A semiconductor structure
By optimizing the trench structure, alternating stacked seed layers, and multilayer doping design, the problems of electric field concentration, stress cracking, and uneven doping in semiconductor devices in high-voltage applications were solved, improving the reverse blocking voltage of the devices, reducing the on-resistance and crack rate, and achieving cost-effective process compatibility.
Patent Information
- Application Number
- CN202522094773.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-29
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-09-29
AI Technical Summary
In high-voltage applications, existing semiconductor devices suffer from performance bottlenecks caused by electric field concentration at the bottom corner of the trench, stress cracking of the epitaxial layer, and uneven doping distribution. Traditional doping processes struggle to balance forward conduction resistance and reverse withstand voltage characteristics, and trench isolation materials are prone to internal stress during filling.
The design incorporates curved trench corners, alternating seed layers, multi-layered doped regions with depth gradient distribution and buffer layers, combined with a low-roughness buffer layer and a porous dielectric liner layer, to optimize electric field distribution and stress buffering, and is achieved through conventional semiconductor processes.
It increases reverse blocking voltage by 20%~30%, reduces crack incidence by more than 40%, reduces forward conduction resistance by 20%, reduces leakage current by 50%, and reduces production costs by 15%~20%.
Smart Images

Figure CN224987893U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of semiconductor processing technology, and specifically relates to a semiconductor structure. Background Technology
[0002] Existing semiconductor devices (such as gallium nitride-based power devices) often face performance bottlenecks in high-voltage applications due to electric field concentration at the bottom corners of trenches, epitaxial layer stress cracking, and uneven doping distribution. Traditional trench structures often employ right-angle or acute-angle corner designs, which easily generate peak electric fields and reduce reverse blocking voltage. Due to lattice mismatch and differences in thermal expansion coefficients between the epitaxial layer and the substrate, through-cracks are prone to occur. Seed layers are often single-material layers, which cannot effectively buffer the stress between the substrate and the epitaxial layer, leading to a decrease in device reliability.
[0003] Furthermore, in traditional doping processes, the doping concentration of epitaxial layers is often uniformly distributed or designed with a simple gradient, making it difficult to simultaneously achieve both forward conduction resistance and reverse breakdown voltage characteristics. At the same time, the trench isolation material is prone to internal stress due to volume expansion during filling, further exacerbating epitaxial layer defects. To address these issues, this design aims to improve the uniformity of electric field distribution, structural stability, and electrical performance of semiconductor devices by optimizing the trench structure, alternating seed layer stacking design, and controlling the depth gradient of the doping region. Utility Model Content
[0004] In order to solve the above-mentioned problems in the prior art, the present invention provides a semiconductor structure that can improve the above deficiencies.
[0005] This utility model relates to a semiconductor structure, including a substrate; A seed layer is disposed on the upper part of the substrate and is composed of alternating layers of silicon-doped aluminum nitride and aluminum nitride, wherein the silicon-doped aluminum nitride layer is formed by ion implantation. A buffer layer is disposed on the upper part of the seed crystal layer, and the material of the buffer layer is the same as the base material of the seed crystal layer (i.e., aluminum nitride). An epitaxial layer is disposed on the upper part of the buffer layer, including a first doped layer, a second doped layer and a third doped layer stacked from top to bottom. The first doped layer is located above the second doped layer and the third doped layer is located below the second doped layer. The depth of the doped region of the first doped layer is smaller than that of the second doped layer, and the depth of the doped region of the second doped layer is smaller than that of the third doped layer. The trench is formed in the epitaxial layer. The bottom corner of the trench has an arc-shaped structure. The inner wall is covered with a porous dielectric material lining layer and the interior is filled with an insulating material.
[0006] Furthermore, the total thickness of the seed layer is ≤500nm, and the ratio of silicon-doped aluminum nitride layer to aluminum nitride layer is 1:1 to 2:1.
[0007] Furthermore, the depth of the doped regions of the first doped layer, the second doped layer, and the third doped layer ranges from 10% to 80% of the substrate thickness, and the depth increases linearly from top to bottom.
[0008] Furthermore, the trench is V-shaped, with the bottom corners transitioning to an arc surface, wherein the corner radius is 50~100nm, the porosity of the lining layer is 20%~50%, and the insulating material is a silicon oxide-based composite material.
[0009] Furthermore, a metal layer is disposed on the bottom surface of the substrate, the thickness of the metal layer being 1~5μm, and electrically connected to the metal filling layer inside the trench.
[0010] Furthermore, the epitaxial layer also includes an aluminum nitride insertion layer, which is located between the second doped layer and the third doped layer, and has a thickness of 50~200nm.
[0011] Furthermore, the thickness of the buffer layer is ≤500nm, and the interlayer roughness between the buffer layer and the seed crystal layer is ≤5nm.
[0012] Furthermore, it also includes a fourth doped layer, which extends downward from the top surface of the first doped layer to a depth of 1 / 2 to 2 / 3 of the depth of the doped region of the first doped layer.
[0013] Furthermore, the substrate is a silicon substrate, and the substrate surface has a nanoscale uneven structure. Beneficial effects: Electric field optimization: The trench arc corner design reduces the local electric field intensity, and combined with the depth gradient distribution of the epitaxial layer doping region, the reverse blocking voltage is increased by 20%~30%; Stress buffering: The alternating stacked seed crystal layer structure and low roughness buffer layer alleviate the lattice mismatch stress between the substrate and the epitaxial layer, reducing the crack incidence rate by more than 40%. Precise control of doping: By replacing the concentration gradient with the depth of the doping region, the limitation of material composition is avoided, which meets the requirements of utility model examination, while ensuring the balance between forward conduction resistance and reverse withstand voltage. Process compatibility: All structural parameters are achieved through conventional semiconductor processes (such as ion implantation and PECVD deposition), without the need for special equipment, reducing production costs by 15% to 20%. Attached Figure Description
[0014] Figure 1 This is a schematic diagram of the structure of this utility model.
[0015] Figure 2 This is a diagram showing the relationship between the second doped layer, the aluminum nitride insertion layer, and the third doped layer.
[0016] Figure 3 This is a schematic diagram of the channel structure.
[0017] The diagram shows: 1. Substrate, 2. Seed layer, 3. Buffer layer, 4. Epitaxial layer, 41. First doped layer, 42. Second doped layer, 43. Third doped layer, 44. Fourth doped layer, 5. Metal layer, 6. Channel, 61. Liner layer, 62. Isolation material, 7. Aluminum nitride insertion layer. Detailed Implementation
[0018] To make the objectives, technical solutions, and advantages of this utility model clearer, the present utility model will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the present utility model and are not intended to limit the scope of the present utility model.
[0019] like Figure 1 As shown in Embodiment 1, this utility model relates to a semiconductor structure, including a substrate 1; a seed layer 2, a buffer layer 2, an epitaxial layer 4, and a trench 6.
[0020] Substrate 1: The substrate is the fundamental supporting component of this semiconductor structure, and its material selection must comprehensively consider factors such as lattice mismatch, coefficient of thermal expansion, and cost. In this embodiment, substrate 101 is made of n-type silicon with a thickness of 500 μm. To enhance the electrical performance of substrate 101, a titanium-nickel-gold metal layer with a total thickness of 3 μm is sputtered onto its bottom surface. Furthermore, the surface of substrate 101 has a nanoscale uneven structure with a height of 10 nm and a spacing of 50 nm. This structure helps improve the adhesion between substrate 101 and subsequent layers, as well as its electrical performance.
[0021] Seed layer 2: Located on the upper surface of the substrate, the seed layer's main function is to form nucleation sites on the substrate surface, which is beneficial for the subsequent growth of the epitaxial layer. It also effectively prevents silicon from diffusing from the substrate into the epitaxial layer, reducing the reaction between silicon and the epitaxial layer material, thereby obtaining a high-quality epitaxial layer. Seed layer 102 is composed of alternating layers of silicon-doped aluminum nitride and aluminum nitride, with the silicon-doped aluminum nitride layers formed by ion implantation. In this embodiment, the seed layer comprises a four-layer structure, where the silicon-doped aluminum nitride layer is 50 nm thick with a silicon doping concentration of 1E18; the aluminum nitride layer is also 50 nm thick, for a total thickness of 200 nm. This alternating layer structure can better buffer the lattice mismatch stress between the substrate and the epitaxial layer, improving device reliability.
[0022] Buffer layer 3: The buffer layer is disposed above the seed layer. Its main function is to effectively alleviate lattice mismatch and thermal mismatch between the epitaxial layer and the substrate, reduce strain caused by stress in the epitaxial layer, and reduce the occurrence of dislocations and defects. The material of the buffer layer 103 is the same as the base material of the seed layer, namely aluminum nitride. In this embodiment, the thickness of the buffer layer 103 is 300 nm, which is prepared by atomic layer deposition (ALD) process, and the interface roughness is 3 nm. The ALD process parameters are: temperature 300°C, pressure 1 Torr, and deposition rate 0.1 nm / cycle. This low-roughness buffer layer can further improve the quality of the epitaxial layer and reduce the generation of cracks.
[0023] Epitaxial Layer: The epitaxial layer, located on top of the buffer, is the core component of this semiconductor structure and is used to implement the main electrical functions of the device. The epitaxial layer comprises a first doped layer 41, a second doped layer 42, and a third doped layer 43, stacked sequentially from top to bottom. The first doped layer is located above the second doped layer, and the third doped layer 43 is located below the second doped layer. The first doped layer has a doping depth of 50 μm, is implanted with magnesium ions at a doping concentration of 1E17 / cm³, and the ion implantation parameters are: implantation energy 100 keV, dose 1E14 / cm². The second doped layer has a doping depth of 100 μm and a doping concentration of 5E16 / cm³. The third doped layer has a doping depth of 200 μm and a doping concentration of 1E16 / cm³. This gradient distribution of doping depth optimizes the electric field distribution, improves the reverse blocking voltage of the device, and reduces the forward conduction resistance.
[0024] In addition, a fourth doped layer and an aluminum nitride insertion layer 7 are also provided in the epitaxial layer. The fourth doped layer 1044 extends downward from the top surface of the first doped layer, with an extension depth of 1 / 2 to 2 / 3 of the depth of the doped region of the first doped layer, i.e., an extension depth of 0.6 μm. This design can further optimize the electric field distribution and reduce electric field concentration. The aluminum nitride insertion layer is located between the second and third doped layers, with a thickness of 100 nm. The main function of the insertion layer is to place the subsequently grown epitaxial layer in a compressive strain state, reduce stress and dislocations in the epitaxial layer, and thus eliminate cracks in the epitaxial layer, resulting in a high-quality, crack-free epitaxial layer.
[0025] Trench 6: Trench 6 is formed in the epitaxial layer by dry etching to form a V-shaped trench (4μm deep). The bottom corner is transitioned by an arc surface with a corner radius of 50~100nm. This design can reduce the local electric field intensity and avoid the formation of peak electric field, thereby improving the reverse blocking voltage of the device.
[0026] The inner wall of trench 106 is covered with a porous dielectric liner layer with a porosity of 30% and a thickness of 50 nm. The liner layer is made of porous silicon nitride, prepared by PECVD deposition using SiH4 and NH3 as deposition gases at a temperature of 350°C. The interior of trench 106 is filled with an insulating material, SiO2, deposited by CVD using SiH4 and O2 as deposition gases at a temperature of 400°C. This insulating material effectively isolates different areas, preventing electrical interference. Furthermore, the filling process does not generate internal stress due to volume expansion, further improving device reliability. Example
[0027] This embodiment has a basically the same structure as Embodiment 1, except that: The seed layer has a layer ratio of 2:1, consisting of 6 silicon-doped aluminum nitride layers and 3 aluminum nitride layers, with a total thickness of 450 nm. This structure can further optimize the performance of the seed layer and improve its ability to buffer lattice mismatch stress between the substrate and the epitaxial layer.
[0028] The trench lining is made of silicon oxynitride with a porosity of 40%. The insulating material, 1062, is made of SiON. This combination of materials provides better electrical performance and stability, making it suitable for various applications. Example
[0029] This embodiment has a basically the same structure as Embodiment 1, except that: Substrate 1 is made of silicon carbide, which has better thermal conductivity and electrical properties and is suitable for special applications such as high temperature and high frequency.
[0030] The epitaxial layer 4 does not have an aluminum nitride insertion layer 105. This structure simplifies the manufacturing process, reduces production costs, and can still meet performance requirements in certain application scenarios.
[0031] Trench 6 is U-shaped with a bottom corner radius of 100 nm. This structure can further optimize the electric field distribution, improve the reverse blocking voltage of the device, and reduce stress concentration, thereby improving the reliability of the device.
[0032] Compared to traditional right-angle corner structures, the semiconductor structure described in the above embodiments exhibits a 30% increase in reverse blocking voltage (from 900V to 1200V), a 20% reduction in forward conduction resistance (from 0.625Ω·cm² to 0.5Ω·cm²), a 50% reduction in leakage current (reaching 1E-7A / cm²), and a 40% reduction in crack incidence. These performance improvements demonstrate that the semiconductor structure of this invention possesses significant advantages in electric field optimization, stress buffering, precise doping control, and process compatibility. It can effectively solve the problems existing in the prior art and improve the overall performance and reliability of semiconductor devices.
[0033] Note: In the above embodiments, the thickness of each layer, the doping depth, and the material selection can be adjusted according to actual needs.
Claims
1. A semiconductor structure, characterized in that: Including substrate; A seed layer is disposed on the upper part of the substrate and is composed of alternating layers of silicon-doped aluminum nitride and aluminum nitride, wherein the silicon-doped aluminum nitride layer is formed by ion implantation. A buffer layer is disposed on the upper part of the seed crystal layer and is made of the same base material as the seed crystal layer. An epitaxial layer is disposed on the upper part of the buffer layer, including a first doped layer, a second doped layer and a third doped layer stacked from top to bottom. The first doped layer is located above the second doped layer and the third doped layer is located below the second doped layer. The depth of the doped region of the first doped layer is smaller than that of the second doped layer, and the depth of the doped region of the second doped layer is smaller than that of the third doped layer. The trench is formed in the epitaxial layer. The bottom corner of the trench has an arc-shaped structure. The inner wall is covered with a porous dielectric material lining layer and the interior is filled with an insulating material.
2. A semiconductor structure according to claim 1, characterized in that: The total thickness of the seed crystal layer is ≤500nm, and the ratio of silicon-doped aluminum nitride layer to aluminum nitride layer is 1:1 to 2:
1.
3. A semiconductor structure according to claim 1, characterized in that: The depth of the doped regions of the first, second, and third doped layers ranges from 10% to 80% of the substrate thickness, and the depth increases linearly from top to bottom.
4. A semiconductor structure according to claim 1, characterized in that: The trench is V-shaped, with the bottom corners transitioning to an arc surface, where the corner radius is 50~100nm, the porosity of the lining layer is 20%~50%, and the insulating material is a silicon oxide-based composite material.
5. A semiconductor structure according to claim 1, characterized in that: A metal layer with a thickness of 1~5μm is disposed on the bottom surface of the substrate and is electrically connected to the metal filling layer inside the trench.
6. A semiconductor structure according to claim 1, characterized in that: The epitaxial layer also includes an aluminum nitride insertion layer, which is located between the second doped layer and the third doped layer and has a thickness of 50~200nm.
7. A semiconductor structure according to claim 1, characterized in that: The thickness of the buffer layer is ≤500nm, and the interlayer roughness between the buffer layer and the seed crystal layer is ≤5nm.
8. A semiconductor structure according to claim 1, characterized in that: It also includes a fourth doped layer, which extends downward from the top of the first doped layer to a depth of 1 / 2 to 2 / 3 of the depth of the doped region of the first doped layer.
9. A semiconductor structure according to claim 1, characterized in that: The substrate is a silicon substrate, and the substrate surface has a nanoscale uneven structure.