Target material, magnetron sputtering electrode, and magnetron sputtering film forming apparatus

By increasing the thickness in the non-effective film-forming area of ​​the target, the problem of uneven target erosion was solved, the target utilization rate and lifespan were improved, and the process stability and equipment compatibility were maintained.

CN224981699UActive Publication Date: 2026-11-17CHENGDU TIANMA MICROELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522603898.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-08
Publication Date
2026-11-17
Estimated Expiration
2035-12-08

AI Technical Summary

Technical Problem

In existing magnetron sputtering film deposition technology, the utilization rate of the target material is low and the lifespan is short, mainly due to the uneven erosion of the target material at both ends caused by the movement of the magnet assembly.

Method used

By increasing the thickness of the non-effective film-forming area of ​​the target, a certain height difference is formed on the target surface, ensuring that the thickness of the effective film-forming area remains unchanged, maintaining the stability of the magnetic field and electric field distribution, and providing more sputtering material.

Benefits of technology

It significantly improves the utilization rate and extends the lifespan of the target material, while maintaining process stability and reducing production costs and equipment complexity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224981699U_ABST
    Figure CN224981699U_ABST
Patent Text Reader

Abstract

The application provides a target material, a magnetron sputtering electrode and a magnetron sputtering film forming device, and relates to the technical field of physical vapor deposition. The target material comprises a first area corresponding to an effective film forming guarantee area and a second area corresponding to a non-effective film forming area, wherein the second area is arranged around the first area or at both ends of the first area and close to the edges of the target material; and the target surface of the target material at a predetermined position of the second area is higher than the target surface of the target material in the first area. The target material provided by the application can balance the erosion proportion of each area of the target material due to uneven sputtering by freely adjusting and increasing the thickness of the second area, thereby improving the utilization rate of the target material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of physical vapor deposition technology, and in particular to a target, a magnetron sputtering electrode, and a magnetron sputtering film deposition apparatus. Background Technology

[0002] Magnetron sputtering is a physical vapor deposition technique widely used in fields such as displays to prepare various thin films with conductive, insulating, or protective functions. For example... Figure 35 As shown, this technology involves injecting a small amount of inert gas into a vacuum sputtering chamber 003 and applying an electric field to ionize it, thereby forming a plasma containing ionized gas particles and electrons. A magnet assembly 500 is positioned behind the target material 001. This assembly can reciprocate linearly along both ends of the target material 001, generating a magnetic field during the movement. This magnetic field confines electrons to the vicinity of the target material 001 surface, significantly increasing the plasma density. Under the influence of the electric field, the ionized gas particles are accelerated and bombard the surface of the target material 001, sputtering atoms or molecules from the target material 001 surface, which are then deposited on the substrate 400 to form a thin film.

[0003] However, as Figure 36 The target erosion curve shown illustrates that, due to the linear reciprocating motion of the magnet assembly 500, it needs to decelerate and pause at both ends of the target 001 before accelerating back. This results in a relatively longer residence time for the magnet assembly 500 at the ends of the target 001, leading to prolonged particle bombardment and more severe erosion in these areas. In contrast, the erosion in the central region of the target 001 is less severe. This uneven erosion distribution significantly shortens the target's lifespan and reduces its utilization rate.

[0004] Therefore, how to effectively improve the utilization rate of the target material and extend its lifespan has become an urgent technical problem to be solved. Utility Model Content

[0005] To address the aforementioned technical problem of how to improve the utilization rate of target materials, the first aspect of this application provides a target material, comprising:

[0006] The first region corresponds to the effective film formation guarantee region, and

[0007] The second region corresponds to the non-effective film-forming region. It is arranged around the first region or at both ends of the first region, close to the edge of the target material.

[0008] In this case, the target surface of the target material at the predetermined position in the second zone is higher than that of the target material in the first zone.

[0009] A second aspect of this application provides a magnetron sputtering electrode, comprising:

[0010] At least one magnet assembly, at least one backplate, and a target as provided in the first aspect of the embodiments of this application.

[0011] A third aspect of this application provides a magnetron sputtering film deposition apparatus, comprising:

[0012] The magnetron sputtering electrode provided in the second aspect of the embodiments of this application;

[0013] A vacuum sputtering chamber is used to provide a vacuum environment, and the magnetron sputtering electrodes are disposed in the vacuum sputtering chamber;

[0014] A substrate handling device, installed in a vacuum sputtering chamber, is used to handle and process substrates;

[0015] A gas introduction device is used to introduce gas into the vacuum sputtering chamber;

[0016] A sputtering power source for sputtering a target material as provided in the first aspect of the embodiments of this application.

[0017] The beneficial effects that the embodiments of this application can achieve are as follows:

[0018] This application increases the thickness of the second region of the target material, creating a certain height difference on the target surface. This structure allows the thicker portion of the target material to withstand a longer erosion time compared to the thinner portion, thereby promoting more uniform consumption of the target material as a whole, significantly improving the utilization rate of the target material, and effectively extending the service life of the target material.

[0019] Furthermore, the method for increasing the thickness of the second region of the target material provided in this application has good equipment compatibility and can be widely used in various magnetron sputtering film deposition equipment. The target material, magnetron sputtering electrode, and magnetron sputtering film deposition equipment provided in this application break through the limitations of the fixed and unadjustable target surface and step size in the stepped back plate of traditional planar targets, significantly improving the adaptability of target material design and process flexibility. Attached Figure Description

[0020] To more clearly illustrate the technical solutions in the embodiments of this application or the background art, the accompanying drawings used in the embodiments of this application or the background art will be described below.

[0021] Figure 1 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application, wherein the target material at the predetermined position is a right-angled stepped target material, and the back plate is a back plate with a constant cross section.

[0022] Figure 2 This illustration shows a schematic diagram of an optional target material disposed on a back plate according to an embodiment of this application, wherein the target material at a predetermined position is a gradient stepped target material, and the back plate is a back plate with a constant cross section.

[0023] Figure 3The diagram shows an optional target material disposed on a back plate according to an embodiment of this application. The target material at the predetermined position is a right-angled stepped target material, the back plate is a back plate with a constant cross section, and a gasket is also provided between the back plate and the target material.

[0024] Figure 4 This illustration shows a schematic diagram of an optional target material disposed on a back plate according to an embodiment of this application, wherein the target material at a predetermined position is a right-angled stepped target material, and the back plate is a stepped back plate.

[0025] Figure 5 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application. The target material at the predetermined position is a right-angled stepped target material, the back plate is a stepped back plate, and a gasket is also disposed between the back plate and the target material.

[0026] Figure 6 The illustration shows a schematic diagram of an optional target material disposed on a back plate according to an embodiment of this application, wherein the target material at a predetermined position in the second region of the target material is a right-angled stepped target material, the back plate is a stepped back plate, and its first part extends into the target material at the predetermined position.

[0027] Figure 7 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application, wherein the target material is a circular tube target material, the back plate is a circular tube with a constant cross section, and the target material at the predetermined position is a circular tube gradient step target material.

[0028] Figure 8 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application. The target material is a circular tube target material, the back plate is a circular tube with a uniform cross-section, the target material at a predetermined position is a circular tube gradient step target material, and a gasket is also disposed between the back plate and the target material.

[0029] Figure 9 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application, wherein the target material is a circular tube target material, the back plate is a circular tube stepped back plate, and the target material at a predetermined position is a circular tube gradient stepped target material.

[0030] Figure 10 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application. The back plate is a back plate with a uniform cross section, and the target material at the predetermined position is a right-angled stepped target material. The target material is integrally formed and disposed.

[0031] Figure 11 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application. The back plate is a back plate with a uniform cross section, the target material at the predetermined position is a right-angled stepped target material, and the target material in the first area is formed by splicing together multiple first target material units.

[0032] Figure 12 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application. The back plate is a stepped back plate, the target material at the predetermined position is a right-angled stepped target material, and the target material in the first and second regions is formed by splicing together multiple first target material units and multiple second target material units.

[0033] Figure 13 The diagram shows an optional target material disposed on a back plate according to an embodiment of this application. The back plate is a back plate with a uniform cross section, and the target material at the predetermined position is a right-angled stepped target material. The target material in the first region and the second region is formed by splicing together multiple first target material units and multiple second target material units.

[0034] Figure 14 The diagram shows a schematic representation of the structure of the second region of an optional target material provided in an embodiment of this application, wherein the target material at a predetermined position in the second region of the target material is a right-angled step target material.

[0035] Figure 15 This illustration shows a schematic diagram of the structure of the second region of an optional target material provided in an embodiment of this application, wherein the target material at a predetermined position in the second region of the target material is a rounded-corner stepped target material.

[0036] Figure 16 The diagram shows a schematic representation of the structure of the second region of an optional target material provided in an embodiment of this application, wherein the target material at a predetermined position in the second region of the target material is a target material with large rounded corners and a stepped shape.

[0037] Figure 17 The diagram shows a schematic of the structure of the second region of an optional target provided in an embodiment of this application, wherein the target at a predetermined position in the second region of the target is a gradient step target, and the distance between the predetermined position and the target extending from the first region is L1.

[0038] Figure 18 The diagram shows a schematic of the structure of the second region of an optional target provided in an embodiment of this application, wherein the target at a predetermined position in the second region of the target is a gradient step target, and the distance between the predetermined position and the target extending from the first region is L2.

[0039] Figure 19 The diagram shows a schematic of the structure of the second region of an optional target provided in an embodiment of this application, wherein the target at a predetermined position in the second region of the target is a gradient step target, and the gradient angle of the target at the predetermined position is θ1.

[0040] Figure 20The diagram shows a schematic of the structure of the second region of an optional target provided in an embodiment of this application, wherein the target at a predetermined position in the second region of the target is a gradient step target, and the gradient angle of the target at the predetermined position is θ2.

[0041] Figure 21 The diagram shows a schematic representation of the structure of the second region of an optional target material provided in an embodiment of this application, wherein the target material at a predetermined position in the second region of the target material is a curved stepped target material.

[0042] Figure 22 The diagram shows a top view of a magnetron sputtering electrode provided in an embodiment of this application, wherein the target is a square target, and the predetermined positions of the second region of the target are disposed at both ends of the target along a second direction.

[0043] Figure 23 The diagram shows a top view of a magnetron sputtering electrode provided in an embodiment of this application, wherein the target is a square target, and the predetermined positions of the second region of the target are disposed at both ends of the target along a first direction.

[0044] Figure 24 The diagram shows a top view of a magnetron sputtering electrode provided in an embodiment of this application, wherein the target is a square target and a predetermined position of the second region of the target is set around the edge of the target.

[0045] Figure 25 The diagram shows a top view of a magnetron sputtering electrode provided in an embodiment of this application, wherein the target is a square target and the predetermined positions of the second region of the target are located at the four corners of the target.

[0046] Figure 26 The diagram shows a top view of a magnetron sputtering electrode provided in an embodiment of this application, wherein the target is a circular target and a predetermined position of the second region of the target is set around the edge of the target.

[0047] Figure 27 The diagram shows a top view of a magnetron sputtering electrode provided in an embodiment of this application, wherein the target is a strip-shaped target, and the predetermined positions of the second region of the target are disposed at both ends of the target along a second direction.

[0048] Figure 28 The diagram shows a top view of a magnetron sputtering electrode with at least two target components integrated internally, according to an embodiment of this application. The target is a strip-shaped target, and the predetermined positions of the second region of the target are disposed at both ends of the target along a second direction.

[0049] Figure 29 The diagram shows a top view of a magnetron sputtering electrode provided in an embodiment of this application, wherein the target is a cylindrical target, and predetermined positions of the second region of the target are disposed at both ends of the target along a second direction.

[0050] Figure 30 The diagram shows a top view of a magnetron sputtering electrode with at least two target components integrated internally, provided by an embodiment of this application. The target is a cylindrical target, and predetermined positions of the second region of the target are disposed at both ends of the target along a second direction.

[0051] Figure 31 The diagram shows a cross-sectional view of a circular tube target at a predetermined position according to an embodiment of this application, wherein the back plate is a uniform cross-section back plate.

[0052] Figure 32 The diagram shows a cross-sectional view of a circular tube target in the first region according to an embodiment of this application, wherein the back plate is a uniform cross-section back plate.

[0053] Figure 33 The diagram shows a cross-sectional view of a circular tube target in the first region according to an embodiment of this application. The back plate is a uniform cross-section back plate, and a gasket is provided between the back plate and the target.

[0054] Figure 34 The diagram shows a cross-sectional view of a circular tube target in the first region according to an embodiment of this application, wherein the back plate is a stepped back plate.

[0055] Figure 35 A cross-sectional view of the structure of a magnetron sputtering electrode in the prior art is shown;

[0056] Figure 36 The erosion distribution curve of the target material is shown;

[0057] Figure 37 This diagram illustrates a structure in the prior art where the target material is disposed on a backplate.

[0058] Figure 38 This diagram illustrates another structural design in the prior art where the target material is mounted on a backplate.

[0059] Figure 39 A top view of the structure of a magnetron sputtering electrode in the prior art is shown.

[0060] Marked in the image:

[0061] 001: Target material in the background art; 002: Target material backing plate in the background art; 003: Vacuum sputtering chamber in the background art;

[0062] 100: Target material, 110: Zone 1, 120: Zone 2, 121: Designated position;

[0063] 210: Uniform cross-section back plate; 220: Stepped back plate; 221: First part; 222: Second part;

[0064] 300: Gasket;

[0065] 400: Substrate; 410: Effective film formation guarantee area; 420: Ineffective film formation area;

[0066] 500: Magnet assembly;

[0067] a: Target thickness set under the flat backplate; b: Target thickness at the predetermined position; c: Target thickness when the shim is set on the flat backplate; d: Target thickness set under the stepped backplate; e: Target thickness when the shim is set on the stepped backplate. Detailed Implementation

[0068] In the following description, exemplary embodiments will be illustrated in more detail with reference to the accompanying drawings, wherein the same reference numerals denote the same elements throughout the drawings. However, this application may be embodied in a variety of different forms and should not be considered as limited to the embodiments shown herein. Rather, these embodiments are provided as examples so that this application will be sufficient and complete, and will fully convey to those skilled in the art the aspects and features of this application. Therefore, processes, elements, and techniques that are not essential for a complete understanding of the aspects and features of this application may not be described to those skilled in the art. Unless otherwise stated, the same reference numerals denote the same elements throughout the drawings and written description, and therefore their description will not be repeated. In the figures, the relative dimensions of elements, layers, and regions may be exaggerated for clarity.

[0069] It will be understood that while the terms “first,” “second,” etc., may be used herein to describe various elements, components, regions, layers, and / or parts, these elements, components, regions, layers, and / or parts should not be limited by these terms.

[0070] It will be understood that when an element or layer is referred to as being “between” two elements or two layers, it can be the only element or the only layer between the two elements or two layers, or there can be one or more intermediate elements or intermediate layers.

[0071] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of this application. As used herein, the singular forms “a,” “an,” and “the” are intended to include the plural forms as well, unless otherwise expressly stated. It will be further understood that, when used in this specification, the terms “comprising” and “including” indicate the presence of stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof.

[0072] To make the technical problems solved by this application, the technical solutions adopted, and the technical effects achieved clearer, the technical solutions of the embodiments of this application will be further described in detail below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments.

[0073] Of course, the definition of the effective film-forming area and the ineffective film-forming area described in this application is not strictly limited. In some applications, the first and second regions of the target material act together on the substrate under the action of an electromagnetic field to achieve a certain coating purpose.

[0074] For ease of description, in the embodiments of this application, the target portion corresponding to the effective film formation guarantee area of ​​the substrate is defined as the effective target area, and the target portion corresponding to the ineffective film formation area of ​​the substrate is defined as the ineffective target area. Figure 37 As shown, one existing improvement involves placing a spacer between the effective area of ​​the target and the planar backing plate. Another solution is as follows... Figure 38 As shown, a boss structure is machined into the flat back plate used to support the effective area of ​​the target. Both solutions aim to ensure that the surface of the target closest to the substrate remains a smooth plane while keeping the distance between the magnet assembly and the target surface, as well as the distance between the effective area of ​​the target and the substrate, unchanged. This avoids fluctuations in product process performance caused by changes in the aforementioned distances, ultimately making the thickness of the effective area of ​​the target smaller than the thickness of the non-effective area, reducing target residue, and thus improving target utilization.

[0075] However, both of the above solutions have certain limitations. For Figure 37 The gasket design shown has two main drawbacks. First, the introduction of the gasket alters the distance between the target surface and the substrate, as well as the distance between the target surface and the magnet assembly. This significantly changes the distribution and intensity of the magnetic and electric fields in the affected areas, thus impacting plasma density and distribution characteristics, and consequently negatively affecting the stability of the sputtering process. Second, the introduction of the gasket significantly increases the thermal resistance between the target and the cooling water of the planar backplate, leading to an increase in the operating temperature of the target during sputtering and raising the risk of target cracking. Furthermore, the gasket requires regular maintenance and replacement, further increasing the complexity and cost of equipment operation.

[0076] for Figure 38 The backplate boss solution shown eliminates the need for gaskets, reducing additional costs and maintenance requirements. However, because this solution directly alters the hardware structure, it lacks flexibility from the design stage. The boss structure fixes the shape of the effective area of ​​the target material, limiting its adaptability to targets of different thicknesses or splicing methods. Therefore, it imposes limitations on equipment design and initial process debugging, making it difficult to adapt to the application requirements of multiple target material specifications.

[0077] To address the aforementioned shortcomings, this application provides a target material that improves target utilization and process stability by increasing the thickness of the non-effective region of the target while maintaining the distance between the target surface and the substrate, as well as the distance between the target surface and the magnet assembly. This is achieved without introducing additional spacers or altering the backplate structure. Firstly, because the distance between the target surface and the substrate, and between the target surface and the magnet assembly, remains constant, the corresponding magnetic field distribution and electric field strength maintain their original characteristics, thus ensuring process stability. Simultaneously, increasing the thickness of the non-effective region allows for greater sputtering etching of the non-effective region, significantly reducing target residue and improving target utilization and extending the overall lifespan. Secondly, this solution eliminates the need for spacers or bosses, reducing thermal resistance and avoiding the complexity and high cost associated with additional components. Furthermore, since no hardware modifications are required, the target material provided in this application has excellent versatility and adaptability, meeting the requirements of various existing magnetron sputtering equipment, making target splicing and thickness design more flexible and suitable for diverse process scenarios.

[0078] The following is a detailed description of a target material provided in the embodiments of this application, such as... Figure 1 and Figure 2 As shown.

[0079] The first aspect of this application provides a target 100, comprising:

[0080] The first zone 110 corresponds to the effective film formation guarantee zone 410, and

[0081] The second region 120 corresponds to the non-effective film-forming region 420. The second region 120 is disposed around the first region 110, or disposed at both ends of the first region 110, close to the edge of the target material 100.

[0082] In this case, the surface of the target material at the predetermined position 121 in the second region 120 is higher than the target surface of the target material in the first region 110.

[0083] It should be understood that in magnetron sputtering, the effective film-forming guarantee zone refers to the portion of the substrate area on the target surface directly opposite it where a thin film meeting the requirements for quality, thickness, and uniformity can be formed. This zone corresponds to the actual film-forming area on the substrate and is the effective range for sputtering deposition. Figure 35 The diagram shows the location of the effective film formation guarantee area 410. Conversely, the ineffective film formation area refers to the portion of the target material corresponding to the outer periphery of the substrate or the non-deposition area, where sputtered particles cannot be effectively deposited on the substrate 400.

[0084] In this embodiment, the first region 110 of the target material corresponds to the effective film formation guarantee region 410 on the substrate 400. This region is the main area for material deposition during sputtering, where sputtered particles can deposit on the substrate surface with high utilization and uniformity to form a thin film that meets the requirements. The second region 120 of the target material corresponds to the non-effective film formation region 420, where sputtered particles cannot effectively form a film on the substrate. Its main design purpose is to ensure that the thin film generated in the first region 110 meets the process requirements in terms of overall area and edge uniformity, thereby ensuring the area of ​​the effective film formation guarantee region, maintaining process stability, and improving the overall utilization rate of the target material.

[0085] In some embodiments, the target 100 is rectangular, and its cross-sectional structure can be referenced. Figure 1 and Figure 2 In this embodiment, the target surface at a predetermined position 121 of the second region 120 of the target material is set higher than the target surface of the first region 110. That is, the target material provided in this embodiment significantly increases the thickness of the second region 120, rather than changing the original thickness of the first region 110, thereby maintaining the thickness and surface morphology of the first region 110. This ensures that the distance between the target surface of the first region 110 and the substrate 400, and the distance between the target surface of the first region 110 and the magnet assembly 500 remain unchanged, thus ensuring that the electric and magnetic field distribution above this region is not distorted and maintaining plasma stability. Simultaneously, the increased thickness of the second region 120 provides more sufficient material for the sputtering process, enabling deeper sputtering etching, significantly reducing target residue in the first region 110, fundamentally improving the utilization rate of the target 100, and further extending the lifespan of the target 100.

[0086] In summary, the target 100 provided in this application embodiment abandons the practice of setting a gasket or boss structure between the target 100 and the back plate. This not only avoids the increase in thermal resistance caused by introducing additional structures, but also gets rid of the dependence on a specific back plate structure, breaking through the inherent limitation that its step height is fixed and cannot be adjusted.

[0087] In one specific embodiment, the thickness of the target material in the second region 120 provided in this application is set to 1.5 times the thickness of the target material in the first region 110. Actual test results show that, under the same conditions, the service life of the target material 100 is correspondingly extended to 1.5 times, and the utilization rate of the target material can be increased to over 50%, effectively reducing production costs and extending the service life of the target material.

[0088] In some embodiments, such as Figure 1The target cross-section diagram shown has a uniform cross-section backplate 210. The target material at the predetermined position 121 in the second region 120 is a right-angled stepped target, meaning the thickness of the predetermined position 121 in the second region 120 is uniform from the boundary to the edge, forming a vertical step with the non-predetermined position in the second region 120. The thickness of the first region 110 is denoted as 'a', and the thickness of the predetermined position 121 in the second region 120 is denoted as 'b', with 'b' greater than 'a', to ensure sufficient target material for the sputtering process. The target material at the non-predetermined position in the second region 120 is distributed on both sides of the first region 110 and is integrally formed with the first region 110. In this embodiment, the predetermined position 121 is rectangular, allowing for direct forming through a simple process, significantly reducing manufacturing costs and cycle time. Simultaneously, the uniform thickness ensures more balanced internal stress in the target material, reducing edge cracks caused by stress concentration and improving the overall mechanical strength and reliability of the structure.

[0089] In other embodiments, such as Figure 2 The target cross-sectional diagram shown illustrates a gradient stepped target located at a predetermined position 121 in the second region 120. This means the thickness of the target at the predetermined position 121 gradually increases from the boundary with the non-predetermined position of the second region 120 towards the edge, and continues to extend towards the edge at a predetermined point while maintaining a constant thickness, ultimately presenting a trapezoidal cross-section. The thickness of the first region 110 is denoted as 'a', and the thickness of the predetermined position 121 is denoted as 'b', where b is greater than a. The target thickness in the sloping region of the predetermined position 121 continuously transitions from 'a' to 'b' to ensure sufficient target material for the sputtering process. In one embodiment, the non-predetermined positions of the second region 120 are distributed on both sides of the first region 110. A portion of this portion is integrally formed with the target material of the first region 110, and another portion is integrally formed with the target material of the predetermined position 121, with the thickness of this portion being consistent with the target thickness of the first region 110.

[0090] It should be understood that the magnet assembly 500 spends the longest time at both ends of the target 100. As the magnet assembly 500 decelerates towards both ends, the erosion of the target in the corresponding areas gradually deepens. Therefore, setting the predetermined position 121 to a trapezoidal shape better suits the movement trajectory of the magnet assembly 500, thereby reducing the production cost of the target to some extent and achieving higher target utilization. Simultaneously, the trapezoidal second region 120 provides a gradual transition zone for the plasma, avoiding electric field distortion and localized plasma concentration or weakening that may occur at the steep rectangular steps, ultimately improving process stability and thin film quality.

[0091] The target material provided in this application embodiment can also be applied to magnetron sputtering electrodes with other hardware structures, exhibiting good compatibility and scalability.

[0092] In some embodiments, such as Figure 3 , Figure 5 and Figure 8 The diagram shows a cross-sectional view of a target material, wherein a gasket 300 is provided between the first region 110 of the target material and the portion of the first region 110 extending into the second region 120 of the target material and the back plate.

[0093] In one specific embodiment, such as Figure 3 As shown, the thickness of the first region 110 of the target material is c, and the sum of the thicknesses of the first region 110 and the spacer 300 is a, which is consistent with the thickness of the first region 110 in the above embodiment, to ensure that the distance between the target surface of the first region 110 and the substrate 400, and the distance between the target surface of the first region 110 and the magnet assembly 500 remain unchanged. When the target material at the predetermined position 121 is a right-angled stepped target material, the target material thickness at the predetermined position 121 of the second region 120 of the target material is b, and b is greater than a and greater than c. When the target material at the predetermined position 121 is a gradient stepped target material, the target material thickness at the predetermined position 121 increases from a to b.

[0094] In another specific embodiment, such as Figure 5 As shown, the thickness of the first region 110 of the target material is e, the total thickness of the first region 110 and the spacer 300 is d, and the total thickness of the first region 110, the spacer 300, and the boss structure of the back plate is a. This total thickness is consistent with the thickness a of the first region 110 in the above embodiment, to ensure that the distance between the target surface of the first region 110 and the substrate 400, and the distance between the target surface of the first region 110 and the magnet assembly 500 remain unchanged. When the target material at the predetermined position 121 is a right-angled stepped target material, the target material thickness at the predetermined position 121 of the second region 120 of the target material is b, and b is greater than a, greater than d, and greater than e. When the target material at the predetermined position 121 is a gradient stepped target material, the target material thickness at the predetermined position 121 increases from a to b.

[0095] In another specific embodiment, such as Figure 8 As shown, the thickness of the first region 110 of the target material disposed around the edge of the back plate is c, and the total thickness of the first region 110 and the pad 300 is a, which is consistent with the thickness of the first region 110 target material in the above embodiment, so as to ensure that the distance between the target material surface of the first region 110 and the substrate 400, and the distance between the target material surface of the first region 110 and the magnet assembly 500 remain unchanged. When the target material at the predetermined position 121 is a right-angled stepped target material, the target material thickness at the predetermined position 121 of the second region 120 of the target material is b, and b is greater than a and greater than c. When the target material at the predetermined position 121 is a gradient stepped target material, the target material thickness at the predetermined position 121 increases from a to b.

[0096] To further enhance compatibility with equipment, the non-uniform thickness target 100 provided in this application embodiment can also be adapted to the stepped back plate 220 with a boss structure. Its core design principle is still to keep the target surface position of the first region 110 constant to ensure that the critical plasma process spacing remains unchanged.

[0097] In one specific embodiment, such as Figure 4 As shown, the target thickness in the first region 110 is d, and the total thickness of the target and the boss structure in the first region 110 is a, to ensure that the distance between the target surface in the first region 110 and the substrate 400, and the distance between the target surface in the first region 110 and the magnet assembly 500 remain unchanged. When the target at the predetermined position 121 is a right-angled stepped target, the target thickness at the predetermined position 121 in the second region 120 of the target is b, and b is greater than a and greater than d. This relationship ensures that the target at the predetermined position 121 can provide sufficient material. When the target at the predetermined position 121 is a gradient stepped target, the target thickness at the predetermined position 121 increases from a to b.

[0098] In another specific embodiment, such as Figure 9 As shown, the target material of the first region 110 is arranged around the edge of the back plate. The thickness of the target material in the first region 110 is d, and the sum of the thicknesses of the target material in the first region 110 and the boss structure is a, to ensure that the distance between the target material surface of the first region 110 and the substrate 400, and the distance between the target material surface of the first region 110 and the magnet assembly 500 remain unchanged. When the target material at the predetermined position 121 is a right-angled stepped target material, the target material thickness at the predetermined position 121 of the second region 120 of the target material is b, and b is greater than a and greater than d. This relationship ensures that the target material at the predetermined position 121 can provide sufficient material. When the target material at the predetermined position 121 is a gradient stepped target material, the target material thickness at the predetermined position 121 increases from a to b.

[0099] In some embodiments, such as Figures 14 to 21 As shown, the target material located at the predetermined position 121 in the second region 120 includes one or more of the following: right-angle step target material, rounded-corner step target material, gradient step target material and / or curved step target material. In the embodiments of this application, each configuration has its own characteristics in terms of processability, electric and magnetic field stability and mechanical reliability.

[0100] In one specific embodiment, a right-angled stepped target material, such as Figure 14 As shown, the target material at the predetermined position 121 has a rectangular cross-section structure and can be integrally formed with the target material at other positions or manufactured using a splicing process. In this embodiment, the advantage of the right-angled stepped target material is that it has a simple structure, intuitive design, and low processing cost, and it is easier to determine the thickness and width of the target material at the predetermined position 121 based on the target material's erosion curve data.

[0101] In one specific embodiment, such as Figure 15 and Figure 16 The target material with rounded corners shown in this embodiment has a rounded or large rounded corner transition area compared to a right-angled step target material configuration. The rounded corner design effectively suppresses arc discharge, thereby improving the yield and quality of the thin film. Furthermore, the rounded corners effectively alleviate localized stress concentration, resulting in a more uniform stress distribution at the predetermined position 121 during use. This improves the structural reliability of the target material at position 121, reduces the risk of cracking, and further enhances the utilization rate of the target material.

[0102] In one specific embodiment, such as... Figures 17 to 20 The gradient-step target shown has a trapezoidal cross-section at the predetermined position 121, offering high design flexibility. In this embodiment, key design parameters of the gradient-step target include the length L (L2 greater than L1) from the boundary between the predetermined position 121 and the non-predetermined position of the second region 120 to the boundary between the non-predetermined position of the second region 120 and the boundary where the first region target extends into the second region 120, and the inclination angle of the slope (i.e., the gradient angle θ). This means that the erosion distribution of the target can be controlled by rationally designing the gradient angle θ and the length L. Specifically, a larger gradient angle θ1 makes the step transition steeper, thus tending towards the characteristics of a right-angled step. A smaller gradient angle θ2 makes the step transition gentler, tending towards the characteristics of a curved step. Therefore, the gradient-step target can achieve an optimal balance between manufacturing cost and overall performance, adapting to different erosion rates and erosion distribution requirements.

[0103] In one specific embodiment, such as Figure 21 The curved stepped target shown achieves a smooth transition between the predetermined position 121 and the non-predetermined position. Since the smooth surface minimizes interference with the plasma, the curved stepped target in this embodiment ensures the most uniform and stable magnetic and electric field distribution. Furthermore, because the curved stepped target completely eliminates sharp corners and edges, it fundamentally avoids electric field concentration problems caused by geometry, making it particularly suitable for process environments requiring high electric field uniformity.

[0104] In summary, the embodiments of this application provide a variety of stepped target material configurations, enabling the flexible selection of the most suitable target material structure based on specific process requirements, cost budgets, and performance indicators during product manufacturing, thereby achieving process optimization and efficient resource utilization.

[0105] In some embodiments, such as Figure 10As shown, the target 100 is integrally formed. In this embodiment, the integrally formed target avoids splicing seams, thus the target 100 has higher mechanical strength and rigidity. During installation and sputtering, the integrally formed target can more effectively withstand the backplate stress, thereby exhibiting excellent resistance to deformation and damage, significantly improving the reliability and service life of the target.

[0106] In some embodiments, such as Figures 1 to 9 As shown, the target material in the first zone 110 extends into the second zone 120 and is joined to the target material at a predetermined position 121 in the second zone 120 via a splicing process, or spliced ​​to a portion of a non-predetermined position in the second zone 120. Specifically, a joint treatment process is used at the step difference of the splicing steps, i.e., splicing is achieved by transitioning to a uniform surface through a stepped slope. This design minimizes interference with plasma uniformity caused by the presence of joints, thereby significantly improving the utilization rate of the target material and the product yield without affecting the product process and quality.

[0107] In some embodiments, such as Figures 11 to 13 As shown, the target 100 can be further designed with a modular multi-unit splicing mechanism. Specifically, the target in the first region 110 includes multiple first target units, which are formed by splicing together the first target units. And / or, the target in the second region 120 includes multiple second target units, which are formed by splicing together the second target units. This modular design significantly improves the overall flexibility of target application, facilitating not only the manufacture of large targets but also allowing for targeted replacement of target units based on the actual erosion distribution, thereby improving target utilization and reducing overall process costs.

[0108] Furthermore, the spliced ​​target design makes it easier to achieve complex shapes and thickness combinations. The thickness of each region of the spliced ​​target can be adjusted according to magnetic flux uniformity and the target erosion surface, thus demonstrating good target structural flexibility and improving target utilization. When the predetermined position 121 of the first region 110 or the second region 120 of the target is completely etched away during the splicing process, only the local part can be replaced without replacing the entire target, further reducing the overall product cost.

[0109] In some embodiments, along the width direction of the predetermined position 121 of the second region 120, the size of the effective film formation guarantee region 410 is inversely proportional to the width of the predetermined position 121. Specifically, as Figures 22 to 34The top view of the magnetron sputtering electrode structure shown indicates that the first region 110 of the target is located in the central region of the back plate 200, and the second region 120 of the target is located around the first region 110. With the overall size of the target 100 fixed, the larger the size of the effective film formation guarantee region 410, the smaller the width of the predetermined position 121 of the second region 120.

[0110] In one specific embodiment, such as Figure 22 As shown, when the size of the effective film-forming guarantee region 410 increases in the second direction, the size of the corresponding first region 110 in the second direction also increases accordingly. At this time, the width of the target material located at the predetermined position 121 decreases accordingly, thereby matching the geometric requirements of the effective film-forming guarantee region 410, so as to ensure that the film thickness uniformity and film quality in the effective film-forming guarantee region 410 meet the process requirements.

[0111] In one specific embodiment, such as Figure 23 As shown, when the size of the effective film-forming guarantee region 410 increases in the first direction, the size of the corresponding first region 110 in the first direction also increases accordingly. At this time, the width of the target material located at the predetermined position 121 decreases accordingly, thereby matching the geometric requirements of the effective film-forming guarantee region 410, so as to ensure that the film thickness uniformity and film quality in the effective film-forming guarantee region 410 meet the process requirements.

[0112] In one specific embodiment, such as Figure 24 As shown, when the size of the effective film-forming guarantee region 410 increases in the first direction and / or the second direction, the size of its corresponding first region 110 also increases accordingly in the first direction and / or the second direction. At this time, the width of the target material surrounding the predetermined position 121 disposed on the inner edge of the target material 100 decreases accordingly to ensure that the film thickness uniformity and film quality within the effective film-forming guarantee region 410 meet the process requirements.

[0113] In one specific embodiment, such as Figure 25 As shown, when the size of the effective film-forming guarantee area 410 increases in the first direction and / or the second direction, the size of its corresponding first area 110 also increases accordingly in the first direction and / or the second direction. At this time, the width of the target material disposed at the predetermined positions 121 at the four corners of the target material 100 decreases accordingly to ensure that the film thickness uniformity and film quality within the effective film-forming guarantee area 410 meet the process requirements.

[0114] In some embodiments, the width of the target material located at the predetermined position 121 is proportional to the erosion area of ​​the second region 120. Specifically, as... Figure 36The target erosion surface diagram shown clearly indicates that the erosion depth at both ends of the target is significantly greater than that at the center, indicating a higher target consumption rate in this region. To ensure uniform erosion and improve target utilization, this embodiment employs a thicker target structure in areas with more severe erosion; specifically, the target at predetermined position 121 requires a wider design. Therefore, the determination of the target width at this position directly depends on the erosion distribution exhibited by the second region 120 during sputtering.

[0115] In some embodiments, the target thickness at a predetermined position 121 within the second region 120 can also be designed specifically according to the target erosion curve. That is, the more severe the target erosion, the thicker the target at the predetermined position 121 within the second region 120, which further saves process costs.

[0116] In some embodiments, this application provides a variety of target surface shapes for the target material 100, including rectangular, circular, and strip shapes, to adapt to different processes and film formation requirements. The predetermined positions 121 of the second region 120 can be precisely configured according to the actual erosion distribution and erosion rate, and can all utilize one or more configurations of the aforementioned right-angled step target material, rounded-corner step target material, gradient step target material, and / or curved step target material, thereby achieving performance optimization.

[0117] In one specific embodiment, such as Figures 22 to 25 As shown, the target surface of the target 100 in this embodiment is rectangular. The predetermined position 121 can be located at either end of the target 100, at one of the four corners, or around the edge of the target 100. This embodiment does not explicitly limit the predetermined position 121; it can be located in other positions. Specifically, the predetermined position 121 in this application can be precisely set according to the erosion distribution of the target to maximize target utilization and film uniformity.

[0118] In one specific embodiment, such as Figure 26 As shown, the target surface of the target 100 in this embodiment is circular. Specifically, the target material at predetermined position 121 in the second region 120 is arranged in a ring or segmented ring around the center of the target 100. This design fully conforms to the typical ring erosion characteristics of a circular target during sputtering, contributing to significant film thickness uniformity on a circular substrate.

[0119] In one specific embodiment, such as Figures 27 to 30As shown, the target 100 includes at least one target component, the target surface of its first region 110 is strip-shaped, and the second region 120 is disposed at both ends of the target 100 along its length, with the first region 110 disposed between the second region 120; wherein, at least one target component is arranged along the width direction of the first region 110. This target structure design can effectively compensate for end effects, thereby improving the target utilization rate.

[0120] Specifically, the strip-shaped target material in this embodiment has a high aspect ratio, and its width (in the first direction) is much smaller than the width (in the first direction) of the square target material in the above embodiment. Since the width of the strip-shaped target material in the first direction is limited, when the effective film formation guarantee area 410 and the strip-shaped target material are in a relatively static state, the first area 110 cannot completely cover the effective film formation guarantee area 410, that is, it cannot guarantee the formation of a complete film on the effective film formation guarantee area 410.

[0121] Therefore, in a specific embodiment, such as Figure 27 and Figure 29 As shown, when there is a non-overlapping area between the first region 110 of the target component and the effective film formation guarantee region 410, full-area film formation inside the effective film formation guarantee region 410 can be achieved by introducing a relative scanning motion along the first direction, including: the substrate 400 is translated along the first direction, or the back plate 400 and the target 100 fixed thereon are translated along the first direction as a whole, so as to ensure that each area in the effective film formation guarantee region 410 can receive the sputtered particle stream, thereby forming a continuous and uniform thin film on the entire substrate.

[0122] In one specific embodiment, such as Figure 28 and Figure 30 As shown, when the first region 110 of the target component can cover the effective film formation guarantee region 410, the target component and the effective film formation guarantee region 410 remain relatively stationary, so that the projection of the effective film formation guarantee region 410 is always located on the first region 110 among all the target components. At this time, keeping the substrate 400 and the target component relatively stationary ensures that a continuous and uniform thin film can be formed on the substrate 400.

[0123] In one specific embodiment, when the projection of the effective film-forming guarantee region 410 is located within the entire range of the target components other than the first region, the effective film-forming region 410 can also maintain relative movement with each target component within the entire range of the target components. For example, the substrate 400 reciprocates along the length or width direction of the target within the entire range of the target components.

[0124] The above embodiments, by employing a strip-shaped target material in conjunction with the effective film formation guarantee region 410 in a design that allows for relative movement, not only meet the film formation requirements of large-size substrates but also significantly improve the utilization rate of the target material. Furthermore, in practical applications, one or more combinations of the solutions provided in the above specific embodiments can be used to achieve the formation of a continuous and uniform thin film on the entire substrate.

[0125] In some embodiments, such as Figures 27 to 30 As shown, the target component includes one or more of a strip target component or a circular tube target component; wherein the outer diameter of the predetermined position 121 of the second region of the circular tube target component is larger than the outer diameter of the first region 110 of the circular tube target component.

[0126] In one specific embodiment, such as Figure 27 and Figure 28 As shown, the target component is a strip-shaped target component. The second region 120 is located at both ends along the length of the strip-shaped target component, and the first region 110 is located between the second regions 120. The strip-shaped target component has a high aspect ratio, and its width (in the first direction) is much smaller than the width (in the first direction) of the square target in the above embodiment. In this embodiment, at least one strip-shaped target component is applicable to the target configuration and the thickness relationship between the first region 110 and the predetermined position 121 in the above embodiments, which will not be elaborated here. The target configuration includes at least one or more of right-angled step targets, rounded-corner step targets, gradient step targets, and / or curved-surface step targets to achieve precise compensation and optimization of the specific erosion distribution of the circular tube target during rotary sputtering.

[0127] In one specific embodiment, such as Figures 29 to 32 As shown, the target component is a cylindrical target component, and the cross-sectional diameter of the target at the predetermined position 121 in the second region 120 is larger than the cross-sectional diameter of the target in the first region 110. Specifically, Figure 29 The target material thickness at the predetermined position 121 shown is b. Figure 30 The target thickness in the first region 110 shown is 'a', and the relationship 'b' is greater than 'a' is satisfied. The circular tube target component in this embodiment is also applicable to the above-mentioned target configuration, wherein the target configuration includes at least one or more of right-angle step target, rounded corner step target, gradient step target and / or curved surface step target, so as to achieve precise compensation and optimization of the specific erosion distribution of the circular tube target during the rotary sputtering process.

[0128] In some embodiments, Figure 31 and Figure 32 The diagrams show two schemes: one where a spacer 300 is placed between the cylindrical target and the backing plate, and the other where the target is placed on a stepped backing plate. Figure 31As can be seen, the thickness of the target material in the first zone 110 is c, the sum of the thicknesses of the gasket 300 and the target material in the first zone 110 is a, and the thickness b of the target material at the predetermined position 121 also satisfies the relationship b > a. From Figure 32 As can be seen, the thickness of the target material in the first region 110 is d, the sum of the thickness of the boss structure of the back plate and the target material in the first region 110 is a, and the thickness of the target material at the predetermined position 121, b, also satisfies the relationship b > a.

[0129] In some embodiments, such as Figure 6 As shown, the target material at the predetermined position 121 can also be stacked on the stepped back plate 220. As can be seen from the figure, the thickness of the overlapping part of the boss structure of the predetermined position 121 and the stepped back plate 220 is still greater than the thickness of the target material itself in the first region 110.

[0130] In some embodiments, the target 100 includes at least one of the following: ITO (indium tin oxide) target, IGZO (indium gallium zinc oxide) target, IZO (indium zinc oxide) target, Al (aluminum) target, Ag (silver) target, Mo (molybdenum) target, Cu (copper) target, MTD (molybdenum nickel titanium alloy) target, MoNb (molybdenum niobium alloy) target, MoTi (molybdenum titanium alloy) target, and MoOx (molybdenum oxide) target.

[0131] The second aspect of this application provides a magnetron sputtering electrode, such as... Figures 22 to 32 As shown, it includes:

[0132] At least one magnet assembly 500, at least one backplate, and a target 100 as provided in the first aspect of the embodiments of this application.

[0133] In some embodiments, the target 100 is rectangular, specifically as follows: Figures 22 to 25 The square-shaped backplate is fixedly disposed on the side surface of the backplate near the substrate 400. To match the structure of the target material, the backplate is also square and its size is larger than that of the target material 100, serving to support the target material 100. At least a portion of the substrate 400 serves as the effective film formation guarantee region 410, and the remaining region serves as the non-effective film formation region 420. The effective film formation guarantee region 410 is used to receive the particle stream sputtered from the target material 100 to deposit a thin film on its surface that meets the requirements of thickness uniformity and structural integrity. Typically, the effective film formation guarantee region 410 is disposed corresponding to the central region of the target material 100, so that the target material 100 can fully cover the effective film formation guarantee region 410, thereby forming a uniform and complete thin film structure in that region. In this embodiment, the target area corresponding to the effective film formation guarantee area 410 is defined as the first area 110, and the remaining target areas are defined as the second area 120. The second area 120 is mainly used to sputter particles to the non-effective film formation area 420 to avoid uneven film formation at the edge of the effective film formation guarantee area 410.

[0134] In some embodiments, a backplate is disposed on the side of the target 100 away from the effective film formation guarantee area 410, including a uniform cross-section backplate 210 or a stepped backplate 220; wherein, the uniform cross-section backplate 210 includes a rectangular uniform cross-section backplate, a circular uniform cross-section backplate or a circular tube uniform cross-section backplate; the stepped backplate 220 includes a rectangular stepped backplate, a circular stepped backplate or a circular tube stepped backplate.

[0135] Specifically, the step back plate 220 includes a first part 221 and a second part 222. The first part 221 is corresponding to the first region 110 of the target and the portion of the target extending from the first region 110 to the second region 120. The second part 222 is corresponding to the second region 120 of the target. The thickness of the first part 221 is greater than the thickness of the second part 222. The sum of the thicknesses of the first part 221 and the first region 110 of the target is less than the sum of the thicknesses of the second part 222 and the target at a predetermined position 121 of the second region 120 of the target.

[0136] In some embodiments, a gasket 300 is provided between the back plate and the first region 110 of the target; wherein the total thickness of the gasket 300, the first portion 221, and the first region 110 of the target is less than the total thickness of the second portion 222 and the target at a predetermined position 121 of the second region 120 of the target; or, the total thickness of the gasket 300, the back plate, and the first region 110 is less than the total thickness of the back plate and the target at the predetermined position 121.

[0137] In some embodiments, the sputtering process employs a 500-point dual-origin or multi-origin motion mode of the magnet assembly for film formation, such as... Figure 22 The diagram shows a top view of the magnetron sputtering electrode. The magnet assembly 500 reciprocates linearly along a first direction at both ends of the target 100. In the dual-origin motion mode, the magnet assembly 500 has at least two predetermined dwell points at positions corresponding to the two ends of the second region 120 along the first direction (i.e., the turning points of the magnet assembly 500's movement). By controlling the dwell time of the magnet assembly at these positions, the sputtering intensity of the corresponding region can be adjusted. In this structure, the second region 120 extends along the first direction and is arranged at both ends of the first region 110 along the second direction.

[0138] It should be understood that during sputtering, the dual-origin or multi-origin motion mode causes the magnet assembly 500 to pause multiple times in the reversal region. Since the magnetic field at both ends of the magnet assembly 500 in the second direction is typically stronger than that in the middle region, when the magnet assembly 500 reciprocates linearly along the first direction at both ends of the target 100, the degree of erosion on the target at both ends in the second direction is often more pronounced than in the middle region. To address this issue, the structure in this embodiment solves the problem by placing the second region 120 at both ends of the target in the second direction. This arrangement effectively compensates for the erosion differences caused by uneven magnetic field distribution, thereby achieving a more uniform erosion profile on the target. This design not only further improves the utilization rate of the target but also helps extend its service life.

[0139] In other embodiments, the sputtering process employs a 500-magnet assembly in a single-origin motion mode for film formation, such as... Figure 23 The schematic diagram of the top view of the magnetron sputtering electrode shows that the magnet assembly 500 reciprocates linearly at both ends of the target 100 along a first direction. In the single-origin motion mode, the magnet assembly 500 has a predetermined stopping point at the position corresponding to the second region 120 (i.e., the turning point of the magnet assembly 500's movement). At this time, the second region 120 extends along the second direction and is arranged at both ends of the first region 110 along the first direction.

[0140] It should be understood that during sputtering, the single-origin motion mode requires the magnet assembly 500 to complete one stop at each end of the return region in the first direction of the target 100. During this process, the magnet assembly 500 needs to undergo deceleration, stopping, and reverse acceleration, resulting in a significantly longer effective working time in the two ends of the target in the first direction compared to the middle uniform scanning region. To solve the above problem, this embodiment sets the second region 120 at both ends of the target in the first direction. This structure increases the target thickness in the two ends of the target to uniformly distribute the erosion amount, thereby improving the utilization rate of the target.

[0141] In some embodiments, such as Figure 24 The diagram shows a top view of the magnetron sputtering electrode. The magnet assembly 500 reciprocates linearly along a first direction at both ends of the target 100. A predetermined position 121 within the second region 120 is arranged around the edge of the first region 110. It should be noted that this configuration is not only applicable to single-origin motion modes but also compatible with dual-origin or multi-origin motion modes. By setting the predetermined stopping point at the edge region surrounding the first region 110, finer sputtering intensity distribution control can be achieved, thereby significantly improving the thickness uniformity of the film within the effective film formation guarantee region 410.

[0142] In other embodiments, such as Figure 25The diagram shows a top view of the magnetron sputtering electrode. The magnet assembly 500 reciprocates linearly along a first direction at both ends of the target 100. Predetermined positions 121 within the second region 120 are located at the four corners of the target 100. It should be noted that this configuration is applicable not only to single-origin motion modes but also to dual-origin or multi-origin motion modes. By setting the predetermined stopping points at the four corners of the target 100, finer sputtering intensity distribution control can be achieved, thereby significantly improving the thickness uniformity of the film within the effective film formation guarantee region 410.

[0143] In some embodiments, such as Figure 26 As shown, the target surface of the target 100 is circular and is specifically fixed on the side surface of the back plate near the substrate 400. To match the structure of the target, the back plate is also circular and together with the target in the first region 110, the target in the second region 120, and the back plate, they form a concentric circle structure. The size of the back plate is larger than that of the target 100, so that the target 100 can fully cover the effective film formation guarantee area 410, thereby forming a uniform and complete circular thin film structure in this area. The circular target in this embodiment is suitable for film formation of small-sized devices.

[0144] Specifically, in this embodiment, the sputtering process uses a static configuration where the magnet assembly 500 and the target material 100 are relatively stationary during sputtering film formation. Figure 26 The diagram shows a top view of the magnetron sputtering electrode. In one specific embodiment, the magnet assembly 500 includes a magnetic ring disposed on the side of the backplate facing away from the target. The magnetic ring remains relatively stationary with respect to the target and forms a closed annular magnetic field above the surface of the target 100. This magnetic field effectively confines electron motion and enhances the ionization efficiency of the working gas, thereby generating a high-density plasma near the target surface. The plasma uniformly bombards the target 100, ultimately depositing a high-quality thin film within the effective film deposition guarantee region 410.

[0145] In some embodiments, such as Figure 27 and Figure 28 As shown, the target 100 includes at least one target component arranged along a first direction, and the target component is a strip-shaped target surface component.

[0146] According to the above embodiments, at least one magnet assembly 500 is correspondingly disposed with at least one target component, that is, each strip-shaped target component is correspondingly provided with a magnet assembly 500, and is disposed on the side of the back plate away from the target. The movement direction of the magnet assembly 500 includes one or more of the following: both the strip-shaped target component and the magnet assembly 500 are stationary; the magnet assembly 500 is stationary relative to the target 100; the magnet assembly 500 moves back and forth along the length direction of the target 100 or along the width direction of the target 100; and, within the corresponding target component area, the magnet assembly 500 is provided with at least one or a set of predetermined stopping points in a first direction or a second direction. A set of predetermined stopping points includes two stopping positions: a starting stopping point and a dwelling stopping point. Specifically, to meet the structural and functional requirements of the target material of the strip-shaped target surface, the back plate also has a strip-shaped cross-section, and the dimensions of the back plate in both the first and second directions are larger than those of the target 100 to provide stable support. At least a portion of the substrate 400 serves as an effective film formation guarantee area 410, and the remaining area serves as a non-effective film formation area 420. In this embodiment, as Figures 27 to 28 As shown, the target 100 has a second region 120 at both ends in the second direction, and a predetermined position 121 in the second region 120 is located on the side of the second region 120 away from the first region 110.

[0147] In one specific embodiment, such as Figure 27 As shown, the first region of all strip-shaped target components cannot fully cover the effective film-forming guarantee region 410. That is, the width of the cross-section of the strip-shaped target 100 in the first direction is smaller than the width of the effective film-forming guarantee region 410 in the first direction, and the length of the first region 110 in the second direction is greater than the length of the effective film-forming guarantee region 410 in the second direction. To overcome the limited static coverage of the first region 110, this embodiment adopts a method in which at least one strip-shaped target component and the effective film-forming guarantee region 400 are kept in relative motion. By making the two relative positions, it is ensured that the orthographic projection of each point of the effective film-forming guarantee region 410 on the first region 110 is located within the first region 110. At this time, the particle stream sputtered from the target in the first region 110 can fully cover every area of ​​the effective film-forming guarantee region 410, thereby ensuring the integrity and uniformity of the film formation.

[0148] In another specific embodiment, the first region 110 of all strip-shaped target components can effectively cover the effective film formation guarantee region 410. That is, the sum of the widths of the first regions 110 of the multiple strip-shaped target components in the first direction is greater than the width of the effective film formation guarantee region 410 in the first direction, and the length of the first regions 110 of the multiple strip-shaped target components in the second direction is greater than the length of the effective film formation guarantee region 410 in the second direction. Based on the above target conditions, sputtering of the effective film formation guarantee region 410 can be completed by keeping all strip-shaped target components relatively stationary with the substrate 400. Without moving the substrate 410 or the strip-shaped target components, the first regions 110 of the multiple strip-shaped target components can completely cover the effective film formation region 410 of the substrate in a static range.

[0149] In one specific embodiment, such as Figure 27 As shown, a sputtering mode in which the target is stationary and the substrate 400 moves in a straight line along the first direction is used to sputter the effective film formation guarantee area 410 on the substrate 400, thereby achieving continuous and uniform film formation in the effective film formation guarantee area 40.

[0150] It should be noted that the magnetron sputtering electrode structure provided in this embodiment has high flexibility. For example, the movement mode of the magnet assembly 500 is not limited to a single-origin movement mode, a dual-origin movement mode, or a multi-origin movement mode. The movement direction of the magnet assembly 500 is also not limited to being stationary relative to the target, moving back and forth in a straight line along a first direction, or moving back and forth in a straight line along a second direction, thereby adapting to various process requirements.

[0151] In some embodiments, such as Figure 29 and Figure 30 As shown, the target 100 includes at least one target component arranged along a first direction, and the target component is a circular tube target component.

[0152] According to the above embodiments, at least one magnet assembly 500 is coaxially disposed in the central cavity of a circular tube with a uniform cross-section back plate or a circular tube with a stepped back plate. The circular tube target material component and its back plate rotate around the center of the target material 100, and each circular tube target material is correspondingly provided with a magnet assembly 500. The movement direction of the magnet assembly 500 includes a stationary state or rotation around the central axis of the target material 100, thereby ensuring that the target material is uniformly etched and a large-area uniform film is formed.

[0153] Specifically, to meet the structural and functional requirements of the aforementioned cylindrical target component, the backplate is also a cylindrical structure, and the outer diameter of the backplate is smaller than the inner diameter of the target 100, thereby providing stable and reliable internal support for the target. In this embodiment, as... Figure 29 and Figure 30As shown, the target 100 has second regions 120 at both ends in the second direction. A predetermined position 121 within the second region 120 is located on the side of the second region 120 away from the first region 110. The width of the target at the predetermined position 121 in the first direction is greater than the width of the target in the first region 110. This radial widening design at the predetermined position can specifically compensate for the abnormally rapid erosion of the circular tube target caused by the magnetic field end effect during rotary sputtering, thereby optimizing the overall utilization rate of the target and extending the service life of the target.

[0154] In one specific embodiment, such as Figure 29 As shown, the first region 110 of all the cylindrical target components cannot fully cover the effective film formation guarantee region 410. To overcome the limited static coverage of the first region 110, this embodiment employs at least one cylindrical target component to maintain relative motion with the effective film formation guarantee region 400. By creating a relative position between the two, it is ensured that the orthographic projection of each point of the effective film formation guarantee region 410 onto the first region 110 is located within the first region 110. At this time, the particle stream sputtered from the target in the first region 110 can fully cover every area of ​​the effective film formation guarantee region 410, thereby ensuring the integrity and uniformity of the film formation. The movement directions of the magnet assembly 500 include: the cylindrical target component rotating along the central axis, the substrate and the magnet assembly 500 maintaining relative motion, wherein the substrate or the magnet assembly remains stationary, the magnet assembly 500 reciprocates along the first direction in the effective film formation guarantee region 410, and rotates and oscillates around the central axis of the target at a certain angle.

[0155] In another specific embodiment, the first region 110 of all the cylindrical target components can effectively cover the effective film formation guarantee region 410. Sputtering of the effective film formation guarantee region 110 can be completed by keeping all the cylindrical target components relatively stationary with respect to the substrate. Without moving the substrate 410 or the cylindrical target components, the first region 110 of multiple cylindrical target components can completely cover the effective film formation region 410 of the substrate in a static range.

[0156] In one specific embodiment, such as Figure 29 As shown, a sputtering mode in which the target is stationary and the substrate 400 moves in a straight line along the first direction is used to sputter the effective film formation guarantee area 410 on the substrate 400, thereby achieving continuous and uniform film formation in the effective film formation guarantee area 40.

[0157] In some embodiments, such as Figure 6 As shown, the first portion 221 of the stepped backplate 220 can also extend into the interior of the target material at the predetermined position 121, and the thickness of the overlapping area between the predetermined position 121 and the first portion 221 is still greater than the thickness of the target material itself in the first region 110. In the embodiments of this application, the above design is also applicable to the target material configuration in other embodiments.

[0158] In some embodiments, the at least one magnet component 500 included in the magnetron sputtering electrode provided in the second aspect of the present application can be one or more of a single flux magnet component, a dual flux magnet component, or a multi-flux magnet component.

[0159] In some embodiments, the target thickness ratio, splicing target size parameters, and splicing configuration of each region can be adjusted in a coordinated manner based on the uniformity of the magnetic flux of the magnet assembly, the actual erosion rate of the target material, and the usage requirements of the effective film formation guarantee area, thereby improving the target material utilization rate.

[0160] In some embodiments, the thickness of the target material at a predetermined position 121 within the second region 120 can be flexibly varied according to the usage of the effective film formation guarantee region 420. The thickness and thickness ratio of the first region 110 and the second region 120 can also be flexibly varied. By dynamically adjusting the thickness at this position and combining it with the overall thickness ratio of the first region 110 and the second region 120, precise matching of target material supply and consumption can be achieved. This design effectively ensures the uniformity of film quality and thickness in key areas, further improving target material utilization.

[0161] In some embodiments, the size, shape, area, and number of splicing planes of the target material can be arbitrarily adjusted and varied according to the design, further increasing the flexibility and adaptability of the target material.

[0162] A third aspect of this application provides a magnetron sputtering film deposition apparatus, comprising:

[0163] The magnetron sputtering electrode provided in the second aspect of the embodiments of this application;

[0164] Vacuum sputtering chamber 003 is used to provide a vacuum environment, and the magnetron sputtering electrode is disposed in vacuum sputtering chamber 003;

[0165] A substrate handling device is provided in a vacuum sputtering chamber 003 for handling and processing substrates 400;

[0166] A gas introduction device is used to introduce gas into the vacuum sputtering chamber 003;

[0167] A sputtering power source for supplying power to the target 100 provided as described in the first aspect of the embodiments of this application.

[0168] In summary, the target material provided in this application adapts to different erosion distributions by splicing together a first zone and a second zone with different thicknesses (the thickness of the first zone is less than the thickness of the second zone): the target material is thicker in areas with deeper erosion and thinner in areas with shallower erosion, thus achieving optimized target material configuration. Through this differentiated thickness design, the overall erosion distribution of the target material is more uniform, thereby significantly improving the utilization rate of the target material and extending its service life.

[0169] Meanwhile, the spliced ​​thickness partition design of the target material provided in this application embodiment has good structural flexibility, is compatible with a variety of backplate configurations, meets the diverse needs of different sputtering processes and application scenarios for target material support, and enhances the adaptability and configurability of the target material in practical applications.

[0170] The above description of this application is illustrative and is not limited thereto. The figures shown are only one of the embodiments of this application. If researchers in the art propose a similar structural form without departing from the spirit of this application, it shall fall within the protection scope of this application.

Claims

1. A target material, characterized by, The target material (100) comprises: a first area (110) corresponding to an effective film formation guarantee area (410), and a second area (120) corresponding to a non-effective film formation area (420) arranged around the first area (110) or arranged at both ends of the first area (110) close to the edge of the target material (100); wherein the target surface of the target material at a predetermined position (121) of the second area (120) is higher than the target surface of the target material in the first area (110).

2. The target of claim 1, wherein The target material at the predetermined position (121) of the second area (120) comprises one or more of a right-angle stepped target material, a round-angle stepped target material, a gradient stepped target material, and / or a curved surface stepped target material.

3. The target of claim 1, wherein The target material (100) is integrally formed, or the target material of the first area (110) extends into the second area (120) and is spliced with the target material at the predetermined position (121) of the second area (120); and / or, the target material of the first area (110) comprises a plurality of first target material units and is spliced by the plurality of first target material units; and / or, the target material of the second area (120) comprises a plurality of second target material units and is spliced by the plurality of second target material units.

4. The target of claim 1, wherein The target surface of the target material (100) is rectangular; wherein the predetermined position (121) of the second area (120) is arranged at opposite ends of the target material (100); or the predetermined position (121) of the second area (120) is arranged at the corner regions of the target material (100); or the predetermined position (121) of the second area (120) is arranged around the edge of the target material (100).

5. The target of claim 1, wherein The target material (100) comprises at least one target material component, the target surface of the first area (110) of the target material component is in a strip shape, the second area (120) is arranged at both ends of the length direction of the first area (110), and the first area (110) is arranged between the second areas (120); wherein the at least one target material component is arranged along the width direction of the first area (110).

6. The target of claim 5, wherein The target material component comprises one or more of a strip-shaped target material component or a circular pipe target material component; wherein the outer diameter of the predetermined position (121) of the second area of the circular pipe target material component is greater than the outer diameter of the first area (110) of the circular pipe target material component.

7. The target of claim 6, wherein The target material (100) is configured to: when the first area (110) of the target material component has a non-overlapping area with the effective film formation guarantee area (410), the target material (100) and the effective film formation guarantee area (410) remain relative motion so that the orthographic projection of the effective film formation guarantee area (410) on the at least one target material component is located in the first area (110).

8. The target of claim 6, wherein The target material (100) is configured to: when the first area (110) of the target material component can cover the effective film formation guarantee area (410), the target material component and the effective film formation guarantee area (410) remain relative static.

9. The target of claim 1, wherein The target surface of the target material (100) is circular; wherein the predetermined position (121) of the second area (120) is arranged around the target material (100).

10. The target according to any one of claims 1 to 8, wherein The size of the effective film-forming guarantee area (410) is inversely proportional to the size of the target surface at the predetermined position (121); The size of the target surface at the predetermined position (121) is proportional to the erosion area of ​​the second region (120).

11. A magnetron sputtering electrode, characterized by include: At least one magnet assembly (500), at least one back plate, and a target (100) as claimed in any one of claims 1 to 10.

12. The magnetron sputtering electrode of claim 11, wherein, The backplate is disposed on the side of the target (100) away from the effective film formation guarantee area (410), including a backplate with equal cross section (210) or a stepped backplate (220). in, The equal cross-section back plate (210) includes a rectangular equal cross-section back plate, a circular equal cross-section back plate, or a circular tube equal cross-section back plate; The step back plate (220) includes a rectangular step back plate, a circular step back plate, or a round tube step back plate.

13. The magnetron sputtering electrode of claim 12, wherein, The stepped back plate (220) includes a first part (221) and a second part (222). The first part (221) is corresponding to the first region (110) of the target and the portion of the target extending from the first region (110) to the second region (120). The second part (222) is corresponding to the second region (120) of the target. The thickness of the first part (221) is greater than the thickness of the second part (222). The sum of the thicknesses of the first part (221) and the first region (110) of the target is less than the sum of the thicknesses of the second part (222) and the target at a predetermined position (121) of the second region (120) of the target.

14. The magnetron sputtering electrode of claim 13, wherein, A gasket (300) is provided between the back plate and the first region (110) of the target material. Wherein, the total thickness of the gasket (300), the first portion (221), and the first region (110) of the target material is less than the total thickness of the second portion (222) and the target material at a predetermined position (121) of the second region (120); or, The total thickness of the gasket (300), the back plate, and the first region (110) is less than the total thickness of the back plate and the target material at the predetermined position (121).

15. The magnetron sputtering electrode of claim 11, wherein, The magnet assembly (500) includes one or more of a single flux magnet assembly, a dual flux magnet assembly, or a multi-flux magnet assembly.

16. The magnetron sputtering electrode of claim 11, wherein, Configured as: The target surface of the target material (100) is a rectangular target surface. The magnet assembly is disposed on the side of the back plate away from the target material. The magnet assembly (500) moves back and forth in a straight line at both ends of the target material (100) along a first direction. The magnet assembly (500) has a predetermined stopping point at the position corresponding to the second area (120) of the target material. The second region (120) of the target material extends along the second direction and is arranged at both ends of the first region (110) of the target material along the first direction, or, The second region (120) of the target material is disposed around the edge of the first region (110) of the target material; or, The second region (120) of the target material is located at the four corners of the target material (100), and the first region (110) of the target material is located at the remaining positions of the target material (100). Wherein, the first direction and the second direction are perpendicular to each other.

17. The magnetron sputtering electrode of claim 11, wherein Configured as: The target surface of the target material (100) is a rectangular target surface. The magnet assembly is disposed on the side of the back plate away from the target material. The magnet assembly (500) moves back and forth along the first direction at both ends of the target material (100). The magnet assembly (500) has at least two predetermined stopping points at the corresponding positions at both ends of the target material along the first direction. The second region (120) of the target material extends along the first direction and is arranged at both ends of the first region (110) of the target material along the second direction, or, The second region (120) of the target material is disposed around the edge of the first region (110) of the target material; or, The second region (120) of the target material is located at the four corners of the target material (100), and the first region (110) of the target material is located at the remaining positions of the target material (100). Wherein, the first direction and the second direction are perpendicular to each other.

18. The magnetron sputtering electrode of claim 11, wherein, Configured as: The target material (100) includes at least one target material component arranged along a first direction, and the target material component is a strip-shaped target surface component; The at least one magnet assembly (500) is correspondingly disposed to the at least one strip-shaped target component and is disposed on the side of the back plate opposite to the strip-shaped target component. The movement direction of the at least one magnet assembly (500) includes one or more of the following: stationary relative to the target (100), reciprocating motion along the length direction of the target (100), or reciprocating motion along the width direction of the target (100); and, The magnet assembly (500) has at least one or a group of predetermined stopping points in the corresponding strip target component area in a first direction or a second direction; The set of predetermined stops includes an initial stop and a final stop.

19. The magnetron sputtering electrode of claim 12, wherein, Configured as: The target material (100) includes at least one target material component, which is a circular tube target material component and is arranged along a first direction. The target material component and the circular tube equal cross-section back plate or circular tube stepped back plate corresponding to the circular tube target material component both rotate around the central axis of the target material component. The at least one magnet assembly (500) is correspondingly disposed with the at least one circular tube target component and is correspondingly disposed in the central region of the circular tube equal cross section back plate or the circular tube stepped back plate. The movement direction of the at least one magnet assembly (500) includes being stationary relative to the central axis of the target (100) or swinging back and forth.

20. The magnetron sputtering electrode of claim 11, wherein, Configured as: The target surface of the target material (100) is circular, and the magnet assembly (500) is disposed on the side of the back plate away from the target material (100). The movement direction of the magnet assembly (500) includes being stationary relative to the target material (100).

21. A magnetron sputter film deposition apparatus, characterized by include: The magnetron sputtering electrode as described in any one of claims 11 to 20; A vacuum sputtering chamber is used to provide a vacuum environment, and the magnetron sputtering electrode is disposed in the vacuum sputtering chamber; A substrate handling device, disposed in the vacuum sputtering chamber, is used to handle and process substrates; A gas introduction device is used to introduce gas into the vacuum sputtering chamber; A sputter power source for a target as claimed in any of claims 1-10.