Silicon carbide gold oxide semiconductor field-effect transistor
By setting three-dimensional trenches and voltage-resistant rings in silicon carbide gold-oxide-semiconductor field-effect transistors, the source contact resistance is reduced, solving the problem of high on-resistance of existing SiC MOSFETs, achieving higher stability and power loss performance, and making it suitable for electronic devices for high-speed computing and high-frequency communication.
Patent Information
- Application Number
- CN202522394629.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Priority Date
- 2025-09-26
- Filing Date
- 2025-11-12
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-12
AI Technical Summary
Existing silicon carbide metal-oxide-semiconductor field-effect transistors (SiC MOSFETs) have high source-to-source contact resistance, which prevents the on-resistance (Ron) from being further reduced, thus failing to meet the requirements of high-speed computing, high-frequency communication, and high-power electronic devices.
A silicon carbide metal-oxide-semiconductor field-effect transistor (MOSFET) was designed. By setting a three-dimensional trench between the source and the heavily doped region and connecting the contact metal through the via of the dielectric layer, the contact area is increased to reduce the contact resistance of the source. At the same time, a voltage-resistant ring is set around the transistor to distribute the voltage evenly, simplifying the fabrication process.
It effectively reduces the on-resistance of transistors and improves stability and power loss performance under high temperature, high pressure or high current environments, meeting the needs of high-frequency communication and high-power electronic devices.
Smart Images

Figure CN224987892U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to a field-effect transistor, and more particularly to a silicon carbide gold oxide field-effect transistor. Background Technology
[0002] In response to the development of 5G, artificial intelligence, and other technological industries, there is a need to develop electronic devices that can support high-speed computing, high-frequency communication, and high power. Existing silicon (Si)-based components are no longer sufficient to meet these demands. In contrast, silicon carbide (SiC) has a bandgap approximately three times that of silicon, a collapse electric field ten times that of silicon, and a higher thermal conductivity. Therefore, electronic components based on silicon carbide exhibit better stability under high-temperature, high-pressure, or high-current operating environments.
[0003] Taking a planar SiC MOSFET as an example, the transistor's on-resistance (R) on It must include at least the channel resistance (R) of the source. Channel ) and the drift resistance (R) of the drift region Drift On-resistance represents the resistance between the source and drain of a transistor when it is in the on-state. A lower on-resistance indicates lower power loss during conduction. However, the contact resistance between the source electrodes in current transistors is still relatively high, leading to an overall on-resistance (R0). on The on-resistance (Ron) of SiC MOSFETs cannot be further reduced. Therefore, it is necessary to develop a method that can further reduce the on-resistance (Ron) of SiC MOSFETs. on ) component design. Utility Model Content
[0004] The purpose of this invention is to provide a silicon carbide metal oxide field-effect transistor that can reduce the source contact resistance.
[0005] The silicon carbide metal-oxide-semiconductor field-effect transistor of this invention comprises a silicon carbide substrate, an epitaxial layer, a well region, a heavily doped region, a source, a planar gate structure, and a contact metal.
[0006] The epitaxial layer is disposed on the upper side of the silicon carbide substrate. The well region is disposed on the upper side of the epitaxial layer. The heavily doped region is located in the well region. The source electrode is disposed in the well region and distributed on the upper side of the heavily doped region, and together with the heavily doped region, defines an upward-opening three-dimensional trench. The planar gate structure is disposed above the epitaxial layer and is connected to the source electrode. The contact metal is electrically connected to the heavily doped region and the source electrode through the three-dimensional trench.
[0007] The silicon carbide gold oxide field-effect transistor of this invention further includes at least one voltage-delay ring surrounding the outside of the well region, the depth of the at least one voltage-delay ring being the same as the depth of the heavily doped region.
[0008] The silicon carbide gold oxide field-effect transistor of this invention has a heavily doped region with a top surface, a source electrode with a top surface and an inner surface, and a three-dimensional trench formed by the top surface of the heavily doped region and the inner surface of the source electrode.
[0009] In this invention, a silicon carbide gold-oxide-semiconductor field-effect transistor is provided, wherein the contact metal is electrically connected to the top surface of the heavily doped region and the top and inner surfaces of the source electrode.
[0010] The silicon carbide gold oxide semiconductor field-effect transistor of this invention further includes an ohmic contact layer, which is disposed between the contact metal and the electrically connected region of the heavily doped region and the source electrode.
[0011] The silicon carbide gold oxide semiconductor field-effect transistor of this invention also includes a junction field-effect transistor, which is disposed between the epitaxial layer and the planar gate structure.
[0012] The silicon carbide gold oxide field-effect transistor of this invention further includes a dielectric layer, which fills the space between the planar gate structure, the source and the contact metal. The dielectric layer has a through-hole that communicates downward with the three-dimensional trench, and the through-hole allows the contact metal to extend downward and fill the three-dimensional trench.
[0013] The beneficial effect of this utility model is that the contact metal electrically connects the source and the heavily doped region through the three-dimensional trench, thereby increasing the contact area and reducing the contact resistance of the source, thereby reducing the overall on-resistance of the MOSFET. Attached Figure Description
[0014] Other features and effects of this utility model will be clearly presented in the embodiments with reference to the accompanying drawings, wherein:
[0015] Figure 1 This is a schematic diagram of one embodiment of the silicon carbide gold oxide semiconductor field-effect transistor of this utility model;
[0016] Figure 2 This is a schematic diagram of a transistor unit in the embodiment described above;
[0017] Figure 3 This is a flowchart of the manufacturing method of the embodiment described;
[0018] Figure 4 This is a partial cross-sectional side view of steps S1 to S3 of the manufacturing method described above;
[0019] Figure 5 This is a partial cross-sectional side view of step S4 of the manufacturing method;
[0020] Figure 6This is a partial cross-sectional side view of step S5 of the manufacturing method;
[0021] Figure 7 This is a partial cross-sectional side view of step S6 of the manufacturing method;
[0022] Figures 8-10 This is a partial cross-sectional side view of step S7 of the manufacturing method;
[0023] Figures 11-12 This is a partial cross-sectional side view of step S8 of the manufacturing method;
[0024] Figure 13 This is a partial cross-sectional side view of step S9 of the manufacturing method;
[0025] Figure 14 This is a partial cross-sectional side view of step S10 of the manufacturing method. Detailed Implementation
[0026] See Figure 1 An embodiment of the silicon carbide gold oxide field-effect transistor of the present invention includes a plurality of transistor units 1 and an outer ring structure 2.
[0027] It should be noted that the silicon carbide gold-oxide-semiconductor field-effect transistor of this invention comprises multiple periodically arranged transistor units 1, but for ease of explanation, Figure 2 The diagram shows the structure of a single transistor unit 1. The transistor unit 1 includes a silicon carbide substrate 11, an epitaxial layer 12, a well region 13, a heavily doped region 14, a source 15, a planar gate structure 16, a junction field-effect transistor 17, a dielectric layer 3, an ohmic contact layer 4, and a contact metal 5.
[0028] The epitaxial layer 12 is disposed on the upper side of the silicon carbide substrate 11, and its material includes silicon carbide. The well region 13 is disposed on the upper side of the epitaxial layer 12 and is formed by a portion of the epitaxial layer 12 through a first type of doping. Optionally, the first type of doping is P-type doping. The heavily doped region 14 is located in the well region 13 and is formed by a portion of the well region 13 through a first type of heavy doping. The source 15 is disposed in the well region 13 and is formed by a portion of the epitaxial layer 12 through a second type of doping, and is distributed on the upper side of the heavily doped region 14, and together with the heavily doped region 14 defines an upward-facing three-dimensional trench 101. Optionally, the second type of doping is N-type doping. It should be noted that... Figure 2The transistor unit 1 appears to have two sources 15, but in reality there is only one source 15, which is located on both sides above the heavily doped region 14 when viewed from the side.
[0029] Specifically, the heavily doped region 14 has a top surface 141, the source electrode 15 has a top surface 151 and an inner surface 152, and the three-dimensional trench 101 is formed by the top surface 141 of the heavily doped region 14 and the inner surface 152 of the source electrode 15.
[0030] The planar gate structure 16 is disposed above the epitaxial layer 12 and connected to the source 15. Specifically, the planar gate structure 16 has an oxide layer 161 and a polysilicon layer 162. (See also...) Figure 1 The junction gate field effect transistor 17 (JFET) is disposed between the epitaxial layer 12 and the planar gate structure 16, and is located between adjacent well regions 13. It should be noted that... Figure 2 In the single transistor unit 1 shown, the planar gate structure 16 appears to be present on both the left and right sides, but in reality, there is half on each side. Therefore, in general, the single transistor unit 1 includes only one planar gate structure 16. (See reference...) Figure 1 Half of the planar gate structure 16 needs to be combined with the other half of the planar gate structure 16 of the adjacent transistor unit 1 to constitute a complete planar gate structure 16. Similarly, the junction field-effect transistor 17 is calculated in the same way, and in general, only one junction field-effect transistor 17 is included in a single transistor unit 1.
[0031] Specifically, when the first type of doping of the well region 13 is P-type doping, the junction field-effect transistor 17 will adopt an N-type JFET to reduce the on-resistance.
[0032] The dielectric layer 3 fills the space between the planar gate structure 16, the source 15, and the contact metal 5. The dielectric layer 3 has a via 301 that communicates downward with the three-dimensional trench 101.
[0033] The contact metal 5 extends downward through the through-hole 301 and fills the three-dimensional trench 101, and electrically connects the top surface 141 of the heavily doped region 14 and the top surface 151 and inner surface 152 of the source electrode 15 through the three-dimensional trench 101. The ohmic contact layer 4 is disposed between the contact metal 5 and the electrical connection regions of the heavily doped region 14 and the source electrode 15.
[0034] See Figure 1 The outer ring structure 2 includes multiple edge termination rings 21 surrounding the outside of the transistor unit 1. The edge termination rings 21 are also first-type doped like the well region 13, and their depth (D1) is the same as the depth (D2) of the heavily doped region 14. By adjusting the width and spacing of the edge termination rings 21, the voltage in the transistor unit 1 can be distributed more evenly, increasing the stability of MOSFET operation.
[0035] In the embodiment described above, the number of pressure-resistant rings 21 is four, but this is not the limitation in other embodiments of this embodiment. The number of pressure-resistant rings 21 can be arbitrarily changed as needed.
[0036] See Figure 3 The flowchart of the manufacturing method of the embodiment includes steps S1 to S10, which will be used in conjunction with the following. Figures 4-14 Explanation in sections.
[0037] See Figure 4 In step S1, a silicon carbide substrate 11 is provided.
[0038] In step S2, an epitaxial layer 12 is formed on the silicon carbide substrate 11. Specifically, the material of the epitaxial layer 12 includes silicon carbide.
[0039] In step S3, a first mask 71 is formed, and a portion of the epitaxial layer 12 is subjected to a first type of doping to form a predetermined well region 61. Specifically, the first type of doping is p-type doping, and the corresponding dopant is, for example, but not limited to, aluminum, boron, gallium, or beryllium.
[0040] In step S4, refer to Figure 5 A second mask 72 is formed, and then the middle region of the predetermined well region 61 is subjected to a second type of doping to form a second type of doped region 62. The region in the predetermined well region 61 that has not undergone the second type of doping forms a well region 13. Then, the first mask 71 and the second mask 72 are removed. Specifically, the second type of doping is N-type doping, and the corresponding dopant is, for example, but not limited to, nitrogen or phosphorus.
[0041] The second mask 72 is formed while retaining the first mask 71, and the second mask 72 covers the top and side surfaces of the first mask 71, thereby enabling the first type of doping and the second type of doping to be performed continuously to define the well region predetermined region 61 and the second type of doped region 62 respectively. Finally, the first mask 71 and the second mask 72 are removed together, which has the advantage of simplifying the process steps.
[0042] In step S5, refer to Figure 6 A first-type doped region 63 is formed by performing first-type doping on the middle region of the second-type doped region 62 of each transistor cell 1 through a third mask 73. Simultaneously, first-type doping is performed on the outer periphery of the well region 13 of the outermost transistor cell 1 to form multiple breakdown rings 21. Specifically, the third mask 73 has multiple heavily doped region openings 701 and multiple breakdown ring openings 702. This allows first-type dopants to reach the epitaxial layer 12 and the second-type doped region 62 through the heavily doped region openings 701 and the breakdown ring openings 702. Then, the third mask 73 is removed.
[0043] In this way, the source 15 is formed in the region on both sides of the first type doped region 63 in the second type doped region 62. A portion of the first type doped region 63 overlaps with the well region 13 to form a heavily doped region 14. The doping concentration of the heavily doped region 14 is higher than that of the well region 13. The depth (D1) of the breakdown ring 21 is the same as the depth (D2) of the heavily doped region 14.
[0044] Optionally, the depth (D2) of the heavily doped region 14 can be flush with the depth (D3) of the well region 13, such as... Figure 1 As shown. Alternatively, the depth (D2) of the heavily doped region 14 can be greater than the depth (D3) of the well region 13, as shown. Figure 2 As shown.
[0045] It should be noted that in the above embodiment, the depth (D1) of the withstand voltage ring 21, the depth (D2) of the heavily doped region 14, and the depth (D3) of the well region 13 are all calculated with reference to the top surface 151 of the source electrode 15 and in the direction towards the silicon carbide substrate 11.
[0046] Since the heavily doped region 14 and the withstand voltage ring 21 are formed in the same step, it can be ensured that the depth of the withstand voltage ring 21 is the same as the depth of the heavily doped region 14, and the withstand voltage ring 21 and the heavily doped region 14 can be formed in the same process step, simplifying the process steps.
[0047] In step S6, refer to Figure 7 The planar gate structure 16 is formed above the epitaxial layer 12, and the planar gate structure 16 is connected to the source 15. Optionally, before forming the planar gate structure 16, the junction field-effect transistor 17 can be formed on the left and right sides of the well region 13.
[0048] In step S7, refer to Figure 8A photoresist 91 is coated on the planar gate structure 16, the first type of doped region 63, and the upper surface of the source 15. A pattern is formed on the photoresist 91 using a photolithography process with a photomask 8. Specifically, the photomask 8 is a Contact Trench P+ Process Mask (CTPP Mask), mainly used to form the three-dimensional trench 101. (See also...) Figure 9 The photoresist 91 forms an etching opening 901. The etching opening 901 exposes the upper surface of the first type of doped region 63.
[0049] See Figure 10 The etching process removes the portion of the first type of doped region 63 other than the heavily doped region 14 through the etching opening 901, so that a three-dimensional trench 101 with the opening facing upward is formed between the source 15 and the heavily doped region 14.
[0050] It must be specifically noted that steps S4 to S7 of the manufacturing method in this embodiment involve first performing a second type of doping on the middle region of the predetermined well region 61, then performing a first type of doping on the middle region of the second type of doped region 62 to form the heavily doped region 14, and finally removing the portion of the first type of doped region 63 other than the heavily doped region 14, thereby defining the range of the source electrode 15 and the heavily doped region 14. Since this process method does not require forming an island-shaped photoresist on the upper side of the middle region of the predetermined well region 61 before performing the second type of doping to form the source electrode 15, the problem of low process yield caused by the collapse and deformation of the island-shaped photoresist can be avoided during the process.
[0051] In step S8, refer to Figure 11 A dielectric material 92 is deposited, and a fourth mask 74 is formed on the dielectric material 92. For example... Figure 12 As shown, the via 301 connecting the three-dimensional trench 101 is formed in the dielectric material 92 by means of the fourth mask 74 through an etching process, and then the fourth mask 74 is removed to form the dielectric layer 3.
[0052] In step S9, refer to Figure 13 The ohmic contact layer 4 is formed in the via 301, and the ohmic contact layer 4 covers the heavily doped region 14 and the source electrode 15.
[0053] In step S10, refer to Figure 14The contact metal 5 is formed on the dielectric layer 3. The contact metal 5 extends downward from a top surface 31 of the dielectric layer 3 through the via 301 and fills the three-dimensional trench 101, and is electrically connected to the top surface 141 of the heavily doped region 14, the top surface 151 of the source 15, and the inner surface 152 of the source 15 via the ohmic contact layer 4.
[0054] In summary, the silicon carbide gold-oxide-semiconductor field-effect transistor and its manufacturing method of this invention, wherein the contact metal 5 electrically connects the source 15 and the heavily doped region 14 through the three-dimensional trench 101, thereby increasing the contact area and reducing the contact resistance of the source 15, thus reducing the overall on-resistance of the MOSFET, and thus effectively achieving the purpose of this invention. On the other hand, the outer ring structure 2 of this invention makes the depth of the withstand voltage ring 21 the same as the depth of the heavily doped region 14, which simplifies the manufacturing process.
[0055] The above description is merely an embodiment of this utility model and should not be construed as limiting the scope of this utility model. Any simple equivalent changes and modifications made in accordance with the claims and description of this utility model shall still fall within the scope of this utility model.
Claims
1. A silicon carbide gold oxide semiconductor field-effect transistor, characterized in that: The silicon carbide gold-oxide-semiconductor field-effect transistor includes: Silicon carbide substrate; An epitaxial layer is disposed on the upper side of the silicon carbide substrate; A trap region is disposed on the upper side of the epitaxial layer; The heavily doped region is located in the well region; The source electrode is disposed in the well region and distributed on the upper side of the heavily doped region, and together with the heavily doped region, defines an upward-facing three-dimensional trench. A planar gate structure is disposed above the epitaxial layer and connected to the source electrode; and The contact metal is electrically connected to the heavily doped region and the source electrode through the three-dimensional trench.
2. The silicon carbide gold oxide semiconductor field-effect transistor according to claim 1, characterized in that: The silicon carbide gold-oxide-semiconductor field-effect transistor further includes at least one breakdown ring surrounding the outside of the well region, wherein the depth of the at least one breakdown ring is the same as the depth of the heavily doped region.
3. The silicon carbide gold oxide semiconductor field-effect transistor according to claim 1, characterized in that: The heavily doped region has a top surface, the source electrode has a top surface and an inner surface, and the three-dimensional trench is formed by the top surface of the heavily doped region and the inner surface of the source electrode.
4. The silicon carbide gold oxide semiconductor field-effect transistor according to claim 3, characterized in that: The contact metal is electrically connected to the top surface of the heavily doped region and the top and inner surfaces of the source electrode.
5. The silicon carbide gold oxide semiconductor field-effect transistor according to claim 4, characterized in that: The silicon carbide gold-oxide-semiconductor field-effect transistor further includes an ohmic contact layer, wherein the ohmic contact layer is disposed between the contact metal and the electrically connected region of the heavily doped region and the source electrode.
6. The silicon carbide gold oxide semiconductor field-effect transistor according to claim 1, characterized in that: The silicon carbide gold-oxide-semiconductor field-effect transistor further includes a junction field-effect transistor, wherein the junction field-effect transistor is disposed between the epitaxial layer and the planar gate structure.
7. The silicon carbide gold oxide semiconductor field-effect transistor according to claim 1, characterized in that: The silicon carbide gold-oxide-semiconductor field-effect transistor further includes a dielectric layer, wherein the dielectric layer fills the space between the planar gate structure, the source and the contact metal, and the dielectric layer has a via that communicates downward with the three-dimensional trench, the via allowing the contact metal to extend downward and fill the three-dimensional trench.