Semiconductor components, power semiconductor components and methods for forming a semiconductor component
By employing distinct drift region sections with controlled doping and trenches in semiconductor components, the issues of high switch-on resistance and reduced robustness are addressed, enhancing performance and avalanche resistance.
Patent Information
- Application Number
- DE102016118543
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2015-10-15
- Filing Date
- 2016-09-29
- Publication Date
- 2025-01-30
- Estimated Expiration
- 2036-09-29
AI Technical Summary
New generations of semiconductor construction elements face challenges with high switch-on resistance and reduced robustness due to strong diffusion of semiconductor doping regions and flat, wide diffusion profiles, particularly under avalanche conditions.
The solution involves creating semiconductor components with distinct drift region sections having different doping species and concentrations, and incorporating trenches that extend into the semiconductor layer, with a controlled vertical distance and doping concentration gradient to optimize the transition from the drift region to the substrate, using epitaxial growth with low diffusivity doping atoms like arsenic or antimony.
This approach reduces switch-on resistance and improves avalanche robustness by achieving sharp doping profiles and controlled diffusion, optimizing performance while maintaining component integrity.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
TECHNICAL FIELD
[0001] Embodiments relate to concepts for semiconductor device structures and in particular to semiconductor devices, power semiconductor devices and methods for forming a semiconductor device. BACKGROUND
[0002] New generations of semiconductor devices (e.g., power devices) may need to be optimized for cost. High doping levels in power semiconductor devices can lead to strong diffusion from semiconductor doping regions and to shallow and broad diffusion profiles. These can increase the on-resistance of the devices and reduce their robustness, e.g., against avalanche conditions.
[0003] The documents US 2015 / 0 118 810 A1, US 9 318 566 B2 and US 2004 / 0 178 444 A1 disclose known semiconductor devices. SUMMARY
[0004] There is a need to provide concepts for semiconductor devices with improved robustness and / or improved device characteristics.
[0005] Such a need can be met by the subject matter of the claims.
[0006] Some embodiments relate to a semiconductor device comprising a drift region of a device structure arranged in a semiconductor layer. The drift region comprises at least a first drift region portion and at least a second drift region portion. A majority of dopants within the first drift region portion is a first species of dopants having a diffusivity less than a diffusivity of phosphorus within the semiconductor layer. Furthermore, a majority of dopants within the second drift region portion is a second species of dopants. In addition, the semiconductor device comprises a trench extending from a surface of the semiconductor layer into the semiconductor layer.A vertical distance between the surface of the semiconductor layer and a boundary between the first drift region portion and the second drift region portion is greater than 0.5 times the maximum depth of the trench and less than 1.5 times the maximum depth of the trench. The second drift region portion is arranged between the surface of the semiconductor layer and the first drift region portion.
[0007] Some embodiments relate to a semiconductor device. The semiconductor device comprises a drift region of a device structure arranged in a semiconductor layer disposed adjacent to a semiconductor substrate. A doping concentration at a junction from the drift region to the semiconductor substrate varies between a first doping concentration value and a second doping concentration value over a distance of less than 550 nm. The first doping concentration value is an average net doping concentration of a central portion of the drift region plus 20% of the average net doping concentration of the central portion of the drift region. The central portion of the drift region lies within a central 50% of a vertical dimension of the drift region. The second doping concentration value is an average net doping concentration of the central portion of the drift region plus one decade.
[0008] Some embodiments relate to a method for forming a semiconductor device. The method comprises epitaxially growing a first epitaxial semiconductor sublayer of a semiconductor layer. A majority of dopants within the first epitaxial semiconductor sublayer are dopants having a diffusivity of less than a diffusivity of phosphorus within the semiconductor layer. Further, the method comprises epitaxially growing a second epitaxial semiconductor sublayer of a semiconductor layer after forming the first epitaxial semiconductor sublayer. A majority of dopants within the second epitaxial semiconductor sublayer are phosphorus atoms. Additionally, the method comprises forming a trench extending from a surface of the semiconductor layer into the semiconductor layer.A vertical distance of a boundary between the first epitaxial semiconductor sublayer and the second epitaxial semiconductor sublayer to the surface of the semiconductor layer is greater than 0.5 times a maximum depth of the trench and less than 1.5 times the maximum depth of the trench. The second epitaxial semiconductor sublayer is arranged between the surface of the semiconductor layer and the first epitaxial semiconductor sublayer. SHORT DESCRIPTION OF THE CHARACTERS
[0009] Some embodiments of devices and / or methods are described below solely by way of example and with reference to the accompanying figures, in which: Fig. 1a shows a schematic representation of a semiconductor device; Fig. 1b and Fig. 1c graphical representations of a deviation of the average net doping concentration (per cm 3) in terms of dopant depth (µm); Fig. Figure 2a shows a schematic diagram of a semiconductor device; Fig. Figure 2b shows a plot of drain current (A) versus drain voltage (V) for semiconductor devices with different doping characteristics; Fig. Figure 2c shows a plot of drain current (A) versus gate voltage (V) for semiconductor devices with different doping characteristics; Fig. 3a shows a schematic representation of a semiconductor device with a plurality of gate trenches; Fig. 3b shows a schematic representation of a semiconductor device with a dense arrangement of a plurality of gate trenches; and Fig. 4 shows a flow diagram of another method for forming a semiconductor device. Fig. 5 shows a schematic representation of a semiconductor device; Fig. 6 shows a schematic diagram of a semiconductor device with a gate electrode and a field electrode in a gate trench; Fig. 7 shows a schematic representation of another semiconductor device with a gate electrode and a field electrode in a gate trench; and Fig. 8 shows a flow diagram of a method for forming a semiconductor device. DETAILED DESCRIPTION
[0010] Various examples will now be described in more detail with reference to the accompanying drawings, which illustrate some examples. In the figures, the thicknesses of lines, layers, and / or regions may be exaggerated for clarity.
[0011] Accordingly, while other examples of various modifications and alternative forms are susceptible of interpretation, some examples thereof are shown by way of example in the figures and are described in detail herein. It should be understood, however, that examples are not intended to limit the specific forms disclosed, but rather, examples are intended to cover all modifications, equivalents, and alternatives falling within the scope of the disclosure. Throughout the description of the figures, like reference numerals refer to like or similar elements.
[0012] It is understood that when an element is described as being "connected" or "coupled" to another element, it may be directly connected or coupled to the other element, or intervening elements may be present. Conversely, when an element is described as being "directly connected" or "coupled" to another element, no intervening elements are present. Other terms used to describe the relationship between elements should be interpreted similarly (e.g., "between" versus "directly between," "adjacent" versus "directly adjacent," etc.).
[0013] The terminology used herein is for the purpose of describing specific examples only and is not intended to be limiting of further examples. As used herein, the singular forms "a," "an," and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise. It is further understood that the terms "comprises," "comprising," "having," and / or "comprising," as used herein, indicate the presence of specified features, integers, steps, operations, elements, and / or components, but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof.
[0014] Unless defined otherwise, all terms used herein (including technical and scientific terms) have the same meaning as commonly understood by one of ordinary skill in the art to which examples belong. Furthermore, it is understood that terms, e.g., those defined in commonly used dictionaries, should be construed as having a meaning consistent with their meaning in the context of the relevant technology. Should this disclosure assign a particular meaning to a term that differs from a meaning commonly understood by one of ordinary skill in the art, that meaning should be considered in the specific context in which the definition is given.
[0015] Fig. 1a shows a schematic representation of a semiconductor device 100 according to an embodiment.
[0016] The semiconductor device 100 comprises a drift region 101 of a device structure arranged in a semiconductor layer 102 arranged adjacent to a semiconductor substrate 103.
[0017] A doping concentration at a junction from the drift region 101 to the semiconductor substrate 103 varies between a first doping concentration value and a second doping concentration value over a distance of less than 500 nm.
[0018] The first doping concentration value is an average net doping concentration of a central part of the drift region plus 20% of the average net doping concentration of the central part of the drift region.
[0019] The central part of the drift region 101 lies within the middle 50% of a vertical dimension of the drift region 101.
[0020] The second doping concentration value is an average net doping concentration of the central part of the drift region plus one decade.
[0021] Since the doping concentration at the junction from the drift region 101 to the semiconductor substrate 103 varies between the first doping concentration value and the second doping concentration value over a distance of less than 500 nm, an on-resistance value of the semiconductor device can be reduced and / or an avalanche robustness of the semiconductor device can be improved.
[0022] The transition from the drift region to the semiconductor substrate may be a region at an interface where the drift region of the device structure and the semiconductor substrate meet. For example, the transition from the drift region to the semiconductor substrate may refer to a region comprising an interface (or surface) between the drift region and the semiconductor substrate, and / or at least a portion of the drift region (e.g., no more than 50% or 25% of the total drift region) directly adjacent to the interface, and / or at least a portion of the semiconductor substrate (no more than 50% or 25% of the total semiconductor substrate) directly adjacent to the interface.
[0023] The drift region 101 may, for example, extend vertically (e.g., substantially perpendicularly or orthogonally) from a body region of the field-effect transistor or insulated-gate bipolar transistor or from an anode / cathode region of a diode towards (or to) the semiconductor substrate 103. The middle part of the drift region 101 (from which the average net doping concentration value is derived) lies within a middle 50% (or, for example, within a middle 40% or, for example, within a middle 30%) of a vertical extension of the drift region 101. The part of the middle 50% of the drift region 101 may refer to a part of the drift region between a first interface region of the drift region and a second interface region of the drift region, which is separated from the first interface region by a minimum vertical dimension (extension) or vertical separation distance. The first interface region of the drift region 101 may, for example,a boundary between (or a transition from) the drift region 101 and the body region or anode / cathode region of the device structure. The second interface region of the drift region 101 can, for example, be a boundary between (or a transition from) the drift region 101 and the semiconductor substrate 103.
[0024] For example, the middle portion of the drift region 101 may have a minimum vertical dimension of 50% of the vertical dimension between the first interface region and the second interface region, and may be a region of the drift region 101 that is equidistant from the first interface region and the second interface region. For example, for a drift region with a minimum vertical dimension of 4 µm between the first interface region and the second interface region, the middle 50% portion may be a region that has a minimum vertical dimension of 2 µm and may have a separation distance of 1 µm from the first interface region and a separation distance of 1 µm from the second interface region.
[0025] The first doping concentration value is an average net doping concentration of the central part of the drift region 101 plus 20% (or e.g. plus 25%) of the average net doping concentration of the central part of the drift region 101. If, e.g., the average net doping concentration value of the central part of the drift region 101 is 1*10 16 Dopant atoms per cm 3 the first doping concentration value is 1.2*10 16 (or 1.25*10 16 ) Dopant atoms per cm 3 . The average net doping concentration value of the central part of the drift region 101 may be at least 1*10 16 Dopant atoms per cm 3 be (or e.g. at least 1*10 17 Dopant atoms per cm 3 or can be between 1*10 16 Dopant atoms per cm 3 and 1*10 17 Dopant atoms per cm 3The average net doping concentration of the central part of the drift region 101 can, for example, be a measured number of dopant atoms per volume averaged over the central part of the drift region 101 of the device structure.
[0026] The second doping concentration value is the average net doping concentration of the drift region's central part plus one decade. In other words, the second doping concentration value is an order of magnitude (or, for example, ten times) higher than the average net doping concentration of the drift region's central part on a logarithmic scale. For example, if the average net doping concentration of the drift region's central part is 101 1*10 16 Dopant atoms per cm 3 the second doping concentration value is 1*10 17 Dopant atoms per cm 3 and the first doping concentration value is 1.2*10 16 Dopant atoms per cm 3.
[0027] The doping concentration at the junction from the drift region to the semiconductor substrate varies between the first doping concentration value and the second doping concentration value over a distance of less than 500 nm (or e.g., less than 400 nm, or e.g., less than 300 nm, or e.g., less than 200 nm). For example, the doping concentration at the junction from the drift region 101 to the semiconductor substrate 103 can be 1.2*10 16 Dopant atoms per cm 3 to 1*10 17 Dopant atoms per cm 3 over a distance of less than 500 nm in the case of the example above.
[0028] The semiconductor layer 102 can be grown epitaxially on a surface of the semiconductor substrate 103. For example, the semiconductor layer 102 can be grown epitaxially on a front-facing surface of the semiconductor substrate 103 such that the epitaxially grown semiconductor layer 102 is arranged on the surface of the semiconductor substrate 103. The semiconductor layer 102 can have a minimum (or smallest) thickness of less than 8 µm (or e.g., less than 6 µm or e.g., less than 4 µm) measured in a substantially vertical direction (or perpendicular to the surface of the semiconductor substrate 103). The semiconductor layer 102 can, for example, extend laterally over the front-facing surface of the semiconductor substrate 103. The semiconductor layer 102 can, for example, extend vertically (e.g.,substantially perpendicular or orthogonal) from a surface of the semiconductor layer 102 adjacent to metal layers, insulation layers and / or passivation layers towards the front-facing surface of the semiconductor substrate 103.
[0029] The drift region 101 can be formed in the semiconductor layer 102 by doping the semiconductor layer 102. The drift region 101 of the semiconductor layer 102 can be doped with dopant atoms having a diffusivity of less than the diffusivity of phosphorus within the semiconductor layer 102 at a temperature T = 300 K and standard atmospheric pressure. For example, the diffusivity of phosphorus in silicon at T = 300 K and standard atmospheric pressure is 10.5 cm 2 / s. Thus, for a silicon-based semiconductor layer 102, the drift region 101 of the semiconductor layer 102 can be filled with doping atoms with a diffusivity of less than 10.5 cm 2 / s will be endowed.
[0030] The semiconductor layer 102 can be doped, for example, with arsenic doping atoms (which have a diffusivity of 0.06 cm 2 / s in silicon). Alternatively, the semiconductor layer 102 can be doped with antimony doping atoms, for example (which have a diffusivity of 3.9 cm 2 / s in silicon). Being doped with arsenic or antimony dopant atoms refers to arsenic or antimony dopant atoms being the majority dopant atoms during doping. For example, the average net doping concentration of the drift region of semiconductor layer 102 is mainly caused by the arsenic (or antimony) dopant atoms. For example, more than 70% (or, for example, more than 80%, or, for example, more than 90%, or, for example, more than 95%) of the dopant atoms incorporated into semiconductor layer 102 to cause the average net doping of semiconductor layer 102 (or drift region 101) may be arsenic (or antimony) dopant atoms.
[0031] The semiconductor substrate 103 may (also) be doped with dopant atoms having a diffusivity of less than the diffusivity of phosphorus within the semiconductor substrate 103 at a temperature T = 300 K and at standard atmospheric pressure. For example, the semiconductor substrate 103 may be doped with arsenic dopant atoms or antimony dopant atoms. For example, more than 70% (or, for example, more than 80%, or, for example, more than 90%, or, for example, more than 95%) of the dopant atoms incorporated into the semiconductor substrate 103 to cause the average net doping of the semiconductor substrate 103 may be arsenic (or antimony) dopant atoms.
[0032] For example, semiconductor layer 102 and semiconductor substrate 103 can be doped with the same doping atoms. For example, semiconductor layer 102 and semiconductor substrate 103 can both be doped purely (or only) with arsenic doping atoms, or alternatively, only with antimony doping atoms.
[0033] The semiconductor substrate 103 may be a silicon-based semiconductor substrate (e.g., a silicon substrate) or a silicon carbide (SiC)-based semiconductor substrate. Alternatively or optionally, the semiconductor substrate 103 may be, for example, a gallium arsenide (GaAs)-based semiconductor substrate or a gallium nitride (GaN)-based semiconductor substrate.
[0034] The semiconductor substrate 103 may have a minimum (or smallest) thickness of less than 200 µm (or e.g., less than 150 µm, or e.g., less than 100 µm, or e.g., less than 600 µm) measured in a substantially vertical direction.
[0035] The device structure of the semiconductor device 100 can be, for example, a power metal oxide semiconductor field-effect transistor (MOSFET) structure, a power insulated gate bipolar transistor (IGBT) structure, or a power diode structure. For example, each device structure can have a highly doped first source / drain or collector / emitter region with a second conductivity type (e.g., n ++-doped), a body region with a first conductivity type (e.g., p-doped), and a drift region (e.g., n-doped). The first source / drain or collector / emitter region of the device structure, the body region of the device structure, and the drift region of the device structure may be arranged adjacent to a gate (or a gate-trench structure). The first source / drain region of the device structure, the body region of the device structure, the drift region of the device structure, and the gate or the gate-trench structure may be arranged within the semiconductor layer 102.
[0036] A gate voltage applied to the gate (or gate trench structure) may include a conductive channel (e.g., an n-type channel) in the body region between the first source / drain region and the drift region. The conductive channel may be formed in a portion of the body region adjacent to the gate (or gate trench structure), and a current flow may occur, e.g., between the first source / drain region of the device structure and the drift region through the induced conductive channel.
[0037] A (second) source / drain or collector / emitter region of the device structure may be arranged (or formed) in the semiconductor substrate 103 due to the doping of the semiconductor with dopant atoms having a diffusivity of less than phosphorus. A net (or average) doping concentration of the (second) source / drain or collector / emitter region arranged in the semiconductor substrate may be at least 1*10 19Dopant atoms per cm 3 (or at least 1*10 19 Dopant atoms per cm 3 ). The average doping concentration can, for example, be a measured number of dopant atoms per volume averaged over the (second) source / drain or collector / emitter region of the device structure.
[0038] If the device structure is a MOSFET structure, the drift region of the device structure may be arranged between (e.g., directly between or directly adjacent to) the body region of the device structure and the (second) source / drain region of the device structure. The (second) source / drain region of the device structure may extend from the drift region 101 toward (or to) the second lateral side (e.g., a backside surface) of the semiconductor substrate 103 opposite to the first lateral side of the semiconductor substrate 103 on which the semiconductor layer 103 is formed. The source / drain region of the FET structure may, for example, have a second conductivity type (e.g., n ++ -endowed).
[0039] If the device structure is an IGBT structure, the drift region of the device structure may be arranged between the body region of the device structure and an emitter / collector region of the device structure. The emitter / collector region of the device structure may extend from the drift region toward (or to) a second lateral side (e.g., a backside surface) of the semiconductor substrate 103. The emitter / collector region of the device structure may have a first conductivity type (e.g., p + -endowed).
[0040] Due to the presence of sharp doping profiles and reduced out-diffusion of dopants, a field-stop region located between the drift region and the emitter / collector region is not required. Thus, the drift region of the device structure can be located directly between (or directly adjacent to) the body region of the device structure and the (second) emitter / collector region of the device structure.
[0041] The first source / drain region of the device structure, which is formed on a first lateral side of the semiconductor layer 102, may have an average doping concentration of more than 1 × 10 18 Dopant atoms per cm 3 (or e.g. between 1 × 10 18 Dopant atoms per cm 3 and 5 × 10 19 Dopant atoms per cm 3). The average doping concentration can, for example, be a measured number of dopant atoms per volume averaged over a region of interest of the first source / drain region of the device structure.
[0042] The body region of the device structure can have an average doping concentration of between 5*10 16 Dopant atoms per cm 3 and 1*10 19 Dopant atoms per cm 3 (or e.g. between 2*10 17 Dopant atoms per cm 3 and 1*10 18 Dopant atoms per cm 3 ). The average doping concentration can, for example, be a measured number of dopant atoms per volume averaged over a region of interest in the body region of the device.
[0043] A region comprising the first conductivity type may be a p-doped region (e.g., caused by the introduction of aluminum ions or boron ions) or an n-doped region (e.g., caused by the introduction of nitrogen ions, phosphorus ions, or arsenic ions). Consequently, the second conductivity type indicates an opposite n-doped region or p-doped region. In other words, the first conductivity type may indicate p-doping, and the second conductivity type may indicate n-doping, or vice versa.
[0044] The semiconductor device 100 may include a plurality of gate trenches extending from a first (or front) side surface of the semiconductor layer 102 into the semiconductor layer 102. The plurality of gate trenches may extend vertically into the semiconductor layer such that a bottom of each gate trench may be disposed within or below the drift region (e.g., within or below the central portion of the drift region).
[0045] Each gate trench of the plurality of gate trenches may comprise at least one electrically conductive electrode and a gate oxide layer arranged within a trench structure. The gate oxide layer may be arranged adjacent to (e.g., encapsulate or surround) the at least one electrically conductive electrode. A (lateral) thickness of a portion of the gate oxide layer toward the bottom of the gate trench may be greater than a (lateral) thickness of a portion of the gate oxide layer toward the surface of the semiconductor layer.
[0046] Optionally, each gate trench may comprise more than one electrically conductive electrode (e.g., one or two or three or more electrically conductive electrodes). The electrically conductive electrodes (e.g., the first electrically conductive electrode and the second electrically conductive electrode) may be electrically insulated from each other, e.g., by the gate oxide layer. A (lateral) thickness of a portion of the gate oxide layer adjacent to (or surrounding) the second electrically conductive electrode (towards the bottom of the gate trench) may be greater than a (lateral) thickness of a portion of the gate oxide layer adjacent to (or surrounding) the first electrically conductive electrode.
[0047] Optionally or additionally, a lateral distance between adjacent gate trenches of the plurality of gate trenches may be, for example, 1.5 times or less than 1.5 times a lateral dimension (e.g., a width) of a gate trench of the plurality of gate trenches. Alternatively or additionally, a lateral distance between adjacent gate trenches of the plurality of gate trenches may be, for example, between 2.5 times the thickness of the field oxide (adjacent to or surrounding the (lower) part of the electrically conductive electrode towards the bottom of the gate trench) to 7.5 times the thickness of the field oxide. The lateral dimension of each gate trench (and / or a lateral distance between adjacent gate trenches) may be based on an average of at least three gate trench lateral dimension values. For example, a first gate trench lateral dimension value may be a lateral dimension of the gate trench at a (vertical) gate trench depth of 20% from the first lateral surface of the semiconductor layer.A second gate trench lateral dimension value may be a lateral dimension of the gate trench at a (vertical) gate trench depth of 50% from the first lateral surface of the semiconductor layer. A third gate trench lateral dimension value may be a lateral dimension of the gate trench at a (vertical) gate trench depth of 80% from the first lateral surface of the semiconductor layer.
[0048] The semiconductor component may be a power semiconductor component with a blocking voltage of at least 10 V. For example, the semiconductor component may have a breakdown voltage or blocking voltage of more than 10 V (e.g., a breakdown voltage of 10 V, 20 V, or 50 V), more than 100 V (e.g., a breakdown voltage of 200 V, 300 V, 400 V, or 500 V), more than 500 V (e.g., a breakdown voltage of 600 V, 700 V, 800 V, or 1000 V), or more than 1000 V (e.g., a breakdown voltage of 1200 V, 1500 V, 1700 V, 2000 V, 3300 V, or 6500 V). An on-resistance value of the semiconductor component may, for example, be less than 4 mΩmm 2 for a semiconductor component with a blocking voltage of 40V.
[0049] A first lateral surface or front surface of the semiconductor layer 102 may be a surface of the semiconductor layer 102 toward metal layers, insulation layers, and / or passivation layers on the semiconductor layer 102 or a surface of one of these layers. For example, a front side of a semiconductor layer 102 may be the side on which active elements of the chip are formed. For example, in a power semiconductor chip, a chip front side may be a side of the chip on which a first source / drain region and a gate region are formed, and a chip back side may be a side of the chip on which a second source / drain region is formed. For example, more complex structures may be arranged on the chip front side than on the chip back side.
[0050] A lateral surface of the semiconductor layer 102 and / or the semiconductor substrate 103 may be a substantially flat plane (e.g., neglecting unevenness of the semiconductor structure due to the manufacturing process and trenches). For example, the lateral dimension of the lateral surface of the semiconductor layer 102 or the semiconductor substrate 103 may be more than 100 times larger (or more than 1000 times, or more than 10,000 times) than a maximum height of structures on the main surface. Compared to a substantially vertical edge (e.g., resulting from the separation of the substrate of the chip from others) of the semiconductor layer 102 or the semiconductor substrate 103, the lateral surface may be a substantially horizontal surface extending laterally. The lateral dimension of the lateral surface of the semiconductor layer 102 or the semiconductor substrate 103 may, for example,be more than 100 times larger (or more than 1000 times or more than 10000 times) than a substantially vertical edge of the semiconductor layer 102 or the semiconductor substrate 103.
[0051] Fig. Figure 1b shows a graphical representation 150 of a deviation of an average net doping concentration (per cm 3 ) 151 with respect to a dopant depth (µm) 152 at a transition from a drift region to the semiconductor substrate for different semiconductor devices with different substrate doping combinations.
[0052] Line 153 represents an average net doping concentration with respect to a dopant depth at the junction of the drift region and the semiconductor substrate for a semiconductor device in which both the drift region and the semiconductor substrate are purely doped with phosphorus dopant atoms - in other words when more than 70% (or e.g. more than 80% or e.g. more than 90% or e.g. more than 95%) of the doping atoms for causing the average net doping of the drift region are phosphorus doping atoms and when more than 70% (or e.g. more than 80% or e.g. more than 90% or e.g. more than 95%) of the doping atoms for causing the average net doping of the semiconductor substrate are phosphorus doping atoms.
[0053] As shown by the gradual gradient of line 153 at the transition from the drift region to the semiconductor substrate, the doping concentration at the transition from the drift region to the semiconductor substrate varies between the first doping concentration value and the second doping concentration value, e.g., over a distance of more than 1 µm (or e.g., more than 1.5 µm). The gradient of line 153 is flat over the entire transition from the drift region to the semiconductor substrate. For example, the transition from the drift region to the semiconductor substrate may be the transition between an average net doping concentration value within the middle 50% (or e.g., within the middle 40% or e.g., within the middle 30%) of the drift region 101 to an average net doping concentration value within the middle 50% (or e.g., within the middle 40% or e.g., within the middle 30%) of the semiconductor substrate 103.The doping concentration may vary from the average net doping concentration value within the middle 50% of the drift region 101 to the average net doping concentration value within the middle 50% of the semiconductor substrate 103, e.g., over a distance of more than 5 µm (or e.g., more than 6 µm or more than 8 µm).
[0054] Line 154 represents an average net doping concentration with respect to a dopant depth at the junction from the drift region to the semiconductor substrate of a semiconductor device in which the drift region is doped with phosphorus dopant atoms, and when the semiconductor layer 102 is doped with dopant atoms having a diffusivity less than phosphorus (e.g., arsenic dopant atoms) - or in other words, when more than 70% (or, e.g., more than 80% or, e.g., more than 90% or, e.g., more than 95%) of the dopant atoms for causing the average net doping of the drift region are phosphorus dopant atoms, and when more than 70% (or, e.g., more than 80% or, e.g., more than 90% or, e.g., more than 95%) of the dopant atoms for causing the average net doping of the semiconductor substrate are arsenic dopant atoms.
[0055] The doping concentration at the transition from the drift region to the semiconductor substrate varies between the first doping concentration value and the second doping concentration value, e.g., over a distance of more than 500 nm (or, e.g., more than 1 µm). The gradient of line 154 shows that the doping concentration can vary from the average net doping concentration value within the middle 50% of the drift region 101 to the average net doping concentration value within the middle 50% of the semiconductor substrate 103, e.g., over a distance of more than 1.5 µm (or, e.g., more than 2 µm).
[0056] Line 155 represents an average net doping concentration with respect to a dopant depth at the junction from the drift region to the semiconductor substrate of a semiconductor device, in which the drift region is doped with dopant atoms having a diffusivity less than phosphorus (e.g., arsenic dopant atoms) and when the semiconductor layer 102 is doped with the same dopant atoms having a diffusivity of less than phosphorus (e.g., arsenic dopant atoms) - in other words, when more than 70% (or, e.g., more than 80% or, e.g., more than 90% or, e.g., more than 95%) of the dopant atoms for causing the average net doping of the drift region are arsenic dopant atoms and when more than 70% (or, e.g., more than 80% or, e.g., more than 90% or, e.g., more than 95%) of the dopant atoms for causing the average net doping of the semiconductor substrate are arsenic dopant atoms are.
[0057] Line 155 shows that the doping concentration at a transition from the drift region to the semiconductor substrate varies between a first doping concentration value and a second doping concentration value over a distance of less than 500 nm. The gradient of line 155 shows that the doping concentration can vary from the average net doping concentration value within the middle 50% of the drift region 101 to the average net doping concentration value within the middle 50% of the semiconductor substrate, for example, over a distance of less than 1.5 µm.
[0058] Fig. Figure 1c shows a graphical representation 160 of a deviation of an average net doping concentration (per cm 3 ) 161 with respect to the dopant depth (µm) 162 at a junction from the drift region to the semiconductor substrate. The graphical representation 160 represents an enlarged portion of the graphical representation of Fig. 1b at a depth of between 1 µm and 4 µm.
[0059] The steepness of the ends can be obtained for lines 154 and lines 155.
[0060] As shown by line 154 (for a phosphorus-doped semiconductor layer and an arsenic-doped semiconductor substrate), the doping concentration at the junction from the drift region to the semiconductor substrate varies between the first doping concentration value A1 and the second doping concentration value A2, e.g., over a distance of more than 500 nm (or, e.g., more than 1 µm). For line 154, the first doping concentration value A1 can be achieved at a depth of 2.92 µm, e.g., and the second doping concentration value A2 can be achieved at a depth of 2.92 µm. Thus, a slope of 650 nm per decade can be obtained.
[0061] As shown by line 155 (for a phosphorus-doped semiconductor layer and a phosphorus-doped semiconductor substrate), the doping concentration at the junction from the drift region to the semiconductor substrate varies between the first doping concentration value C1 and the second doping concentration value C2, e.g., over a distance of less than 500 nm (or, e.g., less than 400 nm, or, e.g., less than 300 nm). For line 155, the first doping concentration value C1 can be obtained at, e.g., a depth of 3.29 µm, and the second doping concentration value C2 can be achieved at, e.g., a depth of 3.62 µm. Thus, a steepness of 330 nm per decade can be obtained, which is almost twice the steepness of line 154.
[0062] The first doping concentration value is, for example, an average net doping concentration of the central part of the drift region 101 plus 20% (or, for example, plus 25%) of the average net doping concentration of the central part of the drift region 101. The second doping concentration value is an average net doping concentration of the central part of the drift region plus one decade. Alternatively or optionally, the first doping concentration value (initial value of the end) may be a concentration in the epitaxial semiconductor layer at the bottom or base of the gate trench plus 20%. The second doping concentration value (final value of the end) may be a concentration in the epitaxial semiconductor layer at the bottom or base of the gate trench plus one decade.
[0063] The various examples describe a device structure (e.g., a transistor or diode cell) having a steep out-diffusion dopant tail in the semiconductor substrate and a steep dopant tail for the epitaxial semiconductor layer in the direction of the substrate toward the drain.
[0064] Although the out-diffusion tail of the epitaxial semiconductor layer in the depth direction toward the drain may previously have been considered negligible and covered by the semiconductor substrate out-diffusion tail, the various examples herein show that the profile gradient (of the epitaxial semiconductor layer) is important for optimizing (or improving) Ron*A.
[0065] By using low-diffusivity dopant atoms to dope the semiconductor substrate 103 and the semiconductor layer 102, low out-diffusion (e.g., preferably steep ends) can be achieved. As shown, a very steep net concentration profile gradient of at least 330 nm per decade can be obtained directly below the trench bottom. The steepness of the end can be determined by a difference between a first doping concentration value and a second doping concentration value.
[0066] Fig. 1b and Fig. Figure 1c shows the average net doping profile of the semiconductor substrate and the doping of the epitaxial semiconductor layer at the end of the (doping) process. The various examples represent concepts for a new generation of power MOSFETs that are optimized for cost and can achieve low Ron*A with avalanche robustness. Optimal steep doping gradients between the semiconductor substrate level and the epitaxial semiconductor layer level can be achieved. Until now, approaches have been applied with highly doped substrates containing phosphorus. Although the highest possible doping is preferred, strong out-diffusion of phosphorus and the flat and wide diffusion end are undesirable, especially with thinner chips (with a thickness of less than 60 µm). For example,The transition between the semiconductor substrate doping ends and the epitaxial semiconductor layer is more blurred when phosphorus is used as a dopant in the epitaxial semiconductor layer, as it leads to undesirable Ron*A in transistors. Relatively strong diffusion dopants are therefore undesirable in the semiconductor substrate and the epitaxial device semiconductor layer.
[0067] Fig. 2a shows a schematic representation of a power semiconductor device 200 according to an embodiment.
[0068] The power semiconductor device 200 comprises an epitaxial semiconductor layer 102 arranged adjacent to a semiconductor substrate 103. The epitaxial semiconductor layer 102 is doped with dopant atoms having a diffusivity of less than phosphorus in the epitaxial semiconductor layer 102. The semiconductor substrate 103 is doped with dopant atoms having a diffusivity of less than phosphorus in the semiconductor substrate 103.
[0069] Since the epitaxial semiconductor layer 102 is doped with dopant atoms having a diffusivity of less than phosphorus, and the semiconductor substrate 103 is doped with dopant atoms having a diffusivity of less than phosphorus, sharp doping profiles can be obtained at a transition from the epitaxial semiconductor layer to the semiconductor substrate, resulting in a reduced on-resistance value of the semiconductor device and / or improved avalanche robustness.
[0070] The power semiconductor device 200 may be similar to the semiconductor device used in conjunction with Fig. 1a-1c is described.
[0071] The epitaxial semiconductor layer 102 may be doped with doping atoms having a diffusivity of less than a diffusivity of phosphorus (e.g., less than 10.5 cm 2 / s) within the semiconductor layer 102 at a temperature of T = 300 K and standard atmospheric pressure. The semiconductor layer 102 can be doped, for example, with arsenic doping atoms or antimony doping atoms.
[0072] The semiconductor substrate 103 can be doped with dopant atoms having a diffusivity of less than the diffusivity of phosphorus within the semiconductor substrate 103 at a temperature T = 300 K and at standard atmospheric pressure. For example, the semiconductor substrate can be doped with arsenic dopant atoms or antimony dopant atoms. The epitaxial semiconductor layer 102 and the semiconductor substrate 103 can be doped with the same dopant atoms. For example, the semiconductor layer 102 and the semiconductor substrate 103 can both be doped with arsenic dopant atoms to achieve their respective average net doping concentrations.
[0073] The power semiconductor component may have a blocking voltage of less than 10 V. For example, the power semiconductor component may have a breakdown voltage or blocking voltage of more than 10 V (e.g., a breakdown voltage of 10 V, 20 V, or 50 V), more than 100 V (e.g., a breakdown voltage of 200 V, 300 V, 400 V, or 500 V), more than 500 V (e.g., a breakdown voltage of 600 V, 700 V, 800 V, or 1000 V), or more than 1000 V (e.g., a breakdown voltage of 1200 V, 1500 V, 1700 V, 2000 V, 3300 V, or 6500 V).
[0074] Fig. Figure 2b shows a graphical representation 250 of characteristics of a drain current (A) 251 versus a drain voltage (V) 252 (breakdown characteristics) for different semiconductor devices with different substrate epitaxial doping configurations.
[0075] Line 253 represents a drain current versus drain voltage curve for a semiconductor device in which both the drift region and the semiconductor substrate are doped with phosphorus dopant atoms. A turn-on voltage for such a semiconductor device can be 46 V with a semiconductor layer thickness of 7.6 µm.
[0076] Line 254 represents a drain current versus drain voltage curve for a semiconductor device with a drift region (or semiconductor layer) doped with phosphorus dopant atoms and a semiconductor substrate doped with arsenic dopant atoms. A turn-on voltage for such a semiconductor device can be 47 V with a semiconductor layer thickness of 4.2 µm.
[0077] Line 255 represents a drain current versus drain voltage curve for a semiconductor device with a drift region (or semiconductor layer) doped with arsenic dopant atoms and a semiconductor substrate doped with arsenic dopant atoms. A turn-on voltage for such a semiconductor device can be 44.5 V with a semiconductor layer thickness of 3.7 µm.
[0078] Line 255 shows that for a power semiconductor device 200 having an epitaxial semiconductor layer 102 and a semiconductor substrate 103, both doped with dopant atoms having a diffusivity of less than phosphorus, an improved turn-on behavior of the power semiconductor device 200 can be achieved.
[0079] Fig. Figure 2c shows a graphical representation 260 of transfer characteristics (of drain current (A) 261 versus gate voltage (V) 262) for different semiconductor devices.
[0080] Line 263 represents a drain current versus gate voltage curve for a semiconductor device in which both the drift region and the semiconductor substrate are doped with phosphorus dopant atoms. The on-resistance value (Ron × A) of the semiconductor device can be 6 mΩmm. 2 with a semiconductor layer thickness of 7.2 µm.
[0081] Line 264 represents a drain current versus drain voltage curve for a semiconductor device with a drift region (or semiconductor layer) doped with phosphorus dopant atoms and the semiconductor substrate doped with arsenic dopant atoms. The on-resistance value (Ron × A) of the semiconductor device can be 5.5 mΩmm. 2 with a semiconductor layer thickness of 4.2 µm.
[0082] Line 265 represents a drain current versus drain voltage curve for a semiconductor device with a drift region (or semiconductor layer) doped (purely) with arsenic dopant atoms and the semiconductor substrate doped (purely) with arsenic dopant atoms. The on-resistance value of the semiconductor device can be 4 mΩmm. 2 with a semiconductor layer thickness of 3.7 µm.
[0083] Due to the steepness of the arsenic-doped semiconductor substrate and the arsenic-doped semiconductor layer, optimization of Ron*A can be achieved at a constant breakdown voltage of more than 40 V. Due to the steep profile, optimization of Ron can be achieved by reducing the thickness of the epitaxial semiconductor layer alone, thus reducing the high-resistance section of the cell. Simulation data of the devices show that, for example, a reduction of Ron*A of 5.1 mΩmm 2 up to 3.99 mΩmm 2e.g. in the case of a 40 V power MOS transistor.
[0084] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. The embodiments shown in Figures 2A to 2C may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 1c) or subsequently (e.g. Fig. 3a to 4) are mentioned.
[0085] Fig. 3a shows a schematic representation of a semiconductor device 300 according to an embodiment. The semiconductor device 300 may be similar to the semiconductor devices described in connection with Fig. 1a-1c and 2a-2c are described.
[0086] The semiconductor device 300 may include a plurality of gate trenches 311 extending into the semiconductor layer 102 from a first (front) side surface 312 of the semiconductor layer 102. Each gate trench 311 of the plurality of gate trenches 311 may include at least one electrically conductive electrode 314 and a gate oxide layer 315 disposed adjacent to the at least one electrically conductive electrode 314.
[0087] Each gate trench structure 311 may be arranged adjacent to a first source / drain region 316 of a device structure, a body region 317 of the device structure, and a drift region 101 of the device structure. A first source / drain contact structure 318 may be arranged on the first side surface 312 of the semiconductor layer 102. The first source / drain contact structure 318 may comprise one or more electrically conductive layers (e.g., metallization layers and / or barrier layers) ohmically connected to the first source / drain region 316 (and / or body region 317) of the device structure.
[0088] A bottom of each gate trench 311 may, for example, be arranged within (or below) the drift region 101 (e.g., within the central portion of the drift region 101). For example, the gate trench 311 may extend to a vertical depth within the semiconductor layer 102 such that a bottom of the gate trench 311 may, for example, be arranged within (or below) the central 50% of the drift region 101.
[0089] A (lateral) thickness of a portion of the gate oxide layer 315 toward the bottom of the gate trench 311 may be greater than a (lateral) thickness of a portion of the gate oxide layer 315 toward the (front-side) surface 312 of the semiconductor layer 102. For example, the gate trench 311 may be formed according to a field plate trench concept. A thinner gate oxide (e.g., with a thickness of less than 5 nm) may be formed adjacent to the electrically conductive electrode 314 at an (upper) portion of the electrically conductive electrode 314 toward the (front-side) surface 312 of the semiconductor layer 102. A thicker field oxide may be formed adjacent to the electrically conductive electrode 314 at a (lower) part of the electrically conductive electrode 314 closer toward the bottom of the gate trench 311 than the (upper) part.The (lower) part of the electrically conductive electrode 314 may have a smaller lateral dimension than the (upper) part of the electrically conductive electrode 314.
[0090] The (second) source / drain or collector / emitter region 319 of the device structure may be arranged (or formed) in the semiconductor substrate 103 due to the average net doping of the semiconductor substrate 103. A second source / drain contact structure may be ohmically connected to the second source / drain region 319 of the device structure, e.g., at the opposite second (backside) side surface of the semiconductor substrate 103.
[0091] Optionally or additionally, a lateral distance between adjacent gate trenches 311 (or separating them) of the plurality of gate trenches 311 may be 1.5 times (or less than 1.5 times) a smallest lateral dimension (e.g., a width) of a gate trench 311 of the plurality of gate trenches 311. Alternatively or additionally, a lateral distance between adjacent gate trenches 311 of the plurality of gate trenches 311 may be between 2.5 times the minimum thickness of the field oxide (adjacent to or surrounding the (lower) part of the electrically conductive electrode 314 toward the bottom of the gate trench 311) up to 7.5 times the minimum thickness of the field oxide. The maximum thickness of the field oxide may, for example, be the smallest thickness of the field oxide measured from the at least one electrode 314 to a drift region surrounding the gate trench.
[0092] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. 3a may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 2c) or subsequently (e.g. Fig. 3b to 4) are mentioned.
[0093] Fig. 3b shows a schematic representation of a semiconductor device 350 according to an embodiment. The semiconductor device 350 may be similar to the semiconductor device described in connection with Fig. 3a is described.
[0094] Each gate trench 331 of the plurality of gate trenches 331 may comprise a first electrically conductive electrode 314 and a second electrically conductive electrode 321. The first electrically conductive electrode 314 may, for example, be arranged closer towards the front surface 312 of the semiconductor layer 102 (e.g., at an upper part of the gate trench 331) than the second electrical electrode 321. The second electrically conductive electrode 321 may be arranged closer towards the bottom of the gate trench 331 than, for example, the first electrically conductive electrode 314. Optionally, each gate trench 331 may comprise more than one electrically conductive electrode (e.g., one or two or three or more electrically conductive electrodes), which may be vertically spaced with respect to one another in the trench structure. The electrically conductive electrodes (e.g.,the first electrically conductive electrode 314 and the second electrically conductive electrode 321) may be electrically insulated from each other, e.g., by the gate oxide layer 315.
[0095] The gate oxide layer 315 may be arranged adjacent to the first electrically conductive electrode 314 and the second electrically conductive electrode 321. A (lateral) thickness of a portion of the gate oxide layer 315 adjacent to the second electrically conductive electrode 321 (toward the bottom of the gate trench 311) may be greater than a (lateral) thickness of a portion of the gate oxide layer 315 adjacent to the first electrically conductive electrode 314 (toward the front surface 312 of the semiconductor layer 102). For example, a thinner gate oxide may be formed adjacent to the first electrically conductive electrode 314. A thicker field oxide may be formed adjacent to the second electrically conductive electrode 321. The second electrically conductive electrode 321 may, for example, have a smaller lateral dimension than the first electrically conductive electrode 314.
[0096] A gate voltage (or potential) applied to the first electrically conductive electrode 314 (gate electrode) of the gate trench 331 may induce a conductive channel (e.g., an n-channel) in the body region 317 between the first source / drain region 316 and the drift region 101. A source voltage (or potential) may be applied to the second electrically conductive electrode 321 (a field electrode). As a result, a gate-to-drain capacitance may be reduced and replaced by a source-to-drain capacitance. Thus, a gate charge for switching the transistor may be reduced, and thus switching losses may be reduced.
[0097] The majority of gate trenches 331 may be denser than the majority of gate trenches formed in conjunction with Fig. 3a. For example, a lateral distance between adjacent gate trenches 331 of the plurality of gate trenches 331 may be 1.5 times (or less than 1.5 times) a smallest lateral dimension (e.g., a width) of a gate trench 331 of the plurality of gate trenches 331. Alternatively or additionally, a lateral distance between adjacent gate trenches 331 of the plurality of gate trenches 331 may be between 2.5 times the minimum thickness of the field oxide (adjacent to or surrounding the second electrically conductive electrode 314) to 7.5 times the minimum thickness of the field oxide.
[0098] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. 3b may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 3a) or subsequently (e.g. Fig. 4) described embodiments are mentioned.
[0099] Fig. 4 shows a flowchart of a method 400 for forming a semiconductor device.
[0100] The method 400 includes forming 410 a semiconductor layer on a semiconductor substrate. The semiconductor substrate includes doping with dopant atoms having a diffusivity less than the diffusivity of phosphorus.
[0101] The method 400 further comprises introducing 420 dopant atoms having a diffusivity of less than a diffusivity of phosphorus into the semiconductor layer to form a drift region of a device structure in the semiconductor layer during or after forming the semiconductor layer.
[0102] Since the semiconductor layer is doped with dopant atoms having a diffusivity less than phosphorus and the semiconductor substrate is doped with dopant atoms having a diffusivity less than phosphorus, sharp doping profiles can be obtained at a transition from the semiconductor layer to the semiconductor substrate, resulting in a reduced on-resistance value of the semiconductor device and / or improved avalanche robustness.
[0103] The method 400 may include forming 410 (e.g., growing) the semiconductor layer epitaxially on a surface of the semiconductor substrate.
[0104] The method 400 may include introducing the dopant atoms (e.g., by ion implantation) to dope the semiconductor substrate (bulk) with arsenic or antimony dopant atoms such that a source / drain or collector / emitter region is formed in the semiconductor substrate prior to forming 410 the semiconductor layer on the surface of the semiconductor substrate. The method 400 may further include co-implanting fluorine atoms into the semiconductor substrate during (or after) introducing the dopant atoms into the semiconductor substrate to form the source / drain or collector / emitter region. The introduction of the doping atoms and the co-implantation of fluorine atoms may be carried out such that a net (or average) doping concentration of the (second) source / drain or collector / emitter region arranged in the semiconductor substrate caused by the introduction of the doping atoms is at least 1*10 19 Dopant atoms per cm3 (or at least 1*10 19 Dopant atoms per cm 3 ) can be.
[0105] The method 400 may include introducing 420 the dopant atoms (e.g., by ion implantation) with a diffusivity of less than a diffusivity of phosphorus (e.g., arsenic or antimony dopant atoms) into the epitaxial semiconductor layer after introducing the dopant atoms into the semiconductor substrate such that a drift region is formed in the semiconductor layer. The method 400 may further include co-implanting fluorine atoms into the semiconductor layer during or after introducing the dopant atoms into the semiconductor layer to form the drift region. The introduction of the dopant atoms and the co-implanting of fluorine atoms may be carried out such that a net (or average) doping concentration value of a central part of the drift region, caused by the introduction of the dopant atoms, is at least 1*1016 Dopant atoms per cm 3 can be (or e.g. at least 1*10 17 Dopant atoms per cm 3 or e.g. between 1*10 16 Dopant atoms per cm 3 and 1*10 17 Dopant atoms per cm 3 may be).
[0106] Co-implantation with fluorine atoms can reduce the out-diffusion of dopant atoms in the semiconductor substrate and the semiconductor layer such that a doping concentration at a transition from a drift region of the semiconductor layer to the semiconductor substrate varies between a first doping concentration value and a second doping concentration value over a distance of less than 500 nm. The first doping concentration value can be, for example, an average net doping concentration of a central portion of the drift region plus 20% of the average net doping concentration of the central portion of the drift region. The central portion of the drift region 101 lies, for example, within the central 50% of the drift region 101.
[0107] The method 400 may further include forming a body region and a source / drain or emitter / collector region in the semiconductor layer after forming the drift region in the semiconductor layer.
[0108] The method 400 may, for example, further comprise forming a plurality of gate trenches in the semiconductor layer after forming the body region and the source / drain or emitter / collector region in the semiconductor layer.
[0109] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. 4 may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 3b) or embodiments described below.
[0110] Various examples relate to a concept for power MOSFETs with steep epitaxial and substrate ends. Various examples relate to an optimal, very steep doping profile gradient in the transition region between the device epitaxial semiconductor layer and the semiconductor substrate doping. Various examples relate to a semiconductor device with a doping concentration that varies by less than 500 nm per decade at a transition from the drift region to the semiconductor substrate.
[0111] Aspects and features (e.g., the semiconductor substrate, the semiconductor layer, the drift region, the first doping concentration value, the second doping concentration value, the average net doping concentration, the plurality of gate trenches, the first source / drain or emitter / collector region, the second source / drain or emitter / collector region, the body region, the drift region, the gate oxide, and the field oxide) mentioned in connection with one or more specific examples may be combined with one or more of the other examples.
[0112] Fig. 5 shows a schematic cross-section of a semiconductor device according to an embodiment. The semiconductor device 500 comprises a drift region of a device structure arranged in a semiconductor layer 102. The drift region comprises at least a first drift region portion 502 adjacent to at least a second drift region portion 504. A majority of dopants within the first drift region portion 502 are a first species of dopants. The first species of dopants has a diffusivity of less than a diffusivity of phosphorus within the semiconductor layer 102. Furthermore, a majority of dopants within the second drift region portion 504 are a second species of dopants. In addition, the semiconductor device 500 comprises a trench 510 extending from a surface of the semiconductor layer 102 into the semiconductor layer 102.A vertical distance between the surface of the semiconductor layer 102 and a boundary 503 between the first drift region portion 502 and the second drift region portion 504 is greater than 0.5 times a maximum depth of the trench and less than 1.5 times the maximum depth of the trench 110.
[0113] By using different dopant species for a region of the drift region located at a depth of the trench and a region below or at the bottom of the trench, segregation of low-diffusivity dopants adjacent to the trench or an upper part of the trench can be avoided or reduced, while low diffusion of dopants toward a backside of the device can be obtained due to the use of low-diffusivity dopants at a part of the drift region located closer to the backside. E.g.an on-resistance value of the semiconductor device can be reduced and / or the avalanche robustness of the semiconductor device can be improved due to the implementation of the first drift region portion, while disturbance of structures near the trench can be avoided or reduced due to a low lateral variation of the doping concentration within the drift region near the trench due to the implementation of the second drift region portion.
[0114] The majority of dopants within the first drift region section 502 are atoms of the first species of dopants, which may mean that a number of dopants of the first species is greater than a number of dopants of any other individual species of dopants (e.g., the second species of dopants) within the first drift region section 502 and / or is greater than a total number of all dopants that differ from the first species (e.g., resulting from impurities or diffusion into the first drift region section) within the first drift region section 502. For example, the first species of dopants may be arsenic atoms or antimony atoms.
[0115] The majority of dopants within the second drift region section 504 are atoms of the second species of dopants, which may mean that a number of dopants of the second species is greater than a number of dopants of any other individual species of dopants (e.g., the first species of dopants) within the second drift region section 504 and / or greater than a total number of all dopants that differ from the second species (e.g., resulting from impurities or diffusion in the second drift region section) within the second drift region section 504. For example, the second species of dopants may be phosphorus atoms or hydrogen-related donors (e.g., caused by intercalated hydrogen ions).
[0116] For example, the first dopant species and the second dopant species are dopants of the first conductivity type. For example, the first dopant species and the second dopant species are donors, and the drift region is an n-type doping region.
[0117] The boundary 503 between the first drift region portion 502 and the second drift region portion 504 may be an area comprising a number of dopants of the first species equal to a number of dopants of the second species. The boundary 503 may extend substantially parallel to a surface of the front side surface of the semiconductor layer (e.g., a straight plane, although trenches may extend from the surface into the semiconductor layer) within the entire semiconductor chip or at least in the vicinity of the one or more trenches. For example, the vertical distance between the boundary 503 and the surface of the semiconductor layer is greater than 0.5 times (or greater than 0.6 or greater than 0.7) a maximum depth of the trench and less than 1.5 times (or less than 1.4 or less than 1.3) the maximum depth of the trench, e.g., at least within a lateral region comprising a lateral distance to the trench 510 of less than 10 µm (or less than 50 µm). For example, the vertical distance from the boundary 503 between the first drift region portion 502 and the second drift region portion 504 to the surface of the semiconductor layer is greater than the maximum depth of the trench 510.
[0118] The trench 510 may be formed by forming a patterned mask layer on the surface of the semiconductor layer 102 (e.g., the front surface of the semiconductor chip of the semiconductor device) and etching the semiconductor layer 102 at regions exposed by the mask layer. The trench 510 may be one of a plurality of trenches that are etched simultaneously. For example, the trench 510 may be a field electrode trench with a field electrode (e.g., connected or connectable to a source potential or a gate potential) disposed within the field electrode trench, or a gate trench with a gate electrode (e.g., electrically connected to a gate wiring structure of the semiconductor device) disposed within the gate trench.
[0119] The first drift region portion may be a first sub-layer semiconductor layer 102 (e.g., epitaxially grown or implemented by implanting the first species of dopants) and the second drift region portion may be a second sub-layer (e.g., epitaxially grown or implemented by implanting the second species of dopants) of the semiconductor layer 102. For example, a plurality of trenches may extend into the semiconductor layer, and the first drift region portion may be a common drift region portion extending laterally beneath the plurality of trenches, wherein a second drift region portion of a plurality of second drift region portions is arranged between each two adjacent trenches. For example, a maximum doping concentration within the first drift region portion and / or the second drift region portion of the drift region is less than 1*10 18 Dopant atoms per cm 3 (or less than 5*10 17or less than 1*10 17 ). For example, an average net doping concentration value of the drift region can be at least 1*10 16 Dopant atoms per cm 3 (or at least 1*10 15 , at least 5*10 15 , at least 5 * 10 16 or at least 1*10 17 ). For example, a vertical extension of the first drift region portion 502 is greater than 1 µm (or greater than 5 µm or greater than 10 µm). The vertical extension of the first drift region portion 502 may depend on the voltage class of the semiconductor device 500.
[0120] For example, a local minimum of the net doping concentration of the drift region may be located at the boundary 503 between the first drift region portion 502 and the second drift region portion 504. The local minimum may be caused by a diffusion of the dopants of the second species into the first drift region portion 502 at the boundary 503. The net doping concentration at the local minimum may be lower than 90% of an average net doping concentration of the first drift region portion 502 or the second drift region portion 503. Optionally, an additional implantation of dopants (e.g., of the first or second or another species) may be performed to compensate for the local minimum.
[0121] Optionally, the semiconductor device 500 may further comprise a semiconductor substrate arranged adjacent to the semiconductor layer 102. A doping concentration of the semiconductor substrate may be substantially higher than an average doping concentration of the drift region (e.g., the first drift region portion and the second drift region portion). For example, a doping concentration at a transition from the drift region to the semiconductor substrate may vary between a first doping concentration value and a second doping concentration value over a distance of less than 500 nm (e.g., may increase from the first doping concentration value to the second doping concentration value). The first doping concentration value may be an average net doping concentration of a central portion of the drift region plus 20% of the average net doping concentration of the central portion of the drift region.The central portion of the drift region may be within the middle 50% of a vertical dimension of the drift region. Furthermore, the second doping concentration value may be an average net doping concentration of the central portion of the drift region plus one decade.
[0122] For example, the doping concentration at the junction between the drift region and the semiconductor substrate may increase from the first doping concentration value to the second doping concentration value over a distance of more than 100 nm. Although a very steep increase may be desirable, at least some slope exists due to dopant diffusion.
[0123] The component structure of the semiconductor component 500 may, for example, be a transistor structure (e.g., a metal-oxide-semiconductor field-effect transistor (MOSFET) structure or an insulated-gate bipolar transistor (IGBT) structure) or a diode structure. For example, the component structure may be a transistor cell of a transistor arrangement comprising a plurality of identical or similar transistor cells. A transistor cell of the transistor arrangement may comprise at least a source region, a body region, and a gate (e.g., a lateral gate on a front-side surface of the semiconductor substrate or a trench gate arranged within a gate trench extending into the semiconductor substrate). Furthermore, the transistor cells of the plurality of transistor cells of the transistor arrangement may have a common (mutual) drift region and / or a common drain region (e.g.,The device structure may share a common collector region (e.g., the transistor cells are MOSFET cells) or a common collector region (e.g., the transistor cells are IGBT cells). For example, the device structure may have at least one body region disposed adjacent to at least one second drift region portion 502.
[0124] For example, the device structure may have a breakdown voltage of more than 10 V. For example, the semiconductor device 100 may be a power semiconductor device. A power semiconductor device, an electrical structure (e.g. transistor structure or diode structure) of the power semiconductor device or the device structure may have a breakdown voltage or blocking voltage of more than 10 V (e.g. a breakdown voltage of 10 V, 20 V or 50 V), more than 100 V (e.g. a breakdown voltage of 200 V, 300 V, 400 V or 500 V), more than 500 V (e.g. a breakdown voltage of 600 V, 700 V, 800 V or 1000 V) or more than 1000 V (e.g. a breakdown voltage of 1200 V, 1500 V, 1700 V, 2000 V, 3300 V or 6500 V).
[0125] The semiconductor layer 102 and / or the semiconductor substrate may be a silicon layer or substrate. Alternatively, the semiconductor layer 102 and / or the semiconductor substrate may be a broadband semiconductor layer or substrate with a band gap greater than the band gap of silicon (1.1 eV). For example, the semiconductor layer 102 and / or the semiconductor substrate may be a silicon carbide (SiC)-based semiconductor layer or substrate, a gallium arsenide (GaAs)-based semiconductor layer or substrate, or a gallium nitride (GaN)-based semiconductor layer or substrate. Furthermore, the semiconductor layer 102 and / or the semiconductor substrate may be a semiconductor wafer or a semiconductor chip.
[0126] For example, a lateral direction or lateral dimensions may be measured parallel to a front surface of the semiconductor layer 102 and / or the semiconductor substrate, and a vertical direction or vertical dimensions may be measured orthogonal to the front surface of the semiconductor layer 102 and / or the semiconductor substrate. For example, the surface of the semiconductor layer 102 is a front surface layer of the semiconductor chip of the semiconductor device 500. The front side or front surface of the semiconductor layer 102 may be an interface toward a wiring layer stack of the semiconductor device (e.g., comprising wiring structures and insulation layers).The front side or front surface of the semiconductor layer 102 or the semiconductor chip may be the side used to implement more sophisticated and complex structures than the back side of the semiconductor substrate 110, since the process parameters (e.g., temperature) and handling for the back side may be limited if structures are already formed on one side of the semiconductor substrate 110.
[0127] For example, the drift region of the devices described in connection with one or more of the semiconductor devices described in Fig. 1a-4, a first drift region portion 502 and a drift region portion 504 as described in connection with the semiconductor device shown in Fig. 5 is shown.
[0128] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. 5 may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 4) or subsequently (e.g. Fig. 6 to 8) are mentioned.
[0129] Fig. 6 shows a schematic diagram of a semiconductor device with a gate electrode and a field electrode in a gate trench according to an embodiment. The implementation of the semiconductor device 600 may be similar to the implementation described in connection with Fig. 5. The semiconductor device 600 comprises a plurality of gate trenches 610 having a gate electrode 612 and a field electrode 614 in each gate trench 610. The gate electrodes 612 are electrically connected to a gate wiring structure (e.g., comprising a gate pad and optionally a gate ring). The field electrodes 614 are electrically connected to a source wiring structure or a wiring structure connectable to another defined potential. The gate electrodes 612 are insulated from the field electrodes 614 at least within the gate trenches. A thickness of the insulation layer between a semiconductor material of the semiconductor layer and the field electrode 614 is greater than (e.g., greater than twice) a thickness of the insulation layer between a semiconductor material of the semiconductor layer and the gate electrode 612.The first drift doping region section 502 is arranged vertically between the second drift doping region section 504 and the semiconductor substrate 103. The boundary 503 between the first drift region section 502 and the second drift region section 504 is arranged near the bottom of the trenches. For example, the vertical distance of the boundary 503 between the first drift region section 502 and the second drift region section 504 and the surface of the semiconductor layer is more than 0.8 times the maximum depth of the trench and less than the maximum depth of the trench.
[0130] Fig. Figure 6 can be an example using a two-step epitaxial growth process. The concentrations of the individual layers can be selected identically or can be individually optimized.
[0131] Optionally, the thicknesses of the multilevel epi layers can be varied within a broad range. The lower layer thickness can be at least as thick as the outdiffusion from the substrate, while the upper epi layer can be approximately as thick as the field oxide FOX trench depth, for example.
[0132] Optionally, a further epi-layer with modified dopants can be deposited in the channel region of the trench transistor. For example, a p-doped layer (e.g., comprising boron atoms as dopants) can be grown to implement a body region of a transistor structure or an anode region of a diode structure.
[0133] Optionally, implantations of any species can be introduced between the epi layers to further optimize the dopant profile, which can be activated by subsequent annealing.
[0134] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. 6 may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 5) or subsequently (e.g. Fig. 7 to 8) are mentioned.
[0135] Fig. 7 shows a schematic diagram of a semiconductor device with a gate electrode and a field electrode in a gate trench according to an embodiment. The implementation of the semiconductor device 700 may be similar to the implementation described in connection with Fig. 3b. However, the semiconductor layer comprises a first drift doping section 502 and a second drift doping section 504. A boundary 503 between the first drift region section 502 and the second drift region section 504 is arranged below (a greater distance from the surface of the semiconductor layer) the bottom of the gate trenches. For example, a vertical distance between a bottom of the gate trenches (e.g., maximum depth of trenches) and the boundary 503 is less than 1 µm.
[0136] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. 7 may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 6) or subsequently (e.g. Fig. 8) described embodiments are mentioned.
[0137] Fig. 8 shows a flowchart of a method for forming a semiconductor device according to an embodiment. The method 800 includes epitaxial growth 810 of a first epitaxial semiconductor sublayer of a semiconductor layer. A majority of dopants within the first epitaxial semiconductor sublayer is a first species of dopants having a diffusivity of less than a diffusivity of phosphorus within the semiconductor layer. Furthermore, the method 800 includes epitaxial growth 820 of a second epitaxial semiconductor sublayer of a semiconductor layer after forming the first epitaxial semiconductor sublayer. A majority of dopants within the second epitaxial semiconductor sublayer is a second species of dopants. In addition, the method 800 includes forming 830 a trench extending from a surface of the semiconductor layer into the semiconductor layer.A vertical distance between a boundary between the first epitaxial semiconductor sublayer and the second epitaxial semiconductor sublayer and the surface of the semiconductor layer is greater than 0.5 times a maximum depth of the trench and less than 1.5 times the maximum depth of the trench.
[0138] By using different species of dopants for different sublayers, segregation of low diffusivity dopants adjacent to the trench or an upper part of the trench can be avoided or reduced, while low diffusion of dopants toward a backside of the device can be obtained due to the use of low diffusivity dopants at a sublayer located closer to the backside.
[0139] The first epitaxial semiconductor sublayer can be formed on a surface of a semiconductor substrate (e.g. highly doped).
[0140] For example, the first epitaxial semiconductor sublayer and the second epitaxial semiconductor sublayer comprise the same conductivity type and the first species of dopants and the second species of dopants are dopants of a first conductivity type.
[0141] The semiconductor layer may comprise further epitaxial sublayers (e.g., a body doping region sublayer having a second conductivity type).
[0142] For example, the surface of the semiconductor layer is a front surface layer of the semiconductor chip of the semiconductor device to be formed.
[0143] The method 800 may further include forming (e.g., by thermal oxidation) an insulating layer within the trench and / or forming a trench electrode (e.g., gate electrode or field electrode) within the trench.
[0144] Further details and aspects are mentioned in connection with the embodiments described above or below. Fig. The embodiments shown in Figure 8 may comprise one or more optional additional features corresponding to one or more aspects that may be used in connection with the proposed concept or one or more of the preceding (e.g. Fig. 1a to 7) or embodiments described below.
[0145] Some embodiments relate to power MOSFETs with steep epi and substrate ends.
[0146] Pure arsenic epitaxy combined with processes exhibiting strong arsenic segregation, such as trench transistors comprising a thick thermal trench bottom oxide, can be challenging because a major portion of the arsenic concentration may remain close to the trench sidewall surface and negatively impact the field plate breakdown parameters. Strong accumulation at the FOX interface for arsenic epi may occur.
[0147] Utilizing the good characteristics of arsenic epitaxy and the very steep transition towards the arsenic substrate in the bottom portion of the transistor cell can be proposed by including a first (thinner) arsenic-doped epitaxial layer followed by a phosphorus-doped second epitaxial layer, which can be essentially as thick as the target trench depth. In this way, it can be guaranteed that phosphorus is the only dopant (or main dopant) throughout the entire trench depth range, thus allowing the good characteristics of phosphorus segregation and, in turn, outdiffusion in the trench region to occur. For example, a 40 V power transistor may have a trench depth of approximately 2 µm, and the total thickness of the epitaxial layer required to block 40 V may be approximately 3.5 µm.From this, an n++-doped arsenic substrate followed by an arsenic-doped 1.5 µm thick epitaxial layer 1, in turn followed by a phosphorus-doped 2.0 µm thick epitaxial layer 2 can be implemented.
[0148] For example, the use of a multilevel epitaxial layer with different dopants to prevent adverse segregation effects in the direct trench (bottom) region with a simultaneously optimized steep substrate epi-end can be proposed.
[0149] The doping profile and used dopant species can be measured, for example, by secondary ion mass spectrometry SIMS.
[0150] Examples may further provide a computer program having program code for performing any of the above methods when the computer program is executed on a computer or processor. One skilled in the art would readily recognize that steps of various methods described above may be performed by programmed computers. Herein, some examples are also intended to cover program storage devices, e.g., digital data storage media, that are machine- or computer-readable and encode machine-executable or computer-executable programs of instructions, where the instructions perform some or all of the steps of the above-described methods. The program storage devices may be, for example, digital memories, magnetic storage media such as magnetic disks and magnetic tapes, hard disk drives, or optically readable digital data storage media.Also, further examples are intended to cover computers programmed to perform the steps of the methods described above or (field) programmable logic arrays ((F)PLA = (Field) Programmable Logic Arrays) or (field) programmable gate arrays ((F)PGA = (Field) Programmable Gate Arrays) programmed to perform the steps of the methods described above.
[0151] The description and drawings only illustrate the principles of the disclosure. It is therefore to be understood that those skilled in the art can devise various arrangements which, although not expressly described or illustrated herein, embody the principles of the disclosure and are included within its spirit and scope. Further, any examples provided herein are expressly intended to be for instructional purposes only to assist the reader in understanding the principles of the disclosure and the concepts contributed by the inventor(s) to advance the art, and are to be construed as serving without limitation to such specifically recited examples and conditions. Furthermore, all statements herein concerning principles, aspects, and examples of the disclosure, as well as specific examples thereof, are intended to include equivalents thereof.
[0152] Function blocks described as "means for..." (performing a certain function) are to be understood as functional blocks comprising circuits, each of which is configured to perform a certain function. Therefore, a "means for something" can also be understood as "means configured for or suitable for something." Therefore, a means configured to perform a certain function does not mean that such a means necessarily performs the function (at a given time).
[0153] Those skilled in the art should understand that all block diagrams herein represent conceptual views of exemplary circuits embodying the principles of the disclosure. Similarly, it should be understood that all sequence diagrams, flowcharts, state transition diagrams, pseudocode, and the like represent various processes substantially embodied in computer-readable medium and thus capable of being executed by a computer or processor, regardless of whether such a computer or processor is explicitly depicted.
[0154] Furthermore, the following claims are hereby incorporated into the Detailed Description, where each claim may stand on its own as a separate example. While each claim may stand on its own as a separate example, it should be noted that although a dependent claim may refer to a particular combination with one or more other claims in the claims, other examples may include a combination of the dependent claim with the subject matter of any other dependent or independent claim. These combinations are suggested herein unless it is stated that a particular combination is not intended. Furthermore, features of a claim for any other independent claim are also intended to be included, even if that claim is not made directly dependent on the independent claim.
[0155] It should further be noted that methods disclosed in the description or in the claims may be implemented by an apparatus having means for performing each of the respective steps of those methods.
[0156] Furthermore, it should be understood that the disclosure of multiple steps or functions disclosed in the description or claims should not be construed as being in that particular order. Therefore, the disclosure of multiple steps or functions does not limit them to any particular order, unless those steps or functions are not interchangeable for technical reasons. Furthermore, in some examples, a single step may include or be broken down into multiple substeps. Such substeps may be included and form part of the disclosure of that single step unless expressly excluded.
Claims
[1] A semiconductor device (500) comprising: a drift region of a device structure arranged in a semiconductor layer (102), the drift region comprising at least a first drift region portion (502) and at least a second drift region portion (504), a majority of dopants within the first drift region portion (502) being a first species of dopants having a diffusivity of less than a diffusivity of phosphorus within the semiconductor layer (102), a majority of dopants within the second drift region portion (504) being a second species of dopants; and a trench (510) extending from a surface of the semiconductor layer (102) into the semiconductor layer (102), wherein a vertical distance between the surface of the semiconductor layer (102) and a boundary (503) between the first drift region portion (502) and the second drift region portion (504) is greater than 0.5 times a maximum depth of the trench (510) and less than 1.5 times the maximum depth of the trench (510), wherein the second drift region portion (504) is arranged between the surface of the semiconductor layer (102) and the first drift region portion (502). [2] The semiconductor device according to claim 1, wherein the device structure is a transistor structure and the trench (510) is a gate trench of the transistor structure, wherein a gate electrode of the transistor structure is arranged within the gate trench. [3] The semiconductor device according to any one of the preceding claims, further comprising a body region of the device structure, wherein the body region is arranged adjacent to the at least one second drift region portion (504). [4] The semiconductor device according to any one of the preceding claims, wherein a maximum doping concentration within the first drift region portion (502) and the second drift region portion (504) of the drift region is less than 1*10 18 Dopant atoms per cm 3 . [5] The semiconductor device according to any one of the preceding claims, wherein an average net doping concentration value of the drift region is at least 1*10 16 Dopant atoms per cm 3 is. [6] The semiconductor device according to any one of the preceding claims, wherein a local minimum of the net doping concentration of the drift region is located at the boundary (503) between the first drift region portion (502) and the second drift region portion (504). [7] The semiconductor device according to any one of the preceding claims, wherein the vertical distance between the surface of the semiconductor layer (102) and a boundary (503) between the first drift region portion (502) and the second drift region portion (504) is greater than the maximum depth of the trench (510). [8] The semiconductor device according to any one of the preceding claims, wherein the second species of dopant atoms is phosphorus. [9] The semiconductor device according to any one of the preceding claims, wherein a vertical extension of the first drift region portion (502) is greater than 1 µm. [10] The semiconductor device according to any one of the preceding claims, further comprising a semiconductor substrate (103) arranged adjacent to the semiconductor layer (102), wherein a doping concentration at a transition from the drift region to the semiconductor substrate (103) varies between a first doping concentration value and a second doping concentration value over a distance of less than 500 nm, wherein the first doping concentration value is an average net doping concentration of a central portion of the drift region plus 20% of the average net doping concentration of the central portion of the drift region, wherein the central portion of the drift region lies within a central 50% of a vertical dimension of the drift region; and wherein the second doping concentration value is an average net doping concentration of the central portion of the drift region plus one decade. [11] A semiconductor device (100, 200, 300) comprising: a drift region (101) of a component structure arranged in a semiconductor layer (102) arranged adjacent to a semiconductor substrate (103), wherein a doping concentration at a transition from the drift region (101) to the semiconductor substrate (103) varies between a first doping concentration value and a second doping concentration value over a distance of less than 500 nm, wherein the first doping concentration value is an average net doping concentration of a central portion of the drift region plus 20% of the average net doping concentration of the central portion of the drift region, wherein the central portion of the drift region lies within a central 50% of a vertical dimension of the drift region; and wherein the second doping concentration value is an average net doping concentration of the central portion of the drift region plus one decade. [12] The semiconductor device according to any one of claims 10 to 11, wherein the doping concentration at the junction from the drift region (101) to the semiconductor substrate (103) increases from the first doping concentration value to the second doping concentration value over a distance of more than 100 nm. [13] The semiconductor device according to any one of claims 10 to 12, wherein the semiconductor substrate (103) is doped with dopant atoms having a diffusivity of less than a diffusivity of phosphorus within the semiconductor substrate. [14] The semiconductor device according to any one of claims 10 to 13, wherein the semiconductor layer (102) and the semiconductor substrate (103) are doped with the same doping atoms. [15] The semiconductor device according to any one of claims 10 to 14, wherein an average net doping concentration of a source or collector region arranged in the semiconductor substrate is at least 1*10 19 Dopant atoms per cm 3 is. [16] The semiconductor device according to any one of the preceding claims, wherein the semiconductor layer (102) has a thickness of less than 8 µm. [17] The semiconductor device according to any one of the preceding claims, wherein the semiconductor layer (102) is an epitaxially grown semiconductor layer. [18] The semiconductor device according to any one of the preceding claims, wherein the device structure of the semiconductor device has a breakdown voltage of at least 10 V. [19] A method (800) of forming a semiconductor device, the method comprising: epitaxially growing (810) a first epitaxial semiconductor sublayer of a semiconductor layer, wherein a majority of dopants within the first epitaxial semiconductor sublayer are a first species of dopants having a diffusivity of less than a diffusivity of phosphorus within the semiconductor layer; epitaxially growing (820) a second epitaxial semiconductor sublayer of a semiconductor layer after forming the first epitaxial semiconductor sublayer, wherein a majority of dopants within the second epitaxial semiconductor sublayer are a second species of dopants; and Forming (830) a trench extending from a surface of the semiconductor layer into the semiconductor layer, wherein a vertical distance of a boundary between the first epitaxial semiconductor sub-layer and the second epitaxial semiconductor sub-layer to the surface of the semiconductor layer is greater than 0.5 times a maximum depth of the trench and less than 1.5 times the maximum depth of the trench, wherein the second epitaxial semiconductor sublayer is arranged between the surface of the semiconductor layer (102) and the first epitaxial semiconductor sublayer.
Citation Information
Patent Citations
Double diffused field effect transistor having reduced on-resistance
US20040178444A1
Buried field ring field effect transistor (BUF-FET) integrated with cells implanted with hole supply path
US20150118810A1
Method of fabricating semiconductor device having grooved source contact region
US9318566B2