Aluminum-plastic film and electrochemical device
By setting a thinning zone and an adhesive layer on the aluminum-plastic film, the problem of decreased battery energy density and safety hazards caused by tab bending is solved, thereby improving battery energy density and enhancing safety performance.
Patent Information
- Application Number
- CN202522500630.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-25
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-25
AI Technical Summary
In electrochemical energy storage devices, bending of the tabs increases the space at the head of the aluminum-plastic film, affecting the battery's energy density and potentially damaging the electrode structure, thus posing a safety hazard.
A thinning area is set on the aluminum-plastic film to correspond to the position of the electrode tab, increasing the space for placing the electrode tab. An adhesive layer is set in the thinning area to fix the electrode tab and prevent it from shaking.
The overall battery size has been optimized, improving energy density and safety performance, and avoiding structural damage and short-circuit risks caused by tab compression.
Smart Images

Figure CN224979321U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of electrochemical energy storage technology, and in particular to an aluminum-plastic film and an electrochemical device. Background Technology
[0002] In the development of electrochemical energy storage devices, improving battery energy density and ensuring its safety performance have always been core research goals. In actual battery production, the battery cells need to be encapsulated within an aluminum-plastic film. As a packaging material with good barrier properties, flexibility, and mechanical strength, aluminum-plastic film is widely used in battery encapsulation, effectively protecting the battery cells from external environmental influences.
[0003] However, a series of problems affecting battery performance arose during the process of loading the battery cell into the aluminum-plastic film and encapsulating it. Specifically, after the battery cell is loaded into the aluminum-plastic film, the tabs are bent and ultimately squeezed into the head area of the film. This bending action creates a compression effect, increasing the space in the head area of the aluminum-plastic film. This increased space directly leads to a larger overall battery size. An increased overall battery size means that, within the same volume or mass constraints, there is a relative reduction in the amount of active material available for storing electrical energy, thus decreasing the battery's energy density. Furthermore, the bending of the tabs also exerts a compressive force on the electrode sheets. The electrode sheets are the core components in the battery cell where electrochemical reactions occur, and their structural integrity is crucial for the normal operation of the battery. The compressive force from the tabs can damage the structural integrity of the electrode sheets, leading to cracks and detachment. Damage to the electrode sheet structure can cause internal short circuits, localized overheating, and other safety hazards, affecting the battery's safety performance. Utility Model Content
[0004] The main objective of this application is to propose an aluminum-plastic film and an electrochemical device, which aims to improve the energy density and safety performance of the electrochemical device.
[0005] To achieve the above objectives, this application proposes an aluminum-plastic film for wrapping a battery cell. The aluminum-plastic film includes a PP layer close to the battery cell and a nylon layer facing away from the battery cell, with an aluminum layer disposed between the PP layer and the nylon layer. The PP layer and / or the nylon layer are provided with thinning areas, the positions of which correspond to the positions of the tabs of the battery cell.
[0006] In some embodiments, a first thinning region is provided on the PP layer, the thickness of the PP layer is 30um to 60um, and the depth of the first thinning region is 10um to 40um.
[0007] In some embodiments, an adhesive layer is provided on the inner wall of the first thinning zone.
[0008] In some embodiments, the thickness of the adhesive layer is 5 μm to 16 μm.
[0009] In some embodiments, the adhesive layer is a tape applied to the first thinned area.
[0010] In some embodiments, a second thinning zone is provided on the nylon layer.
[0011] In some embodiments, the thickness of the nylon layer is 15 μm to 25 μm.
[0012] In some embodiments, the depth of the second thinning zone is 10 μm to 20 μm.
[0013] In another aspect, this application also proposes an electrochemical device, including a battery cell and an aluminum-plastic film covering the battery cell, wherein the aluminum-plastic film is the aforementioned aluminum-plastic film.
[0014] In some embodiments, the battery cell includes a positive electrode, a negative electrode, a separator, and tabs. The positive electrode includes a positive current collector and a positive active material layer, and the negative electrode includes a negative current collector and a negative active material layer. Tabs are attached with tab adhesive at positions corresponding to the positive and negative electrode.
[0015] This application proposes an aluminum-plastic film and an electrochemical device. By setting a thinning region on the aluminum-plastic film, with the position of the thinning region corresponding to the position of the battery cell's tab, the placement space of the tab within the aluminum-plastic film is increased, thereby optimizing the overall size and improving the energy density. Furthermore, an adhesive layer is set on the thinning region, allowing the battery cell's tab to be fixed in the thinning region by the adhesive force of the adhesive layer, preventing the tab from shifting within the aluminum-plastic film and improving safety performance. Attached Figure Description
[0016] Figure 1 This is a schematic diagram of the aluminum-plastic film structure in one embodiment of this application; Figure 2 This is a schematic diagram of the aluminum-plastic film structure in another embodiment of this application; Figure 3 This is a schematic diagram of the aluminum-plastic film structure in another embodiment of this application; Figure 4 This is a schematic diagram of the aluminum-plastic film structure in another embodiment of this application; Figure 5 This is a schematic diagram of the structure of the battery cell and aluminum-plastic film in one embodiment of this application.
[0017] Explanation of reference numerals in the attached figures: Aluminum-plastic film 100; PP layer 110; first thinning zone 111; adhesive layer 112; aluminum layer 120; nylon layer 130; second thinning zone 131; thinning zone 140; battery cell 200; tab 210. Detailed Implementation
[0018] The solutions in the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments in this application, and not all of the embodiments. Based on the embodiments in this application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of this application.
[0019] It should be noted that all directional indicators (such as up, down, left, right, front, back, etc.) in the embodiments of this application are only used to explain the relative positional relationship and movement of each component in a certain specific posture (as shown in the figure). If the specific posture changes, the directional indicator will also change accordingly.
[0020] It should also be noted that when a component is described as "fixed to" or "set on" another component, it can be directly on the other component or there may be an intervening component present. When a component is described as "connected to" another component, it can be directly connected to the other component or there may be an intervening component present.
[0021] Furthermore, the use of terms such as "first" and "second" in this application is for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. Additionally, the technical solutions of the various embodiments can be combined with each other, but only on the basis of being achievable by those skilled in the art. When the combination of technical solutions is contradictory or impossible to implement, such a combination of technical solutions should be considered non-existent and not within the scope of protection claimed in this application.
[0022] Please see Figures 1 to 3 This application provides an aluminum-plastic film 100 for wrapping a battery cell 200. The aluminum-plastic film 100 includes a PP layer 110 close to the battery cell 200 and a nylon layer 130 facing away from the battery cell 200. An aluminum layer 120 is disposed between the PP layer 110 and the nylon layer 130. The PP layer 110 and / or the nylon layer 130 are provided with a thinning area 140, the position of which corresponds to the position of the tab 210 of the cell 200.
[0023] In this embodiment, the aluminum-plastic film 100 is used for battery encapsulation. Specifically, in the actual production process, the battery cell 200 is prepared by winding or stacking the positive electrode sheet, separator, and negative electrode sheet. After the cell 200 is prepared, it needs to be encapsulated within the aluminum-plastic film 100.
[0024] The aluminum-plastic film 100 comprises a multilayered film, wherein "multilayered" means three or more layers. For example, in this embodiment, the aluminum-plastic film 100 comprises a three-layered film, namely a PP layer 110, an aluminum layer 120, and a nylon layer 130. Specifically, the PP layer 110, the aluminum layer 120, and the nylon layer 130 are arranged sequentially from the direction closest to the battery cell 200 to the direction furthest from the battery cell 200.
[0025] The PP layer 110, which is in direct contact with the battery cell 200, is made of polypropylene (PP). This material choice offers significant advantages: firstly, it imparts excellent resistance to electrolyte corrosion to the aluminum-plastic film 100, ensuring its long-term stability in the battery operating environment; secondly, it reduces internal stress caused by differences in the thermal expansion coefficients of the materials, thus contributing to the stability of the entire aluminum-plastic film 100 structure. It should be noted that in other embodiments, ethylene-acrylic acid copolymer (EAA) or other materials can also be used, as long as they provide corrosion resistance and sealing properties to the aluminum-plastic film 100; this application does not impose specific limitations here.
[0026] The aluminum layer 120 is made of aluminum, a material that gives it excellent barrier properties, effectively preventing the penetration of moisture, oxygen, and light. During actual battery use, this prevents the battery from becoming damp due to contact with moisture or undergoing oxidation due to contact with oxygen, thus ensuring battery performance and lifespan.
[0027] The nylon layer 130, located on the outermost layer of the aluminum-plastic film 100, possesses excellent abrasion and puncture resistance, providing reliable protection for the inner aluminum layer 120 during daily use and transportation, preventing scratches or tears. Furthermore, the nylon layer 130 enhances the impact resistance and ductility of the aluminum-plastic film 100, enabling it to better adapt to the various complex requirements of the battery encapsulation process and ensuring the integrity and reliability of the battery encapsulation.
[0028] It is important to note that, such as Figure 5As shown, in the structural design of the battery cell 200, one end is provided with a tab 210. When the battery cell 200 is installed inside the aluminum-plastic film 100 for encapsulation, the tab 210 is bent and ultimately pressed into the head region of the aluminum-plastic film 100. During this process, the tab 210 generates compression when bending at the head. This compression increases the space in the head region of the aluminum-plastic film 100, resulting in an increase in the overall size of the battery and a decrease in energy density. Furthermore, the tab 210 also exerts a compressive force on the electrode sheet during bending, which may damage the integrity of the electrode sheet structure and affect the battery's safety performance.
[0029] Furthermore, in the existing wound cell 200 structure, the tab 210 is typically welded to the central area of the electrode sheet. Since this location is surrounded by positive and negative active material layers, burrs are prone to form at the welding point of the tab 210. These burrs can easily puncture the separator between the positive and negative electrode sheets, leading to a short circuit. Therefore, to avoid short circuits, tab adhesive is usually applied to the tab 210 to cover the burrs and separate them from the separator. However, applying tab adhesive to the tab 210 increases its thickness, resulting in an overall increase in the thickness of the cell 200 and affecting the battery's energy density.
[0030] To address the aforementioned issues, the aluminum-plastic film 100 proposed in this application has a thinning area 140 corresponding to the tab 210 of the battery cell 200. This thinning area 140 is thinner than other parts of the aluminum-plastic film 100, thereby increasing the space inside the aluminum-plastic film 100 for placing the tab 210. This avoids the tab 210 being squeezed inside the aluminum-plastic film 100, which would cause the overall battery size to increase. It also avoids the safety issues that may be caused by the tab 210 squeezing the electrode sheet, thus optimizing the overall size, improving the energy density of the battery, and enhancing the safety performance of the battery.
[0031] In actual production, the thinning area 140 can be set on the PP layer 110 of the aluminum-plastic film 100 near the cell 200, or on the outermost nylon layer 130, or both the PP layer 110 and the nylon layer 130 can be thinned. The choice can be made freely according to the application scenario. Specifically, when the produced battery requires better impact resistance and ductility, such as... Figure 1 As shown, the thinning area 140 can be set only on the PP layer 110, and the nylon layer 130 can be left unthinned; when the produced battery requires better corrosion resistance and sealing performance, such as Figure 2 As shown, the thinning area 140 can be provided only on the nylon layer 130, while the PP layer 110 is not thinned; similarly, both the PP layer 110 and the nylon layer 130 can be thinned, such as... Figure 3As shown, compared to thinning only the PP layer 110 or the nylon layer 130, the overall thickness that needs to be thinned of the aluminum-plastic film 100 can be distributed across the PP layer 110 and the nylon layer 130. In this way, the impact on the individual thickness of the PP layer 110 or the individual thickness of the nylon layer 130 can be reduced, and the overall performance of the aluminum-plastic film 100 can be degraded due to excessive thinning of a single layer.
[0032] Please see Figure 1 In some embodiments, the PP layer 110 is provided with a first thinning region 111, the thickness of the PP layer 110 is 30um to 60um, and the depth of the first thinning region 111 is 10um to 40um.
[0033] In this embodiment, the thinning area 140 is only provided on the PP layer 110 of the aluminum-plastic film 100. The PP layer 110 is in contact with the battery cell 200, and a first thinning area 111 is provided at the position where the PP layer 110 contacts the tab 210 of the battery cell 200. In actual production, the thickness of the PP layer 110 is set in the range of 30µm to 60µm. For example, the thickness of the PP layer 110 can be set to different values such as 30µm, 45µm, and 60µm according to different design requirements. Specifically, if the thickness of the PP layer 110 is too large, it will cause the overall size of the battery to increase and reduce the energy density; if the thickness of the PP layer 110 is too small, it will cause the sealing performance of the aluminum-plastic film 100 to decrease. Setting the thickness of the PP layer 110 to 30µm is to avoid adversely affecting the sealing performance and corrosion resistance of the aluminum-plastic film 100; setting the thickness of the PP layer 110 to 60µm is to avoid reducing the overall energy density of the battery; setting the thickness of the PP layer 110 to 45µm can achieve a balance between battery energy density, sealing performance and corrosion resistance.
[0034] Furthermore, such as Figure 1As shown, the depth of the first thinning area 111 is denoted as h1, and the value of h1 is set in the range of 10um to 40um. For example, the depth of the first thinning area 111 can be set to 10um, 25um, and 40um. Specifically, the thickness of the thinning area 140 on the PP layer 110 is the thickness of the PP layer 110 minus the depth of the first thinning area 111. Therefore, if the depth of the first thinning area 111 is too large, the thickness of the thinning area 140 on the PP layer 110 will be too low, and the sealing performance and corrosion resistance of the thinning area 140 on the PP layer 110 cannot be guaranteed; if the depth of the first thinning area 111 is too small, the space for placing the tab 210 inside the aluminum-plastic film 100 cannot be increased. Taking a PP layer 110 thickness of 60µm as an example, if the depth of the first thinning area 111 is greater than 40µm, the thickness of the thinning area 140 on the PP layer 110 will be less than 20µm. This will lead to a decrease in the sealing performance and corrosion resistance of the PP layer 110 at this point, affecting safety performance. If the depth of the first thinning area 111 is less than 10µm, the thickness of the thinning area 140 on the PP layer 110 will be greater than 50µm, which is almost the same as not thinning at all, and cannot achieve the purpose of increasing the space inside the aluminum-plastic film 100 for placing the tab 210. Setting the depth of the first thinning area 111 to 25µm can increase the placement space for the tab 210 while ensuring battery safety performance.
[0035] This embodiment limits the thickness of the PP layer 110 to between 30µm and 60µm, and the thickness of the first thinning region 111 to between 10µm and 40µm. This ensures battery safety performance while increasing the space inside the aluminum-plastic film 100 for placing the tabs 210. It also prevents the tabs 210 from being squeezed inside the aluminum-plastic film 100, which would cause the overall battery size to increase. This optimizes the overall size and thus improves the energy density of the battery.
[0036] Please see Figure 4 In some embodiments, the inner wall of the first thinning region 111 is provided with an adhesive layer 112.
[0037] In some embodiments, the thickness of the adhesive layer 112 is 5 μm to 16 μm.
[0038] In some embodiments, the adhesive layer 112 is an adhesive tape applied to the first thinned area 111.
[0039] In this embodiment, an adhesive layer 112 is also provided within the first thinned area 111, and the adhesive layer 112 covers the inner wall of the first thinned area 111. The specific arrangement of the adhesive layer 112 can be flexibly selected; either a layer of glue can be applied to the first thinned area 111, or a layer of tape can be attached to the first thinned area 111. In actual implementation, the adhesive layer 112 should be evenly and smoothly adhered to the inner wall of the first thinned area 111. The main purpose of providing the adhesive layer 112 is to attach and fix the tab 210 inside the first thinned area 111 by means of the adhesive force of the adhesive layer 112.
[0040] Specifically, the thickness of the adhesive layer 112 is set within the range of 5µm to 16µm. For example, the thickness of the adhesive layer 112 can be set to different values such as 5µm, 10µm, and 16µm. Since the adhesive layer 112 is located within the first thinning area 111, if the thickness of the adhesive layer 112 is too large, the first thinning area 111 will be filled by the adhesive layer 112, and the thickness of the thinning area 140 on the PP layer 110 will be similar to that of other areas. This means that the aluminum-plastic film 100 has not been thinned at the tab 210, and the purpose of increasing the space inside the aluminum-plastic film 100 for placing the tab 210 cannot be achieved. If the thickness of the adhesive layer 112 is too low, on the one hand, it will increase the process difficulty in setting the adhesive layer 112. For example, in the operation of applying glue or sticking tape, the lower thickness requires higher operation precision, resulting in a decrease in yield and an increase in production costs. On the other hand, an adhesive layer 112 that is too thin will not provide sufficient adhesion strength, and the tab 210 may not be firmly adhered. Specifically, taking a thickness of 5µm for the adhesive layer 112 as an example, if it is less than 5µm, it will increase the difficulty of setting the adhesive layer 112 and may also affect the bonding strength. Taking a thickness of 16µm for the adhesive layer 112 as an example, if it is greater than 16µm, the adhesive layer 112 will be too thick, which will cause the thickness of the thinned area 140 on the PP layer 110 to be similar to the thickness of other areas, resulting in a limited increase in the space for placing the tab 210 inside the aluminum-plastic film 100. Taking a thickness of 10µm for the adhesive layer 112 as an example, the space for placing the tab 210 inside the aluminum-plastic film 100 can be increased while ensuring the bonding strength.
[0041] This embodiment limits the thickness of the adhesive layer 112 to between 5µm and 16µm, which increases the space for placing the tabs 210 inside the aluminum-plastic film 100 while reducing the difficulty of setting the adhesive layer 112 and ensuring the bonding strength. This allows the tabs 210 of the battery cell 200 to be fixed in the first thinning area 111 under the adhesive force of the adhesive layer 112, preventing the tabs 210 from shaking inside the aluminum-plastic film 100 and improving safety performance.
[0042] Please see Figure 2In some embodiments, the nylon layer 130 is provided with a second thinning region 131.
[0043] In some embodiments, the thickness of the nylon layer 130 is 15 μm to 25 μm.
[0044] In some embodiments, the depth of the second thinning region 131 is 10 μm to 20 μm.
[0045] In this embodiment, the thinning area 140 is only provided on the nylon layer 130 of the aluminum-plastic film 100. The nylon layer 130 is positioned away from the battery cell 200 and is located on the outermost layer of the aluminum-plastic film 100. A second thinning area 131 is provided at the position corresponding to the tab 210 of the battery cell 200 on the nylon layer 130. In actual production, the thickness of the nylon layer 130 is set in the range of 15µm to 25µm. For example, the thickness of the nylon layer 130 can be set to different values such as 15µm, 20µm, and 25µm according to different design requirements. If the thickness of the nylon layer 130 is too large, it will cause the overall size of the battery to increase and reduce the energy density; if the thickness of the nylon layer 130 is too small, it will cause the wear resistance of the aluminum-plastic film 100 to decrease, making it easy for the aluminum layer 120 inside the aluminum-plastic film 100 to be scratched or torn. Specifically, taking a nylon layer 130 thickness of 15µm as an example, if it is less than 15µm, the protective effect of the nylon layer 130 will be reduced, which will adversely affect the safety performance of the aluminum-plastic film 100. Taking a nylon layer 130 thickness of 25µm as an example, if it is greater than 25µm, it will increase the overall thickness of the aluminum-plastic film 100, which will indirectly increase the volume of the battery and reduce the energy density. Setting the thickness of the nylon layer 130 to 20µm can balance the battery energy density and the protective effect of the nylon layer 130.
[0046] Furthermore, such as Figure 2As shown, the depth of the second thinning region 131 is denoted as h2, and the value of h2 is set in the range of 10um to 20um. For example, the depth of the second thinning region 131 can be set to different values such as 10um, 15um, and 20um. Specifically, the thickness of the thinning region 140 on the nylon layer 130 is the thickness of the nylon layer 130 minus the depth of the second thinning region 131. Therefore, if the depth of the second thinning region 131 is too large, the thickness of the thinning region 140 on the nylon layer 130 will be too low, and the protective performance of the thinning region 140 on the nylon layer 130 cannot be ensured; if the depth of the second thinning region 131 is too small, the space for placing the tab 210 inside the aluminum-plastic film 100 cannot be increased. Taking a nylon layer 130 thickness of 25µm as an example, if the depth of the second thinning region 131 is greater than 20µm, the thickness of the thinning region 140 on the nylon layer 130 will be less than 5µm. This will reduce the protective performance of the nylon layer 130 at this point, making the aluminum layer 120 in the aluminum-plastic film 100 easily scratched or torn, affecting the overall safety performance of the battery. If the depth of the second thinning region 131 is less than 10µm, the thickness of the thinning region 140 on the nylon layer 130 will be greater than 15µm, which is almost the same as not thinning at all, and cannot achieve the purpose of increasing the space inside the aluminum-plastic film 100 for placing the tab 210. Setting the depth of the first thinning region 111 to 15µm can increase the placement space for the tab 210 while ensuring the battery's safety performance.
[0047] This embodiment limits the thickness of the nylon layer 130 to between 15µm and 25µm, and the thickness of the second thinning region 131 to between 10µm and 20µm. This allows for increased space inside the aluminum-plastic film 100 for placing the tabs 210 while ensuring battery safety. This prevents the tabs 210 from being squeezed inside the aluminum-plastic film 100, which would increase the overall size of the battery. This optimizes the overall size and thus improves the energy density of the battery.
[0048] This application also proposes an electrochemical device comprising the aforementioned battery cell 200 and the aforementioned aluminum-plastic film 100. The specific structure of the aluminum-plastic film 100 is as described in the above embodiments. Since this electrochemical device adopts all the technical solutions of all the above embodiments, it possesses at least all the technical effects brought about by the technical solutions of the above embodiments, which will not be elaborated here. In some embodiments, the battery cell 200 includes a positive electrode, a negative electrode, a separator, and tabs 210. The positive electrode includes a positive current collector and a positive active material layer, and the negative electrode includes a negative current collector and a negative active material layer. Tabs 210 are attached with tab adhesive at positions corresponding to the positive and negative electrode cells.
[0049] Specifically, such as Figure 5As shown, the electrochemical device is a battery, in which an aluminum-plastic film 100 is used to encapsulate a battery cell 200. One end of the battery cell 200 is also provided with a tab 210. When the battery cell 200 is inserted into the aluminum-plastic film 100, the position of the tab 210 corresponds to the thinned area 140 of the aluminum-plastic film 100. In this embodiment, the tab 210 is welded to the middle region of the positive and negative electrode plates. Since positive and negative active material layers are arranged around this location, burrs are easily generated at the welding position of the tab 210 during the cycling process of the battery cell 200. These burrs can easily puncture the separator between the positive and negative electrode plates, leading to a short circuit. To avoid short circuits, tab adhesive is usually pasted on the tab 210 to cover the burrs, thereby separating the burrs from the separator. However, the addition of tab adhesive increases the thickness of the tab 210, resulting in an increase in the overall thickness of the battery cell 200, which affects the battery energy density.
[0050] In summary, this application proposes an aluminum-plastic film 100 and an electrochemical device. By providing a thinning region 140 on the aluminum-plastic film 100, and with the position of the thinning region 140 corresponding to the position of the tab 210 of the battery cell 200, the placement space of the tab 210 within the aluminum-plastic film 100 is increased, thereby optimizing the overall size and improving the energy density. Furthermore, an adhesive layer 112 is provided on the thinning region 140, allowing the tab 210 of the battery cell 200 to be fixed to the thinning region 140 under the adhesive force of the adhesive layer 112, preventing the tab 210 from shaking within the aluminum-plastic film 100 and improving safety performance.
[0051] The above description is only a part or preferred embodiment of this application. Neither the text nor the drawings should limit the scope of protection of this application. All equivalent structural transformations made using the content of this application's specification and drawings under the overall concept of this application, or direct / indirect applications in other related technical fields, are included within the scope of protection of this application.
Claims
1. An aluminum laminate film for wrapping an electrode group, characterized by comprising: The aluminum-plastic film includes a PP layer close to the battery cell and a nylon layer facing away from the battery cell, with an aluminum layer disposed between the PP layer and the nylon layer; The PP layer and / or the nylon layer are provided with thinning areas, the positions of which correspond to the positions of the tabs of the battery cell.
2. The aluminum-plastic film according to claim 1, characterized in that, The PP layer has a first thinning zone, the thickness of the PP layer is 30um to 60um, and the depth of the first thinning zone is 10um to 40um.
3. The aluminum-plastic film according to claim 2, characterized in that, An adhesive layer is provided on the inner wall of the first thinning zone.
4. The aluminum-plastic film according to claim 3, characterized in that, The thickness of the adhesive layer is 5 μm to 16 μm.
5. The aluminum-plastic film according to claim 4, characterized in that, The adhesive layer is a tape applied to the first thinned area.
6. The aluminum-plastic film according to claim 1, characterized in that, The nylon layer has a second thinning zone.
7. The aluminum-plastic film according to claim 6, characterized in that, The thickness of the nylon layer is 15 μm to 25 μm.
8. The aluminum-plastic film according to claim 7, characterized in that, The depth of the second thinning zone is 10um to 20um.
9. An electrochemical device, comprising a battery cell and an aluminum-plastic film covering the battery cell, characterized in that, The aluminum-plastic film is the aluminum-plastic film as described in any one of claims 1 to 8.
10. The electrochemical device according to claim 9, characterized in that, The battery cell includes a positive electrode, a negative electrode, a separator, and tabs. The positive electrode includes a positive current collector and a positive active material layer. The negative electrode includes a negative current collector and a negative active material layer. Tabs are attached with tab adhesive at positions corresponding to the positive and negative electrode.