MICROELECTRO-MECHANICAL SYSTEM AND METHOD FOR ITS MANUFACTURING
The integration of a bonding layer and conductive structures between circuit and carrier substrates enhances the structural integrity and electrical connectivity of MEMS devices, addressing manufacturing challenges and enabling precise beam control.
Patent Information
- Application Number
- DE102020125201
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-28
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2040-09-28
AI Technical Summary
Existing methods for manufacturing microelectromechanical system (MEMS) devices are not fully satisfactory in all respects, particularly in terms of structural integrity and efficient integration of electronic circuits with mechanical features.
A method involving the use of a bonding layer, such as silicon oxide, to integrate a circuit substrate with a carrier substrate, along with conductive layers and through-substrate vias, allowing for the formation of MEMS devices with enhanced structural integrity and electrical connectivity.
The method enables the production of MEMS devices with improved structural integrity and efficient electrical connectivity, facilitating the deflection of electron beams or light beams, and enabling precise control over beam direction for applications like electron beam lithography.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
STATE OF THE ART
[0001] Microelectromechanical system (MEMS) devices have recently been developed. MEMS- Devices include devices manufactured using semiconductor technology to mechanical and electrical features. MEMS devices are used in pressure sensors, microphones, actuators, mirrors, heating elements and / or printer nozzles. Although existing devices and methods for Forming the MEMS devices has generally been adequate for their intended purposes, they are not in been completely satisfactory in all respects.
[0002] WO 2015 / 164 266 A1 discloses an electronic package comprising an adhesive layer between a first substrate and a second substrate. The adhesive layer is structured to define openings that can be connected to through-substrate Connections and corresponding bond pads are aligned. Between the first substrate and the second substrate A conductive layer is formed adjacent to the adhesive layer.
[0003] JP 2006- 332 256 A deals with the problem of how to form a structure without a projection on the printed circuit board surface As a solution, a method for producing a printed circuit board is proposed, which is provided with a front surface formed wiring pad, a through hole and a shielding electrode consisting of a first metal film and a second metal film which are electrically grounded on at least one side.
[0004] JP 2018- 137 358 A discloses a lithography method capable of reducing the influence of faulty beams in the Multi-beam lithography regardless of the faulty beams that occur during lithography The method comprises the steps of: forming a plurality of beams by allowing a portion of charged Particle beams pass through each of a plurality of openings of a shaped aperture array substrate that supports the plurality of openings formed therein; and drawing a plurality of small areas using the plurality of Rays so that small areas adjacent to each other in the several small areas formed by dividing a lithography area of a sample, with each small area having a minimum irradiation unit area per Beam is multiple beams, not irradiated with beams passing through the same opening of the plurality of openings go.
[0005] US 2020 / 0 317 504 A1 discloses an imaging element comprising a semiconductor chip with microelectromechanical system (MEMS) devices and voltage generators, each voltage generator configured to generate a voltage used by one or more of the MEMS devices. A floating mass can be used to add a voltage to that generated by the voltage generators. to add tension.
[0006] US 2013 / 0 168 740 A1 discloses a compact MEMS motion sensor device comprising a CMOS Substrate layer comprising a plurality of anchor posts having an insulating oxide layer containing a conductive layer On one side of the CMOS substrate layer, the device includes a field oxide layer (FOX), a first set and a second set of implanted doped silicon regions, a first polysilicon layer, an oxide layer coated with embedded in several metal layers that are nested with a through-hole layers, a Nitride deposition layer, an under-bump metal (UBM) layer, and a multitude of solder balls. On the other side the CMOS substrate layer, the disclosure further comprises a backside interconnect isolation oxide layer, a first MEMS bonding layer, a first metal interconnect layer, a second MEMS bonding layer, a MEMS layer, a first eutectic MEMS bonding layer, a second metal interconnect layer, a second eutectic MEMS bonding layer and a MEMS cover layer.
[0007] The invention is defined in the claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] The present disclosure can best be understood from the following detailed description in conjunction with with the accompanying drawings. Please note that according to industry practice, various Features are not shown to scale. In fact, the dimensions of the various features may be arbitrarily enlarged or reduced in size for the sake of clarity. Fig. 1A, Fig. 1B, Fig. 1C and Fig. 1D show schematic cross-sectional views of MEMS devices according to Embodiments of the present disclosure. Fig. 2A, Fig. 2B, Fig. 2C, Fig. 2D, Fig. 2E and Fig. 2F show schematic cross-sectional views of the different phases of a manufacturing operation for a MEMS device according to an embodiment of the this disclosure. Fig. 3A, Fig. 3B, Fig. 3C, Fig. 3D and Fig. 3E show schematic cross-sectional views of the different Phases of a manufacturing operation for a MEMS device according to an embodiment of the present disclosure. Fig. 4A, Fig. 4B, Fig. 4C and Fig. 4D show schematic cross-sectional views of the different phases a manufacturing operation for a MEMS device according to an embodiment of the present Revelation. Fig. 5A, Fig. 5B and Fig. 5C show schematic cross-sectional views of the different phases of a Manufacturing operation for a MEMS device according to an embodiment of the present disclosure. Fig. 6A, Fig. 6B and Fig. 6C show schematic cross-sectional views of the different phases of a Manufacturing operation for a MEMS device according to an embodiment of the present disclosure. Fig. 7A shows a top view of the MEMS device and Fig. 7B shows a cross-sectional view of a pad Structural component according to an embodiment of the present disclosure. Fig. 8 shows a use of the MEMS device according to an embodiment of the present disclosure. Fig. 9A, Fig. 9B, Fig. 9C and Fig. 9D show schematic cross-sectional views of the different phases a manufacturing operation for a MEMS device according to an embodiment of the present Revelation. DETAILED DESCRIPTION
[0009] The MEMS device according to the present disclosure may be any of a electron beam deflector, an electromagnetic beam deflector, an accelerometer, a gyroscope, a pressure sensor, a microphone, an RF resonator, an RF switch or an ultrasonic transducer.
[0010] Fig. 1A and Fig. 1B show schematic cross-sectional views of MEMS devices 10A and 10B according to Embodiments of the present disclosure.
[0011] In some embodiments, the MEMS devices 10A and 10B include a circuit substrate 20 in which an electronic circuit 25 (e.g. transistors comprising semiconductor field effect transistors, such as complementary metal oxide semiconductor devices (CMOS devices)), and a carrier substrate 30 having an opening (cavity or recess) 35 for receiving sound, pressure and / or light. In some Embodiments, a bonding layer 40 is formed between the circuit substrate 20 and the carrier substrate 30. In In some embodiments, the bonding layer 40 is a silicon oxide layer. In some embodiments, the Circuit substrate electronic circuits 25, such as a signal processing circuit and / or a Amplifier circuit formed by electronic circuits. In some embodiments, the recess 35 a rectangular (e.g. square) shape in plan view. In some embodiments, at least one of the Circuit substrate 20 and carrier substrate 30 are made of crystalline silicon. In some Embodiments, as shown in Fig. 1A, the bonding layer remains at the bottom of the recess 35 and in other In embodiments as shown in Fig. 1B, the bonding layer is not present at the bottom of the recess 35.
[0012] Furthermore, in some embodiments, a first conductive layer 50 is provided on a front surface of the circuit substrate 20 and a second conductive layer 55 is formed on a back surface of the carrier substrate 30, as shown in Fig. 1A and Fig. 1B. In some embodiments, as shown in Fig. 1A, the bonding layer 40 in contact with the second conductive layer 55, and the second conductive layer 55 is not in contact with the Circuit substrate 20. In other embodiments, the second conductive layer 55 is in contact with the Circuit substrate 20, as shown in Fig. 1B. In some embodiments, the first and second conductive Layer one or more layers of AU, Ti, Cu, Ag and Ni.
[0013] In some embodiments, the distance L1 is the size of the recess 35 at the bottom of the Circuit substrate 20 in a range of about 10 mm to about 50 mm and in other embodiments is in a Range from about 15 mm to about 20 mm. In some embodiments, the distance L2 is the size of the cavity 35 at the bottom of the carrier substrate 30 is greater than L1 and is in a range of about 11 mm to about 52 mm and is in other embodiments in a range of about 16 mm to about 22 mm. In some embodiments, the Distance L3 from the edge of the MEMS device and the edge of the recess 35 at the bottom of the circuit substrate 20 (a width of a frame section) in a range of about 2 µm to about 10 µm and is in other Embodiments in a range of about 3 µm to about 5 µm. In some embodiments, the thickness T1 of the Bonding layer 40 in a range of about 200 nm to about 5 µm and in other embodiments is in a range from about 500 nm to about 2 µm. In some embodiments, the total thickness T2 of the MEMS device is in a Range from about 300 µm to about 2 mm and in other embodiments in a range of about 600 µm to about 800 µm.
[0014] Fig. 1C and Fig. 1D show schematic cross-sectional views of MEMS devices 10C and 10D according to Embodiments of the present disclosure. In some embodiments, the MEMS devices 10C and 10D a beam deflector through which one or more electron or extreme ultraviolet light beams (EUV rays) deflected by an operation of an electronic circuit embedded in the MEMS device.
[0015] Similar to the MEMS devices 10A and 10B, the MEMS devices 10C and 10D have a circuit substrate 20 in which an electronic circuit 25 is formed, and a carrier substrate 30 having an opening (cavity or recess) 35 for receiving sound, pressure and / or light. In some embodiments, a Bond layer 40 is formed between the circuit substrate 20 and the carrier substrate 30. In some embodiments the bonding layer 40 is a silicon oxide layer. In some embodiments, one or more through holes 60 arranged which pass through the circuit substrate 20 and the bonding layer 40, so that rays pass through the Through holes 60. In some embodiments, the through holes 60 are arranged in an n×m matrix in a Arranged in plan view, where n and m are integers of 2 or more and equal to or less than, for example, 128.
[0016] In some embodiments, a first conductive layer 50 is disposed on a front surface of the circuit substrate 20 and a second conductive layer 55 is formed on a back surface of the carrier substrate 30, as shown in Fig. 1C and Fig. 1D. In some embodiments, as shown in Fig. 1C, the Bonding layer 40 in contact with the second conductive layer 55, and the second conductive layer 55 is not in contact with the circuit substrate 20. In other embodiments, the second conductive layer 55 is in contact with the circuit substrate 20, as shown in Fig. 1D. Further, a third conductive layer 57 is formed on an inner wall of each of the Through holes 60 are arranged which connect the first conductive layer 50 and the second conductive layer 55.
[0017] In some embodiments, the circuit substrate 20 comprises electronic circuits 25, such as a Signal processing circuit and / or an amplifier circuit formed by electronic circuits. In In some embodiments, the electronic circuits are connected to the first, second and / or third conductive layer to control the potential of the third conductive layer in each of the through holes 60, thereby the rays passing through the through hole 60 are deflected.
[0018] In some embodiments, the recess 35 has a rectangular (e.g. square) shape in plan view. In some embodiments, at least one of the circuit substrate 20 and the carrier substrate 30 is made of crystalline silicon. In some embodiments, as shown in Fig. 1C, the bonding layer remains on the Bottom of the recess 35 and in other embodiments, as shown in Fig. 1D, the bonding layer is not present at the Bottom of depression 35.
[0019] The dimensions of L1, L2 and L3 of the MEMS devices 10C and 10D are the same or similar to those for the MEMS devices 10A and 10B.
[0020] Fig. 2A, Fig. 2B, Fig. 2C, Fig. 2D, Fig. 2E and Fig. 2F show schematic cross-sectional views of the different phases of a manufacturing operation for a MEMS device according to an embodiment of the present disclosure. It is understood that additional operations before, during, and after are illustrated by Figs. 2A-2F shown processes and some of the operations described below for additional Embodiments of the method may be replaced or eliminated. The order of operations / processes may be interchangeable. Materials, configurations, dimensions and processes described with reference to Fig. 1A-1D, can be applied to the following embodiments and a detailed description thereof can be left out.
[0021] As shown in Fig. 2A, a CMOS (complementary metal oxide semiconductor) circuit 25 is incorporated in a front surface area of the circuit substrate 20. One or more passivation films 28 are formed over the front surface of the circuit substrate. In some embodiments, the one or more Passivation films 28 silicon oxide, silicon nitride or an organic film. Then, as shown in Fig. 2B, the The back side of the circuit substrate 20 is thinned by a grinding or polishing process. The remaining thickness of the thinned circuit substrate 20 is in some embodiments in a range of about 100 µm to about 500 µm.
[0022] Next, as shown in Fig. 2C and Fig. 2D, the thinned circuit substrate 20 is Bond layer 40 is bonded to a carrier substrate 30. In some embodiments, as shown in Fig. 2C, the Bonding layer 40 silicon oxide, which is deposited on the surface of the carrier substrate 30 by for example, a thermal oxidation process or a chemical vapor deposition (CVD) process In other embodiments, the bonding layer 40 is formed by, for example, a CVD process on the back of the circuit substrate 20.
[0023] Then, the back side of the carrier substrate 30 is formed using one or more lithography and etching processes In some embodiments, the etching operation comprises plasma dry etching or wet etching. In some In some embodiments, wet etching uses a tetramethylammonium hydroxide (TMAH) or KOH solution.
[0024] In some embodiments, the bonding layer 40 functions as an etch stop layer for forming the recess 35, as shown in Fig. 2E. In some embodiments, one or more conductive layers are applied to the back of the carrier substrate 30 and on the bonding layer 40.
[0025] In other embodiments, after the recess etching stops at the bonding layer 40, the bonding layer 40 is further etched by one or more dry etching or wet etching operations. In some embodiments, a or more conductive layers are formed on the back of the carrier substrate 30. In other embodiments, as in As shown in Fig. 2F, after the bonding layer 40 is removed, a part of the back of the circuit substrate 20 is etched and then one or more conductive layers are formed.
[0026] Fig. 3A-7B show schematic cross-sectional views of the different phases of a manufacturing operation for a MEMS device according to an embodiment of the present disclosure. It is clear that additional Operations before, during and after the processes shown by Fig. 3A-7B can be provided and some the operations described below are replaced or eliminated for additional embodiments of the method. The sequence of operations / processes can be interchangeable. Materials, configurations, dimensions and the The process described with reference to Figs. 1A-1D and 2A-2F can be applied to the following embodiments and a detailed description thereof may be omitted.
[0027] As shown in Fig. 3A, after the electronic circuit is formed over a circuit substrate 20, one or more planar electrodes 100 are formed and one or more passivation layers 110 are formed. The Electrode 100 is electrically connected to the electronic circuit formed in the circuit substrate 20. In In some embodiments, the circuit substrate 20 comprises a crystalline silicon substrate. In some Embodiments are one or more openings above the electrode 100 in the one or more passivation layers. In some embodiments, the electrodes 100 are made of one or more Layers of Cu, Al, Au, Ni, Ag or another suitable conductive material are manufactured. The passivation layers 110 contain silicon nitride, SiON, silicon oxide, aluminum nitride or an organic material.
[0028] Then, one or more holes 120 for silicon vias (TSVs) are formed in areas other than the Electrodes 100 are formed. The TSV holes 120 are formed by one or more lithography and etching operations. In In some embodiments, the TSV holes 120 are arranged in an n×m matrix in a plan view (see Fig. 7A), where n and m are integers of 2 or more and equal to or less than, for example, 128. The depth of the TSVs is in some embodiments in a range of about 20 µm to about 100 µm from the top of the passivation layer 110. In some embodiments, the depth is determined such that after a subsequent thinning process of the back of the circuit substrate exposed the bottoms of the TSV holes 120 In some embodiments, the shape of the TSV holes 120 in plan view is circular or rectangular (e.g. square). In some embodiments, a diameter (or a length of sides) of the TSV holes 120 at the Aperture in a range from about 100 nm to about 12,000 nm.
[0029] Then, a first conductive layer 130 is deposited over the electrodes 100, the passivation layer 110 and within the TSV holes 120 are formed. Then, a filling layer 140 is formed to fill the TSV holes 120 as shown in Fig. 3B The first conductive layer 130 has the same or similar functionality as that shown in Fig. 1A-1D shown first conductive layer 50. In some embodiments, the first conductive layer 130 comprises one or several layers of Au, Ti, Cu, Ag and Ni. In certain embodiments, a layer formed over a Ti layer Gold layer is used as the first conductive layer 130. In some embodiments, the thickness of the Ti layer is a range of about 50 nm to about 500 nm and in other embodiments is in a range of about 80 nm to about 300 nm. In some embodiments, the thickness of the gold layer (Au layer) is in a range of about 10 nm to about 10,000 nm and in other embodiments is in a range of about 150 nm to about 250 nm. In In some embodiments, the fill layer 140 includes silicon oxide or any other suitable insulating material. In some embodiments, a cover layer of a filler material is disposed over the first conductive layer 130 formed and then a planarization operation, such as a chemical-mechanical polishing process or a Etch-back process, performed to leave the fill material only within the TSV holes 120, as shown in Fig. 3B. In In other embodiments, the filling material also remains at a concave portion above the electrodes 100.
[0030] Next, as shown in Fig. 3C, the conductive layer 130 is patterned to form one or more openings over the passivation layer 110 near the TSV hole 120 to partially expose the passivation layer. Then, an insulating layer is formed and patterned to form island-shaped insulating structures 150 to cover the openings In some embodiments, the insulating structures 150 include silicon nitride.
[0031] Further, as shown in Fig. 3D, a first carrier bonding layer 160 is deposited over the front surface of the Circuit substrate 20 is formed on which the conductive layer 130 and the structures 150 are formed, and then a first carrier substrate 165. The first carrier substrate 165 is, in some embodiments, a glass substrate, a ceramic substrate, a semiconductor substrate, or a resin substrate. In some embodiments, the first Carrier bonding layer 160 is an organic material, silicon oxide, or any other suitable material.
[0032] Then, the back side of the circuit substrate 20 is subjected to a grinding or polishing operation (e.g., CMP operation) In some embodiments, the circuit substrate 20 after thinning has a residual thickness in a range of about 20 µm to about 300 µm and the remaining thickness in other embodiments is in a Range from about 40 µm to about 180 µm. As shown in Fig. 3D, the bottom of the filler layer 140, which is incorporated into the TSV Hole 120 is filled. In other embodiments, after the thinning operation, the first Carrier substrate 165 attached to the front surface of the circuit substrate 20.
[0033] Further, as shown in Fig. 3E, a bonding layer 170 is deposited on the thinned back surface of the circuit substrate 20. The bonding layer 170 has the same or similar functionalities as those shown in Fig. 1A-2F shown bonding layer 40. In some embodiments, the bonding layer 170 contains, for example, a CVD Silicon oxide formed in the process.
[0034] Then, as shown in Fig. 4A, a carrier substrate 30 is prepared and bonded through the bonding layer 170 (oxide fusion bonding) to the circuit substrate 20. In some embodiments, the carrier substrate 30 made of crystalline silicon. After oxide fusion bonding, the first carrier substrate 165 and the first carrier bonding layer 160 is removed, as shown in Fig. 4B. As shown in Fig. 4A, the bonding layer 170 is Filler layer 140 in the TSV holes 120. In some embodiments, the bond layer 170 and the filling material 140 is made of the same material.
[0035] In other embodiments, the bonding layer 170 is on the carrier substrate 30 or on both the carrier substrate 30 and the circuit substrate 20. In some embodiments, the thickness of the Carrier substrate 30 without the bonding layer in a range of about 200 µm to about 1.8 mm and is in other Embodiments in a range of about 500 µm to about 750 µm.
[0036] Next, as shown in Fig. 4C, a first hard mask layer 180 is formed and then a second Hard mask layer 190 is formed over the front surface of the circuit substrate 20. In some embodiments the first hard mask layer 180 contains silicon oxide and the second hard mask layer 190 contains polysilicon or amorphous silicon. In some embodiments, the silicon oxide hard mask layer 180 is formed by a CVD process formed and then a planarization operation, such as a CMP operation, is performed. Similarly, in some Embodiments, the polysilicon hard mask layer 190 is formed by chemical vapor deposition (CVD) and then a CMP operation is optionally performed. In some embodiments, the thickness of the Polysilicon hard mask layer 190 in a range of about 30 µm to about 70 µm.
[0037] Then, using one or more lithography and etching operations, the second hard mask layer 190 and the first hard mask layer 180 are patterned to form one or more openings 200 above the electrode 100. as shown in Fig. 4D. In some embodiments, the size of the opening 200 is larger than the size of the Opening formed in the passivation layer 110 above the electrode 100. Furthermore, in some embodiments the insulating structure 150 is partially exposed in the opening 200, as shown in Fig. 4D.
[0038] Next, as shown in Fig. 5A, one or more conductive layers 210 (column electrodes) are deposited in the Openings 200 are formed. In some embodiments, the conductive layers contain gold or a gold alloy (e.g. AuCu and AuNi) formed by a plating operation (electroplating or electroless plating). In In some embodiments, the thickness of the plated conductive layer 210 is a range of about 20 µm to about 50 µm. In some embodiments, the thickness (height) of the plated conductive layer 210 is smaller than the top surface of the second hard mask layer 190, as shown in Fig. 5A.
[0039] Further, as shown in Fig. 5B, a portion of the plated layer 210 is deposited over one or more electrodes 100 covered by a mask structure 220. In some embodiments, the mask structure 220 has a photoresist structure. Then, an additional conductive layer 215 (column electrode) is deposited over the conductive plating layer 210. In some embodiments, the additional conductive layer 215 is formed by a plating operation (electroplating or electroless plating). In some embodiments, the additional conductive layer 215 made of the same material as the plated conductive layer 210 and contains Gold or a gold alloy (e.g., AuCu, AuNi). In other embodiments, the additional conductive layer 215 is made of a different material than the plated conductive layer 210. Then, the photoresist structure 220 is formed as shown in Fig. 5C shown removed.
[0040] In some embodiments, the thickness of the additional conductive layer 215 is in a range of about 10 µm to about 35 µm. In some embodiments, the total thickness (height) of the plated conductive layer 210 and the additional conductive layer 220 is smaller than the top surface of the second hard mask layer 190, as shown in Fig. 5C shown. In some embodiments, two different thicknesses (heights) of plated conductive layers 210 control / 220 different electrical circuits. For example, the higher one is used to protect electrons and the lower one is used to control an electric field.
[0041] Then, as shown in Fig. 6A, a second carrier bond layer 305 is deposited over the front side of the circuit substrate 20 and then a second carrier substrate 300 is attached to the front side of the circuit substrate 20 by means of the second Carrier bond layer 305 is attached. The second carrier substrate 300 is, in some embodiments, a glass substrate, a ceramic substrate, a semiconductor substrate, or a resin substrate. In some embodiments, the second Carrier bonding layer 305 is an organic material, silicon oxide, or any other suitable material.
[0042] Then, the entire substrate is turned vertically and then the back of the carrier substrate 30 is structured to to form a recess 35. In some embodiments, the recess 35 is formed by one or more lithography and etching operations using a mask structure 310. In some embodiments, the Mask structure 35 made of a photoresist.
[0043] In some embodiments, the etching operation comprises plasma dry etching or wet etching. In some Embodiments, the bonding layer 170 functions as an etch stop layer for forming the recesses 35. If a Plasma dry etching process is used to form the recess 35, the plasma etching essentially stops at the Bond layer 170 and plasma damage to the electronic circuit formed in the circuit substrate 20 can can therefore be prevented.
[0044] In some embodiments, after the recess etching stops at the bonding layer 170, the Bond layer 170 is further etched by one or more dry etching or wet etching operations. In some Embodiments, the etching of the bonding layer has a higher etch selectivity with respect to the circuit substrate 20 (e.g. B. Si). For example, the etching rate of the bonding layer is 10 times or more higher than the etching rate of the circuit substrate 20. In some embodiments, when the bonding layer 170 is made of silicon oxide, a wet etching process is performed Using RF or buffered RF to avoid damage to the electronic circuitry used in the circuit substrate 20. When the bonding layer 170 is removed, the filling material layer 140 is TSC holes 120 are also removed if the filler layer 140 is made of the same material as the bonding layer 170 (e.g. silicon oxide). If the filler layer 140 is made of a different material (e.g. silicon nitride) than the Bond layer 170 is produced, an additional etching operation, such as a wet etching operation, is performed to To remove filler layer 140.
[0045] After the filler layer 140 is removed from TSV holes 120, a second conductive layer 320 formed within the recess 35, as shown in Fig. 6B.
[0046] In some embodiments, as shown in Fig. 6B, the second conductive layer 320 is formed to contact with the first conductive layer 130 formed on the inner wall of each of the TSV holes 120. In some Embodiments, the second conductive layer 320 is also formed on the inner wall of the TSV holes 120 where the first conductive layer 130 is already formed. In some embodiments, the second conductive layer 320 is made of the same or a different material than the first conductive layer 130 and has one or more layers of Au, Ti, Cu, Ag and Ni. In certain embodiments, a gold layer formed over a Ti layer is used as the second conductive layer 320. In some embodiments, the thickness of the Ti layer is in a range of about 50 nm to about 200 nm and in other embodiments is in a range of about 80 nm to about 120 nm. In some Embodiments, the thickness of the gold layer (Au layer) is in a range of about 10 nm to about 400 nm and is in other embodiments in a range of about 150 nm to about 250 nm.
[0047] In some embodiments, a plurality of MEMS devices are formed on a Si wafer and the Wafers are cut into individual MEMS devices (chips) by sawing (a separation operation) at scribe lines 390. In some embodiments, the separation operation does not completely cut the second support bond layer 305, as shown in Fig. 6B. By removing the second carrier bonding layer 305 and thus the second carrier substrate 300 is removed, an individual MEMS device is released.
[0048] In some embodiments, the separation operation is performed after the second conductive layer 320 is formed. In such a case, no conductive layer is formed on side surfaces (separated surfaces) of the MEMS device In other embodiments, the separation operation is performed before the second conductive layer 320 In such a case, the second conductive layer 320 is also formed on the side surfaces of the MEMS device formed.
[0049] In some embodiments, after the second carrier substrate 300 and the second carrier bonding layer 305 removed, the individual MEMS device is mounted on a frame 400, as shown in Fig. 6C. As shown in Fig. 6C shown, by removing the second carrier substrate 300 and the second carrier bonding layer 305, the TSV Holes 120 are exposed so that an electron beam or a light beam can pass through.
[0050] Fig. 7A shows a top view of the MEMS device and Fig. 7B shows a cross-sectional view of a bonding pad Structure at the peripheral region PR. As shown in the top view of Fig. 7A, the MEMS device has a central region CR and a peripheral region PR surrounding the central region. The TSV holes 120 and the conductive layers 210 / 220 are arranged in the central region CR. In the peripheral region PR, one or more underbump pad electrodes 250 formed to connect the electronic circuit formed in the circuit substrate 20 with one or more circuits outside the MEMS device. In some embodiments, the perimeter area overlaps PR does not coincide with the recess 35 in plan view. In other embodiments, the peripheral area PR partially overlaps with the recess 35 in plan view.
[0051] The underbump pad electrodes 250 are formed on the front side of the circuit substrate 20. In some Embodiments, the underbump pad electrodes 250 are arranged in a matrix in the peripheral region PR. In In some embodiments, a ball bump 260 is disposed on each of the underbump pad electrodes 250. In some In some embodiments, the underbump pad electrodes 250 are formed prior to recess etching, as shown in Figure 6A. In some embodiments, the underbump pad electrodes 250 are formed after the carrier substrate 30 is attached to the circuit substrate 20 by means of oxide fusion bonding, as shown in Fig. 4A and Fig. 4B.
[0052] In some embodiments, the underbump pad electrode 250 is formed on a metal pad 225 that is in a Interlayer dielectric layer 230 is embedded and consists of the top metal layer (e.g. eighth to twelfth metal levels) of the electronic circuit. In some embodiments, the metal pad 225 has one or several layers of conductive material. In some embodiments, the metal pad contains 225 Cu or a Cu- Alloy.
[0053] Further, as shown in Fig. 7B, the underbump pad electrode 250 comprises several layers of conductive material In some embodiments, the underbump pad electrode 250 includes a first metal layer 252, a second metal layer 254, a third metal layer 256 and a fourth metal layer 258. In some embodiments, the first metal layer is a TiW layer, the second metal layer is a Cu layer, the third metal layer is a Ni- layer and the fourth metal layer is a Sn layer.
[0054] In some embodiments, the thickness of the TiW layer 252 is in a range of about 50 nm to about 1000 nm and in other embodiments in a range of about 100 nm to about 500 nm. In some embodiments, the thickness of the Cu layer 254 is in a range of about 10 nm to about 2000 nm and is in other Embodiments in a range of about 500 nm to about 1000 nm. In some embodiments, the thickness of the Ni layer 256 in a range of about 1000 nm to about 5000 nm and in other embodiments in a range from about 2500 nm to about 3500 nm. In some embodiments, the thickness of the Sn layer 258 is in a range of about 500 nm to about 4000 nm, and in other embodiments in a range of about 1500 nm to about 2500 nm. The metal layers are deposited by CVD, physical vapor deposition (PVD), comprising sputtering, plating or any other suitable film forming process, and one or more Lithography and etching operations.
[0055] In some embodiments, the surface of the electronic circuit is protected by one or more passivation layers. In some embodiments, the passivation layers have a first passivation layer 242, a second passivation layer 244 and a third passivation layer 246. The Underbump pad electrode 250 is formed in an opening formed in the passivation layers, as shown in Fig. 7B In some embodiments, the first passivation layer 242 is a SiC layer, the second Passivation layer 244 is a silicon oxide layer and the third passivation layer 246 is a silicon nitride layer.
[0056] Fig. 8 shows a use of the MEMS device according to an embodiment of the present disclosure. In some embodiments, the MEMS device 10 is for an electron or an electromagnetic Wave lithography is used. In some embodiments, electron beams (or EUV beams) 500 are used to MEMS device 10 from the front side of the circuit substrate 20. The in the circuit substrate 20 The electronic circuit formed independently controls the voltage applied to the conductive layer (e.g. the first conductive Layer 130) is applied, which is formed independently on the inner wall of each of the TSV holes 120. By the conductive layer in the TSV hole 120 is adjusted, a part of the electron beam 500 passes through one or more of the TSV holes and a part of the electron beam 500 does not pass through the TSV holes. The part of the Electron beam passing through the TSV holes is directed to a wafer or substrate on which a photoresist layer is formed. In some embodiments, the wafer is a semiconductor wafer. In some Embodiments are the substrate for a photomask, such as a transmissive substrate or a reflective substrate. By controlling the electronic circuit, the positions of the TSV holes 120 are controlled, through which the electron beam, and with it a desired shape can be drawn on the photoresist structure.
[0057] In other embodiments, a silicon-on-insulator (SOI) wafer is used. In such a case, a Fusion bonding process is omitted and the oxide layer of an SOI wafer acts as an etch stop layer in the Deep etching. Fig. 9A, Fig. 9B, Fig. 9C and Fig. 9D show schematic cross-sectional views of the different Phases of a manufacturing operation for a MEMS device according to an embodiment of the present Disclosure. It is clear that additional operations before, during and after the processes shown by Figs. 9A-9D may be provided and some of the operations described below may be applicable to additional embodiments of the procedure can be replaced or eliminated. The sequence of operations / processes can be interchangeable. In Materials, configurations, dimensions and processes described with reference to Fig. 1A-7B may be applied to the following embodiments are applied and a detailed description thereof may be omitted.
[0058] The SOI substrate has a device layer (semiconductor layer) 20', an oxide layer 40' and a bulk layer (semiconductor substrate) 30' as shown in Fig. 9A.
[0059] As shown in Fig. 9A, a CMOS circuit 25 is formed in a front surface region of the device layer 20' One or more passivation films 28 are formed over the front surface of the device layer 20'. In In some embodiments, the one or more passivation films 28 include silicon oxide, silicon nitride, or an organic film. In some embodiments, TSV holes 120 filled with a filler material 140 are formed, which pass through the component layer 20'. Furthermore, one or more first conductive layers 50 are provided on the front side the device layer and in the TSV holes as shown in Fig. 9A.
[0060] Then, as shown in Fig. 9B, the back side of the bulk layer 30' is recessed by one or more lithography and etching operations. In some embodiments, the etching operation includes plasma dry etching and Wet etching. In some embodiments, wet etching uses a tetramethylammonium hydroxide (TMAH) or KOH Solution.
[0061] In some embodiments, the oxide layer 40' functions as an etch stop layer for forming the recess 35, as shown in Fig. 9B.
[0062] After the recess etching stops at the oxide layer 40', the oxide layer 40' is further formed by one or several dry etching or wet etching operations. During the etching of the oxide layer 40', the filler material layer 140 also away from the TSV holes 120, as shown in Fig. 9C.
[0063] In some embodiments, one or more conductive layers 55 are disposed on the backside of the bulk layer 30' formed, as shown in Fig. 9D.
[0064] In the embodiments of the present disclosure, a MEMS device is formed by bonding a Circuit substrate and a carrier substrate by means of a silicon oxide bonding layer by oxide fusion bonding or formed using an SOI substrate. The oxide bonding layer (oxide layer) also acts as an etch stop layer for plasma dry etching when the carrier substrate is etched to form a recess and therefore protects electronic circuits formed in the circuit substrate from damage caused by plasma etching Since the silicon oxide bonding layer can be removed by wet etching operations, the removal process of the Silicon oxide bonding layer does not damage the electronic circuits formed in the circuit substrate.
Claims
1. Microelectromechanical system (MEMS), comprising: a circuit substrate (20) having electronic circuits (25); a carrier substrate (30) having a recess (35); a bonding layer (40) arranged between the circuit substrate (20) and the carrier substrate (30); through holes (60) passing through the circuit substrate (20) to the recess (35); a first conductive layer (50) disposed on a front side of the circuit substrate (20); a second conductive layer (55) arranged on an inner wall of the recess (35); and a third conductive layer (57) disposed on an inner wall of each of the through holes (60); wherein the circuit substrate has electrodes (100) having different configurations, wherein a) the electrodes (100) comprise first electrodes (100), on each of which a first column electrode is arranged and second electrodes (100), on each of which a second column electrode is arranged, and a height of the first column electrode differs from a height of the second column electrode; or wherein b) in plan view, the circuit substrate (20) has a central region in which the through holes (60) are provided, and a peripheral area surrounding the central area, and a plurality of bump electrodes (250) having a different configuration than the electrodes (100), in which circumferential area.
2. MEMS according to claim 1, wherein the bonding layer (40) contains silicon oxide.
3. MEMS according to claim 1 or 2, wherein no bonding layer (40) is arranged in the recess (35) and a bottom of the Circuit substrate (20) is in contact with the second conductive layer (55).
4. MEMS according to one of the preceding claims, wherein the height of the first column electrode differs from the height of the second column electrode and a height difference between the first column electrode and the second Column electrode is in a range of 10 µm to 30 µm.
5. MEMS according to one of the preceding claims, wherein in plan view the circuit substrate (20) has the central region, in in which the through holes (60) are provided, and the peripheral region surrounding the central region, and the The peripheral area does not overlap the recess (35) in plan view.
6. A method for producing a microelectromechanical system (MEMS), comprising: Forming electronic circuits over a front surface of a first substrate; forming one or more holes (120) penetrating the first substrate; Filling the holes (120) with a filling material (140); Thinning a backside of the first substrate to expose a portion of the filled holes; Bonding a second substrate (15) with a bonding layer (40) inserted therebetween to the back of the first substrate; Forming a recess (35) in the second substrate (15) so that a bottom of the first substrate is exposed; Forming a first conductive layer (50) over the front side of the first substrate and on an inner wall of each of the holes (120); and Forming a second conductive layer (55) over an inner wall of the recess (35).
7. The method of claim 6, wherein the bonding layer (40) is silicon oxide.
8. The method according to claim 6 or 7, wherein the bonding layer (40) is formed on the back side of the first substrate.
9. The method according to any one of claims 6 to 8, wherein the bonding layer (40) is formed on the second substrate (15).
10. Method according to one of claims 6 to 9, wherein the recess (35) is formed by: Etching a part of the second substrate (15) by plasma dry etching to expose the bonding layer (40) without first substrate to etch; and Etching the bonding layer (40) by an etching which Bond layer (40) is selectively removed from the first substrate.
11. The method according to claim 10, wherein during etching of the bonding layer (40) the filling material (140) is also removed from the holes (120) is removed, thereby forming through holes (60).
12. The method according to claim 10 or 11, wherein at least one of the first and second conductive layers (50, 55) has a stacked layer of an Au layer on a Ti layer.
13. The method according to any one of claims 6 to 12, wherein the holes (120) are arranged in a matrix in plan view.
14. A method for manufacturing a microelectromechanical system (MEMS), comprising: Forming electronic circuits over a front surface of a first substrate; Forming electrodes (100) over the first substrate; Forming one or more holes (120) formed in the first substrate in regions other than the formed electrodes penetrate; Filling the holes (120) with a filling material (140); Thinning a backside of the first substrate to expose a portion of the filled holes; Bonding a second substrate (15) to the back of the first substrate with a bonding layer inserted therebetween (40) made of silicon oxide; Forming column electrodes respectively above the electrodes (100); and Forming a recess (35) in the second substrate (15) so that a bottom of the first substrate is exposed; wherein the Recess (35) is formed by: Etching a part of the second substrate (15) by plasma dry etching to form the bonding layer (40) without etching the first substrate; and Etching the bond layer (40) by wet etching.
15. The method of claim 14, wherein the columns are formed by one or more plating operations.
Citation Information
Patent Citations
Semiconductor Device and Method
DE102020101520A1
Method of manufacturing wiring board
JP2006332256A
Multiple charged particle beam lithography method and multiple charged particle beam lithography system
JP2018137358A
Integrated compact MEMS device with deep trench contacts
US20130168740A1
MEMS image forming element with built-in voltage generator
US20200317504A1