment only illustrate the basic concept of the present application in a schematic manner, and although only the components related to the present application are shown in the illustrations, the actual implementation does not draw the components in the number, shape and size, and the shape, number, positional relationship and proportion of each component can be changed arbitrarily under the premise of realizing the technical solutions of the present application, and the component layout form can also be more complex.

[0029] This embodiment provides a cover plate structure disposed on a substrate. The main function of the cover plate structure is to apply uniform pressure to the substrate during the welding process, thereby reducing substrate deformation caused by thermal stress and improving packaging yield and reliability. The size and shape of the cover plate body 1 match the substrate. In this embodiment, the specific dimensions of the cover plate body 1 can be adjusted according to actual packaging requirements to adapt to substrates and chips of different sizes. In an optional embodiment of this embodiment, the size of the cover plate body 1 is 253mm × 86.3mm. The thickness of the cover plate body 1 is between 0.5mm and 2mm to ensure the stability and sufficient rigidity of the cover plate structure under high-temperature environments. During high-temperature welding, the substrate and cover plate are subjected to significant thermal stress; therefore, the cover plate body 1 needs to have sufficient thickness to resist these stresses and prevent deformation or damage.

[0030] Reference Figure 1The cover plate structure of this embodiment includes a cover plate body 1 and a hollow portion 11. The hollow portion 11 includes a central hollow portion 111 and a peripheral hollow portion 112. The central hollow portion 111 is composed of a plurality of first windows 1111 arranged in an array, with the spacing between adjacent first windows 1111 ranging from 0.6 mm to 1.0 mm. The peripheral hollow portion 112 is composed of a plurality of second windows 1121 arranged around the central hollow portion 111, with the spacing between adjacent second windows ranging from 0.6 mm to 1.0 mm. The shortest distance between the first windows and the second windows is 0.6 mm to 1.0 mm. This design not only optimizes the layout of the welding area but also ensures a more uniform distribution of thermal stress in the cover plate body 1 during the welding process. In an optional embodiment of this embodiment, the spacing between adjacent first windows 1111 is 0.8 mm. The peripheral hollow portion 112 is composed of a plurality of second windows 1121 arranged around the central hollow portion 111, with the spacing between adjacent second windows being 0.8 mm. The shortest distance between the first and second openings is 0.8 mm. Optionally, in this embodiment, both the first opening 1111 and the second opening 1121 are rectangular openings. The rectangular opening design not only facilitates processing and manufacturing but also ensures precise exposure of the welding area, thereby improving the accuracy and reliability of welding. The specific dimensions and shapes of the first opening 1111 and the second opening 1121 are designed according to actual needs and are not limited here. In this embodiment, the width of the first opening 1111 is ≤ 5 mm, and the width of the second opening 1121 is ≤ 5 mm. These size ranges ensure sufficient exposure of the welding area while avoiding insufficient rigidity of the cover plate structure due to excessively large openings. In this embodiment, the shortest distance D between the outer perforated portion 112 and the outer edge of the cover plate body 1 is between 6 mm and 12 mm to ensure the structural strength and stability of the cover plate body 1. In addition, this distance range also takes into account the overall structural strength of the cover plate body 1. During the design, it is necessary to ensure that the cover plate body 1 will not deform or be damaged due to external forces or thermal stress during the welding process. By setting the shortest distance D between 6mm and 12mm, the usable space in the welding area can be maximized while ensuring structural strength. Furthermore, the shortest distance D between the outer perforated portion 112 and the outer edge of the cover plate body 1 is between 6mm and 8mm. In an optional embodiment of this example, the shortest distance D between the outer perforated portion 112 and the outer edge of the cover plate body 1 is 6.6mm.

[0031] Specifically, refer to Figure 1The fabrication of the cover plate structure begins with stamping the outer shape of the cover plate body 1 onto a steel sheet, followed by wire cutting on a lathe to form the hollowed-out portion 11. The cut and stamped areas are then deburred. Finally, surface treatment is performed. In an optional embodiment of this work, the overall shape of the cover plate body 1 is first stamped onto SUS430, SUS301, or SK5 steel sheets. These materials not only possess excellent mechanical properties but also maintain stability under high temperatures. The stamping process ensures the shape accuracy and surface flatness of the cover plate body 1 while improving production efficiency. During the stamping process, precise mold design and control ensure that the dimensions and shape of the cover plate body 1 meet design requirements. Then, wire cutting on a lathe is used to precisely cut out the central hollowed-out portion 111 and the first and second openings 1111 and 1121 of the peripheral hollowed-out portion 112. The wire cutting process enables high-precision window processing, ensuring that the dimensions and shape of the openings meet design requirements. The specific dimensions and shapes of the first window 1111 and the second window 1121 are adjusted according to actual packaging requirements to ensure full exposure of the welding area while reducing substrate deformation. Next, the cutting and stamping areas are deburred to remove burrs and sharp edges generated during processing. Deburring improves the surface quality and reliability of the cover plate, preventing short circuits or poor contact caused by burrs during use. Deburring typically employs mechanical grinding or chemical treatment methods to ensure a smooth and clean cover plate surface. Finally, the cover plate body 1 undergoes surface treatment. Specifically, a rust-proof coating is applied to the upper surface of the cover plate structure. The thickness of the rust-proof coating is between 2μm and 3μm, and the specific thickness can be adjusted according to environmental conditions and usage requirements. The rust-proof coating uses high-performance rust-proof materials, effectively preventing corrosion of the cover plate body 1 due to environmental factors during use. This material has excellent corrosion resistance and weather resistance, protecting the cover plate body 1 in various harsh environments. The thickness of the rust-proof coating is precisely controlled to ensure that it provides sufficient protection without adding excessive weight or affecting the dimensional accuracy of the cover plate body 1. This design extends the service life of the cover structure and improves its reliability and durability. Furthermore, the anti-rust coating provides wear resistance and scratch resistance, further enhancing the surface quality of the cover body 1. This surface treatment not only prevents surface damage caused by daily operation but also maintains the appearance quality of the cover body 1, ensuring a good visual effect over long-term use. The material selection and thickness control of the anti-rust coating ensure the long-term stability and reliability of the cover structure in various application scenarios. Magnetic adsorption components are provided on the lower surface of the cover body 1. The magnetic strength of these components is sufficient to overcome thermal stress and mechanical vibration during welding, ensuring a tight fit between the cover body 1 and the substrate. The magnetic adsorption components are evenly distributed on the lower surface of the cover body 1, ensuring uniform magnetic force distribution and thus improving the stability and reliability of the welding process.In this embodiment, the thickness of the magnetic adsorption component is between 0.5 mm and 1 mm. Optionally, an anti-loosening groove is also provided around the periphery of the cover plate body 1, with a depth between 0.5 mm and 1 mm. The anti-loosening groove design can effectively reduce the displacement of the cover plate body 1 during welding, improving the welding accuracy and reliability. The anti-loosening groove surrounds the periphery of the cover plate body 1, forming a continuous groove structure, effectively restricting the movement of the cover plate body 1, thereby reducing the loosening of the cover plate due to thermal expansion. Specifically, during high-temperature welding, the substrate and cover plate structure will displace due to thermal expansion, which will cause the welding point to shift, thus affecting the welding quality. The anti-loosening groove ensures precise alignment of the welding point by restricting the movement of the cover plate body 1, thereby improving the welding success rate and the reliability of the encapsulation. In addition, the design of the anti-loosening groove also considers the distribution of thermal stress during the welding process. By providing an anti-loosening groove around the periphery of the cover plate body 1, thermal stress can be effectively dispersed, reducing deformation or damage to the cover plate body 1 caused by stress concentration. This design not only improves the stability of the welding process but also extends the service life of the cover plate structure. In practical applications, the combined use of the magnetic adsorption component and the anti-loosening groove provides dual protection for the cover body 1. The magnetic adsorption component ensures the initial alignment and stability of the cover body 1 during the welding process, while the anti-loosening groove further restricts the displacement of the cover body 1 under high-temperature environments. This dual protection mechanism significantly improves the reliability of the welding process and the packaging quality. Preferably, the cover structure also includes positioning holes 14, which are located on the edge of the cover body 1 to ensure precise alignment of the cover structure during the welding process, thereby improving the accuracy and reliability of the packaging.

[0032] Reference Figure 1 The cover structure of this embodiment also includes an engraving area 12. The engraving area 12 is located on the edge of the cover body 1 and is used to identify relevant information about the cover, such as production batch and model number. This information is crucial for product traceability and management, helping to quickly identify specific information about the cover during production, transportation, and use. In an optional embodiment of this embodiment, the area of ​​the engraving area 12 does not exceed 10% of the total area of ​​the cover body 1 to ensure that the overall structural integrity of the cover body 1 is not affected. The position and size of the engraving area 12 are carefully designed to provide sufficient space for information identification without affecting the function of the cover body 1. The cover structure also includes a QR code printing area 13, located on the edge of the cover body 1, for quickly identifying detailed information about the cover, such as production date, specifications, and quality inspection results. The area of ​​the QR code printing area 13 does not exceed 25% of the area of ​​the cover body 1. As an efficient information storage and identification method, QR codes can be quickly read by scanning devices, providing detailed product information. This design not only improves the efficiency of information management but also reduces the possibility of human error in identification.

[0033] This application improves soldering workability and significantly increases chip packaging yield by forming a hollow portion 11 on the cover plate body 1, making the pressing force in the corners and peripheral areas of the substrate equivalent to that in the interior. This design overcomes problems such as soldering rejection, bridging, and chip breakage caused by uneven pressing in traditional cover plate structure designs.

[0034] The cover plate structure of this application can effectively control the deformation of the substrate during the reflow soldering process, solving the problem of reduced substrate rigidity caused by substrate thinning and package size reduction in the prior art. This design significantly reduces warping and stress concentration during the soldering process, improving soldering quality and chip packaging reliability.

[0035] The cover plate structure of this application employs a simple stamping and cutting process, simplifying the design and assembly of the chip cap and significantly improving the integration and assembly efficiency of the packaging structure. This design overcomes the complexity of traditional cover plate structure manufacturing processes, reduces production costs, and improves production efficiency.

[0036] The cover plate structure of this application, through a reasonable window design, effectively presses the chip welding area while ensuring the rigidity of the substrate, solving the problem of substrate deformation caused by uneven cover plate pressing in the prior art, thereby significantly improving the overall quality and reliability of chip packaging.

[0037] The above embodiments are merely illustrative of the principles and effects of this utility model and are not intended to limit the scope of this utility model. Any person skilled in the art can modify or alter the above embodiments without departing from the spirit and scope of this utility model. Therefore, all equivalent modifications or alterations made by those skilled in the art without departing from the spirit and technical concept disclosed in this utility model should still be covered by the claims of this utility model.

Claims

1. A cover plate structure, characterized in that, include: Cover plate body; The hollow section includes a central hollow section and an outer hollow section. The central hollow section is composed of multiple first windows arranged in an array, and the outer hollow section is composed of multiple second windows arranged around the central hollow section. The shortest distance D between the outer perforated portion and the outer edge of the cover plate body is between 6mm and 12mm.

2. The cover plate structure according to claim 1, characterized in that, Both the first window and the second window are rectangular windows.

3. The cover plate structure according to claim 1, characterized in that, Also includes: The engraving area is located on the edge of the cover plate body.

4. The cover plate structure according to claim 1, characterized in that, The width of the first window opening is ≤5mm, and the width of the second window opening is ≤5mm.

5. The cover plate structure according to claim 1, characterized in that, Also includes: The QR code printing area is located on the edge of the cover plate body.

6. The cover plate structure according to claim 1, characterized in that, Also includes: A rust-proof coating is applied to the upper surface of the cover plate body.

7. The cover plate structure according to claim 1, characterized in that, The thickness of the cover plate body is between 0.5mm and 2mm.

8. The cover plate structure according to claim 1, characterized in that, The shortest distance D between the outer perforated portion and the outer edge of the cover plate body is between 6mm and 8mm.

9. The cover plate structure according to claim 1, characterized in that, The spacing between adjacent first windows is between 0.6mm and 1.0mm, the spacing between adjacent second windows is between 0.6mm and 1.0mm, and the shortest distance between the first window and the second window is between 0.6mm and 1.0mm.

10. The cover plate structure according to claim 1, characterized in that, Also includes: Positioning holes are provided on the edge of the cover plate body.