Integrated circuit structure with backside dielectric layer with air gap and method for its manufacture

DE102021101178B4Active Publication Date: 2024-10-02TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102021101178
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-01-15
Filing Date
2021-01-21
Publication Date
2024-10-02
Estimated Expiration
2041-01-21

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

IC structure comprising: a gate structure (220); an epitaxial source structure (190S) and an epitaxial drain structure (190D) each on opposite sides of the gate structure (220); a front interconnect structure (250) on a front side of the epitaxial source structure (190S) and a front side of the epitaxial drain structure (190D); a back dielectric layer (270, 410) on a back side of the epitaxial source structure (190S) and a back side of the epitaxial drain structure (190D), wherein the back dielectric layer (270, 410) has an air gap (272, 412);and a rear via (292, 432) extending through the rear dielectric layer (270, 410) to a first of the epitaxial source structure (190S) and the epitaxial drain structure (190D), wherein the air gap (272, 412) has a width that decreases with increasing distance from the front interconnect structure (250), and wherein the air gap (272, 412) overlaps a second of the epitaxial source structure (190S) and the epitaxial drain structure (190D).
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUNDAs the semiconductor industry has moved into nanometer technology process nodes in its quest for higher device density, higher performance, and lower cost, challenges from both manufacturing and design issues have led to the development of three-dimensional designs, such as a multi-gate field-effect transistor (FET), including a fin-FET (FinFET) and a gate-all-around FET (GAA-FET). In a fin-FET, a gate electrode borders three side faces of a channel region, with a gate dielectric layer between them. Because the gate structure surrounds (wraps around) the fin on three faces, the transistor essentially has three gates that control current through the fin or channel region. Unfortunately, the fourth side, the bottom of the channel, is far from the gate electrode and thus is not under the direct control of the gate. In contrast, in a GAA-FET, all side surfaces of the channel region are surrounded by the gate electrode, allowing for more complete depletion in the channel region and resulting in less short-channel effects due to steeper subthreshold current swing (SS) and lower drain-induced barrier depression (DIBL).WO 2018 / 004 653 A1 discloses techniques for reducing the contact resistance on the back side for semiconductor devices with double-sided metallization. US 2020 / 0 035 560 A1 discloses integrated circuit cell architectures comprising both front and back side structures. US 2019 / 0 259 699 A1 discloses transistor cell architectures comprising both front and back side structures. US 2018 / 0 047 615 A1 discloses semiconductor devices with air gap spacers formed as part of BEOL or MOL layers of the semiconductor devices, as well as methods for producing such air gap spacers.SHORT DESCRIPTION OF THE DRAWINGSThe invention provides an IC structure according to claim 1, an IC structure according to claim 10 and a method according to claim 13. Particular embodiments are set out in the dependent claims. Aspects of the present invention are best understood from the following detailed description when read in conjunction with the accompanying figures. It should be noted that, in accordance with common practice in the industry, various features are not drawn to scale. Rather, the dimensions of the various features may be increased or decreased as desired for clarity of discussion. 1A-1C are a flow diagram illustrating a method of forming an integrated circuit structure in accordance with some embodiments. Fig. 2, Fig. 3, Fig. 4, Fig. 5A, Fig. 6A, Fig. 7A and Fig. 8A are perspective views of some embodiments of an integrated circuit structure at intermediate stages of the process of Figs. 1A-1C. Figs. 5B, 6B, 7B, 8B, 9-13, 14A, 15-25 are cross-sectional views of some embodiments of the integrated circuit structure at intermediate stages of the process of Figs. 1A-1C along a first section.14B is a cross-sectional view of some embodiments of the integrated circuit structure at intermediate stages of the process of FIGS. 1A-1C along a second section. 26-33 are cross-sectional views of various stages for fabricating an integrated circuit structure in accordance with some other embodiments of the present disclosure.DETAILED DESCRIPTIONThe following disclosure provides many different embodiments or examples for implementing various features of the invention. Specific examples of components and arrangements are described below to simplify the present disclosure. For example, forming a first feature over or on a second feature in the following description may include embodiments where the first and second features are formed in direct contact, and may also include embodiments where additional features may be formed between the first and second features such that the first and second features are not necessarily in direct contact. Moreover, the present disclosure may repeat reference numbers and / or letters in the various examples. This repetition is for the purpose of simplicity and clarity and does not automatically create a relationship between the various embodiments and / or configurations discussed.Furthermore, spatially relative terms such as "below," "under," "lower," "above," "upper," and the like may be used herein for convenience of description to describe the relationship of an element or feature to one or more other elements or features as illustrated in the figures. The spatially relative terms are intended to encompass other orientations of the device in use or operation besides the orientation shown in the figures. The device may also be oriented differently (rotated 90 degrees, or other orientations), and the spatially relative descriptors used herein may be similarly interpreted accordingly. For the purposes of this text, "approximately," "about," "approximately," or "substantially" generally mean within 20 percent, within 10 percent, or within 5 percent of a given value or range. The numerical quantities provided in this text are approximate, meaning that the term "approximately," "about," "approximately," or "substantially" can be inferred unless explicitly stated.The present disclosure generally relates to integrated circuit structures and methods of forming them, and more particularly relates to the fabrication of gate-all-around (GAA) transistors having backside vias beneath source regions and / or drain regions of the GAA transistors. It should also be noted that the present disclosure presents embodiments in the form of multi-gate transistors. Multi-gate transistors include those transistors whose gate structures are formed on at least two sides of a channel region. These multi-gate devices may include a p-type metal-oxide-semiconductor device or an n-type metal-oxide-semiconductor device. Specific examples may be presented herein and referred to as a FINFET due to their fin-like structure. Additionally, the present disclosure presents embodiments of a type of multi-gate transistor referred to as a gate-all-around (GAA) device. A GAA device includes any device whose gate structure (or a portion thereof) is formed on 4 sides of a channel region (e.g., around a portion of a channel region). The devices presented herein also include embodiments having channel regions arranged in one or more nanolayer channels, nanowire channels, and / or other suitable channel configurations. Embodiments of devices are presented herein that may have one or more channel regions (e.g., nanolayers) associated with a single, contiguous gate structure. However, one of ordinary skill in the art will recognize that the teachings may also be applied to a single channel (e.g., a single nanolayer) or any number of channels. One of ordinary skill in the art may recognize other examples of semiconductor devices that may benefit from aspects of the present disclosure.As the fin width in fin field effect transistors (FinFETs) is scaled down, variations in channel width could lead to mobility losses. GAA transistors, such as nanolayer transistors, are currently being investigated as an alternative to fin field effect transistors. In a nanolayer transistor, the gate of the transistor is placed completely around the channel (for example, a nanolayer channel or a nanowire channel) such that the channel is surrounded or encapsulated by the gate. Such a transistor has the advantage that the electrostatic control of the channel by the gate is improved, which also reduces leakage currents.In order to provide more routing space for an integrated circuit (IC) with a large number of GAA transistors, backside power rails connected to the backside of the source regions of the GAA transistors using backside metal vias are currently being investigated as an alternative to frontside power rails formed on the frontside of the source regions of the transistors. However, due to the shortened distances between the backside metal vias, the resistance capacitance (RC) time delay could increase, thereby degrading the device performance of GAA transistors. Therefore, in some embodiments of the present disclosure, a backside interlayer dielectric (ILD) layer with one or more air gaps is formed around the backside metal vias. An advantageous feature of the presence of the air gaps is that air in the air gap has a relative permittivity (or dielectric constant) of approximately 1. Such a low dielectric constant helps to reduce the capacitive coupling between adjacent back vias. Such reduced capacitive coupling can help to improve the reliability characteristics.1A-1C, a method M1 of semiconductor fabrication is illustrated that includes fabricating an integrated circuit structure having multi-gate devices. As used herein, the term “multi-gate device” is used to describe a device (e.g., a semiconductor transistor) in which at least a portion of the gate material is disposed on multiple sides of at least one channel of the device. In some examples, the multi-gate device may be referred to as a GAA device or a nanolayer device in which gate material is disposed on at least four sides of at least one channel of the device. The channel region may be referred to as a “nanowire,” which as used herein includes channel regions of various geometries (e.g., cylindrical, rod-shaped) and various dimensions.2, 3, 4, 5A, 6A, 7A and 8A are perspective views of some embodiments of an integrated circuit structure 100 at intermediate stages of the process M1 of FIGS. 1A-1C. FIGS. 5B, 6B, 7B, 8B, 9-13, 14A, 15-25 are cross-sectional views of some embodiments of the integrated circuit structure 100 at intermediate stages of the process M1 along a first section (e.g., section X-X in FIG. 5A) running along a longitudinal direction of the channel and perpendicular to a top surface of the substrate. 14B is a cross-sectional view of some embodiments of the integrated circuit structure 100 at intermediate stages of the process M1 along a second section (e.g., section Y-Y in FIG. 5A) located in the gate region and perpendicular to the longitudinal direction of the channel.As with the other method embodiments and example devices discussed herein, it is understood that portions of the integrated circuit structure 100 may be fabricated using a CMOS technology process flow, and therefore some processes are only briefly described herein. In addition, the example integrated circuit structure may include various other devices and features, such as other types of devices such as additional transistors, bipolar transistors, resistors, capacitors, inductors, diodes, fuses, static random access memory (SRAM) and / or other logic circuitry, etc., but is simplified for better understanding of the concepts of the present disclosure. In some embodiments, the example integrated circuit structure includes multiple semiconductor devices (e.g., transistors), including PFETs, NFETs, etc., that may be interconnected. Furthermore, it should be noted that the process steps of method M1, including any descriptions given with reference to Figures 2-25, as well as the remainder of the method and exemplary figures presented in this disclosure, are merely exemplary.Referring to FIG. 1A, method M1 begins with step S101 in which one or more epitaxial layers are grown on a substrate. Referring to the example of FIG. 2, in some embodiments, from step S101, an epitaxial stack 120 is formed over substrate 110. In some embodiments, substrate 110 may include silicon (Si). Alternatively, substrate 110 may include germanium (Ge), silicon germanium (SiGe), a III-V material (e.g., GaAs, GaP, GaAsP, AlInAs, AlGaAs, GaInAs, InAs, GaInP, InP, InSb, and / or GaInAsP; or a combination thereof), or other suitable semiconductor materials. In some embodiments, substrate 110 may include a semiconductor-on-insulator (SOI) structure, such as a buried dielectric layer. Alternatively, the substrate 110 may also include a buried dielectric layer, such as a buried oxide (BOX) layer, such as one formed by a process referred to as separation by implantation of oxygen (SIMOX) technology, wafer bonding, SEG, or another suitable process.The epitaxial stack 120 includes epitaxial layers 122 of a first composition sandwiched between epitaxial layers 124 of a second composition. The first and second compositions may be different. In some embodiments, the epitaxial layers 122 are SiGe and the epitaxial layers 124 are silicon (Si). However, other embodiments are possible, including those that provide a first composition and a second composition with different oxidation rates and / or etch selectivities. In some embodiments, the epitaxial layers 122 include SiGe, and when the epitaxial layers 124 include Si, the Si oxidation rate of the epitaxial layers 124 is less than the SiGe oxidation rate of the epitaxial layers 122.The epitaxial layers 124 or portions thereof may form one or more nanolayer channels of the multi-gate transistor. The term "nanolayer" is used herein to refer to any portion of material having nanoscale or even microscale dimensions that has an elongated shape, regardless of the cross-sectional shape of that portion. Thus, this term refers to both elongated portions of material having a circular and substantially circular cross-section, as well as bar or rod-shaped portions of material having, for example, a cylindrical shape or a substantially rectangular cross-section. The use of the epitaxial layers 124 to define one or more channels of a device is discussed in more detail below.It is noted that three layers of epitaxial layers 122 and three layers of epitaxial layers 124 are arranged alternately as illustrated in FIG. 2, but this is for illustrative purposes only. It is appreciated that any number of epitaxial layers may be formed in the epitaxial stack 120; the number of layers depends on the desired number of channel regions for the transistor. In some embodiments, the number of epitaxial layers 124 is between 2 and 10.In some embodiments, each epitaxial layer 122 has a thickness ranging from about 1 nanometer (nm) to about 10 nm, but other ranges are also within the scope of various embodiments of the present disclosure. The epitaxial layers 122 may have a substantially uniform thickness. In some embodiments, each epitaxial layer 124 has a thickness ranging from about 1 nm to about 10 nm, but other ranges are also within the scope of various embodiments of the present disclosure. In some embodiments, the epitaxial layers 124 of the stack have a substantially uniform thickness. As described in more detail below, the epitaxial layers 124 may serve as one or more channel regions for a subsequently formed multi-gate device, and the thickness is chosen based on device performance considerations. The epitaxial layers 122 in the one or more channel regions may eventually be removed and serve to define a vertical distance between the one or more adjacent channel regions for a subsequently formed multi-gate device, and the thickness is chosen based on device performance considerations. Accordingly, the epitaxial layers 122 may also be referred to as sacrificial layers and the epitaxial layers 124 may also be referred to as channel layers.For example, the epitaxial growth of the layers of stack 120 may be performed by a molecular beam epitaxy (MBE) process, a metal organic chemical vapor deposition (MOCVD) process, and / or other suitable epitaxial growth processes. In some embodiments, the epitaxially grown layers, such as epitaxial layers 124, include the same material as substrate 110. In some embodiments, epitaxially grown layers 122 and 124 include a different material than substrate 110. As mentioned above, in at least some examples, epitaxial layers 122 include an epitaxially grown silicon germanium (SiGe) layer, and epitaxial layers 124 include an epitaxially grown silicon (Si) layer. Alternatively, in some embodiments, each of the epitaxial layers 122 and 124 may include other materials such as germanium, a compound semiconductor such as silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide, an alloy semiconductor such as SiGe, GaAsP, AlInAs, AlGaAs, InGaAs, GaInP, and / or GaInAsP, or combinations thereof. As discussed, the materials of the epitaxial layers 122 and 124 may be selected based on providing different oxidation and / or etch selectivity characteristics. In some embodiments, the epitaxial layers 122 and 124 are substantially dopant-free (i.e., having an extrinsic dopant concentration of about 0 cm-3 to about 1×1018cm-3), for example, with no intentional doping performed during the epitaxial growth process.The method M1 then proceeds to step S102 in which semiconductor fins are formed by patterning. Referring to the example of FIG. 3, in some embodiments, a plurality of semiconductor fins 130 are formed extending from the substrate 110 by block S102. In various embodiments, each of the fins 130 comprises a substrate portion 112 formed from the substrate 110 and portions of each of the epitaxial layers of the epitaxial stack comprising the epitaxial layers 122 and 124. The fins 130 may be formed using any suitable methods, including double patterning or multiple patterning processes. Generally, double patterning or multiple patterning processes combine photolithography and self-alignment processes, which may produce structures that, for example, have pitches that are smaller than those that may otherwise be obtained by a single, direct photolithography process. For example, in one embodiment, a sacrificial layer is formed over a substrate and patterned by a photolithography process. Spacers are formed along the patterned sacrificial layer by a self-aligned process. The sacrificial layer is then removed, and the remaining spacers, or mandrels, can then be used to pattern the fins 130 by etching the original epitaxial stack 120. The etching process may include dry etching, wet etching, reactive ion etching (RIE), and / or other suitable processes.In the illustrated embodiment, as illustrated in FIGS. 2 and 3, prior to patterning the fins 130, a hard mask (HM) layer 910 is formed over the epitaxial stack 120. In some embodiments, the HM layer includes an oxide layer 912 (e.g., a pad oxide layer that may include SiO2) and a nitride layer 914 (e.g., a pad nitride layer that may include Si3N4) formed over the oxide layer. The oxide layer 912 may act as an adhesion layer between the epitaxial stack 120 and the nitride layer 914 and may act as an etch stop layer for etching the nitride layer 914. In some examples, the HM oxide layer 912 includes thermally grown oxide, oxide deposited by chemical vapor deposition (CVD), and / or oxide deposited by atomic layer deposition (ALD). In some embodiments, the HM nitride layer 914 is deposited on the HM oxide layer 912 by CVD and / or other suitable techniques.The fins 130 may then be fabricated using suitable processes, including photolithography and etching processes. The photolithography process may include forming a photoresist layer (not shown) over the HM layer 910, exposing the photoresist to a pattern, performing post-exposure firing processes, and developing the resist to form a patterned mask comprising the resist. In some embodiments, patterning the photoresist to form the patterned mask element may be performed using an electron beam (e-beam) lithography process or an extreme ultraviolet (EUV) lithography process using light in the EUV region having a wavelength of, for example, about 1-100 nm. The patterned mask may then be used to protect regions of the substrate 110 and layers formed thereon while an etching process forms trenches 102 in unprotected regions through the HM layer 910, through the epitaxial stack 120, and into the substrate 110, leaving the plurality of extending fins 130. The trenches 102 may be etched using a dry etch (e.g., reactive ion etch), a wet etch, and / or a combination thereof. Numerous other embodiments of methods for forming the fins on the substrate may also be used, including, for example, defining the fin region (e.g., through mask or isolation regions) and epitaxially growing the epitaxial stack 120 in the shape of the fin elements 130.Referring to FIGS. 1A and 4, method M1 proceeds to step S103 by forming shallow trench isolation (STI) features 140 disposed between fins 130. For example, and not by way of limitation, a dielectric layer is first deposited over substrate 110, filling trenches 102 with the dielectric material. In some implementations, the dielectric layer may include silicon oxide, silicon nitride, silicon oxynitride, fluorine-doped silicate glass (FSG), a low-k dielectric, combinations thereof, and / or other suitable materials. In various examples, the dielectric layer may be deposited by a CVD process, a subatmospheric CVD (SACVD) process, a flowable CVD process, an ALD process, a physical vapor deposition (PVD) process, and / or another suitable process. In some embodiments, the integrated circuit structure 100 may be annealed after deposition of the dielectric layer, for example, to improve the quality of the dielectric layer. In some embodiments, the dielectric layer (and the subsequently formed STI features 140) may include a multi-layer structure, for example, having one or more liner layers.In some embodiments of forming the isolation features (STI features), the deposited dielectric material is thinned and planarized after deposition of the dielectric layer, for example, by a chemical mechanical polishing (CMP) process. In some embodiments, the HM layer 910 (as illustrated in FIG. 3) functions as a CMP stop layer. The STI features 140 disposed between the fins 130 are recessed. As seen in the example of FIG. 4, the STI features 140 are recessed, thereby creating the fins 130 extending over the STI features 140. In some embodiments, the recessing process may include a dry etch process, a wet etch process, and / or a combination thereof. The HM layer 910 may also be removed before, during, and / or after recessing the STI features 140. The nitride layer 914 of the HM layer 910 may be removed, for example, by a wet etch process using H3PO4 or other suitable etchants. In some embodiments, the oxide layer 912 of the HM layer 910 is removed by the same etchant used for recessing the STI features 140. In some embodiments, a recess depth is controlled (e.g., by controlling an etch time) to obtain a desired height of the exposed upper portion of the fins 130. In the illustrated embodiment, the desired height exposes each of the layers of the epitaxial stack 120 in the fins 130.The method M1 then proceeds to step S104 in which sacrificial layers / features are formed, and in particular a dummy gate structure. Although the present discussion refers to a replacement gate process in which a dummy gate structure is formed and subsequently replaced, other configurations are also possible.Referring to FIGS. 5A and 5B, a gate structure 150 is formed. In some embodiments, the gate structure 150 is a dummy or sacrificial gate structure that is subsequently removed. Thus, in some embodiments using a gate last process, the gate structure 150 is a dummy gate structure and is replaced by the final gate structure at a subsequent processing stage of the integrated circuit structure 100. In particular, the dummy gate structure 150 may be replaced by a high-k dielectric (HK) layer and a metal gate electrode (MG) at a later processing stage, as discussed below. In some embodiments, the dummy gate structure 150 is formed over the substrate 110 and is at least partially disposed over the fins 130. The portion of the fins 130 underlying the dummy gate structure 150 may be referred to as the channel region. The dummy gate structure 150 may also define a source / drain (S / D) region of the fins 130, for example, the regions of the fin 130 adjacent to, and on opposite sides of, the channel region.In the illustrated embodiment, in step S104, a dummy gate dielectric layer 152 is first formed over the fins 130. In some embodiments, the dummy gate dielectric layer 152 may include SiO2, silicon nitride, a high-k dielectric material, and / or another suitable material. In various examples, the dummy gate dielectric layer 152 may be deposited by a CVD process, a subatmospheric CVD (SACVD) process, a flowable CVD process, an ALD process, a PVD process, and / or another suitable process. The dummy gate dielectric layer 152 may be used, for example, to prevent damage to the fins 130 by subsequent processes (e.g., subsequent formation of the dummy gate structure). Subsequently, in step S104, other portions of the dummy gate structure 150 are formed, including a dummy gate electrode layer 154 and a hard mask that may include multiple layers 156 and 158 (e.g., an oxide layer 156 and a nitride layer 158). In some embodiments, the dummy gate structure 150 is formed by various process steps, such as layer deposition, patterning, etching, and other suitable process steps. Example layer deposition processes include CVD (including low pressure CVD and plasma enhanced CVD), PVD, ALD, thermal oxidation, electron beam evaporation, or other suitable deposition techniques, or combinations thereof. In forming the gate structure, the patterning process includes, for example, a lithography process (e.g., photolithography or electron beam lithography), which may further include photoresist coating (e.g., spin coating), soft firing, mask alignment, exposure, post-exposure firing, photoresist development, rinsing, drying (e.g., spin drying and / or hard firing), other suitable lithography techniques, and / or combinations thereof. In some embodiments, the etching process may include dry etching (e.g., RIE etching), wet etching, and / or other etching techniques. In some embodiments, the dummy gate electrode layer 154 may include polycrystalline silicon (polysilicon). In some embodiments, the hard mask includes an oxide layer 156, such as a pad oxide layer that may include SiO2, and a nitride layer 158, such as a pad nitride layer that may include Si3N4 and / or silicon oxynitride. In some embodiments, after patterning the dummy gate electrode layer 154, the dummy gate dielectric layer 152 is removed from the S / D regions of the fins 130. The etching process may include a wet etch, a dry etch, and / or a combination thereof. The etching process is chosen to selectively etch the dummy gate dielectric layer 152 without substantially etching the fins 130, the dummy gate electrode layer 154, the oxide layer 156, and the nitride layer 158.Referring to FIG. 1A, method M1 then proceeds to step S105 where gate spacers are formed on sidewalls of the dummy gate structures. As illustrated in FIGS. 5A and 5B, in some embodiments of step S105, a spacer material layer is deposited on the substrate. The spacer material layer may be a conformal layer that is subsequently etched back to form gate sidewall spacers. In the illustrated embodiment, a spacer material layer 160 is conformally disposed on the top and sidewalls of the dummy gate structure 150. The spacer material layer 150 may include a dielectric material such as silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, SiCN films, silicon oxycarbide, SiOCN films, and / or combinations thereof. In some embodiments, the spacer material layer 160 includes multiple layers, such as a first spacer layer 162 and a second spacer layer 164 (illustrated in FIG. 5B) formed over the first spacer layer 162. The spacer material layer 160 may be formed, for example, by depositing a dielectric material over the gate structure 150 using processes such as a CVD process, a subatmospheric CVD (SACVD) process, a flowable CVD process, an ALD process, a PVD process, or another suitable process. An anisotropic etch process is then performed on the deposited spacer material layer 160 to expose portions of the fins 130 that are not covered by the dummy gate structure 150 (e.g., in source / drain regions of the fins 130). Portions of the spacer material layer directly above the dummy gate structure 150 may be completely removed by this anisotropic etch process. Portions of the spacer material layer on sidewalls of the dummy gate structure 150 may remain and form gate sidewall spacers, which are referred to as the gate spacers 160 for convenience. Note that while the gate spacers 160 are multi-layer structures in the cross-sectional view of FIG. 5B, they are illustrated as single-layer structures in the perspective view of FIG. 5A for convenience.Referring to FIG. 1A, the method M1 then proceeds to step S106 in which exposed portions of the fins are removed. Referring to FIGS. 6A and 6B, in some embodiments of step S106, exposed portions of the semiconductor fins 130 that extend laterally beyond the gate spacers 160 (e.g., in source / drain regions of the fins 130) are etched, for example, using an anisotropic etch process that uses the dummy gate structure 150 and the gate spacers 160 as an etch mask, resulting in recesses R1 in the semiconductor fins 130 and between corresponding dummy gate structures 150. After the anisotropic etch, the end faces of the sacrificial layers 122 and the channel layers 124 are aligned with respective outermost sidewalls of the gate spacers 160 due to the anisotropic etch. In some embodiments, the anisotropic etch may be performed by a dry chemical etch using a plasma source and a reactant gas. The plasma source may be an inductively coupled plasma (ICP) source, a transformer coupled plasma (TCP) source, an electron cyclotron resonance (ECR) source, or the like, and the reaction gas may be, for example, a fluorine-based gas (such as SF6, CH2F2, CH3F, CHF3, or the like), a chloride-based gas (for example, Cl2), hydrogen bromide gas (HBr), oxygen gas (O2), the like, or combinations thereof.Referring to FIG. 1A, method M1 then proceeds to step S107, in which the sacrificial layers 122 are laterally recessed. Referring to FIGS. 7A and 7B, in some embodiments of step S107, the sacrificial layers 122 are laterally or horizontally recessed using suitable etching techniques, resulting in lateral recesses R2 each vertically sandwiched between corresponding channel layers 124. Step S107 may be performed using a selective etching process. By way of example, and not limitation, the sacrificial layers 122 are SiGe and the channel layers 124 are silicon, allowing selective etching of the sacrificial layers 122. In some embodiments, the selective wet etch includes an APM etch (e.g., an ammonia hydroxide-hydrogen peroxide-water mixture), which etches SiGe at a faster etch rate than Si. In some embodiments, the selective etching includes SiGe oxidation followed by SiGeOx removal. For example, the oxidation may be performed by O3 cleaning and then SiGeOx is removed by an etchant such as NH4OH, which selectively etches SiGeOx at a faster etch rate than Si. Furthermore, because the oxidation rate of Si is much lower (sometimes 30 times lower) than the oxidation rate of SiGe, the channel layers 124 are not significantly etched by the process of laterally recessing the sacrificial layers 122. As a result, the channel layers 124 extend laterally beyond the opposite end faces of the sacrificial layers 122.Referring to FIG. 1A, the method M1 then proceeds to step S108 where the inner spacers are formed on opposite end surfaces of the laterally recessed sacrificial layers. As illustrated in FIGS. 8A and 8B, in some embodiments of step S108, an inner spacer material layer 170 is formed to fill the recesses R2 left by the lateral etching of the sacrificial layers 122, discussed above with reference to FIGS. 7A and 7B. The inner spacer material layer 170 may be a low-k dielectric material, such as SiO2, SiN, SiCN, or SiOCN, and may be formed by a suitable deposition process, such as ALD. After depositing the inner spacer material layer 170, an anisotropic etch process may be performed to trim the deposited inner spacer material 170 such that only portions of the deposited inner spacer material 170 remain that fill the recesses R2 left by the side etching of the sacrificial layers 122. After trimming, the remaining portions of the deposited inner spacer material are referred to as inner spacers 170 for convenience. The inner spacers 170 serve to isolate the metal gates from the source / drain regions that will be formed in subsequent processing. In the example of FIGS. 8A and 8B, the sidewalls of the inner spacers 170 are aligned with sidewalls of the channel layers 124.Referring to FIG. 1A, the method M1 then proceeds to step S109 where source regions of the fins are further recessed. Referring to FIG. 9, in some embodiments of step S109, a patterned mask P1 is first formed to cover the drain regions D of the fins 130 but not cover the source regions S of the fins 130, and then the source regions S of the fins 130 are recessed, resulting in source region recesses R3 in the semiconductor fins 130. In some embodiments, the patterned mask P1 may be a photoresist mask formed by a suitable photolithography process. For example, the photolithography process may include spin-coating a photoresist layer over the structure as illustrated in FIGS. 8A and 8B, performing post-exposure firing processes, and developing the photoresist layer to form the patterned mask P1. In some embodiments, patterning the photoresist to form the patterned mask element may be performed using an electron beam (e-beam) lithography process or an extreme ultraviolet (EUV) lithography process.Once the patterned mask P1 is formed, the source region recesses R3 may be formed in the source regions S, for example, by an anisotropic etching process. In some embodiments, the anisotropic etching may be performed by a dry chemical etching with a plasma source and a reactant gas. As an example, and without limitation, the plasma source may be an inductively coupled plasma (ICP) source, a transformer coupled plasma (TCP) source, an electron cyclotron resonance (ECR) source, or the like, and the reactant gas may be a fluorine-based gas (such as SF6, CH2F2, CH3F, CHF3, or the like), a chloride-based gas (e.g., Cl2), hydrogen bromide gas (HBr), oxygen gas (O2), the like, or combinations thereof.The source region recesses R3 have a depth T3 that is deep enough to allow for the formation of air gaps in a subsequently formed backside ILD layer, as will be discussed in more detail below. In other words, the deeper the source region recesses R3 are, the easier it is to form air gaps in the backside ILD layer. As a result, the depth T3 of the source region recesses R3 is selected to allow for air gap formation in subsequent processing. For example, the depth T3 of the source region recesses R3 is in a range from about 30 nm to about 100 nm. If the depth T3 of the source region recesses R3 is excessively small, the air gap (for example, the air gap 272 illustrated in FIG. 21) may not be well formed because the gap height of the subsequently formed gap G4 (as illustrated in FIG. 20) in the z-direction is insufficient. If the depth T3 of the source region recesses R3 is excessively large, the equivalent k-value (i.e., the dielectric constant) in the subsequently formed backside ILD layer 270 (as illustrated in FIG. 21) may not be as low because the air space in the backside ILD layer 270 is insufficient. However, other ranges of the depth T3 of the source region recesses R3 are also within the scope of various embodiments of the present disclosure as long as air gaps can be formed in the backside ILD layer. However, the shorter the lateral distance D3 between the source region recesses R3, the easier it is to form air gaps in the backside ILD layer. As a result, the lateral distance D3 between the source region recesses R3 is selected to allow air gap formation in the subsequent processing. For example, the lateral distance D3 between the source region recesses R3 is in a range from about 50 nm to about 100 nm. If the lateral distance D3 between the source region recesses R3 is excessively small, the equivalent dielectric constant in the subsequently formed backside ILD layer 270 (as illustrated in FIG. 21) may not be low enough because the air gap may be too small resulting from premature fusion of deposited dielectrics during deposition of the backside ILD layer 270. If the lateral distance D3 between the source region recesses R3 is excessively large, the air gap 272 (as illustrated in FIG. 21) may not be well formed. However, other ranges of the lateral distance D3 between the source region recesses R3 are also within the scope of various embodiments of the present disclosure, as long as air gaps can be formed in the backside ILD layer.The etching time / duration for forming the source region recesses R3 is selected such that the depth T3 of the source region recesses R3 can reach a target value within the range described above. For example, and without limitation, the etching time / duration for forming the source region recesses R3 is in a range from about 30 seconds to about 300 seconds. If the etching time / duration for forming the source region recesses R3 is excessively short, the depth T3 of the source region recesses R3 may be insufficient to allow the formation of air gaps in the backside ILD layer. If the etching time / duration for forming the source region recesses R3 is excessively long, the depth T3 of the source region recesses R3 may be too deep such that the equivalent dielectric constant in the subsequently formed backside ILD layer 270 may not be low enough because the air space in the backside ILD layer 270 is insufficient.In some embodiments, as illustrated in FIG. 9, the source region recesses R3 may have sidewalls that are laterally offset from outermost sidewalls of the inner spacers 170. This is due to the shadowing effect created by directing etch ions into the deep recesses R1 between dummy gate structures 150. However, in some other embodiments, sidewalls of the source region recesses R3 may be aligned with outermost sidewalls of the inner spacers 170.Referring to FIG. 1B, the method M1 then proceeds to step S110 where sacrificial epitaxial plugs are formed in the respective source region recesses. Referring to FIG. 10, in some embodiments, from step S110, with the patterned mask P1 in place, an epitaxial growth process is performed to grow an epitaxial material in the source region recesses R until the epitaxial material builds up sacrificial epitaxial plugs 180 filling the source region recesses R3. The epitaxial material has a different composition than the substrate 110, resulting in a different etch selectivity between the sacrificial epitaxial plugs 180 and the substrate 110. For example, the substrate 110 is Si, and the sacrificial epitaxial plugs 180 are SiGe. In some embodiments, the sacrificial epitaxial plugs 180 are formed of SiGe that is free of p-dopants (e.g., boron) and n-dopants (e.g., phosphorus) because the sacrificial epitaxial plugs 180 are removed during subsequent processing and do not serve as source terminals of transistors in a final IC product. In some embodiments, the sacrificial epitaxial plugs 180 each have a first SiGe layer 182 and a second SiGe layer 184 over the first SiGe layer 182. The first and second SiGe layers 182 and 184 differ at least in terms of germanium atomic percentage (Ge%), which in turn allows for different etch selectivity between the first and second SiGe layers 182 and 184. In certain embodiments, the first SiGe layer 182 has a higher germanium atomic percentage than the second SiGe layer 184. For example, and without limitation, the germanium atomic percentage in the first SiGe layer 182 is in a range of about 20% to about 50%, and the germanium atomic percentage in the second SiGe layer 184 is in a range of about 5% to about 20%. Once the formation of the epitaxial sacrificial plugs 180 is complete, the patterned mask P1 is removed, for example, by ashing.To prevent SiGe from being inadvertently formed at end faces of the Si channel layers 124, the SiGe plugs 180 may be grown from the bottom up in accordance with some embodiments of the present disclosure. For example, and without limitation, the SiGe plugs 180 may be grown by an epitaxial deposition / partial etch process in which the epitaxial deposition / partial etch process is repeated at least once. Such a repeated deposition / partial etch process is also referred to as a "cyclic deposition-etch" (CDE) process. In some embodiments, these SiGe plugs 180 are grown by selective epitaxial growth (SEG) wherein an etching gas is added to promote the selective growth of silicon germanium from the bottom surface of the source region recesses R3 having a first crystal plane, but not from the vertical end surfaces of the channel layers 124 having a second crystal plane different from the first crystal plane. For example, the SiGe plugs 180 are epitaxially grown using reactant gases such as HCl as an etching gas, GeH4as a Ge precursor gas, DCS and / or SiH4as a Si precursor gas, H2and / or N2as a carrier gas. In some embodiments, the etching gas may be other chlorine-containing gases or bromine-containing gases such as Cl2, BCl3, BiCl3, BiBr3, or the like.The conditions for SiGe deposition are controlled (for example, by adjusting the flow rate ratio between Ge precursor gas, Si precursor gas, and carrier gas) such that the SiGe growth rate on the bottom surfaces of the source region recesses R3 is faster than the SiGe growth rate on the vertical end surfaces of the channel layers 124 because the bottom surfaces of the source region recesses R3 and the vertical end surfaces of the channel layers 124 have different crystal orientation planes. Accordingly, the SiGe deposition step including the etching step promotes SiGe growth from bottom to top. For example, SiGe is grown from the bottom surface of the source region recesses R3 at a faster rate than the rate from the end surfaces of the channel layers 124. The etching gas etches SiGe grown from the end surfaces of the channel layers 124 as well as SiGe grown from the bottom surface of the source region recesses R3 at comparable etch rates. However, since the SiGe growth rate from the bottom surfaces of the source region recesses R3 is faster than from the end surfaces of the channel layers 124, the net effect is that SiGe essentially grows from the bottom surfaces of the source region recesses R3 from the bottom up. For example, and without limitation, in each deposition-etch cycle of the CDE process, once the end faces of the channel layers 124 are exposed, the etching step stops, and the SiGe grown from the bottom faces of the source region recesses R3 remains in the source region recesses R3 because it is thicker than the SiGe grown from the end faces of the channel layers 124. In this way, bottom-up growth can be realized. The CDE process described above is just an example to explain how SiGe plugs 180 are formed in the source region recesses R3 but not at the end faces of Si channel layers 124; and other suitable techniques for forming the SiGe plugs 180 may also be used.To achieve different germanium atomic percentages in the first and second SiGe layers 182 and 184, a ratio of a flow rate of the Ge precursor gas (e.g., GeH4) to a flow rate of the Si precursor gas (e.g., SiH4) is varied for their respective growth processes. For example, the ratio of Ge to Si precursor flow rate during epitaxial growth of the first SiGe layer 182 is larger than that of the second SiGe layer 184. In this way, the germanium atomic percentage of the first SiGe layer 182 is larger than that of the second SiGe layer 184.Referring to FIG. 1B, the method M1 then proceeds to step S111 in which epitaxial source structures are formed over the epitaxial sacrificial plugs and epitaxial drain structures are formed over drain regions of the fins. Referring to the example of FIG. 11, in some embodiments of step S111, epitaxial source structures 190S are formed over the respective epitaxial sacrificial plugs 180 and epitaxial drain structures 190D are formed over the drain regions D of the semiconductor fins 130. The epitaxial source / drain structures 190S / 190D may be formed by performing an epitaxial growth process that provides an epitaxial material on the epitaxial sacrificial plugs 180 and the fins 130. During the epitaxial growth process, the dummy gate structures 150 and gate sidewall spacers 160 confine the epitaxial source / drain structures 19oS / 19oD to the source / drain regions S / D. Suitable epitaxial processes include CVD deposition techniques (e.g., vapor-phase epitaxy (VPE) and / or ultra-high vacuum CVD (UHV-CVD)), molecular beam epitaxy, and / or other suitable processes. The epitaxial growth process may use gaseous and / or liquid precursors that interact with the composition of the semiconductor materials of the fins 130, the sacrificial epitaxial plugs 180, and the channel layers 124.In some embodiments, the epitaxial source / drain structures 19oS / 19oD may include Ge, Si, GaAs, AlGaAs, SiGe, GaAsP, SiP, or other suitable materials. The epitaxial source / drain structures 190S / 190D may be doped in-situ during the epitaxial process by incorporating doping species such as: p-dopants, such as boron or BF2; n-dopants, such as phosphorus or arsenic; and / or other suitable dopants, including combinations thereof. If the epitaxial source / drain structures 190S / 190D are not doped in-situ, an implantation process (i.e., a junction implantation process) is performed to dope the epitaxial source / drain structures 19oS / 19oD. In some example embodiments, the epitaxial source / drain structures 190S / 190D in an NFET device include SiP, while those in a PFET device include GeSnB and / or SiGeSnB.In some embodiments, the epitaxial source / drain structures 190S / 190D each include a first epitaxial layer 192 and a second epitaxial layer 194 above the first epitaxial layer 192. The first and second epitaxial layers 192 and 194 may differ at least in terms of germanium atomic percentage (Ge%) or phosphorus concentration (P%). In the embodiment shown, the first epitaxial layer 192 may not only be grown from the top surfaces of the epitaxial sacrificial plugs 180 and the fins 130, but may also be grown from end surfaces of the channel layers 124. This is because forming the epitaxial source / drain structures 190S / 190D does not require the bottom-up approach as previously discussed with respect to the epitaxial sacrificial plugs 180.In some embodiments where the epitaxial source / drain structures 190S / 190D include GeSnB and / or SiGeSnB to form PFETs, the first and second epitaxial layers 192 and 194 differ at least in terms of germanium atomic percentage (Ge%). In certain embodiments, the first SiGe layer 192 has a lower germanium atomic percentage than the second SiGe layer 194. A low germanium atomic percentage in the first SiGe layer 192 helps reduce the Schottky barrier with the undoped Si in the fins 130. A high germanium atomic percentage in the second SiGe layer 194 helps reduce the source / drain contact resistance. For example, and without limitation, the germanium atomic percentage in the first SiGe layer 192 is in a range of about 5% to about 20%, and the germanium atomic percentage in the second SiGe layer 194 is in a range of about 30% to about 50%. In some embodiments, the second SiGe layer 194 may have a gradient of germanium atomic percentage. For example, the germanium atomic percentage in the second SiGe layer 194 increases with increasing distance from the first SiGe layer 192.In some embodiments where the epitaxial source / drain structures 190S / 190D include SiP to form NFETs, the first and second SiP layers 192 and 194 differ at least in phosphorus concentration (P%). In certain embodiments, the first SiP layer 192 has a lower phosphorus concentration than the second SiP layer 194. A low phosphorus concentration in the first SiP layer 192 helps reduce the Schottky barrier with the undoped Si in the fins 130. A high phosphorus concentration in the second SiP layer 194 helps reduce the source / drain contact resistance. For example, and without limitation, the phosphorus concentration in the first SiP layer 192 is in a range of about 10% to about 30%, and the phosphorus concentration in the second SiP layer 194 is in a range of about 20% to about 60%. In some embodiments, the second SiP layer 194 may have a gradient of phosphorus concentration. For example, the phosphorus concentration in the second SiP layer 194 increases with increasing distance from the first SiP layer 192.Once the epitaxial source / drain structures 190S / 190D have been formed, an annealing process may be performed to activate the p-dopants or n-dopants in the epitaxial source / drain structures 190S / 190D. The annealing process may be, for example, a rapid thermal anneal (RTA), a laser anneal, a millisecond thermal annealing (MSA) process, or the like.Referring to FIGS. 1B and 12, the method M1 then proceeds to step S112 in which a front side ILD layer 210 is formed on the substrate 110. The ILD layer 210 is referred to as a “front side” ILD layer in this context because it is formed on a front side of the multi-gate transistors (i.e., on a side of the multi-gate transistors whose gates protrude from the source / drain regions 190S / 190D). In some embodiments, a contact etch stop layer (CESL) 200 is also formed prior to forming the ILD layer 210. In some examples, the CESL includes a silicon nitride layer, a silicon oxide layer, a silicon oxynitride layer, and / or other suitable materials having a different etch selectivity than the front-side ILD layer 210. The CESL may be formed by a plasma-enhanced chemical vapor deposition (PECVD) process and / or other suitable deposition or oxidation processes. In some embodiments, the front side ILD layer 210 comprises materials such as tetraethyl orthosilicate oxide (TEOS oxide), undoped silicate glass, or doped silicon oxide such as borophosphosilicate glass (BPSG), fused silica glass (FSG), phosphosilicate glass (PSG), boron doped silicon glass (BSG), and / or other suitable dielectric materials having a different etch selectivity than the CESL 200. The front side ILD layer 210 may be deposited by a PECVD process or other suitable deposition technique. In some embodiments, after forming the front side ILD layer 210, the integrated circuit structure 100 may be subjected to a high thermal management process to anneal the front side ILD layer 210.In some examples, after depositing the front side ILD layer, a planarization process may be performed to remove excess materials of the front side ILD layer. For example, a planarization process includes a chemical mechanical planarization (CMP) process in which portions of the front side ILD layer 210 (and the CESL layer, if present) overlying the dummy gate structures 150 are removed and a top surface of the integrated circuit structure 100 is planarized. In some embodiments, the CMP process also removes hard mask layers 156, 158 (as shown in FIG. 11) and exposes the dummy gate electrode layer 154.Referring to FIG. 1B, the method M1 then proceeds to step S113 where first dummy gate structures 150 (as shown in FIG. 12) and then sacrificial layers 122 are removed. The resulting structure is illustrated in FIG. 13. In the illustrated embodiments, in step S113, the dummy gate structures 150 are first removed using a selective etch process (e.g., selective dry etch, selective wet etch, or a combination thereof) that etches the materials in the dummy gate structures 150 at a faster etch rate than other materials (e.g., the gate sidewall spacers 160, the CESL 200, and / or the front-side ILD layer 210), resulting in gate trenches GT1 between corresponding gate sidewall spacers 160, exposing the sacrificial layers 122 in the gate trenches GT1. Subsequently, in step S113, the sacrificial layers 122 in the gate trenches GT1 are removed using another selective etching process that etches the sacrificial layers 122 at a faster etching rate than the channel layers 124, thereby forming openings O1 between adjacent channel layers 124. In this way, the channel layers 124 become nanolayers suspended above the substrate 110 and between the epitaxial source / drain structures 190S / 190D. This step is also referred to as a channel exposure process. In this intermediate processing step, the openings 119 between the nanolayers 124 may be filled with ambient matter (e.g., air, nitrogen, etc.). In some embodiments, the nanolayers 124 may also be interchangeably referred to as nanowires, nanoplates, and nanorings depending on their geometry. For example, in some other embodiments, the channel layers 124 may be trimmed to have a substantially rounded shape (i.e., cylindrical) due to the selective etching process to completely remove the sacrificial layers 122. In this case, the resulting channel layers 124 may also be referred to as nanowires.In some embodiments, the sacrificial layers 122 are removed using a selective wet etch process. In some embodiments, the sacrificial layers 122 are SiGe and the channel layers 124 are silicon, which enables the selective removal of the sacrificial layers 122. In some embodiments, the selective wet etch comprises an APM etch (e.g., an ammonia hydroxide-hydrogen peroxide-water mixture). In some embodiments, the selective removal comprises SiGe oxidation followed by SiGeOx removal. For example, the oxidation may be performed by an O3 cleaning and then SiGeOx is removed by an etchant such as NH4OH, which selectively etches SiGeOx at a faster etch rate than Si. Furthermore, because the oxidation rate of Si is much lower (sometimes 30 times lower) than the oxidation rate of SiGe, the channel layers 124 may not be significantly etched by the channel exposure process. It may be noted that both the channel exposure step and the previous step of side-recessing the sacrificial layers (i.e., step S107) use a selective etch process that etches SiGe at a faster etch rate than Si, and therefore, in some embodiments, these two steps may use the same etch chemistry. In this case, the etch time / duration of the channel exposure step is longer than the etch time / duration of the previous step of side-recessing the sacrificial layers to completely remove the SiGe sacrificial layers.Referring to FIG. 1B and FIGS. 14A, 14B, the method M1 then proceeds to step S114 where replacement gate structures 220 are formed in the gate trenches GT1, respectively, to surround each of the nanolayers 124 suspended in the gate trenches GT1. The gate structure 220 may be the final gate of a GAA-FET. The final gate structure may be a metal gate stack or a high-k gate stack; however, other compositions are also possible. In some embodiments, each of the gate structures 220 forms the gate connected to the multiple channels provided by the plurality of nanolayers 124. For example, the high-k / metal gate structures 220 are formed within the openings O1 (as illustrated in FIG. 13) provided by exposing the nanolayers 124. In various embodiments, the high-k / metal gate structure 220 includes a gate dielectric layer 222 formed around the nanolayers 124, a work function metal layer 224 formed around the gate dielectric layer 222, and a fill metal 226 formed around the work function metal layer 224 and filling a remaining portion of the gate trenches GT1. The gate dielectric layer 222 includes an interface layer (e.g., a silicon oxide layer) and a high-k gate dielectric layer over the interface layer. High-k gate dielectrics, as used and described herein, include dielectric materials having a high dielectric constant, for example, greater than that of thermal silicon oxide (about 3.9). The work function metal layer 224 and / or the fill metal layer 226 used within the high-k / metal gate structures 220 may include a metal, a metal alloy, or a metal silicide. Forming the high-k / metal gate structures 220 may include depositions to form various gate materials or one or more liner layers, as well as one or more CMP processes to remove excess gate materials. As illustrated in a cross-sectional view of FIG. 14B taken along a longitudinal axis of a high-k / metal gate structure 220, the high-k / metal gate structure 220 surrounds each of the nanolayers 124 and is therefore referred to as a gate of a GAA-FET.In some embodiments, the interface layer of the gate dielectric layer 222 may include a dielectric material such as silicon oxide (SiO2), HfSiO, or silicon oxynitride (SiON). The interface layer may be formed by chemical oxidation, thermal oxidation, atomic layer deposition (ALD), chemical vapor deposition (CVD), and / or another suitable method. The high-k dielectric layer of the gate dielectric layer 222 may include hafnium oxide (HfO2). Alternatively, the gate dielectric layer 222 may include other high-k dielectrics such as hafnium silicon oxide (HfSiO), hafnium silicon oxynitride (HfSiON), hafnium tantalum oxide (HfTaO), hafnium titanium oxide (HfTiO), hafnium zirconium oxide (HfZrO), lanthanum oxide (LaO), zirconium oxide (ZrO), titanium oxide (TiO), tantalum oxide (Ta2O5), yttrium oxide (Y2O3), strontium titanium oxide (SrTiO3, STO), barium titanium oxide (BaTiO3, BTO), barium zirconium oxide (BaZrO), hafnium lanthanum oxide (HfLaO), lanthanum silicon oxide (LaSiO), Aluminum silicon oxide (AlSiO), aluminum oxide (Al2O3), silicon nitride (Si3N4), oxynitrides (SiON) and combinations thereof.The work function metal layer 224 may include work function metals to provide a suitable work function for the high-k / metal gate structures 220. For an n-GAA FET, the work function metal layer 224 may include one or more n-type work function metals (N-type metal). The n-type work function metals may include, for example: titanium aluminide (TiAl), titanium aluminum nitride (TiAlN), carbo-nitride tantalum (TaCN), hafnium (Hf), zirconium (Zr), titanium (Ti), tantalum (Ta), aluminum (Al), metal carbides (for example, hafnium carbide (HfC), zirconium carbide (ZrC), titanium carbide (TiC), aluminum carbide (AlC)), aluminides, and / or other suitable materials. On the other hand, for a p-GAA FET, the work function metal layer 224 may include one or more p-type work function metals (P-metal). The p-type work function metals may include, for example: titanium nitride (TiN), tungsten nitride (WN), tungsten (W), ruthenium (Ru), palladium (Pd), platinum (Pt), cobalt (Co), nickel (Ni), conductive metal oxides, and / or other suitable materials.In some embodiments, the filler metal 226 may include, for example, tungsten, aluminum, copper, nickel, cobalt, titanium, tantalum, titanium nitride, tantalum nitride, nickel silicide, cobalt silicide, TaC, TaSiN, TaCN, TiAl, TiAlN, or other suitable materials.Referring to FIG. 1B, the method M1 then proceeds to step S115 in which a drain contact is formed over the epitaxial drain structure. Referring to FIG. 15, in some embodiments, in step S115, a drain contact opening is first formed through the front side ILD layer 210 and the CESL 200 to expose the epitaxial drain structure 190D using suitable photolithography and etching techniques. Subsequently, in step S115, a drain silicide region 230 is formed on the front side of the epitaxial drain structure 190D using a silicide process, followed by forming a drain contact 240 over the drain silicide region 230. The silicide may be performed by: depositing a metal layer (e.g., a nickel layer or a cobalt layer) over the exposed epitaxial drain structure 190D, annealing the metal layer such that the metal layer reacts with silicon (and germanium, if present) in the epitaxial drain structure 190D to form the metal silicide region 230 (e.g., nickel silicide or cobalt silicide), and then removing the unreacted metal layer. The drain contact 240 may be formed by depositing one or more metal materials (e.g., tungsten, cobalt, copper, the like, or combinations thereof) to fill the drain contact hole using suitable deposition techniques (e.g., CVD, PVD, ALD, the like, or combinations thereof), followed by a CMP process to remove excess metal materials outside the drain contact opening.Referring to FIGS. 1B and 16, the method M1 then proceeds to step S116 in which a front side multilayer interconnection (MLI) structure 250 is formed over the substrate 110. The front side MLI structure 250 may include a plurality of front side metallization layers 252. The number of front side metallization layers 252 may vary according to design specifications of the integrated circuit structure 100. For simplicity, only two front side metallization layers 252 are illustrated in FIG. 16. The front side metallization layers 252 each include a first front side inter-metal dielectric (IMD) layer 253 and a second front side IMD layer 254. The second front side IMD layers 254 are formed over the corresponding first front side IMD layers 253. The front side metallization layers 252 include one or more horizontal interconnects, such as front side metal lines 255, each extending horizontally or laterally in the second front side IMD layers 254, and vertical interconnects, such as front side conductive vias 256, each extending vertically in the first front side IMD layers 253.In some embodiments, a front-side conductive via 256 in a bottom-most front-side metallization layer 252 is in contact with the gate structure 220 to electrically connect to the gate structure 220, and a front-side conductive via 256 in the bottom-most front-side metallization layer 252 is in contact with the drain contact 240 to electrically connect to the epitaxial drain structure 190D.For example, the front side metal lines 255 and the front side metal vias 256 may be formed using a single damascene process, a double damascene process, the like, or combinations thereof. In some embodiments, the front side IMD layers 253-254 may include low-k dielectric materials, for example, lower than about 4.0 or even 2.0, disposed between such conductive features. In some embodiments, the front side IMD layers may be made of, for example, phosphosilicate glass (PSG), borophosphosilicate glass (BPSG), fluorosilicate glass (FSG), SiOxCy, spin-on glass, spin-on polymers, silicon oxide, silicon oxynitride, combinations thereof, or the like, and may be formed by any suitable process such as spin-on coating, chemical vapor deposition (CVD), plasma enhanced CVD (PECVD), or the like. The front side metal lines and vias 255 and 256 may comprise metal materials such as copper, aluminum, tungsten, combinations thereof, or the like. In some embodiments, the front side metal lines and vias 255 and 256 may further comprise one or more barrier / adhesion layers (not shown) to protect the respective front side IMD layers 253-254 from metal diffusion (e.g., copper diffusion) and metal poisoning. The one or more barrier / adhesion layers may comprise titanium, titanium nitride, tantalum, tantalum nitride, or the like, and may be formed by physical vapor deposition (PVD), CVD, ALD, or the like.Referring to FIGS. 1B and 17, method M1 then proceeds to step S117 where a carrier substrate 260 is bonded to front-side MLI structure 250 in accordance with some embodiments of the present disclosure. Carrier substrate 260 may be silicon, doped or undoped, or may include other semiconductor materials such as germanium, a compound semiconductor, or combinations thereof. Carrier substrate 260 may provide structural support during subsequent processing on the backside of integrated circuit structure 100 and may remain in the final product in some embodiments. In some other embodiments, carrier substrate 260 may be removed after subsequent processing on the backside of integrated circuit structure 100 is complete. In some embodiments, carrier substrate 260 is bonded to a top dielectric layer of MLI structure 250, for example, by fusion bonding. Subsequently, the integrated circuit structure 100 is turned over so that a back surface of the substrate 110 faces upward, as illustrated in Fig. 18.Referring to Figures 1B and 19, the method M1 then proceeds to step S118 where the substrate 110 is thinned to expose the sacrificial epitaxial plugs 180. In some embodiments, the thinning is accomplished using a CMP process, a grinding process, or the like.Referring to FIG. 1B, the method M1 then proceeds to step S119 where the substrate 110 is removed. Referring to FIG. 20, in some embodiments, from step S119, the Si substrate 110 is removed using a selective etch process that etches Si at a faster etch rate than the SiGe plugs 180. In some embodiments, the selective etch process for selectively removing the Si substrate 110 may be a wet etch process using a wet etch solution such as tetramethylammonium hydroxide (TMAH), potassium hydroxide (KOH), NH4OH, the like, or combinations thereof.As a result of the selective etching process, the epitaxial sacrificial plugs 180 protrude from the back sides of the epitaxial source structure 190S by a protruding height H4 and are separated from each other by a lateral distance D4. Because the epitaxial sacrificial plugs 180 adopt the geometry of the source region recesses R3 (as illustrated in FIG. 9), the protruding height H4 of the epitaxial sacrificial plugs 180 is substantially the same as the depth T3 of the source region recesses R3, and the lateral distance D4 between the epitaxial sacrificial plugs 180 is also the same as the lateral distance D3 between the source region recesses R3. As an example, the protruding height H4 of the epitaxial sacrificial plugs 180 is in a range from about 30 nm to about 100 nm, and the lateral distance D4 between the epitaxial sacrificial plugs 180 is in a range from about 50 nm to about 100 nm.Referring to FIG. 1C, the method M1 then proceeds to step S120 in which a backside ILD layer having one or more air gaps is formed around the sacrificial epitaxial plugs 180. Referring to FIG. 21, in some embodiments, in step S120, a dielectric material of the backside ILD layer 270 is first deposited over the sacrificial epitaxial plugs 180 using suitable deposition techniques, such as a conformal deposition technique such as CVD. Subsequently, in step S120, the deposited dielectric material is thinned, for example, using an etch-back process, a CMP process, or the like, until the sacrificial epitaxial plugs 180 are exposed from the backside ILD layer 270. The ILD layer 270 is referred to in this context as a “backside” ILD layer because it is formed on a backside of the multi-gate transistors opposite the front side of the multi-gate transistors whose replacement gates 220 protrude from the source / drain regions 190S / 190D.Depositing dielectric material into a narrow gap G4 (as indicated in FIG. 20) between the sacrificial epitaxial plugs 180 results in one or more air gaps 272 (i.e., air-filled gaps) in the resulting backside ILD layer 270 due to the high aspect ratio (i.e., the ratio of gap height (i.e., the protruding height H4 of the sacrificial epitaxial plugs 180) to the gap width (i.e., the lateral distance D4 between sacrificial epitaxial plugs)) of the gap G4 between the sacrificial epitaxial plugs 180. More specifically, the high aspect ratio of the gap G4 between the sacrificial epitaxial plugs 180 may result in overhangs 271 (as illustrated in FIG. 20) being formed in an upper portion of the gap G4 between the sacrificial epitaxial plugs 180 during the conformal deposition process. Such overhangs 271 may prevent the dielectric material 270 from completely filling the gap G4 between the epitaxial sacrificial plugs 180 such that the air gap 272 remains and is sealed in the resulting backside ILD layer 270, as illustrated in FIG. 21. In some embodiments, the conformal deposition process is a plasma-free deposition, such as a thermal CVD process or the like. This is because the plasma used in a deposition process (e.g., high density plasma CVD (HDP-CVD)) may result in a sputter etch during deposition, which in turn may prevent overhangs 271 from forming at the upper portion of the gap G4 between the epitaxial sacrificial plugs 180, which in turn may prevent the formation of an air gap 272 in the backside ILD layer 270.In some embodiments, as illustrated in FIG. 21, the air gap 272 may have a tapered profile whose width decreases with increasing distance from the epitaxial drain structure 190D. This is because the formation of overhangs begins at the upper portion of the gap G4 between the epitaxial sacrificial plugs 180. It should be noted, however, that the shape shown in FIG. 21 is selected purely for demonstration purposes and is not intended to limit the various embodiments of the present disclosure. For example, the air gap 272 may also comprise other shapes, such as a rectangle, an oval, a square, a trapezoid, a triangle, and / or the like. In some embodiments, the air gap 272 may overlap the epitaxial drain structure 190D because the formation of the overhangs begins at upper portions of the epitaxial sacrificial plugs 180 extending from the epitaxial source structures 190S.In some embodiments, the backside ILD layer 270 includes materials such as tetraethyl orthosilicate oxide (TEOS) oxide, undoped silicate glass, or doped silicon oxide such as borophosphosilicate glass (BPSG), fused silica (FSG), phosphosilicate glass (PSG), boron-doped silicon glass (BSG), and / or other suitable dielectric materials. In some embodiments, the backside ILD layer 270 has the same material as the frontside ILD layer 210.Referring to FIGS. 1C and 22, the method M1 then proceeds to step S121 in which the epitaxial sacrificial plugs 180 are removed to form backside via openings O5 that extend through the backside ILD layer 270 to expose backsides of the epitaxial source structures 190S. In some embodiments of step S121, the epitaxial sacrificial plugs 180 are removed using a selective etch process that etches the SiGe of the epitaxial sacrificial plugs 180 at a faster etch rate than the dielectric material of the backside ILD layer 270. In other words, the selective etch process uses an etchant that attacks SiGe and has little attack on the backside ILD layer 270. Therefore, after completion of the selective etch process, the air gap 272 remains sealed in the backside ILD layer 270. For example, and without limitation, the sacrificial epitaxial plugs 180 are removed by a selective wet etch, such as an APM etch (e.g., an ammonia hydroxide-hydrogen peroxide-water mixture), which selectively etches SiGe at a faster etch rate than dielectric materials.As previously discussed, the second SiGe layer 184 has a lower germanium atomic concentration than the first SiGe layer 182, allowing for different etch selectivity between the first and second SiGe layers 182 and 184. As a result, in some embodiments, the SiGe selective etch process may etch the second SiGe layer 184 at a slower etch rate than the first SiGe layer 182. Therefore, the second SiGe layer 184 may slow down the SiGe selective etch recess and thus act as a detectable etch endpoint in the SiGe selective etch process to prevent the epitaxial source structures 190S from being attacked by the SiGe selective etch process. In this way, the epitaxial source structures 190S may remain substantially intact after the SiGe selective etch process in some embodiments of the present disclosure. In some other embodiments, the backsides of the epitaxial source structures 190S are recessed due to the SiGe selective etch process. In this case, the first epitaxial layers 192 of the epitaxial source structures 190S may be etched through at bottoms of the backside via openings O5 such that the second epitaxial layers 194 (having a higher Ge or P percentage than the first epitaxial layers 192) may be exposed at the bottoms of the backside via openings O5.Referring to Fig. 1C, the method M1 then proceeds to step S122 in which a metal material layer of back vias is formed in the back openings. Referring to Fig. 23, in some embodiments, in step S122, a source silicide region 280 is first formed on the backside of each of the epitaxial source structures 190S using a silicide process, followed by depositing a metal material layer 290 over the source silicide region 280. The silicide may be performed by: depositing a metal layer (e.g., a nickel layer or a cobalt layer) over the exposed backsides of the epitaxial source structures 190S, annealing the metal layer such that the metal layer reacts with silicon (and germanium, if present) in the epitaxial source structures 190S to form the metal silicide region 280 (e.g., nickel silicide or cobalt silicide), and then removing the unreacted metal layer. Once the formation of the source silicide regions 280 is completed, one or more metal materials (tungsten, cobalt, copper, the like, or combinations thereof) may be deposited using suitable deposition techniques (e.g., CVD, PVD, ALD, the like, or combinations thereof) to form a metal material layer 290 overfilling the backside via openings O5.Referring to FIGS. 1C and 24, the method M1 then proceeds to step S123 in which the metal material layer 290 is thinned to form backside vias 292 in the backside via openings O5. In some embodiments of step S123, a CMP process is performed to thin the metal material layer 290 (as illustrated in FIG. 23) until the backside ILD layer 270 is exposed while leaving separate portions of the metal material 290 in the backside via openings O5 to serve as backside vias 292. In some embodiments, the CMP process uses a high removal selectivity (HSS) slurry that has a high removal selectivity between the metal material 290 and the dielectric material of the backside ILD layer 270 so that the determination of the polishing endpoint becomes more clear. In particular, in the CMP process using HSS, the metal material 290 has a faster removal rate (RR) than the dielectric material of the backside ILD layer 270, so that the backside ILD layer 270 can slow down or even stop the CMP process, and thus the backside ILD layer 270 acts as a detectable polishing endpoint in the CMP process. In this way, the backside ILD layer 270 can remain substantially intact after the CMP process, so that the air gap 272 in the backside ILD layer 270 remains sealed. Because air in the sealed air gap 272 has a relative permittivity (or dielectric constant) of approximately 1, the capacitive coupling between adjacent backside vias 292 can be reduced to reduce the RC time delay, which in turn improves the operating speed of the integrated circuit 100. In some embodiments, the HSS used in this CMP process includes, for example, and without limitation, alumina, potassium hydroxide, malonic acid, ferric nitrate, deionized water, or combinations thereof.Referring to FIGS. 1C and 25, the method M1 then proceeds to step S124 where a backside MLI structure 300 is formed over the backside vias 292 and the backside ILD layer 270. The backside MLI structure 300 may include a bottommost metallization layer 301 and a plurality of upper backside metallization layers 302 over the bottommost backside metallization layer 301. The number of upper backside metallization layers 302 may vary according to design specifications of the integrated circuit structure 100. For simplicity, only two backside metallization layers 302 (also called backside M1 layer and backside M2 layer) are illustrated in FIG. 25.The bottommost backside metallization layer 301 (also called backside M0 layer) includes a backside IMD layer 303 over the backside ILD layer 270 and one or more horizontal interconnects, such as backside metal lines 305, extending horizontally or laterally in the backside IMD layer 303. A metal line 305 in the bottommost backside metallization layer 301 is a power rail that extends across and contacts one or more backside source vias 292 to electrically connect to one or more epitaxial source structures 190S. Because the power rail is formed in the backside MLI structure 300, more routing space may be provided for the integrated circuit structure 100.The backside metallization layers (e.g., the backside M1 layer and the M2 layer) 302 each include a first backside inter-metal dielectric (IMD) layer 304 and a second backside IMD layer 306. The second backside IMD layers 306 are formed over the corresponding first backside IMD layers 304. The backside metallization layers 302 include one or more horizontal interconnects, such as backside metal lines 307, each extending horizontally or laterally in the second backside IMD layers 306, and vertical interconnects, such as backside conductive vias 308, each extending vertically in the first backside IMD layers 304.In some embodiments, the backside vias 308 have a tapered profile (as illustrated in dashed lines) with a width that decreases with decreasing distance from the backside ILD layer 270 due to the nature of etching via openings in the backside IMD layers 304 after the IC structure 100 is flipped. In addition, the backside vias 292 have a tapered profile with a width that decreases with increasing distance from the epitaxial source structures 190S due to the nature of etching source region recesses R3 (as illustrated in FIG. 9) before the IC structure 100 is flipped. Therefore, the backside vias 292 narrow in a direction opposite to a direction in which the backside vias 308 narrow. More specifically, the backside vias 292 narrow toward the backside MLI structure 300, and the backside vias 308 narrow toward the frontside MLI structure 250.26-33 illustrate exemplary cross-sectional views of various stages for fabricating an integrated circuit structure 100' in accordance with some other embodiments of the present disclosure. It should be understood that additional operations may be performed before, during, and after the processes shown in FIGS. 26-33, and that some of the operations described subsequently may be replaced or omitted to obtain additional embodiments of the method. The operations or processes may be interchangeable in their order. The same or similar configurations, materials, processes, and / or operations as described with respect to FIGS. 2-25 may be used in the following embodiments, and their detailed explanation may be omitted.After the structure shown in Figure 19 is formed, the substrate 110 is etched back such that the upper portions of the sacrificial epitaxial plugs 180 protrude from the etched back substrate 110a. The resulting structure is illustrated in Figure 26. In some embodiments, the Si substrate 110 is etched back using a selective etch process that etches Si at a faster etch rate than the SiGe plugs 180. In some embodiments, the selective etch process for selectively removing the Si substrate 110 may be a wet etch process using a wet etch solution such as tetramethylammonium hydroxide (TMAH), potassium hydroxide (KOH), NH4OH, the like, or combinations thereof. The etching time / duration is controlled such that a lower portion 110a of the Si substrate 110 remains around the epitaxial sacrificial plugs 180 after the etchback is completed.Next, epitaxial sacrificial caps 400 are formed on the protruding portions of the epitaxial sacrificial plugs 180. The resulting structure is illustrated in Figure 27. In some embodiments, the epitaxial sacrificial caps 400 are formed of SiGe that is free of p-dopants (e.g., boron) and n-dopants (e.g., phosphorus) because the epitaxial sacrificial caps 400 will be removed during subsequent processing and will not serve as source terminals of transistors in a final IC product. A combined structure of an epitaxial sacrificial cap 400 and an epitaxial sacrificial plug 180 may be hammer-shaped in a cross-sectional view and is therefore referred to as a hammer-shaped sacrificial via 409, which is replaced by a hammer-shaped back via during subsequent processing. In some embodiments, the SiGe sacrificial caps 400 have a higher germanium atomic concentration than the second SiGe layer 184 of the SiGe sacrificial plugs 180, which in turn enables the SiGe caps 400 to be etched at a faster etch rate than the second SiGe layer 184 during subsequent etching of the backside via openings. For example, and without limitation, the germanium atomic percentage in the SiGe sacrificial caps 400 is in a range of about 20% to about 50%. In some embodiments, the SiGe sacrificial caps 400 have a comparable germanium atomic percentage as the first SiGe layer 182 of the SiGe sacrificial plugs 180 because the first SiGe layer 182 does not serve as an etch endpoint during subsequent etching of backside via openings.Due to different growth rates on different crystal planes of the different faces of the epitaxial sacrificial plugs 180, the growth of the epitaxial sacrificial caps 400 includes lateral growth and vertical growth. Therefore, facets are formed as the faces of the sacrificial caps 400. For example, and without limitation, in the cross-sectional view of Figure 27, the epitaxial sacrificial caps 400 each have a hammerhead profile or an octagonal profile that includes a horizontal facet 401 at its top, a pair of upwardly inclined facets 402 facing away from the substrate 110a and extending at an angle from opposite sides of the horizontal facet 401, a pair of vertical facets 403 each extending from the lower edges of the pair of upwardly inclined facets 402, and a pair of downwardly inclined facets 404 facing the substrate 110a and each extending at an angle from the lower edges of the pair of vertical facets 403. The lateral growth of the epitaxial sacrificial caps 400 decreases the lateral distance D6 of the gap G6 between the hammer-shaped sacrificial vias 409, and the vertical growth of the epitaxial sacrificial caps 400 increases a height H6 of the hammer-shaped sacrificial via 409. As a result, the epitaxial sacrificial caps 400 can increase the aspect ratio of the gap G6 between the hammer-shaped sacrificial vias 409, which in turn assists in forming air gaps in the subsequently formed backside ILD layer.In some embodiments, the epitaxial sacrificial caps 400 may be grown by an epitaxial deposition / partial etch process, wherein the epitaxial deposition / partial etch process is repeated at least once. Such a repeated deposition / partial etch process is also referred to as a cyclic deposition-etch (CDE) process, which includes one or more repetitions of a deposition step and an etch step. For example, the CDE process may perform a deposition step followed by an etch step, and then repeats the deposition and cleaning steps. In some example embodiments where the epitaxial sacrificial caps 400 are SiGe, the SiGe caps 400 may be epitaxially grown using reactant gases such as HCl as an etching gas, GeH4as a Ge precursor gas, DCS and / or SiH4as a Si precursor gas, H2and / or N2as a carrier gas. In some embodiments, the etching gas may be other chlorine-containing gases or bromine-containing gases such as Cl2, BCl3, BiCl3, BiBr3, or the like.The conditions for SiGe deposition may be controlled in such a manner (for example, by tuning the flow rate ratio between Ge precursor gas, Si precursor gas, and carrier gas) that the SiGe growth rate on the surfaces of the SiGe plugs 180 is faster than the SiGe growth rate on the back surface of the etched back Si substrate 110a because the surfaces of the SiGe plugs 180 have different crystal orientation planes than the back surface of the etched back Si substrate 110a. Moreover, the etching gas etches SiGe grown from the etched back Si substrate 110a at an etching rate comparable to that at which it etches SiGe grown from the SiGe plugs 180. The end effect of the CDE process is that SiGe caps 400 selectively grow from the SiGe plugs 180 while the back surface of the Si substrate 110a remains exposed. For example, and without limitation, in each deposition-etch cycle of the CDE process, the etching step is stopped once the back surface of the Si substrate 110a is exposed, while the SiGe grown from the SiGe plugs 180 remains on the SiGe plugs 180 because it is thicker than the SiGe grown from the back surface of the Si substrate 110a.The CDE process described above is just an example to explain how SiGe caps 400 are formed on the SiGe plugs 180 but not on the back surface of the Si substrate 110a; and other suitable techniques for forming the SiGe caps 400 may also be used. For example, in some other embodiments, a patterned mask (e.g., an oxide mask) may be formed over the back surface of the Si substrate 110a prior to forming the SiGe caps 400, such that the patterned mask may prevent SiGe growth on the back surface of the Si substrate 110a. The patterned mask may be formed, for example, by depositing a dielectric material over the back surface of the Si substrate 110a and also over the SiGe plugs 180, followed by etching back the dielectric material such that upper portions of the SiGe plugs 180 protrude above the etched back dielectric material. With the patterned mask in place, the SiGe caps 400 may be formed on the SiGe plugs 180 using MOCVD, MBE, and / or other suitable epitaxial growth processes. The patterned mask is then removed from the back surface of the Si substrate 110a after forming the SiGe caps 400, leaving a gap between the lowermost ends of the SiGe caps 400 and the back surface of the Si substrate 110a. In this case, the SiGe caps 400 are completely separated from the Si substrate 110a due to the gap created by removing the structure mask.After the formation of the epitaxial sacrificial caps 400 is complete, the substrate 110 is removed using a selective etch process, leaving a high aspect ratio gap G6 between the hammer-shaped sacrificial vias 409. The resulting structure is illustrated in Figure 28. For example, in some embodiments where the substrate 110 is Si and the hammer-shaped sacrificial vias 409 are SiGe, the Si substrate 110 is removed using a selective etch process that etches Si at a faster etch rate than the SiGe via structures 409. In some embodiments, the selective etch process for selectively removing the Si substrate 110 may be a wet etch process using a wet etch solution such as tetramethylammonium hydroxide (TMAH), potassium hydroxide (KOH), NH4OH, the like, or combinations thereof.As a result of the selective etching process, the hammer-shaped sacrificial vias 409 protrude from backsides of the epitaxial source structure 190S by a protruding height H6 and are separated from each other by a lateral distance D6. For example, and without limitation, the protruding height H6 of the hammer-shaped sacrificial vias 409 is in a range from about 40 nm to about 150 nm, and the lateral distance D6 between the hammer-shaped sacrificial vias 409 is in a range from about 20 nm to about 80 nm.Next, as illustrated in Figure 29, a backside ILD layer 410 is formed over the hammer-shaped sacrificial vias 409, the epitaxial source / drain structures 190S / 190D, the replacement gate structures 220, and the inner spacers 170 using suitable deposition techniques, such as a conformal deposition technique such as CVD. Depositing dielectric material into a narrow gap G6 (as indicated in FIG. 28) between the hammer-shaped sacrificial vias 409 results in one or more air gaps 412 (i.e., air-filled gaps) in the resulting backside ILD layer 410 due to the high aspect ratio (i.e., the ratio of gap height (i.e., the protruding height H6 of the hammer-shaped sacrificial vias 409) to the gap width (i.e., the lateral distance D6 between the hammer-shaped sacrificial vias 409)) of the gap G6 between the hammer-shaped sacrificial vias 409. More specifically, the high aspect ratio gap G6 may result in overhangs formed in an upper portion of the gap G6 between the hammer-shaped sacrificial vias 409 during the conformal deposition process, which in turn prevents the dielectric material 410 from filling the gap G6 between the hammer-shaped sacrificial vias 409, leaving one or more air gaps 412 in the resulting backside ILD layer 410.In some embodiments, the conformal deposition process for forming the backside ILD layer 410 is a plasma-free deposition, such as thermal CVD or the like, which may assist in overhang formation and thus the formation of air gaps. In the illustrated embodiment, the air gap 412 may have a width that decreases with increasing distance from the epitaxial drain structure 190D. However, it should be noted that the shape shown in Figure 29 is selected purely for demonstration purposes. For example, the air gap 412 may also comprise other shapes, such as a rectangle, an oval, a square, a trapezoid, a triangle, and / or the like. In some embodiments, the air gap 412 may overlap the epitaxial drain structure 190D.In some embodiments, the backside ILD layer 410 includes materials such as tetraethyl orthosilicate oxide (TEOS) oxide, undoped silicate glass, or doped silicon oxide such as borophosphosilicate glass (BPSG), fused silica (FSG), phosphosilicate glass (PSG), boron-doped silicon glass (BSG), and / or other suitable dielectric materials. In some embodiments, the backside ILD layer 410 has the same material as the frontside ILD layer 210.Once the deposition of the backside ILD layer 410 is completed, the backside ILD layer 410 is thinned until the hammer-shaped sacrificial vias 409 are exposed. The thinning may be accomplished by an etch-back process, a CMP process, or the like. Taking the etchback process as an example, because the hammer-shaped sacrificial vias 409 are formed from SiGe, which is different from the dielectric material of the backside ILD layer 410, the etchant used in the etchback process may be chosen in such a way that the hammer-shaped sacrificial vias 409 have a slower etch rate than the backside ILD layer 410. In this way, the hammer-shaped vias 409 may act as a detectable etch endpoint, which in turn prevents over-etching of the backside ILD layer 410 so that the air gap 412 in the backside ILD layer 410 remains sealed after completion of the etchback process.In the illustrated embodiment, the etch-back process stops at a level height of the top horizontal facet 401 of the epitaxial sacrificial caps 400 to reduce the risk that the air gap 412 may be exposed due to over-etching. However, in some other embodiments, the etch-back time / duration may be fine-tuned to stop at a slightly lower level height, such as at level height 403h between the top and bottom positions of the vertical facet 403, so that the top portions of the epitaxial sacrificial caps 400 may protrude from the backside ILD layer 410 while the air gap 412 remains sealed after completion of the etch-back process.Next, the exposed hammer-shaped sacrificial vias 409 are removed to form backside via openings O7 that extend through the backside ILD layer 410 to expose backsides of the epitaxial source structures 190S. The resulting structure is illustrated in Figure 31. The backside via openings O7 may be hammer-shaped in a cross-sectional view because they inherit the geometry of the hammer-shaped sacrificial via openings 409. More specifically, the backside via openings O7 each have a first portion O71 having a tapered profile with a width that decreases with increasing distance from the epitaxial source structure 190S; a second portion O72 above the first portion O71 having a tapered profile with a width that decreases with decreasing distance from the epitaxial source structure 190S; a third section O73 above the second section O72 having vertical sidewalls and a width that remains unchanged with increasing distance from the epitaxial source structure 190S; and a fourth section O74 above the third section O73 having a tapered profile with a width that decreases with increasing distance from the epitaxial source structure 190S.In some embodiments, where the previous etch-back process performed on the backside ILD layer 410 stops at the level height 403h between the top and bottom positions of the vertical facet 403, the backside via openings O7 are free of the fourth tapered portions O74. In this scenario, the upper portions of the backside via openings O7 are the third portions O73 having vertical sidewalls and the largest widths, which in turn increases the contact area for subsequently formed backside via openings, thereby reducing the contact resistance and further reducing the RC time delay.Next, as illustrated in FIG. 32, source silicide regions 420 are formed on backsides of the epitaxial source structures 190S, respectively, using a silicide process, and then a metal material layer 430 is deposited over the source silicide region 280. The formation processes and materials of the source silicide regions 420 and the metal material layer 430 have already been discussed with respect to the silicide regions 280 and the metal material layer as illustrated in FIG. 23, and thus will not be repeated here in the interest of brevity.The metal material layer 430 is then thinned, for example, using CMP, until the backside ILD layer 410 is exposed. After completion of the CMP process, portions of the metal material layer 430 remain in the respective backside via openings O7 and serve as backside vias 432. A backside MLI structure 300 is then formed over the backside vias 432 and the backside ILD layer 410. The resulting structure is illustrated in FIG. 33. Example details of the CMP process for forming the backside vias 432 have already been discussed in the context of the process for forming the backside vias 292 as illustrated in FIG. 24 and thus will not be repeated here in the interest of brevity. Example formation methods and materials of the backside MLI structure 300 have already been discussed with respect to FIG. 25 and thus will not be repeated here in the interest of brevity.In the illustrated embodiment of Figure 34, the back vias 432 each have a first portion 4321 having a tapered profile with a width that decreases with increasing distance from the epitaxial source structure 190S; a second portion 4322 above the first portion 4321 having a tapered profile with a width that decreases with decreasing distance from the epitaxial source structure 1905; a third portion 4323 above the second portion 4322 having vertical sidewalls and a width that remains unchanged with increasing distance from the epitaxial source structure 1905; and a fourth portion 4324 above the third portion 4323 having a tapered profile with a width that decreases with increasing distance from the epitaxial source structure 190S.In some embodiments, where the previous etch-back process performed on the backside ILD layer 410 stops at the level height 403h between the top and bottom positions of the vertical facet 403 (see FIG. 30 ), the backside via openings 432 are free of the fourth tapered portions 4324. In this scenario, the upper portions of the backside vias 432 are the third portions 4323 with vertical sidewalls and the largest widths, which in turn increases the contact area with the backside power rail 305, thereby reducing the contact resistance and further reducing the RC time delay.From the above discussions, it can be seen that the present disclosure provides advantages. However, it should be understood that other embodiments may provide additional advantages, that not all advantages are necessarily disclosed herein, and that no particular advantage is required for all embodiments. One advantage is that backside vias and backside metal lines (e.g., backside power rails) can be formed on a backside of transistors, which in turn allows for more routing space and thus higher routing density. Another advantage is that one or more backside dielectric layers laterally surrounding the backside vias and / or backside metal lines include one or more air gaps, which in turn reduces capacitive coupling between the backside vias and / or backside metal lines, resulting in lower RC time delay.

Claims

An IC structure comprising: a gate structure (220); an epitaxial source structure (190S) and an epitaxial drain structure (190D), each on opposite sides of the gate structure (220); a front-side interconnect structure (250) on a front side of the epitaxial source structure (190S) and a front side of the epitaxial drain structure (190D); a backside dielectric layer (270, 410) on a backside of the epitaxial source structure (190S) and a backside of the epitaxial drain structure (190D), the backside dielectric layer (270, 410) having an air gap (272, 412); and a backside via (292, 432) extending through the backside dielectric layer (270, 410) to a first one of the epitaxial source structure (190S) and the epitaxial drain structure (190D), wherein the air gap (272, 412) has a width that decreases with increasing distance from the frontside interconnect structure (250), and wherein the air gap (272, 412) overlaps a second one of the epitaxial source structure (190S) and the epitaxial drain structure (190D).The IC structure of claim 1, wherein the rear via (292, 432) has a tapered profile with a width that decreases with increasing distance from the front interconnect structure (250).The IC structure of claim 1, wherein - viewed in an orientation in which a back surface of the structure faces upward - the back via (292, 432) has a first portion (4321) above the first of the epitaxial source structure (190S) and the epitaxial drain structure (190D) and a second portion (4322) above the first portion (4321), the first portion having a width that decreases with increasing distance from the front interconnect structure (250) and the second portion having a width that increases with increasing distance from the front interconnect structure (250).The IC structure of claim 3, wherein the rear via (292, 432) further comprises a third portion (4323) above the second portion (4322), the third portion having a width that remains unchanged with increasing distance from the front interconnect structure (250).The IC structure of claim 4, wherein the rear via (292, 432) further comprises a fourth portion (4324) above the third portion (4323), the fourth portion having a width that decreases with increasing distance from the front interconnect structure (250).The IC structure of any preceding claim, wherein the first of the epitaxial source structure (190S) and the epitaxial drain structure (190D) is the epitaxial source structure (190S).The IC structure of any preceding claim, wherein a second one of the epitaxial source structure (190S) and the epitaxial drain structure (190D) is free of a backside via (292, 432) extending in the backside dielectric layer.The IC structure of claim 7, wherein the second of the epitaxial source structure (190S) and the epitaxial drain structure (190D) is the epitaxial drain structure (190D).The IC structure of any preceding claim, further comprising: a backside interconnect structure (300) on a backside of the backside dielectric layer.An IC structure comprising: a plurality of first channel layers (124) stacked in a spaced-apart manner and a plurality of second channel layers (124) stacked in a spaced-apart manner; a first gate structure (220) surrounding each of the plurality of first channel layers (124) and a second gate structure (220) surrounding each of the plurality of second channel layers (124); a first epitaxial source structure (190S) and an epitaxial drain structure (190D) respectively at opposite end faces of the plurality of first channel layers (124); a second epitaxial source structure (190S) and the epitaxial drain structure (190D) respectively at opposite end faces of the plurality of second channel layers (124); a front-side interconnect structure (250) on a front side of the first epitaxial source structure (190S), a front side of the epitaxial drain structure (190D), and a front side of the second epitaxial source structure (190S); a first back-side via (292, 432) and a second back-side via (292, 432) on a back side of the first epitaxial source structure (190S) and a back side of the second epitaxial source structure (190S), respectively; and a dielectric layer (270, 410) laterally surrounding the first back via (292, 432) and the second back via (292, 432), the dielectric layer (270, 410) having an air gap (272, 412) laterally between the first back via (292, 432) and the second back via (292, 432), the air gap (272, 412) overlapping the epitaxial drain structure (190D), and the air gap (272, 412) having a width that decreases with increasing distance from the epitaxial drain structure (190D).The IC structure of claim 10, further comprising: silicide regions (280, 420) on the backside of the first epitaxial source structure (190S) and the backside of the second epitaxial source structure (190S), respectively.The IC structure of claim 10 or 11, wherein a backside of the epitaxial drain structure (190D) is free of a silicide region.A method of forming a semiconductor device, the method comprising: etching a recess in a substrate (110, 112); forming a sacrificial epitaxial plug (180) in the recess in the substrate (110, 112); forming an epitaxial source structure (190S) and an epitaxial drain structure (190D) over the substrate (110, 112), one of the epitaxial source structure (190S) and the epitaxial drain structure (190D) being formed over the sacrificial epitaxial plug (180); forming a gate structure (150, 220) laterally between the epitaxial source structure (190S) and the epitaxial drain structure (190D); Removing at least a portion of the substrate (110, 110a, 112) such that the epitaxial sacrificial plug (180) protrudes from a backside of the one of the epitaxial source structure (190S) and the epitaxial drain structure (190D); forming a dielectric layer (270, 410) over the epitaxial sacrificial plug (180), the dielectric layer having an air gap (272, 412); removing the epitaxial sacrificial plug (180) to form a backside via opening (O5, O7) extending through the dielectric layer; and forming a backside via (292, 432) in the backside via opening (432).The method of claim 13, wherein forming the epitaxial sacrificial plug (180) is performed such that a first silicon germanium layer is formed in a lower portion of the recess in the substrate (110, 112) and a second silicon germanium layer is formed in an upper portion of the recess in the substrate (110, 112), and the second silicon germanium layer has a lower germanium atomic percentage than the first silicon germanium layer.The method of claim 14, wherein removing the epitaxial sacrificial plug (180) is performed using a selective etching process that etches the first silicon germanium layer at a faster etch rate than etching the second silicon germanium layer.The method of claim 13, 14 or 15, wherein during forming the dielectric layer an overhang (271) is formed at an upper portion of the epitaxial sacrificial plug (180).

Citation Information

Patent Citations

  • Air gap spacer formation for nano-scale semiconductor devices

    US20180047615A1

  • Integrated circuit device with back-side inerconnection to deep source / drain semiconductor

    US20190259699A1

  • Integrated circuit device structures and double-sided fabrication techniques

    US20200035560A1

  • Backside contact resistance reduction for semiconductor devices with metallization on both sides

    WO2018004653A1