A novel sealing structure for expansion joints in glass melting furnaces
By using room-temperature pre-installed sealing bricks and hot-state replenishment of sealing material in glass melting furnaces, the problems of high-temperature construction difficulty and poor sealing reliability are solved, achieving convenient construction, reliable sealing and equipment stability, reducing operation and maintenance costs and extending equipment life.
Patent Information
- Application Number
- CN202522738516.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-24
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-12-24
AI Technical Summary
The existing sealing structure of the expansion joint of glass melting furnace has problems such as high construction difficulty and poor sealing reliability in high-temperature construction, resulting in unstable operation of melting furnace and high operation and maintenance costs.
The method of pre-installing sealing bricks at room temperature and filling with hot-applied sealant utilizes the self-adaptive expansion characteristics of the sealing bricks to achieve stability and ease of construction of the sealing structure.
Reduce the intensity of high-temperature construction, improve sealing quality and equipment operation stability, reduce operation and maintenance costs, extend equipment service life, and ensure the quality stability of glass products.
Smart Images

Figure CN224981504U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of glass melting furnace technology, specifically a novel sealing structure for the expansion joint of a glass melting furnace. Background Technology
[0002] As a core thermal equipment in the glass manufacturing industry, the glass melting furnace undertakes the critical tasks of high-temperature melting, clarification, and homogenization of glass raw materials. Its operational stability directly determines the quality, output, and economic efficiency of glass products. This equipment operates in an extremely harsh environment for extended periods: the internal temperature is continuously maintained above 1500℃, and it must withstand the erosion of molten glass, the scouring of high-temperature flue gas and dust, and the thermal stress impact generated by temperature fluctuations within the furnace. This places extremely high demands on the safety and sealing of the structural design.
[0003] The arch is a key component of a glass melting furnace, primarily used to construct the enclosed top structure of the furnace. The expansion joints at its joints are a core design element ensuring the structural safety of the arch. The core function of these expansion joints is to absorb the thermal expansion and contraction of the arch during temperature changes, releasing thermal stress by reserving space for deformation. This prevents serious structural failures such as cracking, detachment, or even collapse due to stress concentration, and is a crucial guarantee for the long-term safe operation of the melting furnace.
[0004] However, existing sealing technologies for expansion joints in glass melting furnaces still have significant shortcomings, such as... Figure 3 As shown, it is difficult to balance structural reliability and ease of construction: traditional sealing structures often adopt a "one-time high-temperature sealing" mode, requiring construction personnel to directly fill the expansion joints with sealing material after the furnace has been heated and is in a high-temperature working state. Due to the extremely high operating temperature, construction personnel must endure intense heat, resulting in not only high labor intensity but also difficulty in ensuring construction accuracy. Furthermore, the sealing quality is highly dependent on the experience and operational standards of the construction personnel. Problems such as sealing gaps and uneven filling caused by human factors occur frequently, easily leading to premature failure of the sealing structure, which in turn triggers a chain reaction of increased furnace hot repair frequency and increased operation and maintenance costs.
[0005] In summary, existing arch expansion joint sealing structures for glass melting furnaces suffer from problems such as high construction difficulty and poor sealing reliability, which restrict the operational stability and production economy of glass melting furnaces. Developing a new arch expansion joint sealing structure that can reduce the intensity of high-temperature construction and improve sealing reliability has become an urgent technical need for the glass production industry. Utility Model Content
[0006] The purpose of this invention is to provide a novel sealing structure for the expansion joint of a glass melting furnace, in order to solve the problems mentioned in the background art.
[0007] To achieve the above objectives, this utility model provides the following technical solution: a novel glass melting furnace arch expansion joint sealing structure, comprising a first arch body and a second arch body arranged opposite to each other, with an expansion joint formed between the first arch body and the second arch body; a first sealing brick and a second sealing brick are arranged at a lower position within the expansion joint; after the glass melting furnace is heated and sealed, the space between the first sealing brick and the second sealing brick within the expansion joint is filled with heat-applied sealant, and the upper part of the second sealing brick is entirely covered with heat-applied sealant.
[0008] Preferably, each of the first arch and the second arch has a stepped front body on the opposite side, and each of the adjacent sides of the front body has a first step and a second step. The first step and the second step are arranged opposite each other to form an expansion joint that is wider at the top and narrower at the bottom.
[0009] Preferably, the expansion joint includes a first expansion joint, a second expansion joint, and a third expansion joint, wherein the width of the first expansion joint is greater than that of the second expansion joint, and the width of the second expansion joint is greater than that of the third expansion joint.
[0010] Preferably, the first sealing brick is disposed within the second expansion joint, and the second sealing brick is disposed within the first expansion joint.
[0011] Preferably, the first sealing brick is a cylindrical brick, the second sealing brick is a straight brick, and the materials of the first sealing brick and the second sealing brick are the same as those of the first arch and the second arch, both being silica bricks.
[0012] Compared with the prior art, the beneficial effects of this utility model are as follows: The glass melting furnace arch expansion joint sealing structure of this utility model, through the process of "room temperature pre-installation + hot sealing", and the adaptive expansion characteristics of the cylindrical sealing brick during the heating process of the melting furnace arch, significantly reduces the intensity and time of high-temperature operations, improves construction efficiency and sealing quality stability; effectively reduces the frequency of melting furnace hot repairs and maintenance costs, extends equipment service life, and ensures the stability of glass product quality, while also having the advantages of convenient operation, strong adaptability, and significant economic benefits. Attached Figure Description
[0013] Figure 1 This is a schematic diagram of the structure of this utility model;
[0014] Figure 2 This is a schematic diagram of the structure of the first and second arches after preliminary installation of this utility model;
[0015] Figure 3 This is a common structure for traditional expansion joint seals.
[0016] In the figure: 1. First arch body; 11. Precursor body; 12. First step; 13. Second step; 2. Second arch body; 3. First sealing brick; 4. Second sealing brick; 5. Hot-applied sealant; 6. Expansion joint; 61. First expansion joint; 62. Second expansion joint; 63. Third expansion joint. Detailed Implementation
[0017] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.
[0018] Please see Figure 1 This utility model provides a technical solution: a novel glass melting furnace arch expansion joint sealing structure, including a first arch body 1 and a second arch body 2 arranged opposite to each other, forming an expansion joint 6 between the first arch body 1 and the second arch body 2; a first sealing brick 3 and a second sealing brick 4 are arranged at a lower position in the expansion joint; after the glass melting furnace is heated and sealed, the space between the first sealing brick 3 and the second sealing brick 4 in the expansion joint is filled with a heat-repairing sealant 5, and the upper part of the second sealing brick 4 is entirely covered with the heat-repairing sealant 5, which is a silica-based heat-repairing sealant.
[0019] In an embodiment of this utility model, a stepped front body 11 is provided on each side of the first arch body 1 and the second arch body 2, and a first step 12 and a second step 13 are provided on each side of the front body 11. The first step 12 and the second step 13 are arranged opposite each other to form an expansion joint 6 that is wider at the top and narrower at the bottom. In an embodiment of this utility model, the first sealing brick is a cylindrical brick, the second sealing brick is a straight brick, and both the first sealing brick and the second sealing brick are made of silica brick.
[0020] In an embodiment of this utility model, the expansion joint 6 includes a first expansion joint 61, a second expansion joint 62, and a third expansion joint 63. The width of the first expansion joint is greater than that of the second expansion joint, and the width of the second expansion joint is greater than that of the third expansion joint. The first expansion joint 61 and the third expansion joint 63 are provided with vertical sidewalls, and the second expansion joint 62 is provided with a sidewall with a 5° slope. The bottom end of the sidewall of the second expansion joint is provided with an arc surface, which can be adapted to the shape of the first sealing brick.
[0021] In an embodiment of this utility model, the first sealing brick is disposed within the second expansion joint, and the second sealing brick is disposed within the first expansion joint.
[0022] In embodiments of this invention, the first sealing brick is a cylindrical brick, and the second sealing brick is a straight brick. Furthermore, the materials of the first and second sealing bricks are the same as those of the first and second arches, both being silica bricks. This ensures a high degree of material compatibility between the sealing bricks and the arch, preventing chemical reactions under high-temperature conditions and avoiding sealing failure or structural corrosion due to material conflicts.
[0023] Please see Figure 2During construction, the first arch 1 and the second arch 2 are constructed first, with a large expansion joint left between them, meaning the two walls of the third expansion joint are not fitted together. Then, the first sealing brick is placed into the second expansion joint, with the gap in the third expansion joint smaller than the diameter of the first sealing brick to prevent it from falling into the third expansion joint. Next, the second sealing brick is placed into the first expansion joint. When the kiln begins to heat up, the first arch 1 and the second arch 2 expand as the temperature inside the kiln rises, reducing the distance between the expansion joints. After the arches stop expanding, the second sealing brick is temporarily removed, and hot-applied sealant 5 is filled into the second expansion joint. Then, the second sealing brick is placed back into the first expansion joint, and hot-applied sealant 5 is filled into the first expansion joint. Furthermore, to improve the sealing effect, the hot-applied sealant is piled up along the upper and outer sides of the first expansion joint, completely covering it.
[0024] Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the present invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A novel sealing structure for the expansion joint of a glass melting furnace, characterized in that, It includes a first arch (1) and a second arch (2) arranged opposite to each other, with an expansion joint (6) formed between the first arch (1) and the second arch (2); a first sealing brick (3) and a second sealing brick (4) are arranged at the lower position in the expansion joint; after the glass melting furnace is heated and sealed, the space between the first sealing brick (3) and the second sealing brick (4) in the expansion joint is filled with heat-repairing sealant (5), and the upper part of the second sealing brick (4) is completely covered with heat-repairing sealant (5).
2. The novel sealing structure for the expansion joint of a glass melting furnace according to claim 1, characterized in that: The first arch (1) and the second arch (2) are each provided with a stepped front body (11) on opposite sides. The front body (11) is provided with a first step (12) and a second step (13) on adjacent sides. The first step (12) and the second step (13) are arranged opposite each other to form an expansion joint (6) that is wider at the top and narrower at the bottom.
3. The novel sealing structure for the expansion joint of a glass melting furnace according to claim 2, characterized in that: The expansion joint (6) includes a first expansion joint (61), a second expansion joint (62) and a third expansion joint (63), wherein the width of the first expansion joint is greater than that of the second expansion joint, and the width of the second expansion joint is greater than that of the third expansion joint.
4. The novel sealing structure for the expansion joint of a glass melting furnace according to claim 3, characterized in that: The first sealing brick (3) is placed inside the second expansion joint, and the second sealing brick (4) is placed inside the first expansion joint.
5. The novel sealing structure for the expansion joint of a glass melting furnace according to claim 4, characterized in that: The first sealing brick is a cylindrical brick, the second sealing brick is a straight brick, and both the first and second sealing bricks, as well as the first and second arch bodies, are made of silica bricks.