Method and apparatus for thin slab continuous casting

DE102014105870B4Active Publication Date: 2024-10-10THYSSENKRUPP AG +1
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
DE102014105870
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2014-04-25
Publication Date
2024-10-10
Estimated Expiration
2034-04-25

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A process for the continuous casting of thin slabs with a thickness between 40 and 120 millimeters, comprising the process steps of: - feeding a metallic melt (2) into a mold (5), - forming a partially solidified thin slab strand (9) from the metallic melt (2) in the mold (5), - reducing the flow velocity of the metallic melt (2) in the partially solidified thin slab strand (9) by means of an electromagnetic brake (16) arranged in the region of the mold (5), and - removing the partially solidified thin slab strand (9) from the mold (5) by means of a strand guide system (12), characterized in that - unsolidified parts of the partially solidified thin slab strand (9) are stirred by means of an electromagnetic stirrer arranged downstream below the mold (5) along the strand discharge direction (15) of the thin slab strand (9). (17) be stirred,- wherein an electromagnetic traveling field (19) is generated by means of the electromagnetic stirrer (17) in an area of ​​the thin slab strand (9) located between 50 and 3,000 millimeters away from the mold (5) along the strand withdrawal direction (15).
Need to check novelty before this filing date? Find Prior Art

Description

Prior ArtThe present invention is based on a method for thin slab continuous casting according to the preamble of claim 1.It is generally known from the prior art to produce thin slabs by continuous casting. In this case, a metallic melt is produced, which is transferred by means of a steel casting ladle into a distributor. From the distributor, the metallic melt flows via a pouring tube into a mold which is cooled and moved in an oscillating manner. In the mold, a strand is formed from the metallic melt with a solidified shell and a cross section, which is largely not yet solidified, within the solidified shell. Upon leaving the mould, the strand is taken up by a transport system having a plurality of strand guide rollers, between which the strand is guided through the so-called casting arch and cooled until it solidifies completely. It is also known to slow down the flow velocity of the metallic melt inside the already semi-solidified strand inside the ingot mould by means of an electromagnetic brake (EMBR: Electromagnetic Brake). The aim here is to reduce the flow speed of the steel melt at the bath level and to make the bath level profile uniform in order to improve the lubrication between the strand and the ingot mold and to reduce strand surface defects which can arise as a result of the capture of casting slag.To produce the thin slabs having thicknesses between 40 and 120 millimeters, the mold typically has a funnel-shaped widened cross section in the upper part and a rectangular cross section in the lower part. Due to these small thicknesses, the solidification times in the thin slab continuous casting are comparatively short and the proportion of liquid melt in the interior of the semi-solidified strand is low. This inevitably results in a coarse, strictly directed, columnar-crystalline structure in the continuous casting of thin slabs. However, such a structure can have a disadvantageous effect on the surface and internal nature of the products produced from the thin slabs. For example, depending on the type of steel and casting conditions, longitudinal striations on the product surface, inhomogeneous mechanical properties, structural characteristics, core segregations, reduced HIC resistance (hydrogen induced cracking) and internal cracking susceptibilitys can occur on the products manufactured from the thin slab material.It is known from conventional thick slab continuous casting to avoid longitudinal parasitics on dynamo steels by very low overheat casting. In the case of thick slab continuous casting, however, a comparatively long solidification time is given, so that overheating of the steel melt in the tundish below about 12 Kelvin is sufficient to achieve a sufficient structural refinement. The grain refinement can be said to be sufficient if the expansion of the globular core zone in the thickness direction is more than 30%. In order to achieve the same effect in the case of thin slabs, such a low superheating would have to be selected on account of the shorter solidification times that casting problems would occur in the form of additions of the immersion tubes in the mold (so-called "logging"), which might result in strand surface defects or even strand breaks.From the technical literature (e.g. "Improved quality and productivity in slab casting by electromagnetic breaking and stitching", C. Crister et al., 41th Steel making Semiconductor International, Resend, Brazil, 23.-26. May 2010, pages 1-15) further discloses that electromagnetic stirrers are used in some thick slab continuous casting plants to refine the solidification structure. The stirrers are installed either in the mold area or several meters below the mold bath level.From the document DE 698 24 749 T2 is further known an apparatus for casting metal, which comprises a mould for forming a cast strand and means for feeding a primary flow of hot metallic melt to the mould. The apparatus thereby comprises magnetic means which apply a static or periodic magnetic field to the flow of metal in the non-solidified parts of the casting strand to affect the molten metal in the mould during casting. This is intended to slow down and split the flow of hot metal to provide a secondary flow pattern in the mold. Moreover, it is also known from this publication to provide a further device in the form of an electromagnetic stirrer in order to act on the melt in the mold or on the melt downstream of the mold. However, it is not disclosed in this publication in which region the electromagnetic stirrer is to be arranged with respect to the mold.The use of an electromagnetic brake and / or an electromagnetic stirrer in continuous casting of steel is also known for thick slab formats from the publications DE 21 2009 000 056 U1 and DE 10 2009 056 000 A1. Further relevant prior art is formed, for example, by the publications JP 2001-087 846 A, JP 3 180 164 B2, US 2012 / 0 012 274 A1, JP 2011-101 895 A, DE 103 50 076 A1, DE 33 22 891 A1, EP 0 010 041 A1 and DE 28 10 491 A1.In the case of thin slab continuous casting, electromagnetic stirrers have not been used up to now. In thin slab continuous casting, the particular difficulty is to achieve a significant reduction in the structure at the solidification times which are short compared to thick slab continuous casting and at the small-volume liquid content in the interior of the strand. The present invention solves this problem.Disclosure of the InventionIt is an object of the present invention to provide a method and an apparatus for producing thin slabs in a continuous casting process which, despite short solidification times and comparatively small volume liquid fractions in the interior of the slab, make it possible to produce a large core zone having a fine-grained, globeitic structure in the thin slab strand, in order to prevent the disadvantages which are caused in the prior art by a coarse, strictly directed, columnar crystalline structure in the thin slab strand. Furthermore, the risk of immersion pipe additions due to excessively low overheating is to be avoided.This object is achieved by a method according to claim 1.Compared to the prior art, the device according to the invention has the advantage that, by a design for electromagnetic stirring specifically designed for thin slab continuous casting, a refinement of the solidification structure in the interior of the thin slab strand is achieved and, by the simultaneous use of an electromagnetic brake, it is prevented that the increase in the flow speed of the steel melt induced by the stirrer in the mold region leads to unacceptably high local bath level fluctuations, i.e. to bath level fluctuations of, for example, more than 15 mm. High turbulence at the bath level can lead to ingot apertures or to ingot surface defects due to casting slag trapped at the bath level of the ingot mold. Both strand breaks and strand surface defects are to be avoided. It has surprisingly been found that the electromagnetic stirring at a distance of 20 to 7,000 millimeters below the mold and in particular from the mold bottom side brings about an accelerated and uniform overheating reduction, which advantageously leads to the formation of a sufficiently large core zone, i.e. in particular at least 30% in the thickness direction, having a fine-grained, globeitic structure in the interior of the thin slab strand, while coarse, columnar-crystalline structures are limited by the stirring. Despite the short solidification times and small-volume liquid fractions in the interior of the thin slab strand that are typical in the continuous casting of thin slabs, this fine-grained, globular core zone forms in the solidification structure, whereby the formation of stalk crystals between the edge zone and the central region of the strand is greatly reduced. The extent of the globular core zone in the thickness direction is then in particular at least 30%. In the product produced, it is thus possible to reduce longitudinal striations, structural characteristics, core segregations and susceptibilitys to internal cracks and to increase the HIC resistance and the homogeneity of the mechanical and magnetic properties. Advantageously, it is also possible to prevent a higher and non-critical overheating, so that the risk of casting defects in the form of immersion pipe additions and strand surface defects or strand openings resulting therefrom is eliminated. It is conceivable that in the present method, for example, an overheating of the steel melt in the tundish between 10 and 50 Kelvin, preferably around 20 Kelvin, is used. By means of the electromagnetic stirrer, an electromagnetic traveling field is generated in a region of the thin slab strand which is spaced apart from the mold along the strand draw-off direction between 20 and 7,000 millimeters. A region of the thin slab strand which is spaced apart from the mold by between 20 and 7,000 millimeters is to be understood in the sense of the present invention in particular as that region of the thin slab strand which is spaced apart from the mold bottom side by between 20 and 7,000 millimeters. Alternatively, the position of the electromagnetic stirrer and of the traveling electromagnetic field relative to the mold could also be defined by the distance from the bath level in the mold, which is typically 100 millimeters below the mold top side. The electromagnetic stirrer is preferably arranged in such a way that the traveling field acts directly below the mold on the still nonsolidified parts of the strand, since a positive influence on the grain structure is no longer possible by the traveling field in the case of already solidified parts of the strand. According to the invention, the electromagnetic traveling field is generated in a region spaced from the mold or from the bottom side of the mold along the strand draw-off direction of between 50 and 3,000 millimeters. It is also conceivable to define the position of the electromagnetic stirrer or of the alternating electromagnetic field along the strand draw-off direction via the distance from the bath level in the mold: the distance from the bath level along the strand draw-off direction preferably comprises between 0.9 and 3.8 meters and preferably between 1.5 and 2.5 meters. In the sense of the present invention, in particular, either a single electromagnetic stirrer is arranged on one side of the thin slab strand, either on the fixed side or the loose side, or a separate electromagnetic stirrer is arranged on each side, i.e. both on the fixed side and on the loose side. The fixed side here refers in particular to that broad side of the strand guide segments which always remains unchanged in its position and serves as a so-called reference line. Adaptations of the strand thickness formats are then always carried out via the opposite loose side. The method according to the invention is used in particular for producing thin slabs in the continuous casting process and hot strip or cold strip produced therefrom. The hot strip or cold strip is used in particular for the production of electrical steel sheets (non-grain-oriented or grain-oriented) or steel sheets of relatively high strength steels having yield strength values of greater than 400 megapascals (for example. The heat-treated steel) is used. A thin slab in the sense of the present invention comprises a slab with a thickness between 40 and 120 millimeters. For the precise description of the geometric relationships, two transverse directions, a first transverse direction and a second transverse direction, are mentioned below in addition to the strand draw-off direction. The first transverse direction always extends perpendicular to the strand draw-off direction and parallel to the strand surface normal of the slab broad side, while the second transverse direction always extends perpendicular to the strand draw-off direction and parallel to the strand surface on the slab broad side. The slab broad side is understood here to mean that side of the rectangular cross section of the thin slab strand which has the greater extent. The first and the second transverse direction thus both run perpendicular to the strand draw-off direction and perpendicular to one another.Advantageous embodiments and developments of the invention can be derived from the dependent claims and from the description with reference to the drawings.According to a preferred embodiment of the present invention, it is provided that the non-solidified parts are stirred inside the mold and / or during the discharge of the semi-solidified thin slab strand from the mold by the strand guiding system by means of the electromagnetic stirrer which is positioned below the mold. This advantageously ensures that, during stirring, the proportion of metallic melt which has not yet solidified in the interior of the thin slab strand is still sufficiently large, i.e. is at least 50% of the strand thickness, in order to obtain a core zone which is as large as possible in cross section and has a fine-grained, globeitic structure, i.e. in order to obtain a globular core zone having an extent of at least 30% from the slab in the direction of thickness.According to a further preferred embodiment of the present invention, it is provided that the electromagnetic stirrer is adjusted such that the traveling electromagnetic field runs along a second transverse direction, which runs perpendicular to the strand draw-off direction and parallel to a strand surface on a broad side of the thin slab strand, from a first edge region of the thin slab strand to a second edge region of the thin slab strand opposite the first edge region. In this way, stirring of the metallic melt which has not yet solidified is achieved in the thin slab strand, so that fine, globular grains form in the solidification structure during solidification. Preferably, the electromagnetic traveling field is reversed after a period of time of 1 to 60 seconds has elapsed, particularly preferably between 1 and 10 seconds, so that the electromagnetic traveling field then runs along the second transverse direction from a second edge region of the thin slab strand to the first edge region of the thin slab strand. After a further lapse of the time interval of 1 to 60 seconds, preferably again 1 to 10 seconds, the travelling electromagnetic field is reversed again and the cycle starts from the beginning.According to an alternative preferred embodiment of the present invention, it is provided that a bidirectional, symmetrical electromagnetic traveling field is generated over the width of the thin slab strand by means of the electromagnetic stirrer, wherein the electromagnetic stirrer is adjusted such that a first sub-field of the electromagnetic traveling field runs from the center of the thin slab strand to a first edge region of the thin slab strand and that a second sub-field of the electromagnetic traveling field runs from the center to a second edge region of the thin slab strand opposite the first edge region. This electromagnetic travelling field is preferably kept for 1 to 60 seconds, particularly preferably between 1 and 10 seconds. Thereafter, the traveling electromagnetic field generated by the electromagnetic stirrer and thus the direction of the two sub-fields are reversed. This reverse traveling electromagnetic field is also preferably maintained between 1 to 60 seconds, and more preferably between 1 and 10 seconds. Thereafter, the traveling electromagnetic field is again reversed and the cycle starts from the beginning. This preferred embodiment ensures symmetrical stirring of the metallic melt which has not yet solidified within the already solidified edge zone of the thin slab strand, so that a symmetrical solidification structure with fine, globular grains is produced.According to a further alternative preferred embodiment of the present invention, it is provided that a bidirectional, symmetrical electromagnetic traveling field is generated over the width of the thin slab strand by means of the electromagnetic stirrer, wherein the electromagnetic stirrer is adjusted such that a first sub-field of the electromagnetic traveling field runs from a first edge region of the thin slab strand to the center of the thin slab strand and that a second sub-field of the electromagnetic traveling field runs from a second edge region of the thin slab strand opposite the first edge region to the center of the thin slab strand. This electromagnetic travelling field is preferably held for 1 to 60 seconds, in particular between 1 and 10 seconds. Thereafter, the traveling electromagnetic field generated by the electromagnetic stirrer and thus the direction of the two sub-fields are reversed. This reverse travelling electromagnetic field is also maintained between 1 and 60 seconds, in particular between 1 and 10 seconds. Thereafter, the traveling electromagnetic field is again reversed and the cycle starts from the beginning. This preferred embodiment also ensures symmetrical stirring of the metallic melt which has not yet solidified within the already solidified edge zone of the thin slab strand, so that a symmetrical solidification structure with fine, globular grains is produced.According to a further preferred embodiment of the present invention, it is provided that an electromagnetic traveling field is generated over the width of the thin slab strand by means of the electromagnetic stirrer, the magnetic flux density of which on average is preferably 0.1 to 0.6 Tesla, particularly preferably 0.3 to 0.5 Tesla and very particularly preferably substantially 0.4 Tesla. It has been found that an alternating field with amplitudes in the range of preferably 0.1 to 0.6 Tesla, particularly preferably 0.3 to 0.5 Tesla and very particularly preferably substantially 0.4 Tesla is sufficient to achieve an accelerated and uniform overheating reduction in the metallic melt. This effect is advantageously achieved by an electromagnetic stirrer set in such a way that the flow velocity of the nonsolidified parts in the semisolidified thin slab strand is at most 0.7 meters per second or at least 0.2 meters per second and is preferably between 0.2 and 0.7 meters per second. The circulation of the non-solidified parts in the thin slab strand connected therewith ensures the accelerated and uniform degradation of the overheating and thus the desired refinement of the microstructure, without it being necessary to choose a lower overheating from the outset, as a result of which the risk of immersion pipe deposits would drastically increase.According to a further preferred embodiment of the present invention, it is provided that the electromagnetic stirrer is adjusted such that the stirring frequency is at least 0.1 Hz or at most 10 Hz and is preferably between 1 and 10 Hz. It has been found that this stirring frequency range is particularly advantageous. At a stirring frequency of less than 0.1 Hz, there is no traveling electromagnetic field, so that no stirring effect occurs. If the stirring frequency is higher than 10 Hz, the penetration depth of the traveling electromagnetic field into the inside of the strand is too small, and no texture refinement is obtained.According to a further preferred embodiment of the present invention, it is provided that an electromagnetic field is generated within the mold by means of the electromagnetic brake, the magnetic flux density of said field preferably being 0.1 to 0.3 Tesla, particularly preferably 0.15 to 0.25 Tesla and very particularly preferably substantially 0.2 Tesla. Advantageously, the flow speed of the metallic melt between the semi-solidified edge regions of the strand is braked as a result, and thus casting level fluctuations, as well as surface defects (so-called shell defects) and internal defects (for example, resulting from casting level fluctuations. Preventing Cast Slag Inclusions).According to a further preferred embodiment of the present invention, it is provided that the magnetic field strengths of the traveling electromagnetic field caused by the electromagnetic stirrer and of the field caused by the electromagnetic brake are matched to one another. It has been found that it is advantageous to match the magnetic field strengths of the traveling electromagnetic field caused by the electromagnetic stirrer and of the field caused by the electromagnetic brake. The adjustment is preferably effected by raising the magnetic field strength of the field of the electromagnetic brake by 20 to 80% of its basic value to values between 0.1 and 0.3 Tesla when the electromagnetic stirrer is switched on. In this context, the basic value is understood to mean the magnetic field strength of the field of the electromagnetic brake, as is typically used without the additional use of an electromagnetic stirrer. Typical basic settings for an electromagnetic brake without the use of an electromagnetic stirrer are fields with magnetic field strengths between 0.08 and 0.2 Tesla.The present invention further provides an apparatus for thin slab continuous casting according to claim 14.The device according to the invention has the advantage over the prior art that the metallic melt is stirred by the electromagnetic stirrer during the continuous casting, whereby a refinement of the solidification structure in the interior of the thin slab strand is achieved. Stirring the metallic melt ensures an accelerated and uniform overheat degradation, which advantageously leads to the formation of a core zone with a fine-grained, globeitic structure in the interior of the thin slab strand, while coarse columnar structures are broken up by the stirring. Despite the short solidification times and small-volume liquid fractions in the interior of the thin slab strand that are typical in the continuous casting of thin slabs, this fine-grained, globular core zone forms in the solidification structure, whereby the formation of stalk crystals between the edge zone and the central region of the strand is avoided or at least suppressed. The products produced from the thin slabs thus have significantly reduced striations, structural characteristics and susceptibility to internal cracks, and also increased HIC resistance and homogeneity of the mechanical and magnetic properties. The electromagnetic stirrer generates in particular a spatially and / or temporally variable magnetic field in the region of the thin slab strand. The electromagnetic stirrer preferably comprises a linear field stirrer which is arranged on one of the two broad sides of the thin slab strand. However, it would also be conceivable for a linear field stirrer to be arranged on each of the two opposite broad sides of the thin slab strand. Alternatively, the electromagnetic stirrer comprises a rotating field stirrer or a spheroidal stirrer.The electromagnetic stirrer is arranged along the strand draw-off direction of the thin slab strand below the electromagnetic brake. In an advantageous manner, a rapid and uniform degradation of the overheating is thus achieved in the still non-solidified parts of the thin slab strand before the solidification proceeds into the interior of the thin slab strand, so that the refinement of the solidification structure is achieved. In principle, the proportion of the globular core zone in the thin slab is greater the closer the electromagnetic stirrer is arranged to the meniscus of the thin slab strand or to the bath level. At the same time, however, it must be ensured that the electromagnetic stirrer is also effective in the lower region of the mold in order that an early and rapid reduction of the overheating in the interior of the strand is achieved, and the currents in the metallic melt generated by the electromagnetic stirrer do not lead to increased bath level fluctuations and not to increased local bath level elevations in the mold. It has been found that the electromagnetic stirrer should for this purpose advantageously be arranged at a distance of 50 to 3,000 millimeters from the mold and in particular from the mold bottom side along the strand draw-off direction. In other words, the distance between the electromagnetic stirrer and the bath level preferably comprises between 0.9 and 3.8 metres and preferably between 1.5 and 2.5 metres. Furthermore, it is provided in particular that the electromagnetic stirrer is spaced apart from a surface of the thin slab strand along the first transverse direction by 20 to 1000 millimeters, preferably 20 to 200 millimeters and particularly preferably 20 to 40 millimeters.The device according to the invention is used in particular for producing thin slabs by the continuous casting process and hot strip or cold strip produced therefrom. The hot strip or cold strip is used in particular for the production of electrical steel sheets (not grain-oriented or grain-oriented) or steel sheets of relatively high strength steels having yield strength values of greater than 400 megapascals (for example. The heat-treated steel) is used. A thin slab in the sense of the present invention comprises a slab with a thickness between 40 and 120 millimeters.According to a further preferred embodiment of the present invention, it is provided that the electromagnetic stirrer comprises a linear field stirrer for generating a traveling electromagnetic field in the region of the thin slab strand, wherein the direction of travel of the traveling electromagnetic field is oriented parallel to the second transverse direction. The electromagnetic stirrer is configured in particular in such a way that a first sub-field of the traveling electromagnetic field runs from the center of the thin slab strand to a first edge region of the thin slab strand and a second sub-field of the traveling electromagnetic field runs from the center to a second edge region of the thin slab strand opposite the first edge region. This travelling electromagnetic field is maintained between 1 and 60 seconds, preferably between 1 and 10 seconds. It is then reversed, so that the first sub-field runs from the first edge region of the thin slab strand and the second sub-field runs from the second edge region of the thin slab strand opposite the first edge region to the center of the thin slab strand. This field is also kept between 1 and 60 seconds, preferably between 1 and 10 seconds. The cycle then begins again from the beginning. In an advantageous manner, a uniform and symmetrical flow in the interior of the strand and thus also a uniform discharge of the superheating are thus achieved. On the one hand, this is intended to bring about a homogeneous reduction in the structure in the strand interior and, on the other hand, to bring about uniform strand shell growth over the strand width. In this way, it is prevented that strand breaks or longitudinal surface cracks are produced.According to a further preferred embodiment of the present invention, it is provided that the electromagnetic stirrer is adjusted such that the flow velocity of the metallic melt produced by the stirrer is at least 0.2 meters per second or at most 0.7 meters per second and is in particular between 0.2 and 0.7 meters per second. In this way, it is ensured that, on the one hand, the strand shell growth on the strand narrow side is not too strongly weakened (reduction of the risk of strand break-through) and, on the other hand, strong element depletions (so-called white bands, i.e. depletion of C, Mn, Si, P, S, etc.) at the solidification front in the effective region of the stirrer are avoided. It has been found that the flow velocity should not be less than 0.2 meters per second, because otherwise sufficient structural refinement cannot be achieved. A globular core zone, for example, whose extent in the thickness direction is less than 30% can be considered to be inadequate. The flow velocity should also be not greater than 0.7 meters per second in order to avoid depletion of the melt of alloying elements in the region of the solidification front. The depletion of the melt from alloying elements in the region of the solidification front can be measured in the solidified material. This phenomenon is referred to as "white bands" or "white stripes". White bands result in inhomogeneous properties of the final product.According to a further preferred embodiment of the present invention, it is provided that the electromagnetic brake in the upper half of the mold is spaced apart from a surface of the thin slab strand along the first transverse direction by 20 to 150 millimeters, preferably 25 to 100 millimeters and particularly preferably substantially 75 millimeters. The aforementioned distance is to be understood in the sense of the present invention as meaning in particular the smallest distance between the electromagnetic brake and the strand surface.Further details, features and advantages of the invention are evident from the drawings and from the following description of preferred embodiments with reference to the drawings. The drawings illustrate only exemplary embodiments of the invention, which do not restrict the essential inventive concept.Brief Description of the DrawingsFIG. 1 is a schematic sectional view of a thin slab continuous casting apparatus according to an exemplary embodiment of the present invention. FIGS. 2 aand 2 b show schematic detailed views of the device for thin slab continuous casting according to the exemplary embodiment of the present invention in the region of the mold and below the mold.Embodiments of the InventionIn the various figures, identical parts are always provided with the same reference numerals and are therefore generally also designated or mentioned only once in each case.FIG. 1 shows a schematic sectional view of an apparatus 1 for producing thin slabs by the continuous casting method according to an exemplary embodiment of the present invention.In the present example, metallic melt 2 is transferred from a steel ladle 6 into a distributor 3 and poured from the distributor 3 via a pouring tube 4 (feed means) into a mold 5 of the apparatus 1. The flow through the pouring tube is controlled in dependence on the pouring level 7 in the mould 5 by means of a plug 8 or a slide. The mold 5 comprises a mold with a downwardly open passage opening with a rectangular cross section. The broad sides 28 of the mold are spaced between 40 and 120 millimeters apart so that the mold 5 is suitable for casting thin slabs. The mold consists of water-cooled copper plates which cause solidification of the supplied metallic melt in the edge region of the mold 5. In the mold 5, a thin slab strand 9 having a solidified shell 10 and a cross section 11 which is largely not yet solidified is thus formed from the continuously supplied metallic melt 2 within the solidified shell 10. The thin slab strand 9 passes through the ingot mould 5 along a vertical strand draw-off direction 15. On leaving the ingot mould 5 which is open at the bottom, the thin slab strand 9 is taken up by a transport system 12 (also referred to as strand guide system) having a multiplicity of strand guide rollers 13 and guided through a so-called casting arch 14. The thin slab strand 9 is cooled until it solidifies completely.In addition to the strand draw-off direction 15, a first transverse direction 18 and a second transverse direction 30 are outlined in FIG. 1. The first transverse direction 18 extends perpendicular to the strand draw-off direction 15 and parallel to a strand surface normal of the slab broad side 28 (the slab broad side 28 projects into the plane of the drawing in FIG. 1 ), while the second transverse direction 30 extends perpendicular to the strand draw-off direction 15 and parallel to the strand surface on the slab broad side 28, i.e. perpendicular to the first transverse direction 18.An electromagnetic brake 16 (EMBR: electromagnetic brake) is arranged in the upper region of the ingot mold 5, which brake slows down the flow speed of the metallic melt 2 in the interior of the already partially solidified thin slab strand 9 and thus reduces bath level fluctuations in the ingot mold 5. In the present example, the electromagnetic brake 16 comprises two coils arranged on both sides of the thin slab strand 9. The electromagnetic brake 16 generates an electromagnetic field inside the mold 5, the magnetic flux density of which is preferably 0.1 to 0.3 Tesla and particularly preferably substantially 0.2 Tesla. By braking the flow speed of the metallic melt 2 between the semi-solidified edge regions 10 of the thin slab strand 9, it is possible to reduce casting level fluctuations, as well as surface defects (so-called shell defects) and internal defects (for example, resulting from casting level fluctuations. Thus, the slag inclusion) can be prevented.Below the mold 5, the apparatus 1 according to the invention has an electromagnetic stirrer 17 for stirring non-solidified parts of the semi-solidified thin slab strand 9. In the present example, the electromagnetic stirrer 17 comprises a linear field stirrer which extends along one of the two broad sides 28 of the strand. The linear field stirrer generates an electromagnetic traveling field 19 over the width of the thin slab strand 9 (see FIGS. 2 aand 2 b ) which, along a second transverse direction 30 perpendicular to the strand draw-off direction 15 and parallel to the broad side 28 of the strand surface, cycles back and forth between a first edge region 20 of the thin slab strand 9 and an opposite second edge region 21 of the thin slab strand 9. The traveling electromagnetic field 19 is generated in a region away from the mold 5 or from the mold bottom side 29 along the strand draw-off direction 15 of between 50 and 3,000 millimeters and comprises on average a magnetic flux density of between 0.1 and 0.6 Tesla and preferably of substantially 0.4 Tesla. The electromagnetic traveling field results in stirring of the metallic melt, causing an accelerated and uniform overheating reduction in the metallic melt. This advantageously leads to the formation of a larger core zone with a fine-grained, globeitic structure in the interior of the thin slab strand 9, while coarse columnar-crystalline structures are restricted by the electromagnetic stirring. This effect is advantageously achieved by an electromagnetic stirrer 17 set in such a way that the flow velocity of the non-solidified parts in the semi-solidified thin slab strand is less than 0.7 metres per second and preferably between 0.2 and 0.7 metres per second. Despite the short solidification times and small-volume liquid fractions in the interior of the thin slab strand 9 that are typical in the continuous casting of thin slabs, the fine-grained, globular core zone then forms in the solidified structure, as a result of which the formation of stalk crystals between the edge zone and the central region of the thin slab strand 9 is suppressed. In the case of a final product produced from the continuously cast thin slabs, longitudinal striatedness, structural properties, segregations of the core and susceptibility to internal cracks can thus be reduced and the HIC resistance and the homogeneity of the mechanical and magnetic properties can be increased. In the present case, for example, casting is carried out with an overheating, i.e. with a temperature difference of actual melt temperature minus liquidus temperature, of between 10 and 50 Kelvin, preferably around 30 Kelvin. Thus, higher and non-critical overheating can be observed, so that the risk of casting defects in the form of immersion pipe additions and resulting strand surface defects or strand openings is eliminated.With the above-described device or the above-described method, thin slabs are produced, in particular for hot strip or cold strip. The hot strip or cold strip is used in particular for the production of electrical steel sheets (non-grain-oriented or grain-oriented) or steel sheets of relatively high strength steels having yield strength values of greater than 400 megapascals (for example. The heat-treated steel) is used.FIGS. 2 aand 2 b show schematic detailed views of the apparatus 1 for thin slab continuous casting in the region of the mold and below the mold according to the exemplary embodiment of the present invention explained above with reference to FIG. 1. In the upper region of FIGS. 2 aand 2 b, a sectional view along a sectional plane parallel to the strand draw-off direction 15 and parallel to the second transverse direction 30 is illustrated in each case. In the lower region of FIGS. 2 aand 2 b, a sectional view along a sectional plane perpendicular to the strand draw-off direction 15, i.e. perpendicular to the first transverse direction 18 and to the second transverse direction 30, in the region of the electromagnetic stirrer 17, is illustrated in each case, which sectional view corresponds to the cross section of the strand 9.It can be seen from the upper figure in each case that the feed means comprises the pouring tube 4, which dips into the metallic melt 2 located in the mould 5, and pouring holes 22 formed on the pouring tube 4 below the pouring level 7 in the lower part of the pouring tube 4. The metallic melt 2 is introduced by means of the pouring holes 22 at an angle to the strand draw-off direction 15 of the thin slab strand 9 (see flow arrows 23). Below the mold 5 is arranged the traveling electromagnetic field 19 induced by the non-illustrated electromagnetic stirrer 17. The electromagnetic stirrer 17, which is arranged below the mold 5, generates the electromagnetic traveling field 19 below the mold 5, which in turn causes flows which can reach into the mold 5--possibly even to the bath level. In the embodiment according to FIG. 2 a, the electromagnetic stirrer 17 is configured such that the traveling electromagnetic field 19 comprises two subfields, a first subfield 24 and a second subfield 25. The first sub-field 24 of the traveling electromagnetic field 19 moves cyclically back and forth between a center 26 of the thin slab strand 9 and the first edge region 20 of the thin slab strand 9, while the second sub-field 25 of the traveling electromagnetic field 19 moves cyclically back and forth between the center 26 and the second edge region 21 of the thin slab strand 9. The movement of the traveling electromagnetic field 19 is schematically represented by the movement arrows 27. The division of the traveling electromagnetic field 19 into two bidirectional, symmetrical sub-fields leads to a uniform and symmetrical flow in the interior of the thin slab strand 9 and thus also to a rapid and uniform discharge of the overheating. On the one hand, this is intended to bring about a homogeneous reduction in the structure in the strand interior and, on the other hand, to bring about uniform strand shell growth over the strand width. In this way, the electromagnetic stirring prevents the potential risk of a strand break or of longitudinal surface cracks from arising. The electromagnetic stirrer 17 is preferably also adjusted in such a way that the flow velocity of the metallic melt at the solidification front generated by the stirrer is between 0.2 and 0.7 meters per second. In this way, it is ensured that, on the one hand, the strand shell growth on the strand narrow side is not too strongly weakened (reduction of the risk of strand break-through) and, on the other hand, strong element depletions (so-called white bands, i.e. depletion of C, Mn, Si, P, S, etc.) at the solidification front in the active region of the electromagnetic stirrer 17 are avoided. In addition, the electromagnetic stirrer 17 must be adjusted in such a way that the currents in the metallic melt 2 generated by the electromagnetic stirrer 17 do not lead to increased bath level fluctuations and not to increased local bath level elevations in the mold 5. The magnetic field strengths of the electromagnetic stirrer 17 and of the electromagnetic brake 16 should be matched to one another. The adjustment is effected, for example, by the magnetic field strength of the electromagnetic brake 16 being raised by 20 to 80% of its basic value to values between 0.1 and 0.3 Tesla when the electromagnetic stirrer 17 is switched on. In this context, the basic value is understood to mean the magnetic field strength of the electromagnetic brake 16, as is typically used without the additional use of an electromagnetic stirrer 17. Typical basic settings for an electromagnetic brake 16 without the use of an electromagnetic stirrer 17 are 0.08 to 0.2 Tesla.In the lower illustration of FIG. 2 a, the rectangular cross section of the passage opening of the mold 5 can be seen schematically. The electromagnetic traveling field 19 or the two sub-fields 24, 25 travel along the broad sides 28 through the thin slab strand 9.Alternatively, the electromagnetic traveling field 19 is not divided into two sub-fields 24, 25, but rather cycles along the second transverse direction 30 between the first edge region 20 of the thin slab strand 9 and the opposite second edge region 21 of the thin slab strand 9. This exemplary embodiment is illustrated by way of example in FIG. 2 b.The following exemplary embodiments were carried out with an apparatus according to FIGS. 1 and 2 a:Embodiment 1:One measure of the success in refining the solidification structure inside the thin slab strand is the proportion of the globular core zone (GKZ). The percent expansion of the globular core zone is defined as GKZ (%) = D GKZ( mm) / D (mm) · 100 with D GKZ= thickness of the globular core zone and D = slab thickness.An experiment was therefore carried out with the steel type S420MC, a casting speed of 5 meters per minute, an overheating in the tundish of 30 Kelvin, a strand thickness of 65 millimeters, a strand width of 1550 millimeters and a mold height of 1100 millimeters, in which the electromagnetic brake (EMBR) was arranged in the upper half of the mold and the electromagnetic stirrer (EMS) was arranged below the mold behind a-magnetic rollers of the transport system. The electromagnetic stirrer or the alternating electromagnetic field of the electromagnetic stirrer was arranged at a distance of 2960 millimeters from the casting level. The results listed in the following table were obtained:1EMBR0,1750-1040 - 50EMS0,13102EMBR0,2750-1050 - 60EMS0,4310The test series demonstrate that, by the connection of an electromagnetic stirrer arranged below the mold, the proportion of the globular core zone (GKZ) increases from 0 to 10 percent to a proportion of 40 to 60 percent.Embodiment 2:A relationship between overheating of the steel melt in the tundish and the proportion of the globular core zone on the one hand and the resulting longitudinal brushiness on the finished strip in the case of dynamo steels and the center segregation was determined experimentally in the case of dynamo steels with 2.4% silicon:370The strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strongagents243The strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strong strongagents116medium - strongagents630light-averagelight-average350 - 70no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no nono no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no noIt follows from this that to avoid longitudinal striation and to reduce center segregation, the proportion of globular core zone (GKZ) should be at least 30 percent and preferably greater than 50 percent. Overheating of less than 20 K is to be avoided, however, since otherwise problems would occur in the form of additions of the immersion tubes in the mold (so-called "logging"), which can result in strand surface defects or even strand breakthroughs.In the following, the example for the dynamo steel with 2.4% silicon and thin slabs with a thickness of 63 millimeters, an overheating in the tundish of 30 Kelvin, a strand width of 1550 millimeters and a mold height of 1100 millimeters, the casting level was 1000 millimeters above the mold bottom side, the stirring frequency was 6 Hz, the flow speed at the solidification front was 0.4 m / s, shows that by a corresponding selection of the distance between the casting level and the electromagnetic stirrer (EMS), the required proportion of the globular core zone (GKZ) of at least 30 percent and preferably at least 50 percent can be achieved at different casting speeds V G :30224,86,17,340193,64,55,450162,63,23,860131,72,12,5The above series of measurements show that the electromagnetic stirrer must be arranged at the casting speeds (V G) between 4 and 6 m / min for a proportion of the globular core zone of 50 percent between 2.6 and 3.8 meters, of 60 percent between 1.7 and 2.5 meters below the bath level of the mold. Satisfactory results are also achieved, however, even with a distance of the electromagnetic stirrer from the bath level of between 3.6 and 7.3 metres.The distance between the mold or the mold bottom side and the electromagnetic stirrer is thus advantageously between 20 and 7,000 millimeters and preferably between 50 and 3,000 millimeters. Alternatively, it is also evident that a distance between 100 and 7,000 millimeters, between 500 and 6,500 millimeters, between 700 and 6,300 millimeters, between 700 and 4,400 millimeters, or between 700 and 2,800 millimeters is particularly advantageous.List of reference characters1 Apparatus 2 Metallic melt 3 Distributor 4 Casting tube 5 Mould 6 Steel casting ladle 7 Casting level 8 Plug 9 Thin slab strand 10 Solidified strand shell 11 Non-solidified cross section 12 Transport system 13 Strand guide roller 14 Casting sheet 15 Strand draw-off direction 16 Electromagnetic brake 17 Electromagnetic stirrer 18 First transverse direction (runs perpendicular to the strand draw-off direction and parallel to the strand surface normal of the slab broad side) 19 Electromagnetic traveling field 20 First edge region 21 Second edge region 22 Pouring holes in the lower part of the casting tube 23 Flow arrow 24 First sub-field 25 Second sub-field 26 Center 27 Movement arrow 28 Broad sides 29 Mould underside 30 Second transverse direction (runs perpendicular to the strand draw-off direction and parallel to the strand surface on the slab broad side or parallel to the strand surface. The direction of the drawing-off of the ingot is perpendicular to the direction of the strand and perpendicular to the first transverse direction) 31 of the upper side of the ingot mould

Claims

Method for continuously casting thin slabs having a thickness of between 40 and 120 millimetres, having the method steps: - feeding a metallic melt (2) into a mould (5), - forming a semi-solidified thin slab strand (9) from the metallic melt (2) in the mould (5), - reducing the flow speed of the metallic melt (2) in the semi-solidified thin slab strand (9) by means of an electromagnetic brake (16) arranged in the region of the mould (5), and - discharging the semi-solidified thin slab strand (9) from the mould (5) by means of a strand guide system (12), characterized in that, that - non-solidified parts of the semi-solidified thin slab strand (9) are stirred by means of an electromagnetic stirrer (17) arranged downstream below the mold (5) along the strand draw-off direction (15) of the thin slab strand (9), - wherein an electromagnetic travelling field (19) is generated by means of the electromagnetic stirrer (17) in a region of the thin slab strand (9) which is spaced apart from the mold (5) between 50 and 3,000 millimeters along the strand draw-off direction (15).Method according to claim 1, wherein an electromagnetic field is generated within the mould (5) by means of the electromagnetic brake (16), wherein the electromagnetic brake (16) in the upper half of the mould is preferably spaced apart between 20 to 150 millimetres from a surface of the thin slab strand along a first transverse direction (18), which runs perpendicular to the strand draw-off direction (15) and parallel to a strand surface normal on a broad side (28) of the thin slab strand (9).Method according to one of the preceding claims, wherein the electromagnetic stirrer (17) is adjusted such that the electromagnetic traveling field (19) runs along a second transverse direction (30), which runs perpendicular to the strand draw-off direction (15) and perpendicular to the first transverse direction (18), from a first edge region (20) of the thin slab strand (9) to a second edge region (21) of the thin slab strand (9) opposite the first edge region (20).Method according to claim 3, wherein the travelling electromagnetic field (19) is reversed after a period of time of 1 to 60 seconds, preferably of 1 to 10 seconds, has elapsed in such a way that the travelling electromagnetic field (19) runs along the second transverse direction (30) from a second edge region (21) of the thin slab strand (9) to the first edge region (20) of the thin slab strand (9).Method according to either of Claims 1 and 2, wherein a bidirectional, symmetrical electromagnetic traveling field (19) is generated over the width of the thin slab strand (9) by means of the electromagnetic stirrer (17), wherein the electromagnetic stirrer (17) is set in such a way that a first sub-field (24) of the electromagnetic traveling field (19) runs from a center (26) of the thin slab strand (9) to a first edge region (20) of the thin slab strand (9) and that a second sub-field (25) of the electromagnetic traveling field (19) runs from the center (26) of the thin slab strand (9) to a second edge region (21) of the thin slab strand (9) opposite the first edge region (20).Method according to claim 5, wherein the electromagnetic traveling field (19) is reversed after a time period of 1 to 60 seconds has elapsed, preferably between 1 and 10 seconds, in such a way that the first sub-field (24) runs from the first edge region (20) of the thin slab strand (9) to the center (26) of the thin slab strand (9) and that the second sub-field (25) runs from the second edge region (21) of the thin slab strand (9) to the center (26) of the thin slab strand (9).Method according to either of Claims 1 and 2, wherein a bidirectional, symmetrical electromagnetic traveling field (19) is generated over the width of the thin slab strand (9) by means of the electromagnetic stirrer (17), wherein the electromagnetic stirrer (17) is set in such a way that a first sub-field (24) of the electromagnetic traveling field (19) runs from a first edge region (20) of the thin slab strand (9) to a center (26) of the thin slab strand (9), and that a second sub-field (25) of the electromagnetic traveling field (19) runs from a second edge region (21) of the thin slab strand (9), which second edge region is opposite the first edge region (20), to the center (26) of the thin slab strand (9).Method according to claim 7, wherein the travelling electromagnetic field (19) is reversed after a time period of 1 to 60 seconds has elapsed, preferably between 1 and 10 seconds, in such a way that the first sub-field (24) runs from a center (26) of the thin slab strand (9) to the first edge region (20) and that the second sub-field (25) runs from the center (26) to the second edge region (21).Method according to one of the preceding claims, wherein an electromagnetic travelling field is generated in the region of the thin slab strand (9) by means of the electromagnetic stirrer (17), the magnetic flux density of said electromagnetic travelling field on average preferably being 0.1 to 0.6 Tesla, particularly preferably being 0.3 to 0.5 Tesla and very particularly preferably substantially being 0.4 Tesla.Method according to any one of the preceding claims, wherein the electromagnetic stirrer (17) is adjusted such that the flow speed of the non-solidified parts in the semi-solidified thin slab strand (9) is at least 0.2 metres per second or at most 0.7 metres per second and is preferably between 0.2 and 0.7 metres per second.Method according to one of the preceding claims, wherein the electromagnetic stirrer (17) is adjusted such that the stirring frequency is at least 0.1 Hz or at most 10 Hertz and is preferably between 0.1 and 10 Hz.Method according to one of the preceding claims, wherein an electromagnetic field is generated within the mould (5) by means of the electromagnetic brake (16), the magnetic flux density of said field preferably being 0.1 to 0.3 Tesla, particularly preferably being 0.15 to 0.25 Tesla and very particularly preferably substantially being 0.2 Tesla.Method according to one of the preceding claims, wherein the method is used for producing thin slabs for the production of hot strip or cold strip, in particular for producing electrical sheets or sheets of higher-strength steels, preferably with yield limits greater than 400 megapascals.Device (1) for continuously casting thin slabs having a thickness of between 40 and 120 millimetres, in particular by means of a method according to one of the preceding claims, having - a feed means for feeding a metallic melt (2), - a chill mould (5) for forming a semi-solidified thin slab strand (9) from the fed metallic melt (2), - an electromagnetic brake (16), arranged in the region of the chill mould (5), for reducing the flow speed of the metallic melt (2) in the interior of the semi-solidified thin slab strand (9), and - a strand guide system (12) for discharging the semi-solidified thin slab strand (9) from the chill mould (2), characterized in that, the device (1) has an electromagnetic stirrer (17), which is arranged downstream below the mold (5) along the strand draw-off direction (15) of the thin slab strand (9) and is intended for stirring non-solidified parts of the semi-solidified thin slab strand (9), which stirrer is spaced apart from the mold (5) between 50 and 3,000 millimeters along the strand draw-off direction (15).The device (1) according to claim 14, wherein the electromagnetic stirrer (17) comprises a linear field stirrer for generating a traveling electromagnetic field (19) in the region of the thin slab strand (9), wherein the running direction of the traveling electromagnetic field (19) is oriented perpendicular to the strand draw-off direction (15) and parallel to a second transverse direction (30), which runs perpendicular to the strand draw-off direction (15) and parallel to a strand surface on a broad side (28) of the thin slab strand (9), and wherein the running direction of the traveling electromagnetic field (19) is reversible.The device (1) according to claim 15, wherein the electromagnetic stirrer (17) is configured such that a first sub-field (24) of the traveling electromagnetic field (19) runs from a center (26) of the thin slab strand (9) to a first edge region (20) of the thin slab strand (9) and that a second sub-field (25) of the traveling electromagnetic field (19) runs from the center (26) of the thin slab strand (9) to a second edge region (21) of the thin slab strand (9) opposite the first edge region (20).The device (1) according to claim 15, wherein the electromagnetic stirrer (17) is configured such that the traveling electromagnetic field (19) runs along the second transverse direction (30) from a first edge region (20) of the thin slab strand (9) to a second edge region (21) of the thin slab strand (9) opposite the first edge region (20).The device (1) according to any one of claims 14 to 17, wherein the electromagnetic stirrer (17) is spaced apart from a surface of the thin slab strand (9) by 20 to 1000 millimeters, preferably 20 to 200 millimeters and particularly preferably 20 to 40 millimeters along a first transverse direction (18), which runs perpendicular to the strand draw-off direction (15) and perpendicular to the second transverse direction (30).The device (1) according to any one of claims 14 to 18, wherein the electromagnetic stirrer (17) is configured such that the flow velocity of the non-solidified parts in the semi-solidified thin slab strand (9) is between 0.2 and 0.7 meters per second and / or that the stirring frequency is between 0.1 and 10 Hz.The device (1) according to any one of claims 14 to 18, wherein the electromagnetic brake (16) in the upper half of the mould is preferably spaced between 20 to 150 millimetres from a surface of the thin slab strand along the first transverse direction (18).Device (1) according to one of Claims 14 to 20, wherein the device (1) is provided for producing thin slabs for the production of hot strip or cold strip, in particular for producing electrical sheets or sheets of higher-strength steels, preferably with yield limits greater than 400 megapascals.

Citation Information

Patent Citations

  • Casting molten metal, preferably molten steel materials in form of strand in mold of continuous casting machine, useful for producing slabs- and thin slab products, comprises introducing molten metal through dipping tube

    DE102009056000A1

  • Device and method for electromagnetic stirring or braking of metal castings, in particular continuous steel castings

    DE10350076A1

  • Continuous casting plant for producing thick slabs

    DE212009000056U1

  • PROCESS TO INFLUENCE THE SOLIDIFICATION OF A MELT DURING CONTINUOUS CASTING

    DE2810491A1

  • Apparatus for the electrodynamic stirring of the liquid pool of a metal slab

    DE3322891A1