Method for forming semiconductor devices with preparatory trenches formed in interface areas for die singulation

DE102019129091B4Active Publication Date: 2024-10-10INFINEON TECHNOLOGIES AG
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
DE102019129091
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-10-31
Filing Date
2019-10-28
Publication Date
2024-10-10
Estimated Expiration
2039-10-28

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A method for forming a semiconductor device, the method comprising: providing a semiconductor wafer (100) having a main surface (102) and a back surface (104) opposite the main surface (102); performing a step to prepare a die singulation in kerf regions (108) of the semiconductor wafer (100), wherein the kerf regions (108) encompass a plurality of the die sites (106), the step to prepare a die singulation comprising forming one or more preparatory kerf trenches (112) between at least two immediately adjacent die sites (106) in the plurality; forming active semiconductor devices in the die sites (106);and singling of the semiconductor wafer (100) in the kerf regions (108), whereby a plurality of separate semiconductor dies (110) are formed from the die sites (106), wherein the one or more kerf trenches (112) are not filled during singling, and wherein the singling comprises the removal of semiconductor material from a surface of the semiconductor wafer (100) located between opposite side walls of the one or more preparatory kerf trenches (112), and wherein the formation of the active semiconductor devices comprises the formation of a trench-formed electrode structure (118) in cell field trenches (122) in the die sites (106), and wherein the cell field trenches (122) and the one or more preparatory kerf trenches (112) are formed simultaneously by means of a common etching step.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELDThe present application relates to fabrication of semiconductor devices and, in particular, relates to dicing wafers.BACKGROUNDDie singulation refers to the step or steps used to separate individual die locations from the semiconductor wafer and form separate semiconductor dies. A variety of different techniques can be used to cut the semiconductor wafer in a singulation process. Examples of these techniques are known from publications US 2006 / 0 292 830 A1, US 2017 / 0 140 989 A1 and DE 10 2006 037 789 A1. Singulation processes include mechanical sawing, laser cutting and chemical etching techniques, to name a few. These techniques suffer from various disadvantages including the formation of cracks in the active region of the semiconductor dies and / or the formation of a recast material on the main surface of the semiconductor wafer. These disadvantages adversely affect the yield and / or performance of the separate semiconductor dies.One technique used to improve known die singulation processes is the inclusion of a so-called kerf cleaning process. This process is used to remove structures such as test structures and / or lithography alignment features formed in the kerf regions of the semiconductor wafer prior to singulation. This prevents the kerf region structures from interfering with the cutting mechanism (e.g., a saw blade). However, known kerf cleaning processes add additional cost to the process and result in rough surfaces that are prone to cracking and / or reducing die strength.Silicon carbide (SiC) technology presents unique challenges with regard to die singulation. Due to the hardness of the SiC material, mechanical sawing techniques generally cause chipping of the material, resulting in yield losses. In addition, the hardness of the SiC material causes saw blades to wear and break. For this reason, laser ablation is commonly used to cut SiC or SiC-based wafers. A disadvantage of laser ablation is that evaporated semiconductor material on the main surface of the semiconductor die can reform as recast material, which can lead to yield losses and complete device failure.SUMMARYThose skilled in the art will recognize additional features and advantages upon reading the following detailed description and upon viewing the accompanying drawings.The invention is defined in the independent claims. Further embodiments are defined in the dependent claims. A method of forming a semiconductor device is disclosed. According to one embodiment, the method comprises providing a semiconductor wafer having a main surface and a back surface opposite the main surface. A die singulation preparation step is performed in kerf regions of the semiconductor wafer. The kerf regions enclose a plurality of die sites. The die singulation preparation step comprises forming one or more preparatory kerf trenches between at least two immediately adjacent die sites in the plurality. The method further comprises forming active semiconductor devices in the die sites and singulating the semiconductor wafer in the kerf regions, thereby forming a plurality of separate semiconductor dies from the die sites. The one or more preparatory kerf trenches are not filled during singulation, and singulation includes removing semiconductor material from a surface of the semiconductor wafer that lies between opposing sidewalls of the one or more preparatory kerf trenches. Forming the active semiconductor devices includes forming a trenched electrode structure in cell array trenches in the die sites. The cell array trenches and the one or more preparatory kerf trenches are formed simultaneously using a common etching step.According to another embodiment, the method comprises providing a semiconductor wafer having a main surface and a back surface opposite the main surface. Cell field trenches and preparatory kerf trenches are formed in the main surface of the semiconductor wafer by means of a common etching step. The preparatory kerf trenches are formed in a grid pattern enclosing a plurality of die sites. The cell field trenches are formed within the die sites. The plurality of die sites are singulated from the semiconductor wafer into a plurality of separate semiconductor dies. The singulation includes forming a cut between bottom surfaces of the preparatory kerf trenches and the back surface.According to another embodiment, the method includes providing a silicon carbide-containing wafer having a main surface and a back surface opposite the main surface. A grid pattern of preparatory kerf trenches is formed in the main surface of the silicon carbide-containing wafer. The grid pattern encloses a plurality of die sites. Laser ablation is performed on a top surface of the silicon carbide-containing wafer that lies between opposing sidewalls of the preparatory kerf trenches. Performing the laser ablation causes recast material to form substantially along the opposing sidewalls. The main surface of the semiconductor wafer in the active die sites is substantially free of recast material after performing the laser ablation.SHORT DESCRIPTION OF THE CHARACTERSThe elements of the drawings are not necessarily to scale with respect to one another. Like reference numerals indicate corresponding similar parts. The features of the various embodiments illustrated may be combined unless they are mutually exclusive. Embodiments are illustrated in the drawings and are set forth in detail in the description that follows. Fig. 1, which includes Fig. 1A and Fig. 1B, illustrates a technique for singulating a semiconductor wafer according to an embodiment. Fig. 1A illustrates a top view of the semiconductor wafer before singulation. Fig. 1B illustrates a cross-sectional view of the semiconductor wafer after singulation. 2 illustrates a method for forming a preparatory kerf trench in the kerf region of a semiconductor wafer prior to singulation according to an embodiment. 3 illustrates a method of singulating the semiconductor wafer after forming the preparatory kerf trench according to an embodiment. Fig. 4 illustrates forming a further trench in the preparatory kerf trench prior to singulation according to one embodiment. Fig. 5 illustrates forming a further trench in the preparatory kerf trench prior to singulation according to another embodiment. Fig. 6 illustrates a formation of a splinter stop structure adjacent to the preparatory kerf trench prior to singulation according to an embodiment. 7, which includes FIGS. 7A and 7B, illustrates various layouts of the preliminary kerf trenches. FIG. 7A illustrates a layout with substantially perpendicular intersections between sidewalls of the preliminary kerf trenches according to an embodiment. FIG. 7B illustrates a layout with obtuse-angled transitions between intersecting sidewalls of the preliminary kerf trenches according to an embodiment. 8 illustrates a method for forming preparatory kerf trenches in the kerf region of a semiconductor wafer prior to singulation according to another embodiment. 9 illustrates forming active semiconductor devices in the die sites after forming the preparatory kerf trenches according to an embodiment. Fig. 10 illustrates singulation of the semiconductor wafer after forming the active semiconductor devices according to an embodiment. 11 illustrates performing a further step of removing semiconductor material after forming the preparatory kerf trenches and prior to singulation according to an embodiment. Fig. 12 illustrates a singulation of the semiconductor wafer according to an embodiment.DETAILED DESCRIPTIONAccording to embodiments described herein, preparatory kerf trenches are formed in kerf regions of a semiconductor wafer prior to singulation. The semiconductor wafer is cut at a position that is within one of the preparatory kerf trenches or between adjacent trenches of the preparatory kerf trenches. In any case, the preparatory kerf trenches provide a cost-effective technique for singulating semiconductor dies with improved yield and reliability of the final products. Benefits of the technique include smoother edge sides in the singulated semiconductor dies, a reduced likelihood of cracking from singulation, and the avoidance of accumulation of recast material on the surface of the singulated semiconductor dies. In addition, the formation of the preparatory kerf trenches eliminates the need for a kerf cleaning process, thereby reducing costs and increasing the speed of the singulation process.Referring to FIG. 1, a general overview of a technique for singulating a semiconductor wafer 100 is illustrated. The semiconductor wafer 100 includes a main surface 102 and a back surface 104 opposite the main surface 102. The main and back surfaces 102, 104 may be substantially planar surfaces. The semiconductor wafer 100 may include any crystalline semiconductor material suitable for fabricating semiconductor devices. Example materials for the semiconductor wafer 100 include silicon (Si), Group IV compound semiconductor materials such as silicon carbide (SiC) or silicon germanium (SiGe). Alternatively, the semiconductor wafer 100 may include a Type III-V semiconductor including gallium nitride, gallium arsenide (GaAs), aluminum nitride (AlN), aluminum arsenide (AlAs), indium nitride (InN), indium arsenide (InAs), etc. The semiconductor wafer 100 may be formed from a commercially available bulk semiconductor wafer. According to one embodiment, the semiconductor wafer 100 includes a base substrate (e.g., a bulk silicon wafer) forming the back surface 104 and one or more epitaxial layers formed on the base substrate, the topmost of which extends to the main surface 102.As shown in FIG. 1A, the semiconductor wafer 100 includes a plurality (i.e., two or more) of the die sites 106. The die sites 106 are locations on the semiconductor wafer 100 that contain active semiconductor devices, e.g., transistors, diodes, thyristors, etc. The die sites 106 are bounded by kerf regions 108 that enclose the die sites 106. As shown, the kerf regions 108 form a grid pattern with intersecting kerf regions 108 that may be perpendicular to each other. The kerf regions 108 are inactive regions that do not contain active semiconductor devices. Various temporary structures may be formed in the kerf regions 108 prior to singulation. Examples of these temporary structures include test structures for testing technology-specific parameters of the wafer (e.g., a process control monitoring (PCM) structure) and / or mask alignment features.As shown in FIG. 1B, the semiconductor wafer 100 is singulated (i.e., cut) in the kerf regions 108. As a result, the die sites 106 of the semiconductor wafer 100 are separated into a plurality of separate semiconductor dies 110. Various techniques for performing this singulation process are described in further detail below. Each separate semiconductor die forms a complete functional integrated circuit. Examples of these devices include power transistors, amplifier devices, processors, controllers, etc.Referring to FIG. 2, a cross-sectional view of a semiconductor wafer 100 is shown in accordance with an embodiment. In this example, the semiconductor wafer 100 was processed prior to singulation to form a preparatory kerf trench 112 in the kerf region 108 in accordance with an embodiment. The cross-sectional view is taken between two of the die sites 106 and one of the kerf regions 108 as described with reference to FIG. 1. In this embodiment, each die site 106 includes an active device region 114 and a termination region 116. The active device region 114 includes active semiconductor devices that directly contribute to the logical functionality of the finished semiconductor die. In contrast, the termination region 116 includes structures that do not directly contribute to the logical functionality of the finished semiconductor die. The termination region 116 is disposed between the active device region 114 and the kerf region 108. Thus, the termination region 116 separates the active device region from the outer chip edges of the singulated semiconductor dies. In one embodiment, the termination region 116 forms a closed loop that bounds the kerf regions 108 and the active device region 114 in all directions.In the illustrated embodiment, the active device region 114 includes one or more vertical transistor devices. These vertical transistor devices are formed from a plurality of trenched electrode structures 118 formed between doped semiconductor regions 120 (e.g., n-type or p-type regions). The trenched electrode structures 118 comprise cell array trenches 122 extending from the main surface 102 into the semiconductor body. A conductive electrode and a trench dielectric are formed in each cell array trench. The conductive electrode may be made of an electrically conductive material, e.g., polysilicon or a conductive metal. The trench dielectric may be made of an electrical insulator, e.g., silicon dioxide (SiO2), silicon nitride (SiN), silicon oxynitride (SiOxNy), etc. The doped semiconductor regions 120 form the active regions of the semiconductor device, e.g., drain regions, body regions, source regions, emitter regions, collector regions, etc. The electrode structures 118 formed in trenches may be configured as gate structures that control a conduction state of a current flowing between the doped semiconductor regions 120. Additionally or alternatively, the electrode structures 118 formed in trenches may be configured as field electrode structures that provide compensating charges for neighboring semiconductor regions (e.g., drift regions) within the semiconductor body.More generally, the active device region 114 may include a wide variety of active semiconductor devices such as transistors, diodes, thyristors, etc. These active devices may be so-called vertical devices configured to conduct in a vertical direction of the semiconductor wafer 100 between the main and back surfaces 102, 104, or so-called lateral devices configured to conduct in a lateral direction of the semiconductor wafer 100 that is parallel to the main surface 102.In the illustrated embodiment, the termination region 116 includes a number of field termination trenches 124 immediately adjacent to the trenched electrode structures 118 of the active semiconductor devices. These field termination trenches 124 include a conductive electrode and a dielectric material. According to an embodiment, the field termination trenches 124 have a different geometry (i.e., depth and / or width) to the cell array trenches 122. The field termination trenches 124 may be configured to direct equipotential lines away from the chip edge of the singulated semiconductor die. More generally, the termination region 116 may include a variety of different structures serving a variety of different purposes, e.g., field termination, chip stop, mask alignment, etc.In the illustrated embodiment, the semiconductor wafer 100 additionally includes first and second dielectric layers 126, 128 formed on the main surface 102 of the semiconductor wafer 100. Both the first and second dielectric layers 126, 128 may include an electrically insulating material, e.g., silicon dioxide (SiO2), silicon nitride (SiN), silicon oxynitride (SiOxNy), etc. These first and second dielectric layers 126, 128 may be formed according to known deposition and / or thermal oxidation techniques. As illustrated, the first dielectric layer 126 may be formed in the field termination trenches 124 to provide dielectric isolation of the trench-formed electrode structures 118. A first metallization layer 130 of e.g. copper is provided on the second dielectric layer 128 and provides device terminals (e.g. gate, source, etc.) for the active semiconductor devices. Finally, an interlayer dielectric layer 132 is formed on the first metallization layer 130 and the second dielectric layer 128. The interlayer dielectric layer 132 may be a relatively thick (e.g. 5 - 20 µm) layer of an electrically insulating material, e.g. silicon dioxide (SiO2), imide, etc. A notch 134 may be formed in the termination region 116, with the interlayer dielectric layer 132 filling the notch 134. This provides a so-called diffusion stop structure that prevents potentially harmful ions (e.g. Na+ ions) from reaching the active semiconductor devices.A preparatory kerf trench 112 is formed in the kerf region 108. The preparatory kerf trench 112 is a recessed structure having opposing sidewalls 136 extending from the main surface 102 toward the back surface 104. These opposing sidewalls 136 may be perpendicular to the main surface 102, but are not necessarily so. A bottom surface 138 of the preparatory kerf trench 112 extends between the opposing sidewalls 136. Generally speaking, the dimensions of the preparatory kerf trench 112 may vary. As will be explained in further detail below, the preparatory kerf trench 112 may be formed in a common process as the cell array trenches 122. However, these two trenches may have different dimensions, i.e., depth and / or width. For example, the trenches 122 of cell trenches may have a depth in the range of 2 - 3 µm, whereas the preparatory kerf trench 112 may have a depth in the range of 3 - 6 µm. Furthermore, the cell array trenches 122 may have a width in the range of 0.5 - 2.5 µm, whereas the preparatory kerf trench 112 may have a width in the range of 25 - 100 µm. In a particular embodiment, the preparatory kerf trench 112 has a width of about 75 µm. In the case of a semiconductor wafer 100 comprising a base substrate and an epitaxial layer extending to the main surface 102 of the semiconductor wafer 100, the depth of the preparatory kerf trench 112 may be correlated with the thickness of the epitaxial layer. For example, the preparatory kerf trench 112 may have a depth that is between 50% and 150% of a thickness of the epitaxial layer. In the case of a preparatory kerf trench 112 having a depth that is 100% or more of the thickness of the epitaxial layer, the preparatory kerf trench 112 extends into the underlying base substrate. The width of the preparatory kerf trench 112 may occupy all or at least substantially all (i.e., at least 50-75%) of the width of the kerf region 108. From the perspective of a top view of the semiconductor wafer 100, the preparatory kerf trenches 112 may be formed in the same grid pattern as the kerf regions 108 as shown in FIG. 1, such that each die site 106 is separated from an immediately adjacent die site 106 in all directions by the preparatory kerf trench 112. Alternatively, the preparatory kerf trenches may be provided only in selected kerf areas in the grid pattern.According to an embodiment, the preparatory kerf trenches 112 and the cell array trenches 122 are formed by means of a common etching process. This means that the same etchant step that forms the cell array trenches 122 simultaneously forms the preparatory kerf trenches 112. For example, a common hard mask (not shown) may be provided on the main surface 102 and patterned to include openings in the geometry of the preparatory kerf trenches 112 and the cell array trenches 122. Subsequently, the semiconductor wafer 100 may be etched (e.g., by means of reactive ion etching) to remove semiconductor material through these openings. In various etching techniques including reactive ion etching, according to the values described above, the preparatory kerf trenches 112 may be formed deeper and wider than the cell array trenches 122 by patterning the hard mask such that openings for the preparatory kerf trenches 112 have a larger exposed semiconductor area than the openings for the cell array trenches 122. After this etching step, the first dielectric layer 126 may be deposited on the semiconductor body. As a result, the first dielectric layer 126 is formed in the cell array trenches 122 and also lines the sidewalls 136 and the bottom surface 138 of the preparatory kerf trenches 112. Advantageously, using common processing steps, the preparatory kerf trenches 112 may be formed with the first dielectric layer 126 lining the sidewalls 136 thereof without adding additional cost or time delay to the manufacturing process.More generally, the preparatory kerf trenches 112 may be formed at any point in the manufacturing process prior to singulation. That is, the preparatory kerf trenches 112 may be formed before, during, or after forming the active semiconductor devices in the active device regions 114. Moreover, the preparatory kerf trenches 112 may be formed using any conventional trench formation technique, e.g., wet chemical etching, dry etching, etc.Optionally, the preparatory kerf trench 112 as well as the adjacent termination regions 116 may be covered by the layer (not shown in Figure 2) of a soft material such as, but not limited to, imide. This additional layer encapsulates the kerf trench sidewall 136 and adjacent regions and protects the substrate against stress induced cracks. Such stress may originate from hard material particles commonly used in cast joints. The size and hardness of these particles in the cast joints are randomly distributed. By adding a soft material, the particles are particularly kept away from the device corners and stress transfer from particles to the substrate is prevented.3, a dicing process is performed on the semiconductor wafer 100. According to this process, semiconductor material is removed from a lateral surface of the semiconductor wafer 100 (i.e., a surface parallel to the main surface 102) that lies within the kerf region 108 and is disposed between opposing sidewalls 136 of the preparatory kerf trench 112. This process is performed until the semiconductor wafer 100 is completely severed in the kerf region 108, meaning that each die site 106 is physically detached from the semiconductor wafer 100, thereby forming a plurality of separate semiconductor dies from the die sites 106. In this example, the cut is formed between the bottom surface 138 and the back surface 104 of the semiconductor wafer. As a result, an outer edge side for each of the separate semiconductor dies is formed by the interface and one of the sidewalls 136.The dicing process may be performed using a variety of known techniques for cutting a semiconductor wafer 100. For example, the dicing process may include a mechanical sawing process, whereby the semiconductor wafer 100 is physically cut using a saw blade. Alternatively, the dicing process may include a laser cutting process, whereby the semiconductor wafer 100 is exposed to a high energy beam of light that forms a cut in the semiconductor material. Alternatively, the dicing process may include a plasma etching technique, whereby a chemically reactive plasma is used to remove the semiconductor material.According to an embodiment, the preparatory kerf trenches 112 are not filled during singulation of the semiconductor wafer 100. This means that during dicing, the preparatory kerf trenches 112 comprise an accessible or open area with an ambient atmosphere between the opposing sidewalls 136 and below the main surface 102. The semiconductor surfaces of the preparatory kerf trenches 112 (i.e., the outer sidewalls 136 and the bottom surface 138) may be lined by one or more layers (e.g., the first dielectric layer 126 as shown) and may be considered “unfilled” according to the present application. In contrast, a trench containing any or a combination of a dielectric, semiconductive or conductive material extending at least to the main surface 102 is considered filled according to the present application.The above-described method of forming preparatory kerf trenches 112 prior to dicing provides several advantages over conventional dicing techniques. The preparatory kerf trenches 112 ensure that there are no structures that can interfere with the dicing mechanism (e.g., a saw blade) during dicing and potentially induce cracking. Consequently, the preparatory kerf trenches 112 eliminate the need for a kerf cleaning process that adds time delay and cost to the dicing process. In addition, the preparatory kerf trenches 112 reduce the effective thickness of the wafer to be diced and, consequently, reduce mechanical stress of adjacent die sites 106 during the dicing process. This reduces the likelihood of chipping. In addition, since the preparatory kerf trenches 112 extend deeper into the semiconductor body than the cell array trenches 122, the semiconductor material susceptible to crystalline defects (i.e., the region near the main surface 102) is protected from fracture by the first dielectric layer 126 on the sidewalls 136 of the preparatory kerf trenches 112.Referring to Fig. 4, an optional step that may be added to the singulation process described above is illustrated according to an embodiment. According to this technique, after forming the preparatory kerf trench 112, another trench 140 is formed in the bottom of the preparatory kerf trench 112. The another trench 140 is narrower than the preparatory kerf trench 112, which means that a distance between opposing side walls of the another trench 140 is less than the distance between the opposing side walls 136 of the preparatory kerf trench 112. Generally speaking, the width of the another trench 140 may be between half the width of the preparatory kerf trench 112 and substantially the entire width of the preparatory kerf trench 112, e.g., between about 50% and 90% of a width of the preparatory kerf trench 112. The depth of the further trench 140 may vary substantially, for example, between about 5% and 50% of a thickness of the semiconductor wafer 100, measured from the bottom surface 138 of the preparatory kerf trench 112 to the back surface 104.An advantage of this technique of Fig. 4 is a reduction in the thickness of the semiconductor material that must be cut, thereby providing further stress relief. Furthermore, in the case of a laser cutting process, the sidewalls of the further trench 140 form a surface that attracts recast material.The further trench 140 may be formed by performing an additional etching process at any time between the formation of the preliminary kerf trench 112 and the singulation process. Thereafter, the singulation process is performed as described above at the position 142 indicated in the figure. As can be seen, the cut is formed within the further trench 140. That is, the cut is formed between the bottom of the further trench 140 and the back surface 104.Referring to Fig. 5, an alternative technique involving forming the further trenches 140 is described according to an embodiment. According to this, the cut is formed at a position 142 that lies outside the further trench 140. In the illustrated embodiment, a plurality of the further trenches 140 are formed. The further trenches 140 are substantially narrower than the preliminary kerf trench 112, e.g., about 10% of the width of the preliminary kerf trench 112. In the illustrated embodiment, two of the further trenches 140 are formed. More generally, any number such as one, three, four, etc. of the further trenches 140 may be formed. The width of these further trenches 140 may vary substantially between about 50% and 5% of the width of the preliminary kerf trench 112. The depth of these further trenches 140 may vary substantially, e.g., between 5% and 50% of a thickness of the semiconductor wafer 100, measured from the bottom surface 138 of the preparatory kerf trench 112 to the back surface 104. An advantage of these further trenches 140 is an additional crack-stopping mechanism that prevents cracks caused by the cutting mechanism from reaching the die locations 106.Referring to FIG. 6, an optional step that may be added to any of the above-described variants of a singulation process is illustrated according to an embodiment. According to this technique, a splitter stop structure 144 is formed in the termination region 116 prior to singulation. The splitter stop structure 144 is arranged immediately adjacent to one of the sidewalls 136 of the preparatory kerf trench 112. This means that no intentionally formed structures necessary for the function or performance of the separate semiconductor dies (e.g., gate trenches, field plates, edge termination structures, etc.) are provided between the splitter stop structure 144 and the preparatory kerf trench 112. The splitter stop structure 144 comprises a splitter stop trench 146 extending from the main surface 102 into the semiconductor body. The splitter stop trench 146 is separated from the back surface 104 by semiconductor material. That is, the splitter stop trench 146 does not extend entirely through the semiconductor material. If the semiconductor wafer 100 includes an epitaxial layer formed on a base substrate (e.g., a bulk semiconductor wafer), the splitter stop trench 146 may extend partially into the epitaxial layer such that it is separated from the base substrate by a region of the epitaxial layer. The splitter stop trench 146 additionally includes a dielectric material filling the splitter stop trench 146. According to an embodiment, the splitter stop trench 146 includes a dielectric layer (e.g., SiO2) and an electrically conductive material (e.g., polysilicon) formed within the splitter stop trench 146. The dielectric layer and the electrically conductive material may be formed according to similar or identical techniques as the cell array trenches 122 with a conductive electrode and a dielectric material. In one embodiment, each of these structures is formed by a common processing step or steps.The splitter stop structure 144 is configured to provide a termination or end point for cracks that propagate from the kerf region 108 into the die site 106 during the singulation process. In the singulation steps described above, there is a possibility that cracks may form at the corner of the preparatory kerf trenches 112. Some of these cracks may propagate away from the preparatory kerf trenches 112 and toward the main surface 102. Since the splitter stop structure 144 does not contribute to the functionality of the device, these cracks may terminate at or in the material filling the splitter stop structure 144 without affecting the function of the singulated semiconductor die.Referring to FIG. 7, two different configurations are illustrated in a top view for the preparatory kerf trenches 112 at the wafer level. As shown in FIG. 7A, the preparatory kerf trenches 112 may be formed in a grid pattern that mirrors the pattern of the kerf regions 108 as shown in FIG. 1A. In this configuration, the preparatory kerf trenches 112 extend laterally across the semiconductor wafer 100 in two different directions and thus intersect with each other at regularly spaced points. These two different directions may be orthogonal to each other such that the intersecting trenches of the preparatory kerf trenches 112 are perpendicular to each other.In the embodiment of Fig. 7A, the side walls 136 of the intersecting preparatory kerf trenches 112 form a substantially perpendicular angle at the intersections. In contrast, in the embodiment of Fig. 7B, obtuse-angled transitions 148 are formed between the side walls 136 of the intersecting preparatory kerf trenches 112. The obtuse-angled transitions 148 are formed by an angled side wall portion 150 that is angled with respect to the side walls 136 of the intersecting trenches of the preparatory kerf trenches 112. In a particular embodiment, this angled sidewall portion 150 forms an angle of about 45 degrees with both sidewalls 136 of the intersecting preparatory kerf trenches 112. More generally, the angled sidewall portion 150 may be angled between about 30 and 60 degrees with respect to the adjacent sidewall of the respective preparatory kerf trenches 112. Additionally, rather than a planar structure as shown, the obtuse-angled transition 148 may include a variety of geometries including curved and / or conical surfaces. An advantage of the obtuse-angled transitions 148 is a reduced possibility of cracking of the semiconductor wafer 100 during dicing, e.g., from a mechanical sawing process.Referring to FIG. 8, another embodiment for singulating a semiconductor wafer 100 is illustrated that includes forming preparatory kerf trenches 112 prior to singulation. According to this technique, a semiconductor wafer 100 is provided. After providing the semiconductor wafer 100, first and second preparatory kerf trenches 112 are formed in the kerf region 108 between each die site 106. From a top view perspective of the semiconductor wafer 100, the first and second preparatory kerf trenches 112 may be formed in a grid pattern as shown in FIG. 1. The first and second preparatory kerf trenches 112 may be formed according to the techniques previously described, e.g., by means of a masked etch.9, after forming the first and second preparatory kerf trenches 112, further processing steps are performed to form active semiconductor devices in the die sites 106. In a specific example, the semiconductor wafer 100 is a silicon carbide wafer and the active semiconductor devices are SiC-based power devices such as a SiC-based JFET, diode, MOSFET, etc. More generally, the active semiconductor devices may have any of the previously described configurations and the semiconductor wafer 100 may include any of the previously described materials. Terminals of the active semiconductor devices may be provided by means of a front side metallization 152 provided on the main surface 102 and a back side metallization 154 provided on the back surface 104.10, after forming the preparatory kerf trenches 112 and the active semiconductor devices, a singulation process may be performed. In this example, the semiconductor wafer 100 is cut at a position located between opposing sidewalls 156 and 158 of two different trenches. Specifically, the cut is formed at a position located between a first sidewall 156 of the first preparatory kerf trench 112 and a second sidewall 158 of the second preparatory kerf trench 112. More specifically, the cut is formed at the portion of the upper surface 162 of the main surface 102 that extends between the first and second preparatory kerf trenches 112. As described in further detail below, further processing steps may be performed to lower the upper surface 162 in the kerf region 108. In any case, the cut is formed in a surface of the kerf region 108 that is parallel to the main surface 102 and disposed between the opposing sidewalls 156 and 158 of the preparatory kerf trenches 112. As a result, an outer edge side for each of the separate semiconductor dies is formed by the cut surface and one of the first and second sidewalls 156, 158.According to one embodiment, the singulation process is performed using laser ablation. According to this technique, the laser is applied to the top surface 156 of the semiconductor wafer 100 in central areas of the kerf regions 108 that lie between opposing sidewalls 156 and 158. During laser ablation, the evaporated semiconductor material removed from the semiconductor wafer 100 may accumulate along exposed semiconductor surfaces. Advantageously, the first and second opposing sidewalls 156, 158 of the first and second preparatory trenches provide respective exposed semiconductor surfaces that attract this recast material 160. In one embodiment, substantially all of the recast material 160 that forms on the semiconductor wafer 100 accumulates on the sidewalls 156, 158 of the preparatory kerf trenches 112. This means that only a minimal amount (e.g., less than 5% of the recast material 160) forms on the main surface 102 of the semiconductor wafer 100. This reduces the potential for device failure or performance degradation in the singulated semiconductor dies.Referring to Fig. 11, an alternative process sequence is illustrated according to an embodiment. According to this technique, the semiconductor wafer 100 is provided and processed as described with reference to Figs. 8 and 9. After these processing steps and before performing the dicing process, the upper surface 162 of the semiconductor wafer 100 extending between the first and second preparatory trenches is lowered to lie below the main surface 102 of the semiconductor wafer 100. That is, semiconductor material is removed from the area of the kerf regions 108 between the first and second preparatory kerf trenches 112 such that this area no longer extends to the main surface 102. In this example, the upper surface 162 is lowered to reach the bottom surfaces 138 of the first and second preparatory kerf trenches 112, thus forming a trench of a single depth across the kerf region 108. Alternatively, the upper surface 162 may be lowered to lie above or below the first and second preparatory trenches. This process of lowering the upper surface 162 may be accomplished, for example, using known etching techniques.Referring to Fig. 12, after lowering the top surface 162, the semiconductor wafer 100 is singulated using a laser ablation technique, e.g., as described above. As a result, the recast material 160 forms along the opposing first and second sidewalls 156, 158 in a manner similar to that described above. An advantage of the technique of Figs. 11-12 compared to the technique of Figs. 8-10 is that it lowers the surface to which the laser is applied, i.e., the top surface 162. This reduces the likelihood of the recast material 160 reaching the main surface 102 of the semiconductor wafer 100 outside of the kerf region 108.An embodiment of a method of forming a semiconductor device is disclosed. The method includes providing a semiconductor wafer having a main surface and a back surface opposite the main surface, performing a step of preparing for die singulation in kerf regions of the semiconductor wafer, the kerf regions enclosing a plurality of die sites, the step of preparing for die singulation comprising forming one or more preparatory kerf trenches between at least two immediately adjacent die sites in the plurality, forming active semiconductor devices in the die sites; and dicing the semiconductor wafer in the kerf regions, thereby forming a plurality of separate semiconductor dies from the die locations, wherein the one or more preparatory kerf trenches are not filled during dicing, and wherein dicing comprises removing a semiconductor material from a surface of the semiconductor wafer that lies between opposing sidewalls of the one or more preparatory kerf trenches.In one embodiment of the method, which may be combined with others, one of the opposite sidewalls forms an outer chip edge side for each of the separate semiconductor dies.In one embodiment of the method, which may be combined with others, forming the active semiconductor devices comprises forming a trenched electrode structure in cell array trenches in the die sites, and the cell array trenches and the one or more preparatory kerf trenches are formed simultaneously by means of a common etching step.In one embodiment of the method, which may be combined with others, the one or more preparatory kerf trenches are formed to be wider and deeper than the cell array trenches.In one embodiment of the method, which may be combined with others, after performing the common etching step, a dielectric layer is formed by means of a common deposition step along sidewalls of the cell array trenches and the one or more preparatory kerf trenches, and the dielectric layer is present on the sidewalls of the one or more preparatory kerf trenches during singulation of the semiconductor wafer.In one embodiment of the method, which may be combined with others, the step of preparing for die singulation comprises forming a single preparatory kerf trench between at least two of the die sites, and singulating comprises forming a cut in the semiconductor wafer between a bottom of the single preparatory kerf trench and the back surface.In one embodiment of the method, which may be combined with others, after forming the single preparatory kerf trench, one or more further trenches are formed in a bottom surface of the single preparatory kerf trench, the one or more further trenches being narrower than the single preparatory kerf trench, and the cut is formed at a position lying outside the one or more further trenches.In an embodiment of the method, which may be combined with others, after forming the single preparatory kerf trench, a further trench is formed in a bottom surface of the single preparatory kerf trench, and the cut is formed within the further trench.In one embodiment of the method, which may be combined with others, a splitter stop structure is formed immediately adjacent to a sidewall of one of the preparatory kerf trenches, and the splitter stop structure comprises a splitter stop trench extending from the main surface and separated from the back surface by semiconductor material, and a dielectric material filling the splitter stop trench.In one embodiment of the method, which may be combined with others, forming the one or more preparatory kerf trenches comprises forming two intersecting trenches of the preparatory kerf trenches with obtuse-angled transitions between side walls of the two intersecting trenches of the preparatory kerf trenches.In an embodiment of the method, which may be combined with others, forming the one or more preparatory kerf trenches comprises forming first and second preparatory kerf trenches between each of the die sites, an outer sidewall of the first preparatory trench and an outer sidewall of the second preparatory trench form the opposing sidewalls, and the opposing sidewalls are exposed semiconductor surfaces during singulation.In one embodiment of the method, which may be combined with others, the singulating comprises performing laser ablation on a top surface of the semiconductor wafer in central portions of the kerf regions located between the opposing sidewalls, performing the laser ablation causes recast material to form substantially along the opposing sidewalls, and the main surface of the semiconductor wafer in the die locations is substantially free of the recast material after performing the laser ablation.In one embodiment of the method, which can be combined with others, the semiconductor wafer comprises silicon carbide.In one embodiment of the method, which can be combined with others, before performing the laser ablation, the upper surface of the semiconductor wafer is lowered in the central regions so that it lies below the main surface of the semiconductor wafer.A method of forming a semiconductor device is disclosed. The method comprises providing a semiconductor wafer having a main surface and a back surface opposite the main surface, forming cell array trenches and preparatory kerf trenches in the main surface of the semiconductor wafer using a common etching step, the preparatory kerf trenches being formed in a grid pattern enclosing a plurality of die sites, the cell array trenches being formed within the die sites, singulating the plurality of die sites from the semiconductor wafer into a plurality of separate semiconductor dies, the singulating comprising forming a cut between bottom surfaces of the preparatory kerf trenches and the back surface.In one embodiment of the method, which may be combined with others, after performing the common etching step, a dielectric layer is formed along sidewalls of the cell array trenches and the preparatory kerf trenches by means of a common deposition step, and the dielectric layer is present on the sidewalls of the preparatory kerf trenches during the singulation of the semiconductor wafer.In one embodiment of the method, which may be combined with others, the preparatory kerf trenches are formed to be wider and deeper than the cell field trenches.A method of forming a semiconductor device is disclosed, and the method includes providing a silicon carbide-containing wafer having a major surface and a back surface opposite the major surface, forming a grid pattern of preparatory kerf trenches in the major surface of the silicon carbide-containing wafer, the grid pattern enclosing a plurality of die sites, performing laser ablation on a top surface of the silicon carbide-containing wafer that lies between opposing sidewalls of the preparatory kerf trenches, wherein performing the laser ablation causes recast material to form substantially along the opposing sidewalls, and wherein the major surface of the semiconductor wafer in the die sites is substantially free of recast material after performing the laser ablation.In one embodiment of the method, which may be combined with others, the laser ablation singulates the semiconductor wafer, thereby forming a plurality of separate semiconductor dies from the die sites, and one of the opposing sidewalls forms an outer chip edge side for each of the separate semiconductor dies.In one embodiment of the method, which may be combined with others, forming the grid pattern of preparatory kerf trenches comprises forming first and second preparatory kerf trenches between each of the die sites, wherein the first and second preparatory kerf trenches are separated from each other by a central kerf region of the semiconductor wafer extending to the main surface, and the method further comprises removing semiconductor material from the central kerf region so as to depress a top surface of the silicon carbide-containing wafer between the first and second preparatory kerf trenches, and wherein the laser ablation is performed on the depressed surface.The term "substantial" includes absolute conformity to a requirement as well as minor deviation from absolute conformity to the requirement due to variations in the manufacturing process, assembly, and other factors that may cause deviation from a desired parameter. Provided that the deviation is within process tolerances to achieve practical conformity and the components described herein are capable of performing in accordance with the application requirements, the term "substantial" includes any such deviation.Spatially relative terms such as "under," "beneath," "lower," "above," "upper," and the like are used for ease of description to explain the positioning of one element with respect to a second element. These terms are intended to encompass various orientations of the assembly in addition to different orientations from those shown in the figures. Furthermore, terms such as "first," "second," and the like are also used to describe various elements, regions, sections, etc. and are also not intended to be limiting. Like terms refer to like elements throughout the description.As used herein, the terms "having," "containing," "comprising," "having," and the like are open-ended terms that indicate the presence of the stated elements or characteristics, but do not exclude the presence of additional elements or characteristics. The indefinite articles and the definite articles are intended to include both the plural and the singular, unless the context clearly indicates otherwise.In view of the above range of variations and applications, it should be understood that the present invention is not limited by the foregoing description, nor is it limited by the accompanying drawings. Instead, the present invention is limited only by the following claims and their legal equivalents.

Claims

A method of forming a semiconductor device, the method comprising: providing a semiconductor wafer (100) having a main surface (102) and a rear surface (104) opposite the main surface (102); performing a step of preparing for die singulation in kerf regions (108) of the semiconductor wafer (100), the kerf regions (108) enclosing a plurality of the die sites (106), the step of preparing for die singulation comprising forming one or more preparatory kerf trenches (112) between at least two immediately adjacent die sites (106) in the plurality; forming active semiconductor devices in the die sites (106); and dicing the semiconductor wafer (100) in the kerf regions (108), thereby forming a plurality of separate semiconductor dies (110) from the die locations (106), wherein the one or more kerf trenches (112) are not filled during dicing, and wherein dicing comprises removing semiconductor material from a surface of the semiconductor wafer (100) that lies between opposing sidewalls of the one or more preparatory kerf trenches (112), and wherein forming the active semiconductor devices comprises forming a trenched electrode structure (118) in cell array trenches (122) in the die locations (106), and wherein the cell array trenches (122) and the one or more preparatory kerf trenches (112) are formed simultaneously using a common etching step.The method of claim 1, wherein one of the opposing sidewalls forms an outer chip edge side for each of the separate semiconductor dies (110).A method according to any preceding claim, wherein the one or more preparatory kerf trenches (112) are formed to be deeper than the cell array trenches (122).The method of any preceding claim, further comprising, after performing the common etching step, forming a dielectric layer (126) along sidewalls of the cell array trenches (122) and the one or more preparatory kerf trenches (112) by means of a common deposition step, and wherein the dielectric layer (126) is present on the sidewalls of the one or more preparatory kerf trenches (112) during the singulation of the semiconductor wafer (100).The method of claim 1, wherein the step of preparing for die singulation comprises forming a single preparatory kerf trench between two immediately adjacent die locations (106), and wherein singulation comprises forming a cut in the semiconductor wafer (100) between a bottom (138) of the single preparatory kerf trench (112) and the back surface (104).The method of claim 5, further comprising, after forming the single preparatory kerf trench (112), forming one or more additional trenches (140) in a bottom surface of the single preparatory kerf trench (112), wherein the one or more additional trenches (140) are narrower than the single preparatory kerf trench (112), and wherein the cut is formed at a position external to the one or more additional trenches (140).The method of claim 5, further comprising, after forming the single preparatory kerf trench (112), forming another trench (140) in a bottom surface (138) of the single preparatory kerf trench (112), and wherein the cut is formed within the another trench (140).The method of any preceding claim, further comprising forming a chip stop structure (144) immediately adjacent to a sidewall of one of the preparatory kerf trenches (112), and wherein the chip stop structure (144) comprises: a chip stop trench (146) extending from the main surface (102) and separated from the back surface (104) by semiconductor material; and a dielectric material filling the chip stop trench (146).A method according to any preceding claim, wherein forming the one or more preparatory kerf trenches (112) comprises forming two intersecting trenches of the preparatory kerf trenches (112) with obtuse-angled transitions between sidewalls of the two intersecting trenches of the preparatory kerf trenches (112).The method of any preceding claim, wherein forming the one or more preparatory kerf trenches (112) comprises forming first and second preparatory kerf trenches (112) between two immediately adjacent die locations (106), wherein an outer sidewall of the first preparatory trench and an outer sidewall of the second preparatory trench form the opposing sidewalls, and wherein the opposing sidewalls are semiconductor surfaces exposed during singulation.The method of claim 10, wherein singulating comprises performing laser ablation on a top surface of the semiconductor wafer (100) in central portions of the kerf regions (108) located between the opposing sidewalls, wherein performing the laser ablation causes recast material to form substantially along the opposing sidewalls, and wherein the major surface (102) of the semiconductor wafer (100) in the die locations (106) is substantially free of the recast material after performing the laser ablation.Method according to one of the preceding claims, wherein the semiconductor wafer (100) comprises silicon carbide.The method of claim 11, further comprising, prior to performing the laser ablation, lowering the upper surface of the semiconductor wafer (100) in the central regions so that it lies below the main surface (102) of the semiconductor wafer (100).A method of forming a semiconductor device, the method comprising: providing a semiconductor wafer (100) having a main surface (102) and a rear surface (104) opposite the main surface (102); forming cell array trenches (122) and preparatory kerf trenches (112) in the main surface (102) of the semiconductor wafer (100) by means of a common etching step, the preparatory kerf trenches (112) being formed in a grid pattern enclosing a plurality of die sites (106), the cell array trenches (122) being formed within the die sites (106); dicing the plurality of die locations (106) from the semiconductor wafer (100) into a plurality of separate semiconductor dies (110), wherein dicing comprises forming a cut between bottom surfaces (138) of the preparatory kerf trenches (112) and the back surface (104).The method of claim 14, further comprising, after performing the common etching step, forming a dielectric layer (126) along sidewalls of the cell array trenches (122) and the preparatory kerf trenches (112) by means of a common deposition step, and wherein the dielectric layer (126) is present on the sidewalls of the preparatory kerf trenches (112) during the singulation of the semiconductor wafer (100).The method of claim 14, wherein the preparatory kerf trenches (112) are formed to be deeper than the cell array trenches (122).A method of forming a semiconductor device, the method comprising: providing a silicon carbide-containing wafer having a major surface (102) and a rear surface (104) opposite the major surface (102); forming a grid pattern of preparatory kerf trenches (112) in the major surface (102) of the silicon carbide-containing wafer, the grid pattern enclosing a plurality of die sites (106); and performing laser ablation on a top surface of the silicon carbide-containing wafer lying between opposing sidewalls of the preparatory kerf trenches (112), wherein performing the laser ablation causes recast material to form substantially along the opposing sidewalls, and wherein the major surface (102) of the semiconductor wafer (100) in the die sites (106) is substantially free of recast material after performing the laser ablation.The method of claim 17, wherein the laser ablation singulates the semiconductor wafer (100), thereby forming a plurality of separate semiconductor dies (110) from the die locations (106), and wherein one of the opposing sidewalls forms an outer chip edge side for each of the separate semiconductor dies (110).The method of claim 17, wherein forming the grid pattern of preparatory kerf trenches (112) comprises forming first and second preparatory kerf trenches (112) between each of the die sites, the first and second preparatory kerf trenches (112) being separated from each other by a central kerf region of the semiconductor wafer (100) extending to the main surface (102), the method further comprising removing semiconductor material from the central kerf region so as to depress a top surface of the silicon carbide-containing wafer between the first and second trenches of the preparatory kerf trenches (112), and wherein the laser ablation is performed on the depressed surface.

Citation Information

Patent Citations

  • Separating semiconducting devices from semiconducting wafer involves etching separating trenches in first surface, reducing wafer from second main surface until reduced second surface reaches trenches, semiconducting devices are separated

    DE102006037789A1

  • Chip dicing

    US20060292830A1

  • Wafer dividing method

    US20170140989A1