A creep testing system for simulating highly corrosive seawater environments

By introducing and expelling inert gas into the inner cavity of the corrosion chamber to drive the deformation of flexible components, the problem that traditional creep testing systems cannot realistically simulate tidal environments is solved, achieving high-precision and reliable liquid level control, which is suitable for long-term creep testing.

CN224985193UActive Publication Date: 2026-11-17SINOMA TECH PROVING GROUND (LUOYANG) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522521366.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-27
Publication Date
2026-11-17
Estimated Expiration
2035-11-27

AI Technical Summary

Technical Problem

Traditional marine environment corrosion creep testing systems cannot realistically simulate tidal environments, and liquid pumping schemes have risks of failure, vibration interference, and leakage, making it difficult to accurately control changes in liquid level.

Method used

Employing the principle of pneumatic liquid control, the corrosion chamber simulates a tidal environment by introducing and expelling inert gas into and out of the sealed cavity of the corrosion chamber, thereby driving the deformation of flexible components. This eliminates the need for a liquid pump circulation system and uses a corrosion chamber made of transparent plexiglass and fluorinated rubber.

Benefits of technology

It achieves high-precision and smooth liquid level control, reduces vibration interference and leakage risk, improves the simulation fidelity of the test, and is suitable for long-term creep tests.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224985193U_ABST
    Figure CN224985193U_ABST
Patent Text Reader

Abstract

A creep testing system for simulating highly corrosive seawater environments includes a vertical creep testing machine and a corrosion chamber for holding a corrosive solution. The corrosion chamber has perforations for the upper and lower clamps of the vertical creep testing machine to extend into. The corrosion chamber comprises an upper rigid part and a lower flexible part that are sealed together to form a closed inner cavity, the volume of which can change due to changes in the shape of the lower flexible part. The corrosion chamber also has an air inlet and an air outlet. The air inlet allows external gas to enter, causing the lower flexible part to expand and lowering the level of the corrosive solution below the sample. The air outlet allows gas to exit, causing the lower flexible part to recover and raising the level of the corrosive solution to cover the sample. This simulates tidal corrosion of the sample by seawater by releasing gas into the closed inner cavity of the corrosion chamber. This invention offers more reliable operation, more precise control, and is more suitable for simulating tidal environments in long-term creep testing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of creep testing equipment for metallic materials, specifically a creep testing system for simulating highly corrosive seawater environments. Background Technology

[0002] Metallic materials are widely used in marine engineering equipment, such as platforms, pipelines, and mooring chains. These components bear loads for extended periods and are exposed to harsh marine corrosive environments, with their failure modes primarily exhibiting the interaction between corrosion and creep. Therefore, it is crucial to accurately simulate the marine environment in the laboratory to test the creep performance of these materials.

[0003] Traditional marine corrosion creep testing systems typically consist of a vertical creep testing machine and a corrosion chamber. The corrosion chamber contains a corrosive solution such as artificial seawater, into which the sample is immersed to simulate the environment of a fully submerged seawater zone. However, many critical components in the ocean, such as those in tidal zones and splash zones, operate in a periodic alternating wet and dry environment, i.e., a tidal environment. Traditional static immersion tests cannot realistically simulate this condition, leading to discrepancies between experimental data and actual conditions.

[0004] To address the aforementioned issues, existing technologies have developed solutions that simulate tidal environments by pumping corrosive solutions into or out of the corrosion chamber. However, creep testing cycles typically last for hundreds or even thousands of hours. Such liquid-pumping-based solutions may present the following problems during long-term operation: First, the continuous operation of the solution circulation pump carries a risk of failure, and the vibrations generated during its operation may interfere with high-precision creep deformation measurements. Second, the pump and piping system has a relatively complex structure and potential leakage points. In tests lasting several months, a leak could lead to test failure and damage to the expensive creep testing machine. Furthermore, achieving liquid level changes through pumping has limited precision in controlling the circulation rate and surface stability, making it difficult to accurately simulate real tidal processes. Utility Model Content

[0005] The present invention aims to provide a creep testing system for simulating a highly corrosive seawater environment, which is more reliable in operation, more precise in control, and more suitable for long-term creep testing and tidal environment simulation.

[0006] To solve the above technical problems, the specific solution adopted by this utility model is as follows: a creep testing system for simulating a highly corrosive seawater environment, including a vertical creep testing machine and a corrosion box for holding a corrosive solution. The corrosion box has a through hole for the upper and lower clamps of the vertical creep testing machine to extend into. The corrosion box includes an upper rigid part and a lower flexible part that are sealed to each other to form a closed inner cavity. The volume of the closed inner cavity can be changed due to the shape change of the lower flexible part. The corrosion chamber is also equipped with an air inlet and an air outlet. The air inlet allows external gas to be introduced to expand the lower flexible part and lower the liquid level of the corrosion solution below the sample. The air outlet allows gas to be discharged to restore the lower flexible part and raise the liquid level of the corrosion solution to cover the sample. Thus, the tidal corrosion of the sample by seawater is simulated by releasing gas into the closed inner cavity of the corrosion chamber.

[0007] Preferably, the corrosion box also includes a rigid base, with the lower flexible portion sealed between the upper rigid portion and the rigid base.

[0008] Preferably, the rigid base has a through hole for the lower chuck to pass through, the lower chuck has a thread on its outer periphery, and nuts for sealing are screwed onto the lower chuck on the upper and lower sides of the rigid base respectively.

[0009] Preferably, a sealing ring is provided on the end face of the rigid base corresponding to the nut.

[0010] Preferably, the top of the upper rigid part has an upper through hole for the upper clamp to pass through, and the top of the upper through hole is connected to a clamp through a corrugated pipe. The clamp is fixedly connected to the upper clamp and forms a sealed fit.

[0011] Preferably, the upper rigid part is made of transparent plexiglass, and the lower flexible part is made of fluorinated rubber.

[0012] Preferably, the lower flexible part is recessed towards the center of the closed inner cavity of the corrosion box in its natural state.

[0013] Preferably, both the air inlet and the exhaust outlet are located on the periphery of the upper rigid part.

[0014] Compared with existing technologies, the creep testing system for simulating highly corrosive seawater environments provided by this invention has the following significant advantages: This invention abandons the faulty liquid pump circulation scheme and innovatively adopts the principle of "pneumatic liquid control". By introducing and discharging harmless inert gas (such as nitrogen) into the closed corrosion chamber, the flexible bottom is driven to deform, thereby changing the liquid level. The gas control system has no moving parts, is extremely stable and reliable in operation, and has minimal vibration. It is particularly suitable for creep tests that last for weeks or even months, fundamentally avoiding the risk of test failure and equipment damage caused by pump failure or liquid leakage. It is reliable in operation and suitable for long-term testing.

[0015] This invention, by controlling the introduction and discharge of gas, can precisely and smoothly control the internal gas pressure of the corrosion chamber, thereby achieving accurate and rapid adjustment of the deformation of the lower flexible part and the liquid level. This approach can more realistically simulate the rhythm of tidal rise and fall and liquid level changes, improving the simulation fidelity of the experiment. Attached Figure Description

[0016] Figure 1 This is a cross-sectional structural diagram of the present invention, with the lower flexible part in a natural state; Figure 2 for Figure 1 A schematic diagram of the expanded lower flexible part; The markings in the diagram are: 1. Corrosion box, 101. Upper rigid part, 102. Lower flexible part, 103. Rigid base, 2. Air inlet, 3. Upper clamp, 4. Clamp, 5. Bellows, 6. Upper perforation, 7. Exhaust port, 8. Sample, 9. Lower clamp, 10. Nut, 11. Sealing ring, 12. Lower perforation. Detailed Implementation

[0017] The core of this invention lies in the innovative improvement of the corrosion chamber in traditional creep testing systems, and its application to a conventional vertical creep testing machine. The vertical creep testing machine features a loading mechanism that provides a constant tensile load and a high-precision deformation measurement system. Its lower clamp 9 is fixed to the base of the testing machine, while the upper clamp 3 slides vertically onto the crossbeam of the testing machine and is connected to the loading mechanism. During the test, after the upper and lower ends of the sample 8 are fixed by the upper clamp 3 and the lower clamp 9 respectively, the loading mechanism pulls up the clamp to induce continuous creep in the sample. The aforementioned vertical creep testing machine is a mature existing technology in this field, and its structure and specific testing methods will not be elaborated upon. The improvement of this invention focuses on the environmental simulation module, aiming to simulate tidal environments in a more reliable and economical way.

[0018] like Figure 1 As shown, the innovative corrosion box 1 of this system adopts a design that combines an upper rigid part 101 with a lower flexible part 102, balancing the contradiction between functional requirements and engineering implementation: the upper rigid part 101 provides a stable and reliable installation foundation for observation, pipeline connection and clamp sealing, while the lower flexible part 102 is dedicated to the flexible change of volume. The two work together to achieve precise control of the liquid level. Its structure is simpler and more reliable than the complex pumping circulation system.

[0019] The upper rigid part 101 is made of high-transparency acrylic plexiglass. This material choice is not only cost-effective and easy to process, but also allows testers to directly and clearly observe the surface condition changes, corrosion process, and precise liquid level position of the sample 8 inside the corrosion chamber, greatly facilitating the monitoring and recording of the test process. To achieve a dynamic seal between the upper clamp 3 and the static corrosion chamber 1, a metal bellows 5 is connected to the upper perforation 6 at the top of the upper rigid part 101. The upper end of the bellows 5 forms a tight fit seal with the upper clamp 3 through a clamp 4. This design ensures that the upper clamp 3 can move freely with the creep elongation of the sample 8 during the test, while the expansion and contraction of the bellows 5 compensates for this displacement and always maintains the sealing integrity of the system, solving the sealing problem between the moving parts and the static environment chamber.

[0020] The lower flexible part 102, as the core actuating component for realizing tidal simulation, is made of a corrosion-resistant and fatigue-resistant fluorinated rubber film. Its natural state is designed to be recessed towards the center of the closed inner cavity of the corrosion box 1, which not only facilitates the full drainage of liquid during "low tide" but also makes the structure more rational. The edge of the lower flexible part 102 is reliably clamped and sealed between the upper rigid part 101 and the rigid base 103.

[0021] A through hole 12 is provided on the rigid base 103 for the lower chuck 9 to pass through. By tightening the nuts 10 on the lower chuck 9 on both the upper and lower sides of the rigid base 103, and cooperating with the sealing rings 11 provided on the contact surface, another robust static sealing barrier is formed. This multi-seal design together ensures the sealing reliability of the system during long-term tests lasting hundreds or even thousands of hours.

[0022] An air inlet 2 and an exhaust port 7 are provided on the periphery of the upper rigid part 101. By introducing or expelling an inert gas, such as high-purity nitrogen, into the corrosion chamber 1 to avoid introducing additional chemical reactions, the lower flexible part 102 can be driven to deform, thereby changing the internal cavity volume and realizing the rise and fall of the liquid level. This control method, which uses "pneumatics" instead of a "liquid pump," has a simple structure, no moving parts, and operates quietly and stably, making it very suitable for creep tests that are sensitive to vibration and have long cycles.

[0023] In the specific implementation process, when the test begins, the lower flexible part 102 is in a naturally concave state (corresponding to...). Figure 1 At this point, the liquid level is below sample 8, simulating "ebb tide". When simulating "high tide", the exhaust port 7 is opened (or the air inlet is closed and the exhaust is opened), the air pressure inside the corrosion chamber 1 decreases, and under atmospheric pressure, the lower flexible part 102 recovers upward, pushing the liquid level up until it completely covers sample 8 (corresponding to...). Figure 2When it is necessary to simulate "low tide" again, an appropriate amount of inert gas is introduced into the corrosion chamber 1 through the air inlet 2. The internal air pressure increases, driving the lower flexible part 102 to expand downward, and the liquid level drops accordingly, exposing the sample 8 to air again. By controlling the opening and closing and duration of the air inlet and outlet valves through the program, the periodic tidal environment simulation can be achieved.

Claims

1. A creep testing system for simulating a highly corrosive seawater environment, comprising a vertical creep testing machine and a corrosion chamber (1) for holding a corrosive solution, wherein the corrosion chamber (1) has perforations for the upper clamp (3) and lower clamp (9) of the vertical creep testing machine to extend into, characterized in that: The corrosion box (1) includes an upper rigid part (101) and a lower flexible part (102) that are sealed to each other to form a closed inner cavity, and the volume of the closed inner cavity can be changed due to the shape change of the lower flexible part (102). The corrosion chamber (1) is also provided with an air inlet (2) and an exhaust outlet (7). The air inlet (2) allows external gas to be introduced to expand the lower flexible part (102) and lower the liquid level of the corrosion solution to below the sample (8). The exhaust outlet (7) allows gas to be discharged to restore the lower flexible part (102) and raise the liquid level of the corrosion solution to cover the sample (8). Thus, the tidal corrosion of the sample (8) by seawater is simulated by releasing gas into the closed inner cavity of the corrosion chamber (1).

2. The creep testing system for simulating a highly corrosive seawater environment as described in claim 1, characterized in that: The corrosion box (1) also includes a rigid base (103), and a lower flexible part (102) is sealed between the upper rigid part (101) and the rigid base (103).

3. The creep testing system for simulating a highly corrosive seawater environment as described in claim 2, characterized in that: The rigid base (103) has a lower through hole (12) for the lower chuck (9) to pass through. The lower chuck (9) has a thread on its outer periphery, and nuts (10) for sealing are screwed onto the lower chuck (9) on the upper and lower sides of the rigid base (103).

4. The creep testing system for simulating a highly corrosive seawater environment as described in claim 3, characterized in that: A sealing ring (11) is provided on the end face of the rigid base (103) corresponding to the nut (10).

5. The creep testing system for simulating a highly corrosive seawater environment as described in claim 2, characterized in that: The top of the upper rigid part (101) is provided with an upper through hole (6) for the upper clamp (3) to pass through. The top of the upper through hole (6) is connected to a clamp (4) through a corrugated pipe (5). The clamp (4) is fixedly connected to the upper clamp (3) and forms a sealed fit.

6. The creep testing system for simulating a highly corrosive seawater environment as described in claim 1, characterized in that: The upper rigid part (101) is made of transparent organic glass, and the lower flexible part (102) is made of fluorinated rubber.

7. The creep testing system for simulating a highly corrosive seawater environment as described in claim 6, characterized in that: The lower flexible part (102) is recessed in the natural state toward the center of the closed inner cavity of the corrosion box (1).

8. The creep testing system for simulating a highly corrosive seawater environment as described in claim 1, characterized in that: The air inlet (2) and the exhaust outlet (7) are both located on the periphery of the upper rigid part (101).