A composite roller mechanism and a thermal composite lamination system for a thermal composite process

By using a thermally conductive silicone buffer design and a heat-sealing strip to limit the negative and positive electrode thermal composite roller mechanism, the problems of electrode edge shedding and high short-circuit rate caused by traditional steel rollers are solved, achieving high-quality composite and automated control of lithium-ion battery electrodes.

CN224986334UActive Publication Date: 2026-11-17SHANGHAI XUANYI NEW ENERGY DEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522424143.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-14
Publication Date
2026-11-17
Estimated Expiration
2035-11-14

AI Technical Summary

Technical Problem

In traditional thermal bonding processes, the rolling of steel rollers causes severe material loss at the edges of lithium-ion battery electrodes, resulting in a high short-circuit rate and uneven edge bonding, with under-bonding or over-bonding phenomena.

Method used

The device employs a negative and positive electrode thermal composite roller mechanism, which uses thermally conductive silicone and a metal layer to buffer the edges of the contact electrode to avoid direct contact damage. It also utilizes a heat-sealing strip to improve the positional stability of the electrode and combines it with an automated control system to precisely control the electrode conveying and composite process.

Benefits of technology

This effectively avoids the problems of material loss at the electrode edges and high short-circuit rates, improves the quality of electrode edge composite, and ensures battery performance stability and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224986334U_ABST
    Figure CN224986334U_ABST
Patent Text Reader

Abstract

This utility model discloses a composite roller mechanism and a thermal composite lamination system for a thermal composite process, including a positive electrode thermal composite roller mechanism and a negative electrode thermal composite roller mechanism, which are arranged sequentially along the feeding direction. The negative electrode thermal composite roller mechanism includes a first roller body, a first metal layer, and a first thermally conductive silicone rubber. The two first roller bodies are arranged facing each other. The outer wall of the first roller body is fitted with the first metal layer, and a first mounting groove is formed on the outer wall of the first roller body, in which the first thermally conductive silicone rubber is installed. This utility model can effectively improve the problems caused by material loss at the edges of the positive and negative electrode sheets and the resulting high short-circuit rate, as well as the under-composite phenomenon at the edges of the electrode sheets and the over-composite phenomenon inside the electrode sheets, which are caused by traditional integrated steel rollers for thermal composite.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of lithium-ion battery stacking technology, and in particular to a composite roller mechanism and a thermal composite stacking system for a thermal composite process. Background Technology

[0002] In the battery manufacturing industry, thermal bonding is a crucial process for processing battery electrodes. Traditional thermal bonding processes typically use an integrated steel roller for the thermal bonding operation of the electrodes.

[0003] In the field of power lithium-ion battery manufacturing, the thermal composite lamination process mainly uses steel rollers for thermal composite. Due to the step height difference between the negative electrode and the separator, and the step height difference between the positive electrode and the negative electrode and the separator, the rolling process of the steel roller during the composite process causes serious material loss at the edge of the electrode, resulting in a high short circuit rate. Secondly, in order to avoid direct contact between the steel roller and the edge, the current mainstream solution adopts the composite roller electrode edge under-pressure mode to avoid edge pressure. This process is prone to introducing the electrode edge under-composite phenomenon and the over-composite phenomenon caused by instantaneous pressure on the electrode edge. Utility Model Content

[0004] The purpose of this utility model is to provide a composite roller mechanism and a thermal composite stacking system for a thermal composite process, so as to solve the above-mentioned technical problems.

[0005] The technical solution adopted in this utility model is as follows: A thermal composite roller mechanism for a thermal composite process includes a positive electrode thermal composite roller mechanism and a negative electrode thermal composite roller mechanism. The negative electrode thermal composite roller mechanism and the positive electrode thermal composite roller mechanism are arranged sequentially along the feeding direction. The negative electrode thermal composite roller mechanism includes a first roller body, a first metal layer, and a first thermally conductive silicone. The two first roller bodies are arranged facing each other. The first metal layer is sleeved on the outer wall of the first roller body. A first mounting groove is formed on the outer wall of the first roller body, and the first thermally conductive silicone is installed in the first mounting groove.

[0006] Preferably, the system also includes a heat-sealing strip, wherein the heat-sealing strip is disposed in the middle of the first thermally conductive silicone and extends out of the first thermally conductive silicone.

[0007] Preferably, the arc length of the first metal layer is 0.5~1mm smaller than the width of the negative electrode sheet; The gap between two adjacent negative electrode plates is the first diaphragm blank, and the arc length of the first thermally conductive silicone is 0.5~1mm larger than the width of the first diaphragm blank.

[0008] As a further preferred embodiment, the perimeter of the negative electrode thermal composite roller mechanism is equal to the sum of the width of the negative electrode sheet and the blank width of the first diaphragm.

[0009] Preferably, the positive electrode thermal composite roller mechanism includes a second roller body, a second metal layer, and a second thermally conductive silicone rubber. The two second roller bodies are arranged facing each other. The second metal layer is sleeved on the outer wall of the second roller body. A second mounting groove is opened on the outer wall of the second roller body, and the second thermally conductive silicone rubber is disposed in the second mounting groove.

[0010] As a further preferred embodiment, the arc length of the second metal layer is 0.5-1 mm smaller than the width of the positive electrode sheet, the spacing between two adjacent positive electrode sheets is the blank space of the second separator, and the arc length of the second thermally conductive silicone is 0.5-1 mm larger than the width of the blank space of the second separator.

[0011] A thermal composite lamination system includes a thermal composite process composite roller mechanism, and further includes a first process guide roller, a first conveyor belt, a first heating plate, a first composite guide roller, a first cutting knife, a first electrode positioning laser sensor, and a controller. The first process guide roller, the first conveyor belt, the first cutting knife, the first composite guide roller, the first electrode positioning laser sensor, the negative electrode thermal composite roller mechanism, and the positive electrode thermal composite roller mechanism are arranged sequentially along the feeding direction. The first heating plate, the first cutting knife, and the first electrode positioning laser sensor are all located above the first conveyor belt, and the controller is connected to the first electrode positioning laser sensor.

[0012] As a further preferred embodiment, the system also includes a second heating plate, a second conveyor belt, a positive electrode sheet conveying mechanism, and a second electrode sheet positioning laser sensor. The second conveyor belt, the positive electrode sheet conveying mechanism, and the second electrode sheet positioning laser sensor are sequentially arranged between the negative electrode thermal composite roller mechanism and the positive electrode thermal composite roller mechanism along the feeding direction. The second heating plate is arranged above the second conveyor belt. The second electrode sheet positioning laser sensor is connected to the controller. There are two positive electrode sheet conveying mechanisms, which are distributed on both sides of the second conveyor belt. Each positive electrode sheet conveying mechanism includes a third conveyor belt, a third heating plate, and a second cutting blade. The third conveyor belt is used to convey the positive electrode sheet, and the third heating plate and the second cutting blade are arranged above the third conveyor belt.

[0013] As a further preferred embodiment, the system also includes a second composite guide roller and a second process guide roller, wherein the second composite guide roller is located between the positive electrode sheet conveying mechanism and the positive electrode hot composite roller mechanism, and a plurality of second process guide rollers are provided on the side of the positive electrode hot composite roller mechanism away from the second composite guide roller.

[0014] As a further preferred embodiment, the system also includes a third cutting blade, a CCD sensor, and a stacking platform. The CCD sensor, the third cutting blade, and the stacking platform are sequentially arranged on the side of the second process guide roller away from the positive electrode thermal composite roller mechanism. The CCD sensor is connected to the controller.

[0015] The above technical solution has the following advantages or beneficial effects: (1) In this utility model, the negative electrode thermal composite roller mechanism can use the buffering capacity of the first thermally conductive silicone to allow the first metal layer to transition to the surface of the negative electrode sheet, thereby avoiding damage and material loss at the edge of the negative electrode sheet.

[0016] (2) In this utility model, the positive electrode thermal composite roller mechanism can use the buffering capacity of the second thermally conductive silicone to allow the second metal layer to transition to the surface of the positive electrode sheet, thereby avoiding damage and material loss at the edges of the positive and negative electrode sheets.

[0017] (3) In this utility model, the problem of material loss at the edges of positive and negative electrode sheets caused by traditional hot composite integrated steel rollers and the resulting high short circuit rate can be effectively improved, as well as the problem of undercomposite electrode sheet edges and overcomposite electrode sheet interior. Attached Figure Description

[0018] Figure 1 This is a schematic diagram of the negative electrode thermal composite roller mechanism in this utility model; Figure 2 This is a schematic diagram of the positive electrode thermal composite roller mechanism in this utility model; Figure 3 This is a side view of the negative electrode thermal composite roller mechanism in this utility model; Figure 4 This is a positive attempt at the negative electrode thermal composite roller mechanism in this utility model; Figure 5 This is a schematic diagram of the structure of the heat sealing strip in this utility model; Figure 6 This is a side view of the positive electrode thermal composite roller mechanism in this utility model; Figure 7 This is a front view of the positive electrode thermal composite roller mechanism in this utility model; Figure 8 This is a schematic diagram of a thermal composite stacking system.

[0019] In the diagram: 1. Positive electrode thermal composite roller mechanism; 101. Second roller body; 102. Second metal layer; 103. Second thermally conductive silicone; 2. Negative electrode thermal composite roller mechanism; 201. First roller body; 202. First metal layer; 203. First thermally conductive silicone; 204. Heat sealing strip; 3. First process guide roller; 4. First conveyor belt; 5. First heating plate; 6. First composite guide roller; 7. First cutting blade; 8. First electrode positioning laser sensor; 9. Controller; 10. Second heating plate; 11. ... 12. Conveyor belt; 12. Positive electrode conveying mechanism; 121. Third conveyor belt; 122. Third heating plate; 123. Second cutting blade; 13. Second electrode positioning laser sensor; 14. Second composite guide roller; 15. Second process guide roller; 16. Third cutting blade; 17. CCD sensor; 18. Stacking platform; 19. First diaphragm blank; 20. Third diaphragm blank; 21. Positive electrode; 22. Negative electrode; 23. Diaphragm; 24. Electrode composite unit; 25. Second diaphragm blank. Detailed Implementation

[0020] The technical solution of this utility model will now be clearly and completely described with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this utility model. Based on the embodiments of this utility model, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this utility model.

[0021] In the description of this utility model, it should be noted that the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0022] In the description of this utility model, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "joining" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model based on the specific circumstances.

[0023] Figure 1This is a schematic diagram of the negative electrode thermal composite roller mechanism in this utility model; Figure 2 This is a schematic diagram of the positive electrode thermal composite roller mechanism in this utility model; Figure 3 This is a side view of the negative electrode thermal composite roller mechanism in this utility model; Figure 4 This is a positive attempt at the negative electrode thermal composite roller mechanism in this utility model; Figure 5 This is a schematic diagram of the structure of the heat sealing strip in this utility model; Figure 6 This is a side view of the positive electrode thermal composite roller mechanism in this utility model; Figure 7 This is a front view of the positive electrode thermal composite roller mechanism in this utility model; Figure 8 This is a system schematic diagram of a thermally composite laminated system. Please refer to [link / reference]. Figures 1 to 8 The diagram illustrates a preferred embodiment of a thermal composite roller mechanism, comprising a positive electrode thermal composite roller mechanism 1 and a negative electrode thermal composite roller mechanism 2. The negative electrode thermal composite roller mechanism 1 and the positive electrode thermal composite roller mechanism 2 are arranged sequentially along the feeding direction. The negative electrode thermal composite roller mechanism 2 includes a first roller body 201, a first metal layer 202, and a first thermally conductive silicone rubber 203. The two first roller bodies 201 are positioned opposite each other. The first metal layer 202 is sleeved on the outer wall of the first roller body 201, and a first mounting groove is formed on the outer wall of the first roller body 201. The first thermally conductive silicone rubber 203 is installed within the first mounting groove. In this embodiment, the first metal layer 202 is fixedly disposed on the outer wall of the first roller body 201, and the first thermally conductive silicone rubber 203 is fixedly disposed within the first mounting groove. Meanwhile, the positive electrode thermal composite roller mechanism 1 includes a second roller body 101, a second metal layer 102, and a second thermally conductive silicone 103. The two second roller bodies 101 are arranged facing each other. The second metal layer 102 is sleeved on the outer wall of the second roller body 101. A second mounting groove is opened on the outer wall of the second roller body 101, and the second thermally conductive silicone 103 is disposed in the second mounting groove.

[0024] During the thermal bonding process, for the negative electrode thermal bonding roller mechanism 2, the arc length portion of the first metal layer 202 contacts the area where the negative electrode sheet 22 is located, utilizing the good thermal conductivity of the metal to bond the separator 23 to the negative electrode sheet 22. The first thermally conductive silicone 203 portion mainly contacts the first separator blank 19, and its two sides have an arc length of 0.25~0.5mm contact with the edge of the negative electrode sheet 22. Through its buffering capacity, the first metal layer 202 transitions to the surface of the negative electrode sheet 22, effectively preventing the edge of the negative electrode sheet 22 from being damaged or falling off due to direct contact with the hard metal layer. For the positive electrode thermal composite roller mechanism 1, the arc length portion of the second metal layer 102 contacts the area where the positive electrode sheet 21 is located, achieving the composite of the separator 23 and the positive electrode sheet 21. The second thermally conductive silicone 103 mainly contacts the second separator blank 25, with 0.25~0.5mm arc lengths on both sides contacting the edge of the positive electrode sheet 21. Similarly, its buffering capacity allows the second metal layer 102 to transition to the surface of the positive electrode sheet 21, preventing damage and material loss at the edges of the positive electrode sheet 21 and negative electrode sheet 22. This effectively solves the problem of electrode edge material loss caused by traditional integrated steel rollers, significantly reducing the battery short-circuit rate caused by material loss. Simultaneously, it avoids damage to the electrode edges caused by direct contact with the steel roller, improving the composite quality of the electrode edges and thus enhancing the overall battery performance.

[0025] Furthermore, as a preferred embodiment, a heat-sealing strip 204 is also included. The heat-sealing strip 204 is disposed in the middle of the first thermally conductive silicone 203, extending beyond the first thermally conductive silicone 203. During the operation of the negative electrode thermal bonding roller mechanism 2, the heat-sealing strip 204, in contact with the first separator blank 19, uses its own generated heat to heat the separators 23 on both sides of the negative electrode sheet 22 together, thereby further limiting the position of the negative electrode sheet 22 and preventing positional displacement of the negative electrode sheet 22 during the bonding process. This improves the stability of the negative electrode sheet 22 during the bonding process, avoids bonding defects caused by positional displacement of the negative electrode sheet 22, improves the bonding accuracy of the negative electrode sheet 22 and the separator 23, and ensures the quality stability of the battery electrode sheet. Furthermore, as a preferred embodiment, the arc length of the first metal layer 202 is 0.5~1mm smaller than the width of the negative electrode sheet 22; the smaller arc length of the first metal layer 202 can avoid excessive pressure and heating on the edge of the negative electrode sheet 22.

[0026] The gap between two adjacent negative electrode sheets 22 is the first separator blank 19. The arc length of the first thermally conductive silicone 203 is 0.5~1mm larger than the width of the first separator blank 19. The larger arc length of the first thermally conductive silicone 203 ensures effective bonding to the area of ​​the first separator blank 19. The perimeter of the negative electrode thermal bonding roller mechanism 2 is equal to the sum of the width of the negative electrode sheet 22 and the width of the first separator blank 19. These dimensional designs further improve the bonding effect between the negative electrode sheet 22 and the separator 23, avoiding problems such as material loss at the edge of the negative electrode sheet 22, under-bonding at the edge, and over-bonding inside. The width of the first separator blank 19 is the distance between two adjacent negative electrode sheets 22.

[0027] Furthermore, as a preferred embodiment, the arc length of the second metal layer 102 is 0.5-1 mm smaller than the width of the positive electrode 21. This smaller arc length of the second metal layer 102 avoids excessive pressure and heating on the edge of the positive electrode 21. The spacing between two adjacent positive electrode 21 is the second separator blank 25. The arc length of the second thermally conductive silicone 103 is 0.5-1 mm larger than the width of the second separator blank 25. This larger arc length of the second thermally conductive silicone 103 ensures effective bonding to the second separator blank 25 area. The width of the second separator blank 25 is the spacing between two adjacent positive electrode 21.

[0028] A thermal composite lamination system includes a thermal composite process composite roller mechanism, and further includes a first process guide roller 3, a first conveyor belt 4, a first heating plate 5, a first composite guide roller 6, a first cutting blade 7, a first electrode positioning laser sensor 8, and a controller 9. The first process guide roller 3, the first conveyor belt 4, the first cutting blade 7, the first composite guide roller 6, the first electrode positioning laser sensor 8, the negative electrode thermal composite roller mechanism 2, and the positive electrode thermal composite roller mechanism 1 are arranged sequentially along the feeding direction. The first heating plate 5, the first cutting blade 7, and the first electrode positioning laser sensor 8 are all located above the first conveyor belt 4. The controller 9 is connected to the first electrode positioning laser sensor 8. In this embodiment, the first process guide roller 3 is used to guide the movement of the negative electrode 22, the first conveyor belt 4 is used to drive the movement of the negative electrode 22, the first heating plate 5 is used to heat the negative electrode 22, and two first composite guide rollers 6 are provided. (See also...) Figure 8 As shown, the first composite guide roller 6 is used to guide the diaphragm 23 to move, so that the diaphragm 23 enters the negative electrode hot composite roller mechanism 2, the first cutting blade 7 is used to cut the negative electrode sheet 22, and the first electrode sheet positioning laser sensor 8 is used to detect the position and width information of the negative electrode sheet 22 and feed it back to the controller 9.

[0029] Furthermore, as a preferred embodiment, it also includes a second heating plate 10, a second conveyor belt 11, a positive electrode conveying mechanism 12, and a second electrode positioning laser sensor 13. The second conveyor belt 11, the positive electrode conveying mechanism 12, and the second electrode positioning laser sensor 13 are sequentially arranged between the negative electrode thermal composite roller mechanism 2 and the positive electrode thermal composite roller mechanism 1 along the feeding direction. The second heating plate 10 is arranged above the second conveyor belt 11. The second electrode positioning laser sensor 13 is connected to the controller 9. There are two positive electrode conveying mechanisms 12, which are distributed on both sides of the second conveyor belt 11. Each positive electrode conveying mechanism 12 includes a third conveyor belt 121, a third heating plate 122, and a second cutting blade 123. The third conveyor belt 121 is used to convey the positive electrode 21. The third heating plate 122 and the second cutting blade 123 are arranged above the third conveyor belt 121. The second heating plate 10 is used to heat the negative electrode 22 and the diaphragm 23. The second electrode positioning laser sensor 13 is used to detect the position and width information of the positive electrode 21 and feed it back to the controller 9. The positive electrode conveying mechanism 12 is used to convey the positive electrode 21 into the system.

[0030] Furthermore, as a preferred embodiment, it also includes a second composite guide roller 14 and a second process guide roller 15. The second composite guide roller 14 is located between the positive electrode sheet conveying mechanism 12 and the positive electrode hot composite roller mechanism 1. A plurality of second process guide rollers 15 are arranged on the side of the positive electrode hot composite roller mechanism 1 away from the second composite guide roller 14. In this embodiment, the second composite guide roller 14 is used to guide the movement of the positive electrode sheet 21, the negative electrode sheet 22, and the separator 23. The separator 23, the positive electrode sheet 21, and the negative electrode sheet 22 are composited together by the positive electrode hot composite roller mechanism 1 to form an electrode composite unit 24. A third separator gap 20 is provided between two adjacent electrode composite units 24. The second process guide rollers 15 are used to guide the movement of the electrode composite unit 24.

[0031] Furthermore, as a preferred embodiment, the system also includes a third cutting blade 16, a CCD sensor 17, and a stacking platform 18. The CCD sensor 17, the third cutting blade 16, and the stacking platform 18 are sequentially arranged on the side of the second process guide roller 15 away from the positive electrode hot composite roller mechanism 1. The CCD sensor 17 is connected to the controller 9. The third cutting blade 16 is used to cut the electrode composite unit 24 to meet the finished product size requirements, while the stacking platform 18 stacks the cut electrode sheets. The CCD sensor 17 can perform quality inspection on the composited electrode sheets. This system setup achieves automated and precise control of the hot composite stacking process of power lithium-ion battery electrode sheets. By controlling the coordinated operation of each component through the controller 9, the problems of inaccurate electrode sheet processing and poor composite effect in traditional processes are effectively solved. The entire system can precisely control the electrode sheet conveying, heating, composite, cutting, and stacking processes, improving production efficiency and product quality. In this embodiment, the controller 9 can be a PLC controller 9, which is connected to the first heating plate 5, the second heating plate 10, and the third heating plate 122. The first cutting blade 7, the second cutting blade 123, and the third cutting blade 124 can be driven by an external cylinder to cut the negative electrode 22, the positive electrode 21, and the electrode composite unit 24. The first conveyor belt 4, the second conveyor belt 11, and the third conveyor belt 121 can be driven by an external conveyor belt drive mechanism, and both the cylinder and the conveyor belt drive mechanism can be connected to the controller 9.

[0032] In use, the negative electrode sheet 22 is conveyed to the cutting position via the first conveyor belt 4, while the first heating plate 5 heats the negative electrode sheet 22 to preheat it. The negative electrode sheet 22 is guided into the negative electrode hot composite roller mechanism 2 via the first composite guide roller 6. Simultaneously, the diaphragm 23 enters the negative electrode hot composite roller mechanism 2 via the first composite guide roller 6 to composite with the negative electrode sheet 22. Furthermore, the first electrode positioning laser sensor 8 detects the position and width information of the negative electrode sheet 22 and feeds it back to the controller 9. The controller 9 then transmits the information to the cylinder in the first cutting blade 7 to control the cutting position and cutting time of the first cutting blade 7 to obtain negative electrode sheets 22 with the same width and to control the spacing between pairs of negative electrode sheets 22. Furthermore, the composite process of the diaphragm 23 and the negative electrode sheet 22 is completed by the negative electrode hot composite roller mechanism 2. When the negative electrode thermal composite roller mechanism 2 is used to composite the negative electrode sheet 22 and the separator 23, the arc length portion of the first metal layer 202 contacts the area where the negative electrode sheet 22 is located, which can effectively composite the separator 23 and the negative electrode sheet 22. The first thermally conductive silicone 203 mainly contacts the first separator blank 19, and the arc length of 0.25~0.5mm on each side contacts the edge of the negative electrode sheet 22. That is, the negative electrode thermal composite roller mechanism 2 can use the buffering capacity of the first thermally conductive silicone 203 to make the first metal layer 202 part transition to the surface of the negative electrode sheet 22, avoiding damage and material loss at the edge of the negative electrode sheet 22. Furthermore, the heat sealing strip 204 can heat and heat the separator 23 on both sides of the negative electrode sheet 22 together during the contact with the first separator blank 19, further limiting the position of the negative electrode sheet 22. Furthermore, the first electrode positioning laser sensor 8 can effectively control the accurate positioning of the negative electrode sheet 22 and the negative electrode thermal composite roller mechanism 2.

[0033] After the negative electrode 22 and the separator 23 are combined by the negative electrode thermal composite roller mechanism 2, they continue to be transported by the second conveyor belt 11 and enter the positive electrode conveying mechanism 12 via the second composite guide roller 14. During this process, the second heating plate 10 preheats the negative electrode 22 and the separator 23. Then, the positive electrode 21 is guided into the positive electrode thermal composite roller mechanism 1 by the second composite guide roller 14. Further, the second electrode positioning laser sensor 13 detects the position and width information of the positive electrode 21 and feeds it back to the controller 9. The controller 9 then transmits the information to the cylinder of the second cutting blade 123 to control the cutting position and cutting time to obtain positive electrode 21s of the same width and to control the spacing between pairs of positive electrode 21s. Further, the arc length of the second metal layer 102 is 0.5~1mm smaller than the width of the positive electrode 21; the arc length of the second thermally conductive silicone 103 is 0.5~1mm larger than the width of the second separator blank 25. Furthermore, when the positive electrode thermal composite roller mechanism 1 is composited with the positive electrode 21, the separator 23, and the negative electrode 22, the arc length portion of the second metal layer 102 contacts the area where the positive electrode 21 is located, which can effectively composite the separator 23 with the positive electrode 21 and the negative electrode 22. The second thermally conductive silicone 103 mainly contacts the blank portion of the second separator, and the arc lengths of 0.25~0.5mm on both sides contact the edge of the positive electrode 21. That is, the positive electrode thermal composite roller mechanism 1 can use the buffering capacity of the second thermally conductive silicone 103 to allow the metal part to transition to the surface of the positive electrode 21, avoiding damage and material loss at the edges of the positive electrode 21 and the negative electrode 22.

[0034] The composite positive electrode 21, separator 23 and negative electrode 22, i.e. electrode composite unit 24, are brought to the stacking platform 18 by the second process guide roller 15 for "Z"-shaped stacking. The number of composite electrode layers is further detected by the CCD sensor 17 and fed back to the controller 9 for processing. The controller 9 further compares the number of layers with the preset number and feeds back to the stacking platform 18. The third cutter 16 cuts the third separator blank 20 in time to complete the production of a single core stack.

[0035] The above description is only a preferred embodiment of the present utility model and does not limit the implementation method and protection scope of the present utility model. Those skilled in the art should realize that all solutions obtained by equivalent substitutions and obvious changes made based on the description and illustrations of the present utility model should be included within the protection scope of the present utility model.

Claims

1. A thermal compounding process compounding roll mechanism characterized by, The device includes a positive electrode thermal composite roller mechanism and a negative electrode thermal composite roller mechanism, which are arranged sequentially along the feeding direction. The negative electrode thermal composite roller mechanism includes a first roller body, a first metal layer, and a first thermally conductive silicone. The two first roller bodies are arranged facing each other. The first metal layer is sleeved on the outer wall of the first roller body. A first mounting groove is opened on the outer wall of the first roller body, and the first thermally conductive silicone is installed in the first mounting groove.

2. The composite roller mechanism for the thermal composite process as described in claim 1, characterized in that, It also includes a heat-sealing strip, which is disposed in the middle of the first thermally conductive silicone and extends out of the first thermally conductive silicone.

3. The composite roller mechanism for the thermal composite process as described in claim 1, characterized in that, The arc length of the first metal layer is 0.5~1mm smaller than the width of the negative electrode sheet; The gap between two adjacent negative electrode plates is the first diaphragm blank, and the arc length of the first thermally conductive silicone is 0.5~1mm larger than the width of the first diaphragm blank.

4. The composite roller mechanism for the thermal composite process as described in claim 3, characterized in that, The perimeter of the negative electrode thermal composite roller mechanism is equal to the sum of the width of the negative electrode sheet and the blank width of the first diaphragm.

5. The composite roller mechanism for the thermal composite process as described in claim 1, characterized in that, The positive electrode thermal composite roller mechanism includes a second roller body, a second metal layer, and a second thermally conductive silicone rubber. The two second roller bodies are arranged facing each other. The second metal layer is sleeved on the outer wall of the second roller body. A second mounting groove is opened on the outer wall of the second roller body, and the second thermally conductive silicone rubber is disposed in the second mounting groove.

6. The composite roller mechanism for the thermal composite process as described in claim 5, characterized in that, The arc length of the second metal layer is 0.5-1 mm smaller than the width of the positive electrode sheet, the spacing between two adjacent positive electrode sheets is the blank space of the second separator, and the arc length of the second thermally conductive silicone is 0.5-1 mm larger than the width of the blank space of the second separator.

7. A thermal composite lamination system, comprising the composite roller mechanism of the thermal composite process as described in any one of claims 1-6, characterized in that, It also includes a first process guide roller, a first conveyor belt, a first heating plate, a first composite guide roller, a first cutting blade, a first electrode positioning laser sensor, and a controller. The first process guide roller, the first conveyor belt, the first cutting blade, the first composite guide roller, the first electrode positioning laser sensor, the negative electrode thermal composite roller mechanism, and the positive electrode thermal composite roller mechanism are arranged sequentially along the feeding direction. The first heating plate, the first cutting blade, and the first electrode positioning laser sensor are all located above the first conveyor belt. The controller is connected to the first electrode positioning laser sensor.

8. The thermal composite stacking system as described in claim 7, characterized in that, It also includes a second heating plate, a second conveyor belt, a positive electrode sheet conveying mechanism, and a second electrode sheet positioning laser sensor. The second conveyor belt, the positive electrode sheet conveying mechanism, and the second electrode sheet positioning laser sensor are sequentially arranged between the negative electrode thermal composite roller mechanism and the positive electrode thermal composite roller mechanism along the feeding direction. The second heating plate is arranged above the second conveyor belt. The second electrode sheet positioning laser sensor is connected to the controller. There are two positive electrode sheet conveying mechanisms, which are distributed on both sides of the second conveyor belt. Each positive electrode sheet conveying mechanism includes a third conveyor belt, a third heating plate, and a second cutting blade. The third conveyor belt is used to convey the positive electrode sheet. The third heating plate and the second cutting blade are arranged above the third conveyor belt.

9. The thermal composite stacking system as described in claim 8, characterized in that, It also includes a second composite guide roller and a second process guide roller. The second composite guide roller is located between the positive electrode sheet conveying mechanism and the positive electrode hot composite roller mechanism. The positive electrode hot composite roller mechanism has a plurality of second process guide rollers on the side away from the second composite guide roller.

10. The thermal composite stacking system as described in claim 9, characterized in that, It also includes a third cutting blade, a CCD sensor, and a stacking platform. The CCD sensor, the third cutting blade, and the stacking platform are sequentially arranged on the side of the second process guide roller away from the positive electrode thermal composite roller mechanism. The CCD sensor is connected to the controller.